A method for matching lithium-ion batteries
Through the three-sieving method, the rated capacity, internal resistance, charge holding capacity and operating voltage difference under SOC were used to solve the problems of low accuracy and high cost of lithium-ion battery distribution, and achieve efficient and accurate consistency Set the set to ensure the long-term performance stability of the battery pack.
Patent Information
- Application Number
- CN202010413787.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-05-15
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2040-05-15
AI Technical Summary
The existing lithium-ion battery packing methods are low in accuracy and high in cost, which affects the cycle life and safety performance of the battery pack.
Three-time screening method is adopted: the first screening passes the rated capacity and rated internal resistance rating, the second screening passes the charge holding capacity and capacity recovery ability test, and the third screening passes the working voltage under different SOCs. If the unqualified single cells are eliminated to ensure consistency.
It improves the accuracy and efficiency of lithium-ion battery assembly, ensures that the battery module still has good capacity performance after long-term shelving, and reduces the overall time and cost of the assembly process.
Smart Images

Figure CN113671397B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of lithium ion battery sorting, and in particular relates to a method for consistent grouping of lithium ion batteries. Background Art
[0002] In the prior art, lithium-ion batteries have the advantages of high energy density, long service life and low self-discharge rate, and have been widely used in energy storage and electric vehicles. At present, the development of lithium battery technology has been centered on controlling costs, improving the energy density and power density of lithium batteries, enhancing safety, extending service life and improving group consistency. Among them, in terms of group consistency, the inconsistency of single cells is an important factor affecting the performance of the battery pack. When there is obvious inconsistency between the single cells after grouping, the available capacity of the battery pack will be reduced, which will reduce the cycle life of the battery pack.
[0003] In order to increase the number of cycles of battery packs, it is necessary to select single cells with longer service life to form a battery pack. However, in order to improve the overall performance of the battery pack and obtain a longer service life and higher safety performance, attention should also be paid to the consistency of the single cells. At present, there are various battery sorting and grouping methods in the industry, mainly including static sorting and grouping methods and dynamic sorting and grouping methods. Among them, the static sorting and grouping method is based on open circuit voltage, internal resistance, capacity or self-discharge parameters for sorting and grouping, and the accuracy is not high; the dynamic sorting and grouping method is generally based on the charge and discharge current and voltage curve sorting and grouping method, but this method has high requirements on equipment and requires special lithium-ion battery charging and discharging equipment, which is costly. Summary of the invention
[0004] The purpose of the present invention is to provide a consistency matching method for lithium ion batteries, which is used to solve the problems of low accuracy and high cost of the existing matching methods.
[0005] Based on the above purpose, a technical solution of a lithium-ion battery consistency matching method is as follows:
[0006] Perform the first screening of the single cells: measure the internal resistance and capacity of each single cell, group each single cell according to the set internal resistance classification standard, and classify each single cell in each group according to the set capacity classification standard;
[0007] Performing a second screening of the single cells: performing a charge retention capacity test and a capacity recovery capacity test on each single cell in the same gear, and removing single cells that fail the charge retention capacity test and the capacity recovery capacity test in the gear;
[0008] Performing a third screening of the single cells: in the process of performing the capacity recovery ability test, obtaining the working voltage of each single cell at the first discharge capacity, comparing the pressure difference between the highest working voltage and the lowest working voltage, obtaining a first pressure difference, and eliminating the single cells whose first pressure difference does not meet the first set pressure difference range;
[0009] The operating voltage of each single cell at the second discharge capacity is obtained, and the voltage difference between the highest operating voltage and the lowest operating voltage is compared to obtain a second voltage difference, and single cells whose second voltage difference does not meet the second set voltage difference range are eliminated. The second discharge capacity is less than the first discharge capacity.
[0010] The beneficial effects of the above technical solution are:
[0011] The consistency grouping method of the present invention realizes the first screening by dividing the rated capacity and rated internal resistance into multiple gear groups; the second screening is carried out by charging retention capacity and capacity recovery capacity test; the third screening is realized by working voltage difference under different SOC, which ensures the consistency of lithium-ion battery grouping and has high accuracy. In the three screening processes, the first screening needs to measure the capacity and internal resistance of the single cell, and the screening is carried out by the rated capacity and rated internal resistance. The initial screening takes a short time and is efficient; the third screening is carried out by the discharge capacity data in the second screening process, and no additional testing is required. The screening time is short and the efficiency is high. In comparison, the time for testing during the second screening is longer than that of the first and third screenings, but the overall screening efficiency is higher. In addition, the second screening process carried out by the present invention fully takes into account the requirements of the reversible capacity and irreversible capacity of the battery module for consistency during long-term shelving, which can ensure that the battery module still has good capacity performance after long-term shelving.
[0012] Furthermore, the internal resistance classification of each single cell according to the set internal resistance classification standard includes:
[0013] The internal resistance is divided into three grades: 80-90%, 70-80%, and 60-70% based on 10% of the rated internal resistance of the single cell, and the internal resistance of the single cell is not higher than 90% of the rated internal resistance, nor lower than 60% of the rated internal resistance.
[0014] Alternatively, taking 10% of the rated internal resistance of the single cell as the internal resistance classification standard, and the internal resistance of the single cell is not higher than the rated internal resistance, nor lower than 70% of the rated internal resistance, the internal resistance is divided into three grades: 90-100%, 80-90%, and 70-80%.
[0015] Furthermore, the further grading of each single cell in each grading according to the set capacity grading standard includes:
[0016] The capacity classification standard is 2.5% of the rated capacity of a single cell, and the capacity of a single cell is not less than the rated capacity, nor more than 110% of the rated capacity; the capacity is divided into four grades: 100-102.5%, 102.5-105%, 105-107.5%, 107.5-110%;
[0017] Alternatively, 2% of the rated capacity of the single cell is used as the capacity classification standard, and the capacity of the single cell is not less than the rated capacity, nor more than 106% of the rated capacity; the capacity is divided into three grades: 100-102%, 102-104%, and 104-106%.
[0018] Furthermore, in the second screening process, the single cells that fail the charge retention capacity test are single cells whose charge retention capacity is lower than the first set value.
[0019] Furthermore, the calculation formula of the charge retention capacity is as follows:
[0020]
[0021] Where Q% is the charge retention capability, Qo is the charge of the single cell after being stored for a set time and discharged, and Qn is the rated charge of the single cell.
[0022] Furthermore, in the second screening process, the single cells that fail the capacity recovery test are single cells whose capacity recovery is lower than the second set value.
[0023] Furthermore, the calculation formula of the capacity recovery capability is as follows:
[0024]
[0025] Where C% is the capacity recovery capability, Co is the recovery capacity, and Cn is the rated capacity.
[0026] Furthermore, the first set voltage difference range is 0-5 mV, and the second set voltage difference range is 0-20 mV. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 It is a flow chart of the consistency matching method of lithium ion batteries in Example 1 of the present invention. DETAILED DESCRIPTION
[0028] The specific implementation of the present invention will be further described below in conjunction with the accompanying drawings.
[0029] Embodiment 1:
[0030] This embodiment takes 8Ah lithium iron phosphate battery as an example to illustrate the consistency matching method of lithium ion batteries. Figure 1The specific steps of grouping are as follows:
[0031] (I) The first screening of single cells is carried out by grouping them according to rated capacity and rated internal resistance:
[0032] The internal resistance of a single cell is divided into three grades based on 10% of the rated internal resistance. The internal resistance of a single cell is not higher than the rated internal resistance, nor lower than 60% of the rated internal resistance. The internal resistance is divided into three grades: 80-90%, 70-80%, and 60-70%.
[0033] For each single cell in each internal resistance classification, the capacity classification is further performed, and the single cell is classified by 2.5% of the rated capacity, and the capacity of the single cell is not less than the rated capacity, nor more than 110% of the rated capacity; the capacity is divided into four grades: 100-102.5%, 102.5-105%, 105-107.5%, 107.5-110%. According to the above content, the specific classification standards for the first screening are shown in Table 1.
[0034] Table 1
[0035]
[0036] In the above table, capacity Q represents the rated capacity of the single cell, in mAh; voltage U represents the open circuit voltage of the single cell, in V; internal resistance R represents the rated internal resistance of the single cell, in mΩ; gear Ai-j, i represents the internal resistance grade, i=1,2,3; j represents the capacity grade, j=1,2,3,4.
[0037] Taking into account the module pressure difference problem after long-term use or long-term storage of the battery, in the screening of this step, screening is also carried out according to the open circuit voltage of the single cell, in order to effectively alleviate the impact of excessive pressure difference on the life of the battery module.
[0038] (II) By testing the battery's charge retention and capacity recovery capabilities, a second screening of the single cells in each gear Ai-j is performed:
[0039] For each single cell in the same gear, discharge it to 2.5V at 0.5C constant current and then place it aside for 30 minutes. Charge it to 3.65V at 0.5C constant current and then switch to constant voltage charging. When the charging current drops to 0.05C, stop charging. Place it at 20±5℃ for 28 days. Then discharge it to 2.5V at 0.5C and test its charge retention ability. The charge retention ability is required to be not less than 96%. Therefore, the single cells with charge retention ability less than 96% will be removed from the current grouping.
[0040] In this step, the charge retention capacity refers to the ability of the battery to retain the amount of electricity stored in the battery under certain conditions when the battery is in an open circuit state. The calculation formula is:
[0041]
[0042] Where Q% is the charge retention capacity, Qo is the amount of charge when the battery is discharged to 2.5V at 0.5C after being stored for 28 days, and Qn is the rated capacity of the battery.
[0043] After testing the charge retention capability, the remaining single cells in the current group are charged and discharged three times. The process of each charge and discharge is as follows:
[0044] After charging to 3.65V at a constant current of 0.5C, switch to constant voltage charging. Stop charging when the charging current drops to 0.05C. After leaving it alone for 30 minutes, discharge to 2.5V at a constant current of 0.5C.
[0045] After the above process is cycled three times, the third (i.e., last) discharge capacity data is recorded, and the last discharge capacity (i.e., recovery capacity) is used as the evaluation standard for evaluating the capacity recovery ability, with the requirement that the capacity recovery ability (the ratio of recovery capacity to rated capacity) is not less than 98%. Single cells with a test capacity recovery ability lower than 98% are removed from the current grouping.
[0046] In this step, the calculation formula of its capacity recovery capability is as follows:
[0047]
[0048] Where C% is the capacity recovery capability, Co is the recovery capacity, i.e. the last discharge capacity, and Cn is the rated capacity.
[0049] (III) The pressure difference is calculated by the working voltage under different SOCs, and the third screening of the single cells in each gear Ai-j is performed:
[0050] In the third discharge process, the working voltages at the discharge capacities of 50% SOC and 95% SOC are used as calculation points to calculate their respective pressure differences, that is, the working voltages of the single cells in the current group at the discharge capacity of 4Ah are calculated to obtain the working voltages of several single cells, for example, 1.667, 1.664, 1.665, 1.665, 1.666, 1.661, 1.662, 1.662, 1.663, 1.661, 1.665. The pressure difference between the highest working voltage and the lowest working voltage is compared to obtain the first pressure difference ΔV1, which is calculated as follows:
[0051] ΔV1=Vh1-Vl1
[0052] Wherein, Vh1 is the maximum voltage of the single cell when the discharge capacity is 50% SOC, Vl1 is the minimum voltage of the single cell when the discharge capacity is 50% SOC. According to the working voltage given above, Vh1=1.667, Vl1=1.661 are determined, so ΔV1=0.006V=6mV.
[0053] Similarly, the operating voltage of each single cell in the current combination is calculated when the discharge capacity is 7.7 Ah, and the operating voltages of several single cells are obtained, for example, 0.182, 0.168, 0.178, 0.175, 0.169, 0.173, 0.164, 0.171, 0.170, 0.155, 0.173. The voltage difference between the highest operating voltage and the lowest operating voltage is compared to obtain the second voltage difference ΔV2, which is calculated as follows:
[0054] ΔV2=Vh2-Vl2
[0055] Wherein, Vh2 is the highest voltage of the single cell when the discharge capacity is 50% SOC, Vl2 is the lowest voltage of the single cell when the discharge capacity is 50% SOC, according to the working voltage given above, Vh2=0.182, Vl2=0.155, so ΔV2=0.027V=27mV.
[0056] In this step, the third screening standard is that when the battery is assembled, the first voltage difference ΔV1 of the working voltage of the single battery in the battery pack is required to be no higher than 5mV at 50% SOC, and the second voltage difference ΔV2 of the working voltage is no higher than 20mV at 95% SOC. The mathematical expression is as follows:
[0057]
[0058] Wherein, ΔV1 is the voltage difference between the highest working voltage and the lowest working voltage of the single cell when the discharge capacity is 4Ah, and ΔV2 is the voltage difference between the highest working voltage and the lowest working voltage of the single cell when the discharge capacity is 7.7Ah.
[0059] After obtaining the first pressure difference and the second pressure difference, the single cells with the first pressure difference higher than 5mV are removed from the current grouping, and the single cells with the second pressure difference higher than 20mV are removed from the current grouping. Therefore, according to the calculated results, ΔV1=6mV, ΔV2=27mV, which do not meet the third screening standard, and the first single cell and the tenth single cell are removed.
[0060] Then, in the remaining single cells of the current group, the first pressure difference and the second pressure difference are calculated again according to the above steps, and compared until the first differential pressure and the second pressure difference meet the above third screening standard, that is, the first pressure difference is not higher than 20mV and the second pressure difference is not higher than 5mV. In this embodiment, according to the remaining nine single cells of the current group, the first pressure difference ΔV1=1.666-1.661=5mV and the second pressure difference ΔV2=0.178-0.164=14mV are calculated again, which meet the third screening standard and the single cells are no longer eliminated.
[0061] In this embodiment, the first pressure difference and the second pressure difference are calculated when the discharge capacity is 50% SOC (first discharge capacity) and 95% SOC (second discharge capacity), respectively. As other implementation methods, other values may also be used, such as 45% SOC (first discharge capacity) and 90% SOC (second discharge capacity). The specific discharge capacity value is not limited in this embodiment. It should be noted that when setting the two discharge capacities, it is necessary to ensure that the difference between the two discharge capacities is not too small. In this embodiment, it is preferably not less than 30% SOC.
[0062] In this embodiment, in order to eliminate the single cells that fail the charge retention test, the minimum limit of the charge retention capacity is set to 96%. As other implementations, the minimum limit can also be other percentages, such as 95%. Similarly, in order to eliminate the single cells that fail the capacity recovery test, the minimum limit of the capacity recovery capacity is set to 98%. As other implementations, the minimum limit can also be other percentages, such as 96%.
[0063] The consistency grouping method of the present invention realizes the first screening by grouping the rated capacity and the rated internal resistance into multiple gears; performs the second screening by testing the charge retention ability and the capacity recovery ability; and realizes the third screening by the working voltage difference under different SOCs, thereby ensuring the consistency of lithium-ion battery grouping with high accuracy.
[0064] Overall, during the three screening processes, the first screening requires the capacity and internal resistance of the single cell to be measured, and the screening is performed by the rated capacity and rated internal resistance. The initial screening takes a short time and is highly efficient; the third screening is performed based on the discharge capacity data during the second screening process, and no additional testing is required. The screening time is short and the efficiency is high. In comparison, the time for testing during the second screening is longer than that of the first and third screenings, but the overall screening efficiency is higher. In addition, the second screening process performed by the present invention fully takes into account the requirements of the reversible capacity and irreversible capacity of the battery module for consistency during long-term storage, which can ensure that the battery module still has good capacity performance after long-term storage.
[0065] The consistency matching method of the present invention performs multiple screenings based on the basic characteristics of the battery. Since these characteristics are often the most likely to cause module abnormalities during battery use, it has universal applicability and industrial application prospects.
[0066] Embodiment 2:
[0067] The steps of the lithium-ion battery consistency matching method of this embodiment are as follows:
[0068] (I) The first screening of single cells is carried out by grouping them according to rated capacity and rated internal resistance:
[0069] The internal resistance of a single cell is divided into three grades based on 10% of the rated internal resistance. The internal resistance of a single cell is not higher than the rated internal resistance, nor lower than 70% of the rated internal resistance. The internal resistance is divided into three grades: 90-100%, 80-90%, and 70-80%.
[0070] The capacity of each single cell in each internal resistance classification is classified, and the single cell is classified by 2% of the rated capacity. The capacity of the single cell is not less than the rated capacity, nor more than 106% of the rated capacity; the capacity is divided into three classes: 100-102%, 102-104%, and 104-106%. According to the above content, the specific classification standards for the first screening are shown in Table 2.
[0071] Table 2
[0072]
[0073]
[0074] (ii) By testing the charge retention and capacity recovery capabilities of the battery, a second screening of the single cells in each gear Ai-j is performed.
[0075] (III) The pressure difference is calculated by the working voltage under different SOCs, and the single cells are screened for the third time in each gear Ai-j.
[0076] The implementation process of step (ii) and step (iii) of the consistency matching method of this embodiment is the same as step (ii) and step (iii) in embodiment 1, and will not be repeated here. Unlike step (i) of embodiment 1, step (i) of this embodiment adopts different rated capacity and rated internal resistance classification standards to increase the matching efficiency of the battery. In addition, in step (i) of this embodiment, there is no need to perform initial screening according to the open circuit voltage of the battery. Through the screening in step (iii), the influence of the pressure difference on the life of the battery module can be solved.
[0077] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention rather than to limit it. Although the present invention is described in detail with reference to the above embodiments, those skilled in the art should understand that the specific implementation methods of the present invention can still be modified or replaced by equivalents. For example, the capacity grading in Example 2 can be replaced by the capacity grading in Example 1, and the internal resistance grading in Example 1 can be replaced by the internal resistance grading in Example 2, etc. Therefore, any modification or equivalent replacement that does not depart from the spirit and scope of the present invention should be included in the protection scope of the claims of the present invention.
Claims
1. A method for matching lithium-ion batteries, characterized in that: The following steps are involved: Perform the first screening of the single cells: measure the internal resistance and capacity of each single cell, group each single cell according to the set internal resistance classification standard, and classify each single cell in each group according to the set capacity classification standard; Performing a second screening of the single cells: performing a charge retention capacity test and a capacity recovery capacity test on each single cell in the same gear, and removing single cells that fail the charge retention capacity test and the capacity recovery capacity test in the gear; Performing a third screening of the single cells: in the process of performing the capacity recovery ability test, obtaining the working voltage of each single cell at the first discharge capacity, comparing the pressure difference between the highest working voltage and the lowest working voltage, obtaining a first pressure difference, and eliminating the single cells whose first pressure difference does not meet the first set pressure difference range; The operating voltage of each single cell at the second discharge capacity is obtained, and the voltage difference between the highest operating voltage and the lowest operating voltage is compared to obtain a second voltage difference, and single cells whose second voltage difference does not meet the second set voltage difference range are eliminated. The second discharge capacity is less than the first discharge capacity.
2. The method for matching lithium-ion batteries according to claim 1, characterized in that: The internal resistance classification of each single cell according to the set internal resistance classification standard includes: The internal resistance is divided into three grades: 80-90%, 70-80%, and 60-70% based on 10% of the rated internal resistance of the single cell, and the internal resistance of the single cell is not higher than 90% of the rated internal resistance, nor lower than 60% of the rated internal resistance. Alternatively, taking 10% of the rated internal resistance of the single cell as the internal resistance classification standard, and the internal resistance of the single cell is not higher than the rated internal resistance, nor lower than 70% of the rated internal resistance, the internal resistance is divided into three grades: 90-100%, 80-90%, and 70-80%.
3. The method for matching lithium ion batteries according to claim 1 or 2, characterized in that: The further grading of each single cell in each grading according to the set capacity grading standard includes: The capacity classification standard is 2.5% of the rated capacity of a single cell, and the capacity of a single cell is not less than the rated capacity, nor more than 110% of the rated capacity; the capacity is divided into four grades: 100-102.5%, 102.5-105%, 105-107.5%, 107.5-110%; Alternatively, 2% of the rated capacity of the single cell is used as the capacity classification standard, and the capacity of the single cell is not less than the rated capacity, nor more than 106% of the rated capacity; the capacity is divided into three grades: 100-102%, 102-104%, and 104-106%.
4. The method for matching lithium-ion batteries according to claim 1, characterized in that: In the second screening process, the single cells that fail the charge retention capacity test are single cells whose charge retention capacity is lower than the first set value.
5. The method for matching lithium ion batteries according to claim 1 or 4, characterized in that: The calculation formula of the charge retention capacity is as follows: Where Q% is the charge retention capability, Qo is the charge of the single cell after being stored for a set time and discharged, and Qn is the rated charge of the single cell.
6. The method for matching lithium-ion batteries according to claim 1, characterized in that: In the second screening process, the single cells that fail the capacity recovery test are single cells whose capacity recovery is lower than the second set value.
7. The method for matching lithium ion batteries according to claim 1 or 6, characterized in that: The calculation formula of the capacity recovery capability is as follows: Where C% is the capacity recovery capability, Co is the recovery capacity, and Cn is the rated capacity.
8. The method for matching lithium-ion batteries according to claim 1, characterized in that: The first set voltage difference range is 0-5mV, and the second set voltage difference range is 0-20mV.