Battery life prediction method, device, equipment, medium and program product
By performing charging and discharging cycles on the battery samples under different temperature conditions, fitting the capacity loss curve and creating prediction standard equations, the problem of low battery life prediction efficiency in the prior art is solved, and efficient and accurate battery life prediction is achieved.
Patent Information
- Application Number
- CN202411473954.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-21
- Publication Date
- 2024-12-20
- Estimated Expiration
- 2044-10-21
AI Technical Summary
The prior art tests the capacity attenuation during battery cycles at different ambient temperatures to consume a lot of manpower and material resources, resulting in a significant increase in testing costs and time, and it is difficult to improve the efficiency of battery life prediction.
By obtaining multiple battery samples from the same batch, charging and discharging cycles are carried out under multiple different preset temperature conditions, the discharge capacity data corresponding to different cycles under each preset temperature condition is extracted, and the capacity loss curve is fitted and generated. The capacity loss prediction standard equation is created with temperature and cycle number as independent variables and the capacity loss rate as the dependent variable, which is used to predict battery life.
It significantly improves the efficiency of battery life prediction, reduces the demand for repeated charge and discharge cycle tests, reduces the cost and time of testing, and has high accuracy in prediction results.
Smart Images

Figure CN119165389A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of lithium-ion battery optimization cells, and in particular to a battery life prediction method, device, equipment, medium and program product. Background Art
[0002] With the popularity of new energy vehicles, consumers are increasingly demanding electric vehicles with fast battery charging. However, different charging strategies have different expansion degrees during the battery aging process. When the battery expands to a certain threshold, it will squeeze the battery module, causing a series of safety issues such as capacity diving, battery lithium deposition, and even battery deformation. Therefore, battery life prediction is particularly important. One method of battery life prediction is to obtain the relationship between the number of battery charge and discharge cycles and the change in battery capacity. However, testing the capacity decay during the battery cycle at different ambient temperatures requires a lot of manpower and material resources. For example, if a user wants to obtain the relationship between the battery capacity and the number of battery cycles under the conditions of 10℃, 12℃, 14℃, 16℃, 18℃, and 20℃, the relevant technology needs to perform battery charge and discharge cycles separately under each temperature condition, and then count the battery capacity changes under each temperature condition, so as to measure the relationship between the battery capacity and the number of battery cycles. This method leads to a significant increase in testing costs and time. Therefore, how to reduce testing costs and time and improve the efficiency of battery life prediction while ensuring prediction accuracy is still an urgent problem to be solved. Summary of the invention
[0003] In view of this, the present invention provides a battery life prediction method, device, equipment, medium and program product to solve the problem of low efficiency of battery life prediction.
[0004] In a first aspect, the present invention provides a battery life prediction method, the method comprising: obtaining multiple battery samples from the same batch; performing charge and discharge cycles on different battery samples under multiple different preset temperature conditions; during the charge and discharge cycle process, extracting discharge capacity data corresponding to different numbers of cycles under each preset temperature condition for the battery samples; fitting and generating capacity loss curves under each preset temperature condition based on the extracted discharge capacity data, the capacity loss curve being used to represent the capacity loss rate that varies with the number of cycles; using the capacity loss curves under each preset temperature condition, fitting a standard capacity loss prediction equation with temperature and number of cycles as independent variables and capacity loss rate as dependent variable; obtaining a target temperature for a scenario to be predicted, and substituting the target temperature into the standard capacity loss prediction equation to obtain a capacity loss curve for predicting battery life under the scenario to be predicted, and predicting battery life through the capacity loss curve.
[0005] In a second aspect, the present invention provides a battery life prediction device, which includes: a sample acquisition module for acquiring multiple battery samples from the same batch; a cycle test module for performing charge and discharge cycles on different battery samples under multiple different preset temperature conditions; a capacity data acquisition module for extracting discharge capacity data corresponding to different numbers of cycles under each preset temperature condition for the battery sample during the charge and discharge cycle; a capacity loss curve generation module for fitting and generating capacity loss curves under each preset temperature condition based on the extracted discharge capacity data, the capacity loss curve being used to represent the capacity loss rate that varies with the number of cycles; a first equation generation module for using the capacity loss curves under each preset temperature condition to fit a standard capacity loss prediction equation with temperature and number of cycles as independent variables and capacity loss rate as a dependent variable; a capacity loss prediction module for acquiring a target temperature for a scene to be predicted, and substituting the target temperature into the standard capacity loss prediction equation to obtain a capacity loss curve for predicting battery life under the scene to be predicted.
[0006] In a third aspect, the present invention provides a computer device, comprising: a memory and a processor, the memory and the processor being communicatively connected to each other, the memory storing computer instructions, and the processor executing the method of the first aspect by executing the computer instructions.
[0007] In a fourth aspect, the present invention provides a computer-readable storage medium having computer instructions stored thereon, the computer instructions being used to enable a computer to execute the method of the first aspect.
[0008] In a fifth aspect, the present invention provides a computer program product, comprising computer instructions, wherein the computer instructions are used to enable a computer to execute the method of the first aspect.
[0009] The technical solution provided by the present invention has the following advantages:
[0010] The present invention utilizes multiple battery samples from the same batch to perform charge and discharge cycles under multiple different preset temperature conditions. During the charge and discharge cycle process, the discharge capacity data corresponding to different numbers of cycles under each preset temperature condition are extracted from the battery sample, so as to fit and generate the capacity loss curve under each preset temperature condition. The capacity loss curve is used to represent the capacity loss rate that varies with the number of cycles; then, a capacity loss prediction standard equation with two independent variable parameters is created with temperature and number of cycles as independent variables and capacity loss rate as dependent variable. In the subsequent life prediction project, the R&D personnel only need to obtain the target temperature of the scenario to be predicted, and substitute the target temperature into the capacity loss prediction standard equation to obtain the capacity loss curve used to predict the battery life under the scenario to be predicted. There is no need to repeat the charge and discharge cycle test according to the target temperature. The capacity loss curve is obtained through the capacity loss prediction standard equation, which significantly improves the efficiency of battery life prediction. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0012] Figure 1 is a schematic flow chart of a battery life prediction method according to an embodiment of the present invention;
[0013] Figure 2 is a schematic diagram of a capacity loss prediction standard equation fitting process according to an embodiment of the present invention;
[0014] Figure 3 3 is a schematic diagram of the comparison effect between the calculated capacity retention rate curve and the experimental capacity retention rate curve according to an embodiment of the present invention;
[0015] Figure 4 is a graph showing the relationship between the capacity loss rate and the battery expansion thickness according to an embodiment of the present invention;
[0016] Figure 5 is a schematic diagram of the comparison effect between the calculated thickness growth curve and the experimental thickness growth data according to an embodiment of the present invention;
[0017] Figure 6 2 is a schematic diagram showing the effect of a capacity decay curve and a capacity retention rate curve according to an embodiment of the present invention;
[0018] Figure 7 is a schematic diagram of the comparison effect of the capacity loss rate curve and the battery thickness growth curve according to an embodiment of the present invention;
[0019] Figure 8 is a schematic diagram of the structure of a battery life prediction device according to an embodiment of the present invention;
[0020] Fig. 9 It is a schematic diagram of the hardware structure of a computer device according to an embodiment of the present invention. DETAILED DESCRIPTION
[0021] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present invention.
[0022] According to an embodiment of the present invention, an embodiment of a battery life prediction method is provided. It should be noted that the steps shown in the flowchart of the accompanying drawings can be executed in a computer system such as a set of computer executable instructions, and although a logical order is shown in the flowchart, in some cases, the steps shown or described can be executed in an order different from that shown here.
[0023] In this embodiment, a battery life prediction method is provided. Figure 1 is a flow chart of a battery life prediction method according to an embodiment of the present invention, the flow chart includes the following steps:
[0024] Step S101, obtaining a plurality of battery samples from the same batch.
[0025] Step S102 , performing charge and discharge cycles on different battery samples under a plurality of different preset temperature conditions.
[0026] Step S103 , during the charge and discharge cycle process, the discharge capacity data corresponding to different cycle numbers under various preset temperature conditions are extracted from the battery sample.
[0027] Specifically, the present invention provides a mathematical model of high-temperature capacity loss rate, cycle number and temperature established using historical data, which can effectively calculate the capacity loss rate curve of the target battery at different temperatures and predict the battery life (excluding capacity diving). Compared with the prior art, the method of the present invention is simple, efficient and highly practical. In order to calculate the above mathematical model, the first preparation required is to obtain multiple battery samples from the same batch to ensure that the consistency of each battery sample is good, so as to ensure that the initial state of each battery sample is the same, and the experimental data collected subsequently will have higher reliability in the model creation process.
[0028] Afterwards, this embodiment performs charge and discharge cycles on different battery samples under multiple different preset temperature conditions. To ensure the accuracy of the model, the cycle test requires at least 3 groups of different temperature conditions, one of which is the reference temperature and the rest are comparison temperatures. The cycle test temperature selection range of the embodiment of the present invention is 0°C-80°C, wherein the standard temperature is preferably 25°C. The more comparison temperature groups are set, the more accurate the prediction results are. For example, the first battery sample is charged and discharged at 25°C, the second battery sample is charged and discharged at 35°C, the third battery sample is charged and discharged at 45°C, and the fourth battery sample is charged and discharged at 60°C. This is only an example and is not limited to this.
[0029] Afterwards, during the charge and discharge cycle, the discharge capacity data corresponding to different cycle numbers are extracted for each of the above battery samples. In the embodiment of the present invention, the number of cycle tests is set between 50 and 1000. Under the premise of no lithium precipitation, the more cycles, the more accurate the prediction results. For example, the discharge capacity data of 0, 50, 100, and 150 cycles are recorded. The above parameter selection is only for example, and other values not listed in the numerical range are also applicable.
[0030] Step S104, generating a capacity loss curve under various preset temperature conditions by fitting according to the extracted discharge capacity data, wherein the capacity loss curve is used to represent the capacity loss rate that varies with the number of cycles.
[0031] Specifically, the discharge capacity data extracted through the above steps S101 to S103 can be used to calculate the capacity loss caused by the increase in the number of cycles under different preset temperature conditions. The embodiment of the present invention specifically calculates the capacity loss rate that varies with the number of cycles to obtain a capacity loss curve. For example, the capacity loss curves under 25°C / 35°C / 45°C / 60°C are calculated respectively. The specific calculation method of the capacity loss rate is a prior art and will not be repeated in the embodiment of the present invention.
[0032] Step S105 , using the capacity loss curves under various preset temperature conditions, a standard capacity loss prediction equation is fitted with temperature and cycle number as independent variables and capacity loss rate as a dependent variable.
[0033] Step S106, obtaining the target temperature of the scenario to be predicted, and substituting the target temperature into the standard equation for capacity loss prediction to obtain a capacity loss curve for predicting the battery life in the scenario to be predicted, and predicting the battery life through the capacity loss curve.
[0034] Specifically, after obtaining the capacity loss curves under several typical temperature conditions, the embodiment of the present invention finds the change law of the overall capacity loss curve with temperature, takes the temperature as an independent variable on the basis of the number of cycles as an independent variable, and creates a capacity loss prediction standard equation including two independent variable parameters, temperature and number of cycles, and a capacity loss rate as a dependent variable parameter. Based on this equation, when researchers want to predict the capacity loss of the battery with the number of cycles under any temperature conditions, they can directly substitute the target temperature into the capacity loss prediction standard equation, and the obtained new equation can represent the capacity loss curve under the target temperature conditions, and the battery life can be predicted through this capacity loss curve.
[0035] Through the technical solution provided by the embodiment of the present invention, there is no need to repeat the charge and discharge cycle test on the battery sample each time according to the target temperature required by the user. The capacity loss curve under any temperature condition can be obtained by the capacity loss prediction standard equation provided by the embodiment of the present invention, and then the life prediction can be performed, which significantly improves the efficiency of battery life prediction.
[0036] In some optional implementations, the above step S105 includes:
[0037] Step a1, creating a standard equation for capacity loss prediction before coefficient solution based on the Arrhenius formula;
[0038] Step a2, taking the logarithm of the capacity loss prediction standard equation before solving;
[0039] Step a3, plotting a solution curve of the standard capacity loss prediction equation with the logarithmic number of cycles as the X-axis and the logarithmic capacity loss rate as the Y-axis;
[0040] Step a4, taking values from the capacity loss curve under each preset temperature condition, substituting them into the solution curve, and solving the coefficients of the capacity loss prediction standard equation according to the slope and intercept of the solution curve to obtain the solved capacity loss prediction standard equation.
[0041] Specifically, lithium batteries, as a commonly used rechargeable battery, have the advantages of high energy density and long cycle life, and are widely used in mobile devices. However, as the use time increases, the capacity of lithium batteries gradually decreases, eventually leading to the end of the battery life. Therefore, accurately predicting the life of lithium batteries is of great significance for battery design and application. The Arrhenius formula is a mathematical model that can be used to predict the life of lithium batteries. This formula is based on the relationship between the cycle life and capacity loss of lithium batteries, and can predict the life of batteries by measuring the capacity decay rate of the battery. However, the adaptation of the Arrhenius formula in the related art discards the temperature parameter, and often creates a battery life prediction equation based on the relationship between the cycle life and capacity loss of the battery, and does not apply the relationship between the chemical reaction rate constant and temperature to the capacity loss prediction. For example, the Arrhenius formula commonly used in the related art to predict battery life is:
[0042] N=A′*e B′*Q
[0043] Where N represents the number of cycles, A′ and B′ are the coefficients of the Arrhenius formula, and Q represents the capacity loss.
[0044] It can be seen that the above formula cannot determine the variation law of capacity loss with the number of cycles under any temperature conditions. The embodiment of the present invention improves and adjusts the Arrhenius formula to create a capacity loss rate prediction equation for the temperature independent variable and the number of cycles independent variable, that is, a capacity loss prediction standard equation, and the specific formula is as follows:
[0045]
[0046] In the formula, x represents the number of cycles, y represents the capacity loss rate, T represents the temperature, and A, B and C are the coefficients of the equation.
[0047] In the above formula, if A, B and C can be solved, and then any temperature T is substituted into the solved equation, the capacity loss curve under any temperature condition can be determined.
[0048] Based on this, the embodiment of the present invention adopts an expensive solution method to solve the coefficients of the standard equation for capacity loss prediction using the capacity loss curve under each preset temperature condition, thereby solving the equation coefficients A, B and C. The principle of the expensive solution method is to take the logarithm of both sides of the equal sign of the standard equation for capacity loss prediction, and the formula can be changed to ln(y)=C*ln(x)+ln(A)+B*1 / T. By drawing the solution curve with ln(x) as the X-axis and ln(y) as the Y-axis, the slope of the solution curve is C, and the intercept is ln(A)+B*1 / T. The values of the capacity loss curves at different temperatures obtained from the above experiments are substituted into the solution curve ln(y)=C*ln(x)+lnA+B*1 / T and the graph is drawn, and the specific values of C and lnA+B*1 / T at different temperatures can be determined, where the coefficient C can be obtained by taking the average value of the slopes of each temperature condition. Then, the intercept Z = ln(A) + B*1 / T is plotted in the same way. The Z value and 1 / T under the above-mentioned temperature conditions are plotted with 1 / T as the horizontal axis and the Z value as the vertical axis. The slope of the curve is the coefficient B, and the intercept of the curve is the logarithm of the coefficient A, ln(A), so that the three empirical parameters A, B and C are fitted.
[0049] An example is given to illustrate the specific solution process:
[0050] In this embodiment, a 2.5Ah lithium-ion battery is taken as an example. The charge and discharge cycle test temperature conditions are 25°C / 35°C / 45°C / 60°C, wherein 25°C is the reference temperature; the cycle test ratio is 1C, and the charge and discharge mode is static-constant current constant voltage charging-static-constant current discharge cycle, the charge cut-off voltage is 3.65V, the discharge cut-off voltage is 2.5V, the static time is 30min, the cycled battery cell is taken out of the cabinet at 0 / 250 / 700 cycles, and the thickness is measured with a micrometer at room temperature, wherein the battery cell is discharged at 0.05C to 0% SOC at room temperature before the test.
[0051] During the charge and discharge cycle test, the capacity loss curves under various temperature conditions are obtained through the processing of the above step S104, for example, four curves under four temperature conditions of 25°C / 35°C / 45°C / 60°C, and then the capacity loss rate and the number of cycles are logarithmically plotted with ln(x) as the X-axis and ln(y) as the Y-axis. Figure 2 As shown in (a), since the first 10 cycles (ln value is less than 2) belong to the initial stage of film formation, after 100 cycles (ln value is greater than 4), the film layer is stable and more in line with the linear model, so the embodiment of the present invention only fits the curve after 100 cycles. Figure 2 The slope of each curve in (a) is C = 0.79, and then according to Figure 2(a) The vertical intercepts of the different temperature curves with the Y axis can be determined, and then the vertical intercepts under the four temperature conditions can be plotted against the four temperature parameters 1 / T and connected into a straight line as shown below: Figure 2 (b) Figure 2 (b) The slope of the curve is the coefficient B, Figure 2 The new intercept in (b) is ln(A), and the fitted curve satisfies the functional relationship y=-1249.6x+0.9422, so A=e 0.94 , B = -1250. Finally, the solved capacity loss prediction standard equation is:
[0052]
[0053] If different temperatures (25℃ / 35℃ / 45℃ / 60℃) are substituted into the above fitted capacity loss prediction standard equation The capacity loss curve of lithium-ion soft-pack batteries at the corresponding temperature can be calculated, and the calculated capacity loss curve can be compared with the experimental capacity loss curve (such as Figure 3 As shown, the capacity loss curve is converted into the capacity retention rate for comparison, where groups G, H, I, and J are experimental data). It is verified that the calculated curve is in good agreement with the actual test curve.
[0054] Furthermore, when the user wants to predict the battery life under any target temperature condition (such as 55°C, which is only an example and not limited to this), the target temperature can be directly substituted into the above formula after solution: The capacity loss curve at the target temperature is obtained, and then the battery life is predicted according to the change law of the capacity loss curve. The technical solution provided by the embodiment of the present invention eliminates the need to repeat the charge and discharge cycle test according to the target temperature, and the capacity loss curve is obtained by the capacity loss prediction standard equation, which significantly improves the efficiency of battery life prediction.
[0055] In some optional implementations, the present invention provides a battery life prediction method, further comprising:
[0056] Step b1, during the charge and discharge cycle, collecting thickness expansion data of the battery sample under each preset temperature condition at a preset period;
[0057] Step b2, extracting a number of expansion sub-data with the same number of cycles at different temperatures from the thickness expansion data;
[0058] Step b3, determining the thickness-capacity relationship of the battery sample according to the expansion sub-data and the corresponding discharge capacity data under the same conditions, and obtaining a thickness-capacity relationship equation, the thickness-capacity relationship is used to express the relationship between the thickness growth rate and the capacity loss rate of the battery;
[0059] Step b4, substituting the thickness-capacity relationship equation into the standard capacity loss prediction equation to obtain a thickness prediction standard equation with temperature and cycle number as independent variables and thickness growth rate as dependent variable;
[0060] Step b5, substituting the target temperature into the thickness prediction standard equation to obtain a thickness growth curve for predicting the battery life in the scenario to be predicted, and predicting the battery life through the thickness growth curve.
[0061] Specifically, in addition to predicting battery life through the relationship between capacity loss rate and number of cycles, predicting battery life through the relationship between the number of cycles and changes in battery thickness is also a common method. However, related technologies also face the problem of different changing characteristics at different temperatures, which requires testing the degree of battery expansion at different ambient temperatures, wasting a lot of human resources.
[0062] The embodiment of the present invention considers that if a mathematical model similar to the above capacity prediction can be created and any temperature data is substituted, the relationship between the battery thickness and the number of cycles at any temperature can be obtained, which can further improve the prediction efficiency of the battery life.
[0063] To implement the above scheme, in the embodiment of the present invention, during the charge and discharge cycle process of the above step S102, the thickness expansion data of the battery sample under each preset temperature condition is also collected at a preset period. For example, the number of cycle test turns is between 50-1000. Under the premise of no lithium precipitation, the more cycles, the more accurate the prediction result; the interval of the thickness test collection turns during the cycle test is 50-500 turns. The more data collected, the more accurate the prediction result. Battery cell thickness collection tools include but are not limited to calipers, thickness gauges, force distance sensors, and displacement sensors.
[0064] Afterwards, the embodiment of the present invention statistically discovered the law between battery thickness expansion and capacity change based on measured data, and the specific steps include: 1. First, extract expansion sub-data with the same number of cycles at different temperatures from the thickness expansion data, for example, extract expansion sub-data of 50 cycles at 25°C, expansion sub-data of 50 cycles at 35°C, expansion sub-data of 50 cycles at 45°C, and expansion sub-data of 50 cycles at 60°C from the thickness expansion data obtained during the entire experimental process. 2. Then compare and analyze the above expansion sub-data with the discharge capacity data under four temperature conditions when the cycle is 50 cycles, determine the relationship between battery thickness and capacity under a fixed number of cycles, and obtain the thickness-capacity relationship equation.
[0065] like Figure 4As shown, taking 250 cycles and 700 cycles as examples, the embodiment of the present invention determines through analysis that there is a linear relationship between the thickness growth rate and the capacity loss rate of the battery. The physical meaning of this law is that most of the capacity loss caused by active lithium is used for film formation, and there is a linear relationship between the film thickness growth and the active lithium consumption. Therefore, the thickness capacity relationship equation determined by the embodiment of the present invention through analysis is:
[0066] y=E*d+F
[0067] Where y represents the capacity loss rate, d represents the thickness growth rate, and E and F are the coefficients of the thickness-capacity relationship equation.
[0068] After finding the relationship between capacity loss rate and thickness growth rate, the thickness-capacity relationship equation is substituted into the aforementioned standard capacity loss prediction equation. After transformation and arrangement of the equation, the thickness prediction standard equation with temperature and number of cycles as independent variables and thickness growth rate as dependent variable can be calculated. The specific formula is as follows:
[0069]
[0070] Where x represents the number of cycles, T represents the temperature, A, B, C and E are equation coefficients, d represents the thickness growth rate, T0 represents the reference cycle temperature, and d0 represents the thickness growth rate at the reference temperature.
[0071] Similarly, if Figure 5 As shown in the figure, by substituting different temperatures (25℃ / 35℃ / 45℃ / 60℃) into the above thickness prediction standard equation, the thickness growth curve of the lithium-ion soft-pack battery at this temperature can be calculated, and then the actual test cell thickness change data at different temperatures (25℃ / 35℃ / 45℃ / 60℃) can be marked on Figure 5 After comparison, it is found that the actual test data is in good agreement with the model, so the method provided in the embodiment of the present invention can accurately calculate the cell cycle thickness growth results at different temperatures and has universal applicability.
[0072] In the subsequent battery life prediction process, users can input any target temperature into the standard thickness prediction equation to obtain the thickness growth curve under the target temperature conditions, and use the thickness growth curve to analyze the growth pattern of the battery thickness with the number of cycles, thereby accurately predicting the battery life.
[0073] The technical solution provided by the embodiment of the present invention correlates capacity loss, active lithium film consumption reaction, and film thickness, thereby integrating the three parameters of temperature / number of cycles / thickness. After establishing a model through a small amount of tests, not only can the capacity decay and thickness change at all temperatures be derived, but there is no need to re-model each time a temperature is changed, which significantly improves the efficiency of battery life prediction.
[0074] In some optional implementation manners, before the above step b1, the method further includes:
[0075] Step c1, adjusting each battery sample to the same SOC at a preset current rate under the same temperature condition.
[0076] Specifically, before collecting thickness data, the embodiment of the present invention adjusts each battery sample to the same SOC at a preset current rate. For example, the battery cell may be adjusted to the same SOC at a rate of 0.05C at 25±2°C, including but not limited to 0%, 50% and 100% SOC, etc. The present invention is only taken as an example and is not limited thereto. Because the battery has a reversible thickness change at different SOCs (this phenomenon is caused by different amounts of lithium embedded), and because it is a reversible thickness change, it will not cause safety risks in the later stage. However, when collecting thickness data, this embodiment needs to ensure that this reversible thickness remains consistent on each battery cell sample, so as to ensure that the batteries are adjusted to the same state, thereby ensuring that the thickness data finally collected is an irreversible thickness increase, avoiding poor consistency in thickness data collection due to different reversible thickness changes between battery samples, thereby reducing data errors and improving the accuracy of subsequent model creation.
[0077] In a specific application embodiment, the technical solution provided by the embodiment of the present invention is described as follows, so that the implementation process of how the present application applies technical means to solve technical problems and achieve technical effects can be fully understood and implemented accordingly.
[0078] 1. Prepare multiple battery samples of the same batch with good consistency. This embodiment takes a 2.5Ah soft lithium-ion battery as an example. Record the initial thickness data of each battery sample. Adjust the battery cells to the same SOC at a small current rate at the same temperature, including but not limited to 0%, 50% and 100% SOC, etc., preferably adjust to 0% SOC at 0.05C at 25°C.
[0079] 2. Perform cycle tests on the test battery samples at different temperatures. For example, one battery sample is subjected to cycle test at one temperature. In this embodiment, four battery samples are subjected to cycle test at four temperature conditions of 25°C / 35°C / 45°C / 60°C, respectively. The cycle test ratio is 1C, and the charge and discharge mode is static-constant current constant voltage charging-static-constant current discharge cycle. The charge cut-off voltage is 3.65V, the discharge cut-off voltage is 2.5V, the static time is 30min, and the cycle cells are taken off the cabinet at 0 / 250 / 700 cycles.
[0080] 3. During the cyclic test, the thickness expansion data after a certain number of cycles at different temperatures are measured regularly. The thickness collection tools include but are not limited to calipers, thickness gauges, force distance sensors and displacement sensors. The collection interval of the thickness test during the cyclic test is 50-500 cycles, that is, the thickness is collected every 50 cycles, and then the battery expansion thickness is calculated using the collected thickness expansion data.
[0081] 4. After the cycle is completed, the discharge capacity data at different temperatures and different cycle times are extracted, and the capacity loss rate of each battery sample is calculated. The discharge capacity data of this cycle test is as follows: Figure 6 As shown in (a), it can be seen that the higher the cycle temperature, the higher the initial capacity performance. This is because the higher the temperature, the higher the battery cell kinetic performance; the capacity retention rate curve of the battery cell can be calculated based on the initial capacity, as shown in Figure 6 (b) shows the capacity retention rate curve. The capacity retention rate is inversely proportional to the capacity loss rate. The higher the temperature, the faster the capacity decay of the battery cell. This is because the higher the temperature, the more side reactions of the battery cell film formation or repair of SEI (Solid Electrolyte Interface), the greater the consumption of active lithium, and the faster the capacity decay. Figure 7 (a) and Figure 7 (b) As shown in the comparison, the capacity loss curve obtained by the test is compared with the thickness growth curve. Both have the same growth trend. This is because most of the active lithium with capacity loss is used for the growth of SEI, so both the capacity loss curve and the thickness growth curve can be used to predict battery life.
[0082] 5. Using the data collected in the above steps, the capacity loss rate and the number of cycles during different temperature cycles are fitted and calculated using the improved Arrhenius formula. The fitting relationship is:
[0083]
[0084] In the formula, x represents the number of cycles, y represents the capacity loss rate, T represents the temperature, and A, B and C are the coefficients of the equation.
[0085] The fitting process is as follows: First, take the logarithm of the capacity loss rate and the number of cycles obtained from the cycle test, and draw a graph with ln(x) as the X-axis and ln(y) as the Y-axis. Figure 2 a. Since the first 10 cycles (ln value less than 2) belong to the initial stage of film formation, after 100 cycles (ln value greater than 4), the film layer is stable and more in line with the linear model, so only the curve after 100 cycles is fitted and calculated. Figure 2 The slope of each curve in a is C = 0.79, and then according to Figure 2a can determine the vertical intercepts of different temperature curves with the Y axis, and then plot the vertical intercepts under four temperature conditions with the four temperature parameters 1 / T and connect them into a straight line as shown below: Figure 2 As shown in b, Figure 2 The slope of the b curve is the coefficient B, Figure 2 The new intercept in b is ln(A), and the fitted curve satisfies the functional relationship y=-1249.6x+0.9422, so A=e 0.94 , B = -1250. Finally, the solved capacity loss prediction standard equation is:
[0086]
[0087] 6. Fit the capacity loss rate and thickness data at different temperatures under the same cycle, and the fitted thickness capacity relationship equation is:
[0088] y=E*d+F
[0089] Where y represents the capacity loss rate, d represents the thickness growth rate, and E and F are the coefficients of the thickness-capacity relationship equation.
[0090] like Figure 4 As shown, by fitting the mean slope, E=1.25 can be calculated.
[0091] 7. Substitute the above thickness-capacity relationship equation into the above-mentioned standard equation for predicting capacity loss, and after transformation and arrangement of the equation, the standard equation for predicting thickness with temperature and number of cycles as independent variables and thickness growth rate as dependent variable can be calculated:
[0092]
[0093] In the formula, x represents the number of cycles, T represents the temperature, A, B, C and E are the coefficients of the equation, and the values obtained by fitting in the above steps 5 and 6 can be substituted. d represents the thickness growth rate, T0 represents the reference cycle temperature, and d0 represents the thickness growth rate at the reference temperature.
[0094] 8. Substituting any target temperature into the above thickness prediction standard equation and capacity loss prediction standard equation, the thickness growth curve and capacity loss curve of the lithium-ion soft-pack battery at the target temperature can be calculated, thereby predicting the battery life. It can be seen that the method of the present invention is relatively accurate in the results of the cell cycle thickness growth at different temperatures and has universal applicability.
[0095] Through the technical solution provided by the embodiment of the present invention, it is not necessary to spend a lot of manpower and material resources for batch experiments, nor is it necessary to have expensive and sophisticated testing equipment and perform complex theoretical calculations. Only after a short-term cycle test, the cell cycle thickness growth at different temperatures can be quickly predicted, which greatly reduces the time and resource waste caused by conventional testing. In addition, the higher the temperature, the faster the reaction speed. The active lithium film-forming consumption reaction will be accelerated under high-temperature aging. The model can be quickly established through high-temperature rapid aging data to evaluate the capacity attenuation and thickness change under normal temperature cycling, reduce testing costs and time, and also evaluate the degree of uneven expansion. In addition, according to the usage scenario, the technical solution provided by the present invention can also provide a reference for the margin design of the cell group, and the thickness growth curve calculated by the thickness prediction standard equation can provide a capacity diving warning signal for the battery in the cycle. In addition, the technical solution provided by the present invention can be applied to the life prediction of newly developed cells, and linear models at different temperatures are obtained to evaluate the extreme life of different charging strategies, so as to know the matching of the charging strategy with the battery performance and whether it can meet customer requirements, and optimize it.
[0096] In this embodiment, a battery life prediction device is also provided, which is used to implement the above embodiments and preferred implementation modes, and the descriptions that have been made will not be repeated. As used below, the term "module" can be a combination of software and / or hardware that implements a predetermined function. Although the devices described in the following embodiments are preferably implemented in software, the implementation of hardware, or a combination of software and hardware, is also possible and conceivable.
[0097] This embodiment provides a battery life prediction device, such as Figure 8 As shown, including:
[0098] The sample acquisition module 801 is used to acquire multiple battery samples from the same batch;
[0099] The cycle test module 802 is used to perform charge and discharge cycles on different battery samples under multiple different preset temperature conditions;
[0100] The capacity data acquisition module 803 is used to extract the discharge capacity data corresponding to different cycle numbers under various preset temperature conditions for the battery sample during the charge and discharge cycle;
[0101] The capacity loss curve generation module 804 is used to generate the capacity loss curve under each preset temperature condition according to the extracted discharge capacity data, and the capacity loss curve is used to represent the capacity loss rate that varies with the number of cycles;
[0102] The first equation generation module 805 is used to use the capacity loss curves under various preset temperature conditions to fit a capacity loss prediction standard equation with temperature and cycle number as independent variables and capacity loss rate as a dependent variable;
[0103] The capacity loss prediction module 806 is used to obtain the target temperature of the scenario to be predicted, and substitute the target temperature into the capacity loss prediction standard equation to obtain a capacity loss curve for predicting the battery life in the scenario to be predicted.
[0104] In some optional implementations, the first equation generating module 805 includes:
[0105] An equation creation module for creating a standard equation for capacity loss prediction based on the Arrhenius formula before solving the coefficients;
[0106] The coefficient solving module is used to solve the coefficients of the capacity loss prediction standard equation by using the capacity loss curve under each preset temperature condition through an expensive solution method to obtain the solved capacity loss prediction standard equation.
[0107] In some optional embodiments, the device further comprises:
[0108] A thickness data acquisition module is used to collect thickness expansion data of battery samples under various preset temperature conditions at preset periods during the charge and discharge cycle;
[0109] A dilaton data extraction module, used for extracting a number of dilaton data with the same number of cycles at different temperatures from the thickness dilaton data;
[0110] A thickness-capacity relationship determination module is used to determine the thickness-capacity relationship of a battery sample based on the expansion sub-data and the corresponding discharge capacity data under the same conditions, and obtain a thickness-capacity relationship equation. The thickness-capacity relationship is used to represent the relationship between the thickness growth rate and the capacity loss rate of the battery;
[0111] The second equation generation module is used to substitute the thickness-capacity relationship equation into the capacity loss prediction standard equation to obtain the thickness prediction standard equation with temperature and cycle number as independent variables and thickness growth rate as dependent variable;
[0112] The thickness growth prediction module is used to substitute the target temperature into the thickness prediction standard equation to obtain a thickness growth curve for predicting the battery life in the scenario to be predicted, and to predict the battery life through the thickness growth curve.
[0113] The further functional description of each of the above modules and units is the same as that of the above corresponding embodiments and will not be repeated here.
[0114] The device in this embodiment is presented in the form of a functional unit, where the unit refers to an ASIC (Application Specific Integrated Circuit) circuit, a processor and memory that executes one or more software or fixed programs, and / or other devices that can provide the above functions.
[0115] The embodiment of the present invention also provides a computer device having the above Figure 8 The battery life prediction device shown.
[0116] See also Fig. 9 , Fig. 9 is a schematic diagram of the structure of a computer device provided by an optional embodiment of the present invention, such as Fig. 9 As shown, the computer device includes: one or more processors 10, a memory 20, and interfaces for connecting various components, including high-speed interfaces and low-speed interfaces. Various components are connected to each other using different buses for communication, and can be installed on a common mainboard or installed in other ways as needed. The processor can process the instructions executed in the computer device, including instructions stored in or on the memory to display the graphical information of the GUI on an external input / output device (such as, a display device coupled to the interface). In some optional embodiments, if necessary, multiple processors and / or multiple buses can be used together with multiple memories and multiple memories. Similarly, multiple computer devices can be connected, and each device provides some necessary operations (for example, as a server array, a group of blade servers, or a multi-processor system). Fig. 9 A processor 10 is taken as an example.
[0117] The processor 10 may be a central processing unit, a network processor or a combination thereof. The processor 10 may further include a hardware chip. The hardware chip may be a dedicated integrated circuit, a programmable logic device or a combination thereof. The programmable logic device may be a complex programmable logic device, a field programmable gate array, a general purpose array logic or any combination thereof.
[0118] The memory 20 stores instructions executable by at least one processor 10, so that at least one processor 10 executes the method shown in the above embodiment.
[0119] The memory 20 may include a program storage area and a data storage area, wherein the program storage area may store an operating system, an application required for at least one function; the data storage area may store data created according to the use of the computer device, etc. In addition, the memory 20 may include a high-speed random access memory, and may also include a non-transient memory, such as at least one disk storage device, a flash memory device, or other non-transient solid-state storage device. In some optional embodiments, the memory 20 may optionally include a memory remotely arranged relative to the processor 10, and these remote memories may be connected to the computer device via a network. Examples of the above-mentioned network include, but are not limited to, the Internet, an intranet, a local area network, a mobile communication network, and combinations thereof.
[0120] The memory 20 may include a volatile memory, such as a random access memory; the memory may also include a non-volatile memory, such as a flash memory, a hard disk or a solid state drive; the memory 20 may also include a combination of the above types of memory.
[0121] The computer device further comprises a communication interface 30 for the computer device to communicate with other devices or a communication network.
[0122] The embodiment of the present invention also provides a computer-readable storage medium. The method according to the embodiment of the present invention can be implemented in hardware, firmware, or can be implemented as a computer code that can be recorded in a storage medium, or can be implemented as a computer code that is originally stored in a remote storage medium or a non-temporary machine-readable storage medium and will be stored in a local storage medium through a network download, so that the method described herein can be stored in such software processing on a storage medium using a general-purpose computer, a dedicated processor, or programmable or dedicated hardware. Among them, the storage medium can be a magnetic disk, an optical disk, a read-only storage memory, a random access memory, a flash memory, a hard disk or a solid-state hard disk, etc.; further, the storage medium can also include a combination of the above types of memories. It can be understood that a computer, a processor, a microprocessor controller, or programmable hardware includes a storage component that can store or receive software or computer code. When the software or computer code is accessed and executed by a computer, a processor, or hardware, the method shown in the above embodiment is implemented.
[0123] A part of the present invention may be applied as a computer program product, such as a computer program instruction, which, when executed by a computer, can call or provide the method and / or technical solution according to the present invention through the operation of the computer. Those skilled in the art should understand that the existence of the computer program instruction in a computer-readable medium includes, but is not limited to, a source file, an executable file, an installation package file, etc., and accordingly, the way in which the computer program instruction is executed by the computer includes, but is not limited to: the computer directly executes the instruction, or the computer compiles the instruction and then executes the corresponding compiled program, or the computer reads and executes the instruction, or the computer reads and installs the instruction and then executes the corresponding installed program. Here, the computer-readable medium may be any available computer-readable storage medium or communication medium accessible to the computer.
[0124] Although the embodiments of the present invention have been described in conjunction with the accompanying drawings, those skilled in the art may make various modifications and variations without departing from the spirit and scope of the present invention, and such modifications and variations are all within the scope defined by the appended claims.
Claims
1. A battery life prediction method, characterized in that: The method comprises: Obtain multiple battery samples from the same batch; Perform charge and discharge cycles on different battery samples under multiple different preset temperature conditions; During the charge and discharge cycle, the discharge capacity data corresponding to different cycle numbers under various preset temperature conditions are extracted from the battery sample; Generating a capacity loss curve under various preset temperature conditions by fitting the extracted discharge capacity data, wherein the capacity loss curve is used to represent the capacity loss rate that varies with the number of cycles; Using the capacity loss curves under various preset temperature conditions, a standard capacity loss prediction equation is fitted, with temperature and cycle number as independent variables and capacity loss rate as the dependent variable; The target temperature of the scenario to be predicted is obtained, and the target temperature is substituted into the capacity loss prediction standard equation to obtain a capacity loss curve for predicting the battery life under the scenario to be predicted, and the battery life is predicted by the capacity loss curve.
2. The method according to claim 1, characterized in that The capacity loss curves under various preset temperature conditions are used to fit the capacity loss prediction standard equation with temperature and cycle number as independent variables and capacity loss rate as dependent variable, including: Creating the standard equation for capacity loss prediction before solving the coefficients based on the Arrhenius formula; Taking the logarithm of the capacity loss prediction standard equation before solving; The solution curve of the standard capacity loss prediction equation is plotted with the logarithmic number of cycles as the X-axis and the logarithmic capacity loss rate as the Y-axis; Values are taken from the capacity loss curve under each preset temperature condition, substituted into the solution curve, and the coefficients of the capacity loss prediction standard equation are solved according to the slope and intercept of the solution curve to obtain the solved capacity loss prediction standard equation.
3. The method according to claim 2, characterized in that The capacity loss prediction standard equation is: In the formula, x represents the number of cycles, y represents the capacity loss rate, T represents the temperature, and A, B and C are the coefficients of the equation.
4. The method according to claim 1 or 3, characterized in that: The method further comprises: During the charge and discharge cycle, the thickness expansion data of the battery sample under each preset temperature condition is collected at a preset period; Extracting a plurality of expansion sub-data with the same number of cycles at different temperatures from the thickness expansion data; Determine the thickness-capacity relationship of the battery sample according to the expansion sub-data and the corresponding discharge capacity data under the same conditions, and obtain a thickness-capacity relationship equation, wherein the thickness-capacity relationship is used to represent the relationship between the thickness growth rate and the capacity loss rate of the battery; Substituting the thickness-capacity relationship equation into the capacity loss prediction standard equation, to obtain a thickness prediction standard equation with temperature and cycle number as independent variables and thickness growth rate as dependent variable; The target temperature is substituted into the thickness prediction standard equation to obtain a thickness growth curve for predicting the battery life in the scenario to be predicted, and the battery life is predicted by the thickness growth curve.
5. The method according to claim 4, characterized in that The thickness-capacity relationship equation is: y=E*d+F Wherein, y represents the capacity loss rate, d represents the thickness growth rate, and E and F are coefficients of the thickness-capacity relationship equation.
6. The method according to claim 5, characterized in that The standard equation for thickness prediction is: Where x represents the number of cycles, T represents the temperature, A, B, C and E are equation coefficients, d represents the thickness growth rate, T0 represents the reference cycle temperature, and d0 represents the thickness growth rate at the reference temperature.
7. The method according to claim 4, characterized in that Before collecting the thickness expansion data of the battery samples under each preset temperature condition at a preset period, the method further includes: Each battery sample was adjusted to the same SOC at a preset current rate under the same temperature condition.
8. A battery life prediction device, characterized in that: The device comprises: A sample acquisition module, used to acquire multiple battery samples from the same batch; A cycle test module, used to perform charge and discharge cycles on different battery samples under multiple different preset temperature conditions; A capacity data acquisition module is used to extract discharge capacity data corresponding to different cycle numbers under various preset temperature conditions for the battery sample during the charge and discharge cycle; A capacity loss curve generating module, used for fitting and generating capacity loss curves under various preset temperature conditions according to the extracted discharge capacity data, wherein the capacity loss curves are used for representing the capacity loss rate varying with the number of cycles; The first equation generation module is used to use the capacity loss curves under various preset temperature conditions to fit a capacity loss prediction standard equation with temperature and cycle number as independent variables and capacity loss rate as a dependent variable; The capacity loss prediction module is used to obtain the target temperature of the scene to be predicted, and substitute the target temperature into the capacity loss prediction standard equation to obtain a capacity loss curve for predicting the battery life under the scene to be predicted.
9. A computer device, characterized in that: include: A memory and a processor, wherein the memory and the processor are communicatively connected to each other, the memory stores computer instructions, and the processor executes the method according to any one of claims 1 to 7 by executing the computer instructions.
10. A computer-readable storage medium, characterized in that: The computer-readable storage medium stores computer instructions, and the computer instructions are used to enable a computer to execute the method according to any one of claims 1 to 7.
11. A computer program product, characterized in that The method comprises computer instructions for causing a computer to execute the method according to any one of claims 1 to 7.
Citation Information
Patent Citations
Rapid prediction method for cycle life of lithium ion battery
CN114062955A
Battery life prediction method and device, electronic equipment and storage medium
CN118112421A
Battery cell life prediction method and device and vehicle
CN118519040A
Battery capacity prediction system using charge and discharge cycles of a battery to predict capacity variations, and associated method
US20200386819A1
Cited By
Battery life prediction method for estimating attenuation curve parameters based on LSTM (Long Short Term Memory)
CN120254630A
Battery life degradation curve acquisition method and device, intelligent equipment and storage medium
CN120490876A