Method for manufacturing bismuth-vanadium compounds

TWI946263BActive Publication Date: 2026-11-11NAT FORMOSA UNIV
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
TW114152266
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Filing Date
2025-12-31
Publication Date
2026-11-11
Estimated Expiration
2045-12-30

Smart Images

  • Figure TWG2TB001921015_001
    Figure TWG2TB001921015_001
  • Figure TWG2TB001921015_002
    Figure TWG2TB001921015_002
  • Figure TWG2TB001921015_003
    Figure TWG2TB001921015_003
Patent Text Reader

Abstract

This invention primarily discloses a method for manufacturing bismuth-vanadium compounds, which selectively forms bismuth-vanadium compound powders with different compositions by controlling the precursor composition, pH adjustment conditions, and hydrothermal reaction parameters. The method first involves dissolving a bismuth-containing precursor and a vanadium-containing precursor separately in a first and a second liquid medium, and then mixing them to form a mixed precursor solution. Next, the pH of this mixed precursor solution is adjusted to a weakly alkaline (pH 5-8) or strongly alkaline (pH 10-13) state. Subsequently, the mixed precursor solution is treated hydrothermally to obtain a precipitate of the bismuth-vanadium compound. Specifically, by controlling the bismuth-containing precursor, the vanadium-containing precursor, and the liquid medium to provide / not provide chloride ions, as well as the pH of the mixed precursor solution, the bismuth-vanadium compound can optionally be BiVO₄, BiVO₄ / BiOCl, Bi₂VO₅₅-δ, or Bi₂VO₅₅-δ / BiOCl. Finally, after separation, cleaning and drying, high-purity bismuth-vanadium compound powder with multiple uses can be obtained.
Need to check novelty before this filing date? Find Prior Art

Claims

1. A method for manufacturing a bismuth-vanadium compound, comprising the following steps: (1) dissolving a bismuth-containing precursor in a first liquid medium to obtain a first precursor solution; wherein, (1) The first mixing ratio of the bismuth-containing precursor to the first liquid medium is between 0.15 w / v and 1.9 w / v; (2) A vanadium-containing precursor is dissolved in a second liquid medium to obtain a second precursor solution; wherein the second mixing ratio of the vanadium-containing precursor to the second liquid medium is between 0.12 w / v and 2.5 w / v; (3) The first precursor solution and the second precursor solution are mixed to obtain a mixed precursor solution; (4) A pH adjustment treatment is performed on the mixed precursor solution using a pH adjuster so that the pH of the mixed precursor solution is between pH 5 and pH 8; (5) The mixed precursor solution is placed in a reaction vessel and then heated to perform a hydrothermal reaction treatment on the mixed precursor solution at a temperature between 120°C and 200°C for a reaction time, thereby generating a bismuth-vanadium compound precipitate in the reaction vessel; wherein the reaction time is between 2 hours and 24 hours; and (6) the bismuth-vanadium compound precipitate is separated from the reaction vessel and washed and dried to obtain a bismuth-vanadium compound powder.

2. A method for manufacturing a bismuth-vanadium compound, comprising the following steps: (1) dissolving a bismuth-containing precursor in a first liquid medium to obtain a first precursor solution; wherein, (2) A first mixing ratio of the bismuth-containing precursor to the first liquid medium is between 0.15 w / v and 1.9 w / v; (3) A vanadium-containing precursor is dissolved in a second liquid medium to obtain a second precursor solution; wherein a second mixing ratio of the vanadium-containing precursor to the second liquid medium is between 0.12 w / v and 2.5 w / v; (4) The first precursor solution and the second precursor solution are mixed to obtain a mixed precursor solution; (5) A pH adjustment treatment is performed on the mixed precursor solution using a pH adjuster so that the pH of the mixed precursor solution is between pH 10 and pH 13. (5) The mixed precursor solution is placed in a reaction vessel and then heated to perform a hydrothermal reaction treatment on the mixed precursor solution at a temperature between 120°C and 200°C for a reaction time, thereby generating a bismuth-vanadium compound precipitate in the reaction vessel; wherein the reaction time is between 2 hours and 24 hours; and (6) the bismuth-vanadium compound precipitate is separated from the reaction vessel and washed and dried to obtain a bismuth-vanadium compound powder.

3. A method for manufacturing a bismuth-vanadium compound as described in claim 1 or 2, wherein, The bismuth-containing precursor comprises at least one selected from the group consisting of bismuth nitrate (Bi(NO₃)₃·5H₂O), bismuth sulfate (Bi₂(SO₄)₃), bismuth oxide (Bi₂O₃), anhydrous bismuth chloride (BiCl₃), basic bismuth carbonate (Bi₂O₂CO₃), and bismuth bromide (BiBr₃).

4. A method for manufacturing a bismuth-vanadium compound as described in claim 1 or 2, wherein, The vanadium-containing precursor comprises at least one selected from the group consisting of ammonium metavanadate (NH₄VO₃), vanadium pentoxide (V₂O₅), sodium orthovanadate (Na₃VO₄), sodium metavanadate (NaVO₃), vanadium trichloride (VCl₃), and vanadium trioxide (V₂O₃).

5. A method for manufacturing a bismuth-vanadium compound as described in claim 1 or 2, wherein, The first liquid medium comprises at least one selected from the group consisting of concentrated nitric acid (HNO₃) with a concentration of 65%–70%, diluted nitric acid with a concentration of 0.1M–5.5M, concentrated sulfuric acid (H₂SO₄) with a concentration of 95%–98%, diluted sulfuric acid with a concentration of 0.1M–8M, perchloric acid (HClO₄) with a concentration of 65%–72%, diluted perchloric acid with a concentration of 0.1M–12M, concentrated hydrochloric acid (HCl) with a concentration of 35%–38%, diluted hydrochloric acid with a concentration of 0.1M–6.5M, and deionized water.

6. A method for producing a bismuth-vanadium compound as described in claim 1 or 2, wherein, The second liquid medium comprises at least one selected from the group consisting of diluted hydrochloric acid (HCl) with a concentration of 0.1M to 6.5M, diluted sulfuric acid (H₂SO₄) with a concentration of 0.1M to 8M, diluted perchloric acid (HClO₄) with a concentration of 0.1M to 12M, diluted nitric acid (HNO₃) with a concentration of 0.1M to 5.5M, and deionized water.

7. A method for manufacturing a bismuth-vanadium compound as described in claim 1, wherein, The pH adjuster is ammonia water (NH₃·H₂O).

8. A method for manufacturing a bismuth-vanadium compound as described in claim 2, wherein, The pH adjuster comprises at least one selected from the group consisting of ammonia (NH₃·H₂O), sodium hydroxide (NaOH), and potassium hydroxide (KOH).

9. A method for producing a bismuth-vanadium compound as described in claim 1, wherein, When neither the bismuth-containing precursor nor the first liquid medium provides chloride ions to the first precursor solution, and when the vanadium-containing precursor does not provide chloride ions to the second precursor solution, the precipitate of the bismuth-vanadium compound generated in the reaction vessel is a precipitate of bismuth vanadate (BiVO₄).

10. A method for producing a bismuth-vanadium compound as described in claim 1, wherein, When the bismuth-containing precursor and / or the first liquid medium provides chloride ions to the first precursor solution, and / or the vanadium-containing precursor provides chloride ions to the second precursor solution, the precipitate of the bismuth-vanadium compound generated in the reaction vessel is a precipitate of a bismuth vanadate / bismuth oxychloride (BiVO₄ / BiOCl) complex.

11. A method for manufacturing a bismuth-vanadium compound as described in claim 2, wherein, When neither the bismuth-containing precursor nor the first liquid medium provides chloride ions to the first precursor solution, and when the vanadium-containing precursor does not provide chloride ions to the second precursor solution, the bismuth-vanadium compound precipitate generated in the reaction vessel is a Bi2VO5.5-δ type bismuth vanadium oxide precipitate, and 0≤δ≤0.

5.

12. A method for manufacturing a bismuth-vanadium compound as described in claim 2, wherein, When the bismuth-containing precursor and / or the first liquid medium provides chloride ions to the first precursor solution, and / or the vanadium-containing precursor provides chloride ions to the second precursor solution, the bismuth-vanadium compound precipitate generated in the reaction vessel is a composite precipitate, and the composite precipitate contains Bi2VO5.5-δ type bismuth vanadium oxide and bismuth oxychloride (BiOCl), wherein 0≤δ≤0.5.

Citation Information

Patent Citations

  • Non-stoichiometric broom-like bismuth vanadate fiber and preparation method thereof

    CN104445400A

  • Pucherite visible-light-driven photocatalyst, preparing method and application

    CN105032394A