2N type manganese complex and preparation method thereof, and preparation method of phenyl alkyl disiloxane

The hydrosilylation reaction of hydrogenated siloxanes with olefins catalyzed by 2N-type manganese complex catalysts solved the problems of low activity and narrow substrate application range of cheap metal catalysts in the pentamethyldisiloxane reaction, and achieved efficient and stable preparation of phenylalkyldisiloxane.

CN120590443APending Publication Date: 2025-09-05SHIHEZI UNIVERSITY
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202510715150.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-30
Publication Date
2025-09-05

AI Technical Summary

Technical Problem

Existing cheap metal catalysts have low reactivity in the hydrosilylation reaction of pentamethyldisiloxane and a narrow substrate application range, making it difficult to meet industrial needs.

Method used

The invention adopts 2N-type manganese complex as catalyst, and catalyzes the hydrosilylation reaction of hydrogen-containing siloxane and olefin through the reaction preparation method of specific ligand and manganese compound to prepare phenylalkyl disiloxane.

Benefits of technology

A cheap, highly active, and universal hydrosilylation reaction has been achieved, with good product stability, mild reaction conditions, and high yield, breaking the limitations of precious metal catalysts.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120590443A_ABST
    Figure CN120590443A_ABST
Patent Text Reader

Abstract

The invention relates to a 2N type manganese complex and a preparation method thereof, and a preparation method of phenylalkyl disiloxane. The invention discloses a 2N-type manganese complex and a preparation method thereof, and the preparation method comprises the following steps: (1) adding 2-bromo-pyridine, a ligand, potassium carbonate and cuprous iodide into a dimethyl sulfoxide solution, and reacting at 110-130 DEG C for 20-28 hours to obtain an N, N bidentate ligand; the ligand is 1-(pyridine-2-yl)-1H-indole, or 2-(1H-pyrazole-1-yl) pyridine, or 2-(2H-1, 2, 3-triazole-2-yl) pyridine, and the ligand is one or more of 1-(pyridine-2-yl)-1H-indole, 2-(1H-pyrazole-1-yl) pyridine, 2-(2H-1, 2 And (2) dissolving the N, N bidentate ligand and Mn (CO) 5Br in a tetrahydrofuran solution, and reacting at 65-75 DEG C for 10-14 hours to obtain the 2N type manganese complex. According to the 2N-type manganese complex, the preparation method thereof and the preparation method of the phenyl alkyl disiloxane, the 2N-type manganese complex is used as a catalyst for hydrosilylation reaction of pentamethyldisiloxane, styrene and derivatives thereof to prepare the phenyl alkyl disiloxane.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of organic chemical catalysis, and particularly relates to a 2N-type manganese complex and a preparation method thereof, and a preparation method of phenylalkyldisiloxane. Background Art

[0002] As a class of organic compounds containing silicon-oxygen bonds, siloxanes occupy a core position in organosilicon chemistry due to their unique structural characteristics. The silicon-oxygen bond functional molecules derived from them (such as silyl ethers, silyl esters and cyclosiloxanes) play an irreplaceable role in cutting-edge fields such as industrial catalysis, polymer material modification and semiconductor precursor synthesis. Pentamethyldisiloxane hydrosilylation products are widely used in many fields, especially in organic synthesis, materials science and coatings industry. In organic synthesis, hydrosilylation reaction is an important chemical reaction. Under the action of a catalyst, silicon-hydrogen bonds react with double bonds or triple bonds of unsaturated compounds to form new silicon-carbon compounds. Pentamethyldisiloxane hydrosilylation products are used to prepare silane compounds and silene compounds due to their good reactivity and high selectivity.

[0003] In addition, products such as pentamethyldisiloxane are also widely used in the manufacture of coatings, sealants, lubricants and electronic materials. In the coating field, pentamethyldisiloxane can provide excellent high-temperature resistance, chemical corrosion resistance and good surface properties. In sealants and lubricants, they can enhance the stability of materials, extend service life, and improve surface lubricity. In the electronics industry, pentamethyldisiloxane hydrosilylation products are used to manufacture silicone rubber and other high-performance materials, which are widely used in the packaging and protection of electronic devices. Therefore, pentamethyldisiloxane hydrosilylation products not only have important industrial value, but also play a vital role in the research and development and application of various advanced materials.

[0004] With the development of hydrosilylation reactions, transition metal-catalyzed hydrosilylation reactions have made great achievements. However, the catalysts used are mostly precious metals such as platinum, palladium, and rhodium, which are relatively expensive. In recent years, hydrosilylation reactions catalyzed by cheap metal catalysts such as iron, cobalt, nickel, and manganese have been well developed. However, for hydrosilylation reactions such as pentamethyldisiloxane, the current cheap metal catalysts perform poorly, with problems such as low reaction activity, difficulty in achieving the reaction, and a narrow application range of the substrate. Therefore, it is very necessary to develop metal catalysts with low price, high reaction activity, and good substrate universality for the hydrosilylation reaction of siloxane.

[0005] In view of this, the present invention provides a 2N-type manganese complex and a preparation method thereof, as well as a preparation method of phenylalkyldisiloxane. The 2N-type manganese complex is low in price and has the advantages of high reaction activity and good substrate universality in the hydrosilylation reaction of phenylalkyldisiloxane. Summary of the Invention

[0006] The object of the present invention is to provide a 2N-type manganese complex, which has low cost and can be used in the hydrosilylation reaction of hydrogen-containing siloxanes to prepare phenylalkyldisiloxanes.

[0007] In order to achieve the above object, the technical solution adopted by the present invention is:

[0008] A 2N-type manganese complex, the structural formula of which is shown below:

[0009]

[0010] Another object of the present invention is to provide a method for preparing the above-mentioned 2N-type manganese complex, which is simple and uses cheap and readily available raw materials.

[0011] In order to achieve the above object, the technical solution adopted by the present invention is:

[0012] The preparation method of the above-mentioned 2N-type manganese complex comprises the following steps:

[0013] (1) Add 2-bromo-pyridine, ligand, potassium carbonate, and cuprous iodide to a dimethyl sulfoxide solution, and react at 110-130° C. for 20-28 hours to obtain an N,N bidentate ligand;

[0014] The ligand is 1-(pyridin-2-yl)-1H-indole, or 2-(1H-pyrazol-1-yl)pyridine, or 2-(2H-1,2,3-triazol-2-yl)pyridine;

[0015] (2) Dissolving the N,N bidentate ligand and Mn(CO)5Br in tetrahydrofuran solution, and reacting at 65-75° C. for 10-14 hours to obtain the 2N-type manganese complex.

[0016] Furthermore, in the step (1), the reaction is carried out at 120° C. for 24 hours.

[0017] Furthermore, in the step (2), the reaction is carried out at 70° C. for 12 hours.

[0018] Another object of the present invention is to provide a method for preparing phenylalkyldisiloxane, which uses the above-mentioned 2N-type manganese complex to activate the Si-H bond in the siloxane, catalyzing the hydrosilylation reaction of tertiary hydrogen siloxane with olefins, and has the advantages of low cost, good universality, excellent stability, mild reaction conditions, and high yield.

[0019] In order to achieve the above object, the technical solution adopted by the present invention is:

[0020] A method for preparing phenylalkyldisiloxane comprises: uniformly mixing hydrogen-containing siloxane, olefin, catalyst, reaction activator, and organic solvent, and then performing a hydrosilylation reaction under an inert gas atmosphere to obtain a hydrosilylation siloxane product, namely, the phenylalkyldisiloxane;

[0021] The catalyst is the above-mentioned 2N-type manganese complex.

[0022] Furthermore, the hydrogen-containing siloxane is pentamethyldisiloxane;

[0023] The chemical structural formula of the olefin used is: Wherein, R is an aliphatic chain or a benzene ring substituent.

[0024] Furthermore, the olefins used are styrene, p-methylstyrene, p-methoxystyrene, p-tert-butylstyrene, allylbenzene, but-3-en-1-ylbenzene, 4-vinylbiphenyl, vinylthiophene, N,N-dimethyl-4-vinylaniline, p-fluorostyrene, and p-trifluoromethylstyrene.

[0025] Furthermore, the reaction activator used is NaHBEt3 or LiHBEt3;

[0026] The organic solvent is toluene.

[0027] Furthermore, the molar ratio of the hydrogen-containing siloxane to the olefin, catalyst, and activator is 1:0.8-1.2:0.01-0.03:0.04-0.06;

[0028] The temperature of the hydrosilation reaction is 75-81° C. and the time is 20-28 hours.

[0029] Furthermore, the molar ratio of the hydrogen-containing siloxane to the olefin, the catalyst, and the activator is 1:1:0.02:0.05;

[0030] The temperature of the hydrosilation reaction is 80° C. and the time is 24 hours.

[0031] Compared with the prior art, the present invention has the following beneficial effects:

[0032] 1. The technical solution of the present invention uses a 2N-type manganese complex as the catalyst, which is cheaper and more readily available than precious metal catalysts such as palladium, platinum, and rhodium.

[0033] 2. The technical solution of the present invention uses a 2N-type manganese complex as a catalyst, and the synthesis steps of the hydrosilylation reaction of hydrogen-containing siloxanes and olefins are simple. The obtained products are all anti-Markovnikov structures and have good stability.

[0034] 3. The technical solution of the present invention uses a 2N-type manganese complex as a catalyst to participate in the hydrosilylation reaction of hydrogen-containing siloxanes and olefins. The substrate has good universality and can be applied to aromatic hydrocarbons with different substituents, electron-withdrawing groups, electron-donating groups, short-chain, long-chain and heterocyclic olefins.

[0035] 4. The technical solution of the present invention uses a 2N-type manganese complex as a catalyst for the hydrosilation reaction, which has the characteristics of mild conditions and high yield. It breaks the traditional characteristics of using precious metals to produce organic silicon products and provides a new experimental idea for the production of cheap and efficient silicon chemical products. BRIEF DESCRIPTION OF THE DRAWINGS

[0036] Figure 1 Single crystal structure characterization of 2N-type manganese complex Mn1. DETAILED DESCRIPTION

[0037] To further illustrate the present invention's 2N-type manganese complex, its preparation method, and its preparation method for phenylalkyldisiloxane, and to achieve its intended purpose, the following describes in detail the present invention's 2N-type manganese complex, its preparation method, and its preparation method for phenylalkyldisiloxane, along with preferred embodiments, including their specific embodiments, structures, features, and efficacy. In the following description, different references to "one embodiment" or "embodiment" do not necessarily refer to the same embodiment. Furthermore, specific features, structures, or characteristics of one or more embodiments may be combined in any suitable manner.

[0038] The following is a further detailed introduction to a 2N-type manganese complex and its preparation method, and a preparation method of phenylalkyldisiloxane of the present invention in conjunction with specific examples:

[0039] Organosilicon refers to a class of organic compounds containing silicon, offering promising applications. With the advancement of technology, the organosilicon industry has become a strategic emerging industry worldwide, with an increasingly broad market outlook. Hydrosilylation is an important method for synthesizing and modifying organosilicon, and the resulting products are environmentally friendly. Commonly used hydrogenated siloxanes, also known as silicone oil monomers, include pentamethyldisiloxane, hydrogenated disiloxanes, and alkoxysilanes.

[0040] The present invention mainly uses pentamethyldisiloxane as the main material and styrene-based olefins as the reaction model, and explores the hydrosilylation reaction under the catalytic action of a 2N-type manganese complex. The present invention utilizes a relatively cheap 2N-type manganese complex compared to precious metals such as palladium, platinum, and rhodium to catalyze the hydrosilylation reaction more efficiently, thereby realizing the hydrosilylation modification of silicone oil monomers (pentamethyldisiloxane) to obtain new siloxane products. The method has simple reaction steps, cheap and easily available raw materials, and good stability. The hydrosilylation reaction catalyzed by the 2N-type manganese complex of the present invention has the advantages of mild conditions, high reaction selectivity and reaction activity, and good substrate universality, breaking the characteristics of traditional production of organosilicon products with precious metals, and providing a new experimental idea for realizing cheap and efficient silicon chemical production.

[0041] The technical solution of the present invention is:

[0042] A 2N-type manganese complex, whose Mn1, Mn2, and Mn3 structural formulas are shown below:

[0043]

[0044] The preparation method of the above-mentioned 2N-type manganese complex comprises the following steps:

[0045] (1) Add 2-bromo-pyridine, ligand, potassium carbonate, and cuprous iodide to a dimethyl sulfoxide solution, and react at 110-130° C. for 20-28 hours to obtain an N,N bidentate ligand;

[0046] The ligand is 1-(pyridin-2-yl)-1H-indole, or 2-(1H-pyrazol-1-yl)pyridine, or 2-(2H-1,2,3-triazol-2-yl)pyridine;

[0047] (2) Dissolving the N,N bidentate ligand and Mn(CO)5Br in tetrahydrofuran solution, and reacting at 65-75° C. for 10-14 hours to obtain the 2N-type manganese complex.

[0048] Preferably, in the step (1), the reaction is carried out at 120° C. for 24 hours.

[0049] Preferably, in the step (2), the reaction is carried out at 70° C. for 12 hours.

[0050] A method for preparing phenylalkyldisiloxane comprises: uniformly mixing hydrogenated siloxane, olefin, catalyst, reaction activator and organic solvent, and then carrying out a hydrosilylation reaction under an inert gas atmosphere to obtain a hydrosilylation siloxane product, namely the phenylalkyldisiloxane; the catalyst is the above-mentioned 2N-type manganese complex.

[0051] In the above technical solution, the mixing method of the present invention for hydrogen-containing siloxane, olefin, catalyst, solvent and reaction activator is: first add the catalyst, then add the olefin and hydrogen-containing siloxane, then add the organic solvent, and finally add the reaction activator.

[0052] The reaction formula of the hydrosilylation reaction is:

[0053]

[0054] Preferably, the hydrogen-containing siloxane is pentamethyldisiloxane;

[0055] The chemical structural formula of the olefin used is: Wherein, R is an aliphatic chain or a benzene ring substituent.

[0056] More preferably, the olefins used are styrene, p-methylstyrene, p-methoxystyrene, p-tert-butylstyrene, allylbenzene, but-3-en-1-ylbenzene, 4-vinylbiphenyl, vinylthiophene, N,N-dimethyl-4-vinylaniline, p-fluorostyrene, p-trifluoromethylstyrene, and their structural formulas are shown below:

[0057]

[0058] Preferably, the reaction activator used is NaHBEt3 or LiHBEt3;

[0059] The organic solvent is toluene.

[0060] Preferably, the molar ratio of the hydrogen-containing siloxane to the olefin, catalyst, and activator is 1:0.8-1.2:0.01-0.03:0.04-0.06;

[0061] The temperature of the hydrosilation reaction is 75-81° C. and the time is 20-28 hours.

[0062] Further preferably, the molar ratio of the hydrogen-containing siloxane to the olefin, catalyst, and activator is 1:1:0.02:0.05;

[0063] The temperature of the hydrosilation reaction is 80° C. and the time is 24 hours.

[0064] All drugs are commercially available and require no further processing. The present invention has no particular requirements for olefins, as long as an olefin-like structure that meets the above requirements can be obtained. In the above technical solution, the hydrogen-containing siloxane, catalyst, reaction activator, and cyano ligand can be commercially available products well known in the art.

[0065] Example 1: Synthesis of 2N-type manganese complex

[0066] The structural formula of 2N-type manganese complex is shown below:

[0067]

[0068] The reaction formula is as follows:

[0069]

[0070] The specific steps are as follows:

[0071] (1) 2-Bromo-pyridine (18 mmol), ligand (20 mmol), potassium carbonate (60 mmol), and cuprous iodide (4 mmol) were added to 10 mL of dimethyl sulfoxide solution and reacted at 120°C for 24 h to obtain an N,N bidentate ligand.

[0072] The ligands are 1-(pyridin-2-yl)-1H-indole, 2-(1H-pyrazol-1-yl)pyridine, and 2-(2H-1,2,3-triazol-2-yl)pyridine, respectively. Their structural formulas are shown below:

[0073]

[0074] (2) The N,N bidentate ligand and Mn(CO)5Br were dissolved in tetrahydrofuran solution and reacted at 70°C for 15 h to obtain 2N-type manganese complexes Mn1, Mn2, and Mn3.

[0075] Ligand 1: 1-(pyridin-2-yl)-1H-indole NMR data:

[0076] 1 HNMR (400MHz, CDCl3): δ=8.87-8.84(m,1H),8.54-8.52(m,1H),8.20(s,1H),8.07-8.0 4(m,1H),7.84-7.76(m,2H),7.55-7.50(m,1H),7.30-7.26(m,1H),7.16-7.13(m,1H).

[0077] 13 CNMR (100MHz, CDCl3): δ=154.5,147.8,139.0,138.4,136.9,128.0,126.1,122.6,120.8,120.0,115.4,113.6.

[0078] The single crystal structure of 2N-type manganese complex Mn1 was characterized. Figure 1 As shown. Figure 1 It can be seen that the 2N-type manganese complex Mn1 was synthesized.

[0079] Example 2.

[0080] The specific steps are as follows:

[0081] (1) 2-Bromo-pyridine (18 mmol), 2-(1H-pyrazol-1-yl)pyridine ligand (20 mmol), potassium carbonate (60 mmol), and cuprous iodide (4 mmol) were added to 10 mL of dimethyl sulfoxide solution and reacted at 110°C for 28 h to obtain an N,N bidentate ligand;

[0082] (2) After dissolving the N,N bidentate ligand and Mn(CO)5Br in tetrahydrofuran solution, the mixture was reacted at 65°C for 14 hours to obtain the 2N-type manganese complex.

[0083] Ligand 2: 2-(1H-pyrazol-1-yl)pyridine NMR data:

[0084] 1 HNMR (400MHz, CDCl3): δ=8.56-8.55(m,1H),8.38-8.36(m,1H),7.97-7.95(m,1H),7.79-7.72(m,2H),7.15-7.11(m,1H),6.44-6.43(m,1H).

[0085] 13 CNMR (100MHz, CDCl3): δ=151.6,148.0,142.0,138.7,127.0,121.4,112.4,107.8.

[0086] Example 3.

[0087] The specific steps are as follows:

[0088] (1) 2-Bromo-pyridine (18 mmol), 2-(2H-1,2,3-triazol-2-yl)pyridine ligand (20 mmol), potassium carbonate (60 mmol), and cuprous iodide (4 mmol) were added to 10 mL of dimethyl sulfoxide solution and reacted at 130°C for 20 h to obtain an N,N bidentate ligand;

[0089] (2) After dissolving the N,N bidentate ligand and Mn(CO)5Br in tetrahydrofuran solution, the mixture was reacted at 75°C for 10 hours to obtain the 2N-type manganese complex.

[0090] Product ligand 3: 2-(2H-1,2,3-triazol-2-yl)pyridine NMR data:

[0091] 1HNMR (400MHz, CDCl3): δ = 8.61 (s, 1H), 8.53-8.51 (m, 1H), 8.24-8.22 (m, 1H), 7.96-7.91 (m, 1H), 7.85 (s, 1H), 7.38-7.34 (m, 1H).

[0092] 13 CNMR (100MHz, CDCl3): δ = 148.4, 139.0, 134.0, 123.4, 120.9, 113.8.

[0093] The catalyst in Examples 4-14 was the 2N-type manganese complex Mn1 prepared in Example 1, and the reaction was carried out under an inert gas atmosphere.

[0094] In the embodiment, the hydrogen-containing siloxane, olefin, catalyst and reaction activator are mixed in a manner of adding the catalyst first, then adding the olefin and hydrogen-containing siloxane, then adding the organic solvent, and finally adding the reaction activator.

[0095] Example 4.

[0096] The reaction formula is as follows:

[0097]

[0098] The specific steps are as follows:

[0099] 1.0 mmol of pentamethyldisiloxane, 1.0 mmol of styrene, 2 mol% of a catalyst, and 5 mol% of a reaction activator were heated to 80°C in a toluene solution and reacted for 24 hours. After the reaction, the product was separated by column chromatography with a yield of 90%.

[0100] NMR data of the product 1,1,1,3,3-pentamethyl-3-phenylethyldisiloxane:

[0101] 1 HNMR (400MHz, CDCl3): δ=7.26-7.07(m,5H),2.58-2.54(m,2H),0.83-0.77(m,2H),0.01-0.00(s,15H).

[0102] 13 CNMR (100MHz, CDCl3): δ=145.3,128.4,126.7,125.6,29.6,20.5,2.2,0.5.

[0103] Example 5.

[0104] The reaction formula is as follows:

[0105]

[0106] The specific steps are as follows:

[0107] 1.0 mmol of pentamethyldisiloxane, 1.0 mmol of p-methylstyrene, 2 mol% of a catalyst, and 5 mol% of a reaction activator were heated to 80°C in a toluene solution and reacted for 24 hours. After the reaction, the product was separated by column chromatography with a yield of 92%.

[0108] NMR data of the product 1,1,1,3,3-pentamethyl-3-(4-methylphenethyl)disiloxane:

[0109] 1 HNMR (400MHz, CDCl3): δ = 7.06-7.00 (m, 4H), 2.54-2.50 (m, 2H), 2.22 (s, 3H), 0.81-0.77 (m, 2H), 0.01-0.00 (s, 15H).

[0110] 13 CNMR (100MHz, CDCl3): δ=142.0,134.7,129.1,127.5,28.8,20.8,20.4,0.7,0.2.

[0111] Example 6.

[0112] The reaction formula is as follows:

[0113]

[0114] The specific steps are as follows:

[0115] 1.0 mmol of pentamethyldisiloxane, 1.0 mmol of p-methoxystyrene, 2 mol% of a catalyst, and 5 mol% of a reaction activator were heated to 80°C in a toluene solution and reacted for 24 hours. After the reaction, the product was isolated by column chromatography with a yield of 95%.

[0116] The NMR data of the product 1-(4-methoxyphenethyl)-1,1,3,3,3-pentamethyldisiloxane:

[0117] 1 HNMR (400MHz, CDCl3): δ=7.01-6.99(m,2H),6.72-6.69(m,2H),3.66(s,3H),2.51-2.46(m,2H),0.78-0.73(m,2H),0.02-0.00(m,15H).

[0118] 13CNMR (100MHz, CDCl3): δ=157.7,137.4,128.8,113.8,55.4,28.6,20.8,2.2,0.5.

[0119] Example 7.

[0120] The reaction formula is as follows:

[0121]

[0122] The specific steps are as follows:

[0123] 1.0 mmol of pentamethyldisiloxane, 1.0 mmol of p-tert-butylstyrene, 2 mol% of a catalyst, and 5 mol% of a reaction activator were heated to 80°C in a toluene solution and reacted for 24 hours. After the reaction, the product was isolated by column chromatography with a yield of 93%.

[0124] The NMR data of the product 1-(4-(tert-butyl)phenethyl)-1,1,3,3-pentamethyldisiloxane:

[0125] 1 HNMR (400MHz, CDCl3): δ=7.32-7.30(m,2H),7.16-7.14(m,2H),2.65-2.61(m,2H),1.33-1.32(m,9H),0.92-0.88(m,2H),0.09(s,15H).

[0126] 13 CNMR (100MHz, CDCl3): δ=148.4,142.3,127.6,125.3,34.5,31.5,28.9,20.4,2.2,0.4.

[0127] Example 8.

[0128] The reaction formula is as follows:

[0129]

[0130] The specific steps are as follows:

[0131] 1.0 mmol of pentamethyldisiloxane, 1.0 mmol of allylbenzene, 2 mol% of catalyst, and 5 mol% of reaction activator were heated to 80°C in a toluene solution and reacted for 24 hours. After the reaction, the product was separated by column chromatography with a yield of 67%.

[0132] NMR data of the product 1,1,1,3,3-pentamethyl-3-(3-phenylpropyl)disiloxane:

[0133] 1 HNMR (400MHz, CDCl3): δ=7.30-7.28(m,2H),7.19-7.15(m,3H),2.62(m,2H),1.71-1.61(m,2H),0.59-0.54(m,2H),0.06-0.04(s,15H).

[0134] 13 CNMR (100MHz, CDCl3): δ=142.9,128.6,128.4,125.7,39.8,25.6,18.4,2.1,0.5.

[0135] Example 9.

[0136] The reaction formula is as follows:

[0137]

[0138] The specific steps are as follows:

[0139] 1.0 mmol of pentamethyldisiloxane, 1.0 mmol of but-3-en-1-ylbenzene, 2 mol% of a catalyst, and 5 mol% of a reaction activator were heated to 80°C in a toluene solution and reacted for 24 hours. After the reaction, the product was isolated by column chromatography with a yield of 58%.

[0140] NMR data of the product 1,1,1,3,3-pentamethyl-3-(4-phenylbutyl)disiloxane:

[0141] 1 HNMR (400MHz, CDCl3): δ=7.34-7.28(m,2H),7.19-7.17(m,3H),2.62(m,2H),1.66(m,2H),1.39(m,2H),0.59-0.55(m,2H),0.06(s,15H).

[0142] 13 CNMR (100MHz, CDCl3): δ=143.0,128.6,128.5,125.7,35.9,35.4,23.2,18.4,0.9,0.2.

[0143] Example 10.

[0144] The reaction formula is as follows:

[0145]

[0146] The specific steps are as follows:

[0147] 1.0 mmol of pentamethyldisiloxane, 1.0 mmol of 4-vinylbiphenyl, 2 mol% of a catalyst, and 5 mol% of a reaction activator were heated to 80°C in a toluene solution and reacted for 24 hours. After the reaction, the product was isolated by column chromatography with a yield of 62%.

[0148] The NMR data of the product 1-(2-([1,1'-biphenyl]-4-yl)ethyl)-1,1,3,3,3-pentamethyldisiloxane:

[0149] 1 HNMR (400MHz, CDCl3): δ=7.52-7.50(m,2H),7.45-7.43(m,2H),7.37-7.33(m,2H) ),7.26-7.17(m,3H),2.64-2.59(m,2H),0.88-0.83(m,2H),0.03-0.01(s,15H).

[0150] 13 CNMR (100MHz, CDCl3): δ=144.8,141.7,138.9,129.2,128.7,127.6,127.5,127.4,29.5,20.8,2.5,0.8.

[0151] Example 11.

[0152] The reaction formula is as follows:

[0153]

[0154] The specific steps are as follows:

[0155] 1.0 mmol of pentamethyldisiloxane, 1.0 mmol of vinylthiophene, 2 mol% of a catalyst, and 5 mol% of a reaction activator were heated to 80°C in a toluene solution and reacted for 24 hours. After the reaction, the product was separated by column chromatography with a yield of 65%.

[0156] The NMR data of the product 1,1,1,3,3-pentamethyl-3-(2-(thien-2-yl)ethyl)disiloxane:

[0157] 1 HNMR (400MHz, CDCl3): δ=7.10-7.09(m,1H),6.91-6.89(m,1H),6.80-6.78(m,1H),2.88-2.84(m,2H),1.02-0.97(m,2H),0.08-0.07(s,15H).

[0158] 13CNMR (100MHz, CDCl3): δ=148.7,126.4,122.9,122.4,23.6,20.7,1.8,0.1.

[0159] Example 12.

[0160] The reaction formula is as follows:

[0161]

[0162] The specific steps are as follows:

[0163] 1.0 mmol of pentamethyldisiloxane, 1.0 mmol of N,N-dimethyl-4-vinylaniline, 2 mol% of a catalyst, and 5 mol% of a reaction activator were heated to 80°C in a toluene solution and allowed to react for 24 hours. After the reaction, the product was isolated by column chromatography with a yield of 55%.

[0164] The NMR data of the product N,N-dimethyl-4-(2-(1,1,3,3,3-pentamethyldisiloxane)ethyl)aniline:

[0165] 1 HNMR (400MHz, CDCl3): δ=7.11-7.08(m,2H),6.74-6.71(m,2H),2.92-2.91(m,6H),2.60-2.55(m,2H),0.90-0.84(m,2H),0.10-0.08(s,15H).

[0166] 13 CNMR (100MHz, CDCl3): δ=148.9,128.6,128.4,113.4,41.3,28.4,20.7,2.2,0.5.

[0167] Example 13.

[0168] The reaction formula is as follows:

[0169]

[0170] The specific steps are as follows:

[0171] 1.0 mmol of pentamethyldisiloxane, 1.0 mmol of p-fluorostyrene, 2 mol% of a catalyst, and 5 mol% of a reaction activator were heated to 80°C in a toluene solution and reacted for 24 hours. After the reaction, the product was isolated by column chromatography with a yield of 33%.

[0172] The NMR data of the product 1-(4-fluorophenethyl)-1,1,3,3,3-pentamethyldisiloxane:

[0173] 1 HNMR (400MHz, CDCl3): δ=7.17-7.13(m,2H),6.97-6.92(m,2H),2.64-2.59(m,2H),0.88-0.84(m,2H),0.08-0.07(s,15H).

[0174] 13 CNMR (100MHz, CDCl3): δ=128.9,128.8,114.8,114.6,28.5,20.3,1.8,0.2.

[0175] 19 FNMR (376MHz, CDCl3): δ = -114.3ppm.

[0176] Example 14.

[0177] The reaction formula is as follows:

[0178]

[0179] The specific steps are as follows:

[0180] 1.0 mmol of pentamethyldisiloxane, 1.0 mmol of p-trifluoromethylstyrene, 2 mol% of a catalyst, and 5 mol% of a reaction activator were heated to 80°C in a toluene solution and reacted for 24 hours. After the reaction, the product was isolated by column chromatography with a yield of 58%.

[0181] The NMR data of the product 1,1,1,3,3-pentamethyl-3-(4-(trifluoromethyl)phenethyl)disiloxane:

[0182] 1 HNMR (400MHz, CDCl3): δ=7.53-7.51(m,2H),7.31-7.29(m,2H),2.72-2.67(m,2H),0.92-0.86(m,2H),0.09-0.07(s,15H).

[0183] 13 CNMR (100MHz, CDCl3): δ=149.1,127.9,125.1,125.0(J C-F =3),124.9,29.2,20.0,1.8,0.1.

[0184] 19 FNMR (376MHz, CDCl3): δ = -62.2ppm.

[0185] Example 15.

[0186] The specific operation steps are the same as those in Example 4, except for the catalyst. See Table 1 for details.

[0187] Table 1

[0188]

[0189] Example 16.

[0190] The specific operation steps are the same as those in Example 4, except for the reaction temperature and time. See Table 2 for details.

[0191] Table 2

[0192]

[0193] Example 17.

[0194] The specific operation steps are the same as those in Example 4, except that the amount of styrene, the amount of catalyst, and the amount of reaction activator are shown in Table 3.

[0195] Table 3

[0196]

[0197] As can be seen from the above examples, the present invention provides a 2N-type manganese complex and its preparation method, as well as a method for preparing phenylalkyldisiloxane. By reacting tertiary hydrogen siloxane with different olefins, corresponding hydrosilylation products are obtained. By varying the catalytic reaction using different 2N-type manganese complexes, the yield and structure of the resulting products vary. Electron-donating groups react better than electron-withdrawing groups, short-chain olefins react better than long-chain olefins, and less sterically hindered olefins react better than more sterically hindered olefins. The yield of the resulting hydrosilylation products ranges from 33% to 95%.

[0198] The above is merely a preferred embodiment of the present invention and does not constitute any form of limitation to the embodiments of the present invention. Any simple modifications, equivalent changes, and modifications made to the above embodiments based on the technical essence of the embodiments of the present invention are still within the scope of the technical solutions of the embodiments of the present invention.

Claims

1. A 2N-type manganese complex, characterized in that The structural formula of the 2N-type manganese complex is shown below:

2. The method for preparing the 2N-type manganese complex according to claim 1, characterized in that: The following steps are involved: (1) Add 2-bromo-pyridine, ligand, potassium carbonate, and cuprous iodide to a dimethyl sulfoxide solution, and react at 110-130° C. for 20-28 hours to obtain an N,N bidentate ligand; The ligand is 1-(pyridin-2-yl)-1H-indole, or 2-(1H-pyrazol-1-yl)pyridine, or 2-(2H-1,2,3-triazol-2-yl)pyridine; (2) Dissolving the N,N bidentate ligand and Mn(CO)5Br in tetrahydrofuran solution, and reacting at 65-75° C. for 10-14 hours to obtain the 2N-type manganese complex.

3. The preparation method according to claim 2, characterized in that In the step (1), the reaction is carried out at 120° C. for 24 hours.

4. The preparation method according to claim 2, characterized in that In the step (2), the reaction is carried out at 70° C. for 12 hours.

5. A method for preparing phenylalkyldisiloxane, characterized in that: The preparation method comprises: mixing hydrogen-containing siloxane, olefin, catalyst, reaction activator and organic solvent, and then performing a hydrosilylation reaction under an inert gas atmosphere to obtain a hydrosilylation product, namely the phenylalkyldisiloxane; The catalyst is the 2N-type manganese complex according to claim 1.

6. The preparation method according to claim 5, characterized in that The hydrogen-containing siloxane is pentamethyldisiloxane; The chemical structural formula of the olefin used is: Wherein, R is an aliphatic chain or a benzene ring substituent.

7. The preparation method according to claim 6, characterized in that The olefins used are styrene, p-methylstyrene, p-methoxystyrene, p-tert-butylstyrene, allylbenzene, but-3-en-1-ylbenzene, 4-vinylbiphenyl, vinylthiophene, N,N-dimethyl-4-vinylaniline, p-fluorostyrene, and p-trifluoromethylstyrene.

8. The preparation method according to claim 5, characterized in that The reaction activator used is NaHBEt3 or LiHBEt3; The organic solvent is toluene.

9. The preparation method according to claim 5, characterized in that The molar ratio of the hydrogen-containing siloxane to the olefin, catalyst, and activator is 1:0.8-1.2:0.01-0.03:0.04-0.06; The temperature of the hydrosilation reaction is 75-81° C. and the time is 20-28 hours.

10. The preparation method according to claim 9, characterized in that The molar ratio of the hydrogen-containing siloxane to the olefin, catalyst, and activator is 1:1:0.02:0.05; The temperature of the hydrosilation reaction is 80° C. and the time is 24 hours.

Citation Information

Cited By

  • Catalyst for high-temperature-resistant organic silicon heat-conducting oil and preparation method of catalyst