Method for manufacturing semiconductor device and electrostatic discharge device

By alternately stacking epitaxial layers on the semiconductor substrate and injecting dopants, combined with dummy gates and metal gate stacks, the compatibility problem of backside power rail formation in multi-gate processes is solved and ESD protection is enhanced effect and improve device integration.

CN113471147BActive Publication Date: 2024-10-29TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202110654703.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-06-11
Publication Date
2024-10-29
Estimated Expiration
2041-06-11

AI Technical Summary

Technical Problem

Existing multi-gate transistor processes are difficult to be compatible with and support the formation of backside power rails, resulting in the loss of current paths in ESD devices during the backside thinning process, making it impossible to effectively protect integrated circuits from electrostatic discharge damage.

Method used

The fin structure is formed by alternately stacking epitaxial layers of different material compositions on the semiconductor substrate, and different types of dopants are injected into different areas thereof to form first and second contacts, matching the dummy gate and the metal gate. Stack the components to enhance ESD current conductivity, and after the backside substrate is thinned, a dielectric layer is deposited and a backside trench is formed to enhance the current path.

Benefits of technology

An ESD protection device compatible with the multi-gate process is realized, which enhances the current conductivity of electrostatic discharge, reduces parasitic capacitance, supports the formation of backside metal wiring layers, and improves device integration.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113471147B_ABST
    Figure CN113471147B_ABST
Patent Text Reader

Abstract

The present invention provides a method for manufacturing a semiconductor device. The method includes providing a structure having a front side and a back side, the structure including a substrate and a stack of first type epitaxial layers and second type epitaxial layers of different material compositions alternately stacked on the substrate, wherein the stack is located at the front side of the substrate and the substrate is located at the back side of the structure; patterning the stack to form a fin on the substrate; injecting a first dopant into a first region of the fin, the first dopant having a first conductivity type; injecting a second dopant into a second region of the fin, the second dopant having a second conductivity type opposite to the first conductivity type; forming a first contact on the first region, and forming a second contact on the second region. Embodiments of the present invention also relate to an electrostatic discharge device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] Embodiments of the present invention relate to a method of manufacturing a semiconductor device and an electrostatic discharge device. Background Art

[0002] The semiconductor integrated circuit (IC) industry has experienced exponential growth. Technological advances in IC materials and design have produced multiple generations of ICs, each with smaller and more complex circuits than the previous generation. Over the course of IC evolution, functional density (i.e., the number of interconnected devices per chip area) has generally increased, while geometry size (i.e., the smallest component (or line) that can be produced using a manufacturing process) has decreased. This scaling down process generally provides benefits by increasing production efficiency and reducing associated costs. This scaling down has also increased the complexity of processing and manufacturing ICs.

[0003] For example, as IC technology moves to smaller technology nodes, multi-gate devices have been introduced to improve gate control by increasing gate-channel coupling, reducing off-state current, and reducing short channel effects (SCE). A multi-gate device generally refers to a device having a gate structure or portion thereof disposed on more than one side of a channel region. A gate-all-around (GAA) transistor is an example of a multi-gate device, which has become a popular and promising candidate for high-performance and low-leakage applications. The GAA transistor is named for its gate structure, which can extend around the channel region, providing access to the stacked semiconductor channel layers on four sides. This configuration provides better channel control and greatly reduces SCE (particularly by reducing subthreshold leakage) compared to planar transistors.

[0004] IC includes semiconductor devices with different functions, such as core functions and electrostatic discharge (ESD) functions. These different functions require semiconductor devices to have different structures. At the same time, it is advantageous to have similar processes and similar process windows to manufacture these different semiconductor devices to reduce costs and improve yields. Although existing multi-gate (e.g., GAA) transistors and processes are generally sufficient for their intended purposes, they are not completely satisfactory in every aspect. For example, in the development of ICs, in addition to front-side interconnects, back-side power rails have been introduced to increase the number of metal rails that can be used for greater power drive capabilities and simplified metal routing. How to form an ESD device (e.g., ESD diode) that is compatible with multi-gate processes and also supports the formation of back-side power rails is a challenge faced by the semiconductor industry. The present invention is intended to solve the above problems and other related problems. Summary of the invention

[0005] An embodiment of the present invention provides a method for manufacturing a semiconductor device, comprising: providing a structure having a front side and a back side, the structure comprising a substrate and a stack of first type epitaxial layers and second type epitaxial layers with different material compositions alternately stacked on the substrate, wherein the stack is located at the front side of the structure and the substrate is located at the back side of the structure; patterning the stack to form a fin on the substrate; injecting a first dopant into a first region of the fin, the first dopant having a first conductivity type; injecting a second dopant into a second region of the fin, the second dopant having a second conductivity type opposite to the first conductivity type; and forming a first contact on the first region and a second contact on the second region.

[0006] Another embodiment of the present invention provides a method for manufacturing a semiconductor device, comprising: forming a fin protruding from a semiconductor substrate, wherein the fin comprises a first type epitaxial layer and a second type epitaxial layer located on the semiconductor substrate, the first type epitaxial layer and the second type epitaxial layer having different material compositions and being alternately arranged in a vertical direction; forming a first gate structure and a second gate structure above the fin; doping a first region of the fin with a first dopant of a first conductivity type; doping a second region of the fin with a second dopant of a second conductivity type opposite to the first conductivity type, wherein the first region and the second region are located between the first gate structure and the second gate structure; forming a dielectric layer on the side walls of the first gate structure and the second gate structure; forming a contact hole in the dielectric layer, the contact hole exposing the first region and the second region; and forming a conductive contact in the contact hole.

[0007] Another embodiment of the present invention provides an electrostatic discharge (ESD) device, comprising: a semiconductor substrate; a stack of a first type epitaxial layer and a second type epitaxial layer, located on the semiconductor substrate, the first type epitaxial layer and the second type epitaxial layer having different material compositions, and the first type epitaxial layer and the second type epitaxial layer are alternately arranged in a vertical direction; a first injection region in the stack, wherein the first injection region has a first conductivity type; and a second injection region in the stack, wherein the second injection region has a second conductivity type opposite to the first conductivity type. BRIEF DESCRIPTION OF THE DRAWINGS

[0008] The present invention can be best understood from the following detailed description when read in conjunction with the accompanying drawings. It should be emphasized that, in accordance with standard practice in the industry, the various components are not drawn to scale and are only used for illustrative purposes. In fact, the size of the various components may be arbitrarily increased or reduced for clarity of discussion.

[0009] Figure 1A , Figure 1B and Figure 1C A flow chart of a method of forming a semiconductor structure having an ESD device and a backside power rail according to various aspects of the present invention is shown.

[0010] Figure 2 , Figure 3 and Figure 4 According to some embodiments of the present invention, Figures 1A to 1C A perspective view of a portion of a semiconductor structure during a manufacturing process.

[0011] Figure 5A , Figure 5B , Fig.16A and Fig. 16B According to some embodiments of the present invention, Figures 1A to 1C A top view of a portion of a semiconductor device during a manufacturing process.

[0012] Fig. 6A , Fig. 7A , Fig. 8A , Fig.9A , Fig. 10A , Fig.11A , Fig. 12A , Fig.13A , Fig.14A , Fig.15A , Fig.17A , Fig.18A , Fig.19A , Fig. 20A , Fig.21A , Fig.22A and Fig.23A According to some embodiments of the present invention, Figures 1A to 1C The method during the manufacturing process Figure 5A A cross-sectional view of a portion of the semiconductor device along line AA.

[0013] Figure 6B , Figure 7B , Figure 8B , Fig. 9B , Fig. 10B , Fig. 11B , Fig. 12B , Fig. 13B , Fig. 14B , Fig. 15B , Fig. 17B , Fig.18B , Fig.19B , Fig. 20B , Fig.21B , Fig. 22B and Fig. 23B According to some embodiments of the present invention, Figures 1A to 1C The method during the manufacturing process Figure 5A BB line is a cross-sectional view of a portion of the semiconductor device in FIG. DETAILED DESCRIPTION

[0014] The following disclosure provides many different embodiments or examples for realizing the different features of the provided subject matter. Specific examples of components and arrangements are described below to simplify the present invention. Of course, these are only examples and are not intended to be limiting. For example, in the following description, forming a first component above or on a second component may include an embodiment in which the first component and the second component are directly contacted, and may also include an embodiment in which an additional component may be formed between the first component and the second component so that the first component and the second component may not be in direct contact. In addition, the present invention may repeat reference numbers and / or letters in various examples. This repetition is for the purpose of simplicity and clarity, and does not itself indicate the relationship between the individual embodiments and / or configurations discussed.

[0015] In addition, for ease of description, spatially relative terms such as "below", "beneath", "lower", "above", "upper", etc. may be used herein to describe the relationship of one element or component to another element or component as shown in the figures. Spatially relative terms are intended to include different orientations of the device in use or operating processes in addition to the orientation shown in the figures. The device can be positioned in other ways (rotated 90 degrees or in other orientations), and the spatially relative descriptors used herein can be interpreted accordingly. Further, according to the specific technology disclosed herein, according to the knowledge of those skilled in the art, unless otherwise stated, when "about", "approximately", etc. are used to describe a numerical value or a numerical range, the term covers numerical values ​​within certain variations (such as + / -10% or other variations) of the described numerical value. For example, the term "about 5nm" can cover a size range from 4.5nm to 5.5nm, from 4.0nm to 5.0nm, etc.

[0016] The present application relates generally to semiconductor structures and manufacturing processes, and more particularly to an electrostatic discharge (ESD) protection device compatible with a multi-gate transistor process flow and a method for manufacturing the same.

[0017] As is well known, extremely high voltages may be generated near an integrated circuit (IC) due to the accumulation of static charge. A high potential may be generated to an input or output buffer of an integrated circuit, which may be caused by a person touching a package pin that is in electrical contact with the input or output buffer. When the electrostatic charge is discharged, a high current is generated at the package node of the integrated circuit, and is called electrostatic discharge (ESD). ESD is a serious problem for semiconductor devices because it has the potential to destroy the entire integrated circuit. The duration of the ESD transient is very short, typically in the nanosecond range, and conventional circuit breakers cannot react quickly enough to provide adequate protection. Therefore, it has become a known practice to incorporate ESD devices into ICs. In various embodiments, the IC may have multi-gate transistors (e.g., full-ring gate (GAA) transistors and / or FinFET transistors) placed in a core area that provides core functions (e.g., logic and memory applications) and ESD devices placed in an ESD area that provides ESD protection.

[0018] However, in addition to the interconnect structures (which may also include power rails) on the front side (or front) of the structure, a recent trend in IC development includes providing power rails (or power routing) on ​​the back side (or back side) of the structure containing the transistor. This increases the number of metal rails in the structure that can be used to directly connect to the source / drain contacts and vias. It also increases the gate density to achieve greater device integration compared to existing structures without backside power rails. The backside power rail can have a size that is wider than the first level metal (M0) rail on the front side of the structure, which advantageously reduces the resistance of the power rail. Unfortunately, this approach faces design and process problems. In particular, the backside thinning process when removing the bulk semiconductor substrate substantially eliminates the current path for ESD devices including multiple fin elements. Therefore, there is a need in the art for an ESD protection device whose formation process is compatible with the formation of a multi-gate process flow while overcoming the deficiencies of the prior art.

[0019] The details of the structure and manufacturing method of the present invention are described below in conjunction with the accompanying drawings, which show the process of manufacturing GAA devices in the core area and manufacturing ESD devices in the ESD area according to some embodiments. GAA devices refer to devices with vertically stacked horizontally oriented multi-channel transistors, such as nanowire transistors and nanosheet transistors. Due to the better gate control capability, lower leakage current and full FinFET device layout compatibility of GAA devices, GAA devices are promising candidates for pushing CMOS to the next stage of the roadmap. For simplicity, the present invention uses GAA devices as an example. Those of ordinary skill in the art should understand that they can easily use the present invention as a basis for designing or modifying other processes and structures (such as FinFET devices) to achieve the same purposes and / or achieve the same advantages introduced herein.

[0020] Figures 1A to 1C 1 shows a method 100 of semiconductor fabrication, including forming a multi-gate transistor together with an ESD device (e.g., an ESD diode). The method 100 is merely an example and is not intended to limit the present invention to that expressly recited in the claims. Additional operations may be provided before, during, and after the method 100, and some of the operations described may be replaced, eliminated, or moved for additional embodiments of the method. Figures 2 to 23B Method 100 is described. For clarity, the Figures 2 to 23B To better understand the inventive concept of the present invention. Figures 2 to 4 A perspective view of a semiconductor device (or device or structure) 200 is shown according to various stages of method 100 . Figure 5A , Figure 5B , Fig.16A and Fig. 16B A top view of a device 200 is shown according to various stages of method 100 . Fig. 6A , Fig. 7A , Fig. 8A , Fig.9A , Fig. 10A , Fig.11A , Fig. 12A , Fig.13A , Fig.14A , Fig.15A , Fig.17A , Fig.18A , Fig.19A , Fig. 20A , Fig.21A , Fig.22A and Fig.23A The various stages of the method 100 are shown. Figure 5A FIG. 2 is a cross-sectional view of a portion of the device 200 along line AA, where line AA is located in a channel region of the GAA transistor and along a longitudinal direction of a channel layer of the GAA transistor. Figure 6B , Figure 7B , Figure 8B , Fig. 9B , Fig. 10B , Fig. 11B , Fig. 12B , Fig. 13B , Fig. 14B , Fig. 15B , Fig. 17B , Fig.18B , Fig.19B , Fig. 20B , Fig.21B , Fig. 22B and Fig. 23B Shows Figure 5A FIG. 2 is a cross-sectional view of a portion of the device 200 along line BB, where line BB is along a longitudinal direction of a fin element (or fin) in the ESD device.

[0021] In some embodiments, device 200 is part of an IC chip, a system on a chip (SoC), or a portion thereof, including various passive and active microelectronic devices, such as resistors, capacitors, inductors, diodes, p-type field effect transistors (PFETs), n-type field effect transistors (NFETs), FinFETs, nanosheet FETs, nanowire FETs, other types of multi-gate FETs, metal oxide semiconductor field effect transistors (MOSFETs), complementary metal oxide semiconductor (CMOS) transistors, bipolar junction transistors (BJTs), laterally diffused MOS (LDMOS) transistors, high voltage transistors, high frequency transistors, memory devices, other suitable components, or combinations thereof. Additional components may be added to device 200, and some of the components described below may be replaced, modified, or eliminated in other embodiments of device 200.

[0022] In operation 102 ( Figure 1A ) is provided (or provided with) a device 200. Figure 2 , the device 200 includes a region I for forming transistors and a region II for forming ESD devices. The transistors formed in region I are used for core applications, such as for forming logic circuits, memory circuits, and other core circuits. The ESD devices (such as ESD diodes) formed in region II are used to protect the device 200 from electrostatic discharge events. The device 200 includes a substrate 202 and an epitaxial stack 204 located on the substrate 202. The substrate 202 and the epitaxial stack 204 extend continuously from region I to region II. In addition, a hard mask (HM) layer 212 is formed above the epitaxial stack 204.

[0023] In some embodiments, substrate 202 is a semiconductor substrate such as a silicon substrate. Substrate 202 may include various layers, including a conductive layer or an insulating layer formed on the semiconductor substrate. In the illustrated embodiment, substrate 202 includes a dielectric capping layer 203. In some embodiments, dielectric capping layer 203 is an oxide layer. Dielectric capping layer 203 may be deposited using chemical vapor deposition (CVD), atomic layer deposition (ALD), physical vapor deposition (PVD), or oxidation. Dielectric capping layer 203 divides substrate 202 into a top substrate portion 202a and a bottom substrate portion 202b. In some embodiments, dielectric capping layer 203 is used as an etch stop layer or a chemical mechanical polishing (CMP) stop during a backside thinning process.

[0024] Depending on design requirements known in the art, the substrate 202 may also include various doping configurations. For example, different doping profiles (e.g., n-well, p-well) may be formed in regions designed for different device types (e.g., n-type field effect transistor (N-FET), p-type field effect transistor (P-FET)) on the substrate 202. Suitable doping may include ion implantation and / or diffusion processes of dopants. The substrate 202 may have isolation features (e.g., shallow trench isolation (STI) features) inserted into regions that provide different device types. The substrate 202 may also include other semiconductors, such as germanium, silicon carbide (SiC), silicon germanium (SiGe), or diamond. Optionally, the substrate 202 may include a compound semiconductor and / or an alloy semiconductor. In addition, the substrate 202 may optionally include an epitaxial layer (epi layer), may be strained for performance enhancement, may include a silicon on insulator (SOI) structure, and / or may have other suitable enhancement features.

[0025] The epitaxial stack 204 includes an epitaxial layer 208 of a second component inserted between an epitaxial layer 206 of a first component. The first component and the second component may be different. The epitaxial layer 208 may include the same component as the substrate 202. In the embodiment shown, the epitaxial layer 206 is silicon germanium (SiGe) and the epitaxial layer 208 is silicon (Si). However, other embodiments are also possible, including those that provide a first component and a second component with different oxidation rates and / or etching selectivities. For example, in some embodiments, either the epitaxial layer 206 of the first component or the epitaxial layer 208 of the second component may include other materials, such as germanium; compound semiconductors, such as silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, and / or indium antimonide; alloy semiconductors, such as SiGe, GaAsP, AlInAs, AlGaAs, InGaAs, GaInP, and / or GaInAsP; or combinations thereof. In some embodiments, the epitaxial layers 206 and 208 are substantially dopant-free (i.e., having approximately 0 cm -3 About 1×10 17 cm -3 The epitaxial layer 206 of the first component or the epitaxial layer 208 of the second component may be formed by a molecular beam epitaxy (MBE) process, a metal organic chemical vapor deposition (MOCVD) process, and / or other suitable epitaxial growth processes. In various embodiments, the substrate 202 is a crystalline substrate, the epitaxial layers 206, 208 are crystalline semiconductor layers, and the epitaxial stack 204 is formed as a superlattice structure.

[0026] In some embodiments, the thickness of each epitaxial layer 206 is in the range of about 2 nanometers (nm) to about 6nm. The thickness of the epitaxial layer 206 can be substantially uniform. Still in the embodiment shown, the top epitaxial layer 206 is thinner (e.g., half the thickness) than the other epitaxial layers 206 below. In some embodiments, the thickness of each epitaxial layer 208 is in the range of about 6nm to about 12nm. In some embodiments, the thickness of the epitaxial layer 208 of the stack is substantially uniform. As described in more detail below, the epitaxial layer 208 or a portion thereof can form a channel layer of a subsequently formed GAA transistor in region I, and the thickness is selected based on transistor performance considerations. The term channel layer is used herein to refer to any material portion of a channel in a transistor having nanometer-scale or even micrometer-scale dimensions and having an elongated shape, regardless of the cross-sectional shape of the portion. Therefore, the term refers to both circular and substantially circular cross-sectional elongated material portions, and also refers to beam-shaped or strip-shaped material portions including, for example, cylindrical or substantially rectangular cross-sections. The epitaxial layer 206 in the channel region may eventually be removed and used to define the vertical distance between adjacent channel components of a subsequently formed multi-gate device, and the thickness is selected based on device performance considerations. Therefore, the epitaxial layer 206 may also be referred to as a sacrificial layer, and the epitaxial layer 208 may also be referred to as a channel layer.

[0027] Note that Figure 2 As shown, three (3) layers of epitaxial layer 206 and three (3) layers of epitaxial layer 208 are arranged alternately. Figure 2 For illustrative purposes only, and are not intended to be limiting to the specific contents recited in the claims. It will be appreciated that any number of epitaxial layers may be formed in the epitaxial stack 204; the number of layers depends on the desired number of channel layers of the device 200. In some embodiments, the number of epitaxial layers 208 is between 2 and 10. It should also be noted that while the epitaxial layers 206, 208 are shown as having a particular stacking order in which the epitaxial layer 208 is the topmost layer of the epitaxial stack 204, other configurations are possible. For example, in some cases, the epitaxial layer 206 may optionally be the topmost layer of the epitaxial stack 204. In other words, the growth order of the epitaxial layers 206, 208, and therefore their stacking order, may be switched, or otherwise switched to be different from that shown in the accompanying drawings while still remaining within the scope of the present invention.

[0028] In the illustrated embodiment, a hard mask (HM) layer 212 is formed over the epitaxial stack 204 prior to patterning the semiconductor fins. In some embodiments, the HM layer 212 includes an oxide layer 212A (e.g., a pad oxide layer that may include SiO2) and a nitride layer 212B (e.g., a pad nitride layer that may include Si3N4) formed over the oxide layer 212A. The oxide layer 212A may serve as an adhesion layer between the epitaxial stack 204 and the nitride layer 212B, and may serve as an etch stop layer for etching the nitride layer 212B. In some examples, the HM layer 212 includes a thermally grown oxide, a CVD deposited oxide, and / or an ALD deposited oxide. In some embodiments, the HM layer 212 includes a nitride layer deposited by CVD and / or other suitable techniques.

[0029] Then, method 100 proceeds to operation 104 ( Figure 1A ), wherein the fin element (or fin) 210 is formed by patterning the epitaxial stack 204 using a patterned mask layer 212. Figure 3 In the example of operation 104, a plurality of fins 210 extending from the substrate 202 are formed longitudinally in the X direction, and the fins 210 include fins 210a in region I and fins 210b in region II. In the illustrated embodiment, two fins 210a are arranged in the Y direction in region I, and one fin 210b is shown in region II. However, the number of fins 210a or 210b is not limited thereto, and may be as small as one or three or more. In various embodiments, each fin 210 includes an upper portion consisting of stacked epitaxial layers 206 and 208, and a lower portion formed by the substrate 202. In some embodiments, the width W1 of the upper portion of the fin 210a in region I along the Y direction is in the range of about 10nm to about 40nm. In some embodiments, the width W2 of the upper portion of the fin 210b in region II along the Y direction is wider than W1, such as in the range of about 50nm to about 1000nm. In some embodiments, the length L1 of the upper portion of the fin 210a in region I along the X direction and the length L2 of the upper portion of the fin 210b in region II along the X direction can be in the range of about 90nm to about 900nm, respectively. In region I, the fin 210a can be designed to form an NFET or a PFET. In region II, the fin 210b can be designed to form an ESD diode. The large width W2 of the fin 210b provides lower ESD resistance and stronger ESD current conductivity.

[0030] The fins 210 may be fabricated using a suitable process including a photolithography and an etching process. The photolithography process may include forming a photoresist layer (not shown) over the HM layer 212, exposing the photoresist to a pattern, performing a post-exposure bake process, and developing the photoresist to form a mask element including the photoresist. In some embodiments, an electron beam (e-beam) photolithography process may be used to perform patterning of the photoresist to form a mask element. The mask element may then be used to protect areas of the substrate 202 and layers formed on the areas while an etching process forms trenches 214 through the HM layer 212, through the epitaxial stack 204, and into the substrate 202 in unprotected areas, leaving a plurality of extended fins 210. The trenches 214 may be etched using dry etching, wet etching, RIE, and / or other suitable processes.

[0031] Many other embodiments of the method of forming a semiconductor fin on a substrate may also be used, including, for example, defining a fin region (e.g., by a mask or isolation region) and epitaxially growing the epitaxial stack 204 in the form of a fin 210. In some embodiments, forming the fin 210 may include a trimming process to reduce the width of the fin 210. The trimming process may include a wet and / or dry etching process. In some embodiments, the fin 210 may be manufactured using a suitable process including a double patterning or multiple patterning process. Typically, the double patterning or multiple patterning process combines photolithography and self-aligned processes, allowing the creation of patterns having, for example, a pitch that is smaller than that obtainable using a single direct photolithography process. For example, in one embodiment, a sacrificial layer is formed over the substrate and the sacrificial layer is patterned using a photolithography process. Spacers are formed next to the patterned sacrificial layer using a self-aligned process. The sacrificial layer is then removed, and the remaining spacers or mandrels may then be used to pattern the fin 210 by etching the epitaxial stack 204 and the substrate 202. The etching process may include dry etching, wet etching, reactive ion etching (RIE), and / or other suitable processes.

[0032] At operation 106, method 100 ( Figure 1A ) forms an isolation structure, such as a shallow trench isolation (STI) feature, between the fins 210. Still referring to Figure 3, the STI component 220 is disposed on the substrate 202 in which the fin 210 is inserted. As an example, in some embodiments, a dielectric layer is first deposited over the substrate 202, filling the trench 214 with a dielectric material. In some embodiments, the dielectric layer may include silicon oxide, silicon nitride, silicon oxynitride, fluorine-doped silicate glass (FSG), a low-k dielectric, a combination thereof, and / or other suitable materials. In various examples, the dielectric layer may be deposited by a CVD process, a SACVD process, a flowable CVD process, an ALD process, a PVD process, and / or other suitable processes. In some embodiments, after depositing the dielectric layer, the device 200 may be annealed, for example, to improve the quality of the dielectric layer. In some embodiments, the dielectric layer may include, for example, a multilayer structure having one or more liner layers. In some embodiments in which the STI component 220 is formed, after depositing the dielectric layer, the deposited dielectric material is thinned and planarized, for example, by a chemical mechanical polishing (CMP) process, so that the upper surface of the topmost epitaxial layer 208 is exposed. Subsequently, the dielectric layer of the inserted fin 210 is recessed. As Figure 3 As shown, the STI features 220 are recessed to provide the fins 210 extending above the STI features 220. In some embodiments, the recessing process may include a dry etching process, a wet etching process, and / or a combination thereof. In some embodiments, the recessing depth is controlled (e.g., by controlling the etching time) to produce a desired height of the exposed upper portion of the fin 210. In the embodiment shown, each layer of the epitaxial stack 204 is exposed. In further embodiments, the top surface of the STI features 220 is recessed below the bottom surface of the epitaxial stack 204.

[0033] Then, method 100 proceeds to operation 108 ( Figure 1A ), in which a sacrificial layer / component is formed, particularly a dummy gate structure (or dummy gate stack). Although the present discussion is directed to a replacement gate (or gate last) process, whereby a dummy gate structure is formed and then replaced, other configurations are possible.

[0034] refer to Figure 4 , FIG. 5A to FIG. 5B and FIG. 6A to FIG. 6B , forming a gate stack 232 . Figure 4 is a perspective view of the device 200, Figure 5A and Figure 5B are top views of two embodiments of the device 200, Fig. 6A refers to a portion of the fin 210a and along the longitudinal direction of the fin 210a (eg, along Figure 4 A cross-sectional view of region I taken along line AA in FIG. Figure 6B refers to a portion of the fin 210b and along the longitudinal direction of the fin 210b (eg, along Figure 4BB line in ( ). The gate stack 232 is oriented longitudinally along the Y direction. In some embodiments, the gate stack 232 has a width W3 in the range of about 10nm to about 100nm and a length L3 in the range of about 40nm to about 950nm. In region I, the length L3 of the gate stack 232 is greater than the width W1 of the fin 210a, and the gate stack 232 engages the fin 210 from the top surface and sidewall of the fin 210a. The portion of the fin 210a located below the pseudo gate stack 232 may be referred to as a channel region. The pseudo gate stack 232 may also define a source / drain (S / D) region of the fin 210a, for example, a region of the fin 210a adjacent to the channel region and located on the opposite side of the channel region. The distance D1 between adjacent gate stacks 232 may be in the range of from about 30nm to about 200nm. In region II, the length L3 of the gate stack 232 is less than the width W2 of the fin 210b, and the gate stack 232 is deposited on the top surface of the fin 210b but not on the sidewalls of the fin 210b ( Figure 5A ). In some embodiments, a distance D2 between two adjacent gate stacks 232 in region II is in a range from about 110 nm to about 1020 nm, and the distance D2 is greater than D1. In some embodiments, a ratio of D2 / L2 is not less than about 0.7. If the ratio D2 / L2 is less than 70%, the relatively close distance between two adjacent gate stacks 232 may introduce undesirable stray capacitance and degrade ESD performance. In further embodiments, the ratio D2 / L2 is greater than 1, which means that the distance D2 is greater than the length L2 of the fin 210 b, and the gate stack 232 is deposited on the STI feature 220 surrounding the fin 210 b ( Figure 5B ). A gap G1 between the gate stack 232 and two opposite edges of the fin 210 b may be in a range of about 10 nm to about 60 nm.

[0035] In various embodiments, the gate stack 232 is a dummy (sacrificial) gate stack that is subsequently removed. Therefore, in some embodiments using a gate-last process, the gate stack 232 is a dummy gate stack and will be replaced by a final gate stack at a subsequent processing stage of the device 200. In particular, as will be discussed in more detail below, the dummy gate stack 232 can be replaced by a high-K dielectric layer (HK) and a metal gate electrode (MG) at a later processing stage.

[0036] In some embodiments, the dummy gate stack 232 includes a dummy dielectric layer 234 and a dummy electrode layer 236. In some embodiments, the dummy dielectric layer 234 may include SiO2, silicon nitride, a high-K dielectric material, and / or other suitable materials. In various examples, the dummy dielectric layer 234 may be deposited by a CVD process, a sub-atmospheric pressure CVD (SACVD) process, a flowable CVD process, an ALD process, a PVD process, or other suitable processes. As an example, the dummy dielectric layer 234 may be used to prevent damage to the fin 210 by subsequent processes (e.g., subsequent formation of the dummy gate stack). Subsequently, other portions of the dummy gate stack 232 are formed, including the dummy electrode layer 236 and the hard mask 240, which may include a plurality of layers 240A and 240B (e.g., an oxide layer 240A and a nitride layer 240B). In some embodiments, the dummy gate stack 232 is formed by various process steps, such as layer deposition, patterning, etching, and other suitable processing steps. Exemplary layer deposition processes include CVD (including low pressure CVD and plasma enhanced CVD), PVD, ALD, thermal oxidation, electron beam evaporation or other suitable deposition techniques or combinations thereof. For example, when forming a gate stack, the patterning process includes a lithography process (e.g., photolithography or electron beam lithography), and the lithography may further include photoresist coating (e.g., spin coating), soft baking, mask alignment, exposure, post-exposure baking, photoresist development, rinsing, drying (e.g., spin drying and / or hard baking), other suitable lithography techniques and / or combinations thereof. In some embodiments, the etching process may include dry etching (e.g., RIE etching), wet etching and / or other etching methods. In some embodiments, the pseudo electrode layer 236 may include polycrystalline silicon (polysilicon). In some embodiments, the hard mask 240 includes an oxide layer 240A, such as a pad oxide layer that may include SiO2. In some embodiments, the hard mask 240 includes a nitride layer 240B, such as a pad nitride layer that may include Si3N4, silicon oxynitride and / or silicon carbide.

[0037] In the following figures, for the sake of simplicity, the Figure 5A 2. The manufacturing operations after the structure shown in FIG. 2 show that the dummy gate stack is deposited directly above the fin 210 b. However, the same operations can be applied to Figure 5B The structure shown, wherein the dummy gate stack is deposited directly above the STI feature 220 .

[0038] In operation 110, method 100 ( Figure 1A ) A gate spacer 242 is formed on the sidewall of the dummy gate stack 232. Fig. 7A and Figure 7B, the gate spacer 242 may have a thickness of about 2-10 nm. In some examples, the gate spacer 242 may include a dielectric material such as silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, SiCN, silicon oxycarbide, SiOCN, a low-K material, and / or a combination thereof. In some embodiments, the gate spacer 242 includes a plurality of layers, such as a liner spacer layer 242A and a main spacer layer 242B, etc. As an example, the gate spacer 242 may be formed by conformally depositing a dielectric material over the device 200 using a process such as a CVD process, a sub-atmospheric pressure CVD (SACVD) process, a flowable CVD process, an ALD process, a PVD process, or other suitable processes. After the conformal deposition of the dielectric material, a portion of the dielectric material used to form the gate spacer 242 may be etched back to expose a portion of the fin 210 not covered by the dummy gate stack 232. In some cases, the etch-back process removes a portion of the dielectric material used to form the gate spacer 242 along the top surface of the dummy gate stack 232. In some embodiments, the etch-back process may include a wet etch process, a dry etch process, a multi-step etch process, and / or a combination thereof. Note that after the etch-back process, the gate spacers 242 remain disposed on the sidewalls of the dummy gate stack 232 .

[0039] At operation 112, method 100 ( Figure 1A ) The S / D region in region I is etched to form a recess 246. The recess 246 is also referred to as an S / D trench 246. Fig. 8A and Figure 8B In some embodiments of operation 112, an etching mask (not shown) is formed over the device 200. The etching mask provides an opening above region I, allowing the S / D region of the fin 210a to be recessed through the opening while protecting region II from etching losses. Then, operation 112 applies an etching process that is adjusted to be selective to the material of the semiconductor material (e.g., silicon and silicon germanium) in the fin 210a, and does not etch (or minimally etch) the pseudo gate stack 232 and the STI component 220. In the present embodiment, the etching process recesses the fin 210a in the S / D region to a level below the bottommost epitaxial layer 206. The ends of the epitaxial layers 206 and 208 are exposed in the S / D trench 246. The etching process can be dry etching, wet etching, reactive ion etching, or other etching methods. The etching mask is then removed, for example, by a photoresist stripping process or other suitable process.

[0040] At operation 114, method 100 ( Figure 1A ) forms an internal spacer 248 on the end of the epitaxial layer 206 in region I. Fig.9A and Fig. 9BIn some embodiments, the internal spacer 248 includes a dielectric material including silicon, oxygen, carbon, nitrogen, other suitable materials, or combinations thereof (e.g., silicon oxide, silicon nitride, silicon oxynitride, silicon carbide, or carbon oxynitride). The internal spacer 248 can be formed by a deposition and etching process. For example, after forming the S / D trenches 246, a lateral etching process can be used to recess the epitaxial layer 206 to vertically form a cavity between adjacent epitaxial layers 208. Then, one or more dielectric materials are deposited (e.g., using CVD or ALD) to fill the cavity. Another etching process is performed to remove the dielectric material outside the cavity, thereby forming the internal spacer 248.

[0041] At operation 116, method 100 ( Figure 1A ) in the etching process, the S / D trench 246 in the source region (thus serving as the source trench 246) is further extended downward into the top substrate portion 202a and a bottom S / D layer 252 is formed in the source trench 246. According to an embodiment, in Fig. 10A and Fig. 10BThe resulting structure is shown in . In the illustrated embodiment, operation 114 first forms an etching mask 250 above the device 200. In some embodiments, the etching mask 250 is a liner layer deposited conformally on the device 200. The etching mask 250 provides an opening in region I above the source trench 246 between adjacent pseudo gate stacks 232, while the drain trench 246 and region II remain covered. In various embodiments, the opening of the etching mask 250 may be provided only in the drain trench, only in the source trench, or above both the source trench and the drain trench. In the present invention, the source and drain are used interchangeably. The etching mask 250 includes a material different from the semiconductor material in the top substrate portion 202a to achieve etching selectivity during further etching of the source trench 246. For example, the etching mask 250 includes a photoresist material (and therefore may be referred to as a patterned photoresist layer and / or a patterned photoresist layer). Operation 116 also includes etching the top substrate portion 202a through the etching mask 250 to extend the source trench 246 downward. The etching process can be dry etching, wet etching, reactive ion etching or other suitable etching methods to selectively recess the source trench 246 to a desired level. Subsequently, operation 116 fills the bottom of the extended source trench 246 with a bottom S / D layer 252, which has an etching selectivity with the semiconductor material in the top substrate portion 202a. In some embodiments, the bottom S / D layer 252 is a dielectric layer, which can include one or more dielectric materials selected from La2O3, Al2O3, SiOCN, SiOC, SiCN, SiO2, SiC, ZnO, ZrN, Zr2Al3O9, TiO2, TaO2, ZrO2, HfO2, Si3N4, Y2O3, AlON, TaCN, ZrSi, combinations thereof, and other suitable materials, and can be formed by PE-CVD, F-CVD or other suitable methods. In some embodiments, the bottom S / D layer 252 may include a semiconductor material as long as etching selectivity is achieved between the bottom S / D layer 252 and the top substrate portion 202a. For example, the bottom S / D layer 252 may include SiGe and may be formed by any epitaxial process including chemical vapor deposition (CVD) techniques (e.g., vapor phase epitaxy and / or ultra-high vacuum CVD), molecular beam epitaxy, other suitable epitaxial growth processes, or combinations thereof. The bottom S / D layer 252 reserves space for the backside S / D contacts that are subsequently formed. In the illustrated embodiment, the bottom S / D layer 252 fills the bottom of the source trench 246 and is below the bottommost epitaxial layer 206. Subsequently, the etching mask 250 is removed, for example, by a photoresist stripping process or other suitable process.

[0042] At operation 118, method 100 ( Figure 1B) S / D features 260 are formed in the S / D trenches 246 in region I. According to an embodiment, Fig.11A and Fig. 11B The resulting structure is shown in . In some embodiments, operation 118 may include epitaxially growing a semiconductor material, such as epitaxially grown silicon, germanium, or silicon germanium. The S / D component 260 may be formed by any epitaxial process including chemical vapor deposition (CVD) techniques (e.g., vapor phase epitaxy and / or ultra-high vacuum CVD), molecular beam epitaxy, other suitable epitaxial growth processes, or combinations thereof. The S / D component 260 may be doped with n-type dopants and / or p-type dopants. In some embodiments, for n-type transistors, the S / D component 260 includes silicon and may be doped with carbon, phosphorus, arsenic, other n-type dopants, or combinations thereof (e.g., forming a Si:C epitaxial S / D component, a Si:P epitaxial S / D component, or a Si:C:P epitaxial S / D component). In some embodiments, for p-type transistors, the S / D component 260 includes silicon germanium or germanium and may be doped with boron, other p-type dopants, or combinations thereof (e.g., forming a Si:Ge:B epitaxial S / D component). The S / D feature 260 may include a plurality of epitaxial semiconductor layers having different levels of dopant density. In some embodiments, an annealing process (eg, rapid thermal annealing (RTA) and / or laser annealing) is performed to activate dopants in the S / D feature 260 .

[0043] At operation 120, method 100 ( Figure 1B ) In the fin 210b in region II, an implanted P+ region and an N+ region are formed to form an ESD device. Fig. 12A and Fig. 12B The resulting structure is shown in FIG. Operation 120 may include: performing n-type impurity implantation (or doping) to form a heavily doped n-type region 262 (or N+ region 262); and performing p-type impurity implantation to form a heavily doped p-type region 264 (or P+ region 264). Throughout the specification, the term “heavily doped” means greater than about 10 20 / cm 3impurity concentration. However, it should be understood that the term "heavy doping" is a term of art and relates to a specific technology generation for forming an integrated circuit of an embodiment. When the conductivity type is p-type, suitable impurities include boron, aluminum or other suitable p-type dopants. When the conductivity type is n-type, suitable impurities include phosphorus, arsenic or other suitable n-type dopants. In the illustrated embodiment, the injection is limited to the region between the adjacent pseudo gate stacks 232 in region II. As known in the art, a mask such as a photoresist can be formed to cover the region not injected. In some embodiments, the width of each of the P+ region 264 and the N+ region 262 along the Y direction can be substantially equal to the width W2 of the fin 210b, and the length L4 along the X direction can be in the range of about 30nm to about 200nm. In the illustrated embodiment, the doping depth of the P+ region 264 and the N+ region 262 extends beyond the bottommost epitaxial layer 206 and into the top substrate portion 202a for a distance d. In one embodiment, the distance d is in the range of about 0nm to about 30nm. Such a distance d improves the RC performance of the ESD device in the embodiment. The middle portion of the fin 210b may remain unimplanted. The unimplanted middle portion of the fin 210b is located between and adjacent to the N+ region 262 and the P+ region 264. Fig. 12B as well as Fig.16A , in some embodiments, the length L5 of the unimplanted middle portion along the X direction can be in the range of about 30nm to about 500nm. In various embodiments, the ratio L5 / L4 is about 0.2 to about 2.5. If the ratio is less than 0.2, the relatively small distance between the P+ / N+ regions may cause dopants to diffuse into each other and reduce the effective injection region width. If the ratio is greater than 2.5, the relatively large distance between the P+ / N+ regions may increase the resistance along the ESD path and reduce the ESD performance. In the illustrated embodiment, the dummy gate stack 232 is laterally spaced from the P+ / N+ region by a gap G2 of about 10nm to about 60nm (measured from the sidewall of the gate spacer 242). Optionally, the dummy gate stack 232 may be adjacent to the P+ / N+ region (G2≈0), respectively, or even partially overlap the edge of the P+ / N+ region.

[0044] In the resulting structure after operation 120, a PN junction is formed between the P+ region 264 and the N+ region 262. The PN junction is along the longitudinal direction of the fin 210b. In the illustrated embodiment, the resulting structure is an ESD diode. By locating the P+ / N+ region in the same fin, rather than crossing with multiple fins, the ESD current conductivity can be enhanced and the ESD parasitic capacitance can be reduced. By having a pseudo gate stack outside the P+ / N+ region and a metal gate stack formed subsequently accordingly, the ESD parasitic capacitance between the ESD diode and the gate structure is further reduced. The relatively large width of the fin 210b also provides a low-resistivity ESD current path, which enhances the performance of the ESD device.

[0045] At operation 122, method 100 ( Figure 1B ) An interlayer dielectric (ILD) layer 268 is formed on the sidewalls of the dummy gate stack 232, and the ILD layer 268 covers the fin 210. Fig.13A and Fig. 13B In some embodiments of operation 122, a contact etch stop layer (CESL) 266 is also formed before forming the ILD layer 268. In some examples, the CESL 266 includes a silicon nitride layer, a silicon oxide layer, a silicon oxynitride layer, and / or other materials known in the art. The CESL 266 may be formed by a plasma enhanced chemical vapor deposition (PECVD) process and / or other suitable deposition or oxidation processes. In some embodiments, the ILD layer 268 includes a dielectric material such as tetraethyl orthosilicate (TEOS) oxide, undoped silicate glass, or doped silicon oxide such as borophosphosilicate glass (BPSG), fused silica glass (FSG), phosphosilicate glass (PSG), boron-doped silicate glass (BSG), and / or other suitable dielectric materials. The ILD layer 268 may be deposited by a PECVD process or other suitable deposition techniques. In some embodiments, after forming the ILD layer 268, the device 200 may be subjected to a high thermal budget process to anneal the ILD layer. In some examples, after depositing the ILD layer 268, a planarization process can be performed to remove excess dielectric material. For example, the planarization process includes a CMP process that removes portions of the CESL 266 and the ILD layer 268 that are located above the dummy gate stack 232 and planarizes the top surface of the device 200. In some embodiments, the CMP process exposes the dummy electrode layer 236.

[0046] At operation 124, method 100 ( Figure 1B ) removes the dummy gate stack 232 to form gate trenches 270 in regions I and II, as shown in FIG. Fig.13A and Fig. 13BAs shown. A final gate structure (e.g., including a high-K dielectric layer and a metal gate electrode) may then be formed in the gate trench 270, as will be described below. Operation 124 may include one or more etching processes that are selective to the materials in the pseudo dielectric layer 234 and the pseudo electrode layer 236 of the pseudo gate stack 232. For example, removal of the pseudo gate stack 232 may be performed using a selective etching process, such as selective wet etching, selective dry etching, or a combination thereof. The epitaxial layers 206 and 208 of the fin 210a in region I and the topmost epitaxial layer 208 of the fin 210b in region II are exposed in the gate trench 270.

[0047] At operation 126, method 100 ( Figure 1B ) removes the epitaxial layer 206 from the fin 210a exposed in the gate trench 270 in region I. According to an embodiment, in Fig.13A and Fig. 13B The resulting structure is shown in FIG. In an embodiment, epitaxial layer 206 comprises SiGe and epitaxial layer 208 comprises Si, allowing for selective removal of epitaxial layer 206. In an embodiment, epitaxial layer 206 is removed by a selective wet etching process. In some embodiments, the selective wet etching comprises an APM etch (e.g., a mixture of ammonium hydroxide-hydrogen peroxide-water). In some embodiments, the selective removal comprises oxidation of SiGe followed by oxidation of SiGeO x For example, oxidation can be provided by O3 cleaning, followed by removal of SiGeO by an etchant such as NH4OH. x In region II, the topmost epitaxial layer 208 acts as an etch stop and protects the underlying epitaxial layer 206 from being etched.

[0048] Then, method 100 proceeds to operation 128 ( Figure 1B ), wherein a gate structure is formed. According to an embodiment, Fig.14A and Fig. 14B The resulting structure is shown in . The gate structure can be a high-K / metal gate (HK MG) stack, but other compositions are possible. In some embodiments, the gate structure forms a gate associated with a multi-channel provided by multiple channel layers (e.g., nanosheets or nanowires with gaps between them) in a channel region in region I. In an embodiment of operation 128, an HK MG stack 274 is formed within a gate trench 270 of the device 200. In various embodiments, the HK MG stack 274 includes an interface layer (not shown), a high-K gate dielectric layer 276 formed over the interface layer, and a gate electrode layer 278 formed over the high-K gate dielectric layer 276. As used and described herein, a high-K gate dielectric includes a dielectric material having a high dielectric constant, for example, a dielectric constant greater than that of thermal silicon oxide. The gate electrode layer used in the HK MG stack may include metal, metal alloy or metal silicide. In addition, the formation of the HK MG stack may include deposition to form various gate materials, one or more liner layers, and one or more CMP processes to remove excess gate material and thereby planarize the top surface of the semiconductor device 200. An internal spacer 248 is inserted between the HK MG stack 274 and the S / D component 260 to provide isolation.

[0049] In some embodiments, the interface layer of the HK MG stack 274 may include a dielectric material such as silicon oxide (SiO2), HfSiO, or silicon oxynitride (SiON). The interface layer may be formed by chemical oxidation, thermal oxidation, atomic layer deposition (ALD), chemical vapor deposition (CVD), and / or other suitable methods. The high-K gate dielectric layer 276 of the HK MG stack 274 may include a high-K dielectric such as hafnium oxide (HfO2). Alternatively, the high-K gate dielectric layer 276 of the HK MG stack 274 may include other high-K dielectrics, such as TiO2, HfZrO, Ta2O3, HfSiO4, ZrO2, ZrSiO2, LaO, AlO, ZrO, TiO, Ta2O5, Y2O3, SrTiO3 (STO), BaTiO3 (BTO), BaZrO, HfZrO, HfLaO, HfSiO, LaSiO, AlSiO, HfTaO, HfTiO, (Ba, Sr)TiO3 (BST), Al2O3, Si3N4, oxynitride (SiON), combinations thereof, or other suitable materials. The high-K gate dielectric layer 276 may be formed by ALD, physical vapor deposition (PVD), CVD, oxidation, and / or other suitable methods.

[0050] The gate electrode layer 278 of the HK MG stack 274 may include a single layer or optionally a multilayer structure, such as a metal layer (work function metal layer) having a selected work function to enhance device performance, a liner layer, a wetting layer, an adhesion layer, a metal alloy, or various combinations of metal silicides. As an example, the gate electrode layer 278 of the HK MG stack 274 may include Ti, Ag, Al, TiAlN, TaC, TaCN, TaSiN, Mn, Zr, TiN, TaN, Ru, Mo, Al, WN, Cu, W, Re, Ir, Co, Ni, other suitable metal materials, or combinations thereof. In various embodiments, the gate electrode layer 278 of the HK MG stack 274 may be formed by ALD, PVD, CVD, electron beam evaporation, or other suitable processes. In addition, the gate electrode layer 278 may be formed separately for N-FET and P-FET transistors that may use different metal layers (e.g., for providing N-type or P-type work functions). In various embodiments, a CMP process may be performed to remove excess metal from the gate electrode layer 278 of the HK MG stack 274 and thereby provide a substantially flat top surface of the HK MG stack 274. The HK MG stack 274 includes a portion inserted into each epitaxial layer (channel layer) 208 that forms a channel of a multi-gate transistor in region I.

[0051] At operation 130, method 100 ( Figure 1B ) various features are formed on the front side of the device 200. For example, operation 130 may form contact openings exposing the underlying N+ region 262 / P+ region 264 by etching the ILD layer 268 and the CESL 266, form contacts 282a bonded to the S / D features 260 in region I and contacts 282b bonded to the N+ region 262 / P+ region 264 in region II by filling the contact openings with a conductive material, and form various other contacts / vias / lines and multi-layer interconnect features (e.g., metal layers and interlayer dielectrics) (represented as metal wiring layers 284) on the front side of the device 200. According to an embodiment, at Fig.15A and Fig. 15B The resulting structure is shown in FIG. In a further example, metal wiring layer 284 may include multiple layers of interconnects, such as vertical interconnects (e.g., vias or contacts) and horizontal interconnects (e.g., metal lines). The various interconnect components may be made of various conductive materials, including copper, tungsten, and / or silicide. In one example, a damascene and / or dual damascene process is used to form a copper-related multilayer interconnect structure.

[0052] refer to Fig.16A , Fig.16AA top view of the device 200 after operation 130 according to an embodiment is shown, with the contacts 282b in region II spaced apart along the X direction and extending along the Y direction. Each contact 282b may have a width along the X direction in a range from about 10nm to about 80nm, and may have a length along the Y direction in a range from about 40nm to about 950nm. The contact 282b may be deposited in a portion of the P+ region 262 / N+ region 264, with the contact 282b having an edge-to-edge distance L6' to the inner edge (i.e., the opposite edge) of the P+ / N+ region and an edge-to-edge distance L6 to the outer edge (i.e., the edge facing the HK MG stack 274) of the P+ / N+ region, respectively. In various embodiments, L6' is less than L6. In other words, the contact 282b is closer to the inner edge of the P+N+ region than the outer edge. In some embodiments, the ratio L6' / L6 is less than about 0.4. For example, the distance L6' may be less than about 10 nm, and the distance L6 may be in a range between about 30 nm and about 60 nm. Fig. 16B , Fig. 16B As shown above, Figure 5B A top view of the device 200 after operation 130 of another embodiment discussed, the gate stack 274 is deposited on the STI feature 220, and the P+ / N+ region extends to the lateral ends of the fin 210b. The distance G1 between two opposite edges of the gate stack 274 and the fin 210b is also the distance G2 between two opposite edges of the gate stack 274 and the P+ / N+ region, which is in the range from about 10nm to about 60nm. By having the gate stack 274 outside the fin 210b, the ESD parasitic capacitance between the ESD diode and the gate structure is further reduced.

[0053] At operation 132, method 100 ( Figure 1B ) Turn the device 200 upside down and attach the front side of the device 200 to the carrier 286, such as Fig.17A and Fig. 17B As shown. This allows access to the device 200 from the back side of the device 200 for further processing. Operation 132 may use any suitable attachment process, such as direct bonding, hybrid bonding, using adhesives or other bonding methods. Operation 132 may also include alignment, annealing and / or other processes. In some embodiments, carrier 286 may be a silicon wafer. Figures 2 to 23B , the “z” direction points from the back side of the device 200 to the front side of the device 200 , while the “−z” direction points from the front side of the device 200 to the back side of the device 200 .

[0054] At operation 134, method 100 ( Figure 1C) thins the device 200 from the back side of the device 200 until the bottom S / D layer 252 is exposed from the back side of the device 200. According to an embodiment, Fig.18A and Fig.18B The resulting structure is shown in FIG. The thinning process may include a mechanical grinding process and / or a chemical thinning process. During the mechanical grinding process, a large amount of substrate material may first be removed from the substrate 202. During the removal of the bottom substrate portion 202b, the dielectric cap layer 203 may be used as a CMP stop layer. Thereafter, a chemical thinning process may apply an etching chemical to the back side of the substrate 202 to remove the dielectric cap layer 203 and further thin the top substrate portion 202a until the bottom S / D layer 252 is exposed.

[0055] At operation 136, method 100 ( Figure 1C ) removes the top substrate portion 202a in region I from the back side of the device 200. According to an embodiment, Fig.19A and Fig.19B The resulting structure of the avocado is shown in FIG. Operation 136 may include first forming an etching mask (not shown) covering region II. Then, operation 136 applies an etching process that is adjusted to be selective to the material (e.g., silicon) of the semiconductor material in the top substrate portion 202a and not (or minimizes) etching of the bottom S / D layer 252. The etching process may be dry etching, wet etching, reactive ion etching, or other etching methods. After removing the top substrate portion from region I, the metal gate stack 274, the internal spacer 248, and the S / D component 260 are exposed at the back side of the device 200. The etching mask is then removed, for example, by a photoresist stripping process or other suitable process. The top substrate portion 202a remains in region II of the device 200.

[0056] At operation 138, method 100 ( Figure 1C ) A dielectric layer 288 is deposited on the back side of the device 200. According to an embodiment, Fig. 20A and Fig. 20BThe resulting structure is shown in FIG. Operation 138 may first include a chemical thinning process to recess the top substrate portion 202a in region II to a level lower than the bottom S / D layer 252 in region I. Then, operation 138 deposits a dielectric layer 288 covering regions I and II. The dielectric layer 288 may include tetraethyl orthosilicate (TEOS) oxide, undoped silicate glass, or doped silicon oxide, such as borophosphosilicate glass (BPSG), fluorine-doped quartz glass (FSG), phosphosilicate glass (PSG), boron-doped silicate glass (BSG), low-k dielectric materials, other suitable dielectric materials, or combinations thereof. The dielectric layer 288 may be formed by PE-CVD (plasma enhanced CVD), F-CVD (flowable CVD), or other suitable methods. Operation 138 may also include a CMP process to planarize the dielectric layer 288 to remove excess dielectric material from the back side of the device 200. Since the dielectric layer 288 and the bottom S / D layer 252 include different materials, the bottom S / D layer 252 can be used as a CMP stop when the dielectric layer 288 is planarized by a CMP process. After operation 138, the bottom S / D layer 252 is exposed in region I, while the top substrate portion 202a remains covered by the dielectric layer 288 in region II.

[0057] At operation 140, method 100 ( Figure 1C ) The bottom S / D layer 252 is selectively etched to form a backside trench 290 surrounded by the dielectric layer 288. The backside trench 290 exposes the surface of the source feature 260 from the back side. Fig.21A and Fig.21B The resulting structure is shown in FIG. In the present embodiment, operation 140 applies an etching process that is tuned to be selective to the material in the bottom S / D layer 252 (e.g., SiGe) and does not (or minimizes) etching of the dielectric layer 288. In the present embodiment, the etching process also etches the source feature 260 to recess the source feature 260 to a level below the drain feature 260 that is still covered by the dielectric layer 288. In a further embodiment, the source feature 260 is recessed below the dielectric layer 288 and the bottommost internal spacer 248. Operation 140 may apply more than one etching process. For example, it may apply a first etching process to selectively remove the bottom S / D layer 252, and then apply a second etching process to selectively recess the source feature 260 to a desired level, wherein the first etching process and the second etching process use different etching parameters, such as using different etchants. The etching process may be dry etching, wet etching, reactive ion etching, or other etching methods.

[0058] At operation 142, according to an embodiment, method 100 ( Figure 1C ) Fig.21A and Fig.21B A dielectric liner 292 is deposited on the sidewalls of the backside trench 290 as shown. In some embodiments, the dielectric liner 292 is conformally deposited to have a substantially uniform thickness along the various surfaces of the dielectric layer 288, the internal spacer 248, and the recessed source feature 260. In various embodiments, the dielectric liner 292 may include La2O3, Al2O3, SiOCN, SiOC, SiCN, SiO2, SiC, ZnO, ZrN, Zr2Al3O9, TiO2, TaO2, ZrO2, HfO2, Si3N4, Y2O3, AlON, TaCN, ZrSi, combinations thereof, or other suitable materials. In various embodiments, the dielectric liner 292 may be deposited using ALD, CVD, or other suitable methods, and the dielectric liner 292 may have a thickness of about 0.5 nm to about 10 nm. Operation 142 also includes a breakthrough etching process for penetrating and removing a majority of the horizontal portion of the dielectric liner 292. In some embodiments, the breakthrough etching process may include an anisotropic dry etching process, etc. In some embodiments where the dielectric liner layer 292 is formed of an oxide compound, the BT etching process is a reactive ion etching (RIE) process using an etching process gas including CHF3, Ar, CF4, N2, O2, CH2F2, SF3, etc., or a combination thereof. In the illustrated embodiment, due to operation 142, portions of the dielectric liner 292 remain on the sidewalls of the backside trench 290, including the surfaces of the dielectric layer 288 and the inner spacer 248. After the breakthrough etching process, the recessed source feature 260 is exposed again in the backside trench 290.

[0059] At operation 144, according to an embodiment, Fig.22A and Fig. 22B As shown, method 100( Figure 1C) forms a silicide feature 294 in the backside trench 290 above the source feature 260. In an embodiment, operation 144 first deposits one or more metals into the backside trench 290, performs an annealing process on the device 200 to cause a reaction between the one or more metals and the source feature 260 to produce the silicide feature 294, and removes unreacted portions of the one or more metals, leaving the silicide feature 294 in the backside trench 290. The one or more metals may include titanium (Ti), tantalum (Ta), tungsten (W), nickel (Ni), platinum (Pt), (Yb), iridium (Ir), (Er), cobalt (Co), or combinations thereof (e.g., alloys of two or more metals), and may be deposited using CVD, PVD, ALD, or other suitable methods. The silicide feature 294 may include titanium silicide (TiSi), nickel silicide (NiSi), tungsten silicide (WSi), nickel platinum silicide (NiPtSi), nickel platinum germanium silicide (NiPtGeSi), nickel germanium silicide (NiGeSi), ytterbium silicide (YbSi), platinum silicide (PtSi), iridium silicide (IrSi), erbium silicide (ErSi), cobalt silicide (CoSi), combinations thereof, or other suitable compounds.

[0060] At operation 146, method 100 ( Figure 1C ) forms a backside S / D contact 296 in the backside trench 290 above the silicide feature 294 in region I. According to an embodiment, Fig.22A and Fig. 22B The resulting structure is shown in FIG. In an embodiment, the back side S / D contact 296 may include a conductive barrier layer and a metal filling layer located above the conductive barrier layer. The conductive barrier layer may include titanium (Ti), tantalum (Ta), tungsten (W), cobalt (Co), ruthenium (Ru) or a conductive nitride, such as titanium nitride (TiN), titanium aluminum nitride (TiAlN), tungsten nitride (WN), tantalum nitride (TaN) or a combination thereof, and may be formed by CVD, PVD, ALD and / or other suitable processes. The metal filling layer may include tungsten (W), cobalt (Co), molybdenum (Mo), ruthenium (Ru), nickel (Ni), copper (Cu) or other metals, and may be formed by CVD, PVD, ALD, plating or other suitable processes. In some embodiments, the conductive barrier layer is omitted in the back side S / D contact 296. The dielectric liner 292 is used as a dielectric barrier layer to prevent the metal material in the back side S / D contact 296 from diffusing into the dielectric layer 288.

[0061] At operation 148, method 100 ( Figure 1C ) performs further manufacturing processes on the device 200. For example, it can form a metal wiring layer 298 on the back side of the device 200, such as a back side power line. According to an embodiment, Fig.23A and Fig. 23B The resulting structure is shown. Metal wiring layer 298 is electrically connected to backside S / D contact 296 in region I. In an embodiment, a damascene process, a dual damascene process, a metal patterning process, or other suitable process can be used to form a metal wiring layer. The metal wiring layer may include tungsten (W), cobalt (Co), molybdenum (Mo), ruthenium (Ru), copper (Cu), nickel (Ni), titanium (Ti), tantalum (Ta), titanium nitride (TiN), tantalum nitride (TaN) or other metals, which may be deposited by CVD, PVD, ALD, plating or other suitable processes. Having a backside metal wiring layer advantageously increases the number of metal tracks in device 200 that can be used to directly connect to source / drain contacts and vias. It also increases gate density for greater device integration compared to other structures without a backside metal wiring layer. In some embodiments, one of the two contacts 282b of the ESD diode (e.g., one disposed on the P+ region 264 or one disposed on the N+ region 262) is electrically coupled to the metal wiring layer 284 on the front side of the device 200, and the other contact 282b is electrically coupled to the metal wiring layer 298 on the back side of the device 200, such as through substrate vias (TSVs). The method 100 may also form one or more interconnect layers on the back side of the device 200, form a passivation layer on the back side of the device 200, perform other BEOL processes, and remove the carrier 286 at operation 148. Fig.23A and Fig. 23B As shown, even though the bulk semiconductor substrate is removed from region I in the illustrated multi-gate process flow as part of the formation of the backside metal wiring layer, the top substrate portion 202a remains in region II below the epitaxial layer 206 / 208 and the N+ region 262 / P+ region 264, which provides an additional ESD current path in the substrate and thereby provides less ESD resistance.

[0062] Although not intended to be limiting, embodiments of the present invention provide one or more of the following advantages. For example, embodiments of the present invention form an ESD protection device and a method for manufacturing the same that is compatible with a multi-gate transistor process flow. In various embodiments, the method of the present invention retains a bulk semiconductor substrate for the ESD protection device after the backside substrate thinning process, which provides more current paths for electrostatic discharge events. In addition, some embodiments of the present invention form an implantation region on the same fin element of a stack including an epitaxial layer, which enhances ESD current conductivity and reduces ESD parasitic capacitance. Embodiments of the process flow also support the formation of multi-gate transistors with a backside metal wiring layer (such as a backside power rail) to increase the number of metal rails available in an integrated circuit and increase gate density for greater device integration. Embodiments of the present invention can be easily integrated into existing semiconductor manufacturing processes.

[0063] In one exemplary aspect, the present invention is directed to a method for manufacturing a semiconductor device. The method includes providing a structure having a front side and a back side, the structure including a substrate and a stack of first type epitaxial layers and second type epitaxial layers of different material compositions alternately stacked on the substrate, wherein the stack is located at the front side of the structure and the substrate is located at the back side of the structure; patterning the stack to form a fin on the substrate; implanting a first dopant into a first region of the fin, the first dopant having a first conductivity type; implanting a second dopant into a second region of the fin, the second dopant having a second conductivity type opposite to the first conductivity type; forming a first contact on the first region, and forming a second contact on the second region. In some embodiments, the first region and the second region are separated by a middle portion of the fin. In some embodiments, the method also includes forming a first dummy gate stack and a second dummy gate stack on the fin; depositing an interlayer dielectric (ILD) layer covering the fin on the sidewalls of the first dummy gate stack and the second dummy gate stack; and replacing the first dummy gate stack and the second dummy gate stack with a first metal gate stack and a second metal gate stack. In some embodiments, the first contact and the second contact are located between the first metal gate stack and the second metal gate stack. In some embodiments, the width of each of the first metal gate stack and the second metal gate stack is less than the width of the fin. In some embodiments, the method also includes thinning the substrate from the back side of the structure; and depositing a dielectric layer at the back side of the structure. In some embodiments, the method also includes forming an isolation structure around the fin; and forming at least one gate stack directly above the isolation structure. In some embodiments, where the fin is a first fin and the patterning of the stack also forms a second fin, the method also includes removing the second type epitaxial layer from the second fin, thereby exposing the first type epitaxial layer; and forming a metal gate stack bonded to the first type epitaxial layer in the second fin. In some embodiments, the width of the second fin is less than the width of the first fin.

[0064] In another exemplary aspect, the present invention is directed to a method for manufacturing a semiconductor device. The method includes forming a fin protruding from a semiconductor substrate, wherein the fin includes a first type epitaxial layer and a second type epitaxial layer located on the semiconductor substrate, the first type epitaxial layer and the second type epitaxial layer having different material compositions and being arranged alternately in a vertical direction; forming a first gate structure and a second gate structure on the fin; doping a first region of the fin with a first dopant of a first conductivity type; doping a second region of the fin with a second dopant of a second conductivity type opposite to the first conductivity type, wherein the first region and the second region are located between the first gate structure and the second gate structure; forming a dielectric layer on the sidewalls of the first gate structure and the second gate structure; forming a contact hole in the dielectric layer, the contact hole exposing the first region and the second region; and forming a conductive contact in the contact hole. In some embodiments, the doping of the first region and the second region has a doping depth extending into the semiconductor substrate. In some embodiments, the method also includes thinning the semiconductor substrate; and depositing an oxide layer under the semiconductor substrate. In some embodiments, the width of the fin is greater than the width of the first gate structure or the second gate structure. In some embodiments, after doping the first region and the second region of the fin, the middle portion of the fin is substantially free of the first dopant and the second dopant.

[0065] In yet another exemplary aspect, the present invention is directed to an electrostatic discharge (ESD) device. The ESD device includes: a semiconductor substrate; a stack of a first type epitaxial layer and a second type epitaxial layer, located on the semiconductor substrate, the first type epitaxial layer and the second type epitaxial layer having different material compositions, and the first type epitaxial layer and the second type epitaxial layer are alternately arranged in a vertical direction; a first injection region in the stack, wherein the first injection region has a first conductivity type; and a second injection region in the stack, wherein the second injection region has a second conductivity type opposite to the first conductivity type. In some embodiments, the ESD device also includes an intermediate region in the stack, the intermediate region being located between the first injection region and the second injection region and adjacent to the first injection region and the second injection region. In some embodiments, the ESD device also includes an oxide layer located below the semiconductor substrate. In some embodiments, the ESD device also includes a first gate stack and a second gate stack located above the stack, wherein the first injection region and the second injection region are located between the first gate stack and the second gate stack. In some embodiments, the first gate stack and the second gate stack are located directly above the stack. In some embodiments, the ESD device further includes: an isolation structure located on the semiconductor substrate and surrounding the stack, wherein the first gate stack and the second gate stack are located directly above the isolation structure.

[0066] The features of several embodiments are summarized above so that those skilled in the art can better understand aspects of the present invention. Those skilled in the art should understand that they can easily use the present invention as a substrate to design or modify other processes and structures for implementing the same purpose and / or achieving the same advantages as the embodiments introduced herein. Those skilled in the art should also appreciate that this equivalent configuration does not deviate from the spirit and scope of the present invention, and that they can make multiple changes, substitutions and changes herein without departing from the spirit and scope of the present invention.

Claims

1. A method for manufacturing a semiconductor device, comprising: Providing a structure having a front side and a back side, the structure comprising a substrate and a stack of first type epitaxial layers and second type epitaxial layers having different material compositions alternately stacked on the substrate, wherein the stack is located at the front side of the structure and the substrate is located at the back side of the structure; patterning the stack to form fins over the substrate; implanting a first dopant into a first region of the fin, the first dopant having a first conductivity type; implanting a second dopant into a second region of the fin, the second dopant having a second conductivity type opposite to the first conductivity type; and forming a first contact on the first region and forming a second contact on the second region, The dopant implantation in the first region and the second region has an implantation depth extending into the substrate.

2. The method according to claim 1, wherein: The first region and the second region are separated by a middle portion of the fin.

3. The method according to claim 1, further comprising: forming a first dummy gate stack and a second dummy gate stack on the fin; depositing an interlayer dielectric (ILD) layer on sidewalls of the first dummy gate stack and the second dummy gate stack, the interlayer dielectric layer covering the fin; as well as The first dummy gate stack and the second dummy gate stack are replaced with a first metal gate stack and a second metal gate stack.

4. The method according to claim 3, wherein: The first contact and the second contact are located between the first metal gate stack and the second metal gate stack.

5. The method according to claim 3, wherein: A width of each of the first metal gate stack and the second metal gate stack is smaller than a width of the fin.

6. The method according to claim 1, further comprising: thinning the substrate from the back side of the structure; as well as A dielectric layer is deposited at the back side of the structure.

7. The method according to claim 6, further comprising: forming an isolation structure around the fin; as well as At least a gate stack is formed directly above the isolation structure.

8. The method according to claim 1, wherein: The fin is a first fin, and the patterning of the stack also forms a second fin, further comprising: removing the second type epitaxial layer from the second fin, thereby exposing the first type epitaxial layer; and A metal gate stack is formed that is bonded to the first type epitaxial layer in the second fin.

9. The method according to claim 8, wherein: The width of the second fin is smaller than the width of the first fin.

10. A method for manufacturing a semiconductor device, comprising: Forming a fin protruding from a semiconductor substrate, wherein the fin includes a first type epitaxial layer and a second type epitaxial layer located on the semiconductor substrate, the first type epitaxial layer and the second type epitaxial layer having different material compositions and being alternately arranged in a vertical direction; forming a first gate structure and a second gate structure over the fin; doping a first region of the fin with a first dopant of a first conductivity type; doping a second region of the fin with a second dopant of a second conductivity type opposite to the first conductivity type, wherein the first region and the second region are located between the first gate structure and the second gate structure; forming a dielectric layer on sidewalls of the first gate structure and the second gate structure; forming a contact hole in the dielectric layer, the contact hole exposing the first region and the second region; and forming a conductive contact in the contact hole, The doping of the first region and the second region has a doping depth extending into the semiconductor substrate.

11. The method according to claim 10, wherein: The first region and the second region are located in a same fin.

12. The method according to claim 10, further comprising: thinning the semiconductor substrate; as well as An oxide layer is deposited beneath the semiconductor substrate.

13. The method according to claim 10, wherein: The fin has a width greater than a width of the first gate structure or the second gate structure.

14. The method according to claim 10, wherein: After doping the first region and the second region of the fin, a middle portion of the fin is free of the first dopant and the second dopant.

15. An electrostatic discharge (ESD) device comprising: Semiconductor substrate; A stack of a first type epitaxial layer and a second type epitaxial layer, located on the semiconductor substrate, the first type epitaxial layer and the second type epitaxial layer have different material compositions, and the first type epitaxial layer and the second type epitaxial layer are alternately arranged in a vertical direction; a first implanted region in the stack, wherein the first implanted region has a first conductivity type; and a second implanted region in the stack, wherein the second implanted region has a second conductivity type opposite to the first conductivity type, The implantation of the first implantation region and the second implantation region has an implantation depth extending into the semiconductor substrate.

16. The electrostatic discharge device according to claim 15, further comprising: An intermediate region in the stack is located between and adjacent to the first injection region and the second injection region.

17. The electrostatic discharge device according to claim 15, further comprising: An oxide layer is located below the semiconductor substrate.

18. The electrostatic discharge device according to claim 15, further comprising: A first gate stack and a second gate stack are located on the stack, wherein the first implant region and the second implant region are located between the first gate stack and the second gate stack.

19. The electrostatic discharge device according to claim 18, wherein: The first gate stack and the second gate stack are located directly above the stack.

20. The electrostatic discharge device according to claim 18, further comprising: An isolation structure is located on the semiconductor substrate and surrounds the stack, wherein the first gate stack and the second gate stack are located directly above the isolation structure.

Citation Information

Patent Citations

  • Gate-all-around integrated circuit structures having vertically discrete source or drain structures

    EP3644375A1

  • Apparatus for ESD Protection

    US20140175551A1

  • Backside contact resistance reduction for semiconductor devices with metallization on both sides

    US20190157310A1