A membrane material of bridge-island type conductive material
Through the design of bridge-island conductive material film materials, the multi-dimensional overlapping structure of nano-micron filaments and sheet-like conductive materials is used to solve the inductive reactance problem of the conductive film under high-frequency conditions, improve the conductive performance and cost-effectiveness, and is suitable for 5G , multi-antenna technology and electronic printing products in the 6G era.
Patent Information
- Application Number
- CN201910714849.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-07-22
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2039-07-22
AI Technical Summary
Existing conductive film materials have serious conductive inductance problems under high-frequency conditions, especially in the fields of 5G and 6G ultra-high frequency matrix circuits and massive antennas, which affects product performance and efficiency.
It adopts a bridge-island type conductive material film material, which is composed of a base film, a conductive material ink layer and an auxiliary functional layer. Through the multi-dimensional overlapping structure of nano-micron filamentary conductive materials and flake, spherical and other conductive materials, orderly physical contact points are achieved It can control the direction of microscopic current rheology and reduce the high-frequency alternating inductance of the conductive ink layer.
It effectively reduces the conductive inductance and improves the comprehensive conductivity and cost-effectiveness of the conductive film. It is suitable for roll-to-roll production of flexible conductive films and electronic printing products, especially in the multi-antenna technology in the 5G and 6G era, which significantly improves performance and market demand.
Smart Images

Figure CN112289485B_ABST
Abstract
Description
Technical Field
[0001] Conductive film, a film material of bridge-island conductive material that can overcome the surface inductive reactance of the conductive film, referred to as bridge-island conductive film. It consists of a base film, a conductive material ink layer and necessary auxiliary functional layers; it has a variety of product process application forms such as composite, photolithography, electronic printing, anisotropy, electromagnetic, electrode, etc., which are suitable for the roll-to-roll (R2R) production of flexible conductive films and their secondary products. Its organic, inorganic, and semiconductor conductive material ink layer is a multi-dimensional overlapping structure of nano-micron filamentary conductive material and at least another sheet (including triangular sheet), spherical, olive-shaped, granular (including cube) and other conductive materials. By constructing bridge-island physical contact (sintering) points for conductive materials of different shapes, the direction of microscopic current flow is controlled, and the high-frequency alternating inductive reactance of the conductive ink layer is reduced (or reversed), which is used for various product processes. Such as 5G and 6G antennas containing bridge-island structure conductive material ink layers, and the huge amount of small patches produced by roll-to-roll production, etc.
[0002] The conductive ink layer and auxiliary functional layer of the bridge-island design can be dyed when necessary, or bleached by physical and chemical methods such as electrons, light, and heat to restore the original colorless and transparent ink layer;
[0003] Conductive material membrane material of bridge-island design, wherein each conductive material layer thickness is ≤100μm, and the conductive material content is 50-99.9%;
[0004] When the conductive material membrane material of bridge-island design is used in electronic printing product technology, the conductive material content of each conductive material layer is 50-99.9%, and the thickness of the conductive material transfer ink layer is ≤50μm.
[0005] Conductive materials in the form of nano-micron-sized flakes, spheres, and granules of conductive material films include organic, inorganic, and semiconductor conductors, such as conductive polymers, indium tin oxide (ITO), F-doped tin oxide (FTO), Al-doped zinc oxide (AZO), graphene microsheets, graphene oxide, carbon nanotubes, nano-copper, gold, and silver, etc.
[0006] The main test methods for the conductive properties of conductive membrane materials are: GB / T 3048.3-2007, GB / T1410-2006, GB / T 15662-1995, ASTM D257-07, 14, etc. These test methods only obtain the DC surface resistance (square resistance, sheet resistance) and DC volume resistance of the conductive properties of the membrane material under DC conditions. It is known that conductive membrane materials also have the physical phenomenon of capacitive conduction, and its principle has been adopted by a variety of high-tech process means for products.
[0007] In addition to the ohmic conductivity and capacitive conductivity of the conductive layer of the conductive material film material, there is also the phenomenon of inductive conductivity (inductive reactance). According to its formation mechanism, the present application designs the bridge island type composed of the conductive material for its main conductive material ink layer, reduces the alternating current impedance of the conductive ink layer, and is used for the process innovation of printed electronic products.
[0008] The higher the frequency of the current passing through the conductive layer of the conductive material film, the greater the inductive reactance. In 5G and 6G ultra-high frequency matrix circuits, switch electrode circuits, antennas and other circuits, inductive reactance is an extremely serious objective problem. In the 5G and 6G era, the number of transmitting and receiving antennas is not counted by root, but by "array", that is, large-scale "multiple-input multiple-output" multi-antenna technology (MIMO-Multiple-Input Multiple-Output). One of the applications of bridge-island conductive film is electronic printing (resonant cavity ring, microstrip antenna) patch. When the conductive material adopts a bridge-island structure design, its inductive reactance to ultra-high frequency conduction can be reduced. The market is huge and will last forever.
[0009] The highlight of the bridge-island design is that the bridge-island conductive film has the highest cost-effectiveness. (
[0021] -5); it can be hot-melt pressed, bonded, composited or electronically transferred, and can be photo-, thermally, electronically cured and etched. Background Art
[0010] The main characterizations of the conductive properties of the membrane materials of conductive substances and their test methods are: GB / T3048.3-2007, GB / T1410-2006, GB / T 15662-1995, ASTM D257-07, 14, etc. These test methods only obtain the DC surface resistance (square resistance, sheet resistance) and DC volume resistance of the conductive properties of the membrane materials under DC conditions. It is known that the conductive membrane materials also have the physical phenomenon of capacitive conduction, and its principle has been adopted by a variety of high-tech process means.
[0011] To the best of the applicant’s ability, the recent patent documents in this field mainly include:
[0012] 1. CN201610244164-Manufacturing of a transparent film-Application for publication;
[0013] 2. KR20190069102(A)-TRANSPARENT CONDUCTIVE FILM AND TOUCH PANEL USING THE SAME transparent conductive film and touch panel;
[0014] 3. KR20190073605(A)-CONDUCTIVE FILM AND PRODUCTION METHOD THEREFOR Conductive film and production method thereof;
[0015] 4. CN201110032154-A thermal transfer conductive foil and its preparation method-approval authorization;
[0016] The above-mentioned film materials (conductive films) of conductive substances lack the main characteristic of "conductivity" as shown in
[0012] , and there are no innovative solutions to improve "conductivity". Some of them cannot even be formed into ink and cannot generate practical conductive films.
[0017] CN201110032154-A thermal transfer conductive foil and its preparation method, is a decades-long application style of "using numerical arrangement and combination as its independent claim". Its independent claim states "the thickness of the transfer layer is 2-20μm" and "the transfer layer is composed of 40-90% by mass of a connecting material, 10-60% by mass of a conductive material and 0-5% by mass of an auxiliary agent"; its dependent claim states "the connecting material is dissolved in..., and then the conductive material and the auxiliary agent are added and crushed to a particle size of less than 5μm to obtain a transfer layer ink"...
[0018] The world has long entered the era where the conductive material in the conductive layer accounts for almost 100% and the conductive layer is nanometer-micrometer thick;
[0019] It is common sense that nano-micron conductive materials, especially nano-filaments, are not allowed to be crushed or mechanically stirred when making ink;
[0020] As one of the electronic printing materials, the film material (conductive film) of conductive substances mainly represents the innovation of improving "conductivity" and cost performance, which is the main theme. Without the "conductivity" representation, there is no innovation if it only "takes the numerical arrangement and combination as its independent claim";
[0021] Conductive materials in nanometer and micron form have a very large specific surface area, and their high surface energy makes them always tend to shrink and agglomerate, which is not a "crush" problem. Therefore, overcoming the wrinkles, disorder, shrinkage and agglomeration of conductive materials is a hurdle that cannot be circumvented in various conductive films, which is the primary factor that determines the conductive performance of conductive films. Without this point, the so-called innovation does not exist.
[0022] The present application proposes that: in addition to the ohmic conductivity and capacitive conductivity of the conductive layer of the conductive material film material, there is also the phenomenon of inductive conductivity (inductive reactance). The bridge-island conductive material film material, referred to as the bridge-island conductive film, is composed of a base film, a conductive material ink layer and necessary auxiliary functional layers. It is one of the methods for the conductive material film material to overcome the inductive reactance, improve the comprehensive conductivity and improve the cost performance of the conductive film.
[0023] When the conductive material of the conductive material film material is graphene nanosheets, the thickness of the conductive material layer is 8μm; the surface resistance is 16Ω / sq (ASTM D257-07, i.e. parallel rod surface resistance test method). At the same time, using this test method, for the same sample and the same test point, when the input DC power is changed to AC power supply 4MHz, 8MHz, its surface resistance (including DC ohmic resistance, capacitance resistance, and inductive reactance) increases from 16Ω / sq to 21.03Ω / SqLc, 44.0Ω / SqLc. In the parallel rod square resistance measurement, the comprehensive square resistance increases significantly with the increase of frequency! It is known that the capacitance reactance decreases with the increase of frequency, so the inductive reactance that increases with the frequency is objectively undisputed. Different conductive materials and conductive material film materials of different shapes have the phenomenon of inductive conduction (inductive reactance) to varying degrees.
[0024] According to the formation mechanism of inductive reactance, the present application performs a bridge-island design on the conductive ink layer and the conductive material composition to reduce the alternating impedance (or vice versa) of the conductive ink layer for product process innovation.
[0025] The higher the frequency of the current passing through the conductive layer of the conductive material film material, the greater the inductive reactance. In the fields of switch electrode circuits, printed electronics, 5G, 6G ultra-high frequency matrix circuits, massive antenna patches and other products, there will be excellent application prospects, realizing the roll-to-roll (R2R) production of flexible conductive films and their development products. In the 5G and 6G era, the number of transmitting and receiving antennas is not calculated by root, but by "arrays", that is, large-scale "multiple-input and multiple-output" multi-antenna technology (MIMO-Multiple-InputMultiple-Output). Inductive reactance is an extremely serious objective face for transmitting and receiving antennas. One of the applications of bridge-island conductive film is electronic printing (resonant cavity ring, microstrip antenna) patch. When the conductive material adopts a bridge-island structure design, it can reduce its ultra-high frequency conductive inductive reactance, reduce the amount of conductive material used, and have outstanding cost performance. The market is huge and will last forever. Summary of the invention
[0026] In addition to the ohmic conductivity and capacitive conductivity of the conductive layer of the conductive material film material, there is also the phenomenon of inductive conductivity (inductive reactance). The conductive material film material with a bridge-island structure, referred to as the bridge-island conductive film, is composed of a base film, a conductive material ink layer and necessary auxiliary functional layers. It is one of the methods for conductive material film materials to overcome inductive reactance, improve comprehensive conductivity and improve the cost-effectiveness of conductive films. In the fields of switch electrode circuits, printed electronics, NG ultra-high frequency matrix circuits, massive antenna patches and other product fields, it will have excellent application prospects and realize the roll-to-roll (R2R) production of flexible conductive films and their developed products.
[0027] The above-mentioned conductive materials include: organic and inorganic conductors and semiconductors in the form of nanometer and micrometer-sized flakes (including triangular flakes), spheres, olives, and particles (including cubes), such as conductive polymers, indium tin oxide (ITO), F-doped tin oxide (FTO) and Al-doped zinc oxide (AZO), graphene microsheets, silver-plated nanographite microsheets, graphene oxide, carbon nanotubes, nano-copper, gold, and silver, etc., or their physical and chemical modified structures.
[0028] Conductive materials in nano-micron form have a very large specific surface area, and their high surface energy makes them always tend to shrink and agglomerate. Therefore, overcoming the disordered wrinkles and shrinkage and agglomeration of conductive materials is a hurdle that cannot be circumvented in the production of various conductive films, which is the primary factor that determines the conductive performance of the conductive film. The conductive material film material composed of graphene microsheets with a non-bridge island conductive material film material structure has three-dimensional random physical contact points (see the accompanying drawings
[0025] Table 1: Figure 1), and the conductive microcurrent does not move in a straight line, but has a curved forward part (Figure 1, ①→④). This three-dimensional microscopic curvature is large, that is, it forms an inductive reactance at high frequencies. Different conductive materials and conductive material film materials of different shapes all have the phenomenon of inductive conduction (inductive reactance) to varying degrees.
[0029] The number of effective physical contact points of the micro-sheet conductive material and the curvature of the micro-current determine the main conductive properties of the conductive film, especially at high frequencies. When the "wrinkle disorder, shrinkage and agglomeration" overcomes the disadvantages, the number of effective physical contact points decreases, the curvature of the conductive micro-current is large, so the ohmic resistance increases, and the inductive resistance also increases.
[0030] Description of the drawings,
[0026] Table 2: Figure 2 is a schematic diagram of the structure of the bridge-island type conductive material film. The micro-sheet (island, bridge seat) conductive material and the filament (bridge) conductive material are combined according to the following principles:
[0031] 1. Under the same nano-micron-level film-forming conditions, the coverage rate of filamentous conductive materials and micro-sheet conductive materials is different, and the proportion of filamentous conductive materials is small (
[0021] -5, the relationship between iron ropes and floor boards);
[0032] 2. There are different methods to reduce "wrinkle disorder, shrinkage and agglomeration" and reduce micro-current bending at effective physical contact points in the film-forming process of filamentous conductive materials and micro-sheet conductive materials;
[0033] 3. The filamentous conductive material is easier to stretch than the micro-sheet conductive material, and the micro-current bending at the effective physical contact point is small;
[0034] 4. The micro-sheet conductive material has a large area and can serve as an island or bridge seat for the filamentous conductive material, thereby increasing the effective physical contact points and playing a parallel role in the micro-current, effectively reducing the bending of the micro-current at the physical contact points. (
[0026] Table 2, Figure 2, 1b-2b; 1a-4a);
[0035] 5. Focus on "cost-effectiveness" and take into account comprehensive performance and practicality. The creativity and methods of the bridge-island design (
[0017] -
[0023] ) of the conductive film must be based on the high "cost-effectiveness" requirements of the conductive film. The 24 iron ropes of the Dadu River can be used as a bridge for thousands of troops, so there is no need to build dams or fill the river. For example, after the sintering of a sufficiently large mass (layer thickness) of nanosilver photons, the inductive reactance of its surface resistance may be negligible, but this is the way it should be for non-conductive films.
[0036] This can help us understand the bridge-island design of the conductive film in a simple and intuitive way: filamentous conductive materials cannot be straightened and paralleled like the iron ropes (wires, bridges) of the Dadu River (bending forward, inductive reactance). A small amount of sheet-like conductive materials (boards on the iron ropes, islands) will have a greater parallel effect on the filamentous conductive materials (iron ropes) (reducing micro-current bending). The key to design is to control the amount and orientation of filamentous and sheet-like conductive materials, overcome the disordered wrinkling and shrinkage of conductive materials, and strive for effective physical contact points of conductive materials.
[0037] In this way, 1-5, the coordinated effect of the bridge and the island is 1+1>2, which complement each other.
[0038] Conductive film, a membrane material of bridge-island conductive material that can overcome the surface inductive reactance of the conductive film, referred to as bridge-island conductive film. It consists of a base film, a conductive material ink layer and necessary auxiliary functional layers; it has multiple product process application forms such as composite, photolithography, electronic printing, anisotropy, electromagnetic, electrode, etc., which are suitable for the roll-to-roll (R2R) production of flexible conductive film and its secondary products. Its organic, inorganic, and semiconductor conductive material ink layer is a multi-dimensional overlapping structure of nano-micron filamentary conductive material and at least another sheet (including triangular sheet), spherical, olive-shaped, granular (including cube) and other conductive materials. By constructing bridge-island physical contact (sintering) points for conductive materials of different shapes, the direction of microscopic current flow is controlled, and the high-frequency alternating inductive reactance of the conductive ink layer is reduced (or used in reverse), which is used for various product processes. The so-called "reducing the high-frequency alternating inductive reactance of the conductive ink layer (or using it in reverse)" means that the high-frequency alternating inductive reactance of the conductive ink layer can also be increased in some applications. In this way, the resonant cavity frequency or bandwidth of printed electronics can be changed by reducing or increasing the inductance.
[0039] Figure 3: Figure 3, in the schematic diagram of various bridge-island type conductive material film structures (
[0027] ), spherical, olive-shaped, granular (including cubic) conductive materials (Figures 3-7, 8), a small amount of which is added to the bridge-island type conductive material film structure of Figure 2 also plays the role of "island", which is beneficial to reduce the contact resistance of the physical contact points of the pressure bonding when the bridge-island type conductive material film has the process requirements of hot melting and pressure bonding. Such as the hot melting and pressure bonding process of solder joints, electrodes, wiring electrodes, and anisotropic films.
[0040] The film material of bridge-island conductive material for roll-to-roll coating or special electronic printing and its film forming process tooling are designed according to the principles of
[0021] 1-5. Thus:
[0041] 1. The conductive ink layer and auxiliary functional layer of the bridge-island design can be dyed (by adding reactive acidic or alkaline dyes, dispersed or vat dyes, active dyes or their intermediates, etc.) when necessary, or bleached by physical and chemical methods such as electrons, light, and heat to restore the colorless transparency of the original ink layer;
[0042] 2. Bridge-island design of conductive material membrane material, where each conductive material layer thickness is ≤100μm, and the conductive material content is 50-99.9%;
[0043] 3. When the bridge-island design conductive material membrane material and electronic printing material product process are used, the conductive material content of each conductive material layer is 50-99.9%, and the conductive material transfer ink layer thickness is ≤50μm. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] Table 1: Figure 1, schematic diagram of the structure of non-bridge island conductive material membrane
[0045]
[0046] Figure 1: Non-bridge island conductive material Table 1-1 Conductive material nano-micron sheet, is a single or multi-shaped conductive material, an area conductive structure formed during film material coating or electronic printing, sintering, and active control;
[0047] Table 1-2①→④ physical conductive contact points are micro-current flow table 1-3. Micro-current flow table 1-3①→④ is curved and open, longer than the macroscopic straight current path in Table 1-5, and has different effects on high-frequency electromagnetic waves cutting magnetic lines of force and impedance (inductive reactance) of high-frequency current passing through;
[0048] Table 1-4 are invalid physical contact points (virtual, non-conductive).
[0049] Table 1-3 effective physical contact points and Table 1-4 invalid physical contact points refer to conductive or non-conductive points formed during film material coating, electronic printing, curing and sintering, or active control. Active control refers to the change of conductive state of effective or invalid physical contact points and controlled bridge island structure when conductive materials (in whole or in part) are subjected to sound waves, pressure, electromagnetic force, etc.
[0050] Table 2: Figure 2, schematic diagram of bridge island type conductive material membrane structure
[0051]
[0052] Figure 2: Non-bridge island conductive material Table 2-1 is the shape of nano-micron sheets (referred to as islands in this application), Table 2-4 is nano-micron conductive filaments, lines, and strips (referred to as bridges in this application). In Table 2-2, 1b→2b, 1a→4a are their physical contact points, and Table 2-5 is the direction of micro-currents flowing through these physical contact points. Table 2-3 is the invalid physical contact point. Table 2-6 is the direction of macroscopic currents.
[0053] Table 2-4 and Table 2-1 also form the micro-current conduction pattern of "wire (ribbon)"-"bridge" and "surface"-"island" and "bridge-island" type conductive material film materials through the combination, coating, electronic printing, curing sintering, or active control of conductive materials. The role of the "bridge" is mainly in series conduction, and the role of the "island" is mainly in parallel conduction. The combined effect is to reduce or increase the curvature, tortuosity, opening degree, inductive reactance, etc. of the micro-current flow direction, so that the resonant cavity frequency or bandwidth of printed electronics can be controlled.
[0054] Table 3: Figure 3, schematic diagram of various bridge-island conductive material membrane structures
[0055]
[0056] Table 3, 1-6 of the attached figure 3 is the same as Table 2, 1-6 of the attached figure 2. Table 3, 7-8 of the attached figure 3 are spherical conductors, see
[0023] for details. Table 3, 7-8 are non-sheet-shaped spherical conductors, which can also form "wires (ribbons)"-"bridges" and "surfaces"-"islands" in film material coating, electronic printing, curing and sintering, or active control, which is related to the process formula (see above). DETAILED DESCRIPTION
[0057] Example 1, Bridge-island type conductive film basic process (dyeing / transparent / bleaching)
[0058] 1. Base film: PI, PET, 4.6μm, 12μm, 72-200μm;
[0059] 2. Conductive materials: Nanosilver wire methanol dispersion, produced by Zhejiang Kechuang, wire diameter 25-30nm, length 20-40μm, purity >99.5%; Nanosilver flake methanol dispersion, produced by Qiming, Nanhai, Guangdong, diameter 500nm, thickness 20-30nm; Nanosilver ball, Shanghai Pantian powder material particle size 50nm.
[0060] 3. Primer: Homemade, acrylic mixture, mixed solvent dispersion, highly transparent, dyed red. Dry film melting point 70-80℃, primer has strong initial adhesion to silver wire.
[0061] 4. Primer application: slightly concave, layer thickness 0.5-1μm;
[0062] 5. Silver wire coating (bridge), pre-feeding, dispersion and pre-orientation in a slope flow manner; multi-oriented micro-concave coating on the base glue, 100-200mg / m 2 ; Apply silver wire twice to make the silver wire oriented 45° to the left and right sides along the longitudinal direction of the base film. Drying, dry film surface resistance 2-50Ω / sq; Photon sintering, dry film surface resistance 1-20Ω / sq, (ASTM D257-07, parallel rod surface resistance test method). For the same sample and the same test point, when the input DC power is changed to AC power supply 8MHz, its surface resistance (including DC ohmic resistance, capacitance resistance, and inductance) increases to 3-30Ω / Sq LC .
[0063] 6. Nano-silver flakes (islands) are coated with slope flow narrow slits for pre-feeding, dispersion and pre-orientation; multiple oriented micro-concave coating is applied on the nano-silver wire layer, 100-200 mg / m 2 ; Drying, dry film resistance 0.5-15Ω / sq; Photon sintering, dry film resistance 0.1-10Ω / sq, (ASTM D257-07, parallel rod resistance test method). For the same sample and the same test point, when the input DC power is changed to AC power 8MHz, its resistance (including DC ohmic resistance, capacitance resistance, and inductance) increases to 0.5-10Ω / Sq LC .
[0064] 7. Apply silver balls (islands) and apply additional coatings as required by the application.
[0065] 8. The dyeing of the above glue can be faded and bleached during photon sintering, EB and UV curing.
[0066] Example 2: Electronic printing application of bridge-island conductive film
[0067] One of the applications of bridge-island conductive film is electronic printing (resonant cavity ring, microstrip antenna) patch. When the conductive material adopts the bridge-island structure design, its ultra-high frequency conductive inductance can be reduced.
[0068] 1. Base film: PI heat sealing film, heat sealing temperature 90 / 135℃;
[0069] 2. Bridge-island conductive film: base film PE T, 4.6μm, 12μm,
[0028] Example 1, bridge-island conductive film basic process, not cross-linked and cured. Bridge-island conductive film electronic transfer to PI heat sealing film, temperature 70-80℃.
[0070] 3. Bridge-island conductive film - R2R rotary printing electrode matrix film: electric, oil and other internal heating relief rollers, R2R rotary printing. Depending on the application needs, it can be transferred and laminated multiple times, or processed twice.
Claims
1. A film material of bridge-island type conductive material, characterized in that: It consists of a base film, a conductive material ink layer and necessary auxiliary functional layers. The conductive material ink layer can be an organic, inorganic or semiconductor conductive material ink layer. The conductive material ink layer is a multi-dimensional overlapping structure of nano-micron filamentous conductive material and triangular-containing sheet-shaped, spherical, olive-shaped or cubic granular conductive material. The film material has the product process application forms of composite, photolithography, electronic printing, anisotropy, electromagnetic, and electrode, and is suitable for roll-to-roll production of flexible conductive films and their secondary products. Through the combination, coating, printed electronics, curing sintering, or active control of conductive materials, micro-current conduction types of "wire"-"bridge", "surface"-"island", and "bridge-island" conductive material film materials are formed: the role of the "bridge" is mainly in series conduction, and the role of the "island" is mainly in parallel conduction; The membrane material of the conductive substance has the "bridge island" type inductive reactance phenomenon, which is characterized by the size and change of the "square resistance" measured by the conductive ink layer of the membrane material under alternating current; By synthesizing the "bridge island" type microcurrent conductive pattern of this membrane material, its physical contact points can be changed and the direction of microcurrent flow can be controlled, thereby reducing or increasing the curvature, diameter, and opening degree of the microcurrent flow direction. The high-frequency alternating inductance of the conductive ink layer can be used for various product processes.
2. The film material of bridge-island type conductive material according to claim 1, characterized in that: The "active control" mentioned above means that all or part of the bridge-island type conductive material can be affected by sound waves, pressure, and electromagnetic forces to change the conductive state of effective or invalid physical contact points and the changes in the controlled bridge-island structure, so that the resonant cavity frequency or bandwidth of the printed electronic circuit can be controlled.
3. The film material of bridge-island type conductive material according to claim 1, characterized in that: The bridge-island type conductive material ink layer and the auxiliary functional layer can be dyed when necessary, or bleached by physical and chemical methods to restore the color and transparency of the original ink layer.
Citation Information
Cited By
NC60 + fullerene aerolite radar communication antenna
CN122136623A