Method for producing woven weftwise hollow fabric
A production method and technology in the weft direction, applied in the direction of fabrics, embossed fabrics, and embossed fabrics, etc., to achieve the effects of reducing dosage, improving air permeability, and reducing processing pressure
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2011-04-13
- Estimated Expiration
- Not applicable · inactive patent
Smart Images
Figure 1 Figure 2 Figure 3
Abstract
Description
technical field
[0001] The invention provides a production method of fabric weft hollow fabric, which belongs to the technical field of textile fabric production. Background technique
[0002] The warp hollow fabric is favored by people because of its good air permeability, strong moisture absorption, comfortable wearing, soft hand feeling and low price. However, with the improvement of people's living standards, there are great requirements for the wearing comfort of clothing. improve. At present, in order to increase the comfort of clothing when worn, simple warp hollow fabrics can no longer meet people's requirements. Therefore, there is a great need for a production method of weft hollow fabrics with simple production process and good pattern effect. Contents of the invention
[0003] The object of the present invention is to provide a production method of weft direction hollow fabric which can overcome the above-mentioned defects, is convenient to operate and has exc...
Examples
Embodiment 1
[0021] Example 1: In Figure 1-5 In the shown example 1, the processes of gray cloth weaving, gray cloth washing, singeing and desizing, scouring and bleaching, caustic soda mercerizing, whitening, tentering and pre-shrinking are sequentially carried out, wherein, in the gray cloth weaving process, the fabric warp yarn The thread is made of 11.7 tex pure cotton yarn, the weft direction is made of 14.6 tex pure cotton yarn marked with a and the vinylon filament of 50 denier is marked with b. The weft arrangement is 18a2b, that is, the loom introduces 18 pure cotton yarns and 2 vinylon filaments sequentially during the weft insertion movement, and then introduces them sequentially; in the gray cloth washing process, the washing temperature is 90 ° C; singeing In the desizing process, the washing temperature is 95°C; in the scouring and bleaching process, the washing temperature is 95°C; in the caustic soda mercerizing process, the concentration of caustic soda is 211g / l, and the...
Embodiment 2
[0022] Example 2: In Figure 6-10 In the shown embodiment 2, the processes of gray cloth weaving, gray cloth washing, singeing and desizing, scouring and bleaching, caustic soda mercerizing, dyeing, tentering and pre-shrinking are sequentially carried out, wherein, in the gray cloth weaving process, the fabric warp yarn Use 14.6 tex pure cotton yarn, weft use 14.6 tex pure cotton yarn with a mark and 50 denier vinylon filament with b mark. The weft arrangement is 48a2b10a2b10a2b10a2b48a2b, that is, the loom sequentially introduces 48 pure cotton yarns, 2 vinylon filaments, 10 pure cotton yarns, 2 vinylon filaments, and 10 pure cotton yarns during the weft insertion movement. Thread, 5 vinylon filaments, 10 pure cotton yarns, 5 vinylon filaments, 48 pure cotton yarns, and 2 vinylon filaments; they will be introduced in sequence in turn; in the gray cloth washing process, the washing temperature is 90°C; In the singeing and desizing process, the washing temperature is 95°C. I...