Production method of colored polyester yarn
A production method and technology of polyester, which is applied in the field of polyester colored yarn production, can solve the problems of environmental pollution, high cost, and long time consumption, and achieve the effects of high linear density and strength, stable quality, and good performance
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2013-07-03
- Estimated Expiration
- Not applicable · inactive patent
Abstract
Description
technical field
[0001] The invention relates to a production method of colored polyester yarn, which belongs to the technical field of chemical fibers. Background technique
[0002] Polyester has very good chemical fiber properties, including good dyeability. The existing production method of colored polyester yarn is mainly made of white polyester yarn. This method takes a long time, has high loss, pollutes the environment, and costs high. Contents of the invention
[0003] The purpose of the present invention is to overcome the shortcomings of the prior art and provide a production method of colored polyester yarn.
[0004] The production method of polyester colored yarn of the present invention comprises the following steps: using three kinds of raw yarns of white polyester pre-oriented yarn, cationic fuel dyeable polyester and black polyester pre-oriented yarn as raw materials, passing through the yarn guide, the first roller, The first hot box, twister, second roll...
Examples
Embodiment 1
[0009] The production method of the colored polyester yarn of the present embodiment comprises the following steps: using white polyester pre-oriented yarn, cationic fuel dyeable polyester and black polyester pre-oriented yarn as raw materials, passing through the yarn guide and the first roller in sequence , first heat box, twister, second roller, network nozzle, third roller, oiling roller, stretching and winding forming, said white polyester pre-oriented yarn, cationic fuel dyeable polyester and black silk polyester The mass ratio of pre-oriented filaments is 2:2:3. Said drawing speed is 200-300m / min; said drawing ratio is 1.53-1.56.
[0010] The polyester colored yarn produced in this example has a strength of 4.3cN / dtex, an elongation of 1.7%, a crimp shrinkage of 18%, and a crimp stability of 80%.