Manufacturing method of three-dimensional system chip based on aluminum nitride bonding structure and three-dimensional system chip
By employing aluminum nitride bonding structures and chemical plating interconnect processes in 3D system-on-a-chip (SoC), the heat dissipation and insulation problems in 3D integration are solved, achieving efficient heat dissipation and high-reliability interconnection, which is suitable for high-performance computing and RF power amplifiers.
Patent Information
- Application Number
- CN202610058067.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-01-15
- Publication Date
- 2026-05-01
AI Technical Summary
Existing 3D integration technologies suffer from insufficient heat dissipation performance, complex insulation and interconnection processes that are difficult to optimize in a coordinated manner, and thus cannot meet the heat dissipation requirements of high-power chips.
Aluminum nitride is used as the bonding and filling medium. Vertical interconnection between the mother core and the daughter core is achieved through the aluminum nitride bonding layer. Combined with chemical plating, a metal interconnect is formed, thus constructing an efficient vertical and lateral heat dissipation path.
It achieves high insulation and efficient heat dissipation, simplifies process steps, improves interconnect reliability and integration, and is suitable for high-performance heterogeneous integration.
Smart Images

Figure CN121969196A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the fields of semiconductor manufacturing and advanced packaging technology. Specifically, it relates to a manufacturing method and a three-dimensional system chip suitable for high power density and high integration scenarios, and particularly to an integrated solution that integrates bonding, insulation and heat dissipation using aluminum nitride material. Background Technology
[0002] As Moore's Law approaches its physical limits, heterogeneous integration of chips with different process nodes and functions through 3D stacking technology has become the mainstream direction for improving system performance and achieving "beyond Moore's Law" development. However, while 3D integration brings advantages such as high bandwidth and small size, it also introduces severe challenges: First, the challenge of interconnect density and reliability. Traditional microbump bonding technology has stringent alignment accuracy requirements, and the reflow process introduces thermal stress. Second, the heat dissipation bottleneck. The stacked structure makes it difficult to effectively dissipate the heat generated by high-power chips, and heat accumulation seriously affects chip performance and lifespan. Third, insulation and parasitic effects. The dielectric material between dense interconnects needs to have both good insulation and low dielectric constant to reduce signal crosstalk and delay.
[0003] Currently, mainstream wafer-level 3D integration methods mostly employ silicon dioxide, polymers (such as polyimide PI, benzocyclobutene BCB), or hybrid bonding techniques to achieve inter-chip bonding and insulation. However, these materials generally have low thermal conductivity (typically less than 2 W / m·K), which cannot meet the heat dissipation requirements of high-power chips (such as high-performance computing units and RF power amplifiers). Although existing technologies have attempted to introduce independent metal heat-conducting pillars or thermal interface materials, they often face problems such as complex processes, difficulty in co-designing with electrical interconnect structures, and increased parasitic capacitance.
[0004] Therefore, there is an urgent need to develop an innovative three-dimensional integration method that can combine excellent heat dissipation materials with advanced interconnect technology to fundamentally solve the heat dissipation and reliability problems of high-performance three-dimensional system chips. Summary of the Invention
[0005] In view of this, the purpose of this invention is to provide a three-dimensional system chip based on an aluminum nitride bonding structure and its manufacturing method, so as to solve the problems of insufficient heat dissipation performance, complex insulation and interconnection processes and difficulty in co-optimization in existing three-dimensional integration technologies.
[0006] To achieve the above objectives, the present invention provides a method for manufacturing a three-dimensional system-on-a-chip based on an aluminum nitride bonding structure, comprising the following steps: S10: Provide a mother wafer with a mother core metal electrode array on its surface; provide at least one sub-core with a sub-core metal electrode array on its surface; S20: An aluminum nitride bonding layer is formed on the surface of the mother wafer and / or the surface of the sub-core in the non-electrode interconnect region; S30: Align the sub-core with the mother wafer stack and bond them through the aluminum nitride bonding layer, so that the mother core metal electrode array and the sub-core metal electrode array are vertically interconnected.
[0007] Preferably, the bonding in step S30 is such that the mother core metal electrode array and the daughter core metal electrode array are perpendicularly opposite each other and an interconnection gap is formed therebetween; Metal is selectively grown onto the surfaces of the mother core metal electrode array and the daughter core metal electrode array through the interconnection gaps until the grown metal is connected as one in the interconnection gaps to form a vertical interconnection structure.
[0008] Preferably, a supporting metal block is also provided on the surface of the mother wafer and / or the surface of the sub-core, and the bonding in step S30 causes the supporting metal block and the aluminum nitride bonding layer to be mixed and bonded.
[0009] Preferably, aligning the sub-core with the parent wafer involves stacking the sub-core upside down on the surface of the parent wafer; wherein the sub-core may be located on the sub-wafer, and the parent wafer includes at least one parent core.
[0010] Preferably, the bonding process includes applying pressure and heating to 300°C~900°C in a vacuum or inert atmosphere to promote the formation of a strong bond between the aluminum nitride bonding layer and the contact surface.
[0011] Preferably, the method for forming the aluminum nitride bonding layer is physical vapor deposition or chemical vapor deposition, the deposition thickness is 20 nm to 20 μm, and the substrate temperature during deposition is 200°C to 500°C.
[0012] Preferably, after the bonding in step S30, the method further includes the following step: Aluminum nitride is deposited on the exposed surface of the integral structure formed by bonding the mother wafer and the daughter core particles using a chemical vapor deposition process, so as to fill the area outside the interconnect gaps and form an aluminum nitride filling medium. The process parameters of the chemical vapor deposition include: using trimethylaluminum and ammonia as precursors, the reaction pressure is 10 Pa to 1000 Pa, and the reaction temperature is 300°C to 600°C.
[0013] Preferably, the chemical vapor deposition process deposits aluminum nitride to fill the area outside the interconnect gaps and the lateral gaps between the core particles, forming an aluminum nitride filling medium and a planarized package surface.
[0014] Preferably, in step S20, before or after forming the aluminum nitride bonding layer, metal bumps or metal pillars are formed on the metal electrodes of the mother core metal electrode array and / or the daughter core metal electrode array.
[0015] Preferably, the selective metal growth process is chemical plating, and the metal material includes one or an alloy of copper, aluminum, tungsten, molybdenum, nickel, tin, cobalt, tantalum, silver, and gold.
[0016] Preferably, in step S10, providing the mother wafer includes: providing a carrier substrate and fixing at least two mother cores to the carrier substrate through a temporary bonding layer; after the vertical interconnect structure is formed, the step further includes removing the temporary bonding layer and the carrier substrate.
[0017] Another aspect of the present invention provides a three-dimensional system-on-a-chip based on an aluminum nitride bonding structure, manufactured using the above-described method, comprising: The mother wafer has a mother core metal electrode array on its surface; At least one sub-core is stacked upside down on the mother wafer, and its surface has a sub-core metal electrode array; An aluminum nitride bonding layer is located between the mother wafer and the sub-core, and is distributed outside the interconnection region of the mother core metal electrode array and the sub-core metal electrode array, fixing the mother wafer and the sub-core to bond together, and the mother core metal electrode array and the sub-core metal electrode array are vertically interconnected.
[0018] Preferably, it further includes a vertical interconnect structure located between the vertically opposite electrodes of the mother core metal electrode array and the daughter core metal electrode array, electrically connecting the two.
[0019] Preferably, it further includes a support metal block located between the mother wafer and the daughter core, the support metal block being co-bonded with the aluminum nitride bonding layer.
[0020] Preferably, the thickness of the aluminum nitride bonding layer is 0.05 μm to 20 μm.
[0021] Preferably, it further includes an aluminum nitride filling medium, which fills the area between the mother wafer and the sub-cores excluding the vertical interconnect structure, and the lateral gaps between the plurality of sub-cores; the aluminum nitride filling medium is in physical contact with or integrally formed with the aluminum nitride bonding layer.
[0022] Preferably, metal bumps or metal pillars protruding towards each other are formed on the metal electrodes of the mother core metal electrode array and / or the daughter core metal electrode array.
[0023] Preferably, the vertical interconnect structure is made of a metal material formed by chemical plating, and the metal material includes one or an alloy of copper, aluminum, tungsten, molybdenum, nickel, tin, cobalt, tantalum, silver, and gold.
[0024] Preferably, the aluminum nitride bonding layer is distributed around the interconnection region of the mother core metal electrode array and the daughter core metal electrode array, and is insulated from the interconnection region in the vertical direction; A vertical interconnect structure, penetrating the reserved cavity in the aluminum nitride bonding layer or filling the gap defined by the aluminum nitride sidewalls, electrically connects the mother core metal electrode array and the daughter core metal electrode array accordingly.
[0025] Preferably, the aluminum nitride bonding layer is in direct contact with and bonded to the semiconductor substrate or surface passivation layer of the mother wafer and the daughter core, wherein the passivation layer is made of aluminum nitride.
[0026] The beneficial effects of this invention are as follows: Collaborative solution to heat dissipation and insulation issues: The innovative use of high thermal conductivity aluminum nitride as a bonding and filling medium achieves high insulation while establishing efficient vertical and lateral heat dissipation paths for three-dimensional stacked chips, significantly reducing the junction temperature of high-power chips.
[0027] Simplified process and high integration: The aluminum nitride bonding layer can be integrated with or co-processed with the subsequent aluminum nitride filling medium, reducing process steps. After bonding, in-situ chemical plating forms interconnects, avoiding complex photolithography and reflow soldering processes and improving yield.
[0028] High reliability and high-density interconnects: The thermal expansion coefficients of aluminum nitride and silicon are matched, reducing thermal stress. The electroless plating creates metal interconnects without interface voids, resulting in low resistance and high reliability. Combined with a metal bump design, ultra-fine pitch interconnects with high alignment tolerance can be achieved.
[0029] Excellent heterogeneous integration compatibility: This method is insensitive to the material, size, and process node of the mother wafer and the daughter chip, and is particularly suitable for high-density, high-performance heterogeneous integration of silicon-based logic chips, compound semiconductor RF chips, memory, etc. Attached Figure Description
[0030] To more clearly illustrate the technical solutions in the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0031] Figure 1 This is a flowchart of a three-dimensional system-on-a-chip manufacturing method according to an embodiment of the present invention; Figure 2-6 This is a schematic cross-sectional view of each step in the manufacturing process of an embodiment of the present invention. Figure 7 This is a cross-sectional structural diagram corresponding to the manufacturing process of another embodiment of the present invention.
[0032] Label Explanation: 100 - Mother wafer; 110 - Mother core; 111 - Mother core metal electrode array; 120 - Temporary bonding layer; 200 - Sub-core / sub-wafer; 210 - Sub-core metal electrode array; 300 - Aluminum nitride bonding layer; 310 - Aluminum nitride filling dielectric; 400 - Metal bump; 410 - Metal pillar; 500 - Vertical interconnect structure; 600 - Interconnect gap / reserved cavity. Detailed Implementation
[0033] Preferred embodiments of the invention will now be described in more detail. While preferred embodiments of the invention are described below, it should be understood that the invention can be implemented in various forms and should not be limited to the embodiments set forth herein.
[0034] In this invention, unless otherwise stated, directional terms such as "upper" and "lower" generally refer to the upper and lower parts of the device in its normal operating state, while "inner" and "outer" refer to the parts relative to the outline of the device. Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Thus, a feature defined as "first," "second," or "third" may explicitly or implicitly include one or more of that feature. In the description of this invention, "a plurality of" means two or more, unless otherwise explicitly specified. This invention pertains to electrical devices; therefore, connection and interconnection both refer to conductive interconnection. Since the accompanying drawings describe the same device, the same reference numerals denote the same components. The term "chip front" as used herein refers to the side of the wafer used to form the device during chip manufacturing, and "back" refers to the substrate side of the wafer.
[0035] refer to Figure 1 and Figure 2-6 This embodiment details a basic manufacturing method for a three-dimensional system-on-a-chip based on an aluminum nitride bonding structure.
[0036] Step S10: Provide a mother wafer with a mother core metal electrode array on its surface; provide at least one sub-core with a sub-core metal electrode array on its surface.
[0037] like Figure 2As shown, a mother wafer 100 is provided as an integration carrier. In this embodiment, the mother wafer 100 is a complete silicon wafer that has undergone through-silicon via (TSV) processing. A copper core metal electrode array 111 is formed on its surface through passivation layer openings and a redistribution layer (RDL). The mother wafer may contain mother cores 110; in this embodiment, only two are shown. Simultaneously, pre-manufactured sub-cores 200 to be integrated are provided. For example, a gallium arsenide (GaAs) RF power amplifier core, whose active surface also forms a sub-core metal electrode array 210. In this embodiment, two sub-cores 200 are described as having been cut from the original wafer and undergone backside thinning. In this embodiment, the mother core metal electrode 111 can be a bond pad, or a through-silicon via without a bond pad, a metal interconnect structure, or an exposed metal interconnect lead.
[0038] In one embodiment, the surfaces of the mother chip and daughter chip, except for the electrodes, may be covered with an aluminum nitride passivation layer. The aluminum nitride passivation layer refers to the aluminum nitride insulating film formed on the surface of the chip during the chip manufacturing process, covering the non-electrode areas, as a protective layer and bonding interface for the chip itself.
[0039] It should be noted that if the chip surface already has an aluminum nitride passivation layer, it will provide a better interface for subsequent bonding with the same material. In other embodiments, the sub-chip 200 can also be an uncut chip located on the wafer to be packaged or on the sub-wafer 200 after wafer reconstruction. The wafer can be fabricated using integrated circuit manufacturing technology, such as forming N-type metal-oxide-semiconductor (NMOS) devices and P-type metal-oxide-semiconductor (PMOS) devices on a semiconductor substrate through processes such as deposition and etching. Dielectric layers, metal interconnect structures, and electrodes electrically connected to the metal interconnect junctions are formed on the devices, thereby forming multiple sub-chips 200 in the wafer, and the multiple sub-chips 200 can be chips of the same type or different types.
[0040] Step S20: An aluminum nitride bonding layer is formed on the surface of the mother wafer and / or the surface of the sub-core in the non-electrode interconnect region. The aluminum nitride bonding layer refers to the aluminum nitride thin film layer pre-formed on the surface of the wafer or core in the three-dimensional integrated packaging process to achieve mechanical stacking.
[0041] like Figure 3As shown, an aluminum nitride thin film is deposited on the surface of the mother wafer 100 using magnetron sputtering (a PVD process) to form an aluminum nitride bonding layer 300. Specific process parameters are as follows: high-purity aluminum is used as the target material; the chamber pressure is 0.5 Pa in a mixed atmosphere of argon and nitrogen; the substrate temperature is controlled at 350°C; the deposition power is 5 kW; and the deposition time is approximately 30 minutes, resulting in a dense aluminum nitride layer with a thickness of approximately 2 μm. After deposition, the aluminum nitride directly above the mother core metal electrode 111 is removed using photolithography and reactive ion etching (RIE) processes, exposing the electrode surface so that the aluminum nitride bonding layer 300 remains only in the non-electrode interconnect region. Similarly, the aluminum nitride bonding layer 300 can also be formed on the sub-core or sub-wafer.
[0042] Preferably, the bonding process includes applying pressure and heating to 300°C~900°C in a vacuum or inert atmosphere to promote the formation of a strong bond between the aluminum nitride bonding layer 300 and the contact surface.
[0043] Preferably, the method for forming the aluminum nitride bonding layer 300 is physical vapor deposition or chemical vapor deposition, the deposition thickness is 20 nm to 20 μm, and the substrate temperature during deposition is 200°C to 500°C.
[0044] Step S30: Align the sub-core with the mother wafer stack and bond them through the aluminum nitride bonding layer, so that the mother core metal electrode array and the sub-core metal electrode array are vertically interconnected.
[0045] In this embodiment, the bonding in this step results in the parent core metal electrode array 111 and the daughter core metal electrode array 210 being perpendicularly opposite each other, forming an interconnect gap therebetween. In other embodiments, in addition to the electrodes in the electrode interconnect region, the surface of the parent wafer 100 and / or the surface of the daughter core 200 may also have a supporting metal block. The supporting metal block may be formed together with the interconnect metal electrode array, and the bonding step in step S30 utilizes a mixed bonding of the supporting metal block and the aluminum nitride bonding layer 300.
[0046] like Figure 4As shown, the sub-core 200 is flipped so that its active side (the side with the sub-core metal electrode 210) faces the parent wafer 100. In other embodiments, it is not limited to flipping; as long as the side with the electrode faces the parent wafer 100, it is acceptable. Alignment is performed using a high-precision flip-chip mounter so that the sub-core metal electrode 210 of the sub-core 200 is perpendicularly aligned with the parent core metal electrode 111 of the parent wafer 100. Due to the interconnection method of this invention, precise alignment is not required. Subsequently, it is placed in a vacuum bonding machine, where a uniform pressure of 5 MPa is applied under vacuum (pressure < 10^-3 Pa), and the temperature is increased to 650°C at a rate of 10°C / min, and held at this temperature for 30 minutes. During this process, the aluminum nitride bonding layer 300 undergoes solid-state diffusion and chemical reaction with the aluminum nitride bonding layer 300 on the back side of the sub-core 200 or the silicon substrate (or surface passivation layer), forming a strong covalent bond. After bonding, due to the support of the aluminum nitride bonding layer 300, a uniform interconnect gap cavity 600 with a height of approximately 2 μm exists between the top surfaces of the mother core metal electrode 111 and the daughter core metal electrode 210. Preferably, the passivation layer on the surface of the daughter core 200 is also aluminum nitride, so that the aluminum nitride bonding layer 300 on the surface of the mother wafer 100 and the aluminum nitride passivation layer on the surface of the daughter core 200 can be directly bonded, and the same materials can be directly bonded.
[0047] This embodiment also includes the step of: selectively growing metal on the surfaces of the mother core metal electrode array 111 and the daughter core metal electrode array 210 through the cavity 600 reserved in the interconnect gap, until the grown metal is connected as one in the interconnect gap to form a vertical interconnect structure 500.
[0048] like Figure 5 As shown, the bonded monolithic structure was immersed in a chemical copper plating solution. The solution temperature was 85°C, and the pH was maintained at 12.5. The copper electrodes served as catalytic surfaces, where copper ions in the solution selectively reduced and deposited on their exposed surfaces. Metallic copper grew from the upper and lower electrode surfaces towards each other, as shown... Figure 6 As shown, after about 15 minutes of growth, the copper deposited on both sides meet and fuse at the center of the interconnect gap 600 to form a dense, low-resistance copper pillar, namely the vertical interconnect structure 500, thereby electrically connecting the sub-core 200 to the mother wafer 100. For other metals that can be chemically plated (such as nickel or gold) or metals that require catalytic initiation (such as chemically plated copper on a gold electrode), the electrode surface can be pretreated in accordance with the art, such as cleaning, activation, or application of a catalytic seed layer (such as Pd), before chemical plating.
[0049] In one embodiment, the selective metal growth process is chemical plating, and the metal material includes one or an alloy of copper, aluminum, tungsten, molybdenum, nickel, tin, cobalt, tantalum, silver, and gold.
[0050] In one embodiment, the selective metal growth process is chemical plating. The metal material is preferably copper or nickel, but may also be one or more of aluminum, tungsten, molybdenum, tin, cobalt, tantalum, silver, and gold, or an alloy of these elements. The specific material selection depends on the electrode material, process compatibility, and electrical performance requirements.
[0051] In another embodiment, after completion Figure 6 After the interconnection structure shown, perform the following steps: The structure was transferred to a chemical vapor deposition (CVD) apparatus. Trimethylaluminum (TMA) and ammonia (N2) were used. TMA and N were used as precursors, with high-purity nitrogen as the carrier gas. The reaction chamber pressure was set to 200 Pa, and the substrate temperature was set to 450°C. The gas flow ratio is approximately 1:10. Under these conditions, aluminum nitride films will be uniformly deposited over the entire exposed surface of the structure.
[0052] Deposition continues until aluminum nitride completely fills all areas between the mother wafer 100 and the sub-cores 200, except for the space occupied by the vertical interconnect structure 500, forming the aluminum nitride filling medium 310. "Aluminum nitride filling medium" refers to the aluminum nitride bulk material formed by the deposition process after stacking bonding and electrical interconnection are completed, used to fill voids and complete encapsulation. Simultaneously, this deposition also fills the lateral gaps between adjacent sub-cores 200.
[0053] The deposition process continues until the aluminum nitride layer completely covers the sub-core 200 and forms an interference fit. Then, a chemical mechanical polishing (CMP) process is used to planarize the layer, removing excess aluminum nitride until the silicon substrate on the back of the sub-core 200 is exposed, forming a smooth integrated module completely encapsulated and filled with aluminum nitride. The aluminum nitride filling medium and the previously formed aluminum nitride bonding layer 300 are in contact at the sidewalls, together forming a continuous, highly thermally conductive insulator.
[0054] In this embodiment, step S10, "providing a mother wafer," employs a reconstructed wafer approach. Specifically, a silicon substrate is provided, and a temporary bonding adhesive (such as hot-slip adhesive) is coated onto it as a temporary bonding layer. Multiple tested and known qualified silicon-based logic mother chips 110 (each with a mother core metal electrode 111 on its front side) are temporarily bonded to the substrate 100 with their back sides facing down. Then, redistribution (RDL) and deposition and patterning of the aluminum nitride bonding layer 300 are performed on the front side of the mother chips 110 (as described in the first embodiment). Subsequent bonding steps S3, the chemical plating process for forming the vertical interconnect structure, and the optional aluminum nitride filling dielectric deposition process are the same as in the aforementioned embodiments. After all interconnect and packaging steps are completed, the adhesiveness of the temporary bonding layer is released by heating or laser irradiation, and the substrate is removed, thereby obtaining a three-dimensional system-on-a-chip module based on aluminum nitride bonding and filling, consisting of multiple mother chips 110 and daughter chips 200.
[0055] In step S20 of the basic embodiment, while depositing and patterning the aluminum nitride bonding layer 300, a support metal block is simultaneously (or in another photolithography step) formed at specific locations (e.g., the four corners of the core or the periphery of the electrode array) on the surface of the mother wafer 100 in a non-electrode interconnect region. This support metal block can be electroplated concurrently with the mother core metal electrode 111, and the material can be copper, with a height comparable to the thickness of the aluminum nitride bonding layer 300 (e.g., 2 μm). During the bonding process in the subsequent step S30, the support metal block directly contacts the back side of the sub-core 200 (or the corresponding metal block on the sub-core) and shares the bonding pressure with the aluminum nitride bonding layer 300, achieving metal-dielectric hybrid bonding. This structure helps to provide a more uniform stress distribution and additional mechanical support during bonding, and is particularly suitable for the integration of large-size cores.
[0056] After depositing and patterning the aluminum nitride bonding layer 300 in step S20, and before step S30, copper pillars are formed as metal bumps 400 with a height of approximately 5 μm on the exposed core metal electrode 111 of the mother wafer 100 through an electroplating process. Figure 7 (As shown). Similarly, similar metal bumps (not shown) can be formed on the core metal electrode 210 of the core particle 200. After alignment in subsequent bonding, the tips of these metal bumps 400 may directly contact or retain a small gap. During the chemical plating process to form the vertical interconnect structure, the metal will preferentially grow on the surface of the bumps. The presence of the bumps shortens the gap distance that needs to be bridged and provides a larger growth starting area, thus making the interconnect process faster and more reliable, which is especially beneficial for the interconnection of ultra-high density electrode arrays.
[0057] Another aspect of the present invention provides a three-dimensional system-on-a-chip based on an aluminum nitride bonding structure, manufactured using the above-described method, comprising: The mother wafer 100 has a mother core metal electrode array 111 on its surface; At least one sub-core 200 is stacked upside down on the parent wafer 100, and its surface has a sub-core metal electrode array 210. An aluminum nitride bonding layer is located between the mother wafer 100 and the sub-core 200, and is distributed outside the interconnection region of the mother core metal electrode array 111 and the sub-core metal electrode array 210, fixing the mother wafer 100 and the sub-core 200 together, and the mother core metal electrode array 111 and the sub-core metal electrode array 210 are vertically interconnected.
[0058] In one embodiment, a vertical interconnect structure 500 is also included, located between the vertically opposite electrodes of the mother core metal electrode array 111 and the daughter core metal electrode array 210, electrically connecting the two.
[0059] In one embodiment, a support metal block is also included between the mother wafer 100 and the sub-core 200, the support metal block being co-bonded with an aluminum nitride bonding layer.
[0060] In one embodiment, it further includes an aluminum nitride filling medium filling the region between the mother wafer and the sub-cores, excluding the vertical interconnect structure, and the lateral gaps between the plurality of sub-cores.
[0061] In one embodiment, metal bumps or metal pillars protruding toward each other may be formed on the metal electrodes of the first and / or sub-core metal electrode array 210.
[0062] In one embodiment, the aluminum nitride bonding layer 300 is in direct contact with and bonded to the semiconductor substrate or surface aluminum nitride passivation layer of the mother wafer 100 and the daughter core 200.
[0063] refer to Figure 6 This is a cross-sectional structural diagram of a three-dimensional system chip manufactured using the method of the present invention (e.g., in conjunction with the first and second embodiments). The chip includes: As the lower layer, the mother wafer 100 (or the reconstructed set of mother core particles) has a mother core metal electrode array 111 on its surface.
[0064] Sub-core particles 200 are stacked upside down on top of each other, and their surfaces have sub-core metal electrodes 210.
[0065] An aluminum nitride bonding layer 300 located between the mother wafer 100 and the sub-core 200 is distributed around the electrode region, providing mechanical bonding force and insulation.
[0066] The vertical interconnect structure 500, which fills the space defined by the bonding layer 300, is formed by electroless copper plating and electrically connects electrodes 111 and 210.
[0067] The aluminum nitride filling medium 310, which fills the vertical interconnect structure 500, the sub-core 200 and the sides, together with the bonding layer 300, forms a continuous, highly thermally conductive insulating package.
[0068] This structure not only achieves high-density vertical electrical interconnection, but also efficiently conducts the heat generated by the chip laterally to the edge or conducts it out through subsequent additional heat sinks using an aluminum nitride material system, fundamentally solving the heat dissipation problem of three-dimensional integration.
[0069] In summary, this invention provides a high-heat-dissipation, high-insulation, and high-reliability 3D system-on-a-chip solution by innovatively applying aluminum nitride material to the bonding and filling of 3D chips, combined with in-situ chemical plating interconnection processes after bonding. This method offers flexible processing, compatible with both wafer-level and chip-level integration, and is particularly suitable for chip integration in high-performance computing, 5G / 6G RF front-ends, artificial intelligence, and other fields with stringent requirements for power consumption, heat dissipation, and signal integrity.
[0070] The above description is merely a preferred embodiment of the present invention and does not limit the patent scope of the present invention. Any equivalent structural or procedural transformations made based on the content of the present invention's specification and drawings, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of the present invention.
[0071] The above description is merely an embodiment of this application and does not limit the patent scope of this application. Any equivalent structural or procedural transformations made using the content of this application's specification and drawings, such as the combination of technical features between embodiments, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of this application.
Claims
1. A method for manufacturing a three-dimensional system-on-a-chip based on an aluminum nitride bonding structure, characterized in that, Including the following steps: S10: Provide a mother wafer with a mother core metal electrode array on its surface; provide at least one sub-core with a sub-core metal electrode array on its surface; S20: An aluminum nitride bonding layer is formed on the surface of the mother wafer and / or the surface of the sub-core in the non-electrode interconnect region; S30: Align the sub-core with the mother wafer stack and bond them through the aluminum nitride bonding layer, so that the mother core metal electrode array and the sub-core metal electrode array are vertically interconnected.
2. The manufacturing method as described in claim 1, characterized in that, The bonding in step S30 makes the mother core metal electrode array and the daughter core metal electrode array perpendicular to each other and form an interconnection gap therebetween; Metal is selectively grown onto the surfaces of the mother core metal electrode array and the daughter core metal electrode array through the interconnection gaps until the grown metal is connected as one in the interconnection gaps to form a vertical interconnection structure.
3. The manufacturing method as described in claim 1, characterized in that, The surface of the mother wafer and / or the surface of the sub-core also has a supporting metal block, and the bonding in step S30 causes the supporting metal block and the aluminum nitride bonding layer to be mixed bonded.
4. The manufacturing method as described in claim 2, characterized in that, The sub-core and the parent wafer are stacked and aligned as follows: the sub-core is stacked upside down on the surface of the parent wafer; wherein the sub-core is located on the sub-wafer, and the parent wafer includes at least one parent core.
5. The manufacturing method as described in claim 1, characterized in that, The bonding process involves applying pressure and heating to 300°C to 900°C in a vacuum or inert atmosphere to promote the formation of a strong bond between the aluminum nitride bonding layer and the contact surface.
6. The manufacturing method as described in claim 2, characterized in that, In step S20, the method for forming the aluminum nitride bonding layer is physical vapor deposition or chemical vapor deposition, the deposition thickness is 20 nm to 20 μm, and the substrate temperature during deposition is 200°C to 500°C.
7. The manufacturing method as described in claim 2, characterized in that, After the bonding in step S30, the following steps are also included: Aluminum nitride is deposited on the exposed surface of the integral structure formed by bonding the mother wafer and the daughter core particles using a chemical vapor deposition process, so as to fill the area outside the interconnect gaps and form an aluminum nitride filling medium. The process parameters of the chemical vapor deposition include: using trimethylaluminum and ammonia as precursors, the reaction pressure is 10 Pa to 1000 Pa, and the reaction temperature is 300°C to 600°C.
8. The manufacturing method as described in claim 7, characterized in that, The aluminum nitride deposited by chemical vapor deposition simultaneously fills the lateral gaps between the multiple sub-core particles, forming a planarized aluminum nitride package surface.
9. The manufacturing method as described in claim 2, characterized in that, In step S20, before or after the formation of the aluminum nitride bonding layer, metal bumps or metal pillars are formed on the metal electrodes of the mother core metal electrode array and / or the daughter core metal electrode array.
10. The manufacturing method as described in claim 2, characterized in that, The selective metal growth process is chemical plating, and the growth metal includes one or an alloy of copper, aluminum, tungsten, molybdenum, nickel, tin, cobalt, tantalum, silver, and gold.
11. The manufacturing method as described in claim 2, characterized in that, In step S10, providing the mother wafer includes: providing a carrier substrate and fixing at least two mother cores to the carrier substrate through a temporary bonding layer; after the vertical interconnect structure is formed, the step further includes removing the temporary bonding layer and the carrier substrate.
12. A three-dimensional system-on-a-chip based on an aluminum nitride bonding structure, characterized in that, Manufactured using the method described in any one of claims 1 to 11, and comprising: The mother wafer has a mother core metal electrode array on its surface; At least one sub-core is stacked upside down on the mother wafer, and its surface has a sub-core metal electrode array; An aluminum nitride bonding layer is located between the mother wafer and the sub-core, and is distributed outside the interconnection region of the mother core metal electrode array and the sub-core metal electrode array, fixing the mother wafer and the sub-core to bond together, and the mother core metal electrode array and the sub-core metal electrode array are vertically interconnected.
13. The three-dimensional system-on-a-chip as described in claim 12, characterized in that, It also includes a vertical interconnect structure located between the vertically opposite electrodes of the mother core metal electrode array and the daughter core metal electrode array, electrically connecting the two.
14. The three-dimensional system-on-a-chip as described in claim 12, characterized in that, It also includes a support metal block located between the mother wafer and the sub-core, the support metal block being co-bonded with an aluminum nitride bonding layer.
15. The three-dimensional system-on-a-chip as described in claim 13, characterized in that, The thickness of the aluminum nitride bonding layer is 0.05 μm to 20 μm.
16. The three-dimensional system-on-a-chip as described in claim 13, characterized in that, Also includes: An aluminum nitride filling medium is used to fill the area between the mother wafer and the sub-cores, excluding the space occupied by the vertical interconnect structure, and the lateral gaps between the multiple sub-cores; the aluminum nitride filling medium is in physical contact with or integrally formed with the aluminum nitride bonding layer.
17. The three-dimensional system-on-a-chip as described in claim 13, characterized in that, Metal bumps or metal pillars protruding towards each other are formed on the metal electrodes of the mother core metal electrode array and / or daughter core metal electrode array.
18. The three-dimensional system-on-a-chip as described in claim 13, characterized in that, The vertical interconnect structure is made of a metal material formed by chemical plating, and the metal material includes one or an alloy of copper, aluminum, tungsten, molybdenum, nickel, tin, cobalt, tantalum, silver, and gold.
19. The three-dimensional system-on-a-chip as described in claim 13, characterized in that, The aluminum nitride bonding layer is distributed around the interconnection region of the mother core metal electrode array and the daughter core metal electrode array, and is insulated from the interconnection region in the vertical direction. A vertical interconnect structure, penetrating the reserved cavity in the aluminum nitride bonding layer or filling the gap defined by the aluminum nitride sidewalls, electrically connects the mother core metal electrode array and the daughter core metal electrode array accordingly.
20. The three-dimensional system-on-a-chip as described in claim 13, characterized in that, The aluminum nitride bonding layer is in direct contact with and bonded to the semiconductor substrate or surface passivation layer of the mother wafer and the daughter core, and the passivation layer is made of aluminum nitride material.