A method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst

By immobilizing the enzyme of Lactobacillus paracasei on semiphobic crystal gel, efficient biocatalytic conversion and synthesis of phenyllactic acid is achieved, which solves the problems of environmental pollution and insufficient development of biotransformation synthesis of phenyllactic acid in the existing technology, and has high Conversion rate and large-scale application potential.

CN114369626BActive Publication Date: 2024-10-11ZHEJIANG UNIV OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210064093.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-01-20
Publication Date
2024-10-11
Estimated Expiration
2042-01-20

AI Technical Summary

Technical Problem

The chemical synthesis method of phenyllactic acid in the existing technology has complex technical routes, high energy consumption, many by-products, and serious environmental pollution problems. The biotransformation synthesis method has not yet been fully developed, especially the research based on semi-phobic hydrogel-immobilized enzymes. few.

Method used

The enzyme in the lysate of Lactobacillus paracasei is immobilized on anion exchange semi-phobic crystal gel, and the enzyme is fully adsorbed through chromatography column separation to form a biocatalyst, and is carried out in a reaction solution containing phenylpyruvic acid and NADH coenzyme. Biotransformation reaction produces phenyllactic acid.

Benefits of technology

It achieves the production of phenyllactic acid with high conversion rate and high reusability rate, reduces the difficulty of separation and purification, is environmentally friendly, and has large-scale application prospects, and the molar conversion rate of phenyllactic acid can reach 53%.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure DEST_PATH_IMAGE001
    Figure DEST_PATH_IMAGE001
Patent Text Reader

Abstract

The invention discloses a method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst, which is characterized in that the method comprises the steps of loading the lysed cell solution of Lactobacillus paracasei as a raw material, using a stacked bed of anion exchange semi-phobic crystal gel as a separation adsorption medium, and adsorbing the sample by crystal gel chromatography, so that the active enzyme in the lysed cell solution raw material is fully adsorbed on the anion exchange semi-phobic crystal gel; then the anion exchange semi-phobic crystal gel immobilized with the active enzyme is used as a biocatalyst and added to a reaction solution containing phenylpyruvic acid and NADH coenzyme to carry out a bioconversion reaction to generate phenyllactic acid. The method provided by the invention has the advantages of simple operation, high efficiency, easy large-scale preparation, etc., and the biocatalyst can be reused, and has broad application prospects in the preparation of phenyllactic acid.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of biochemical engineering, and specifically relates to a method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst. Background Art

[0002] As a high-value organic acid with broad-spectrum antibacterial properties, phenyllactic acid can replace chemically synthesized preservatives. It can also be used as a key drug intermediate and a precursor of the engineering material polyphenyllactic acid. It has broad application prospects in the fields of medicine, biology and food industry.

[0003] The chemical synthesis of phenyllactic acid has a complex technical route, high energy consumption, and many by-products, and has prominent environmental pollution problems and many restrictions on large-scale applications. The biotransformation synthesis of phenyllactic acid has attracted widespread attention from researchers in recent years because of its mild conditions and environmental safety. Among them, the key enzyme system in the biosynthesis of phenyllactic acid is immobilized to form a new type of biocatalyst, which is directly catalytically converted to synthesize phenyllactic acid. It has the advantages of high conversion rate, high reuse rate, and environmental friendliness, and has attracted much attention from researchers at home and abroad. At present, there are few research reports on the catalytic conversion synthesis of phenyllactic acid based on semi-phobic crystal gel immobilized enzymes as biocatalysts. Therefore, it is necessary to develop relevant preparation technologies for the catalytic conversion synthesis of phenyllactic acid using biocatalysts. Summary of the invention

[0004] In view of the above problems existing in the prior art, the object of the present invention is to provide a method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst. In the method of the present invention, the enzyme in the cell lysis solution of Lactobacillus paracasei is fixed on a semi-phobic crystal gel to prepare a biocatalyst, and then further catalytic conversion is performed to synthesize phenyllactic acid.

[0005] The technical solution provided by the present invention is:

[0006] The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst is characterized in that the method comprises using the cell lysate of Lactobacillus paracasei as a raw material for loading, using a stacked bed of anion exchange semi-phobic crystal gel as a separation and adsorption medium, and performing sample adsorption by crystal gel chromatography to allow the active enzyme in the cell lysate raw material to be fully adsorbed on the anion exchange semi-phobic crystal gel; then adding the anion exchange semi-phobic crystal gel immobilized with the active enzyme as a biocatalyst to a reaction solution containing phenylpyruvate and NADH coenzyme to carry out a bioconversion reaction to generate phenyllactic acid.

[0007] The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst is characterized in that it specifically comprises the following steps:

[0008] 1) resuspending the cells of the Lactobacillus paracasei strain in a 15-30 mM PBS buffer at a solid-liquid ratio of 1:15-30 to obtain a cell suspension, wherein the unit of the solid-liquid ratio is g / mL, and then subjecting the cell suspension to ultrasonic cell wall disruption, high-speed centrifugation, and taking the supernatant, which is the cell disruption solution of Lactobacillus paracasei, as the loading solution;

[0009] 2) Fill the anion exchange semi-phobic crystal gel in the chromatography column, first rinse the chromatography column with 15-30mM PBS buffer of 5-10 times the volume of the chromatography column, and then take 5-10 times the volume of the chromatography column The sample solution obtained in step 1) is passed through the chromatography column to allow the enzyme in the cell lysis solution to be fully adsorbed on the chromatography column;

[0010] 3) Phenylpyruvate and NADH coenzyme are prepared in 80-120 mM PBS buffer to obtain a conversion solution, wherein the concentration of phenylpyruvate in the conversion solution is controlled at 50 μg / ml-100 μg / ml, preferably 50 μg / ml-80 μg / ml, and the concentration of NADH is controlled at 0.15 μmol / ml-0.3 μmol / ml, preferably 0.25-0.3 μmol / ml;

[0011] 4) The wet particles in the chromatography column of step 2) are added to the conversion solution prepared in step 3), with the solid-liquid ratio of the wet particles to the conversion solution being 1 g: (10-20) mL, preferably 1 g: 15 mL, and then a bioconversion reaction is carried out at a rotation speed of 50-200 rpm and a temperature of 30-50 °C to produce phenyllactic acid.

[0012] The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst is characterized in that in step 1), the ultrasonic wall breaking treatment time is 30-60 min, the high-speed centrifugation speed is 6000-10000 rpm, and the time is 5-20 min.

[0013] The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst is characterized in that the pH of the 15-30 mM PBS buffer in steps 1) to 2) and the pH of the 80-120 mM PBS buffer in step 3) are both 6.8-7.2.

[0014] The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst is characterized in that the flow rate through the chromatography column in step 3) is 0.5 to 5 cm / min, preferably 1 to 2 cm / min.

[0015] The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst is characterized in that in step 1), the bacterial body preparation method of the Lactobacillus paracasei strain is: the Lactobacillus paracasei strain is activated twice in an MRS culture medium to obtain a seed liquid, the seed liquid is inoculated into the MRS culture medium at an inoculation rate of 2-6%, and statically cultured at 30-40°C. After culturing for 40-60 hours, the culture medium is centrifuged to obtain a bacterial body viscous body, and the bacterial body viscous body is the bacterial body of the Lactobacillus paracasei strain.

[0016] The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst is characterized in that the preparation method of the anion exchange semiphobic crystal gel comprises the following steps:

[0017] S1: Dissolve two monomers, hydroxyethyl methacrylate HEMA and butyl methacrylate BMA, and a crosslinker, polyethylene glycol diacrylate PEGDA, in ultrapure water to form a solution, and store it in a refrigerator at 4°C for use;

[0018] S2: adding an initiator ammonium persulfate APS and an accelerator tetramethylethylenediamine TEMED to the solution obtained in step S1 to obtain an aqueous phase; preparing a white oil solution containing a surfactant Span 80 with a volume fraction of 0.5-2.0% to obtain an oil phase;

[0019] S3: preparing cryogel microspheres by using a multi-microtube reactor, injecting the water phase and the oil phase obtained in step S2 into the multi-microtube reactor respectively, and crystallizing and polymerizing at -20 to -34.5 °C to form cryogel microspheres;

[0020] S4: Finally, dimethylaminoethyl methacrylate (DMAEMA) is grafted onto the crystal gel microspheres to obtain the anion exchange semi-phobic crystal gel.

[0021] The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst is characterized in that in step S1, the mass concentrations of HEMA, BMA and PEGDA in the solution are 6-7%, 3-4% and 2-3%, respectively, preferably 6.4-6.6%, 3.2-3.5% and 2.3-2.6%.

[0022] The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst is characterized in that in step S2, the added mass of APS and TEMED accounts for 1.0-1.5% and 1.5-1.8% of the total mass of HEMA, BMA and PEGDA in the solution, respectively, and preferably 1.2% and 1.6%.

[0023] The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst is characterized in that the operation process of grafting dimethylaminoethyl methacrylate (DMAEMA) onto the cryogel microspheres in step S4 is as follows:

[0024] a) Place the cryogel microspheres in a beaker and preheat in a constant temperature water bath at 45-50°C;

[0025] b) Mix 0.05~0.1M Cu (III) solution and 0.5~2M NaCl solution in a volume ratio of 1.5~3:1 to prepare a catalyst solution, and preheat it to 45~50°C in advance; preheat 0.5~2M dimethylaminoethyl methacrylate DMAEMA monomer solution to 45~50°C in advance;

[0026] Pour the prepared catalyst solution into the beaker containing the crystal gel microspheres in step a), seal and react at 45-50°C for 30-60 min, pour out the catalyst solution, pour in the DMAEMA monomer solution and continue to seal and react for 1-3 h. After the reaction is completed, first rinse the unpolymerized or self-polymerized monomers with HCl solution, and finally rinse with ultrapure water to complete the preparation. The amount of the catalyst solution and DMAEMA monomer solution added is 1.5-3 times the wet volume of the crystal gel microspheres.

[0027] By adopting the above technology, compared with the prior art, the present invention has the following beneficial effects:

[0028] (1) The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst provided by the present invention uses a semi-phobic crystal gel to immobilize the biocatalyst. Since the biocatalyst can be well adsorbed on the semi-phobic crystal gel, the cell content in the conversion liquid is low. Compared with the fermentation liquid, the conversion liquid contains fewer impurities, which reduces the difficulty of separating and purifying phenyllactic acid. At the same time, it is easy to reuse, and the number of repeated conversions can reach more than 5 times.

[0029] (2) The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst provided by the present invention uses a strain of Lactobacillus paracasei, which has excellent biosafety, mild reaction conditions, environmental friendliness, simple preparation, convenient operation, and has the prospect of large-scale application.

[0030] (3) The scale-up operation of grafting modification of "poly(hydroxyethyl methacrylate)-based anion exchange monolithic crystal gel" in the prior art is relatively difficult. Compared with it, the grafting of semi-phobic crystal gel microspheres prepared by microchannels in the present invention is simple and convenient, and easy to scale up. The method of catalytic conversion and synthesis of phenyllactic acid using a biocatalyst provided by the present invention can achieve a phenyllactic acid molar conversion rate (molar ratio of phenyllactic acid product to phenylpyruvic acid substrate) of 53%. The new biocatalyst for efficient conversion and synthesis of phenyllactic acid obtained by the present invention has excellent application prospects. DETAILED DESCRIPTION

[0031] The present invention will be further described below in conjunction with specific embodiments, but the protection scope of the present invention is not limited thereto.

[0032] In the embodiments of the present invention, the pH of the PBS buffer is 6.8-7.2.

[0033] Embodiment 1:

[0034] The preparation of anion exchange semi-phobic crystal gel comprises the following steps:

[0035] 1) HEMA, BMA and PEGDA were dissolved in ultrapure water to form a solution with a total mass fraction of 12.2%, which was stored in a refrigerator at 4 ℃ for later use. HEMA, BMA and PEGDA accounted for 6.5%, 3.3% and 2.4% of the total mass of the solution, respectively.

[0036] 2) adding an initiator ammonium persulfate APS and an accelerator tetramethylethylenediamine TEMED to the solution obtained in step 1), wherein the added mass of APS and TEMED respectively accounts for 1.2% and 1.6% of the total mass of HEMA, BMA and PEGDA in the solution, to obtain an aqueous phase; preparing a white oil solution containing a surfactant Span 80 with a volume fraction of 1.0%, to obtain an oil phase;

[0037] 3) Prepare crystal colloid microspheres using a multi-microtube reactor (for the specific structure of the multi-microtube reactor, see the literature: Phase change characteristics of aqueous solution of dextran methyl methacrylate and preparation of crystal colloid microspheres, author Gao Yawei et al., Zhejiang University of Technology). Use a precision syringe pump to inject the water phase through the main branch microchannel of the multi-microtube reactor at a constant rate. At the same time, the oil phase is injected through the side branch microchannel of the multi-microtube reactor by a precision syringe pump at a constant rate. After microfluidic shaping, crystallization, pore formation and polymerization are carried out at -30 °C to form crystal colloid microspheres;

[0038] 4) Finally, dimethylaminoethyl methacrylate (DMAEMA) is grafted onto the crystal gel microspheres. The specific preparation steps are as follows:

[0039] a) Place the cryogel microspheres in a beaker and preheat in a constant temperature water bath at 48°C;

[0040] b) Prepare a Cu (III) catalyst solution with a concentration of 0.056 M, as follows: Measure 400 mL of ultrapure water into a conical flask, and add 7.08 g of CuSO4·5H2O, 14.64 g of KIO4, 4.40 g of K2S2O8, and 18.0 g of KOH in sequence. Stir the above materials thoroughly to dissolve, boil them in a 140°C oil bath for 40 min, and cool them naturally to room temperature. After cooling, filter the solution to remove the precipitate, and dilute the filtrate to 500 mL with ultrapure water. Store the dilute solution in a brown bottle for later use.

[0041] c) 0.056 M Cu (III) solution and 1 M NaCl solution were mixed in a volume ratio of 2:1 to prepare a catalyst solution, which was preheated to 48 °C in advance; 1 M dimethylaminoethyl methacrylate DMAEMA monomer solution was prepared and preheated to 48 °C in advance;

[0042] Pour the prepared catalyst solution into the beaker containing the crystal gel microspheres in step a), seal and react at 48°C for 40 min, pour out the catalyst solution, pour in the DMAEMA monomer solution and continue to seal and react for 2 h. After the reaction is completed, first rinse off the unpolymerized or self-polymerized monomers with HCl solution, and finally rinse with ultrapure water, and the preparation is completed; wherein, the added amount of the above catalyst solution and DMAEMA monomer solution is twice the wet volume of the crystal gel microspheres.

[0043] The method for preparing the bacterial cell of the Lactobacillus paracasei strain is as follows: 1) MRS culture medium is prepared and sterilized at 121°C for 20 minutes. The preserved Lactobacillus paracasei strain is inoculated into 10 mL of MRS liquid culture medium, cultured at 35°C for 12 hours, and then inoculated into liquid MRS culture medium at a 2% inoculation amount, cultured at 35°C for 12 hours, and activated twice to obtain seed liquid. 2) The seed liquid is inoculated into MRS culture medium at a 2% inoculation amount, cultured at 35°C, and after culturing for 48 hours, the culture medium is centrifuged to obtain a bacterial cell viscous body, which is the bacterial cell of the Lactobacillus paracasei strain.

[0044] Example 1 A method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst comprises the following steps:

[0045] S1: Take 1 g of the cells of the Lactobacillus paracasei strain prepared above and resuspend them in 20 ml 20 mM PBS buffer to obtain a cell suspension; then ultrasonically disrupt the 20 ml cell suspension for 40 min at a power of 400 W, centrifuge at 4 °C and 8000 rpm for 8 min, and take the supernatant as the sample solution for later use.

[0046] S2: Fill the anion exchange semi-phobic crystalline gel prepared above into a chromatography column with an inner diameter of 0.5 cm and a height of 8 cm. First, take 5 times the volume of the chromatography column with 20 mM PBS buffer to rinse the chromatography column, and then take 5 times the volume of the chromatography column to pass the sample solution obtained in step S1 through the chromatography column. The flow rate through the chromatography column is 1 cm / min, so that the enzyme in the cell lysate is fully adsorbed on the chromatography column to obtain a biocatalyst.

[0047] S3: Dissolve 0.5 mg of phenylpyruvate and 1.5 μmol of NADH coenzyme in 10 ml of 100 mM PBS buffer to prepare a conversion solution with a phenylpyruvate concentration of 50 μg / ml and a NADH coenzyme concentration of 0.15 μmol / ml. Take 1 g of the biocatalyst in the chromatography column obtained in step S2 into a conical flask, add 10 ml of the conversion solution, and perform the conversion at a speed of 75 rpm and a temperature of 40 °C. After 2 h of conversion, take a sample and detect it by high performance liquid chromatography. The conversion rate of phenyllactic acid reaches 28.9%.

[0048] Comparative Example 1:

[0049] The preparation method of the biocatalyst and the bacterial cells of the Lactobacillus paracasei strain in Control Example 1 was repeated in Example 1.

[0050] The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst in Control Example 1 was repeated in Example 1, except that the experimental conditions of the conversion reaction in step S3 were changed, specifically, the NADH coenzyme concentration in the conversion solution was controlled to be 0.1 μmol / ml, and the other conditions were the same as in Example 1. After 2 hours of conversion reaction in Control Example 1, samples were taken and tested by high performance liquid chromatography, and the conversion rate of phenyllactic acid reached 18.50%.

[0051] Comparative Example 2:

[0052] The preparation method of the biocatalyst and the bacterial cells of the Lactobacillus paracasei strain in Control Example 2 was repeated in Example 1.

[0053] Comparative Example 2 The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst is repeated in Example 1, except that the experimental conditions of the conversion reaction in step S3 are changed, specifically, the concentration of phenylpyruvic acid in the conversion solution is controlled to be 80 μg / ml, the concentration of NADH coenzyme is controlled to be 0.1 μmol / ml, and the volume of the added conversion solution is changed to 15 mL, and the other conditions are the same as in Example 1. After 2 hours of conversion reaction in Comparative Example 1, samples were taken and detected by high performance liquid chromatography, and the conversion rate of phenyllactic acid reached 22.10%.

[0054] Embodiment 2:

[0055] The method for preparing the biocatalyst and the bacterial cells of the Lactobacillus paracasei strain in Example 2 is repeated in Example 1.

[0056] Example 2 A method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst comprises the following steps:

[0057] S1: Take 1 g of Lactobacillus paracasei strain cells and resuspend them in 20 ml PBS buffer at 20 mM to obtain a cell suspension; then ultrasonically disrupt the cell wall of 20 ml of the cell suspension for 40 min at a power of 400 W, centrifuge at 4°C and 8000 rpm for 8 min, and take the supernatant as the sample solution for later use.

[0058] S2: Fill the biocatalyst into a chromatography column with an inner diameter of 0.5 cm and a height of 8 cm. First, take 5 times the volume of the chromatography column with 20 mM PBS buffer to rinse the chromatography column, and then take 10 times the volume of the chromatography column to pass the sample solution obtained in step S1 through the chromatography column. The flow rate through the chromatography column is 1 cm / min, so that the enzyme in the cell lysate can be fully adsorbed on the chromatography column.

[0059] S3: Dissolve 0.5 mg of phenylpyruvate and 2.0 μmol of NADH coenzyme in 10 ml of 100 mM PBS buffer to prepare a conversion solution with a phenylpyruvate concentration of 50 μg / ml and a NADH coenzyme concentration of 0.2 μmol / ml. Take 1 g of the wet particles in the chromatography column into a conical flask, add 10 ml of the conversion solution, and perform the conversion at a speed of 75 rpm and a temperature of 40 °C. After 2 hours of conversion, take a sample and detect it by high-performance liquid chromatography. The conversion rate of phenyllactic acid reaches 40.7%.

[0060] Embodiment 3:

[0061] The method for preparing the biocatalyst and the bacterial cells of the Lactobacillus paracasei strain in Example 3 is repeated in Example 1.

[0062] The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst comprises the following steps:

[0063] S1: Take 1 g of Lactobacillus paracasei strain cells and resuspend them in 20 ml PBS buffer at 20 mM to obtain a cell suspension; then ultrasonically disrupt the 20 ml cell suspension for 40 min at a power of 400 W, centrifuge at 4 °C and 8000 rpm for 8 min, and take the supernatant as the sample solution for later use.

[0064] S2: Fill the biocatalyst into a chromatography column with an inner diameter of 0.5 cm and a height of 8 cm. First, take 5 times the volume of the chromatography column with 20 mM PBS buffer to rinse the chromatography column, and then take 10 times the volume of the chromatography column to pass the sample solution obtained in step S1 through the chromatography column. The flow rate through the chromatography column is 1 cm / min, so that the enzyme in the cell lysate can be fully adsorbed on the chromatography column.

[0065] S3: Dissolve 0.75 mg of phenylpyruvate and 4.5 μmol of NADH coenzyme in 15 ml of 100 mM PBS buffer to prepare a conversion solution with a phenylpyruvate concentration of 50 μg / ml and a NADH coenzyme concentration of 0.3 μmol / ml. Take 1 g of the wet particles in the chromatography column into a conical flask, add 15 ml of the conversion solution, and perform the conversion at a speed of 75 rpm and a temperature of 40 °C. After 2 hours of conversion, take a sample and detect it by high-performance liquid chromatography. The conversion rate of phenyllactic acid reaches 58.2%.

[0066] Embodiment 4:

[0067] The preparation method of the biocatalyst and the bacterial cells of the Lactobacillus paracasei strain in Example 4 is repeated in Example 1.

[0068] The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst comprises the following steps:

[0069] S1: Take 1 g of Lactobacillus paracasei strain cells and resuspend them in 20 ml PBS buffer at 20 mM to obtain a cell suspension; then ultrasonically disrupt the cell wall of 20 ml of the cell suspension for 40 min at a power of 400 W, centrifuge at 4°C and 8000 rpm for 8 min, and take the supernatant as the sample solution for later use.

[0070] S2: Fill the biocatalyst into a chromatography column with an inner diameter of 0.5 cm and a height of 8 cm. First, take 5 times the volume of the chromatography column with 20 mM PBS buffer to rinse the chromatography column, and then take 10 times the volume of the chromatography column to pass the sample solution obtained in step S1 through the chromatography column. The flow rate through the chromatography column is 1 cm / min, so that the enzyme in the cell lysate can be fully adsorbed on the chromatography column.

[0071] S3: Dissolve 0.5 mg of phenylpyruvate and 3 μmol of NADH coenzyme in 10 ml of 100 mM PBS buffer to prepare a conversion solution with a phenylpyruvate concentration of 50 μg / ml and a NADH coenzyme concentration of 0.3 μmol / ml. Take 1 g of the wet particles in the chromatography column into a conical flask, add 10 ml of the conversion solution, and perform the conversion at a speed of 75 rpm and a temperature of 40 °C. After 2 h of conversion, take a sample and detect it by high-performance liquid chromatography. The conversion rate of phenyllactic acid reaches 54.1%.

[0072] Embodiment 5:

[0073] The method for preparing the biocatalyst and the bacterial cells of the Lactobacillus paracasei strain in Example 5 is repeated in Example 1.

[0074] The method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst comprises the following steps:

[0075] S1: Take 1 g of Lactobacillus paracasei strain cells and resuspend them in 20 ml PBS buffer at 20 mM to obtain a cell suspension; then ultrasonically disrupt the 20 ml cell suspension for 40 min at a power of 400 W, centrifuge at 4 °C and 8000 rpm for 8 min, and take the supernatant as the sample solution for later use.

[0076] S2: Fill the biocatalyst into a chromatography column with an inner diameter of 0.5 cm and a height of 8 cm. First, take 5 times the volume of the chromatography column with 20 mM PBS buffer to rinse the chromatography column, and then take 10 times the volume of the chromatography column to pass the sample solution obtained in step S1 through the chromatography column. The flow rate through the chromatography column is 1 cm / min, so that the enzyme in the cell lysate can be fully adsorbed on the chromatography column.

[0077] S3: Dissolve 1 mg of phenylpyruvate and 3 μmol of NADH coenzyme in 10 ml of 100 mM PBS buffer to prepare a conversion solution with a phenylpyruvate concentration of 100 μg / ml and a NADH coenzyme concentration of 0.3 μmol / ml. Take 1 g of the wet particles in the chromatography column into a conical flask, add 10 ml of the conversion solution, and perform the conversion at a speed of 75 rpm and a temperature of 40 °C. After 2 h of conversion, take a sample and detect it by high-performance liquid chromatography. The conversion rate of phenyllactic acid reaches 32.3%.

[0078] Embodiment 6:

[0079] The method for preparing the biocatalyst and the bacterial cells of the Lactobacillus paracasei strain in Example 6 is repeated in Example 1.

[0080] Example 6 A method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst comprises the following steps:

[0081] S1: Take 1 g of Lactobacillus paracasei strain cells and resuspend them in 20 ml PBS buffer at 20 mM to obtain a cell suspension; then ultrasonically disrupt the 20 ml cell suspension for 40 min at a power of 400 W, centrifuge at 4 °C and 8000 rpm for 8 min, and take the supernatant as the sample solution for later use.

[0082] S2: Fill the biocatalyst into a chromatography column with an inner diameter of 0.5 cm and a height of 8 cm. First, take 10 times the volume of the chromatography column with 20 mM PBS buffer to rinse the chromatography column. Then take 10 times the volume of the chromatography column of the sample solution obtained in step S1 to pass through the chromatography column. The flow rate through the chromatography column is 1 cm / min, so that the enzyme in the cell lysate can be fully adsorbed on the chromatography column.

[0083] S3: Dissolve 0.5 mg of phenylpyruvate and 2.5 μmol of NADH coenzyme in 10 ml of 100 mM PBS buffer to prepare a conversion solution with a phenylpyruvate concentration of 50 μg / ml and a NADH coenzyme concentration of 0.25 μmol / ml. Take 1 g of the wet particles in the chromatography column into a conical flask, add 10 ml of the conversion solution, and perform the conversion at a speed of 75 rpm and a temperature of 40 °C. After 2 h of conversion, take a sample and detect it by high-performance liquid chromatography. The conversion rate of phenyllactic acid reaches 53.1%.

[0084] The experimental conditions of step S3 and the corresponding reaction results in the above Examples 1-6 and Comparative Examples 1-2 are summarized in Table 1.

[0085]

[0086] The following conclusions can be drawn from Table 1:

[0087] 1. From the comparative experiments of Example 3 and Example 4, it can be seen that: when the solid-liquid ratio of wet particles to conversion liquid is 1 g:15 mL, a better conversion effect is achieved. This may be due to the effect of product inhibition, that is, when the product reaches a certain concentration, the conversion reaction will no longer continue. Therefore, in the above experiment, when the amount of conversion liquid added is 15 mL, the effect is better than that of 10 mL.

[0088] 2. From the experiments of Examples 2, 4 and 6, it can be seen that the NADH content in the conversion solution also has a great influence on the conversion reaction. When the NADH content reaches 0.25 μmol / mL, it has a good conversion effect, but when the NADH content further reaches 0.3 μmol / mL, the improvement of the conversion reaction effect is not significant.

[0089] 3. From the experimental results of Examples 4 and 5, it can be seen that the content of phenylpyruvic acid in the conversion solution should not be too high.

[0090] Embodiment 7:

[0091] According to the operation of Example 6, the conversion solution was replaced every 2 h in step S3 (that is, the conversion solution after 2 h of conversion was filtered out, and 10 ml of fresh conversion solution was added for re-conversion reaction). After five batches, samples were taken for detection by high performance liquid chromatography, and the conversion rate of phenyllactic acid reached 30.0%.

[0092] The contents described in this specification are merely an enumeration of implementation forms of the inventive concept, and the protection scope of the present invention should not be regarded as being limited to the specific forms described in the embodiments.

Claims

1. A method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst, characterized in that The method is to use the cell lysate of Lactobacillus paracasei as a raw material for sample loading, use a stacked bed of anion exchange semi-phobic crystal gel as a separation adsorption medium, and perform sample adsorption by crystal gel chromatography, so that the active enzyme in the cell lysate raw material is fully adsorbed on the anion exchange semi-phobic crystal gel; then, the anion exchange semi-phobic crystal gel immobilized with the active enzyme is added as a biocatalyst to a reaction solution containing phenylpyruvate and NADH coenzyme to perform a bioconversion reaction to generate phenyllactic acid; The specific steps include: 1) resuspending the cells of the Lactobacillus paracasei strain in a 15-30 mM PBS buffer at a solid-liquid ratio of 1:15-30 to obtain a cell suspension, wherein the unit of the solid-liquid ratio is g / mL, then subjecting the cell suspension to ultrasonic cell wall disruption, high-speed centrifugation, and taking the supernatant, which is the cell disruption solution of Lactobacillus paracasei, as the loading solution; 2) Fill the chromatography column with anion exchange semi-phobic crystal gel, first rinse the chromatography column with 5 to 10 times the volume of the chromatography column with 15-30 mM PBS buffer, and then take 5 to 10 times the volume of the chromatography column to pass the sample solution obtained in step 1) through the chromatography column to allow the enzyme in the cell lysis solution to be fully adsorbed on the chromatography column; 3) Prepare phenylpyruvate and NADH coenzyme in 80-120 mM PBS buffer to obtain a conversion solution, wherein the concentration of phenylpyruvate in the conversion solution is controlled at 50 μg / ml-100 μg / ml, and the concentration of NADH is controlled at 0.15 μmol / ml-0.3 μmol / ml; 4) adding the wet particles in the chromatography column of step 2) to the conversion solution prepared in step 3), with the solid-liquid ratio of the wet particles to the conversion solution being 1 g: (10-20) mL, and then carrying out a bioconversion reaction at a speed of 50-200 rpm and a temperature of 30-50 °C to generate phenyllactic acid; The preparation method of the anion exchange semiphobic crystal gel comprises the following steps: S1: Dissolve two monomers, hydroxyethyl methacrylate HEMA and butyl methacrylate BMA, and a cross-linking agent, polyethylene glycol diacrylate PEGDA, in ultrapure water to form a solution, and store it in a refrigerator at 4°C for later use; the mass concentrations of HEMA, BMA, and PEGDA in the solution of step S1 are 6-7%, 3-4%, and 2-3%, respectively; S2: adding initiator ammonium persulfate APS and accelerator tetramethylethylenediamine TEMED to the solution obtained in step S1 to obtain a water phase; preparing a white oil solution containing 0.5-2.0% by volume of surfactant Span 80 to obtain an oil phase; in step S2, the added mass of APS and TEMED accounts for 1.0-1.5% and 1.5-1.8% of the total mass of HEMA, BMA and PEGDA in the solution, respectively; S3: preparing cryogel microspheres by using a multi-microtube reactor, injecting the water phase and the oil phase obtained in step S2 into the multi-microtube reactor respectively, and crystallizing and polymerizing at -20 to -34.5 °C to form cryogel microspheres; S4: Finally, dimethylaminoethyl methacrylate (DMAEMA) is grafted onto the crystal gel microspheres to obtain the anion exchange semi-phobic crystal gel; The operation process of grafting dimethylaminoethyl methacrylate (DMAEMA) onto the cryogel microspheres in step S4 is as follows: a) Place the cryogel microspheres in a beaker and preheat in a constant temperature water bath at 45-50°C; b) Mix 0.05~0.1M Cu (III) solution and 0.5~2M NaCl solution in a volume ratio of 1.5~3:1 to prepare a catalyst solution, and preheat it to 45~50°C in advance; preheat 0.5~2M dimethylaminoethyl methacrylate DMAEMA monomer solution to 45~50°C in advance; Pour the prepared catalyst solution into the beaker containing the crystal gel microspheres in step a), seal and react at 45-50°C for 30-60 minutes, pour out the catalyst solution, pour in the DMAEMA monomer solution and continue to seal and react for 1-3 hours. After the reaction is completed, first rinse off the unpolymerized or self-polymerized monomers with HCl solution, and finally rinse with ultrapure water, and the preparation is completed; wherein, the added amount of the above catalyst solution and DMAEMA monomer solution is 1-3 times the wet volume of the crystal gel microspheres.

2. A method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst as claimed in claim 1, characterized in that In step 1), the method for preparing the bacterial body of the Lactobacillus paracasei strain is as follows: the Lactobacillus paracasei strain is activated twice in an MRS medium to obtain a seed liquid, the seed liquid is inoculated into the MRS medium at an inoculation rate of 2-6%, and statically cultured at 30-40°C. After culturing for 40-60 hours, the culture medium is centrifuged to obtain a bacterial viscous body, which is the bacterial body of the Lactobacillus paracasei strain.

3. A method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst as claimed in claim 1, characterized in that In step 3), the concentration of phenylpyruvate in the conversion solution is controlled at 50 μg / ml to 80 μg / ml, and the concentration of NADH is controlled at 0.25 to 0.3 μmol / ml.

4. A method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst as claimed in claim 1, characterized in that In step 4), the solid-liquid ratio of wet granules to conversion solution is 1 g:15 mL.

5. A method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst as claimed in claim 1, characterized in that In step 1), the ultrasonic cell wall breaking treatment time is 30 to 60 min, the ultrasonic power is 300 to 500 W; the high-speed centrifugation speed is 6000 to 10000 rpm, and the time is 5 to 20 min.

6. A method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst as claimed in claim 5, characterized in that In step 1), the ultrasonic power is 400W.

7. A method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst as claimed in claim 1, characterized in that The pH of the 15-30 mM PBS buffer in steps 1) to 2) and the 80-120 mM PBS buffer in step 3) are both 6.8-7.

2.

8. A method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst as claimed in claim 1, characterized in that In step 3), the flow rate through the chromatography column is 0.5-5 cm / min.

9. A method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst as claimed in claim 8, characterized in that In step 3), the flow rate through the chromatography column is 1-2 cm / min.

10. A method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst as claimed in claim 1, characterized in that The mass concentrations of HEMA, BMA and PEGDA in the solution of step S1 are 6.4-6.6%, 3.2-3.5% and 2.3-2.6%, respectively.

11. A method for synthesizing phenyllactic acid by catalytic conversion using a biocatalyst as claimed in claim 1, characterized in that In step S2, the added mass of APS and TEMED accounted for 1.2% and 1.6% of the total mass of HEMA, BMA and PEGDA in the solution, respectively.