Secondary battery
The integration of a vent member with a lower melting point resin in the sealing extension of secondary batteries directs gas discharge away from electrode leads, addressing the challenge of uncontrolled gas release and enhancing safety during thermal runaway.
Patent Information
- Application Number
- JP2023527110
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2022-01-04
- Filing Date
- 2022-04-15
- Publication Date
- 2024-10-28
- Estimated Expiration
- 2042-04-15
AI Technical Summary
Conventional secondary batteries face challenges in directing gas discharge during thermal runaway, leading to potential damage from uncontrolled gas release.
Incorporation of a vent member with a vent resin having a lower melting point than the sealant resin, positioned in the extension of the sealing part to guide gas discharge in a specific direction, minimizing contact with electrode leads.
Enhances safety by ensuring controlled gas discharge away from electrode leads, reducing the risk of damage and improving overall battery safety during thermal events.
Smart Images

Figure 0007574439000001 
Figure 0007574439000002 
Figure 0007574439000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a secondary battery, and more particularly to a secondary battery provided with a vent member.
[0002] This application claims priority to Korean Patent Application No. 10-2021-0049400 filed on April 15, 2021, and Korean Patent Application No. 10-2022-0001216 filed on January 4, 2022, the entire contents of which are incorporated herein by reference in their entirety in the specification and drawings. [Background technology]
[0003] Secondary batteries can be applied to a variety of products and have excellent electrical properties such as high energy density. Secondary batteries are used not only in portable devices but also in electric vehicles (EVs) and hybrid electric vehicles (HEVs) that run on electricity. Secondary batteries can significantly reduce the use of fossil fuels and are environmentally friendly as they do not produce by-products during the energy consumption process, and they are attracting attention as a new energy source for improving energy efficiency.
[0004] Currently, widely used secondary batteries include lithium ion batteries, lithium polymer batteries, nickel-cadmium batteries, nickel-metal hydride batteries, and nickel-zinc batteries.
[0005] A secondary battery generally has a structure in which an electrode assembly including at least one unit cell having a positive electrode / separator / negative electrode structure is housed in a battery case made of a laminate sheet in which an outer layer, a metal barrier layer, and a sealant layer are laminated in that order, and the electrode assembly is sealed by welding a sealant resin in the sealant layer.
[0006] In conventional secondary batteries, the battery may catch fire due to various reasons such as an internal short circuit, overcharging or over-discharging, temperature regulation, etc. In this case, the internal temperature of the secondary battery may rise rapidly and a thermal propagation phenomenon may occur in which heat is transferred to adjacent cells, causing the fire to become even more severe.
[0007] When a thermal runaway phenomenon occurs, i.e., when the internal temperature of a secondary battery rises, a directional venting characteristic that exhausts gas in one direction is required to minimize damage to the electrodes caused by gas. However, conventional secondary batteries have a problem in that it is difficult to induce gas exhaust in a specific direction.
[0008] Therefore, an object of the present invention is to provide a secondary battery having improved safety by directing gas discharge in a specific direction. Summary of the Invention [Problem to be solved by the invention]
[0009] A particular object of the present invention is to provide a secondary battery with improved safety by making it possible to induce gas discharge in a specific direction. [Means for solving the problem]
[0010] In order to achieve the above object, according to one aspect of the present invention, there is provided a secondary battery according to the following embodiment.
[0011] The first embodiment is An electrode assembly; an electrode lead attached to the electrode assembly; a case including a sealing portion formed to seal the electrode assembly and a housing portion partitioned by a bent surface and the sealing portion and housing the electrode assembly therein; a vent member including a vent resin having a melting point lower than that of the sealant resin; the sealing portion includes an extension adjacent to and extending from the bending surface; The vent member is at least partially located in the extension.
[0012] The second embodiment is the same as the first embodiment, The vent member may be located at least partially in a bat ear region.
[0013] The third embodiment is the first or second embodiment, The electrode lead may further include a lead film surrounding an outer surface of the electrode lead and interposed between the electrode lead and the sealing portion, wherein the vent member extends through the storage portion, a first end of the vent member is separated from the lead film at the sealing portion, and a second end of the vent member may at least partially overlap or contact the lead film at the storage portion.
[0014] A fourth embodiment is any one of the first to third embodiments, The case may further include a lead film surrounding an outer surface of the electrode lead and interposed between the electrode lead and the sealing portion, the electrode lead extending from the case along a Y-axis, the vent member including a first portion and a second portion, the first portion extending along an X-axis perpendicular to the Y-axis between the lead film and the second portion, and the second portion extending along the Y-axis.
[0015] A fifth embodiment is any one of the first to third embodiments, The case may further include a lead film surrounding an outer surface of the electrode lead and interposed between the electrode lead and the sealing portion, the electrode lead extending from the case along a Y axis, the vent member including a first portion and a second portion, the first portion extending between the lead film and the second portion along a first direction not parallel to the Y axis, and the second portion extending along a second direction perpendicular to the first direction.
[0016] The sixth embodiment is the fourth or fifth embodiment, The vent member may be L-shaped.
[0017] The seventh embodiment is the fourth or fifth embodiment, The vent member may include a tapering section at an intersection of the first and second portions, the tapering section extending into the recess.
[0018] The eighth embodiment is any one of the fourth to seventh embodiments, The first portion can be a bridge portion that at least partially overlaps the lead film.
[0019] The ninth embodiment is any one of the fourth to eighth embodiments, An outer end of the first portion may be spaced from an inner end of the extension portion, and the first portion may be located in the recess.
[0020] A tenth embodiment is any one of the fourth to ninth embodiments, The second portion may not overlap or contact the lead film.
[0021] An eleventh embodiment is any one of the first to tenth embodiments, The vent member may taper in width along a vent direction.
[0022] A twelfth embodiment is any one of the first to eleventh embodiments, The vent member may have any one of a circular shape, an elliptical shape, a stepped shape, a triangular shape, and a trapezoidal shape.
[0023] A thirteenth embodiment is any one of the first to twelfth embodiments, The vent member may have a decreasing thickness along the vent direction.
[0024] A fourteenth embodiment is any one of the third to thirteenth embodiments, The area where the vent member overlaps or contacts the lead film may be 1% to 30% of the area where the lead film does not overlap or contact the electrode lead.
[0025] A fifteenth embodiment is any one of the first to fourteenth embodiments, The vent resin may include a linear low density polyethylene having a comonomer having six or more carbon atoms.
[0026] A sixteenth embodiment is any one of the first to fifteenth embodiments, The vent member may melt at 100° C. to 120° C. to vent gas from the storage portion to the outside of the secondary battery.
[0027] The seventeenth embodiment is the sixteenth embodiment, The vent member is capable of venting gas from the storage portion when the pressure in the storage portion is 1.5 atm or greater.
[0028] The eighteenth embodiment is any one of the first to seventeenth embodiments, The vent member may have a maximum sealing strength of less than 6 kgf / 15 mm at 100° C. or higher.
[0029] A 19th embodiment is any one of the 1st to 18th embodiments, The vent member may have an average sealing strength of less than 4.5 kgf / 15 mm at 100° C. or higher.
[0030] A twentieth embodiment is any one of the first to nineteenth embodiments, The vent member may have a maximum sealing strength at room temperature to 60°C of 6 kgf / 15 mm or more.
[0031] A twenty-first embodiment is any one of the first to twentieth embodiments, The vent member may have an average sealing strength at room temperature to 60°C of 4.5 kgf / 15 mm or more.
[0032] A twenty-second embodiment is any one of the first to twenty-first embodiments, The vent resin may be polymerized in the presence of a metallocene catalyst.
[0033] The 23rd embodiment is any one of the 15th to 22nd embodiments, The content of the comonomer having 6 or more carbon atoms may be 15% by weight or less, based on 100% by weight of the linear low-density polyethylene having a comonomer having 6 or more carbon atoms.
[0034] A twenty-fourth embodiment is any one of the first to twenty-third embodiments, The vent resin may have a polydispersity index (PDI) of 4 or less.
[0035] A twenty-fifth embodiment is any one of the first to twenty-fourth embodiments, The difference between the crystallization temperature of the sealant resin and the crystallization temperature of the vent resin may be 10° C. or less.
[0036] A 26th embodiment is any one of the first to 25th embodiments, The vent resin may have a melting point of 100°C to 130°C.
[0037] A 27th embodiment is any one of the first to 26th embodiments, The vent resin may have a weight average molecular weight of 100,000 g / mol to 400,000 g / mol.
[0038] A 28th embodiment is any one of the first to 27th embodiments, The secondary battery may be a pouch-type secondary battery.
[0039] A 29th embodiment is any one of the 1st to 28th embodiments, The vent member may have a maximum sealing strength of less than 3 kgf / 15 mm at 120° C. or higher.
[0040] A 30th embodiment is any one of the first to 29th embodiments, The vent member may have an average sealing strength of less than 2 kgf / 15 mm at 120° C. or higher. Effect of the Invention
[0041] A secondary battery according to one embodiment of the present invention has a vent member including a vent resin having a lower melting point than the sealant resin in an extension of a sealing portion, which enables gas to be guided to be discharged to the extension, thereby improving safety.
[0042] The following drawings attached to this specification illustrate preferred embodiments of the present invention and, together with the detailed description of the invention, serve to further understand the technical ideas of the present invention. Therefore, the present invention should not be interpreted as being limited to only the matters described in the drawings. [Brief description of the drawings]
[0043] [Figure 1] 1 is a plan view of a secondary battery according to an embodiment of the present invention; [Diagram 2] FIG. 2 is a schematic diagram illustrating the formation of a vent in a secondary battery according to an embodiment of the present invention. [Diagram 3] FIG. 4 is a partial plan view of a secondary battery according to still another embodiment of the present invention. [Figure 4] 11 is a partial plan view of an electrode lead and a vent member of a secondary battery according to still another embodiment of the present invention. FIG. [Diagram 5] 11 is a partial plan view of an electrode lead and a vent member of a secondary battery according to still another embodiment of the present invention. FIG. [Figure 6] 11 is a partial plan view of an electrode lead and a vent member of a secondary battery according to still another embodiment of the present invention. FIG. [Figure 7a] 2 is a cross-sectional view of the vent member of FIG. 1 according to one embodiment of the present invention. [Figure 7b] 2 is a cross-sectional view of the vent member of FIG. 1 according to yet another embodiment of the present invention. [Figure 8]11 is a partial plan view of an electrode lead and a vent member of a secondary battery according to still another embodiment of the present invention. FIG. [Figure 9] 11 is a partial plan view of an electrode lead and a vent member of a secondary battery according to still another embodiment of the present invention. FIG. [Figure 10] 11 is a partial plan view of an electrode lead and a vent member of a secondary battery according to still another embodiment of the present invention. FIG. [Figure 11] 11 is a partial plan view of an electrode lead and a vent member of a secondary battery according to still another embodiment of the present invention. FIG. [Figure 12] 11 is a partial plan view of an electrode lead and a vent member of a secondary battery according to still another embodiment of the present invention. FIG. [Figure 13] 11 is a partial plan view of an electrode lead and a vent member of a secondary battery according to still another embodiment of the present invention. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0044] Hereinafter, a preferred embodiment of the present invention will be described in detail with reference to the attached drawings. Prior to this, the terms and words used in the specification and claims should not be interpreted as being limited to their ordinary or dictionary meanings, but should be interpreted as having meanings and concepts according to the technical ideas of the present invention, in accordance with the principle that the inventor himself can appropriately define the concepts of terms in order to best describe the invention.
[0045] Therefore, it should be understood that the embodiments described in this specification and the configurations shown in the drawings are merely the most preferred embodiment of the present invention and do not represent the entire technical idea of the present invention, and that there may be various equivalents and modifications that can be substituted for them at the time of this application.
[0046] According to one embodiment of the present invention, there is provided a secondary battery comprising: an electrode assembly having an electrode lead attached thereto; a case including a housing for housing the electrode assembly and a sealing portion including a sealant resin and formed to seal the electrode assembly; and a lead film formed to surround a portion of an outer surface of the electrode lead and interposed between the electrode lead and the sealing portion of the case, the sealing portion including an extension portion, and a vent member including a vent resin having a lower melting point than the sealant resin included in the extension portion.
[0047] 1 shows a secondary battery according to an embodiment of the present invention. Referring to FIG. 1, a secondary battery 10 according to an embodiment of the present invention includes an electrode assembly 12 to which an electrode lead 11 is attached, and a case 13.
[0048] The electrode assembly 12 includes a positive electrode plate, a negative electrode plate, and a separator. In the electrode assembly 12, the positive electrode plate and the negative electrode plate may be stacked in order with the separator interposed therebetween.
[0049] The positive electrode plate may include a positive electrode current collector made of a metal thin plate having excellent conductivity, for example, aluminum (Al) foil, and a positive electrode active material layer coated on at least one surface of the positive electrode current collector. The positive electrode plate may also include a positive electrode tab made of a metal material, for example, aluminum material, at one end of the positive electrode plate. The positive electrode tab may protrude from one end of the positive electrode plate. The positive electrode tab may be welded to one end of the positive electrode plate or bonded using a conductive adhesive.
[0050] The negative electrode plate may include a negative electrode current collector made of a conductive metal thin plate, for example, copper (Cu) foil, and a negative electrode active material layer coated on at least one surface of the negative electrode current collector. The negative electrode plate may also include a negative electrode tab formed of a metal material, for example, copper or nickel (Ni), at one end. The negative electrode tab may protrude from one end of the negative electrode plate. The negative electrode tab may be welded to one end of the negative electrode plate or attached using a conductive adhesive.
[0051] The separator may be a porous membrane that is located between the positive and negative electrode plates, electrically insulates the positive and negative electrode plates from each other, and allows lithium ions to pass between the positive and negative electrode plates. The separator may include a porous membrane using, for example, polyethylene (PE), polypropylene (PP), or a composite film thereof.
[0052] An inorganic coating layer may be provided on the surface of the separator. The inorganic coating layer may have a structure in which inorganic particles are bound to each other by a binder to form an interstitial volume between the particles.
[0053] The electrode assembly 12 may be a jelly roll (wound type) electrode assembly having a structure in which long sheet-like positive and negative electrodes are wound with a separator interposed therebetween, a stack type (lamination type) electrode assembly in which a plurality of positive and negative electrodes cut into units of a predetermined size are stacked in sequence with a separator interposed therebetween, a stack / folding type electrode assembly having a structure in which a bi-cell or a full cell in which positive and negative electrodes of a predetermined unit are stacked with a separator interposed therebetween is wound up, etc.
[0054] The case 13 may include a storage portion 13a that stores the electrode assembly 12, a bent surface 17, and a sealing portion 13b that contains a sealant resin and is formed to seal the electrode assembly 12. The bent surface 17 may be formed by bending adjacent portions (an upper case portion and a lower case portion) of the case 13 to face each other as shown in FIG.
[0055] The sealing portion 13b may be sealed on three sides at the periphery of the case 13. In the three-side sealing structure, the case 13 is folded so that the receiving portions 13a formed in the upper and lower cases overlap to form the receiving portion. After folding the case in this manner, the remaining three sides except for the bent portion are sealed at the periphery to form the bent surface 17.
[0056] The sealing portion 13b refers to a portion that is welded along the outer circumferential surface of the receiving portion 13a to seal the electrode assembly 12. The sealing portion 13b may be welded by heat welding, ultrasonic welding, or the like, but is not particularly limited as long as the sealing portion can be welded. The electrode assembly 12 is surrounded by three sides of the sealing portion 13b and a bent surface 17 of the case 13 as shown in FIG. 1.
[0057] The electrode lead 11 may be housed in the case 13 such that a portion of the electrode lead 11 is exposed to the outside of the case 13. As shown in Fig. 1, a secondary battery 10 according to an embodiment of the present invention includes a lead film 14. The lead film 14 surrounds a portion of the outer surface of the electrode lead 11 and is interposed between the electrode lead 11 and a sealing portion 13b of the case 13 at a portion where the electrode lead 11 protrudes, thereby facilitating bonding between the electrode lead 11 and the sealing portion 13b of the case 13.
[0058] In one embodiment of the present invention, the case 13 may be in the form of a pouch.
[0059] In one embodiment, the case 13 may include an upper pouch and a lower pouch. When the case 13 includes an upper pouch and a lower pouch, the upper pouch and the lower pouch may be arranged so that the sealant resins face each other, and then the facing sealant resins may be fused to each other by heat and pressure to seal the battery.
[0060] In one embodiment of the present invention, the case 13 may be provided in the form of a film having a multi-layer structure including an outer layer for protecting against external impact, a metal barrier layer for blocking moisture, and a sealant layer for sealing the case.
[0061] The outer layer may include a polyester film using polyethylene terephthalate (PET), polybutylene terephthalate, polyethylene naphthalate, polybutylene naphthalate, copolymer polyester, polycarbonate, nylon, etc., and may be composed of a single layer or multiple layers. The metal barrier layer may include aluminum, copper, etc.
[0062] The sealant layer includes a sealant resin and may be composed of a single layer or multiple layers. The sealant resin may include polypropylene (PP), acid modified polypropylene (PPa), random polypropylene, ethylene propylene copolymer, or two or more of these. The ethylene propylene copolymer may include, but is not limited to, ethylene propylene rubber, ethylene propylene block copolymer, etc.
[0063] The sealing portion 13b includes an extension 15. When the secondary battery case 13 is folded and the three sides except the folded surface are sealed, an edge of one sealed surface adjacent to the folded surface of the secondary battery may protrude outward. The extension 15 may be a bat ear region. Throughout this specification, the term "bat ear region" refers to an extension of the sealing portion that protrudes outward from the battery, rather than in the direction in which the edge of the folded surface 17 extends. The bat ear region is an example of an extension of the sealing portion that protrudes outward. Other embodiments may have sealing portion extensions of different shapes and sizes.
[0064] In this case, since the sealing strength of the bent surface 17 is greater than that of the sealing portion, there is a very high possibility that vents will occur in the sealing portion except for the sealing portion adjacent to the bent surface, which increases the risk of damaging the lead tabs, bus bars, etc.
[0065] After injecting electrolyte into the sealing portion excluding the sealing portion (i.e., the extension portion) adjacent to the bent surface, the case may be further sealed. Thus, if a vent member is included in the sealing portion excluding the extension portion, the electrolyte may adhere to the vent member. Also, by further sealing after injecting the electrolyte, the sealing strength of the sealing portion excluding the extension portion becomes greater than the sealing strength of the extension portion. Thus, the vent is more likely to be guided to the extension portion instead of the remaining portion of the sealing portion.
[0066] In the secondary battery according to an embodiment of the present invention, the extension 15 includes a vent member 16. In the secondary battery according to an embodiment of the present invention, the gas can be discharged to the extension 15 separated from the electrode lead, and the amount of gas directly contacting the electrode lead 11 can be minimized, so that the safety of the battery can be further improved. That is, the amount of vent gas toward the side of the electrode lead 11 can be minimized, so that the safety of the battery can be further improved. As shown by the arrows in FIG. 1, the gas discharge direction is induced in a direction away from the electrode lead 11. The temperature of the electrode lead 11 may rise sharply in an abnormal situation such as overcharging or an internal short circuit. Thus, the safety of the secondary battery can be improved by minimizing the direct contact between the vented gas and the electrode lead 11. Throughout this specification, the vent member 16 is included in the extension 15, which means that the extension 15 and the vent member 16 may be at least partially overlapped.
[0067] The secondary battery 10 according to an embodiment of the present invention includes a vent member 16 including a vent resin having a melting point lower than that of the sealant resin. Since the vent member 16 includes a vent resin having a melting point lower than that of the sealant resin, the vent member 16 melts before the sealant resin when the temperature rises. Since the sealing strength of the portion into which the vent member 16 is inserted at high temperatures is lower than the sealing strength of the case portion including the sealant resin, the venting characteristic can be easily realized. As a result, when a thermal runaway phenomenon occurs, venting can be induced at the extension portion 15 due to a decrease in sealing strength. That is, the extension portion 15 can act as a passage for releasing gas from the storage portion to the outside of the secondary battery, and can effectively prevent the electrode lead 11 from being damaged by gas, flame, etc.
[0068] 2 is a schematic diagram illustrating the formation of a vent in a secondary battery according to an embodiment of the present invention, specifically, a cross-sectional view illustrating a vent member in a secondary battery according to an embodiment of the present invention.
[0069] 2, at a temperature at which the battery normally operates, the vent member 16 serves to seal the case 13 from the outside. If the temperature of the battery rises excessively due to abnormal battery behavior, the vent member 16 melts and the sealing strength of the portion where the vent member 16 is inserted decreases. As a result, since the sealing strength of the portion where the vent member 16 is inserted decreases, a vent may be formed at that position to release gas from the case. For example, pressure of the internal gas of the battery is applied to the interface between the vent member 16 and the extension portion 15, and a gap or vent may be formed between the vent member 16 and the extension portion 15, allowing the gas to be released.
[0070] The vent member 16 and the case 13 may be laminated by heat welding. In another example, the vent member 16 and the case 13 may be laminated by an adhesive such as glue. In yet another example, the vent member 16 and the case 13 may be physically connected to each other by a clip or the like. In yet another example, at least a portion of the vent member 16 may be embedded in a film that constitutes the case 13, for example, a sealant resin.
[0071] In one embodiment of the present invention, the vent member 16 may be located inside the extension portion 15. In yet another embodiment of the present invention, the vent member 16 may be located in the extension portion 15 through the housing portion 13a. In yet another embodiment of the present invention, the vent member 16 may extend to the outside of the case 13 through the extension portion 15. In yet another embodiment of the present invention, the vent member 16 may extend from the housing portion 13a to the outside of the case 13 through the extension portion 15.
[0072] 3 is a diagram showing a secondary battery according to still another embodiment of the present invention. Referring to FIG. 3, the vent member 16 may be inclined at the extension portion 15. For example, the vent member 16 may have an inclination angle of 10° to 80°, or 20° to 60°, or 40° to 50°. The inclination angle may refer to the angle between the protruding directions of the vent member and the electrode lead 11.
[0073] In one embodiment of the present invention, the vent member 16 may not overlap or contact the lead film 14 .
[0074] The vent member 16 may have an area that partially overlaps or contacts the lead film 14. When the vent member 16 has at least a partial area that overlaps or contacts the lead film 14, the position of the vent member 16 can be consistently and easily fixed. For example, if the vent member 16 is to be inserted and then welded, a portion of the vent member 16 may overlap or contact the lead film 14, allowing the vent member 16 to be inserted and then welded into a predetermined position.
[0075] The vent member 16 may have various shapes to facilitate venting. In one embodiment of the present invention, the vent member 16 may have a structure that tapers along the venting direction indicated by the arrow in FIG. 1. The width of the vent member 16 may taper continuously or discontinuously along the venting direction. When the vent member 16 has a structure that tapers along the venting direction, the discharge angle of the vented gas is reduced to minimize the amount of gas vented to the side of the electrode lead 11, thereby further improving the safety of the battery.
[0076] 4 to 6 are partially enlarged views showing an electrode lead and a vent member in a secondary battery 10 according to another embodiment of the present invention.
[0077] 4 and 5, the vent member 16 may have, for example, an elliptical (FIG. 4) or stepped (FIG. 5) shape. However, in other embodiments, the shape of the vent member 16 may be other shapes, such as a circle, a triangle, a trapezoid, etc.
[0078] As shown in FIG 6, the vent member 16 may have an asymmetrical stepped structure. In the asymmetrical stepped structure, the degree of the step may be formed to correspond to the side of the electrode lead 11. For example, the size (exhaust angle of the vented gas) and position (distance from the electrode lead 11) of the discharge end of the vent member 16 may be configured to minimize contact between the vented gas and the electrode lead, as shown in FIG 6. Thus, by reducing the size of the discharge end of the vent member to guide the gas away from the electrode lead 11 and positioning the discharge end away from the electrode lead, contact between the vented gas and the electrode lead may be minimized.
[0079] In one embodiment of the present invention, the thickness of the vent member 16 may decrease continuously or discontinuously along the protruding direction of the electrode lead 11. Figures 7a and 7b show two embodiments of a cross section of the vent member 16 of Figure 1 having varying thickness. As shown in Figure 7a, the thickness of the vent member 16 may decrease discontinuously along a step. Figure 7b shows a vent member 16 having a gradually or continuously varying thickness.
[0080] The vent member 16 may be positioned at a predetermined distance from the electrode lead 11. This can easily minimize the amount of gas vented in a direction that may directly contact the electrode lead 11, i.e., at the side of the electrode lead 11, thereby further improving the safety of the battery. The temperature of the electrode lead 11 may rise rapidly in an abnormal situation such as overcharging or an internal short circuit. Therefore, minimizing the direct contact between the vented gas and the electrode lead 11 can improve the safety of the secondary battery.
[0081] In one embodiment of the present invention, the vent member 16 may be separated from the lead film 14 at the sealing portion and at least partially overlap or contact the lead film 14 at the receiving portion 13a. By not overlapping or contacting the lead film 14 at the sealing portion, i.e., by positioning the vent member 16 away from the electrode lead 11, the amount of gas vented at the side of the electrode lead 11 can be minimized, further improving the safety of the battery.
[0082] In one embodiment of the present invention, the area where the vent member overlaps or contacts the lead film may be 1% to 30%, or 1.3% to 23%, or 1.5% to 12%, or 2% to 9% of the area where the lead film does not overlap or contact the electrode lead. Here, the area where the lead film does not overlap with the electrode lead means the sum of both the areas of the electrode lead and the lead film where the lead film does not overlap.
[0083] A portion of the vent member 16 and a portion of the lead film 14 may be overlapped or contacted by thermal welding. In another example, a portion of the vent member 16 and a portion of the lead film 14 may be overlapped or contacted by an adhesive such as glue. In another example, a portion of the vent member 16 and a portion of the lead film 14 may be physically connected to each other by a clip or the like. In yet another example, a portion of the vent member 16 may be embedded in a film that constitutes the lead film 14.
[0084] Fig. 8 is a partially enlarged view of an electrode lead 11 and a vent member 16 of a secondary battery according to yet another embodiment of the present invention. Referring to Fig. 8, if the protruding direction of the electrode lead 11 is taken as the Y axis and the direction perpendicular to the Y axis is taken as the X axis, the vent member 16 may include a first portion 16b extending in the X axis direction and a second portion 16a extending in the Y axis direction. As shown in Fig. 8, the first portion 16b is extended or connected to the lead film 14 through the second portion 16a.
[0085] In one embodiment of the present invention, the vent member 16 may have an L-shape, as shown in FIG.
[0086] In yet another embodiment of the present invention, the vent member 16 may be configured such that an inner end of the second portion 16a is cut to form a tapering section, as shown in FIG. 9. For example, the inner end of the second portion 16a may be cut in a direction that is not perpendicular to the Y-axis. When the vent member 16 has the above-mentioned shape, it is possible to more easily prevent the electrode assembly 12 from contacting the inner end of the second portion 16a inside the storage portion 13a. Here, the inner end of the second portion 16a refers to the end of the second portion that is closer to the storage portion.
[0087] Fig. 10 is a partially enlarged view of an electrode lead 11 and a vent member 16 of a secondary battery according to yet another embodiment of the present invention. Referring to Fig. 10, the first portion may extend along a first direction not parallel to the Y axis between the lead film and the second portion. The second portion may extend along a second direction perpendicular to the first direction. For example, when the first direction is set at an angle of 45° along the protruding direction of the electrode lead 11, the vent member 16 may have an L-shape.
[0088] In yet another embodiment of the present invention, the vent member 16 may be configured such that an inner end of the second portion 16a is cut to form a tapered portion. For example, the inner end of the second portion 16a may be cut in a direction that is not perpendicular to the second direction. When the vent member 16 has the above-mentioned shape, it is possible to more easily prevent the electrode assembly 12 from contacting the inner end of the second portion 16a inside the storage portion 13a. Here, the inner end of the second portion 16a refers to the end of the second portion that is closer to the storage portion.
[0089] In one embodiment of the invention, the second portion 16a, such as a body portion, may be substantially vented and the first portion 16b, such as a bridge portion, may be substantially non-vented.
[0090] 8 to 10, in one embodiment of the present invention, the first portion 16b may have at least a partial area overlapping or contacting the lead film 14. By having at least a partial area of the first portion 16b overlapping or contacting the lead film 14, the position of the vent member 16 may be consistently and easily fixed. For example, when the vent member 16 is to be welded after being inserted, the vent member 16 may be welded after being inserted at a predetermined position by having a portion of the first portion 16b overlapping or contacting the lead film 14.
[0091] A part of the first portion 16b and a part of the lead film 14 may be overlapped or contacted by thermal welding. In another example, a part of the first portion 16b and a part of the lead film 14 may be overlapped or contacted by an adhesive such as glue. In still another example, a part of the first portion 16b and a part of the lead film 14 may be physically connected by a clip or the like. In yet another example, a part of the first portion 16b may be embedded in a film that constitutes the lead film 14.
[0092] 8 to 10, in one embodiment of the present invention, the second portion 16a of the vent member 16 and the lead film 14 may not overlap or contact each other. For example, the second portion 16a and the lead film 14 may not overlap or contact each other at the sealing portion. When the second portion 16a of the vent member 16 and the lead film 14 do not overlap or contact each other, the amount of gas vented to the side of the electrode lead 11 is minimized, and the safety of the battery can be further improved.
[0093] 8 to 10, the outer end of the first part 16b may be spaced apart from the inner end of the extension part 15. Here, the "outer end of the first part of the vent member" refers to the end of the first part 16b close to the extension part. The "inner end of the extension part" refers to the end of the extension part adjacent to the storage part. In this case, the entire first part 16b may be located in the storage part 13a. As a result, the gap or space between the first part 16b and the extension part 15 is exposed to the storage part 13a, and as a result, gas pressure is concentrated in this gap or space, allowing for faster venting in an emergency situation.
[0094] In one embodiment of the present invention, the first portion 16b may have a rectangular shape. For example, a long side of the first portion may be located in the X-axis direction, and a short side of the first portion may be located in the Y-axis direction. In one embodiment of the present invention, the second portion 16a may have a rectangular shape. For example, a short side of the second portion may be located in the X-axis direction, and a long side of the second portion may be located in the Y-axis direction.
[0095] 11 to 13 are partially enlarged views showing a lead film and a vent member of a secondary battery according to another embodiment of the present invention.
[0096] 11 to 13, as described above, the vent member 16 includes a first portion 16b and a second portion 16a, and the second portion 16a may have, for example, an elliptical or stepped shape. However, the shape of the second portion 16a may be a circle, a triangle, a trapezoid, etc. in other embodiments.
[0097] Also, referring to FIG. 13, the second portion 16a may have an asymmetrical stepped structure. In the asymmetrical stepped structure, the degree of the step may be formed to correspond to the side of the electrode lead 11. For example, the size (exhaust angle of the vented gas) and position (distance from the electrode lead 11) of the discharge end of the second portion 16a may be configured to minimize contact between the vented gas and the electrode lead, as shown in FIG. 13. In this manner, by reducing the size of the discharge end of the second portion to guide the gas away from the electrode lead 11 and positioning the discharge end away from the electrode lead, contact between the vented gas and the electrode lead can be minimized.
[0098] In one embodiment of the present invention, the vent member 16 can vent at a temperature of 100° C. to 120° C. Also, the vent member 16 can vent at a pressure of 1.5 atm or more.
[0099] By venting the vent member 16 within the above-mentioned temperature range and / or pressure condition, the battery is sealed during normal operation, and gas can be more easily induced to escape only when the battery behaves abnormally.
[0100] In one embodiment of the present invention, the vent resin having a melting point lower than that of the sealant resin may include linear low density polyethylene having a comonomer with a carbon number of 6 or more. By including linear low density polyethylene having a comonomer with a carbon number of 6 or more in the vent resin, the vent resin has excellent sealing properties with the sealant resin in the normal temperature range, and the sealing strength of the sealing part including the vent member 16 decreases at high temperatures, thereby enabling venting.
[0101] In one embodiment of the present invention, the vent resin having a melting point lower than that of the sealant resin may include a linear low density polyethylene having a comonomer having 6 to 8 carbon atoms.
[0102] In one embodiment of the present invention, the vent resin having a lower melting point than the sealant resin may have a melting point of 100° C. to 130° C., or 105° C. to 125° C., or 110° C. to 120° C. When the melting point of the vent resin is within the above-mentioned range, the sealing strength of the sealing part including the vent member 16 decreases at high temperatures, for example, above 100° C., and the vent characteristics can be more easily realized.
[0103] The melting point of the vent resin, which has a lower melting point than the sealant resin, can be measured using a differential scanning calorimeter (DSC). For example, the temperature of the sample is increased from 30°C to 280°C at 10°C / min, then maintained at 280°C for 10 minutes, cooled to 30°C at 10°C / min, and maintained at 30°C for 10 minutes. The temperature of the sample is then increased from 30°C to 280°C at 10°C / min, and maintained at 280°C for 10 minutes to measure the melting point.
[0104] In one embodiment of the present invention, the vent member 16 may have a maximum sealing strength of less than 6 kgf / 15 mm, less than 5 kgf / 15 mm, or less than 4.5 kgf / 15 mm at 100° C. to 120° C. In one embodiment of the present invention, the vent member 16 may have a maximum sealing strength of less than 6 kgf / 15 mm, less than 5 kgf / 15 mm, or less than 4.5 kgf / 15 mm at 100° C. to 120° C. In one embodiment of the present invention, the vent member 16 may have a maximum sealing strength of less than 3 kgf / 15 mm, less than 2 kgf / 15 mm, less than 1 kgf / 15 mm, or less than 0.5 kgf / 15 mm at 120° C. or more. When the vent member satisfies the above-mentioned sealing strength in the above-mentioned temperature range, the sealing strength of the sealing portion including the vent member 16 decreases at high temperatures, for example, 100° C. or more, and the vent characteristics can be more easily realized.
[0105] In addition, in one embodiment of the present invention, the vent member may have a maximum sealing strength of 6 kgf / 15 mm or more, 8 kgf / 15 mm or more, or 10 kgf / 15 mm or more at room temperature to 60° C. When the vent member satisfies the above-mentioned sealing strength in the above-mentioned temperature range, it has excellent sealing strength during normal operation of the battery, and the hermeticity of the battery can be more easily ensured.
[0106] In one embodiment of the present invention, the vent member may have a maximum sealing strength of less than 6 kgf / 15 mm at 100° C. or higher, and a maximum sealing strength of 6 kgf / 15 mm or higher at room temperature to 60° C. When the vent member satisfies the above-mentioned sealing strength, the sealing strength of the sealing part including the vent member 16 decreases at high temperatures, and vent characteristics can be easily realized. In addition, during normal operation of the battery, the sealing strength of the battery is excellent, and the hermeticity of the battery can be more easily ensured.
[0107] In one embodiment of the present invention, the vent member 16 may have an average sealing strength of less than 4.5 kgf / 15 mm or less than 3 kgf / 15 mm at 100° C. or more. In one embodiment of the present invention, the vent member 16 may have an average sealing strength of less than 4.5 kgf / 15 mm or less than 3 kgf / 15 mm at 100° C. to 120° C. In one embodiment of the present invention, the vent member 16 may have an average sealing strength of less than 2 kgf / 15 mm, less than 1 kgf / 15 mm, or less than 0.5 kgf / 15 mm at 120° C. or more. When the vent member satisfies the above-mentioned sealing strength in the above-mentioned temperature range, the sealing strength of the sealing portion including the vent member 16 decreases at high temperatures, and the vent characteristics can be more easily realized.
[0108] In one embodiment of the present invention, the vent member may have an average sealing strength of 4.5 kgf / 15 mm or more, or 5 kgf / 15 mm or more, or 6 kgf / 15 mm or more, or 7 kgf / 15 mm or more at room temperature to 60° C. When the vent member satisfies the above-mentioned sealing strength in the above-mentioned temperature range, it has excellent sealing strength during normal operation of the battery, and the hermeticity of the battery can be more easily ensured.
[0109] In one embodiment of the present invention, the vent member may have an average sealing strength of less than 4.5 kgf / 15 mm at temperatures of 100° C. or higher, and an average sealing strength of 4.5 kgf / 15 mm or higher at room temperature to 60° C. When the vent member has the above-mentioned sealing strength within the above-mentioned temperature range, the sealing strength of the sealing part including the vent member 16 decreases at high temperatures, making it easier to realize vent characteristics. In addition, the vent member has excellent sealing strength during normal operation of the battery, making it easier to ensure the hermeticity of the battery.
[0110] The sealing strength of the vent member according to temperature can be measured by cutting a portion of the case into which the vent member has been inserted to a width of 15 mm and a length of 5 cm, opening both ends at 180°, gripping the cut surface using a UTM jig, and conducting a tensile test at a speed of 5 mm / min.
[0111] In this case, the maximum sealing strength means the maximum value at which the battery case breaks, and the average sealing strength means the average value when the battery case is stretched 8 mm at 4.5 kgf / 15 mm when the maximum sealing strength is 4.5 kgf / 15 mm or more, and means the average value when the battery case is stretched 8 mm at the maximum sealing strength when the maximum sealing strength is less than 4.5 kgf / 15 mm.
[0112] In one embodiment of the present invention, the vent resin may be polymerized in the presence of a metallocene catalyst. When the vent resin is polymerized in the presence of a metallocene catalyst, it may be more advantageous in terms of sealing strength and physical properties than when the vent resin is polymerized in the presence of a Ziegler-Natta catalyst.
[0113] In one embodiment of the present invention, the content of the comonomer having 6 or more carbon atoms in the linear low density polyethylene having a comonomer having 6 or more carbon atoms may be 15% by weight or less, 12% by weight or less, 11.8% by weight or less, 10% by weight or less, 9% by weight or less, 8% by weight or less, or 7.6% by weight or less, based on 100% by weight of the linear low density polyethylene having a comonomer having 6 or more carbon atoms. At the same time, the content of the comonomer having 6 or more carbon atoms may be 5% by weight or more, 7.6% by weight or more, 8% by weight or more, 9.0% by weight or more, 10% by weight or more, 11.8% by weight or more, or 12% by weight or more, based on 100% by weight of the linear low density polyethylene having a comonomer having 6 or more carbon atoms. When the content of the comonomer having 6 or more carbon atoms satisfies the above-mentioned range, the problem of the intermolecular packing density decreasing and the sealing strength decreasing during normal operation of the battery can be more easily prevented.
[0114] The content of the comonomer having 6 or more carbon atoms can be measured by H-NMR. For example, about 10 mg of a sample is completely dissolved in about 0.6 mL of trichloroethylene solvent using a heat gun, and then sampled in an NMR tube. 1 H-NMR or 13 It can be measured using C-NMR.
[0115] In one embodiment of the present invention, the weight average molecular weight of the vent resin having a lower melting point than the sealant resin may be 100,000 g / mol to 400,000 g / mol, or 200,000 g / mol to 350,000 g / mol, or 230,000 g / mol to 300,000 g / mol. When the weight average molecular weight of the vent resin satisfies the above range, the sealing strength with the sealant resin during normal operation of the battery can be further improved.
[0116] In one embodiment of the present invention, the polydispersity index (PDI) of the vent resin having a melting point lower than that of the sealant resin may be 4 or less, or 3.8 or less, or 3.796 or less, or 3.5 or less, or 3.023 or less, or 3 or less, or 2.7 or less, or 2.674 or less. Also, the polydispersity index (PDI) may be 1.0 or more. When the polydispersity index of the vent resin satisfies the above-mentioned range, the molecular weight distribution becomes narrow, and the sealing strength and physical properties with the sealant resin become more excellent during normal operation of the battery.
[0117] The weight average molecular weight and polydispersity index of the vent resin having a melting point lower than that of the sealant resin may be measured by gel permeation chromatography (GPC) under the following conditions.
[0118] - Column: Tosoh HLC-8321 GPC / HT - Solvent: Trichlorobenzene (TCB) + 0.04% BHT (after drying with 0.1% CaCl2) - Flow rate: 1.0ml / min - Sample concentration: 1.5mg / ml - Injection volume: 300μl - Column temperature: 160℃ - Detector: RI detector - Standard: Polystyrene (corrected to a cubic function)
[0119] In one embodiment of the present invention, the crystallization temperature of the sealant resin may be similar to that of the vent resin having a melting point lower than that of the sealant resin. For example, the difference between the crystallization temperature of the sealant resin and that of the vent resin may be 10° C. or less, or 5° C. or less. Also, the difference between the crystallization temperature of the sealant resin and that of the vent resin may be 0.1° C. or more. When the difference between the crystallization temperature of the sealant resin and that of the vent resin is within the above-mentioned range, the adhesion characteristics of the sealant resin and the vent resin during normal operation of the battery can be further improved.
[0120] In one embodiment of the present invention, the crystallization temperature of the vent resin having a lower melting point than the sealant resin may be 90° C. to 115° C., or 95° C. to 110° C., or 100° C. to 110° C., or 105° C. to 110° C. When the crystallization temperature of the vent resin satisfies the above-mentioned range, the adhesion property of the sealant resin and the vent resin can be further improved.
[0121] The crystallization temperature can be measured using a differential scanning calorimeter (DSC). For example, the temperature of the sample can be increased from 30°C to 280°C at 10°C / min, then maintained at 280°C for 10 minutes, cooled to 30°C at 10°C / min, and maintained at 30°C for 10 minutes. The temperature of the sample can then be increased from 30°C to 280°C at 10°C / min, and maintained at 280°C for 10 minutes to measure the crystallization temperature.
[0122] In one embodiment of the present invention, the vent member 16 may have a film thickness.
[0123] The vent member 16 may be formed to have a predetermined thickness of a preset size, and may be inserted into the extension 15 so that the insertion length may be changed or the venting pressure and position may be controlled, depending on the design.
[0124] In one embodiment of the present invention, the vent member 16 may further include an adhesive layer for smoother placement and sealing between the sealant resin and the vent resin having a lower melting point than the sealant resin.
[0125] A secondary battery according to one embodiment of the present invention includes a vent member having a vent resin with a lower melting point than a sealant resin in an extension portion, thereby enabling smoother and faster directional venting in which the sealing strength is reduced at high temperatures when a thermal runaway phenomenon occurs, thereby discharging gas from the extension portion.
[0126] In one embodiment of the present invention, the secondary battery may be a cylindrical, prismatic or pouch-type secondary battery.
[0127] Although the preferred embodiments of the present invention have been illustrated and described above, it goes without saying that the present invention is not limited to the specific preferred embodiments described above, and that various modifications can be made by those having ordinary skill in the art to which the invention pertains without departing from the gist of the present invention as claimed in the claims, and such modifications should not be understood individually from the technical ideas and perspectives of the present invention. [Explanation of symbols]
[0128] 10 Secondary battery 11 Electrode Lead 12 Electrode assembly 13 Cases 13a Storage area 13b Sealing part 14 Lead Film 15 Extension 16 Venting material 16a Part 2 16b Part 1 17 Bent surface
Claims
1. An electrode assembly; an electrode lead attached to the electrode assembly; a case including a sealing portion formed to seal the electrode assembly and a housing portion partitioned by a bent surface and the sealing portion and housing the electrode assembly therein; a vent member including a vent resin having a melting point lower than that of the sealant resin; the sealing portion includes an extension adjacent to and extending from the bending surface; the vent member is at least partially located in the extension; 13. A pouch-type secondary battery, wherein at least a portion of the vent member extends in a direction other than a direction toward the electrode lead.
2. 2. The pouch-type secondary battery according to claim 1, wherein the vent member is at least partially located in a bat's ear region.
3. a lead film surrounding an outer surface of the electrode lead and interposed between the electrode lead and the sealing portion, the vent member extends through the recess; a first end of the vent member spaced apart from the lead film at the sealing portion; The pouch-type secondary battery according to claim 1 , wherein the second end of the vent member at least partially overlaps or contacts the lead film in the storage portion.
4. a lead film surrounding an outer surface of the electrode lead and interposed between the electrode lead and the sealing portion, the electrode lead extends from the case along a Y axis; the vent member includes a first portion and a second portion; the first portion extends along an X-axis perpendicular to the Y-axis between the lead film and the second portion; The pouch-type secondary battery according to claim 1 , wherein the second portion extends along the Y-axis.
5. a lead film surrounding an outer surface of the electrode lead and interposed between the electrode lead and the sealing portion, the electrode lead extends from the case along a Y axis; the vent member includes a first portion and a second portion; the first portion extends between the lead film and the second portion along a first direction that is not parallel to the Y axis; The pouch-type secondary battery according to claim 1 , wherein the second portion extends along a second direction perpendicular to the first direction.
6. 5. The pouch-type secondary battery according to claim 4, wherein the vent member is L-shaped.
7. the vent member includes a tapered portion at an intersection of the first portion and the second portion; The pouch-type secondary battery according to claim 4 , wherein the tapered portion extends into the storage portion.
8. 5. The pouch-type secondary battery according to claim 4, wherein the first portion is a bridge portion at least partially overlapping the lead film.
9. an outer end of the first portion spaced from an inner end of the extension portion; The pouch-type secondary battery according to claim 4 , wherein the first portion is located in the storage portion.
10. The pouch-type secondary battery according to claim 4 , wherein the second portion does not overlap or contact the lead film.
11. The pouch-type secondary battery according to claim 1 , wherein the vent member has a width that narrows along a vent direction.
12. The pouch-type secondary battery according to claim 1 , wherein the vent member has any one of a circular shape, an elliptical shape, a stepped shape, a triangular shape, and a trapezoidal shape.
13. The pouch-type secondary battery according to claim 1 , wherein the vent member has a thickness that decreases along a vent direction.
14. 4. The pouch-type secondary battery according to claim 3, wherein an area of the vent member overlapping or in contact with the lead film is 1% to 30% of an area of the lead film not overlapping or in contact with the electrode lead.
15. 15. The pouch-type secondary battery according to claim 1, wherein the vent resin contains a linear low-density polyethylene having a comonomer having 6 or more carbon atoms.
16. 2. The pouch-type secondary battery according to claim 1, wherein the vent member melts at 100° C. to 120° C. to vent gas from the storage portion to the outside of the pouch-type secondary battery.
17. The pouch-type secondary battery according to claim 16, wherein the vent member vents gas from the storage section when the pressure in the storage section is 1.5 atm or higher.
18. The pouch-type secondary battery according to claim 1 , wherein the vent member has a maximum sealing strength of less than 6 kgf / 15 mm at 100° C. or higher.
19. The pouch-type secondary battery according to claim 1 , wherein the vent member has an average sealing strength of less than 4.5 kgf / 15 mm at 100° C. or higher.
20. 2. The pouch-type secondary battery according to claim 1, wherein the vent member has a maximum sealing strength of 6 kgf / 15 mm or more at room temperature to 60° C.
21. The pouch-type secondary battery according to claim 1, wherein the vent member has an average sealing strength of 4.5 kgf / 15 mm or more at room temperature to 60° C.
22. 16. The pouch-type secondary battery according to claim 15, wherein the content of the comonomer having 6 or more carbon atoms is 15% by weight or less, based on 100% by weight of the linear low-density polyethylene having a comonomer having 6 or more carbon atoms.
23. 16. The pouch-type secondary battery according to claim 15, wherein the linear low-density polyethylene having a comonomer having 6 or more carbon atoms in the vent resin has a polydispersity index (PDI) of 4 or less.
24. 2. The pouch-type secondary battery according to claim 1, wherein the difference between the crystallization temperature of the sealant resin and the crystallization temperature of the vent resin is 10° C. or less.
25. 2. The pouch-type secondary battery according to claim 1, wherein the vent resin has a melting point of 100° C. to 130° C.
26. The pouch-type secondary battery according to claim 1, wherein the vent resin has a weight average molecular weight of 100,000 g / mol to 400,000 g / mol.
27. The pouch-type secondary battery according to claim 1 , wherein the vent member has a maximum sealing strength of less than 3 kgf / 15 mm at 120° C. or higher.
28. The pouch-type secondary battery according to claim 1 , wherein the vent member has an average sealing strength of less than 2 kgf / 15 mm at 120° C. or higher.
Citation Information
Patent Citations
Laminated battery
JP2010244865A
Laminate battery
JP2010251151A
Battery cell and its manufacturing method
JP2018525804A
Cell
JP2019207781A
Secondary Battery of Improved Safety
KR1020080036257A