Liquid metal battery and assembly process thereof

By adopting a vertical battery structure and a composite negative electrode design in liquid metal batteries, the problems of insufficient space utilization and polarization overpotential in traditional liquid metal batteries are solved, higher space utilization efficiency and energy efficiency are achieved, and the stability and high efficiency of the battery are ensured.

CN120784487APending Publication Date: 2025-10-14HENG HUI KE YUAN (XI AN) XIN NENG YUAN JI SHU YOU XIAN GONG SI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510950004.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-07-10
Publication Date
2025-10-14

AI Technical Summary

Technical Problem

In traditional liquid metal batteries, the parallel electrode-electrolyte interface based on density self-stratification makes it impossible to lead out the positive and negative electrode current collectors and seals laterally, resulting in insufficient longitudinal space utilization of the single cell and low space utilization efficiency. In addition, there is a high polarization overpotential during high-rate charge and discharge, which affects the battery energy efficiency.

Method used

A vertical battery structure is adopted. By setting two parallel electrochemical active interfaces in the battery shell, a composite negative electrode and a porous grid design are used to increase the electrode area and ion transmission channels, optimize the electrode interface structure, realize the parallel combination of positive and negative electrodes, and improve space utilization efficiency and ion diffusion efficiency.

Benefits of technology

It improves the battery's space utilization efficiency to 39.5%, reduces energy storage costs, improves the battery's energy density and energy efficiency, reduces concentration polarization, and ensures the battery's stable operation and efficient charge and discharge performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120784487A_ABST
    Figure CN120784487A_ABST
Patent Text Reader

Abstract

The invention provides a liquid metal battery and an assembly process thereof, and relates to the technical field of liquid metal batteries. The liquid metal battery comprises two battery shells, the two battery shells are arranged front and back, a composite cathode piece is arranged at the upper ends of the two battery shells, insulating guide grooves are formed in the positions, close to the two sides, of the center of the lower end face of the composite cathode piece, and the composite cathode piece is arranged between the two insulating guide grooves; the composite negative electrode piece comprises a negative electrode perforated plate, negative electrode current collectors are arranged on the front end face and the rear end face of the negative electrode perforated plate, a mounting groove is formed in the center of the upper end face of the negative electrode perforated plate, and a negative electrode connecting piece is arranged at the upper end of the mounting groove. The two positive electrodes and the two negative electrodes are included, so that two parallel electrochemical active interfaces are formed, the electrode area can be increased when the capacity of the single battery is improved, and more positive and negative electrode series-parallel connection structures are designed, so that the liquid metal battery has great advantages in further development of a high-capacity single liquid metal battery.
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELD

[0001] The present application relates to the technical field of liquid metal batteries, in particular to a liquid metal battery and an assembling process thereof. BACKGROUND

[0002] The liquid metal battery is a molten salt electrochemical energy storage device based on the self-layering characteristics between the medium-high temperature molten salt electrolyte and the liquid metal electrode. This type of battery is different from the conventional solid-state battery system. Under medium-high temperature conditions, the positive and negative electrodes of the battery are both liquid metal, and the middle layer is liquid inorganic molten salt electrolyte, which spontaneously forms a three-layer liquid (negative electrode-electrolyte-positive electrode) according to the density difference. The alloying / de-alloying reactions of the negative metal in the positive metal correspond to the charging and discharging processes, respectively. Due to the full-liquid electrode-electrolyte contact interface and medium-high temperature operating conditions, the electrode interface of the liquid metal battery not only ensures good electron conduction and fast ion transport, but also avoids the dendrite problem caused by solid-liquid phase change due to the full-liquid deposition and dissolution reaction of the negative electrode. Therefore, the liquid metal battery has the characteristics of easy expansion of single battery capacity, high safety, excellent rate performance and long cycle life as a large-scale power storage device.

[0003] In the traditional liquid metal battery, the three-layer full-liquid electrode-electrolyte interface structure provides convenience for the assembly of single batteries. By expanding the lateral reaction area of the electrode-electrolyte, the capacity of the single battery can be flexibly expanded within a certain range. However, this battery structure has the following two problems in industrial production and practical application: In the parallel electrode-electrolyte interface based on density self-layering, the single active material plane leads to the inability to laterally lead out the positive and negative electrode current collectors and sealing elements, resulting in insufficient utilization of the vertical space of the single battery. When increasing the capacity of the single battery, a larger reaction area corresponds to a lower space utilization efficiency. For example, the effective space utilization efficiency of the battery calculated according to the existing battery structure is only 20.3%. In addition, the single electrode-electrolyte interface in the parallel single battery leads to higher polarization overpotential due to the influence of the single interface electrochemical reaction kinetics and ion diffusion rate during the high-capacity single battery and high-rate charging and discharging processes, which affects the energy efficiency of the battery. Therefore, the present application provides a liquid metal battery and an assembling process thereof to solve the problems in the background art. SUMMARY

[0004] (I) Technical problems solved In view of the deficiencies of the prior art, the liquid metal battery and its assembly process provided by the application solve the problem that, in the parallel electrode-electrolyte interface based on density self-layering, a single active material plane causes the positive and negative electrode current collectors and the seal to be unable to be led out laterally, resulting in insufficient longitudinal space utilization of the single battery, and when the capacity of the single battery is improved, a larger reaction area corresponds to a lower space utilization efficiency, for example, the effective space utilization efficiency of the battery calculated according to the existing battery structure is only 20.3%, the electrode interface in the liquid metal in the parallel single battery is single, and in the process of high-capacity single battery and high-rate charging and discharging, a higher polarization overpotential is caused due to the influence of the single interface electrochemical reaction kinetics and ion diffusion rate, thereby affecting the energy efficiency of the battery.

[0005] (II) Technical solutions To achieve the above object, the application is implemented by the following technical solutions: a liquid metal battery comprising two battery housings, the two battery housings being arranged in front and back, and a composite negative electrode piece being arranged at the upper end of the two battery housings, an insulating guide groove being arranged at the center of the lower end surface of the composite negative electrode piece towards the two sides, and a composite negative electrode piece being arranged between the two insulating guide grooves. The composite negative electrode piece comprises a negative electrode porous plate, negative electrode current collectors being arranged at the front and back end surfaces of the negative electrode porous plate, an installation groove being arranged at the center of the upper end surface of the negative electrode porous plate, a negative electrode connecting piece being arranged at the upper end of the installation groove, a clamping groove being arranged at the lower end surface of the negative electrode connecting piece, and an insulating sealing piece being slidably connected to the center of the upper end surface of the composite negative electrode piece, the insulating sealing piece penetrating through the lower end surface of the battery end cover to the upper end of the battery end cover.

[0006] Preferably, a molten salt electrolyte is arranged at the front end of the negative electrode current collector at the front and the rear end of the negative electrode current collector at the back, and a positive electrode porous plate is arranged at the front end of the molten salt electrolyte at the front and the rear end of the molten salt electrolyte at the back. Taking the positive electrode porous plate at the front as an example, the positive electrode porous plate comprises a plate frame, a plurality of through holes being arranged in a rectangular array at the lower part of the rear inner wall of the plate frame, forming a vertical ion transmission channel, and the design logic of the porous carbon nanosheet significantly increases the contact area of the electrolyte and the positive electrode active material.

[0007] Preferably, a porous grid is arranged at the inside of the through hole at the front and the inside of the through hole at the back, and a positive electrode metal is arranged at the inside of the through hole at the front of the porous grid at the front and the inside of the through hole at the back of the porous grid at the back, thereby shortening the diffusion distance of lithium ions in the electrode and reducing the concentration polarization, especially in high-load electrodes, the effect is more significant, the porous grid significantly increases the effective reaction area of the electrode through its porous characteristics, so that the same mass of active material can be dispersed on a larger area to participate in the reaction and improve the surface capacity density.

[0008] Preferably, the two positive porous plates are symmetrically arranged with the center line of the composite negative part as the axis, and the two positive electrodes and the two negative electrodes are arranged to form two parallel electrochemically active interfaces.

[0009] A liquid metal battery assembly process, comprising the following steps: S1. Composite negative part preparation, a proper amount of negative metal or alloy is heated to complete melting, then the cleaned negative current collector is put into the molten negative metal or alloy, the adsorbed negative metal or alloy is calculated according to the weight gain before and after the negative current collector, two composite parts adsorbing the same metal or alloy are respectively obtained by using the same parts and operations, and the composite parts are fixed on the negative porous plate by using fasteners, and the negative porous plate and the insulating sealing part are welded together by using connecting parts to form the whole composite negative part. S2. Positive electrode preparation, the battery shell, the porous grid and the positive porous plate are welded to form a preliminary vertical battery structure, then a proper amount of positive metal is directly added into the positive space between the porous grid and the battery shell, and the metal is uniformly dispersed, and the dispersed area is opposite to the negative current collector. S3. Pre-melting, the composite negative part is arranged in the preliminary battery shell according to the two insulating guide groove structures, a certain amount of powder state inorganic compound is mixed, dried and dehydrated, then pre-melting is carried out, and the pre-melted electrolyte is directly added into the battery shell in a molten state to ensure that the molten salt electrolyte liquid level reaches the upper end height of the negative current collector. S4. Assembly, the above battery is naturally cooled, then the battery end cover is welded with the battery shell, the battery is completely sealed after full welding, and is welded with the lower end of the insulating sealing part, finally, copper wires are welded on the battery end cover and the negative pole respectively, and the test is carried out under constant temperature conditions.

[0010] (Three) beneficial effects The application provides a liquid metal battery and an assembly process thereof. In the application, the vertical battery structure comprises two positive electrodes and two negative electrodes, thereby forming two parallel electrochemically active interfaces, and when the capacity of the single battery is improved, the electrode area can be increased, and by designing more positive and negative electrode series-parallel structures, the single liquid metal battery with large capacity can be further developed.

[0011] In the application, multiple positive and negative electrodes can be arranged in parallel in the vertical battery structure, and the vertical electrode structure is beneficial to fully utilize the longitudinal space of the battery, the space utilization efficiency of the battery is improved to 39.5%, the energy density of the liquid metal battery energy storage module is obviously improved, and in addition, the battery module with higher energy density further reduces auxiliary heating power consumption, thereby reducing the energy storage cost.

[0012] In the present application, the vertical battery structure is combined by multiple positive and negative electrodes in parallel, so that the active sites in the battery can increase the electrochemical reaction. Compared with the traditional battery, the same capacity of the vertical battery and the same mass of active material are dispersed on a larger active area for electrode reaction, the ion diffusion efficiency of the electrode interface is significantly improved, the electronic exchange interface is significantly improved, which leads to smaller concentration polarization of the battery. Therefore, the vertical battery in the present application has higher energy efficiency. BRIEF DESCRIPTION OF DRAWINGS

[0013] Figure 1 is a perspective view of the present application; Figure 2 is a perspective view of the present application; Figure 3 is a perspective view of the present application; Figure 4 is a perspective view of the present application; Figure 5 is a perspective view of the present application; Figure 6 is a perspective view of the present application; Figure 7 is a perspective view of the present application; Figure 8 is a perspective view of the present application; Figure 9 is a perspective view of the present application; Figure 10 is a perspective view of the present application; Figure 11 is a perspective view of the present application; Figure 12 is a perspective view of the present application; Figure 13 is a perspective view of the present application; Figure 14 is a perspective view of the present application.

[0014] 1, battery shell; 2, composite negative electrode; 3, battery end cover; 4, insulating guide groove; 5, molten salt electrolyte; 6, positive porous plate; 7, porous grid; 8, positive metal; 201, insulating sealing piece; 202, negative electrode connecting piece; 203, clamping groove; 204, negative electrode porous plate; 205, mounting groove; 206, negative electrode current collector; 601, plate frame; 602, through hole. DETAILED DESCRIPTION

[0015] The following will clearly and completely describe the technical solutions in the embodiments of the present invention in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of the present invention.

[0016] Example 1: like Figures 1-6 As shown, an embodiment of the present invention provides a liquid metal battery, comprising two battery shells 1, which are arranged in a front-to-back arrangement. A composite negative electrode member 2 is provided at the upper end of the two battery shells 1, and insulating guide grooves 4 are provided on both sides of the center of the lower end surface of the composite negative electrode member 2. A composite negative electrode member 2 is provided between the two insulating guide grooves 4.

[0017] The composite negative electrode component 2 includes a negative electrode porous plate 204, and negative electrode current collectors 206 are provided on the front and rear end surfaces of the negative electrode porous plate 204. A mounting groove 205 is opened at the center of the upper end surface of the negative electrode porous plate 204, and a negative electrode connector 202 is provided at the upper end of the mounting groove 205. A card slot 203 is provided on the lower end surface of the negative electrode connector 202. An insulating seal 201 is slidably connected to the center of the upper end surface of the composite negative electrode component 2, and the insulating seal 201 passes through the lower end surface of the battery end cover 3 and reaches the upper end of the battery end cover 3.

[0018] The front end of the negative electrode current collector 206 at the front and the rear end of the negative electrode current collector 206 at the rear are both provided with a molten salt electrolyte 5, and the front end of the molten salt electrolyte 5 at the front and the rear end of the molten salt electrolyte 5 at the rear are both provided with a positive electrode porous plate 6; Taking the positive electrode porous plate 6 at the front as an example, the positive electrode porous plate 6 includes a plate frame 601. A plurality of through holes 602 are arranged in a rectangular shape at the lower part of the rear inner wall of the plate frame 601, forming a vertical ion transmission channel. The design logic of the porous carbon nanosheet significantly increases the contact area between the electrolyte and the positive electrode active material.

[0019] A porous grid 7 is provided at the rear of the front through-hole 602 and at the front of the rear through-hole 602. A positive electrode metal 8 is provided at the interior of the front through-hole 602 at the front end of the front porous grid 7 and at the interior of the rear through-hole 602 at the rear end of the rear porous grid 7. This shortens the diffusion distance of lithium ions in the electrode and reduces concentration polarization, which is particularly effective in high-load electrodes. The porous grid 7 significantly increases the effective reaction area of ​​the electrode through its porous characteristics, so that the same mass of active material can be dispersed over a larger area to participate in the reaction, thereby improving the surface capacity density.

[0020] The two positive electrode porous plates 6 are symmetrically arranged with the center line of the composite negative electrode member 2 as the axis, and the two positive electrodes and the two negative electrodes thus form two parallel electrochemical active interfaces.

[0021] A liquid metal battery assembly process, comprising the following steps: As shown in Figure 7 S1. Composite negative electrode preparation, a certain amount of negative electrode metal or alloy is heated to complete melting, and then the cleaned negative electrode current collector 206 is placed in the molten negative electrode metal or alloy. The adsorbed negative electrode metal or alloy is calculated according to the weight gain of the negative electrode current collector 206 before and after the adsorption. Two composite parts adsorbing the same metal or alloy are obtained by using the same parts and operations, and are fixed on the negative electrode porous plate 204 by using fasteners. The negative electrode porous plate 204 and the insulating sealing part 201 are welded together by the negative electrode connecting part 202 to form the entire composite negative electrode 2. S2. Positive electrode preparation, welding the battery shell 1, the porous grid 7 and the positive electrode porous plate 6 to form a preliminary vertical battery structure, and then adding a certain amount of positive electrode metal 8 into the positive electrode space between the porous grid 7 and the battery shell 1, and ensuring that the metal is uniformly dispersed, and the dispersed area is opposite to the negative electrode current collector 206. S3. Pre-melting, the composite negative electrode 2 is loaded into the above-mentioned preliminary battery shell 1 according to the structure of the two insulating guide grooves 4. A certain amount of powder state inorganic compound is mixed, dried and dehydrated, and then pre-melted. The pre-melted electrolyte is directly added into the above-mentioned battery shell 1 in a molten state to ensure that the molten salt electrolyte liquid level reaches the upper end of the negative electrode current collector 206. S4. Assembly, naturally cooling the above-mentioned battery, and then welding the battery end cover 3 with the battery shell 1. The battery is completely sealed after full welding, and is welded with the lower end of the insulating sealing part 201. Finally, copper wires are welded on the battery end cover 3 and the negative electrode pole, respectively, and the test is carried out under constant temperature conditions.

[0022] The above steps S1-S3 need to be operated in an inert atmosphere, and the battery test is carried out in an air atmosphere under constant temperature conditions.

[0023] Example two: the difference between this example and example one is: As shown in Figure 7 S1. In the full discharge state, the battery negative electrode surface does not need to adsorb any metal, and two cleaned blank negative electrode current collectors 206 are directly fixed on the negative electrode porous plate 204 by thread engagement, and the negative electrode porous plate 204 and the insulating sealing part 201 are welded together by the negative electrode connecting part 202 to form the entire composite negative electrode. S2. First, the positive metal 8 or alloy, negative metal or alloy are put together in the positive area in the middle of the inside of the battery shell 1 part 10, and make sure the mixed metal powder is evenly dispersed, the area of dispersion is opposite to the negative current collector 206, second, the whole battery shell 1, positive porous plate 6 and porous grid 7 are heated, and when all the metals are melted and form a uniform mixed phase, that is, the full discharge positive product, finally, another completely shaped positive shell 1 and positive full discharge product are prepared according to the above method, and the two completely symmetrical battery shells are welded; S3. The blank negative part in the above is put into the complete battery shell 1 of S2 according to the structure of the insulating guide groove 4, a certain amount of powder state inorganic compound is mixed, dried and dehydrated, and then pre-melted, and the pre-melted electrolyte is directly added into the above battery shell 1 in a molten state, so that the molten salt electrolyte liquid surface reaches the upper end of the negative current collector 206; S4. The above battery is naturally cooled, and then the battery end cover 3 is welded with the battery shell 1, and the battery is completely sealed after full welding, and is welded with the lower end of the insulating sealing piece 201. Finally, copper wires are welded on the battery end cover and the negative pole respectively, and the test is carried out under constant temperature conditions.

[0024] The above steps S1-S3 need to be operated in an inert atmosphere, and the battery test is carried out in an air atmosphere under constant temperature conditions.

[0025] Comparative example: As Figure 7 , 8, 9 and 10, the battery structure and assembly process proposed in the application can avoid the active material in the vertical electrode from flowing or overflowing due to density, and the combined composite negative electrode 2 can be ensured to be always in the center of the two positive electrodes by limiting the negative current collector 206 inside the battery, so as to realize stable operation of the single battery. The discharge capacity of the calcium-based liquid metal battery assembled by the assembly process in the embodiment can reach 14.3 Ah, and after the initial cycle, the battery capacity tends to be stable, and there is almost no capacity decay. After 26 cycles, the battery energy efficiency is 80%, and the coulomb efficiency is 92%. During the charging process, the voltage curve extends to high potential with the increase of capacity, and during the discharging process, the curve corresponding to the battery voltage drop. After a certain number of cycles, the battery voltage curve gradually coincides, indicating that a completely reversible electrochemical reaction occurs in the vertical electrode, and the electrode active material does not appear to shuttle or lose during the charging and discharging process. At a current density of 0.2C, the average charging voltage of the battery is 1.0V, and the average discharging voltage is 0.85V. It can be found that the normal battery after 26 cycles is cut and disassembled, and the positive metal 8 in the black dashed box in the battery profile is limited in the specified area between the porous grid 7 and the battery shell 1, and does not appear to diffuse or overflow. The negative electrode porous plate 204 also does not appear to shift the center line position, indicating that the insulating guide groove 4 in the battery structure can prevent the thermal stress offset of the negative electrode porous plate 204, and finally realizes the stable operation of the liquid metal battery under this structure.

[0026] At the same time, in addition to the above-mentioned full charging assembly method, the vertical battery proposed in the application can also be assembled in a full discharge state. According to the assembly process in Example Two, the positive and negative active metals are assembled in the positive electrode area in the form of a mixed alloy, and the negative electrode is a blank foam metal. After the first charge, the initial positive electrode alloy in the battery is separated, the negative electrode metal is deposited on the negative electrode current collector 206, and the positive electrode metal 8 remains in the positive electrode area. The corresponding battery can realize stable charging and discharging full cycle. The battery assembly capacity is 5 Ah, and after 23 cycles, the battery capacity is stabilized at 3.71 Ah, and shows a reversible charging and discharging reaction platform, indicating that the vertical battery proposed in the application has an expandable assembly method, and the battery structure has stable electrochemical performance in both full charge and full discharge states.

[0027] As Figure 11 And 12As shown in the figure, in order to verify the specific technical effect of the vertical battery structure in the application, the insulating guide groove 4 is not used in the battery assembly process, the battery material system and the assembly process conditions are the same as those in the above embodiment, and only the assembly process of the battery structure without the assembly of the porous grid 7 and the performance of the calcium-based battery after the assembly of the battery structure are different. After 3 complete charging and discharging processes, the voltage curve of the charging capacity of 10.56 Ah begins to appear micro-short circuit, and the battery shows complete short circuit in the 5th charging process, indicating that the positive and negative active materials of the battery exist contact short circuit. The corresponding battery section view shows that due to the offset of the negative porous plate 204 and the negative current collector 206, the difference between the left and right positive and negative electrode spacing in the battery is increased, which further affects the electric field distribution, and finally makes the active metal part of the positive electrode region overflow, which causes the battery short circuit. The comparative example shows that the composite negative electrode 2 in the vertical battery structure will be offset and twisted under the influence of thermal stress, which will affect the distribution of the electric field, magnetic field and other fields in the battery, and finally affect the stability of the battery operation.

[0028] As Figure 13 With 14 As shown in the figure, in order to verify the selective barrier effect of the porous grid 7 in the battery structure in the application, according to the battery structure without welding the porous grid 7, the charging curve of the corresponding battery can find that the battery has obvious short circuit during the first charging process. The section view after cutting in the dashed box in the figure shows that the positive electrode metal 8 in the battery has obvious diffusion. Due to the density difference, the accumulation of the positive electrode metal 8 at the bottom of the battery shell is the main reason for the short circuit of the battery. The white arrow and the dashed box in the figure show that the positive electrode porous plate 6 alone cannot limit the flow and diffusion of the positive electrode metal 8. The porous grid 7 in the application has good confinement effect on the positive electrode metal 8.

[0029] Although the embodiments of the application have been shown and described, it can be understood by those skilled in the art that various changes, modifications, replacements and variations can be made to the embodiments without departing from the principles and spirits of the application, and the scope of the application is defined by the appended claims and their equivalents.

Claims

1. A liquid metal battery comprising two battery shells (1), characterized in that: The two battery housings (1) are arranged front to back, the upper ends of the two battery housings (1) are provided with composite negative electrode members (2), the lower end faces of the composite negative electrode members (2) are provided with insulating guide grooves (4) at both sides of the center, and the composite negative electrode member (2) is provided between the two insulating guide grooves (4); The composite negative electrode member (2) comprises a negative electrode porous plate (204), and negative electrode current collectors (206) are provided on both the front and rear end surfaces of the negative electrode porous plate (204). A mounting groove (205) is provided at the center of the upper end surface of the negative electrode porous plate (204), and a negative electrode connector (202) is provided at the upper end of the mounting groove (205). A clamping groove (203) is provided at the lower end surface of the negative electrode connector (202). An insulating seal (201) is slidably connected at the center of the upper end surface of the composite negative electrode member (2), and the insulating seal (201) passes through the lower end surface of the battery end cover (3) and reaches the upper end of the battery end cover (3).

2. The liquid metal battery according to claim 1, characterized in that: The front end of the negative electrode current collector (206) at the front and the rear end of the negative electrode current collector (206) at the rear are both provided with a molten salt electrolyte (5), and the front end of the molten salt electrolyte (5) at the front and the rear end of the molten salt electrolyte (5) at the rear are both provided with a positive electrode porous plate (6); Taking the positive electrode porous plate (6) at the front as an example, the positive electrode porous plate (6) includes a plate frame (601), and a plurality of through holes (602) are arranged in a rectangular shape at the lower portion of the rear inner wall of the plate frame (601).

3. The liquid metal battery according to claim 2, characterized in that: A porous grid (7) is provided at the rear of the front through hole (602) and at the front of the rear through hole (602). A positive electrode metal (8) is provided at the interior of the front through hole (602) at the front end of the porous grid (7) and at the rear through hole (602) at the rear end of the porous grid (7).

4. The liquid metal battery according to claim 2, characterized in that: The two positive electrode porous plates (6) are symmetrically arranged with the center line of the composite negative electrode member (2) as the axis.

5. A liquid metal battery assembly process, using a liquid metal battery according to any one of claims 1 to 4, characterized in that: The following steps are involved: S1. Preparation of a composite negative electrode member (2): heating an appropriate amount of negative electrode metal or alloy until completely melted, placing a cleaned negative electrode current collector (206) into the molten negative electrode metal or alloy, calculating the adsorbed negative electrode metal or alloy based on the weight gain of the negative electrode current collector (206), obtaining two composite members adsorbing the same metal or alloy using the same parts and operations, fixing them to the negative electrode porous plate (204) using fasteners, and welding the negative electrode porous plate (204) and the insulating seal (201) together through a connector (202) to form the entire composite negative electrode member (2); S2. Preparation of the positive electrode: welding the battery housing (1), the porous grid (7) and the positive electrode porous plate (6) to form a preliminary vertical battery structure, and then adding an appropriate amount of positive electrode metal (8) directly into the positive electrode space between the porous grid (7) and the battery housing (1), and ensuring that the metal is evenly dispersed, and the dispersed area is directly opposite to the negative electrode current collector (206); S3. Pre-melting, placing the composite negative electrode member (2) into the above-mentioned preliminary battery housing (1) according to the two insulating guide grooves (4) structure, mixing a certain amount of powdered inorganic compound, drying, and dehydrating, and then pre-melting, and directly adding the pre-melted electrolyte into the above-mentioned battery housing (1) in a molten state, ensuring that the molten salt electrolyte liquid level reaches the height of the upper end of the negative electrode current collector (206); S4. Assemble, cool the battery naturally, then weld the battery end cap (3) to the battery housing (1), completely seal the battery interior after full welding, and weld to the lower end of the insulating seal (201), and finally weld copper wires to the battery end cap (3) and the negative electrode, respectively, and test under constant temperature conditions.