Inorganic light emitting diode chip and manufacturing method thereof

By filling the support reinforcement layer in the inorganic light emitting diode chip master chip, the problems of chip thickness and strength are solved, and a thin and strong chip structure is realized, suitable for the application of display products, and the production and display effect of optical structures are improved.

CN113767480BActive Publication Date: 2024-11-12BOE TECHNOLOGY GROUP CO LTD +1
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202080000439.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-03-31
Publication Date
2024-11-12
Estimated Expiration
2040-03-31

AI Technical Summary

Technical Problem

The existing inorganic light-emitting diode chips have thicker thickness, making it difficult to make optical structures, and are fragile, making it difficult to perform spot measurement and transfer, affecting the application of display products.

Method used

Provide an inorganic light emitting diode chip master piece, including an epitaxial layer, multiple liners and support reinforcement layers. By filling the support reinforcement layer between the liners, the strength of the chip is enhanced, and through reasonable thickness and material selection, the chip is ensured. Stability in segmentation and transfer.

Benefits of technology

The inorganic light-emitting diode chip is achieved with a thinner thickness and high intensity, and can withstand the force applied during point measurement and transfer, reducing the difficulty of producing optical structures and improving the regulation effect of the luminescent light type.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113767480B_ABST
    Figure CN113767480B_ABST
Patent Text Reader

Abstract

Provided is an inorganic light-emitting diode chip mother sheet, comprising: an epitaxial layer, a plurality of pads and a support reinforcement layer. The two opposite sides of the epitaxial layer are a first side and a second side respectively; the plurality of pads are arranged on the first side of the epitaxial layer; and the support reinforcement layer fills the gaps between the plurality of pads.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the field of display technology, and in particular to an inorganic light emitting diode chip mother sheet, an inorganic light emitting diode chip and a manufacturing method thereof, and a light emitting diode light emitting device. Background Art

[0002] A mini LED (mini Organic Light-Emitting Diode) display device or a micro LED (micro Organic Light-Emitting Diode) display device is a display device composed of a large number of small-size LED arrays. It has the advantages of high brightness, clear display image and low power consumption, and has good application prospects. Summary of the invention

[0003] On the one hand, an inorganic light-emitting diode chip mother sheet is provided, comprising: an epitaxial layer, a plurality of pads and a support reinforcement layer. The two opposite sides of the epitaxial layer are a first side and a second side respectively; the plurality of pads are arranged on the first side of the epitaxial layer; and the support reinforcement layer fills the gaps between the plurality of pads.

[0004] In some embodiments, the ratio of the thickness of the epitaxial layer to the thickness of the liner is in the range of 1:6 to 1:2.

[0005] In some embodiments, at least one liner has a thickness of 20 μm to 30 μm.

[0006] In some embodiments, the material of each pad includes at least one of copper, aluminum, and a copper-aluminum alloy.

[0007] In some embodiments, each pad includes a pad body, and a protection layer covering a sidewall of the pad body and a surface away from the epitaxial layer; the protection layer is conductive.

[0008] In some embodiments, the material of the pad body includes at least one of copper, aluminum, and copper-aluminum alloy, and the material of the protective layer includes nickel-gold.

[0009] In some embodiments, the thickness of the support reinforcement layer is 20 μm to 30 μm.

[0010] In some embodiments, the surface of the support reinforcement layer away from the epitaxial layer is flush with the surfaces of the plurality of pads away from the epitaxial layer. Alternatively, the surface of the support reinforcement layer away from the epitaxial layer is lower than the surfaces of the plurality of pads away from the epitaxial layer.

[0011] In some embodiments, the material of the support reinforcement layer includes a curing glue material.

[0012] In some embodiments, the material of the support reinforcement layer includes silica gel, epoxy resin or photoresist.

[0013] In some embodiments, the support reinforcement layer is white or black.

[0014] In some embodiments, when the support reinforcement layer is white, the material of the support reinforcement layer includes titanium dioxide. When the support reinforcement layer is black, the material of the support reinforcement layer includes carbon powder.

[0015] In some embodiments, a surface of the first side of the epitaxial layer has a plurality of protrusions, and the plurality of protrusions are embedded in the supporting and reinforcing layer.

[0016] In some embodiments, the epitaxial layer has a thickness of 5 μm to 10 μm.

[0017] In some embodiments, the inorganic light emitting diode chip mother sheet has a plurality of inorganic light emitting diode chip regions; the plurality of pads include a plurality of first pads and a plurality of second pads; the epitaxial layer includes a plurality of epitaxial layer units, and each inorganic light emitting diode chip region is provided with an epitaxial layer unit, a first pad and a second pad.

[0018] The epitaxial layer unit includes: a first semiconductor layer, a light-emitting layer, a second semiconductor layer and a flat layer. The first semiconductor layer includes a first part and a second part, the light-emitting layer is arranged on one side of the first part of the first semiconductor layer, the second semiconductor layer is arranged on the side of the light-emitting layer away from the first semiconductor layer, and the flat layer covers the side of the second semiconductor layer away from the light-emitting layer. The flat layer has a first through hole and a second through hole, and in each of the inorganic light-emitting diode chip regions, the first pad is coupled to the first semiconductor layer through the first through hole, and the second pad is coupled to the second semiconductor layer through the second through hole.

[0019] In some embodiments, the epitaxial layer unit further includes: a first contact electrode, an insulating layer, a conductive layer, and a second contact electrode. The first contact electrode is disposed between the second portion of the first semiconductor layer and the planar layer; the first contact electrode is in electrical contact with the second portion of the first semiconductor layer, and the first pad is coupled to the first contact electrode through the first through hole.

[0020] An insulating layer is disposed between the second semiconductor layer and the planar layer. A conductive layer is disposed between the insulating layer and the planar layer, and the conductive layer is in electrical contact with the second semiconductor layer. A second contact electrode is disposed between the conductive layer and the planar layer; the second contact electrode is in electrical contact with the conductive layer, and the second pad is coupled to the second contact electrode through the second through hole; and an orthographic projection of the second contact electrode on the first semiconductor layer at least partially overlaps with an orthographic projection of the insulating layer on the first semiconductor layer.

[0021] On the other hand, an inorganic light emitting diode chip is provided, which is obtained by a splitting process of the inorganic light emitting diode chip mother wafer as described above, and the inorganic light emitting diode chip includes: an epitaxial layer unit, a first pad and a second pad arranged on one side of the epitaxial layer unit, and a supporting reinforcement unit, wherein the supporting reinforcement unit is filled around the first pad and around the second pad.

[0022] In some embodiments, the thickness of the first pad and the second pad is 20 μm to 30 μm; the thickness of the supporting reinforcement unit is 20 μm to 30 μm.

[0023] On the other hand, a method for manufacturing an inorganic light emitting diode chip is provided, comprising: providing a substrate, forming an epitaxial layer on one side of the substrate; preparing a plurality of pads on a side of the epitaxial layer away from the substrate; forming a supporting reinforcement layer in gaps between the plurality of pads; and peeling the substrate from the epitaxial layer to obtain an inorganic light emitting diode chip mother wafer.

[0024] In some embodiments, the support reinforcement layer is formed in the gaps between the multiple pads, including: using an injection molding process or a lamination process to form a support reinforcement film on one side of the epitaxial layer where the multiple pads are formed; using a grinding process to remove a portion of the support reinforcement film that covers the surface of the multiple pads away from the epitaxial layer, so that the surfaces of the multiple pads away from the epitaxial layer are exposed.

[0025] In some embodiments, forming a support reinforcement layer in the gaps between the multiple pads includes: using a photoresist material to form a support reinforcement film on one side of the epitaxial layer where the multiple pads are formed; patterning the support reinforcement film to remove portions of the support reinforcement film covering surfaces of the multiple pads away from the epitaxial layer, so that surfaces of the multiple pads away from the epitaxial layer are exposed.

[0026] In some embodiments, the method for manufacturing an inorganic light emitting diode chip also includes: after peeling the substrate from the epitaxial layer to obtain an inorganic light emitting diode chip mother sheet, dividing the inorganic light emitting diode chip mother sheet into a plurality of inorganic light emitting diode chips; performing point testing on the plurality of inorganic light emitting diode chips respectively, and sorting the plurality of inorganic light emitting diode chips according to the point testing results.

[0027] In yet another aspect, a light emitting diode light emitting device is provided, comprising: an array substrate and a plurality of inorganic light emitting diode chips as described above disposed on the array substrate. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] In order to more clearly illustrate the technical solutions in the present disclosure, the following briefly introduces the drawings required to be used in some embodiments of the present disclosure. Obviously, the drawings described below are only drawings of some embodiments of the present disclosure. For ordinary technicians in this field, other drawings can also be obtained based on these drawings. In addition, the drawings described below can be regarded as schematic diagrams, and are not limitations on the actual size of the product involved in the embodiments of the present disclosure, the actual process of the method, the actual timing of the signal, etc.

[0029] Figure 1 is a structural diagram of an inorganic light emitting diode chip according to some embodiments of the related art;

[0030] Figure 2 is another structural diagram of an inorganic light emitting diode chip according to some embodiments of the related art;

[0031] Figure 3A is a structural diagram of a light emitting diode light emitting device according to some embodiments of the present disclosure;

[0032] Figure 3B is a comparison diagram of light emission patterns of inorganic light emitting diode chips according to some embodiments;

[0033] Figure 4 Based on Figure 3A Cross-sectional view obtained along the mid-section line AA'.

[0034] Figure 5A A structural diagram of an inorganic light emitting diode chip mother wafer according to some embodiments of the present disclosure;

[0035] Figure 5B is another structural diagram of an inorganic light emitting diode chip mother sheet according to some embodiments of the present disclosure;

[0036] Fig. 6A is a structural diagram of a first semiconductor layer of an epitaxial layer unit in an inorganic light emitting diode chip according to some embodiments of the present disclosure;

[0037] Figure 6B is a structural diagram of an epitaxial layer unit in an inorganic light emitting diode chip according to some embodiments of the present disclosure;

[0038] Figure 7 is a structural diagram of an inorganic light emitting diode chip according to some embodiments of the present disclosure;

[0039] Figure 8A to Figure 8G A step diagram of a method for manufacturing an inorganic light emitting diode chip according to some embodiments of the present disclosure;

[0040] Figure 9A to Figure 9G is another step diagram of a method for manufacturing an inorganic light emitting diode chip according to some embodiments of the present disclosure;

[0041] Fig.10 A flow chart of a method for manufacturing an inorganic light emitting diode chip according to some embodiments of the present disclosure;

[0042] Fig.11A is another flow chart of a method for manufacturing an inorganic light emitting diode chip according to some embodiments of the present disclosure;

[0043] Fig. 11B is another flow chart of a method for manufacturing an inorganic light emitting diode chip according to some embodiments of the present disclosure. DETAILED DESCRIPTION

[0044] The following will be combined with the accompanying drawings to clearly and completely describe the technical solutions in some embodiments of the present disclosure. Obviously, the described embodiments are only part of the embodiments of the present disclosure, rather than all the embodiments. Based on the embodiments provided by the present disclosure, all other embodiments obtained by ordinary technicians in this field belong to the scope of protection of the present disclosure.

[0045] Unless the context requires otherwise, throughout the specification and claims, the term "comprise" and other forms thereof, such as the third person singular form "comprises" and the present participle form "comprising", are to be interpreted as open, inclusive, that is, "including, but not limited to". In the description of the specification, the terms "one embodiment", "some embodiments", "exemplary embodiments", "example", "specific example" or "some examples" and the like are intended to indicate that specific features, structures, materials or characteristics associated with the embodiment or example are included in at least one embodiment or example of the present disclosure. The schematic representation of the above terms does not necessarily refer to the same embodiment or example. In addition, the specific features, structures, materials or characteristics may be included in any one or more embodiments or examples in any appropriate manner.

[0046] In the following, the terms "first" and "second" are used for descriptive purposes only and are not to be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the embodiments of the present disclosure, unless otherwise specified, "plurality" means two or more.

[0047] When describing some embodiments, the expressions "coupled" and "connected" and their derivatives may be used. For example, when describing some embodiments, the term "connected" may be used to indicate that two or more components are in direct physical or electrical contact with each other. For another example, when describing some embodiments, the term "coupled" may be used to indicate that two or more components are in direct physical or electrical contact with each other.

[0048] “At least one of A, B, and C” has the same meaning as “at least one of A, B, or C” and both include the following combinations of A, B, and C: A only, B only, C only, the combination of A and B, the combination of A and C, the combination of B and C, and the combination of A, B, and C.

[0049] Some embodiments of the present disclosure provide a light emitting diode lighting device, which includes an array substrate and a plurality of inorganic light emitting diode chips disposed on the array substrate. The plurality of inorganic light emitting diode chips are coupled to a signal source on the array substrate and emit light under the action of the signal source.

[0050] In some examples, such as Figure 3AAs shown, the light-emitting diode light-emitting device provided by the present disclosure is a light-emitting diode display device, such as a mini LED display device or a micro LED display device, including multiple inorganic light-emitting diode chips, specifically, sub-millimeter inorganic light-emitting diode chips (mini LED chips) or micro inorganic light-emitting diode chips (micro LED chips). Exemplarily, the light-emitting diode display device 30 includes an array substrate 20 and multiple inorganic light-emitting diode chips 10 arranged on one side of the array substrate 20. The multiple inorganic light-emitting diode chips 10 have high density, large number, and small spacing, which can reduce the pixel pitch of the display device, improve the resolution, and make the display device have a better display effect.

[0051] Taking the mini LED display device as an example, in order to adjust the light type of the light emitted by the sub-millimeter inorganic light-emitting diode chip, it is necessary to prepare an optical structure at the gap between multiple sub-millimeter inorganic light-emitting diode chips on the array substrate. Figure 3A As shown, in the mini LED display device 30, a wall 5 with a certain height surrounding the inorganic light emitting diode chip 10 is prepared around each inorganic light emitting diode chip 10. For example, the wall 5 is in the shape of a U.S.-shaped wall. The light type of the light emitted by the inorganic light emitting diode chip 10 can be controlled by controlling parameters such as the height of the wall 5, the distance between the wall 5 and the inorganic light emitting diode chip 10, and the inclination angles of each side wall of the wall.

[0052] like Figure 3B As shown in FIG. 1 , the inventor simulated the light pattern of a single inorganic light emitting diode chip. Figure 4 As shown, in the case where no fence is set (see curve B, the inorganic light emitting diode chip used is Figure 1 In the inorganic light emitting diode chip 10' shown in the figure, the intensity of the light emitted by the inorganic light emitting diode chip is low in the positive viewing direction of the light emitting side of the inorganic light emitting diode chip, and the light brightness measured at various angles on the light emitting side of the inorganic light emitting diode chip is generally low, and the emitted light is relatively scattered. In the case of setting a wall (see curve A, the inorganic light emitting diode chip used is Figure 7The inorganic light emitting diode chip 10 shown in the figure has a relatively concentrated light emitted by the inorganic light emitting diode chip. In the positive viewing angle direction of the light emitting side of the inorganic light emitting diode chip, the intensity of the light emitted by the inorganic light emitting diode chip is the highest. It can be seen that if an optical structure is set in the mini LED display device, the brightness of the mini LED display device in the positive viewing angle direction is the highest during display, so that the display effect of the display device is good. It should be noted that the positive viewing angle direction mentioned in the present disclosure refers to the position on the normal line of the plane where the inorganic light emitting diode chip (or display device) is located, and the normal line passes through the geometric center of the inorganic light emitting diode chip (or display device).

[0053] It can be seen that the optical structure can achieve the effect of adjusting the light type and improving the display viewing angle. According to the current process limit, the height of the above optical structure is not more than 50μm; in order to achieve a better dimming effect and to facilitate the production of the optical structure, the thickness of the inorganic light emitting diode chip 10 should be less than the height of the optical structure.

[0054] like Figure 1 and Figure 2 As shown, in the related art, the inorganic light emitting diode chip 10' includes an epitaxial layer 2, and a first pad 31 and a second pad 32 arranged on one side of the epitaxial layer 2, wherein the epitaxial layer 2 includes a light emitting layer, an N-type semiconductor layer, a P-type semiconductor layer and other multiple thin film layers, the first pad 31 and the second pad 32 are respectively coupled to the N-type semiconductor layer and the P-type semiconductor layer in the epitaxial layer 2, the first pad 31 and the second pad 32 are used to couple with an external signal source, and the inorganic light emitting diode chip 10' can emit light by applying voltage to the first pad 31 and the second pad 32.

[0055] In the related art, a method for preparing an inorganic light emitting diode chip is as follows: an epitaxial layer and a plurality of pads are sequentially prepared on a substrate, the substrate is thinned to a desired thickness by a grinding process to obtain an inorganic light emitting diode chip mother sheet, and the inorganic light emitting diode chip mother sheet is then divided to obtain a plurality of inorganic light emitting diode chips. The structure of the obtained inorganic light emitting diode chip 10' is as follows: Figure 1 As shown. In the above preparation method, by grinding the substrate, the inorganic light emitting diode chip mother sheet can be thinned from 700μm to 800μm to a minimum of 80μm. If the substrate is continued to be ground, the entire substrate may be broken, resulting in serious yield loss. In addition, since the substrate (such as a sapphire substrate) has a lattice structure, when the inorganic light emitting diode chip mother sheet is divided into a plurality of inorganic light emitting diode chips by a splitting process, the substrate will be cracked along a specific direction in its lattice structure, resulting in irregularities around the obtained inorganic light emitting diode chip 10' and the appearance of beveled edges. In this way, the light emitting light pattern of the inorganic light emitting diode chip 10' will be asymmetric relative to the front viewing direction of the chip (such as Figure 4 Curve B in Figure 1 As shown, since the thickness d1 of the inorganic light emitting diode chip 10 ′ with the substrate 1 is at least 80 μm, which is greater than the maximum height (50 μm) of the optical structure, the optical structure is difficult to manufacture and the light emitting light type of the inorganic light emitting diode chip cannot be effectively improved.

[0056] Another method for preparing an inorganic light emitting diode chip is: after sequentially preparing an epitaxial layer and a plurality of pads on a substrate, the substrate is peeled off from the epitaxial layer to obtain an inorganic light emitting diode chip mother sheet, and then the inorganic light emitting diode chip mother sheet is divided to obtain a plurality of inorganic light emitting diode chips. The structure of the obtained inorganic light emitting diode chip 10' is as follows: Figure 2 As shown. The inorganic light-emitting diode chip prepared by this method only includes an epitaxial layer and a pad, and due to the poor toughness of the epitaxial layer, it is easy to break when subjected to force. Therefore, it is necessary to perform spot testing on each of the prepared inorganic light-emitting diode chips to sort them as needed, but the epitaxial layer of the inorganic light-emitting diode chip cannot withstand the force applied by the positive and negative probes during spot testing, and will break during spot testing. In addition, the epitaxial layer of the inorganic light-emitting diode chip is also difficult to withstand the force applied during transfer (for example, transferring the inorganic light-emitting diode chip to the array substrate), which increases the difficulty of transferring the inorganic light-emitting diode chip.

[0057] In summary, the preparation method of the inorganic light emitting diode chip in the related art and the prepared inorganic light emitting diode chip 10' have the following problems: when the prepared inorganic light emitting diode chip 10' has a substrate 1, the thickness of the inorganic light emitting diode chip 10' is relatively thick, which is not conducive to the production of the optical structure, and the light emitting light pattern is asymmetric. When the prepared inorganic light emitting diode chip 10' does not have a substrate, the inorganic light emitting diode chip 10' is too fragile, difficult to perform point measurement and transfer, and difficult to apply to display products.

[0058] Based on this, Figure 5A and Figure 5B As shown, some embodiments of the present disclosure provide an inorganic light emitting diode chip mother sheet 20 , comprising: an epitaxial layer 2 , a plurality of pads 3 and a supporting reinforcement layer 4 .

[0059] The two opposite sides of the epitaxial layer 2 are respectively the first side B1 and the second side B2 , a plurality of pads 3 are arranged on the first side B1 of the epitaxial layer 2 , and the supporting reinforcement layer 4 fills the gaps between the plurality of pads 3 .

[0060] The inorganic light emitting diode chip mother sheet 20 is divided to obtain a plurality of inorganic light emitting diode chips 10. For the convenience of description, Figure 5A and Figure 5BAs shown, the inorganic light emitting diode chip mother sheet 20 is divided into a plurality of inorganic light emitting diode chip regions Q, and the plurality of pads 3 include a plurality of first pads 31 and a plurality of second pads 32. The epitaxial layer 2 includes a plurality of epitaxial layer units 2a, and the supporting reinforcement layer 4 includes a plurality of supporting reinforcement units 4a. Each inorganic light emitting diode chip region Q is provided with an epitaxial layer unit 2a, a supporting reinforcement unit 4a, a first pad 31 and a second pad 32.

[0061] like Figure 7 As shown, some embodiments of the present disclosure further provide an inorganic light emitting diode chip 10, which is obtained by segmenting the inorganic light emitting diode chip mother sheet 20, and the inorganic light emitting diode chip 10 includes: an epitaxial layer unit 2a, a first pad 31, a second pad 32 and a support reinforcement unit 4a. The first pad 31 and the second pad 32 are arranged on one side of the epitaxial layer unit 2a, and the support reinforcement unit 4a is filled around the first pad 31 and the second pad 32.

[0062] The inorganic light emitting diode chip mother sheet 20 provided in some embodiments of the present disclosure does not include a substrate. By filling the support reinforcement layer 4 in the gaps between the plurality of pads 3, the strength of the inorganic light emitting diode chip mother sheet 20 is enhanced, and the epitaxial layer 2 is not prone to fracture or damage due to force. In addition, compared with the inorganic light emitting diode chip mother sheet including a substrate in the related art, the inorganic light emitting diode chip mother sheet 20 provided in the present disclosure is thinner. Therefore, the inorganic light emitting diode chip 10 obtained by dividing the inorganic light emitting diode chip mother sheet 20 will not have the problem of irregularity around the edges, and has the advantages of thin thickness and high strength, and can withstand the force applied during point measurement and the force applied during transfer. Moreover, after the inorganic light emitting diode chip 10 is transferred to the array substrate, the thickness of the inorganic light emitting diode chip 10 is thin, which reduces the difficulty of manufacturing the optical structure, and can make the height of the optical structure greater than the thickness of the inorganic light emitting diode chip 10, so that the dimming effect of the light emitted by the inorganic light emitting diode chip 10 is better.

[0063] like Figure 5A and Figure 5B As shown, in some embodiments, since the inorganic light emitting diode chip mother sheet 20 provided by the embodiments of the present disclosure does not include a substrate, in order to enhance the strength of the inorganic light emitting diode chip mother sheet 20 and make it less prone to breakage, the supporting reinforcement layer 4 filling the gaps between the multiple pads 3 needs to have a certain thickness so that the inorganic light emitting diode chip mother sheet 20 is not too thin or too fragile. Similarly, the multiple pads 3 also need to have a certain thickness to ensure that the surfaces of the multiple pads 3 away from the epitaxial layer 2 can be exposed, and the multiple pads 3 cannot be too thick to make the total thickness of the inorganic light emitting diode chip mother sheet 20 too thick.

[0064] In some examples, the thickness d2 of at least one pad 3 is 20 μm to 30 μm, so that the thickness of the pad 3 can match the thickness of the support reinforcement layer 4, so that the total thickness of the inorganic light emitting diode chip mother sheet 20 can be controlled within a reasonable range, and thus an inorganic light emitting diode chip 10 with moderate thickness and certain strength can be obtained. Exemplarily, the thickness of all pads 3 included in the inorganic light emitting diode chip mother sheet 20 is 20 μm to 30 μm, or the thickness of at least one pad 3 is 20 μm, 25 μm or 30 μm, etc.

[0065] In some embodiments, the material of the liner 3 is selected from materials with low cost and good conductivity, and the present disclosure is not limited to this. Exemplarily, the material of each liner 3 includes at least one of copper, aluminum, and copper-aluminum alloy. For example, the material of each liner 3 is copper. Alternatively, the material of a portion of each liner 3 is copper, and the material of another portion of the liner 3 is copper-aluminum alloy.

[0066] In some embodiments, each pad 3 includes a pad body and a protective layer covering the sidewall of the pad body and a surface away from the epitaxial layer 2 , wherein the protective layer is conductive.

[0067] The protective layer is coated on the surface of the gasket body, which can protect the gasket body, prevent the gasket body from being oxidized or corroded by water, and extend the service life of the gasket 3. The protective layer is conductive and can also play a role in electrical coupling.

[0068] In some examples, the material of the pad body includes at least one of copper, aluminum, and copper-aluminum alloy, and the material of the protective layer is a conductive material with high corrosion resistance. Exemplarily, the material of the protective layer includes nickel-gold.

[0069] In some embodiments, in order to enhance the strength of the inorganic light emitting diode chip mother sheet 20 and prevent it from being easily broken, the support reinforcement layer 4 filling the gaps between the plurality of pads 3 needs to have a certain thickness so that the inorganic light emitting diode chip mother sheet 20 is not too thin or too fragile. At the same time, the thickness of the support reinforcement layer 4 cannot be too thick to make the total thickness of the inorganic light emitting diode chip mother sheet 20 too thick. For example, Figure 5A and Figure 5B As shown, the thickness d3 of the support and reinforcement layer 4 is 20 μm to 30 μm. For example, the thickness d3 of the support and reinforcement layer 4 is 20 μm, 25 μm or 30 μm.

[0070] In some embodiments, Figure 5BAs shown, the surface of the support reinforcement layer 4 away from the epitaxial layer 2 is flush with the surface of the plurality of pads 3 away from the epitaxial layer 2. That is, the thickness of the support reinforcement layer 4 is consistent with the thickness of the pad 3. For example, the thickness of the support thickening layer and the thickness of the pad 3 are both 25 μm, so that the surfaces of the plurality of pads 3 away from the epitaxial layer 2 can be exposed to achieve spot measurement and sorting of the inorganic light emitting diode chip 10 or coupling with the signal source on the display substrate.

[0071] In other embodiments, Figure 5A As shown, the surface of the support reinforcement layer 4 away from the epitaxial layer 2 is lower than the surface of the plurality of pads 3 away from the epitaxial layer 2. In other words, the thickness of the support reinforcement layer 4 is less than the thickness of the pads 3. For example, the thickness of the support thickening layer is 25 μm, and the thickness of the pads 3 is 30 μm. In this way, the surfaces of the plurality of pads 3 away from the epitaxial layer 2 and a portion of the sidewalls can be exposed to achieve point measurement and sorting of the inorganic light emitting diode chip 10 or coupling with the signal source on the display substrate.

[0072] In some embodiments, Figure 5A and Figure 5B As shown, the material of the support reinforcement layer 4 includes a curing glue material. The curing glue material has good fluidity before curing, and can be easily filled in the gaps between the multiple pads 3. After filling, the curing glue material can be cured into a solid with high strength, which can play a role in enhancing the strength of the inorganic light-emitting diode chip mother sheet 20. The present disclosure does not limit the material of the support reinforcement layer 4, as long as the material has the above-mentioned characteristics. Exemplarily, the material of the support reinforcement layer 4 includes silica gel, epoxy resin or photoresist.

[0073] In some embodiments, the support reinforcement layer 4 is transparent, so that the light emitted by the inorganic light emitting diode chip 10 can penetrate the support reinforcement layer 4 and emit light on both sides of the inorganic light emitting diode chip 10 .

[0074] In other embodiments, the support and reinforcement layer 4 has a color, for example, the support and reinforcement layer 4 is white or black, so as to adjust the brightness of the emitted light as needed.

[0075] Exemplarily, when the support reinforcement layer 4 is white, the material of the support reinforcement layer 4 includes titanium dioxide. For example, the material of the support reinforcement layer 4 includes silica gel and titanium dioxide, and the titanium dioxide and silica gel are mixed in a certain proportion to form a curing glue material.

[0076] When the supporting reinforcement layer 4 is white, the supporting reinforcement layer 4 can reflect light. The light emitted by the epitaxial layer 2 of the inorganic light emitting diode chip 10 is reflected by the white supporting reinforcement layer 4, and the brightness is enhanced, so that the inorganic light emitting diode chip 10 can be used in light-emitting products that need to provide high-brightness light.

[0077] Exemplarily, when the supporting reinforcement layer 4 is black, the material of the supporting reinforcement layer 4 also includes carbon powder. For example, the material of the supporting reinforcement layer 4 includes silica gel and carbon powder, and the carbon powder and silica gel are mixed in a certain proportion to form a curing glue material.

[0078] When the supporting reinforcement layer 4 is black, the supporting reinforcement layer 4 can absorb light. The light emitted by the epitaxial layer unit 2a of the inorganic light emitting diode chip 10 is absorbed by the black supporting reinforcement layer 4, and the brightness is weakened. Therefore, the inorganic light emitting diode chip 10 can be used in display products that need to provide low-brightness light to increase the contrast of the display products.

[0079] As a possible design, Figure 5A As shown, the surface of the first side B1 of the epitaxial layer 2 has a plurality of protrusions c, and the plurality of protrusions c are embedded in the supporting reinforcement layer 4. By providing a plurality of protrusions c on the surface of the first side B1 of the epitaxial layer 2 and embedding the plurality of protrusions c in the supporting reinforcement layer 4, the bonding force between the epitaxial layer 2 and the supporting reinforcement layer 4 can be increased, so that the epitaxial layer 2 and the supporting reinforcement layer 4 are not easily separated.

[0080] In some embodiments, Figure 5A and Figure 5B As shown, the thickness d4 of the epitaxial layer 2 is 5 μm to 10 μm.

[0081] In some embodiments, Fig. 6A , Figure 6B and Figure 7 As shown, the epitaxial layer unit 2a mentioned above includes: a first semiconductor layer 21, a light emitting layer 22, a second semiconductor layer 23 and a planar layer 28. Among them, Figure 6B What is shown is a top view of the epitaxial layer unit 2a without the planarization layer 28. Figure 5A and Figure 5B , Figure 7 The cross-sectional view of the epitaxial layer unit 2a is taken along Figure 6B The cross section line BB' is obtained.

[0082] The first semiconductor layer 21 includes a first portion 21a and a second portion 21b, illustratively, as Fig. 6A As shown, the first portion 21 a of the first semiconductor layer 21 surrounds the second portion 21 b .

[0083] The light emitting layer 22 is disposed on one side of the first portion 21a of the first semiconductor layer 21. Exemplarily, the light emitting layer 22 includes a quantum well superlattice layer.

[0084] The light emitting layer 22 includes different materials so that the inorganic light emitting diode chip 10 can emit blue, green or red light. For example, the material of the light emitting layer 22 includes aluminum indium gallium phosphide (AlGaInP), so that the inorganic light emitting diode chip 10 can emit red light. Alternatively, the material of the light emitting layer 22 includes indium gallium nitride (InGaN), so that the inorganic light emitting diode chip 10 can emit blue light. Alternatively, the material of the light emitting layer 22 includes aluminum gallium phosphide (AlGaP), so that the inorganic light emitting diode chip 10 can emit green light.

[0085] The second semiconductor layer 23 is disposed on a side of the light emitting layer 22 away from the first semiconductor layer 21 .

[0086] The flat layer 28 covers the side of the second semiconductor layer 23 away from the light emitting layer 22, and the flat layer has a first through hole b1 and a second through hole b2. In each inorganic light emitting diode chip region Q, the first pad 31 is coupled to the first semiconductor layer 21 through the first through hole b1, and the second pad 32 is coupled to the second semiconductor layer 23 through the second through hole b2. Specifically, the first pad 31 contacts the second portion 21b of the first semiconductor layer 21 through the first through hole b1 to achieve coupling with the first semiconductor layer 21.

[0087] In some examples, the first semiconductor layer 21 is an N-type semiconductor layer, for example, the material of the first semiconductor layer 21 is N-type gallium nitride, and the second semiconductor layer 23 is a P-type semiconductor layer, for example, the material of the first semiconductor layer 21 is P-type gallium nitride. Correspondingly, after the inorganic light-emitting diode chip 10 is transferred to the array substrate, the first pad 31 is coupled to the cathode on the array substrate, and the second pad 32 is coupled to the anode on the array substrate, so that a current path is formed between the first semiconductor layer 21, the light-emitting layer 22, and the second semiconductor layer 23, so that the light-emitting layer 22 emits light under the action of the current, so that the inorganic light-emitting diode chip 10 emits light.

[0088] In the above example, when the first semiconductor layer 21 is an N-type semiconductor layer and the second semiconductor layer 23 is a P-type semiconductor layer, the thickness of the first semiconductor layer 21 can be increased so that the thickness of the first semiconductor layer 21 is greater than the thickness of the second semiconductor layer 23. For example, the thickness of the first semiconductor layer 21 is 2 to 5 times, for example, 4 times, of the thickness of the second semiconductor layer 23. In this way, the expansion capability of the electrons from the first pad 31 in the first semiconductor layer 21 can be enhanced. In the N-type semiconductor layer, the electron concentration is high and the carrier transmission rate is high, which can ensure that the electrons from the first pad 31 have a larger transmission range in the first semiconductor layer 21, thereby improving the luminous efficiency of the inorganic light-emitting diode 10. In this way, there is no need to set a structure for expanding the carrier transmission range corresponding to the first semiconductor layer 21 in the epitaxial layer unit 2a. The structure for expanding the carrier transmission range described here can refer to the insulating layer 24 and the conductive layer 25 that appear later.

[0089] In other examples, the first semiconductor layer 21 is a P-type semiconductor layer, for example, the material of the first semiconductor layer 21 is P-type gallium nitride, and the second semiconductor layer 23 is an N-type semiconductor layer, for example, the material of the first semiconductor layer 21 is N-type gallium nitride. Correspondingly, after the inorganic light-emitting diode chip 10 is transferred to the array substrate, the first pad 31 is coupled to the anode on the array substrate, and the second pad 32 is coupled to the cathode on the array substrate, so that a current path is formed between the first semiconductor layer 21, the light-emitting layer 22, and the second semiconductor layer 23, so that the light-emitting layer 22 emits light under the action of the current, so that the inorganic light-emitting diode chip 10 emits light.

[0090] In some embodiments, the epitaxial layer unit 2 a further includes: an insulating layer 24 , a conductive layer 25 , a first contact electrode 26 and a second contact electrode 27 .

[0091] The first contact electrode 26 is disposed on the first semiconductor layer 21, and the first pad 31 is coupled to the first contact electrode 26 through the first through hole. By disposing the first contact electrode 26, the first pad 31 can be better coupled to the first semiconductor layer 21, thereby improving the carrier transmission rate.

[0092] The insulating layer 24 is disposed between the second semiconductor layer 23 and the planarization layer 28 .

[0093] The conductive layer 25 is disposed between the insulating layer 24 and the planar layer 28. The conductive layer 25 is in electrical contact with the second semiconductor layer 23, that is, the conductive layer 25 covers the side of the insulating layer 24 away from the first semiconductor layer 21, and the orthographic projection of the conductive layer 25 on the first semiconductor layer 21 is larger than the orthographic projection of the insulating layer 24 on the first semiconductor layer 21, so that the conductive layer 25 can be coupled with the second semiconductor layer 23 to achieve current transmission.

[0094] Exemplarily, the conductive layer 25 is made of a material with good conductivity and strong bonding with the second semiconductor layer 23, so that the conductive layer 25 can more effectively transmit current to the second semiconductor layer 23. For example, the conductive layer 25 is made of indium tin oxide (ITO).

[0095] The second contact electrode 27 is disposed between the conductive layer 25 and the planar layer 28; the second contact electrode 27 is in electrical contact with the conductive layer 25, and the second pad 32 is coupled to the second contact electrode 27 through the second through hole b2. Moreover, the orthographic projection of the second contact electrode 27 on the first semiconductor layer 21 at least partially overlaps with the orthographic projection of the insulating layer 24 on the first semiconductor layer 21.

[0096] For example, Figure 6B and Figure 7 As shown, the second contact electrode 27 includes a first portion 27a, a second portion 27b, a third portion 27c and a fourth portion 27d, the second portion 27b, the third portion 27c and the fourth portion 27d are connected through the first portion 27a, and the second pad 32 is coupled to the second portion 27b of the second contact electrode 27 through the second through hole b2. In this way, the contact area between the second contact electrode 27 and the conductive layer 25 is increased, the contact resistance is reduced, and a higher current density can be obtained under the same voltage condition, and the current expansion capability in the conductive layer 25 is enhanced. The insulating layer 24 has the same shape as the second contact electrode 17, and the orthographic projection of the insulating layer 24 on the first semiconductor layer 21 substantially coincides with the orthographic projection of the second contact electrode 17 on the first semiconductor layer 21 ( Figure 6B The insulating layer 24 is shielded by the conductive layer 25).

[0097] In the case where the first semiconductor layer 21 is a P-type semiconductor layer and the second semiconductor layer 23 is an N-type semiconductor layer, by providing the insulating layer 24 and the conductive layer 25, and in the direction perpendicular to the plane where the first semiconductor layer 21 is located, the insulating layer 24 and the second contact electrode 27 are at least partially opposite to each other, so that the current received by the second contact electrode 27 from the second pad 32 can be prevented from being vertically injected into the second semiconductor layer 23, and the current transmission direction is changed during the process of the current being transmitted to the second semiconductor layer 23 through the conductive layer 25, so that the current can be horizontally extended in the conductive layer 25. The current is transmitted to the second semiconductor layer 23 through the portion where the conductive layer 25 is coupled to the second semiconductor layer 23, thereby expanding the transmission range of the current in the second semiconductor layer 23, making the distribution of the current in the second semiconductor layer 23 more uniform, thereby making the region of the composite light emission of electrons and holes in the light-emitting layer 22 more uniform, and improving the light-emitting efficiency of the light-emitting layer 22.

[0098] In some embodiments, Figure 7As shown, in the inorganic light emitting diode chip 10 provided in some embodiments of the present disclosure, the thickness d2 of the first pad 31 and the second pad 32 is 20 μm to 30 μm, and the thickness d3 of the supporting reinforcement unit 4a is 20 μm to 30 μm.

[0099] Exemplarily, the thickness of the first liner 31 and the second liner 32 is 30 μm, the thickness of the support reinforcement unit 4a is 30 μm, and the surface of the support reinforcement unit 4a away from the epitaxial layer unit 2a is flush with the surface of the first liner 31 and the second liner 32 away from the epitaxial layer unit 2a.

[0100] Alternatively, the thickness of the first pad 31 and the second pad 32 is 30 μm, the thickness of the support reinforcement unit 4a is 25 μm, and the surface of the support reinforcement unit 4a away from the epitaxial layer unit 2a is lower than the surface of the first pad 31 and the second pad 32 away from the epitaxial layer unit 2a.

[0101] The inorganic light emitting diode chip 10 provided in some embodiments of the present disclosure has the advantages of being thin and high in strength, and can withstand the force applied during point measurement and the force applied during transfer. Moreover, after the inorganic light emitting diode chip 10 is transferred to the array substrate, the difficulty of manufacturing the optical structure is reduced due to the thin thickness of the inorganic light emitting diode chip 10, and the height of the optical structure can be made greater than the thickness of the inorganic light emitting diode chip 10, thereby achieving a better dimming effect on the light emitted by the display substrate.

[0102] like Fig.10 , Figure 8A to Figure 8G , Figure 9A to Figure 9G As shown, some embodiments of the present disclosure also provide a method for manufacturing an inorganic light emitting diode chip 10, the method comprising:

[0103] S1, such as Fig. 8A As shown, a substrate 1 is provided, and an epitaxial layer 2 is formed on one side of the substrate 1 .

[0104] In some examples, the substrate 1 is a sapphire substrate or a silicon substrate. A multilayer thin film including an epitaxial layer 2 is formed on one side of the substrate 1 using a metal organic compound vapor phase epitaxy process. The epitaxial layer 2 includes a plurality of epitaxial layer units 2a. For example, Fig. 8A As shown, there is a certain interval between adjacent epitaxial layer units 2a. The surface of each epitaxial layer unit 2a can be covered with a protective layer, which has strong corrosion resistance. In this way, in the subsequent steps, the chip mother sheet is cut into independent chips along the interval. Since the surface of each epitaxial layer unit 2a is provided with a protective layer, the film layer covered by the protective layer in the epitaxial layer unit 2a can be protected from corrosion, and the film layer covered by the protective layer in the epitaxial layer unit 2a is prevented from being directly exposed and easily oxidized and corroded.

[0105] S2, such as Figure 8B As shown, a plurality of pads 3 are prepared on a side of the epitaxial layer 2 away from the substrate 1 .

[0106] Exemplarily, an electrochemical deposition process or an evaporation process is used to prepare a plurality of pads 3 on a side of the epitaxial layer 2 away from the substrate 1. The plurality of pads 3 include a plurality of first pads 31 and a plurality of second pads 32, for example, Figure 8B As shown, a first pad 31 and a second pad 32 are prepared on a side of each epitaxial layer unit 2 a away from the substrate 1 .

[0107] In some examples, the material of the liner 3 includes at least one of copper, aluminum and copper-aluminum alloy. The thickness of at least one liner 3 is 20 μm to 30 μm.

[0108] In some examples, the pad 3 includes a pad body, and a protective layer covering the side walls of the pad body and the surface away from the epitaxial layer 2, the material of the pad body includes at least one of copper, aluminum and copper-aluminum alloy, and the material of the protective layer includes nickel-gold. In this case, exemplarily, the specific step of S2 is to use an electrochemical deposition process or an evaporation process to form a pad body of multiple pads 3 using at least one material of copper, aluminum and copper-aluminum alloy, and then use chemical plating to coat the nickel-gold material on the side walls and surfaces of the pad bodies of the multiple pads 3 to form a protective layer.

[0109] S3, such as Figure 8C to Figure 8E As shown, a supporting reinforcement layer 4 is formed in the gaps between the plurality of pads 3 .

[0110] Exemplarily, the thickness of the support reinforcement layer 4 is 20 μm to 30 μm. The material of the support reinforcement layer 4 is a curing adhesive material, for example, the material of the support reinforcement layer 4 includes silica gel, epoxy resin or photoresist.

[0111] In some embodiments, Fig.11A , Figure 8C to Figure 8E As shown, S3, a support reinforcement layer 4 is formed in the gaps between the plurality of pads 3, comprising:

[0112] S31 , forming a supporting reinforcement film 4 ′ on one side of the epitaxial layer 2 where a plurality of pads 3 are formed by using an injection molding process or a lamination process.

[0113] In some examples, such as Figure 8C As shown, the stacked structure formed by the substrate 1, the epitaxial layer 2 and the multiple pads 3 is fixed in the mold 6, the material of the support reinforcement layer is injected into the mold 6, so that the material of the support reinforcement layer covers the multiple pads 3, and the material of the support reinforcement layer is cured. Exemplarily, thermal curing or ultraviolet light curing can be used for curing, so as to form a support reinforcement film 4' on the side of the substrate 1 where the multiple pads 3 are formed.

[0114] Exemplarily, the material of the support reinforcement layer is silica gel or epoxy resin, and the thickness of the formed support reinforcement film 4 ′ is greater than the thickness of the plurality of pads 3 .

[0115] S32 , using a grinding process to remove the portion of the support reinforcement film 4 ′ covering the surfaces of the plurality of pads 3 away from the epitaxial layer, so that the surfaces of the plurality of pads 3 away from the epitaxial layer 2 are exposed.

[0116] For example, the support reinforcement film 4' is ground by a grinder until the surface of the plurality of pads 3 away from the epitaxial layer 2 is exposed, for example, by removing Fig.8D The portion of the support reinforcement film 4' shown in FIG. 4 is located above the dotted line, and the portion of the support reinforcement film 4' located below the dotted line is left. Fig. 8E The support reinforcement layer 4 shown in the figure. Here, "removing the portion of the support reinforcement film 4' covering the surface of the plurality of pads 3 away from the epitaxial layer" means removing all portions of the support reinforcement film 4' that are higher than the plurality of pads 3. At this time, the surface of the support reinforcement layer 4 away from the epitaxial layer 2 is flush with the surface of the plurality of pads 3 away from the epitaxial layer 2. For example, the thickness of the support reinforcement layer 4 and the thickness of the pads 3 are both 30 μm.

[0117] In other embodiments, Fig. 11B , Figure 9C to Figure 9E As shown, S3, a support reinforcement layer 4 is formed in the gaps between the plurality of pads 3, comprising:

[0118] S31 ′, using a photoresist material, forming a support reinforcement film 4 ′ on one side of the epitaxial layer 2 where a plurality of pads 3 are formed.

[0119] For example, Fig. 9C As shown, photoresist is spin-coated on one side of the epitaxial layer 2 where a plurality of pads 3 are formed, to form a supporting reinforcement film 4'.

[0120] S32 ′, patterning the support reinforcement film 4 ′, removing the portion of the support reinforcement film 4 ′ covering the surfaces of the plurality of pads 3 away from the epitaxial layer 2 , so that the surfaces of the plurality of pads 3 away from the epitaxial layer 2 are exposed.

[0121] Exemplarily, the supporting reinforcement film 4' is patterned by using an exposure and development process, and the specific steps are as follows:

[0122] The supporting reinforcement film 4' is exposed, and the exposure depth of the supporting reinforcement film 4' is controlled by controlling exposure parameters, such as exposure time, exposure intensity, etc. Fig.9D As shown, the exposure depth in the support reinforcement film 4' is h.

[0123] After the support reinforcement film 4' is exposed, a developer is coated on the surface of the support reinforcement film 4', so that the developer and the exposed portion of the support reinforcement film 4' are dissolved in the developer. For example, Fig.9D The portion of the support reinforcement film 4' located above the dotted line is dissolved in the developer, thereby removing this portion and retaining the Fig.9D The portion of the middle support reinforcement film 4' below the dotted line is used to obtain the support solidification layer 4 (eg Fig.9E At this time, the surface of the support reinforcement layer 4 away from the epitaxial layer 2 is lower than the surface of the plurality of pads 3 away from the epitaxial layer 2. For example, the thickness of the support reinforcement layer 4 is 25 μm, and the thickness of the pads 3 is 30 μm.

[0124] By adopting the above method, the thickness of the support reinforcement layer can be more accurately controlled through the exposure and development process, and the preparation accuracy is relatively high.

[0125] S4, such as Fig.8F As shown, the substrate 1 is peeled off from the epitaxial layer 2 to obtain an inorganic light emitting diode chip mother wafer 20 .

[0126] In some examples, when the substrate 1 is a sapphire substrate, the substrate 1 is peeled off from the epitaxial layer 2 in S4 by using a laser lift-off technique. In this case, before forming the epitaxial layer 2 on one side of the substrate 1 in S1, a buffer layer is formed on one side of the substrate 1. Exemplarily, the material of the buffer layer is gallium nitride. Thus, in S4, the buffer layer between the substrate 1 and the epitaxial layer 2 is vaporized by a laser to achieve the peeling of the substrate 1 from the epitaxial layer 2.

[0127] In other examples, when the material of substrate 1 is a silicon substrate, the method of peeling substrate 1 from the epitaxial layer 2 in S4 is to use acid corrosion technology, for example, immersing substrate 1 in a strong acid corrosion solution to corrode substrate 1 so that substrate 1 falls off from epitaxial layer 2.

[0128] S5, such as Figure 8G As shown, the inorganic light emitting diode chip mother sheet 20 is divided into a plurality of inorganic light emitting diode chips 10 .

[0129] Exemplarily, a cutting process is used to cut the inorganic light emitting diode chip mother sheet 20 into a plurality of inorganic light emitting diode chips 10 according to the divided plurality of inorganic light emitting diode chip regions. The present disclosure does not limit the cutting process, and for example, mechanical cutting or laser cutting may be used. Each inorganic light emitting diode chip 10 includes an epitaxial layer unit 2a, a first pad 31 and a second pad 32 disposed on one side of the epitaxial layer unit 2a, and a support reinforcement unit 4a filled around the first pad 31 and the second pad 32.

[0130] S6 , performing spot tests on the plurality of inorganic light emitting diode chips 10 respectively, and sorting the plurality of inorganic light emitting diode chips 10 according to the spot test results.

[0131] Exemplarily, a probe method is used to perform spot measurements on multiple inorganic light-emitting diode chips 10. For example, two probes are respectively brought into contact with the surfaces of the first pad 31 and the second pad 32 away from the epitaxial layer 2 to measure the optical properties of each inorganic light-emitting diode chip 10. The multiple inorganic light-emitting diode chips 10 are sorted according to the spot measurement results.

[0132] Some embodiments of the present disclosure provide a method for preparing an inorganic light-emitting diode chip 10, which increases the strength of the inorganic light-emitting diode chip mother sheet 20 by forming a supporting reinforcement layer 4 in the gaps between multiple pads 3. Therefore, during the process of peeling off the substrate 1, the inorganic light-emitting diode chip mother sheet 20 can withstand the stress during peeling without breaking or being damaged. The thickness of the obtained inorganic light-emitting diode chip mother sheet 20 is reduced compared to the inorganic light-emitting diode chip mother sheet with the substrate 1, so that the obtained inorganic light-emitting diode chip 10 is thinner and has higher strength.

[0133] Furthermore, the inorganic light emitting diode chip 10 prepared by the preparation method provided by the present invention includes a support reinforcement unit 4a filled around the first pad 31 and the second pad 32, so that the strength of the inorganic light emitting diode chip 10 is improved. Therefore, the inorganic light emitting diode chip 10 can withstand the force applied by the probe during point measurement, and can withstand the example during transfer, and is not prone to breakage.

[0134] In some embodiments, the light emitting diode light emitting device provided by the present disclosure is a light emitting diode display device, such as Figure 3A and Figure 4 As shown, the array substrate in the light emitting diode display device is an array substrate, and a plurality of inorganic light emitting diode chips 10 are packaged on the array substrate 20. For example, the inorganic light emitting diode chips 10 can be packaged on the array substrate in a flip-chip or mounting manner. Figure 4 Take the flip-flop method as an example.

[0135] like Figure 4As shown, the array substrate 20 includes a plurality of thin film transistors TFT, a plurality of anodes 81 and a plurality of cathodes 82, each anode 81 is coupled to the drain of a thin film transistor TFT, and the two pads 3 included in each inorganic light emitting diode chip 10 are coupled to an anode 81 and a cathode 82 respectively. For example, in the case where the first semiconductor layer in the light emitting layer of the inorganic light emitting diode chip 10 is an N-type semiconductor layer and the second semiconductor layer is a P-type semiconductor layer, the first pad 31 of each inorganic light emitting diode chip 10 is bound and connected to the cathode 82 through a conductive material 9 (for example, solder), and the second pad 32 of each inorganic light emitting diode chip 10 is coupled to an anode 81 through the solder 9. By turning on and off the thin film transistor TFT, whether the corresponding inorganic light emitting diode chip 10 emits light is controlled, thereby realizing display.

[0136] In some examples, such as Figure 3A As shown, the plurality of inorganic light emitting diode chips 10 include a plurality of blue light inorganic light emitting diode chips, a plurality of red light inorganic light emitting diode chips, and a plurality of green light inorganic light emitting diode chips, and the three colors of inorganic light emitting diode chips 10 are arranged in an array according to a certain rule. An optical structure 5 is arranged around each inorganic light emitting diode chip 10, for example, a square-shaped wall with a certain height. Since the inorganic light emitting diode chip 10 provided in some embodiments of the present disclosure is thin, the difficulty of the preparation process of the optical structure can be reduced, and the height of the optical structure can be made greater than the thickness of the inorganic light emitting diode chip 10, so that the light emitted by the inorganic light emitting diode chip 10 can be regulated to improve the display viewing angle of the display device.

[0137] In other examples, the LED light-emitting device provided in the present disclosure is an LED light board, such as a mini LED light board, which can be used as a surface light source. Exemplarily, the LED light board can be used as a backlight source in a backlight module to provide light for a liquid crystal display device.

[0138] The above is only a specific embodiment of the present disclosure, but the protection scope of the present disclosure is not limited thereto. Any changes or substitutions that can be thought of by any person skilled in the art within the technical scope disclosed in the present disclosure should be included in the protection scope of the present disclosure. Therefore, the protection scope of the present disclosure should be based on the protection scope of the claims.

Claims

1. A light emitting diode lighting device, comprising: An array substrate; A plurality of inorganic light emitting diode chips are arranged on the array substrate; The inorganic light emitting diode chip is obtained by dividing the inorganic light emitting diode chip mother sheet; The inorganic light emitting diode chip mother sheet has a plurality of inorganic light emitting diode chip areas; A plurality of optical structures are arranged on the array substrate, each of the optical structures is arranged around one of the inorganic light emitting diode chips; The inorganic light emitting diode chip comprises: Epitaxial layer unit; A first pad and a second pad are disposed on a side of the epitaxial layer unit close to the array substrate; surfaces of the first pad and the second pad away from the epitaxial layer unit are further away from the epitaxial layer unit than a surface of the array substrate close to the epitaxial layer unit; A supporting and reinforcing unit, wherein the supporting and reinforcing unit is filled around the first pad and around the second pad; The inorganic light emitting diode chip mother sheet comprises: An epitaxial layer, wherein two opposite sides of the epitaxial layer are respectively a first side and a second side; A plurality of pads disposed on a first side of the epitaxial layer; the plurality of pads comprising a plurality of the first pads and a plurality of the second pads; A support reinforcement layer, wherein the support reinforcement layer fills the gaps between the plurality of pads; Among them, the surface of the supporting reinforcement layer away from the epitaxial layer is lower than the surfaces of the multiple pads away from the epitaxial layer; the surface of the optical structure away from the array substrate is farther away from the array substrate than the surface of the epitaxial layer unit away from the array substrate.

2. The light emitting diode lighting device according to claim 1, wherein: The ratio of the thickness of the epitaxial layer to the thickness of the liner is in the range of 1:6 to 1:

2.

3. The light emitting diode lighting device according to claim 1, wherein: At least one of the spacers has a thickness of 20 μm to 30 μm.

4. The light emitting diode lighting device according to claim 1, wherein: The material of each gasket includes at least one of copper, aluminum, and a copper-aluminum alloy.

5. The light emitting diode lighting device according to claim 1, wherein: Each pad includes a pad body and a protection layer covering the sidewall of the pad body and a surface away from the epitaxial layer; the protection layer is conductive.

6. The light emitting diode lighting device according to claim 5, wherein: The material of the pad body includes at least one of copper, aluminum and copper-aluminum alloy, and the material of the protection layer includes nickel-gold.

7. The light emitting diode lighting device according to claim 1, wherein: The thickness of the support reinforcement layer is 20 μm to 30 μm.

8. The light emitting diode light emitting device according to any one of claims 1 to 7, wherein: The material of the support reinforcement layer includes a curing glue material.

9. The light emitting diode lighting device according to claim 8, wherein: The material of the support reinforcement layer includes silica gel, epoxy resin or photoresist.

10. The light emitting diode light emitting device according to any one of claims 1 to 7, wherein: The supporting and reinforcing layer is white or black.

11. The light emitting diode lighting device according to claim 10, wherein: When the supporting and reinforcing layer is white, the material of the supporting and reinforcing layer includes titanium dioxide; When the supporting and reinforcing layer is black, the material of the supporting and reinforcing layer includes carbon powder.

12. The light emitting diode light emitting device according to any one of claims 1 to 7, wherein: A surface of the first side of the epitaxial layer has a plurality of protrusions, and the plurality of protrusions are embedded in the supporting and reinforcing layer.

13. The light emitting diode light emitting device according to any one of claims 1 to 7, wherein: The thickness of the epitaxial layer is 5 μm-10 μm.

14. The light emitting diode light emitting device according to any one of claims 1 to 7, wherein: The epitaxial layer includes a plurality of epitaxial layer units, and an epitaxial layer unit, a first pad and a second pad are arranged in each inorganic light emitting diode chip region; The epitaxial layer unit comprises: A first semiconductor layer; the first semiconductor layer comprises a first portion and a second portion; a light emitting layer disposed on one side of the first portion of the first semiconductor layer; A second semiconductor layer disposed on a side of the light emitting layer away from the first semiconductor layer; A flat layer covering the second semiconductor layer away from the light emitting layer; the flat layer has a first through hole and a second through hole, and in each of the inorganic light emitting diode chip regions, the first pad is coupled to the first semiconductor layer through the first through hole, and the second pad is coupled to the second semiconductor layer through the second through hole.

15. The light emitting diode lighting device according to claim 14, wherein: The epitaxial layer unit further includes: a first contact electrode disposed between the second portion of the first semiconductor layer and the planar layer; the first contact electrode is in electrical contact with the second portion of the first semiconductor layer, and the first pad is coupled to the first contact electrode through the first through hole; An insulating layer disposed between the second semiconductor layer and the planar layer; A conductive layer disposed between the insulating layer and the planar layer; the conductive layer is in electrical contact with the second semiconductor layer; A second contact electrode is arranged between the conductive layer and the planar layer; the second contact electrode is electrically contacted with the conductive layer, and the second pad is coupled to the second contact electrode through the second through hole; and an orthographic projection of the second contact electrode on the first semiconductor layer at least partially overlaps with an orthographic projection of the insulating layer on the first semiconductor layer.

16. The light emitting diode light emitting device according to any one of claims 1 to 7, wherein: The thickness of the first liner and the second liner is 20 μm to 30 μm; The thickness of the support reinforcement unit is 20 μm to 30 μm.

17. A method for manufacturing an inorganic light emitting diode chip, wherein the inorganic light emitting diode chip is the inorganic light emitting diode chip included in the light emitting diode light emitting device according to any one of claims 1 to 16; the manufacturing method comprising: providing a substrate, and forming an epitaxial layer on one side of the substrate; Prepare a plurality of pads on a side of the epitaxial layer away from the substrate; forming a support reinforcement layer in the gaps between the plurality of pads; The substrate is peeled off from the epitaxial layer to obtain an inorganic light emitting diode chip mother sheet.

18. The method for manufacturing an inorganic light emitting diode chip according to claim 17, wherein: The gaps between the plurality of pads are used to form a support reinforcement layer, comprising: Using a photoresist material, a support reinforcement film is formed on one side of the epitaxial layer where a plurality of pads are formed; The support reinforcement film is patterned to remove a portion of the support reinforcement film covering the surfaces of the plurality of pads away from the epitaxial layer, so that the surfaces of the plurality of pads away from the epitaxial layer are exposed.

Citation Information

Patent Citations

  • Light emitting diode with sandwich-type current blocking structure

    CN102074629A

  • Manufacturing method of light-emitting device and light-emitting device

    CN102270708A

  • Light emitting diode chip having electrode pad

    CN103222074A

  • Light-emitting diode

    CN107690712A

  • Array integrated micro LED chip and manufacturing method thereof

    CN110767642A