Overflow forming dynamic simulation device for OLED display glass and forming quality optimization method thereof

By designing an online dynamically adjustable overflow molding dynamic simulation device, the problem that overflow groove simulation devices in the existing technology cannot be optimized in real time has been solved. This enables precise optimization and efficient development of the overflow molding quality of OLED display glass, meeting the requirements of high resolution and thickness uniformity.

CN122365812APending Publication Date: 2026-07-10SHAANXI UNIV OF SCI & TECH +1
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202610346255.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-03-20
Publication Date
2026-07-10

AI Technical Summary

Technical Problem

Existing overflow tank simulation devices are fixed structures that cannot be dynamically adjusted online, cannot truly reflect the molding quality, and cannot optimize the overflow tank structure in real time, resulting in low experimental efficiency and high cost, making it difficult to meet the high resolution and thickness uniformity requirements of OLED display glass.

Method used

Design an online dynamically adjustable overflow molding dynamic simulation device, including an overflow pull-down mechanism, a simulated liquid cooling mechanism and a traction roller. Construct a physical model through the Reynolds number similarity criterion to realize real-time optimization of overflow groove parameters and real-time measurement and compensation of thickness deviation. Integrate a heating furnace and a cooling system to completely reproduce the overflow molding process.

Benefits of technology

It significantly improves the development efficiency of OLED display glass overflow molding process, reduces experimental costs, and enhances data reliability and molding quality, making it suitable for the research and development and process iteration of high-generation OLED display glass.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN122365812A_ABST
    Figure CN122365812A_ABST
Patent Text Reader

Abstract

This invention discloses a dynamic simulation device and a method for optimizing the molding quality of overflow forming of OLED display glass, belonging to the field of glass overflow forming process development technology. The device includes a support frame, an overflow pull-down mechanism, a simulated liquid heating furnace, a cooling mechanism, and a traction roller. The overflow pull-down mechanism is equipped with an overflow trough, which is provided with a near-end and far-end dual lifting mechanism, a far-end height adjustment component, and a material flow rate control valve. It can dynamically adjust the trough depth, far-end height, and inlet flow rate without stopping the machine for disassembly and assembly, completely replicating the entire process of overflow, cooling, and traction forming, and preparing a solid sheet. The method establishes a physical model based on the Reynolds number as a similarity criterion, and adjusts the inlet flow rate, trough depth, and far-end height in a closed loop according to the sheet thickness deviation to quickly correct the thickness uniformity. The parameters can be proportionally converted to the industrial prototype, improving process development efficiency, reducing costs, and compensating for the deviation between numerical simulation and actual production, providing reliable support for the optimization of OLED display glass overflow forming process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the technical field of glass overflow molding process development, and relates to a dynamic simulation device for glass overflow molding, specifically a dynamic simulation device for OLED display glass overflow molding and its molding quality optimization method. Background Technology

[0002] As OLED display technology advances towards higher resolution, narrower bezels, and greater flexibility, display glass, as a key substrate, faces higher demands regarding thickness uniformity, surface ripples, stress levels, inclusions and bubble defects, and edge quality. The overflow pull-down method is a crucial forming process for producing high-quality display glass. It involves molten glass forming a stable free surface within an overflow channel, which then overflows and converges at the weir, forming a continuous glass ribbon under gravity and traction. This process offers advantages such as non-contact forming of the surface, high surface quality, and suitability for forming ultra-thin and large-size glass.

[0003] The overflow pull-down process involves complex multiphysics behaviors such as free surface flow of high-temperature viscous fluid, temperature-viscosity field coupling, surface tension effects, and shear-tensile deformation in the overflow confluence zone. The forming quality is highly sensitive to the structural parameters and process conditions of the overflow channel. To reduce trial-and-error costs and shorten process development cycles, existing technologies often employ numerical simulation to predict the internal and external flow and forming processes of the overflow channel. Through geometric modeling, boundary condition setting, and material property assignment, the impact of structural parameters and operating condition changes on the free surface, flow field, and defect sensitivity is assessed for scheme selection and structural optimization. However, numerical simulation has limitations such as model simplification and assumption bias, and simulation results are prone to deviating from actual operating conditions, requiring verification and correction through physical simulation.

[0004] Traditional overflow channel physical simulation devices have significant drawbacks: First, the overflow channel is a fixed structure, and adjusting parameters requires stopping the machine to disassemble and replace parts, which disrupts the continuity of the flow field, introduces start-stop disturbances, and results in low experimental efficiency and high cost; second, some devices only simulate the process of fluid flowing through the overflow brick without a cooling and solidification system, making it impossible to form solid plates and accurately reflect the uniformity of the forming thickness; third, they lack online dynamic adjustment and real-time feedback mechanisms, making it impossible to quickly iterate and optimize the overflow channel structure based on the forming quality.

[0005] Existing patent CN110174256A uses a fixed overflow brick structure with no dynamic adjustment function. It uses silicone oil as the simulation liquid, which cannot be cured and molded, and therefore cannot characterize the molding quality of the sheet. Patent CN121118729A focuses on the verification of physical models through numerical simulation. The overflow channel is a static structure, and its parameters cannot be adjusted online, making it difficult to guide real-time optimization of the overflow channel structure. Therefore, there is an urgent need to develop a simulation device and method that can be dynamically adjusted online, completely reproduce the entire overflow-molding process, and provide real-time feedback optimization to improve the development efficiency and reliability of OLED display glass overflow molding process. Summary of the Invention

[0006] The purpose of this invention is to provide a dynamic simulation device for overflow molding of OLED display glass and a method for optimizing its molding quality. By realizing the physical simulation of the entire overflow molding process of OLED display glass, the overflow molding process can be completely reproduced. It can directly mold the sheet material and measure the thickness deviation in real time, adjust the overflow groove structural parameters online, and quickly compensate and correct the thickness uniformity. This significantly improves the efficiency of process development, reduces experimental costs, and improves data reliability, providing precise support for overflow groove structure design and molding quality optimization.

[0007] This invention is achieved through the following technical solution: An overflow molding dynamic simulation device for OLED display glass includes a support frame, on which an overflow pull-down mechanism is provided; The overflow pull-down mechanism is connected to the simulated liquid heating furnace via a feeding pipe at its near end. The lower part of the overflow pull-down mechanism is equipped with a simulated liquid cooling mechanism, and multiple sets of traction rollers are symmetrically arranged on both sides of the lower part of the simulated liquid cooling mechanism. The overflow pull-down mechanism, the simulated liquid cooling mechanism, and the traction roller are all supported by support components respectively located at the near and far ends of the support frame; The overflow pull-down mechanism includes a cover that is snapped into the support frame, and an overflow groove is fixedly provided inside the cover. The overflow pull-down mechanism is provided with an overflow groove height adjustment component at its distal end; The overflow trough includes two vertically parallel side plates, each with an end plate at both ends. The bottom of the side plates is fixedly connected by a horizontal plate. The bottom of the horizontal plate has two extension plates whose top edges are smoothly connected to the side plates and whose bottom edges abut against the side plates. The upper part of the horizontal plate is provided with a set of lifting mechanisms near the near end and the far end, respectively. The top of the lifting mechanism is provided with an overflow trough bottom plate that seals against the side plate and the end plate.

[0008] The present invention also has the following technical features: Preferably, the height adjustment assembly includes any one of a lead screw and nut assembly, an eccentric wheel assembly, or a spring-loaded screw assembly.

[0009] Preferably, the overflow trough is fixedly connected to the cover body via connecting plates at both ends, and a gap is provided between the cover body and the side plate of the overflow trough.

[0010] Preferably, the lifting mechanism includes any one of an electric push rod, a scissor jack, or a scissor lifting support.

[0011] Preferably, the side plate of the overflow channel is configured as a trapezoid with a near-end height greater than the far-end height.

[0012] Preferably, the feeding pipeline is equipped with a feeding flow rate control valve.

[0013] Preferably, a sealing ring is provided on the outer periphery of the overflow trough bottom plate.

[0014] This invention also protects a method for optimizing the molding quality of OLED display glass based on the above-described dynamic simulation device for overflow molding of OLED display glass, comprising the following steps: Step 1: Based on the structural parameters of the overflow tank obtained from numerical simulation, and using the Reynolds number as the similarity criterion, establish a physical model of the overflow tank and determine the target viscosity of the simulated liquid; Step 2: Heat and maintain the temperature of the simulated liquid to stabilize it within the preset range; and ensure that the simulated liquid enters the overflow tank at the preset inlet speed by adjusting the feed flow rate control valve. Step 3: Cool the simulated liquid using a cooling device and then pull it into shape; Step 4: After the overflow condition stabilizes, measure the thickness of the molded sheet and calculate the thickness deviation Δh between the near end and the far end. Step 5: Adjust the structural parameters of the overflow channel based on the measurement results; Step 6: After each adjustment, keep the overflow trough running and wait for the preset stabilization time t. After the flow field returns to stability, repeat step 4 to obtain a new thickness deviation value. If Δh is still greater than Δh0, continue adjusting until Δh≤Δh0, confirm that the optimization target has been achieved, and end the adjustment process. Step 7: Based on the proportional relationship between the physical model and the overflow pull-down mechanism, convert the structural parameter adjustment amount to the prototype scale.

[0015] Preferably, the method for adjusting the structural parameters of the overflow channel in step five is to gradually adjust one or more parameters among the simulated liquid inlet velocity, the near end depth, the far end depth, and the far end height of the overflow channel when there is a deviation in the thickness of the sample at the near end and the far end. This is done to compensate for and correct the local thickness of the sample.

[0016] Furthermore, the method for adjusting the structural parameters of the overflow channel described in step five includes: When the measured sample has a high proximal molding thickness and a low distal molding thickness, reduce the inlet velocity of the simulated liquid to reduce the proximal overflow; reduce the distal height of the overflow trough to increase the distal overflow; and reduce the height of the bottom plate of the proximal overflow trough to increase the inlet depth. When the measured sample has a low proximal molding thickness and a high distal molding thickness, increase the inlet velocity of the simulated liquid to increase the flow rate of the simulated liquid; increase the distal height of the overflow tank to increase the proximal overflow; and increase the height of the bottom plate of the proximal overflow tank to reduce the inlet tank depth.

[0017] Compared with the prior art, the present invention has the following beneficial effects: The overflow molding dynamic simulation device for OLED display glass of the present invention achieves online dynamic adjustment of key parameters such as groove depth, far-end height, and inlet flow velocity through the coordinated configuration of a dual-zone lifting mechanism at the near and far ends of the overflow groove, a far-end height adjustment component, and a flow control valve. This eliminates the need for machine shutdown, disassembly, or component replacement, and allows for multi-parameter iterative optimization under continuous and stable flow field conditions. It effectively eliminates start-up and shutdown disturbances and disassembly / reassembly errors, significantly improving simulation experiment efficiency and data consistency. The device integrates a heating furnace, cooling mechanism, and traction rollers, completely replicating the entire process of overflow, cooling, curing, and traction molding. It can prepare solid plates and measure the near and far-end thicknesses in real time, accurately reflecting molding quality and thickness uniformity, thus overcoming the shortcomings of traditional simulations that cannot form or characterize actual plate shapes. This invention constructs a physical model using Reynolds number as a similarity criterion. Based on thickness deviation, it adjusts the inlet velocity, near-end groove depth, far-end groove depth, and far-end height in real-time using a closed-loop system to precisely compensate for and correct the thickness deviation, quickly controlling it within the target threshold. This achieves visualized and quantifiable optimization of molding quality. The adjusted parameters can be directly converted to industrial prototype scale, providing reliable experimental basis for overflow groove structure design and process parameter tuning, effectively bridging the gap between numerical simulation and actual production. It significantly shortens the development cycle of OLED glass overflow molding technology, reduces mold processing, repeated assembly, and material consumption costs, and improves the molding stability and surface quality of ultra-thin large-size display glass. It is suitable for the research and development and process iteration of high-generation OLED display glass overflow molding technology. Attached Figure Description

[0018] Figure 1 A schematic diagram of the overall structure of the overflow method molding dynamic simulation device for the invention; Figure 2 This is a schematic diagram of the longitudinal section of the overflow channel; Figure 3 This is a schematic diagram of the vertical cross-section of the overflow channel; The meanings of the markings in the diagram are as follows: 1-support frame, 2-feeding pipe, 3-simulated liquid heating furnace, 4-simulated liquid cooling mechanism, 5-traction roller, 6-support assembly, 7-cover, 8-overflow trough, 801-side plate, 802-horizontal plate, 803-lifting mechanism, 804-overflow trough bottom plate, 805-sealing ring, 806-end plate, 807-extension plate, 9-feeding flow rate control valve. Detailed Implementation

[0019] The present invention will be further described in detail below with reference to specific embodiments. These descriptions are for explanation purposes only and are not intended to limit the scope of the invention.

[0020] refer to Figure 1As shown, this embodiment provides a dynamic simulation device for overflow molding of OLED display glass, including a support frame 1, on which an overflow pull-down mechanism is provided; The near end of the overflow pull-down mechanism is connected to the simulated liquid heating furnace 3 through the feeding pipe 2. The feeding pipe 2 is equipped with a feeding flow rate control valve 9. The lower part of the overflow pull-down mechanism is equipped with a simulated liquid cooling mechanism 4. Multiple sets of traction rollers 5 are symmetrically arranged on both sides of the lower part of the simulated liquid cooling mechanism 4. The traction rollers 5 are arranged opposite to each other on both sides of the support frame 1, and are set to 2 or 3 sets according to the target thickness of the sample assembly. The overflow pull-down mechanism, the simulated liquid cooling mechanism 4, and the traction roller 5 are all supported by support components 6 respectively located at the near end and far end of the support frame 1; The overflow pull-down mechanism includes a cover 7 that is snapped into the support frame 1. An overflow groove 8 is fixedly installed inside the cover 7. The overflow groove 8 is fixedly connected to the cover 7 through connecting plates at both ends. A gap is provided between the side plates 801 of the cover 7 and the overflow groove 8. The cover 7 is connected on all four sides and open at the top and bottom. like Figure 2 and Figure 3 As shown, the distal end of the overflow pull-down mechanism is equipped with an overflow groove 8 height adjustment assembly; the height adjustment assembly includes any one of a screw and nut assembly, an eccentric wheel assembly, or a spring set screw assembly; the height adjustment assembly is used to adjust the height of the distal end of the overflow groove 8. A scale for recording the adjustment range is provided on the height adjustment assembly. The side plate 801 of the overflow groove 8 is configured as a trapezoid with a proximal height greater than the distal height.

[0021] The overflow tank 8 includes two vertically parallel side plates 801, with end plates 806 at each end. The bottom of the side plates 801 is fixedly connected by a horizontal plate 802. The bottom of the horizontal plate 802 has two extension plates 807, whose top edges are smoothly connected to the side plates 802 and whose bottom edges abut against the side plates 802. A set of lifting mechanisms 803 is provided on the upper part of the horizontal plate 802 near the proximal and distal ends, respectively. The top of the lifting mechanism 803 is provided with an overflow tank bottom plate 804 that seals against the side plates 801 and the end plates. The inner cavity formed by the side plates 801, end plates 806, and overflow tank bottom plate 804 is used to simulate the formation of an overflow liquid surface. The horizontal plate 802 is used to support the lifting mechanism 803. The extension plates 807 are used to guide the overflowing simulated liquid. The vertical cross-section of the two opposing extension plates 807 is conical.

[0022] The lifting mechanism 803 includes any one of an electric push rod, a scissor jack, or a scissor lifting support. Lifting mechanisms located at the near and far ends are used to adjust the near and far depths of the overflow trough 8, respectively. The overflow trough bottom plate 804 slides along the side wall of the cavity formed by the side plate 801, the end plate 806, and the overflow trough bottom plate 804 under the push of the lifting mechanism 803. A sealing ring 805 is provided on the outer periphery of the overflow trough bottom plate 804. When the overflow trough bottom plate 804 slides up and down, the sealing ring 805 maintains the seal between the overflow trough bottom plate 804 and the four walls.

[0023] An OLED display glass molding quality optimization method based on an overflow molding dynamic simulation device for OLED display glass includes the following steps: Step 1: Based on the structural parameters of overflow tank 8 obtained from numerical simulation, and using the Reynolds number as the similarity criterion, establish the physical model of overflow tank 8 and determine the target viscosity of the simulated liquid; Step 2: Heat and maintain the temperature of the simulated liquid to stabilize it within the preset range; and ensure that the simulated liquid enters the overflow tank 8 at the preset inlet speed by adjusting the feed flow rate control valve 9. Step 3: Cool the simulated liquid using a cooling device and then pull it into shape; Step 4: After the overflow condition stabilizes, measure the thickness of the molded sheet and calculate the thickness deviation Δh between the near end and the far end. Step 5: Adjust the structural parameters of overflow tank 8 according to the measurement results. The method for adjusting the structural parameters of overflow tank 8 is to gradually adjust one or more parameters of the near end depth, far end depth, and far end height of the simulated liquid inlet velocity when there is a deviation in the molding thickness of the sample. This will compensate for and correct the local thickness of the sample. When the measured sample has a high proximal molding thickness and a low distal molding thickness, reduce the inlet velocity of the simulated liquid to reduce the proximal overflow; reduce the distal height of the overflow trough 8 to increase the distal overflow; and reduce the height of the bottom plate 804 of the proximal overflow trough to increase the inlet depth. When the measured sample has a low proximal molding thickness and a high distal molding thickness, the inlet velocity of the simulated liquid is increased to increase the flow rate of the simulated liquid; the distal height of the overflow tank 8 is increased to increase the proximal overflow; and the height of the bottom plate 804 of the proximal overflow tank is increased to reduce the inlet tank depth.

[0024] Step 6: After each adjustment, keep the overflow trough 8 running and wait for the preset stabilization time t. After the flow field returns to stability, repeat step 4 to obtain a new thickness deviation value. If Δh is still greater than Δh0, continue adjusting until Δh≤Δh0, confirm that the optimization target has been achieved, and end the adjustment process. Step 7: Based on the proportional relationship between the physical model and the overflow pull-down mechanism, convert the structural parameter adjustment amount to the prototype scale.

[0025] The following is a specific example of an OLED display glass forming quality optimization method based on an overflow forming dynamic simulation device for OLED display glass, including the following steps: Step 1: Determine the basic structural dimensions of the physical simulation using the overflow structure from the numerical simulation, as shown in the table below: The viscosity of the simulated liquid entering overflow tank 8 in the physical model was determined to be 116 Pa·s using Reynolds number as the similarity criterion. To meet this viscosity requirement, the proportions of a mixture of high-molecular-weight organic compounds such as ethylene-vinyl acetate copolymer, petroleum resin, and dibutyl phthalate were adjusted to achieve a viscosity of 116 Pa·s at 120°C for subsequent physical simulations. Step 2: Start the simulated liquid heating furnace 3 and heat and keep the simulated liquid at a constant temperature. Adjust the temperature control to keep the temperature of the simulated liquid stable at 120℃±2℃ when it flows into the L pipe, so as to ensure viscosity stability and reduce the impact of flow fluctuations on the overflow state. Step 3: By adjusting the opening of the feed flow rate control valve 9 in the feed pipe 2, control the inlet velocity of the simulated liquid entering the overflow tank 8 to be 0.0016 m / s; continue feeding until the simulated liquid can continuously and evenly cover the entire overflow surface and form a stable overflow liquid film. Step 4: Turn on the cooling device to cool the simulated liquid flowing down from the overflow tank 8, so that it forms a continuous plate downstream and gradually hardens, so as to carry out thickness measurement and feedback adjustment. Step 5: After the simulated liquid solidifies into a board, use traction roller 5 to clamp the board and pull it out. Adjust the traction speed of traction roller 5 to 0.12 m / s to make the board pulling process continuous and stable, and reduce the disturbance of traction fluctuations on the board thickness distribution. Step Six: Under the same sheet-forming conditions, measure the sheet thickness along the width direction at the same height position at both the near and far ends; the initial measurement results are as follows: The thickness of the proximal plate is 0.92 mm; The thickness of the distal plate is 1.11 mm; This indicates that the thickness of the plate is too low at the near end and too high at the far end, resulting in uneven thickness distribution. The height of the overflow trough at the far end of the device was adjusted online using the overflow trough height adjustment component: the height of the far end was raised to 1 cm; keeping other operating parameters unchanged, the plate thickness was remeasured after the flow field stabilized for 5 minutes. The thickness of the proximal plate was increased to 1.08 mm; The thickness of the far end plate was reduced to 0.98 mm; This indicates that distal elevation can significantly improve the problem of proximal thinning, but a trend of proximal thickening and distal thinning appears; To further align the thickness of the near and far ends of the overflow trough, the height of the near-end bottom surface of the overflow trough was lowered by 1 mm using the lifting mechanism 803 of the overflow trough 8. Maintaining the same operating conditions, measurements were taken again after the flow field stabilized for 5 minutes. The thickness of the proximal plate is 1.01 mm; The thickness of the distal plate is 1.02 mm; At this point, the plate thickness distribution meets the uniformity requirement, thus achieving the objective. The above process enables rapid feedback optimization of flow and forming results using the overflow channel height adjustment component and lifting mechanism 803 without interrupting the flow, thereby compensating for deviations caused by numerical simulation simplification and actual fluctuations. Step 7: Restore the physical simulation dimensions to the original dimensions; The above are preferred embodiments of the present invention. Any changes made to the technical solution of the present invention that do not exceed the scope of the technical solution of the present invention shall fall within the protection scope of the present invention.

Claims

1. A dynamic simulation device for overflow molding of OLED display glass, characterized in that, Includes a support frame (1), on which an overflow pull-down mechanism is provided; The near end of the overflow pull-down mechanism is connected to the simulated liquid heating furnace (3) through the feeding pipe (2). The lower part of the overflow pull-down mechanism is provided with a simulated liquid cooling mechanism (4). Multiple sets of traction rollers (5) are symmetrically arranged on both sides of the lower part of the simulated liquid cooling mechanism (4). The overflow pull-down mechanism, the simulated liquid cooling mechanism (4) and the traction roller (5) are all supported by support components (6) respectively set at the near end and far end of the support frame (1); The overflow pull-down mechanism includes a cover (7) that is snapped into the support frame (1), and an overflow groove (8) is fixedly provided inside the cover (7). The overflow pull-down mechanism is provided with an overflow groove (8) height adjustment component at its far end; The overflow trough (8) includes two vertically parallel side plates (801), and end plates (806) are respectively provided at both ends of the side plates (801). The bottom end of the side plates (801) is fixedly connected by a horizontal plate (802). The bottom of the horizontal plate (802) is provided with two extension plates (807) whose top edges are smoothly connected to the side plates (802) and whose bottom edges abut against each other. The upper part of the horizontal plate (802) is provided with a set of lifting mechanisms (803) near the near end and the far end respectively. The top of the lifting mechanism (803) is provided with an overflow trough bottom plate (804) that seals against the side plate (801) and the end plate.

2. The overflow molding dynamic simulation device for OLED display glass according to claim 1, characterized in that, The height adjustment assembly includes any one of a lead screw and nut assembly, an eccentric wheel assembly, or a spring set screw assembly.

3. The overflow molding dynamic simulation device for OLED display glass according to claim 1, characterized in that, The overflow trough (8) is fixedly connected to the cover (7) by connecting plates at both ends, and a gap is provided between the cover (7) and the side plate (801) of the overflow trough (8).

4. The overflow molding dynamic simulation device for OLED display glass according to claim 1, characterized in that, The lifting mechanism (803) includes any one of an electric push rod, a scissor jack, or a scissor lifting support.

5. The overflow molding dynamic simulation device for OLED display glass according to claim 1, characterized in that, The side plate (801) of the overflow trough (8) is set as a trapezoid with a near end height greater than the far end height.

6. The overflow molding dynamic simulation device for OLED display glass according to claim 1, characterized in that, The feed pipe (2) is equipped with a feed flow rate control valve (9).

7. The overflow molding dynamic simulation device for OLED display glass according to claim 1, characterized in that, A sealing ring (805) is provided on the outer periphery of the overflow trough bottom plate (804).

8. A method for optimizing the molding quality of OLED display glass based on the overflow molding dynamic simulation apparatus for OLED display glass according to any one of claims 1 to 7, characterized in that, Includes the following steps: Step 1: Based on the structural parameters of the overflow tank (8) obtained by numerical simulation, establish the physical model of the overflow tank (8) and determine the target viscosity of the simulated liquid by using the Reynolds number as the similarity criterion; Step 2: Heat and keep the simulated liquid at a temperature that is within a preset range; and ensure that the simulated liquid enters the overflow tank (8) at a preset inlet speed by adjusting the feed flow rate control valve (9). Step 3: Cool the simulated liquid using a cooling device and then pull it into shape; Step 4: After the overflow condition stabilizes, measure the thickness of the molded sheet and calculate the thickness deviation Δh between the near end and the far end. Step 5: Adjust the structural parameters of the overflow trough (8) according to the measurement results; Step 6: After each adjustment, keep the overflow trough (8) running and wait for the preset stabilization time t. After the flow field returns to stability, repeat step 4 to obtain a new thickness deviation value. If Δh is still greater than Δh0, continue to adjust until Δh≤Δh0, confirm that the optimization target has been achieved and end the adjustment process. Step 7: Based on the proportional relationship between the physical model and the overflow pull-down mechanism, convert the structural parameter adjustment amount to the prototype scale.

9. The method for optimizing the molding quality of OLED display glass according to claim 8, characterized in that, The method for adjusting the structural parameters of the overflow trough (8) in step five is to gradually adjust the simulated liquid inlet velocity, one or more parameters of the near end depth, far end depth, and far end height of the overflow trough (8) when there is a deviation in the near end and far end forming thickness of the sample, and to compensate and correct the local thickness of the sample.

10. The method for optimizing the molding quality of OLED display glass according to claim 9, characterized in that, The method for adjusting the structural parameters of the overflow trough (8) described in step five includes: When the measured sample has a high proximal molding thickness and a low distal molding thickness, reduce the inlet velocity of the simulated liquid to reduce the proximal overflow; reduce the distal height of the overflow trough (8) to increase the distal overflow; reduce the height of the bottom plate (804) of the proximal overflow trough to increase the inlet trough depth. When the near-end forming thickness of the sample is too low and the far-end forming thickness is too high, increase the inlet velocity of the simulated liquid to increase the flow rate of the simulated liquid; increase the height of the far end of the overflow tank (8) to increase the near-end overflow amount; increase the height of the bottom plate (804) of the near-end overflow tank to reduce the inlet tank depth.

Citation Information

Patent Citations

  • Overflow brick mold flow testing device

    CN110174256A

  • Physical model for OLED display glass overflow method forming numerical simulation and building method and verification system thereof