Manufacturing method of eye-protecting 2.5 D glass cover plate
By using a light-sweeping device including a base, a telescope and a pressure plate to perform edge sweeping processing on the 2.5D glass cover plate, the problem of scanning processing in the prior art reducing the eye protection effect is solved, and a better balance between edge sweeping effect and eye protection effect is achieved.
Patent Information
- Application Number
- CN202510298369.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-03-13
- Publication Date
- 2025-06-03
AI Technical Summary
During the production process of the existing 2.5D glass cover, in order to meet the product's requirements for gloss and smoothness, it is necessary to perform brightening treatment, but this treatment reduces the eye protection effect of the product.
A light-sweeping device including a base, a telescope and a pressure plate is used to perform the sweeping processing of the glass cover plate. The telescopic device drives the pressure plate to press down the glass cover. The scanning mechanism only scans the edges of the glass cover, thereby enhancing the brightening effect of the edges while maintaining the eye protection effect of the visible area of the glass cover.
Through the processing of the light-sweeping device, the brightening effect of the edge of the glass cover plate is improved, while maintaining the eye protection effect, solving the problem of reducing the eye protection effect in the prior art.
Smart Images

Figure CN120080227A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of electronic product screens, and particularly relates to a manufacturing method for an eye-protecting 2.5D glass cover plate. Background Art
[0002] With the continuous development of the technology of electronic products, as one of the components of electronic products, the screen has also developed faster and faster. The components of the screen include a glass cover plate, also known as a glass protection screen, which is made of transparent glass material and has characteristics such as strong light transmittance, high strength, good toughness, and strong abrasion resistance.
[0003] Currently, the requirements for the screen of electronic products are getting higher and higher. The glass cover plate not only changes in shape but also has an eye-protecting function. In terms of shape, it has developed from the initial 2D to 2.5D and even 3D. The 2D glass cover plate is completely flat without any arc design. The middle of the 2.5D glass cover plate is flat, but the edge is arc-shaped. This design not only provides a better edge grip but also maintains the flat display effect of the screen. However, when manufacturing this shape of the glass cover plate, due to the high requirements for gloss and smoothness of the product, especially at the edge, a polishing process is required. Although the polishing process greatly improves the light transmittance of the product, it also reduces the eye-protecting effect of the product. Summary of the Invention
[0004] The purpose of the present invention is to provide a manufacturing method for an eye-protecting 2.5D glass cover plate to solve the problems existing in the background art.
[0005] To achieve the above purpose, the present invention provides the following technical solution: A manufacturing method for an eye-protecting 2.5D glass cover plate, comprising the following steps:
[0006] 1) Take a piece of glass, cut and CNC precision carve the glass into a 2.5D glass cover plate, and clean the made 2.5D glass cover plate;
[0007] 2) Perform polishing processing on the 2.5D glass cover plate obtained in step 1) in a polishing device. The polishing device includes a base, a telescopic device, and a pressing plate. The upper end surface of the base is provided with a supporting surface adapted to the surface of the glass cover plate, and a positioning groove is provided outside the edge of the supporting surface; the telescopic device is arranged above the base, the output end of the telescopic device faces downward and is connected to the pressing plate, the surface of the pressing plate is adapted to the flat area of the surface of the glass cover plate, and a soft glue layer is provided on the lower surface of the pressing plate; during the polishing process, place the glass cover plate on the upper end surface of the base, start the telescopic device to drive the pressing plate to press down the glass cover plate, and the polishing mechanism of the polishing device performs polishing processing on the edge of the glass cover plate;
[0008] 3) After processing, lift the polishing mechanism and the pressing plate, take out the glass cover plate on the base, check the condition of the edge of the glass cover plate, and clean it, then the production of the eye-protecting 2.5D glass cover plate is completed.
[0009] As an optimization of this technical solution, the cleaning is ultrasonic cleaning.
[0010] As an optimization of this technical solution, a sealing ring is provided at the lower surface of the pressing plate near the edge.
[0011] As an optimization of this technical solution, an air suction channel penetrating to the supporting surface is provided in the base, and the air suction channel is connected to an air suction mechanism.
[0012] As an optimization of this technical solution, the air suction channel includes a main channel, an air cavity and branch channels. One end of the main channel is connected to the air suction mechanism, the other end is connected to the air cavity, a plurality of branch channels are provided, one end of each branch channel communicates with the air cavity, and the other end leads to the supporting surface.
[0013] Compared with the prior art, the beneficial effects of the present invention are as follows: The glass cover plate of the present invention is processed by a polishing device, which includes a base, a telescopic device and a pressing plate. During processing, the telescopic device drives the pressing plate to press on the glass cover plate, and the surface of the pressing plate is adapted to the flat area on the surface of the glass cover plate. During polishing, the flat area on the surface of the glass cover plate is blocked, and the polishing mechanism processes the edge of the glass cover plate, strengthening the polishing effect of the edge and maintaining the eye-protecting effect of the visible area of the glass cover plate. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 It is a schematic structural diagram of the polishing device of the present invention.
[0015] Figure 2 It is a schematic structural diagram of the base of the polishing device of the present invention.
[0016] Figure 3 It is a schematic structural diagram of the pressing plate of the polishing device of the present invention.
[0017] In the figure: 1. Base; 1.1. Supporting surface; 1.2. Positioning groove; 2. Telescopic device; 3. Pressing plate; 4. Soft rubber layer; 5. Main channel; 6. Air cavity; 7. Branch channel; 8. Glass cover plate; 9. Sealing ring. DETAILED DESCRIPTION OF THE EMBODIMENTS
[0018] Next, the technical solutions in the embodiments of the present invention will be clearly and completely described in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only a part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative work fall within the protection scope of the present invention.
[0019] Refer to Figures 1-3 , the manufacturing method of the eye-protecting 2.5D glass cover plate of the present invention includes the following steps:
[0020] 1) Take a piece of glass. According to the required size requirements, the glass is cut and CNC precision carved into a 2.5D glass cover plate, and the manufactured 2.5D glass cover plate is cleaned.
[0021] 2) The 2.5D glass cover plate obtained in step 1) is subjected to polishing processing in a polishing device. The polishing device includes a base, a telescopic device and a pressing plate. A bracket is arranged above the base, and a polishing mechanism and a telescopic device are arranged on the bracket. The polishing mechanism can also move up and down. The upper end surface of the base is provided with a supporting surface adapted to the surface of the glass cover plate. A positioning groove is arranged outside the edge of the supporting surface. The telescopic device is arranged on the bracket above the base. The output end of the telescopic device faces downward and is connected to the pressing plate. The surface of the pressing plate is adapted to the flat area of the surface of the glass cover plate, that is, the cross-sectional size covers the flat area of the glass cover plate. A soft rubber layer is arranged on the lower surface of the pressing plate to prevent scratching the surface of the glass cover plate. During the polishing process, the glass cover plate is placed on the upper end surface of the base, and the edge of the glass cover plate is stuck in the positioning groove. The telescopic device is started to drive the pressing plate to press down the glass cover plate. A pressure sensor can be arranged on the pressing plate to sense the pressure on the surface of the glass cover plate. The polishing mechanism of the polishing device polishes the edge of the glass cover plate.
[0022] 3) After the processing is completed, the polishing mechanism and the pressing plate are lifted, and the glass cover plate on the base is taken out. Check the situation of the edge of the glass cover plate, such as contour, size, roughness, etc., and clean it, that is, the production of the eye-protecting 2.5D glass cover plate is completed. The cleaning in the production steps is ultrasonic cleaning.
[0023] A sealing ring is arranged on the lower surface of the pressing plate of the polishing device of the present invention near the edge. The sealing ring is arranged outside the soft rubber layer. The soft rubber layer can adopt damping cloth. An air suction channel penetrating to the supporting surface is arranged in the base. The air suction channel is connected to an air suction mechanism. By sucking air through the air suction mechanism, the glass cover plate is adsorbed and closely attached to the supporting surface to prevent movement during the polishing operation. The air suction channel includes a main channel, an air cavity and branch channels. One end of the main channel is connected to the air suction mechanism, and the other end is connected to the air cavity. The transverse cross-sectional area of the air cavity is the same as that of the glass cover plate. A plurality of branch channels are arranged. One end of each branch channel communicates with the air cavity, and the other end leads to the supporting surface. The plurality of branch channels are evenly distributed in the area of the transverse cross-section of the air cavity.
[0024] Finally, it should be noted that the above-described embodiments are only specific embodiments of the present invention, used to illustrate the technical solutions of the present invention, rather than limiting it. The protection scope of the present invention is not limited thereto. Although the present invention has been described in detail with reference to the foregoing embodiments, those of ordinary skill in the art should understand that any person skilled in the technical field of the present invention can still modify the technical solutions described in the foregoing embodiments, or can easily think of changes, or perform equivalent replacements on some of the technical features; and these modifications, changes or replacements do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention, and should all be covered by the protection scope of the present invention. Therefore, the protection scope of the present invention should be subject to the protection scope of the claims.
Claims
1. A method for manufacturing an eye-protecting 2.5D glass cover, characterized in that: The following steps are involved: 1) Take a piece of glass, cut it, and CNC carve it into a 2.5D glass cover plate, and then clean the 2.5D glass cover plate; 2) The 2.5D glass cover plate obtained in step 1) is subjected to a light sweeping process in a light sweeping device, wherein the light sweeping device comprises a base, a retractor and a pressing plate, wherein the upper end surface of the base is provided with a supporting surface adapted to the surface of the glass cover plate, and a positioning groove is provided on the outer side of the edge of the supporting surface; the retractor is provided above the base, and the output end of the retractor faces downward and is connected to the pressing plate, wherein the surface of the pressing plate is adapted to the plane area of the surface of the glass cover plate, and a soft rubber layer is provided on the lower surface of the pressing plate; during the light sweeping process, the glass cover plate is placed on the upper end surface of the base, the retractor is started to drive the pressing plate to press down the glass cover plate, and the light sweeping mechanism of the light sweeping device performs light sweeping process on the edge of the glass cover plate; 3) After the processing is completed, lift the light sweeping mechanism and the pressing plate, take out the glass cover plate on the base, check the edge of the glass cover plate, and clean it, and the production of the eye-protection 2.5D glass cover plate is completed.
2. The method for manufacturing the eye-protecting 2.5D glass cover according to claim 1 is characterized in that: The cleaning is ultrasonic cleaning.
3. The method for manufacturing the eye-protecting 2.5D glass cover according to claim 1, characterized in that: A sealing ring is arranged near the edge of the lower surface of the pressing plate.
4. The method for manufacturing the eye-protecting 2.5D glass cover according to claim 1, characterized in that: An air suction channel penetrating to the supporting surface is arranged in the base, and the air suction channel is connected to the air suction mechanism.
5. The method for manufacturing the eye-protecting 2.5D glass cover according to claim 4, characterized in that: The air suction channel includes a main channel, an air cavity and a branch channel. One end of the main channel is connected to the air suction mechanism and the other end is connected to the air cavity. Multiple branch channels are provided. One end of the branch channel is connected to the air cavity and the other end is connected to the support surface.