Microbial concentration indicating liquid based on nano-gold particles, microbial concentration indicating device, preparation method and application thereof
By preparing a positively charged gold nanoparticle indicator liquid with a particle size of 20-90 nm, combined with a closed container and a microbial sampler, the existing technology problems of late detection and high equipment prices are solved, and the detection of negatively charged microorganisms on the surface is achieved. Fast and accurate detection, suitable for water quality and disinfection effect testing.
Patent Information
- Application Number
- CN202110877737.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-08-01
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2041-08-01
AI Technical Summary
The existing methods used for water quality testing and medical device disinfection testing have problems such as late detection, high equipment prices, and complex operations. Especially when the surface of bacteria or fungi is negatively charged, gold nanoparticles cannot be effectively adsorbed. causing the detection to fail.
Use gold nanoparticles with a particle size of 20-90nm and a positive charge on the surface. Prepare a gold nanoparticle indicator solution by adding a protective agent and a reducing agent to the chloroauric acid solution, and combine it with a closed container, a microbial sampler and a membrane filter. , to achieve fast and portable microbial concentration detection.
It achieves rapid and accurate detection of negatively charged microorganisms on the surface, and the detection time is shortened to 1 hour. It is suitable for water quality and disinfection effect detection, and has the advantages of easy operation and low cost.
Smart Images

Figure BDA0003190940330000041 
Figure BDA0003190940330000051 
Figure BDA0003190940330000071
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of microorganism concentration indication, and in particular to a microorganism concentration indicating liquid based on nano-gold particles, a microorganism concentration indicating device, and a preparation method and application thereof. Background Art
[0002] At present, in order to ensure the safety of water used in cities, medical treatment, industry and food, water quality testing is required. In addition, in the testing of the effect of cleaning, disinfection and sterilization of medical devices, traditional testing methods, such as bacterial culture testing, require 48 hours to interpret the test results, which has the defect of untimely testing; and the method of using biological indicators for testing in the prior art requires a set of special testing equipment, but it is expensive and needs to be tested in a specific place, which is more complicated to operate and inconvenient to use.
[0003] Nanogold particles refer to tiny gold particles with a diameter of 1 to 100 nm, and their color ranges from red to purple depending on the diameter. In addition, they have high electron density, dielectric properties and catalytic effects, and can bind to a variety of biological macromolecules without affecting their biological activity. For example, a large number of studies have shown that colloidal gold can stably and rapidly adsorb proteins, and the biological activity of proteins does not change significantly. It can be used as a probe to accurately locate biological macromolecules such as polysaccharides, proteins, peptides, antigens, hormones, nucleic acids, etc. on the cell surface and in cells. Specifically, colloidal gold is contained in pregnancy test strips. After the nanogold particles electrostatically adsorb human chorionic gonadotropin (hCG) substances and aggregate and precipitate, it appears red, thus playing an indicative role; for another example, the detection of colloidal gold in infectious viruses is to detect whether specific antibodies against the infectious virus appear in the human body, so as to know whether the person is infected by the infectious virus. However, the above detection principles all use colloidal gold to adsorb proteins, thereby aggregating and precipitating to form particles with larger particle sizes, and color changes to achieve the purpose of detection. The above-mentioned nano gold particles are generally made by using gold salts such as chloroauric acid under the effect of a reducing agent. The nano gold particles made in this way have negative charges on their surfaces, and they can disperse to form colorless colloids, which change color when combined with various biomacromolecules by electrostatic adsorption. However, the nano gold particles with negative charges on their surfaces are prepared by existing methods or purchased in an outsourced form. In the detection of the concentration of microorganisms with negative charges on their surfaces such as bacteria or fungi, such nano gold colloids cannot adsorb such microorganisms, and the color of the detection solution does not change, so the detection indication cannot be performed. In addition, there is no related report in the prior art that nano gold particles are applied to the detection of bacteria or fungi. Summary of the invention
[0004] In order to overcome the shortcomings of the prior art, the present invention provides a microbial concentration indicator liquid based on nanogold particles that is easy to operate and quickly readable. The microbial concentration indicator liquid also has the advantages of convenience and low cost in detecting the concentration of microorganisms with negative charges on the surface.
[0005] In order to achieve the above-mentioned purpose, the technical solution adopted by the present invention is: a microbial concentration indicator liquid based on nanogold particles, characterized in that it includes a nanogold indicator liquid that can be built into a closed container, the nanogold indicator liquid includes nanogold particles with a particle size of 20-90nm, the surface of the nanogold particles has a positive charge, and the nanogold indicator liquid indicates a concentration of 100CFU / mL-1000CFU / mL.
[0006] Furthermore, the raw materials of the nano-gold indicator solution include chloroauric acid solution, a protective agent, and a reducing agent in a molar ratio of 1:(10-1000):(1-2000). The protective agent includes or only contains N,N,N-trimethyl-(11-mercaptoundecyl)ammonium chloride.
[0007] Further, the raw materials of the nano-gold indicator solution include chloroauric acid solution, a protective agent and a reducing agent, wherein the protective agent includes N, N, N-trimethyl-(11-mercaptoundecyl) ammonium chloride, and the protective agent also includes 0-3 of 11-mercaptoundecanoic acid, hexadecylamine, and polyvinyl pyrrolidone. The protective agent can be N, N, N-trimethyl-(11-mercaptoundecyl) ammonium chloride alone, or N, N, N-trimethyl-(11-mercaptoundecyl) ammonium chloride and at least one of 11-mercaptoundecanoic acid, hexadecylamine, and polyvinyl pyrrolidone are compounded.
[0008] Furthermore, the raw materials of the nano-gold indicator solution include chloroauric acid solution, a protective agent and a reducing agent, and the reducing agent is at least one of sodium borohydride and Vc.
[0009] Another invention purpose: The present invention also provides a microbial concentration indicating device based on nanogold particles, characterized in that it includes a nanogold indicator solution that can be built into a closed container, the nanogold indicator solution includes nanogold particles with a particle size of 20-90nm, the surface of the nanogold particles has a positive charge, and the nanogold indicator solution indicates a concentration of 100CFU / mL-1000CFU / mL.
[0010] Furthermore, it also includes a closed container, a microorganism sampler, a filter with a filter membrane and a physiological saline bottle, and the closed container is made of plastic or glass.
[0011] Another invention purpose: The present invention also provides a method for preparing a microbial concentration indicator liquid based on nanogold particles, characterized in that it comprises the following steps: first, adding a protective agent to a chloroauric acid solution, stirring evenly at 20-50°C, then adding a reducing agent, stirring until the solution is red, centrifuging at 20-50°C to remove the supernatant, repeating the above centrifugation process twice after replenishing water, and finally diluting the obtained sediment with a buffer solution with a pH of 5.8-7.8 to obtain a nanogold indicator liquid, wherein the molar ratio between the chloroauric acid solution and the protective agent and the reducing agent is 1:(10-1000):(1-2000), and the protective agent includes or only contains N,N,N-trimethyl-(11-mercaptoundecyl)ammonium chloride.
[0012] Furthermore, the protective agent includes N,N,N-trimethyl-(11-mercaptoundecyl)ammonium chloride, and the protective agent also includes 1-3 of 11-mercaptoundecanoic acid, hexadecylamine, and polyvinylpyrrolidone.
[0013] Furthermore, the reducing agent is at least one of sodium borohydride and Vc.
[0014] Another invention purpose: The present invention also provides a method for using a microorganism concentration indicator liquid based on nanogold particles or a microorganism concentration indicator device based on nanogold particles, characterized in that it includes the following steps: aspirating a sample liquid with a sampler, filtering the sample liquid with a filter with a filter membrane, then washing the filter membrane with physiological saline, adding the washed solution to the nanogold indicator liquid, and observing the color change.
[0015] Another invention purpose: The present invention also provides a microorganism concentration indicator liquid based on nanogold particles as claimed in claim 1, or a microorganism concentration indicator liquid based on nanogold particles obtained by the preparation method as claimed in claim 6, or a microorganism concentration indicator device as claimed in claim 5, characterized in that: it is used for detecting bacterial communities and / or fungal communities in water quality testing or instrument disinfection and sterilization effect testing. In particular, it refers to bacteria and fungi with negative charges on the surface, and other microorganisms with negative charges on the surface or microorganisms that can be made to have negative charges on the surface by changing conditions.
[0016] By adopting the above scheme, the microbial concentration indicator liquid of the present invention has the advantages of easy operation, rapidity, accuracy and portability in the detection of bacterial and fungal communities. The color change can be observed by the naked eye for interpretation after 1 hour of detection, and is suitable for application in water quality testing, instrument cleaning and disinfection effect testing, etc.
[0017] The present invention is further described below in conjunction with specific implementation modes. DETAILED DESCRIPTION
[0018] 1. The specific embodiment of the present invention is prepared according to the following steps:
[0019] S1. Add chloroauric acid solution to the protective agent, then add the reducing agent, heat to 30-50℃ and stir.
[0020] S2. Add reducing agent and continue stirring at the temperature of S1 until the solution turns red.
[0021] S3, centrifuge at 10000r / min, 30-50℃ for 15min, remove the supernatant, add water to 10mL, repeat the above centrifugation process twice, and finally dilute the obtained sediment to half of the original volume with pH=5.8-7.8 buffer to obtain nanogold indicator solution.
[0022] The sampler was used to draw different concentrations of Escherichia coli samples, and the samples were filtered with a filter with a filter membrane, and then the filter membrane was washed with physiological saline. The washed solution was added to the nano-gold indicator solution to observe the color change. The specific raw materials and process conditions involved in the following examples are shown in Table 1, and the specific results are shown in Table 2.
[0023] Table 1 Material addition and production conditions of different embodiments
[0024]
[0025]
[0026] In the above examples, in Examples 1-5, the variables are the molar ratios of chloroauric acid solution to the protective agent and the reducing agent; in Examples 6-11, different protective agents are used; in Example 12, compared with Example 11, a different reducing agent Vc is used; in Examples 13-14, compared with Example 11, different reaction process temperatures are used; in Examples 15-16, different pH buffers are used compared with Example 14. Among them, the centrifugation temperature of Example 17 is 30°C, and a buffer with pH=7.5 is used.
[0027] During the preparation of the nano-gold particle indicator solution of the present invention, the nano-gold seed solution can be added after the protective agent is added and before the reducing agent is added.
[0028] Embodiment 18
[0029] S1. Add 5 mL of 0.001 M chloroauric acid solution to 5 mL of 0.2 M N, N-trimethyl-(11-mercaptoundecyl)ammonium chloride and 1 g of 11-mercaptoundecanoic acid, and stir at 30°C.
[0030] S2. Add 0.006 g of sodium citrate to 10 mL of 0.00035 M chloroauric acid solution, and then add 0.3 mL of 0.1 M sodium borohydride, and stir for 2-5 hours to prepare a seed solution.
[0031] S3. Add 0.05 mL of 0.1 M Vc solution to S1. Take 1.2 mL of the seed solution in S2 and add it to S1 while stirring. Stir at 30°C until the solution turns deep red.
[0032] S4, centrifuge at 10000r / min, 30℃ for 15min, remove the supernatant, add water to 10mL, repeat the above centrifugation process twice, and finally dilute the obtained sediment to half of the original volume with pH=6.0 buffer to obtain nanogold indicator solution.
[0033] Use a sampler to absorb Escherichia coli samples of different concentrations, filter the sample using a filter with a filter membrane, then wash the filter membrane with physiological saline, add the washed solution into the nanogold indicator solution, and observe the color change.
[0034] Embodiment 19
[0035] S1. Add 5 mL of 0.0005 M chloroauric acid solution to 5 mL of 0.1 M N, N-trimethyl-(11-mercaptoundecyl)ammonium chloride and 0.5 g of hexadecylamine, and stir at 30°C.
[0036] S2. Add 1 mL of 0.25 mM sodium citrate to 10 mL of 0.00025 M chloroauric acid solution, and then add 2.5 mL of 1 M sodium borohydride, and stir for 2-5 hours to prepare a seed solution.
[0037] S3. Add 0.1 mL of 0.1 M Vc alkaline solution to S1. Take 0.1 mL of the seed solution in S2 and add it to S1 while stirring. Stir at 30°C until the solution turns deep red.
[0038] S4, centrifuge at 10000r / min, 30℃ for 15min, remove the supernatant, add water to 10mL, repeat the above centrifugation process twice, and finally dilute the obtained sediment to half of the original volume with pH=7.0 buffer to obtain nanogold indicator solution.
[0039] Use a sampler to absorb Escherichia coli samples of different concentrations, filter the sample using a filter with a filter membrane, then wash the filter membrane with physiological saline, add the washed solution into the nanogold indicator solution, and observe the color change.
[0040] The above-mentioned comparative example 1 is prepared according to the document "Nan Caiyun, Zhang Yu et al. Basic Experiment: Preparation of Gold Nanoparticles and Their Optical Properties [J]." as follows: 20 mL of 0.01% chloroauric acid solution is placed in a 50 mL round-bottom flask, a magnetic rod is placed, a spherical condenser is installed, and the mixture is heated to boiling. While stirring at high speed, 2 mL of 1% sodium citrate solution is quickly added, and the mixture is refluxed for 10 min under vigorous stirring, the heat source is removed, stirring is continued for 15 min, and the solution is cooled to room temperature.
[0041] The above-mentioned comparative example 2 uses the cationic surfactant CTAB, which is conventionally selected in the art, as a protective agent to prepare the indicator solution. The specific steps are as follows: S1, add 5 mL of 0.0005 M chloroauric acid solution to 5 mL of 0.2 M CTAB, then add 0.5 mL of 0.2 M polyvinyl pyrrolidone, and heat to 40° C. and stir.
[0042] S2. Add 1 mL of 1 M sodium borohydride and continue stirring at 40 °C until the solution turns red.
[0043] S3. Centrifuge at 10,000 r / min, 30°C for 15 min, remove the supernatant, add water to 10 mL, repeat the above centrifugation process twice, and finally dilute the obtained sediment to half of the original volume with a pH = 7.5 buffer to obtain the nanogold indicator solution.
[0044] 2. The specific results are shown in Table 2:
[0045] Table 2 Color indication results of different embodiments under different microbial concentration conditions
[0046]
[0047]
[0048] 3. Results Analysis and Summary
[0049] Compared with Comparative Experiment 1, Examples 1-5 and 9-19 differ in that the preparation temperature conditions are different, and no protective agent is added in Comparative Experiment 1. The surface of the nanogold particles prepared in Comparative Experiment 1 is negatively charged, and the indicator liquid does not change color in detecting bacteria and fungal communities, indicating that the selection of preparation conditions and protective agents is particularly important.
[0050] Compared with Examples 6-8 and Comparative Experiment 2, Examples 1-5, 9-19 differ in that different protective agents are used. Although the protective agent used in Comparative Experiment 1 is also a cationic surfactant, theoretically the surface of the synthesized nanogold particles should be positively charged, but in fact, its surface is negatively charged. The results show that the indicator liquid does not change color in detecting bacteria and fungal communities, indicating that the selection of the protective agent is crucial.
[0051] The present invention is not limited to the above-mentioned specific implementation modes. A person skilled in the art may adopt other various specific implementation modes to implement the present invention based on the contents disclosed in the present invention, or any simple changes or modifications made to the design structure and concept of the present invention shall fall within the protection scope of the present invention.
Claims
1. A microbial concentration indicator solution based on nano-gold particles, characterized in that: The invention comprises a nano-gold indicator solution which can be built into a closed container, wherein the nano-gold indicator solution comprises nano-gold particles with a particle size of 20-90 nm, the surface of the nano-gold particles carries a positive charge, and the nano-gold indicator solution indicates a concentration of 100 CFU / mL-1000 CFU / mL. The raw materials of the nano-gold indicator solution include chloroauric acid solution, a protective agent and a reducing agent, wherein the protective agent includes N,N,N-trimethyl-(11-mercaptoundecyl)ammonium chloride, and the protective agent also includes 0-3 of 11-mercaptoundecanoic acid, hexadecylamine, and polyvinylpyrrolidone. The raw materials of the nano-gold indicator solution include chloroauric acid solution, a protective agent, and a reducing agent in a molar ratio of 1: (10-1000): (1-2000). The reducing agent is at least one of sodium borohydride and Vc.
2. An indicating device comprising the microorganism concentration indicating liquid based on nano-gold particles as claimed in claim 1, characterized in that: It also includes a closed container, a microbial sampler, a filter with a filter membrane and a physiological saline bottle, and the closed container is made of plastic or glass.
3. A method for preparing a microbial concentration indicator solution based on nanogold particles, characterized in that: The method comprises the following steps: firstly, adding a protective agent to a chloroauric acid solution, stirring evenly at 20-50°C, then adding a reducing agent, stirring until the solution turns red, centrifuging at 20-50°C to remove a supernatant, replenishing water, repeating the step of centrifuging at 20-50°C to remove a supernatant twice, and finally diluting the obtained sediment with a buffer solution with a pH of 5.8-7.8 to obtain a nano-gold indicator solution, wherein the molar ratio of the chloroauric acid solution to the protective agent and the reducing agent is 1: (10-1000): (1-2000), and the protective agent comprises N, N, N-trimethyl-(11-mercaptoundecyl)ammonium chloride; The protective agent also includes 1-3 of 11-mercaptoundecanoic acid, hexadecylamine, and polyvinyl pyrrolidone; The reducing agent is at least one of sodium borohydride and Vc.
4. A method for using a microorganism concentration indicating liquid, wherein the microorganism concentration indicating liquid is the microorganism concentration indicating liquid based on nanogold particles according to claim 1, or the microorganism concentration indicating liquid is derived from the indicating device of the microorganism concentration indicating liquid based on nanogold particles according to claim 2, or the microorganism concentration indicating liquid is the microorganism concentration indicating liquid prepared by the preparation method according to claim 3, characterized in that: The following steps are involved: The sample liquid is drawn up with a sampler, filtered with a filter with a membrane, and then the membrane is washed with physiological saline. The washed solution is added to the nanogold indicator solution to observe the color change.
Citation Information
Patent Citations
Preparation method of gold nanometer belt
CN108247039A
Preparation of gold@graphene oxide composite nanomaterial and application in detection of adenosine triphosphate
CN110343522A
Nano-gold colorimetric method for quickly detecting food-borne pathogenic bacteria based on low pH
CN110687110A
Direct detection of disease biomarkers in clinical specimens using cationic nanoparticle-based assays & versatile and green methods for synthesis of anisotropic silver nanostructures
US20150017258A1
MTAB-TA-Coated Gold Nanorods and Method of Fabrication
US20180169023A1