Grain-oriented electrical steel sheet
By introducing linear strains with controlled periodic width changes at specific angles and intervals on grain-oriented electrical steel sheets, the challenges of reducing iron loss and noise are addressed, achieving lower core loss and improved magnetic domain refinement.
Patent Information
- Application Number
- PCT/JP2024/016517
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-27
- Filing Date
- 2024-04-26
- Publication Date
- 2024-10-31
AI Technical Summary
Current grain-oriented electrical steel sheets face challenges in reducing iron loss while minimizing noise and hysteresis loss, as existing techniques either inhibit domain wall movement or fail to achieve significant iron loss reduction due to increased hysteresis loss.
Introducing linear strains at angles of 60 to 120 degrees to the longitudinal direction on the surface of the steel sheet, with specific intervals and periodic width changes to control magnetic domain refinement, allowing domain walls to move freely and reduce both eddy current and hysteresis losses.
This approach effectively suppresses hysteresis loss while reducing eddy current loss, resulting in a grain-oriented electrical steel sheet with lower core loss and improved noise characteristics.
Smart Images

Figure JP2024016517_31102024_PF_FP_ABST
Abstract
Description
grain-oriented electrical steel sheet
[0001] The present invention relates to a grain-oriented electrical steel sheet. This application claims priority to Japanese Patent Application No. 2023-073596, filed on April 27, 2023, the contents of which are incorporated herein by reference.
[0002] Grain-oriented electrical steel sheets are soft magnetic materials primarily used as transformer core materials. Therefore, grain-oriented electrical steel sheets are required to have magnetic properties, including high magnetization and low iron loss. Iron loss is the power loss consumed as thermal energy when an iron core is excited by an AC magnetic field. From an energy conservation perspective, iron loss should be as low as possible. The level of iron loss is influenced by factors such as magnetic susceptibility, sheet thickness, coating tension, impurity content, electrical resistivity, grain size, and magnetic domain size. Even with the development of various technologies for grain-oriented electrical steel sheets, research and development continues to reduce iron loss in order to improve energy efficiency. One method for reducing iron loss is laser irradiation of the steel sheet surface. This technique is believed to reduce eddy current loss, a part of iron loss, by introducing strain into the surface through laser irradiation, which subdivides the magnetic domain width by 180°.
[0003] For example, Patent Document 1 discloses a method for producing a steel sheet having a surface irradiated with a focused continuous wave laser beam while scanning the surface in a direction inclined from the rolling direction of the steel sheet, and a method for repeating the process while shifting the area scanned with the continuous wave laser beam at predetermined intervals, in which the average power of the continuous wave laser beam is represented as P (W), the scanning speed as Vc (mm / s), the predetermined interval as PL (mm), and the input energy Ua as Ua = P / (Vc × PL) (mJ / mm 2 ), 1.0 mm ≦ PL ≦ 3.0 mm, and 0.8 mJ / mm 2 ≦Ua≦2.0mJ / mm 2 Patent Document 1 discloses a method for manufacturing a grain-oriented electrical steel sheet in which magnetic domains are controlled by irradiation with laser light, which method is characterized by satisfying the following: Patent Document 1 shows that it is possible to easily reduce iron loss in both the L direction and the C direction of a grain-oriented electrical steel sheet while ensuring high productivity.
[0004] The technology of Patent Document 1 achieves a certain iron loss reduction effect by reducing eddy current loss. However, the iron loss reduction effect is not as great as expected from the division of magnetic domain width, and there is room for improvement. Furthermore, while laser irradiation of grain-oriented electrical steel sheets as proposed in Patent Document 1 is effective in reducing iron loss, there is a problem in that the closure domains formed by laser irradiation increase magnetostriction, thereby degrading noise characteristics.
[0005] Patent Document 2 discloses a method for manufacturing a grain-oriented electrical steel sheet with excellent magnetic properties, in which the iron loss reduction effect is not lost even after stress relief annealing. Patent Document 2 also discloses that in a method for locally forming grooves in a final cold-rolled sheet, by improving the shape of the grooves, it is possible to obtain even lower iron loss than conventional methods.
[0006] However, the technology of Patent Document 2 is insufficient in reducing eddy current loss compared to the technology of imparting minute thermal strain to steel sheet by laser light irradiation and plasma irradiation, and does not take noise characteristics into consideration.
[0007] Patent Document 3 discloses a grain-oriented electrical steel sheet in which strain regions are locally introduced into a surface layer portion of the steel sheet and extending in a direction transverse to the rolling direction, and are formed at periodic intervals s (mm) in the rolling direction, and in each of the strain regions, closure domain regions are formed that are continuous over 200 mm or more in the width direction, and whose width in the rolling direction at the steel sheet surface changes periodically, and each of the closure domain regions satisfies the following conditions: a ratio of a maximum width Wmax to a minimum width Wmin in the rolling direction at the steel sheet surface (Wmax / Wmin) is 1.2 to 2.2, an average width Wave in the rolling direction at the steel sheet surface is 80 μm to 250 μm, a maximum depth D in the sheet thickness direction is 32 μm or more, and (Wave × D) / s is 0.0007 mm to 0.0016 mm.
[0008] Japanese Patent No. 4669565 Japanese Patent Publication No. 6-299244 Direction Japanese Patent No. 6060988
[0009] Patent Document 3 describes that periodically varying the width of the closure domain region in the rolling direction can reduce the magnetostriction harmonic level, thereby achieving both low iron loss and low noise. However, as a result of studies by the present inventors, the technology of Patent Document 3 has found that, because the width of the region where no strain is introduced changes, domain wall movement is hindered and hysteresis loss increases, so the iron loss reduction effect achieved by dividing the magnetic domain width is not fully achieved. Furthermore, the reason why Patent Document 1 does not achieve the expected reduction in iron loss from dividing the magnetic domain width is thought to be because domain wall movement is hindered and hysteresis loss increases.
[0010] In view of the above problems, an object of the present invention is to provide a grain-oriented electrical steel sheet having lower core loss than conventional steel sheets.
[0011] The inventors of the present invention have focused on the fact that, in a technology for achieving low iron loss and low noise by lowering the magnetostriction harmonic level, eddy current loss is reduced but hysteresis loss increases, and have investigated methods for suppressing the increase in hysteresis loss and achieving even lower iron loss. As a result, they have discovered that when magnetic domain refinement is achieved by introducing linear strain into the surface of a grain-oriented electrical steel sheet by laser irradiation or the like, the increase in hysteresis loss can be suppressed by periodically increasing and decreasing the width of the introduced strain and by shifting the period of increase and decrease of the strain width between adjacent linear strains.
[0012] The present invention has been made in light of the above findings. The gist of the present invention is as follows: [1] A grain-oriented electrical steel sheet according to one aspect of the present invention is a grain-oriented electrical steel sheet having a surface into which a plurality of linear strains extending in a direction of 60 to 120° relative to the longitudinal direction are introduced, wherein the spacing between adjacent linear strains in the longitudinal direction is 2 to 10 mm, the width of the linear strains, which is the width in a direction perpendicular to the extension direction of the linear strains, periodically increases and decreases in the extension direction of the linear strains, with a period of 200 to 400 μm, the period of change in the width of adjacent linear strains among the plurality of linear strains is shifted by 0.4 to 0.6 periods in the extension direction of the linear strains, the ratio of the maximum width to the minimum width is 1.2 to 8.0, and the minimum width is 30 μm or more.
[0013] According to the above aspect of the present invention, by realizing magnetic domain refinement that does not hinder domain wall movement, it is possible to suppress an increase in hysteresis loss while reducing eddy current loss, and as a result, it is possible to obtain a grain-oriented electrical steel sheet with low iron loss.
[0014] 1 is a schematic diagram showing an example of a grain-oriented electrical steel sheet according to an embodiment of the present invention, in which linear strain is introduced into the surface. 2 is an example of a graph drawn using ImageJ, in which the horizontal axis represents distance and the vertical axis represents gray value.
[0015] The grain-oriented electrical steel sheet according to one embodiment of the present invention (the grain-oriented electrical steel sheet according to this embodiment) will be described below. As shown in Fig. 1, the grain-oriented electrical steel sheet 1 according to this embodiment is a grain-oriented electrical steel sheet having, on its surface, a plurality of linear strains 2 extending in a direction of 60 to 120° with respect to the longitudinal direction (longitudinal direction of the grain-oriented electrical steel sheet) RD (which can also be said to be a direction of ±30° with respect to the width direction TD), in which the spacing PL between adjacent linear strains 2 in the longitudinal direction RD is 2 to 10 mm, and the width in the direction perpendicular to the extending direction of the linear strains 2 is The width of the linear strain 2 increases and decreases periodically in the extension direction of the linear strain 2, with a cycle CYC of 200 to 400 μm, the cycles of the width changes of adjacent linear strains 2, 2' among the plurality of linear strains 2 are shifted by 0.4 to 0.6 cycles in the extension direction of the linear strain, the ratio of the maximum width Tmax to the minimum width Tmin (Tmax / Tmin) is 1.2 to 8.0, and the minimum width Tmin is 30 μm or more. The reasons for each limitation will be explained below.
[0016] <Multiple linear strains extending in a direction of 60 to 120° relative to the longitudinal direction (rolling direction) are introduced into the surface> <The longitudinal spacing between adjacent linear strains is 2 to 10 mm> In grain-oriented electrical steel sheets, the axis of easy magnetization is aligned in the longitudinal direction (rolling direction in the manufacturing process) RD. When strain is introduced into the surface of the grain-oriented electrical steel sheet by scanning and irradiating an energy beam such as a laser or electron beam in a direction nearly perpendicular to the longitudinal direction, the 180° magnetic domain refining effect further reduces iron loss. In this embodiment, the extension direction of the strain (corresponding to the scanning direction when strain is introduced using an energy beam such as a laser or electron beam) is set at an angle of 60 to 120° relative to the longitudinal direction (rolling direction). If the angle is outside this range, the 180° magnetic domain refining effect of the steel sheet is reduced, and sufficient iron loss reduction effect cannot be achieved. Furthermore, if the spacing between adjacent linear strains in the longitudinal direction (normally the rolling direction) RD exceeds 10 mm, the magnetic domain refinement effect of the 180° magnetic domains is reduced, resulting in insufficient iron loss improvement. Therefore, the longitudinal spacing between adjacent linear strains is set to 10 mm or less. It is preferable that the spacing between the linear strains be approximately equal. On the other hand, while reducing the irradiation spacing generally reduces iron loss, if the spacing is too small, the magnetic domain refinement effect saturates and eddy current loss is hardly reduced, while the increase in hysteresis loss due to the strain becomes significant, resulting in deterioration of iron loss. Furthermore, noise characteristics may deteriorate. Therefore, the longitudinal spacing between adjacent linear strains is set to 2 mm or more. A linear strain is a continuous strain extending in one direction. In this embodiment, its width is intentionally increased or decreased as described below. Here, in this embodiment, the longitudinal spacing PL between the multiple linear strains is the distance from the center of a linear strain to the center of an adjacent linear strain.
[0017] <The width of the linear strain, which is the width perpendicular to the direction of extension of the linear strain, periodically increases and decreases in the direction of extension of the linear strain.> As described above, irradiating a grain-oriented electrical steel sheet with surface energy rays to introduce linear strain can reduce eddy current loss. Meanwhile, the introduced strain inhibits domain wall movement. Iron loss consists of eddy current loss and hysteresis loss, and the introduction of strain increases hysteresis loss within iron loss. While reducing the amount of strain is preferable to prevent an increase in hysteresis loss, a small amount of strain reduces the magnetic domain refining effect. The inventors have discovered that by periodically increasing and decreasing the width of the strain (the width perpendicular to the direction of extension) in a single linear strain, a magnetic domain refining effect can be achieved with a small amount of strain. However, the period and magnitude of the change must be within the ranges described below to achieve a sufficient effect. Here, in this embodiment, "periodically" means that an error of about ±5% or less of the period is allowed (for example, ±10 μm is allowed for 200 μm, and ±20 μm is allowed for 400 μm).
[0018] <The period of change in width of the linear strain is 200 to 400 μm> <The ratio of the maximum width to the minimum width of the linear strain is 1.2 to 8.0> In the grain-oriented electrical steel sheet according to this embodiment, the width of some of the linear strains is changed and some of them are enlarged to control the position where closure domains occur (controlling them to occur from the largest position), thereby controlling the period of change in width and the magnetic domain width. If the ratio of the maximum width to the minimum width of the linear strain (width ratio) is less than 1.2, the result is the same as in the conventional case (when strain of uniform width is introduced), and there is a concern that the closure domains will occur in unintended locations, and sufficient magnetic domain refinement effects will not be achieved. On the other hand, if the width ratio is more than 8.0, there is a concern that the closure domains will occur in unintended locations, and sufficient magnetic domain refinement effects will not be achieved. Therefore, the width ratio is set to 1.2 to 8.0. Regarding the maximum width, it is preferable that when an isosceles triangle is drawn with the length of one period (the length from one valley to the next when the width profile is illustrated) as the base and the position where the linear distortion has the maximum width as the vertex, the base angle of the triangle is 45° or less. To fully achieve the magnetic domain refinement effect, the width of the linear distortion should be 30 μm or more even at its smallest portion (narrowest portion). Furthermore, the period of the width change corresponds to the final magnetic domain width. If the period of change exceeds 400 μm, the magnetic domain width will be wide and sufficient iron loss improvement effect will not be obtained. Furthermore, although shortening the period reduces the magnetic domain width, if the period is too short, the magnetic domain width will correspond to multiple periods (for example, even if the period is 150 μm, the magnetic domain width will be twice that, 300 μm), which may actually widen the magnetic domain width. Therefore, the period of the width change is set to 200 μm or more.
[0019] <Among the multiple linear strains, the width change period of adjacent linear strains is offset by 0.4 to 0.6 periods in the direction perpendicular to the extension direction of the linear strain.> As described above, the width of the introduced strain is periodically changed to obtain a magnetic domain width equal to one period of the strain. However, if multiple linear strains are introduced uniformly, the domain walls become less mobile, and the iron loss reduction effect of the magnetic domain width reduction cannot be fully achieved. This is thought to be because the periodic change in the width of the linear strains causes the width of the non-strained region to vary depending on the position when viewed in the longitudinal direction of the grain-oriented electrical steel sheet, making it difficult for the domain walls to move. Therefore, in the grain-oriented electrical steel sheet according to this embodiment, the width change period of adjacent linear strains among the multiple linear strains is offset to make the width of the non-strained region approximately constant. As shown in FIG. 1 , the period offset is approximately half a period (0.5 periods), and a period offset of 0.4 to 0.6 periods is acceptable. The amount of deviation is evaluated by using the direction perpendicular to the extension direction of the linear distortion as a reference, and the amount of deviation in the extension direction is evaluated in units of periods.
[0020] The locations where linear strain is introduced into grain-oriented electrical steel sheets can be identified using the following method. Specifically, where strain is introduced into the steel sheet, the strain causes distortion in the iron crystal lattice. X-ray topography is used to detect this distortion. An overview of this method is provided below. Normally, when X-rays are incident on a crystal lattice, they are reflected at specific angles of incidence and reflection corresponding to each crystal lattice plane, and in this case, the angles of incidence and reflection are equal. This is called the Bragg diffraction condition. Depending on the degree of distortion in the crystal, i.e., the magnitude of distortion in the iron crystal in this patent, the reflection angle changes slightly relative to the angle of incidence or the reflection intensity is weakened. This analytical method utilizes this phenomenon. For the analysis, a Rigaku XRTmicron X-ray topography system was used, with a Cu target as the X-ray source. The diffraction plane during imaging was the (310) plane of iron. The CCD resolution was 2.4 μm, and the digital resolution was 16 bits. The procedure involves first preparing a sample by cutting a 100 mm section in the rolling direction and a 100 mm section in the width direction of a grain-oriented electrical steel sheet in which strain has been imparted by energy beams. If processing strain is imparted to the steel sheet during processing, it must be done carefully, as this affects the X-ray reflection behavior. Regarding the obtained sample, while an insulating coating is typically applied to the surface of grain-oriented electrical steel sheets, the location of the imparted strain can be identified regardless of whether or not an insulating coating is applied. Therefore, it is important to prepare the sample so as to minimize the imparted strain, depending on the state of the original sample. Then, a topography image is taken in the width direction using SnapShot in high-resolution mode. The field of view during the image capture is 6-7 mm in the width direction and 7-8 mm in the rolling direction. Time delay integration (TDI) scanning may be performed in advance to determine the locations to be captured. Next, the locations of the imparted strain are specifically identified from the captured topography image using image analysis software called ImageJ. For identification, a topography image is developed on ImageJ, and an ROI (Range of Interest) is set as the analysis range (pixel width and height: 2.406 μm). The ROI is rectangular, and its range is 646 pixels (equivalent to approximately 1.55 mm) in the rolling direction and 84 pixels (equivalent to approximately 0.20 mm) in the plate width direction.Hereinafter, the side parallel to the rolling direction will be referred to as the long side of the ROI, and the side parallel to the sheet width direction will be referred to as the short side of the ROI. The ROI is set so that the area where strain has been applied fits within the rectangle. At this time, visual inspection is acceptable, so the area where strain has been applied should be set so that it is located at the center of the long side of the ROI. Once the ROI has been set, a graph is drawn within the set ROI range, with the horizontal axis representing DISTANCE and the vertical axis representing GRAY VALUE. The graph drawing function is part of the functions of ImageJ, and this function will be used. This results in a spectrum with a negative peak, as shown in Figure 2. The gray scale is read for the plateau-shaped portions at both ends of the spectrum, and their average value is calculated. Hereinafter, this average value will be referred to as I. Ave. The negative peak intensity (minimum value of the spectrum) in the spectrum is called I Bottom Let's say. Ave. and I Bottom The difference is ΔI Height Here, I can be defined by the following formula: HH The concept of (Half Height) is introduced. HH is the Gray Scale value corresponding to half the peak intensity. The width W of the strained portion is defined as I HH is defined as the distance between two points corresponding to I. HH = I Height + (0.5 × I Height ) ... (1)
[0021] <Manufacturing Method> The grain-oriented electrical steel sheet according to this embodiment can achieve the effects described above, regardless of the manufacturing method. However, a manufacturing method including the following configuration is preferable because it allows relatively stable manufacturing. (1) An irradiation step of irradiating the surface of a grain-oriented electrical steel sheet obtained by a known method with energy rays at approximately constant intervals of 2 to 10 mm in the longitudinal direction by scanning in a direction of 60 to 120° with respect to the longitudinal direction while periodically changing the width (thickness) of the energy rays in the direction perpendicular to the scanning direction, thereby introducing multiple linear strains into the grain-oriented electrical steel sheet.
[0022] The grain-oriented electrical steel sheet to be irradiated with energy rays may be a steel sheet obtained by a known method, for example, a grain-oriented electrical steel sheet that satisfies JIS C2553: 2019. The grain-oriented electrical steel sheet preferably has a magnetic flux density B8 (magnetic flux density at 800 A / m) of 1.90 T or more, and more preferably has a B8 of 1.92 T or more.
[0023] The energy beam is irradiated by scanning the energy beam in a direction of 60 to 120° relative to the longitudinal direction at approximately constant intervals of 2 to 10 mm in order to introduce multiple linear strains extending in a direction of 60 to 120° relative to the longitudinal direction, with adjacent linear strains spaced 2 to 10 mm apart in the longitudinal direction (rolling direction). The energy beam is preferably a continuous wave laser in order to obtain continuous linear strain in the extension direction. Furthermore, since electron beams and pulsed waves tend to cause strain in the sheet width direction, a continuous wave laser is preferably used. Known conditions for the laser irradiation can be used as long as they are within the range in which strain can be introduced into the surface of the grain-oriented electrical steel sheet.
[0024] In the case of a continuous wave laser, when scanning with a polygon mirror, the width of the energy beam in the direction perpendicular to the scanning direction can be changed periodically by installing a shutter with a width that varies periodically in the scanning direction immediately after the lens. Also, by changing the position of the shutter during scanning, the period of the width change can be shifted when shifting the period of adjacent linear distortions within a desired range.
[0025] A grain-oriented electrical steel sheet with a Si content of 3.25% and a thickness of 0.23 mm was prepared. The magnetic flux density B8 of this grain-oriented electrical steel sheet was 1.93 T, and the iron loss W17 / 50 was 0.90 W / kg. This grain-oriented electrical steel sheet was scanned and irradiated with a continuous wave laser in the longitudinal direction (rolling direction) at a constant interval (pitch) shown in Table 1, in the direction (angle relative to the longitudinal direction) shown in Table 1. During scanning, scanning was performed using a polygon mirror, and a shutter with a periodically varying width in the scanning direction was installed immediately after the lens, thereby changing the strain width at the period shown in Table 1. The shift in the period of change in strain width between adjacent linear strains was as shown in Table 1. The magnetic properties of the obtained grain-oriented electrical steel sheet were evaluated as follows.
[0026] [Magnetic Property Evaluation] A sample measuring 60 mm wide and 300 mm long was taken from the center of the sheet width of each grain-oriented electrical steel sheet. The length of the sample was parallel to the rolling direction. Using this sample, the magnetic flux density was determined by a single sheet magnetic property test (SST test) in accordance with JIS C 2556 (2015). Specifically, a magnetic field of 800 A / m was applied to the sample to determine the magnetic flux density B8 (T). Furthermore, using the above sample, the iron loss W17 / 50 (W / kg) was measured at a frequency of 50 Hz and a maximum magnetic flux density of 1.7 T in accordance with JIS C 2556 (2015). In addition, a hysteresis loop was measured at a maximum magnetic flux density of 1.7 T, and the eddy current loss was calculated from the obtained hysteresis loss and W17 / 50. The results are shown in Table 2.
[0027]
[0028]
[0029] As can be seen from Tables 1 and 2, in Invention Examples Nos. 2, 3, 5, 7, 11 to 16, 18, 20, 21, 24 to 26, 30, and 31, in which multiple linear strains whose widths changed at a predetermined period were introduced at predetermined intervals in a predetermined direction, the iron loss (W17 / 50) was low, at 0.79 W / kg or less. In contrast, in Comparative Examples Nos. 1, 4, 6, 8 to 10, 17, 19, 22, 23, and 27 to 29, at least one of the period of change in width of the linear strain, maximum / minimum strain width, minimum strain width, periodic shift, spacing between the multiple linear strains, and extension direction was outside the range of the present invention, and the iron loss was large.
[0030] According to the present invention, by realizing magnetic domain refinement that does not inhibit domain wall movement, it is possible to suppress an increase in hysteresis loss while reducing eddy current loss, and as a result, it is possible to obtain a grain-oriented electrical steel sheet with low iron loss, which has high industrial applicability.
[0031] 1 Grain-oriented electrical steel sheet 2 Linear strain 2' Linear strain adjacent to 2 RD Longitudinal direction of steel sheet (grain-oriented electrical steel sheet) TD Width direction of steel sheet (grain-oriented electrical steel sheet) PL Spacing of linear strain in the longitudinal direction of steel sheet (grain-oriented electrical steel sheet) CYC Period Tmin Minimum width Tmax Maximum width
Claims
1. A grain-oriented electrical steel sheet having a surface on which a plurality of linear strains extending in a direction of 60 to 120 degrees to the longitudinal direction have been introduced, wherein the longitudinal spacing between adjacent ones of the plurality of linear strains is 2 to 10 mm, the width of the linear strains, which is the width perpendicular to the extension direction of the linear strains, periodically increases and decreases in the extension direction of the linear strain, with the period being 200 to 400 μm, the period of change in the width of adjacent ones of the plurality of linear strains is shifted by 0.4 to 0.6 periods in the extension direction of the linear strain, the ratio of the maximum width to the minimum width is 1.2 to 8.0, and the minimum width is 30 μm or more.
Citation Information
Patent Citations
Manufacture of silicon steel sheet having excellent magnetic characteristic
JP1994299244A
Abnormal occurrence location determining device, abnormal occurrence location determining method, and program
JP2023073596A
A method for manufacturing grain-oriented electrical steel sheets in which magnetic domains are controlled by laser irradiation.
JP4669565B2
Grain-oriented electrical steel sheet and its manufacturing method
JP6060988B2
Manufacturing method of grain oriented electric steel plate having excellent magnetic characteristic
JP2007277644A