Method for producing a cold casting mold and use of the cold casting mold for producing a mold, especially a denture
By designing the second opening for exporting gas and liquid in cold casting molds and using porous walls, the problem of high cost and material requirements in 3D printing of dental molded parts is solved, and the manufacturing of dental molded parts with complex shapes is achieved at low cost is achieved. , and improves filling efficiency and material utilization.
Patent Information
- Application Number
- CN202080073678.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-10-21
- Filing Date
- 2020-10-20
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2040-10-20
AI Technical Summary
The prior art 3D printing of dental molded parts has problems of high cost and material requirements, especially the difficulty in manufacturing molded parts with complex anatomical shapes and light refractive surface structures, and traditional isostatic pressing methods are not suitable for A mixture with high moisture content.
Design an additively manufactured cold casting mold with at least one second opening into the cavity for deriving gas and liquid, avoiding additional working steps, and improving drying effect through porous or water-absorbing wall design, using Organic materials to reduce costs and improve filling efficiency.
The low-cost manufacturing of dental molded parts in complex shapes is achieved, suitable for any moisture-containing mixture, improves filling efficiency and material utilization, and reduces the impact of thermal expansion on molded parts.
Smart Images

Figure CN114585324B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for producing a cold casting mold for molding a part, in particular a dental molding, from a mixed material, wherein the cold casting mold is additively produced from a raw material by means of an additive manufacturing method, in particular a 3D printing method using a 3D printer, the cold casting mold having a cavity which corresponds geometrically to the dental molding according to a digital data record based on a spatial model of the patient's oral cavity and has at least one first opening into the cavity for filling with a mixed material. The invention also relates to the use or production of such an additively produced cold casting mold for a method for producing a dental molding from a sinterable or light-hardening mixed material. Background Art
[0002] The use of computer-aided methods (CAD / CAM) to manufacture molded parts is known in many technical fields. In many dental clinics and dental laboratories, dental molded parts, especially dentures such as crowns and bridges, as well as dental implants and restorations or orthodontic-related parts, such as brackets, are also manufactured by computer-aided methods (CAD / CAM). Here, a digital spatial model of the patient's oral cavity is first created. For example, the required dentures are planned with the help of software, and the created data records are sent to a milling machine, which mills the manufactured dentures out of the blanks. The blanks are usually manufactured using a cold casting method, in which a mixture is first manufactured from ceramic powders or metal powders suitable for dental technology. For example, a paste, a slurry, a suspension or also a "dry" loose powder can be used as a mixture. A method for manufacturing dentures from dental metal powders is known from EP 2 470 113 B1. Here, CrCo dental metal powder is mixed into a slurry, cold-filled into a casting mold and dried therein. The adhesive added to the slurry provides sufficient shape stability after drying, so that the dried slurry is taken out from the cold casting mold as a green body, and is milled into a desired spatial shape by means of a milling machine according to the data record of the transmitted number. Through final (tight) sintering, the denture obtains the required hardness and density. The material properties required for the approval of dental moldings are clearly defined according to national and / or international standards. This cold casting method is only suitable for manufacturing blanks. Then the fine and complex shape of the real denture is milled out from the blank by cutting. The teaching of metal or ceramic slurry for dental technology is prior art and can be found in, for example, files EP1658018 B1, EP1047355 B1, WO 2013007684 A, EP1558170 B1 and EP1885278B1. Information about its adjustment can be obtained in files DE 102005023727 B4 and DE19801534 A1. The implementation of final dense sintering is also fully described in the prior art; corresponding methods and sintering furnaces can be found in EP2765950B1, EP2844412A1, and WO2011020688A1.
[0003] When using loose powder as a mixture, an additional work step is usually required, namely isostatic pressing, in order to obtain sufficient dimensional stability. In this case, the mixture is subjected to high pressure uniformly from all sides. Corresponding methods for producing ceramic dentures from ceramic powders, such as zirconium oxide, are also well known from the prior art. WO 2008 / 114 142 A1 describes a method for producing tooth components from ceramic powders.
[0004] The digital spatial model of the oral cavity is also used to make temporary parts from plastic. Here, the data record created for the denture is forwarded to a 3D printer, which manufactures the temporary parts layer by layer from the plastic raw material by means of an additive manufacturing method (3D printing).
[0005] At the same time, in addition to plastics, inorganic substances can also be used as raw materials in the field of additive manufacturing methods. Additive manufacturing methods such as SLM (Selective Laser Melting), extrusion methods such as FDM (Fused Deposition Modeling) and FFF (Fused Filament Fabrication) are known. Additive manufacturing methods that use the light hardening properties of raw materials, such as SLA or STL (stereolithography), DLP (Digital Light Processing), LCM (lithography-based ceramic manufacturing) are also known.
[0006] Therefore, preliminary attempts have been made to produce dental prostheses from metal or ceramics by means of additive manufacturing. The production of dental crowns from zirconium oxide by means of additive manufacturing is known from WO 2018 / 065856 A1. However, 3D printers for metal or ceramic objects are very expensive and / or the printed moldings do not meet the high material requirements to allow dental use. In particular, a very high binder content (approximately 30%) is required in the raw material for additive manufacturing, so that the required final density or final hardness cannot be achieved or is extremely expensive to achieve. An economical implementation of printing dental moldings from ceramics or metals is still a long way off.
[0007] WO 2019 / 210285 A2 discloses another possibility, in which the digital spatial data of the oral cavity will be used to manufacture complex-shaped and densely sintered denture parts with the help of a 3D printer. To this end, a self-destructive mold should be printed with the help of a 3D printer instead of a denture. A powder mixture of two components, a sinterable aluminum oxide powder and a powdered binder with a high thermal expansion coefficient (WAK), is used as the raw material for the printing process. The printed mold is filled with sinterable dry zirconium oxide loose powder as a mixture. The mold is then closed with a lid printed from the same material so that the mold and the zirconium oxide loose powder located therein are isostatically pressed together at a pressure of 400MPa. It is crucial in this method that the loose powder does not have a binder so that uniform pressing can be achieved. Here, the loose powder is compacted together with the mold and then sintered without removing the mold. During sintering, the binder contained in the mold expands, causing the mold to burst. In order to separate the sintered molded part from the casting mold, the sintering temperature of the casting mold must be higher than the sintering temperature of the loose powder. The disadvantage of the disclosed method is, on the one hand, the high cost associated with 3D printing of ceramic raw materials and isostatic pressing at extremely high pressures of 400 MPa. However, for the described method, the use of ceramic raw materials with a sintering temperature higher than that of the loose powder is decisive, and on the other hand, the possible uses of the method are also limited. The mixture used must be binder-free to achieve uniform pressing. In addition, the compaction pressing method, in which pressure should act evenly on the molded part from all sides, especially isostatic pressing, is not suitable for mixtures with a water content of more than 7%. Liquids are almost incompressible. In order to perform isostatic pressing, the loose powder needs to be completely enclosed in a casting mold closed with a lid. For this reason, the possible moisture contained in the mixture cannot escape. Summary of the invention
[0008] The object of the present invention is therefore to provide an additively manufactured, in particular 3D-printed, cold casting mold which allows a more cost-effective and mass-producible production of dental moldings with complex anatomical shapes, colors and light-refractive surface structures, such as crowns, bridges, jaw implants, abutments, prostheses, etc., compared to the prior art. At the same time, the possibilities for use should be expanded. In particular, the use of different mixtures of sinterable and non-sinterable, metallic and / or ceramic materials or of plastics should be possible, either in dry powder form or as a slurry, suspension or paste.
[0009] This object is achieved by a method for a cold casting mold according to claim 1. The method for producing a molded part, in particular a cold casting mold of the type described in detail at the beginning, is characterized in that the cold casting mold is additively produced and has at least one second opening leading into the mold cavity and / or out of the mold cavity, which second opening is used to discharge gas, in particular air inclusions and / or liquid, in particular diluent.
[0010] Therefore, according to the invention, it is proposed that, in addition to a first opening designed for filling with the mixture, at least one second opening is formed, in particular drilled, after the additive manufacturing of the cold casting mold is completed, and the second opening, like the first opening, leads into the mold cavity in a fluid-conducting manner and is conducted out of the mold cavity. However, it is advantageous if the first opening and / or the second opening are formed directly during the additive manufacturing, so that additional work steps are avoided. Analogously to, for example, a (vacuum) bottle filling facility, it is also conceivable to form a second opening (for ventilation) in the additive manufacturing device and to form a first opening (for filling) by coaxially introducing a filling channel into the second opening. The second opening makes it possible to introduce a fluid, i.e. a gas and / or a liquid, already during the filling of the cold casting mold (compared to during the use In order to allow the mixture to harden and / or solidify after filling, at least one first opening and / or at least one second opening remain open, thereby allowing the fluid to escape. On the one hand, this makes it possible, for example, to remove air inclusions caused by filling the chill mold with the mixture. On the other hand, liquids such as diluents can also be removed from the mold cavity of the chill mold, wherein the liquid contains a pasty, moist or slurry-like mixture or suspension, thereby allowing the mixture to dry in the chill mold. By forming at least one second opening, the chill mold additively manufactured according to the method according to the invention can not only be used for mixtures with any water content, but the at least one second opening also allows exhaust when using loose powders, which can be assisted by vibration, for example.
[0011] Therefore, according to a preferred embodiment of the present invention, at least one wall portion of the cold casting mold that limits the mold cavity is additively manufactured to have a plurality of second openings that lead into the mold cavity and pass through the wall portion, and the second openings are used to discharge gas, especially air inclusions and / or liquid, especially diluent.
[0012] By penetrating one or more walls of the cold casting mold with a plurality of second openings adjacent to one another, a sieve-like surface can be formed which, on the one hand, allows liquids and gases to pass through, but blocks solids. Preferably, the diameter of the respective second opening is smaller than the particle size of the powder contained in the mixture, such as metal powder, ceramic or glass ceramic powder, and / or the size of the particle agglomerates formed.
[0013] Therefore, in a refinement of this embodiment, the plurality of second openings can also be designed in the form of holes and / or capillaries extending through the wall, so that the wall has completely or partially porous and / or water-absorbing properties.
[0014] This design has the advantage that the moisture contained in the mixture is received or absorbed by the adjacent, porous and / or water-absorbing wall and preferably conveyed from the interior toward the atmosphere surrounding the chill mold. This effect can be assisted by increasing the temperature of the environment surrounding the chill mold or other measures for reducing the humidity of the surrounding air and thus producing dry ambient air.
[0015] It is also advantageous if the cold casting mold is made of different raw materials that have different physical properties from one another. For example, the moisture absorption capacity of porous and / or water-absorbing areas can be increased by suitable raw materials. Other areas or structures of the cold casting mold, such as filling channels, compensation volumes or support structures, can be formed by selecting other raw materials with other properties, such as water solubility, color, transparency, etc.
[0016] In order to facilitate the filling of the chill mold, for example by means of a syringe or a cannula or the like, the chill mold can be additively manufactured with a filling channel adjoining the at least one first opening in a fluid-conducting manner.
[0017] The filling channel is preferably formed in one piece with the cold casting mold. By filling the channel, for example by injection molding, it is especially possible to realize filling the cold casting mold with loading pressure.
[0018] In a further development, the filling channel is connected in a fluid-conducting manner to at least one compensating volume for storing mixed material.
[0019] Preferably, the compensating volume is also additively manufactured in one piece with the chill mold. In particular, when using a mixture with a high water content and / or in the presence of air inclusions, the compensating volume acts as a kind of reservoir and allows a backflow or trickle flow of the mixture to compensate for volume losses caused by the escape of gas and / or liquid from the mold cavity via the at least one second opening.
[0020] According to an alternative variant of the invention, faster and / or more uniform filling of the cavity of a cold casting mold can be achieved, wherein the cold casting mold is additively manufactured to have two or more first openings that respectively lead into the cavity and are used to fill them with mixed material simultaneously or with a time offset.
[0021] The mode that the first opening that is used to fill by two or more designs leads to the mold cavity at different positions, for example, also can carry out filling with different compound at different positions of the mold cavity.As long as the additional first opening is not used for filling, it can be used as the second opening for fluid to be derived, so.
[0022] Particularly advantageously, organic materials, in particular organic waxes and / or polymers and / or plastics, are used as starting materials for the additive production of the cold casting mold, so that the cold casting mold can be plasticized and / or can be decomposed thermally and / or thermochemically.
[0023] Organic materials such as wax and / or polymers and / or plastics are significantly simpler and therefore more cost-effective to use in additive manufacturing methods, such as in 3D printing. The heat resistance of plastics is relatively low, so that the cold casting molds made of organic materials can be plasticized or even decomposed by pyrolysis and / or combustion and / or thermochemical decomposition. Advantageously, for the structures and / or walls of the cold casting mold that do not limit the cavity or are directly adjacent to the cavity, in particular for supporting structures, filling channels, compensation volumes, etc., the following raw materials, such as wax, are used, which have a lower melting point than the walls that limit the cavity of the cold casting mold, such as those made of polymers or plastic additives. In this way, when the cold casting mold is plasticized or decomposed, the stress generated by the influence of heat, which may cause damage to the molded part, can be reduced or even completely avoided. The organic raw material may contain a small amount of organic material additives. For example, it is common to mix inorganic additives into plastics. However, the proportion of organic components is always higher than that of inorganic components.
[0024] Preferably, the organic material used for the additive manufacturing of the chill casting mold has a melting point and / or a decomposition temperature in the temperature range of 40°C to 300°C, preferably 60°C to 300°C.
[0025] Thus, the melting temperature or melting temperature range of the chill casting mold is lower than the melting temperature and / or sintering temperature of the mixture commonly used. Advantageously, the decomposition temperature, i.e. the temperature at which the chill casting mold begins to thermally decompose and / or thermochemically decompose, is lower than the melting temperature and / or sintering temperature of the mixture used.
[0026] In a further development, the organic material used for the additive production of the cold casting mold can be plasticized by the action of heat, in particular at a temperature in the range of 35° C. to 300° C., preferably 50° C. to 300° C., and / or can be thermally decomposed by pyrolysis and / or can be thermochemically decomposed by combustion by the action of heat, in particular at a temperature in the range of 200° C. to 650° C. A material group with particularly high heat resistance is, for example, wax. By using a waxy organic material, softening or plasticizing of the cold casting mold can already be achieved from a temperature of approximately 35° C.
[0027] The thermal and / or thermochemical decomposition can preferably be continued completely and / or at high temperatures in the sintering temperature range of 1300° C. to 2500° C., so that the cold casting mold can be dissolved without residue or at least nearly without residue by the action of heat.
[0028] Alternatively, according to an advantageous embodiment, mechanical damage to the chill mold can also occur during the additive manufacturing method, wherein at least one wall delimiting the cavity of the chill mold is additively manufactured with a predetermined breaking point, in particular with a locally smaller wall thickness.
[0029] The proposed manufacturing method is based on spatial digital data, in particular of the patient's oral cavity. The geometric shape data of the molded part, in particular of the dental molded part, derived therefrom, are directly the basis for the geometric design of the cavity of the cold casting mold in the additive manufacturing method. In order to ensure, for example, that the dental molded part, in particular a crown, a bridge, a dental implant and / or a prosthesis, is accurately placed in the patient's oral cavity in terms of dental technology, the digital data record for the geometric design of the cavity of the cold casting mold thus preferably includes the volume shrinkage of the mixture due to sintering and / or hardening. Depending on the mixture used, the corresponding volume shrinkage must be taken into account during hardening or solidification and / or sintering of the mixture, and the cavity of the cold casting mold is formed with a correspondingly matched (larger) initial geometry. In terms of the initial geometry, for example, a sintering shrinkage in the range of 25% to 50% must be taken into account for a mixture containing ceramic powder, a sintering shrinkage in the range of 50% to 95% must be taken into account for a mixture containing sol and nano zirconium oxide particles, and a sintering shrinkage in the range of 8% to 25% must be taken into account for a mixture containing metal powder. To mitigate the hardening by light and / or drying, a volume shrinkage of approximately 2% to 20% based on the initial geometry is considered. For the cold casting mold itself, a volume shrinkage in the range of 1% to 10% based on the initial geometry can also be considered for the production of the molded part. The cold casting mold produced according to the method according to the invention allows for the cost-effective production of molded parts, in particular dental molded parts, from different compound materials.
[0030] The object of the invention specified at the outset is therefore also achieved by a chill casting mold according to claim 13 .
[0031] The cold casting mold according to the invention has at least one first opening into the mold cavity, which is used to fill it with a mixture, and is characterized in that at least one second opening into the mold cavity is provided, which is used to discharge gas, especially air inclusions and / or liquid, especially diluent.
[0032] In the design scheme, the cold casting mold has an organic material, especially an organic polymer or plastic, which has a melting point and / or decomposition temperature in a temperature range of 40°C to 300°C, especially 60°C to 300°C, so that the cold casting mold can be plasticized, especially at a temperature in the temperature range of 35°C to 300°C, especially 50°C to 300°C, and / or can be thermally decomposed and / or thermochemically decomposed, especially at a temperature in the temperature range of 200°C to 650°C.
[0033] In the case of dental moldings, such as crowns, bridges, dental implants and / or dentures, thin-walled structures are usually required. High sintering temperatures are required precisely for the production of dental moldings from ceramics or metals. In order to avoid damage to the molding due to thermal expansion of the cold casting mold, the linear thermal expansion of the cold casting mold is advantageously a maximum of 10%, preferably a maximum of 3% and particularly preferably a maximum of 0.8%, based on the initial geometry of the cold casting mold, wherein the maximum thermal expansion of the cold casting mold is reached at a temperature of less than or equal to 240° C., preferably less than or equal to 200° C., more preferably less than or equal to 150° C. and particularly preferably less than or equal to 100° C. Preferably, the thermal expansion coefficient (WAK value) of the mixture can be adjusted by the proportion of polyelectrolyte and binder (polymer) of the cold casting mold and the WAK value, taking into account the corresponding WAK values of the metal powder, ceramic powder or glass ceramic powder used, so that the cold casting mold and the mixture are subjected to similar or identical thermal expansion. In addition or alternatively, the mechanical stability of the mixture (in the green state) can be increased by increasing the binder proportion.
[0034] In order to achieve the dimensional accuracy of the cold casting mold, especially for dental moldings, even in the pressure filling method, the cold casting mold has a Shore A hardness of at least 15 and / or a Shore D hardness of at least 10 and an elastic modulus of at least 5 MPa. The walls that delimit the cavity of the cold casting mold preferably each have a wall thickness of at least 0.01 mm. Shore hardness is a material characteristic value for elastomers and plastics and is defined in the standards DIN EN ISO 868, DIN ISO 7619-1 and ASTM D2240-00. The elastic modulus, also called tensile modulus or E modulus, is determined for plastics in particular according to DIN EN ISO 527-1:2019-12.
[0035] An exemplary prototype of a cold casting mold according to the present invention, suitable for manufacturing molded parts, in particular dental molded parts, is manufactured according to a stereolithography 3D printing method and has the following physical characteristics:
[0036]
[0037] Optical monitoring of the filling of the cold casting mold is possible by applying a raw material to the additively manufactured cold casting mold, which raw material forms one or more walls that delimit the cavity of the cold casting mold transparently and / or transparent to UV radiation. For example, the mixture or different mixtures can be optically marked, in particular with food color. The filling of the cold casting mold can then be automatically monitored by a camera.
[0038] Furthermore, the possibilities for using the cold casting mold can be expanded to include light-curing compounds which are light-cured within the cold casting mold in a correspondingly adapted method for producing a molded part, in particular a dental molded part.
[0039] Therefore, the purpose of the present invention set out at the beginning is also achieved by a method for producing a molded part, in particular a dental molded part, from a sinterable mixture according to claim 20, which method is achieved by using a cold casting mold according to the present invention according to one of the embodiments described above, and the purpose is achieved by a method for producing a molded part, in particular a dental molded part, from a light-hardening mixture according to claim 30, which method is achieved by using a cold casting mold according to the present invention according to one of the embodiments described above.
[0040] The method according to the invention for producing molded parts, in particular dental molded parts, in particular crowns, bridges, dental implants, dentures, etc., from sinterable mixed materials, such as dental ceramic or glass ceramic powders or slurries, dental metal powders or slurries, etc., which is carried out by using a cold casting mold according to the invention, and the method comprises the following method steps:
[0041] - providing and / or producing a chill casting mold having a mold cavity and at least one first opening into the mold cavity and at least one second opening into the mold cavity;
[0042] - filling the cavity of the chill casting mold with the sinterable mix via at least one first opening; and
[0043] - Hardening and / or solidifying the sinterable mixture in the cavity of the chilled casting mold.
[0044] Gas and / or liquid contained and / or included in the mixture can be discharged from the mold cavity via the at least one second opening not only when the mixture is filled but also when it hardens and / or solidifies. Optionally and immediately after filling, the gas and / or liquid contained and / or included in the mixture can also escape via the at least one first opening, which remains closed during the entire method.
[0045] Already during the hardening and / or curing of the mixed material, or optionally also after the mixed material has completely hardened, in particular to the green hardness,
[0046] - thermal and / or thermochemical decomposition of the chilled casting mold begins, in particular at a temperature in the range of 200° C. to 650° C.;
[0047] - Sintering the mixture, in particular at a temperature in the temperature range of 900° C. to 2500° C., until a ready-to-use molded part, in particular a dental molded part such as a dental prosthesis, is obtained. Optionally, the thermal and / or thermochemical decomposition of the chill mold can be continued or terminated during the sintering.
[0048] According to the invention, the claimed production method is carried out by using a chill mold having at least two openings connected to the cavity in a fluid-conducting manner, wherein the cavity of the chill mold is filled via a first opening and a fluid contained in the mixture, such as a diluent or a fluid contained by the mixture, such as air inclusions, is discharged from the opening or from the cavity via at least a further second opening. Via the at least two openings, a hardening and / or activation curing of a binder-containing and / or wet or pasty mixture, such as a slurry or suspension, can be achieved in the method according to the invention.
[0049] Therefore, preferably, according to an improvement of the method, the mixture is present in the form of a slurry and / or paste and contains a diluent, in particular water, wherein the mixture hardens in the mold cavity of the cold casting mold by drying and the liquid portion and / or moisture content of the mixture is discharged from the cold casting mold by means of at least one or more second openings, in particular the mixture is extracted.
[0050] In an advantageous method configuration, the mixture comprises metal powder, in particular CrCo powder or ceramic powder, in particular zinc oxide powder and / or aluminum oxide powder or glass ceramic powder, in particular lithium disilicate powder, and a binder, wherein the mixture, in an improved embodiment of the method configuration, hardens to the green hardness in the cavity of a cold casting mold.
[0051] The binder-containing mixture can be hardened to green body hardness in the cold casting mold only by drying, without applying pressure. Thus, the cost-intensive static pressing known according to the invention can be dispensed with by using a binder. However, compared to the methods also described in the prior art, it is necessary to harden the mixture when the cold casting mold is open (performed without a "cover", wherein the fluid is discharged from the mold cavity of the cold casting mold via at least one second opening and optionally also via at least one first opening).
[0052] In various embodiments, the binders are known from the prior art and consist mostly of organic materials, such as resins, surfactants, polyelectrolytes, polymers and / or waxes, which result in a relatively low melting point.
[0053] In order to achieve a gentle separation of the cold casting mold from the mixture before debinding or before starting to melt the binder, according to a method variant, the temperature resistance and / or thermal deformation resistance of the cold casting mold, in particular the melting point and / or decomposition temperature of the cold casting mold is lower than the melting point of the binder and / or lower than the sintering temperature of the metal powder or ceramic powder.
[0054] For the method according to the invention, it is proposed to use a chill mold that can be thermally and / or thermochemically decomposed. Preferably, the thermal and / or thermochemical decomposition of the chill mold is carried out in a sintering furnace, wherein the chill mold is opened and placed in the sintering furnace together with the mixture located therein. The thermal decomposition of the chill mold is already started or completely carried out at a temperature in the range of 200° C. to 650° C. The corresponding sintering temperature of the ceramic powder or metal powder contained in the sinterable mixture is in the range of 1200° C. to 2500° C., so that the chill mold is completely or nearly completely thermally and / or thermochemically decomposed until the final hardness of the finished, i.e. densely sintered, molded part is obtained. In this way, the chill mold can be present without additional working steps and can be removed gently during the sintering process and without damaging the molded part.
[0055] An optional method step provides for pre-sintering of the mixture before the actual sintering, in particular at a temperature in the temperature range of 650° C. to 1300° C., in order to remove the binder content before the molded part is compacted to the final hardness.
[0056] According to one method variant, the decomposition of the chill mold is carried out pyrolytically in the absence of oxygen. In particular, the chill mold is placed for this purpose together with the mixture contained therein in a sintering furnace, which allows sintering under vacuum and / or in a protective atmosphere. This method variant is particularly suitable for producing metallic dental moldings, for example from CrCo alloys, in order to avoid damage due to oxidation.
[0057] However, in particular in order to obtain the dental advantages of ceramics, according to another method variant, decomposition of the cold cast mold by combustion is possible under oxygen supply.
[0058] The method according to the invention for producing a molded part, in particular a dental molded part, from a light-hardening compound is realized by using a cold casting mold according to the invention and comprises the following steps:
[0059] - providing and / or producing a cold casting mold having a mold cavity and at least one first opening into the mold cavity and at least one second opening into the mold cavity,
[0060] - filling the cavity of the chill casting mold with the light-hardened mixture via at least one first opening;
[0061] - hardening and / or solidifying the mixture in the cavity of the chilled casting mold,
[0062] Gas and / or liquid contained and / or included in the light-curing mixture is discharged from the mold cavity via at least one second opening. In order to also produce a molded part, in particular a dental molded part, from the light-curing mixture, it is proposed according to the invention that the fluid contained therein can escape via at least one second opening during filling and / or hardening or curing. Especially when using multi-component materials, which have to be mixed with one another during filling, undesirable air inclusions often result. Also during filling with the mixture, such air inclusions can escape via at least one second opening of the chill mold.
[0063] Optionally, thermal and / or thermochemical decomposition of the cold casting mold can be omitted. According to the invention, the cold casting mold is separated or separated from the mixture along one or more predetermined breaking points of the cold casting mold in order to obtain a molded part that is particularly ready for use, in particular a dental molded part, such as a denture. The predetermined breaking points are preferably already formed during the production of the cold casting mold, and in particular this can involve a wall area with a smaller wall thickness than the remaining wall areas. In particular, by blowing in compressed air or by using an eccentric tool, the cold casting mold can be "torn" along the predetermined breaking points and thus separated from the molded part after the mixture has hardened and / or solidified.
[0064] According to an advantageous method, the mixture comprises an organic material, in particular a plastic or a composite material based on plastic, in particular a hybrid composite material based on plastic or a nanohybrid composite material. Such composites have hitherto been generally used in dental technology for fillings or temporary parts. However, it is also possible in principle to achieve the material properties required for dental moldings, such as dental prostheses, with regard to hardness and density, precisely with the aid of nanohybrid composite materials having a high fiber or particle filler content.
[0065] In an advantageous variant of the method, the mixture hardens in the cavity of the chill mold by a chemical reaction, for example by means of a two-component adhesive. The chemical reaction can be initiated by the action of heat and / or dehumidification. Particularly preferably, the chemical reaction is triggered by the action of light, wherein the walls delimiting the cavity of the chill mold are transparent and / or permeable to UV radiation and the chill mold is irradiated with a light source, in particular a UV lamp.
[0066] Preferably, the mixed material is hardened in the cavity of the chill mold to a desired final hardness, ie the hardness of the produced molded part, before the chill mold is separated or removed.
[0067] The following description paragraphs contain advantageous method variants which are applicable both for the production of molded parts according to the invention from sinterable mixed materials and for the production of molded parts according to the invention from chemically hardening, in particular light-hardening, mixed materials.
[0068] Thus, for example, the chill mold, in particular the walls of the chill mold which bound the cavity, can be coated with a coating agent before filling with the mixture in order to avoid a friction fit and / or a material bond between the chill mold and the mixture.
[0069] It is conceivable that the cold casting mold is immersed in a basin with an organic oily liquid such as petroleum before or immediately before filling with the mixture, or alternatively is flushed with an organic oily liquid such as petroleum. In this way, a heat-resistant protective layer between the walls of the cold casting mold that delimit the mold cavity and the mixture can be formed simply and uncomplicatedly without closing the first and / or second opening.
[0070] Preferably, the cavity of the chill casting mold is filled under pressure, wherein the internal pressure prevailing in the cavity is less than the filling pressure at which the mixed material is supplied to the cavity.
[0071] In a practical embodiment, it is conceivable that in a vacuum filling device represented in this way (similarly, for example, in a filling facility for bottles), a negative pressure (0.1 mbar to 0.5 mbar) can be generated in the cavity relative to the surrounding environment or vacuum, thereby "sucking" the mixture into the cavity. After filling, the vacuum or negative pressure is dissolved so that liquid and / or gas can escape from at least one second opening and / or at least one first opening. In the first variant, the filling pressure then corresponds to the ambient pressure. In the second variant, the mixture can be sprayed into the cavity under pressure, for example, with the help of a pump, a screw conveyor or a simple syringe, with an overpressure in the range of, for example, between 1.5 mbar and 10 bar, wherein liquid and gas can escape from at least one second opening already during filling. A known pressure filling method is, for example, an injection molding method.
[0072] After filling, the mixture is advantageously cured in the cavity of the cold casting mold under the action of heat, wherein the cold casting mold filled with the mixture and opened is placed in a drying cabinet or air conditioning cabinet or sintering furnace and set to a temperature in the temperature range of 35° C. to 120° C., preferably 50° C. to 120° C. If necessary, the air humidity can also be set to the desired value. For gentle, uniform and at the same time rapid drying, an air humidity in the range of 1% to a maximum of 50% has proven to be advantageous.
[0073] The hardening and / or curing of the mixture can be accelerated by the action of heat and, if necessary, by the reduced humidity, for example, in the case of a drying process. In particular, the atmospheric or ambient air present in the environment, i.e. in a drying cabinet or air-conditioning cabinet or in a sintering furnace, is dried, whereby the moisture and / or liquid contained in the mixture is transferred more quickly from the mold cavity to the environment. This effect can have a significant influence on the drying time, especially in the case of a design of the wall of the chill mold with a porous and / or water-absorbing surface, which is penetrated by a plurality of second openings in the form of pores and / or capillaries.
[0074] According to one method option, the cold casting mold is plasticized after being filled with the mixture and preferably also after it has hardened, so as to separate the wall delimiting the cavity from the mixture located therein, wherein the cold casting mold filled with the mixture is placed in a drying cabinet or air-conditioning cabinet or sintering furnace and set to a temperature in the temperature range of 35° C. to 300° C., preferably 45° C. to 180° C. In this case, the material properties of organic materials or plastics can be used. Before the melting point of the cold casting mold is reached, the organic material, in particular the plastic, softens, whereby the cold casting mold is plasticized or plastically deformable. The softened, deformable cold casting mold can be separated from the preferably hardened mixture by blowing in compressed air in a targeted manner.
[0075] Particularly rapid and uniform filling can be achieved, for example, in an embodiment variant of the method in which the cavity of the chill casting mold is filled with the mixed material via a plurality of first openings.
[0076] Thus, for example, a mixture of one or more components can be filled into the cavity of a chill mold via two or more first openings in order, for example, to prevent premature (light-influenced) hardening and / or curing during filling.
[0077] In an improvement of the present embodiment variant, the cavity of the cold casting mold is filled via a plurality of first openings with a corresponding mixture containing additives for coloring and / or for producing opacity in order to produce a molded part, in particular a dental molded part, having areas of different colors and / or opacities.
[0078] In this way, the natural appearance of teeth can be simulated. Different mixtures, in particular different additives, can produce the colors A1 to A4, B1 to B4, C1 to C4 and D1 to D4 according to the standard color wheel of Vita from Bad Säckingen. A number of corresponding additives are known from the prior art. Examples of suitable coloring elements are Fe, Mn, Cr, Ni, Co, Pr, Ce, Eu, Gd, Nd, Yb, Tb, Er and Bi.
[0079] Finally, according to an advantageous method variant, the chill casting mold is produced according to one of the method variants described at the outset for the production of a chill casting mold. BRIEF DESCRIPTION OF THE DRAWINGS
[0080] Further details, features, feature (sub) combinations, advantages and effects of the present invention are apparent from the following description of preferred embodiments of the present invention and from the accompanying drawings. The accompanying drawings show:
[0081] Figure 1 A schematic perspective view showing a first embodiment of a chill casting mold according to the invention with a filling channel and a compensation volume;
[0082] Figure 2 Show Figure 1 A cross-sectional view of a cold casting mold in FIG.
[0083] Figure 3 A schematic perspective view showing a second embodiment of a chill casting mold according to the invention with a filling channel;
[0084] Figure 4 A sectional view showing a third embodiment of a chill casting mold according to the invention having a total of five filling channels;
[0085] Figure 5 A schematic perspective view showing a fifth embodiment of a chill casting mold according to the invention having five filling channels and a mixing mechanism;
[0086] Figure 6 Shown with connected filling mechanism Figure 5 A cross-sectional view of a cold casting mold in FIG.
[0087] Figure 7 A schematic side view showing a fourth embodiment of a chill casting mold according to the invention with a wall reinforcement and a predetermined breaking point;
[0088] Figure 8 A schematic perspective view of a molded part produced by means of a chill casting mold according to the invention is shown;
[0089] Fig. 9 Shown are filled with different mixtures Figure 4 A cross-sectional view of a cold casting mold in FIG.
[0090] Fig.10 Show Fig. 9 Schematic diagram of the cavity of a chill casting mold filled with different mixtures;
[0091] Fig.11 Show Fig. 9 A cross-sectional view of a cavity of a chill casting mold filled with different mixtures;
[0092] Fig.12 A flow chart showing an exemplary process of the method according to the invention for producing a molding, in particular a dental molding;
[0093] Fig.13 Show Figure 1 and 2 A schematic cross-sectional view of a chill casting mold in which the chill casting mold is electrophoretically filled with a mixed material;
[0094] Fig.14 Show Figure 1 and 2 A schematic cross-sectional view of a chill casting mold in which the chill casting mold is filled with a mixture under pressure; and
[0095] Fig.15 A schematic diagram of a chill casting mold is shown, the cavity of which corresponds to the shape of the dental prosthesis.
[0096] The drawings are merely exemplary and serve only to understand the invention. Identical elements are provided with identical reference numerals and are therefore generally only described once. DETAILED DESCRIPTION
[0097] Figure 1 and 2 A first exemplary embodiment of a cold casting mold 100 according to the invention is shown in a schematic perspective view or in a sectional view, respectively. The cold casting mold 100 is designed here as a test body, for example, whose cavity 110 has geometrical properties typical for a dental molding 210, which result in a wall thickness of the molding 210 in the range of 0.30 mm to 10 mm. The cavity 110 of the cold casting mold 100 is delimited by an outer wall 121 and an inner wall 122 of the cold casting mold 100, so that the finished molding 210, for example a crown, has an inner cavity 211 (see Figure 8 ), which cavity corresponds, for example, to the shape of the abutment, so that the crown can be placed on the abutment. For this purpose, the inner wall 122 is formed in the shape of a cylinder or a truncated cone. A first opening 111 is introduced into the cavity 110, which passes through the outer wall 121 that is engaged with the dental molding 210. The cavity 110 is filled with the mixture 200 via the first opening 111. The inner wall 122 is penetrated by a plurality of second openings 112, which, for example, allow the fluid 205, 207 and / or air inclusions 208 contained in the mixture 200 to escape during the filling. After the filling, the fluid 205, 207, 208 can optionally escape additionally via the first opening 111. The plurality of second openings 112 can, as shown here by way of example, pass through the inner surface of the cavity 110 in a sieve-like manner. Alternatively, the plurality of second openings 112 may be designed in the form of pores and / or capillaries and form a porous and / or water-absorbent surface.
[0098] A filling channel 130 having a compensation volume 131 is connected in a fluid-conducting manner to the first opening 111. A filling device 400, such as a syringe 420, in particular a low-pressure syringe (see Fig.15 ) or an input line, such as hose 410 (see Figure 6 ), in order to fill the mold cavity 110 with the mixture 200. The compensation volume 131 serves as a kind of reservoir for the mixture 200, so that the volume loss of the fluid 205, 207, 208 that escapes through the second opening 112 can be compensated by means of the mixture 200 stored in the compensation volume 131. In the embodiment shown, the cold casting mold 100 is manufactured in one piece with the filling channel 130 and the compensation volume 131.
[0099] exist Figure 3 FIG. 2 shows a schematic perspective view of a second embodiment of a cold casting mold 100 according to the present invention. The cold casting mold 100 corresponds to Figure 1 and 2 , with the difference that the filling channel 130 is designed without the (optional) compensation volume 131 and the channel-like second opening 112 opens in one piece into the interlocking, external wall 121. The filling channel 130 can optionally be realized in one piece or also as an additional part of the cold casting mold (100) and opens into the mold cavity (110) with its first opening 111. In this variant, the first opening 111 runs coaxially through the second opening 112. If necessary, a separate compensation volume 131 is connected to the filling channel 130, especially as a component of the filling device 400.
[0100] Figure 4 A sectional view of a third embodiment of a chill mold 100 according to the invention with a total of five filling channels 130 can be found in FIG. The filling channels 130 each lead into the mold cavity 100 via a first opening 111 that penetrates the interlocking, external wall 121 of the chill mold 100. Each filling channel 130 is connected to an associated compensation volume 131 in a fluid-conducting manner. The chill mold 100 can optionally be filled with the same or different mixtures 200 via one or more filling channels 130, wherein the filling channels 130 that are not used for filling are then used as corresponding second openings 112 and for discharging the fluid 205, 207 and / or air inclusions 208 contained in the mixture 200. In particular, when all filling channels 130 are utilized, a rapid and particularly uniform filling of the mold cavity (110) of the chill mold 100 is possible.
[0101] from Figure 5A schematic stereoscopic view of a fourth embodiment of a cold casting mold 100 according to the present invention can be obtained in FIG. The cold casting mold 100 has a total of five filling channels 130, which lead into the mold cavity 110 via a first opening 111 through an interlocking wall 121 located on the outside. One of the filling channels 130 is provided with a conveying and / or mixing mechanism 132, which is in the form of a screw conveyor. The filling channel 130 is designed to have a larger cross-sectional area, in particular a larger diameter, than the remaining four filling channels 130. According to the diagram shown, the conveying and / or mixing mechanism 132 is pushed into the filling channel 130, which is preferably formed integrally with the cold casting mold 100, as an additional component. It is particularly advantageous that the conveying and / or mixing mechanism 132 can be formed directly inside the filling channel 130 during the production of the cold casting mold 100 without indirect material addition.
[0102] Figure 6 According to Figure 5 1 , which has an additional corresponding compensation volume 131, which is connected to the corresponding filling channel 130 in a fluid-conducting manner. A filling device 400 is connected to the filling channel 130, which includes a conveying and / or mixing device 132, via two hoses 420. The mixed material 200 is conveyed to the cold casting mold 100 via the hoses 420. The embodiment shown here is particularly well suited for a mixed material 200, which consists of, for example, two components. Via the two hoses 420, the components can first be conveyed separately to the filling channel 130 and mixed with each other there by means of the conveying and / or mixing device 132, and the mixed mixed material 200 then enters the mold cavity 110 through the first opening 111.
[0103] The fifth embodiment of the cold casting mold 100 according to the present invention can be Figure 7 . Along the outer wall 121 delimiting the cavity 110, the chill mold 100 is formed integrally with two wall reinforcements or projections 123, each in the form of a flange. The section of the respective outer wall 121 between the wall reinforcements 123 is manufactured to have a smaller wall thickness than the wall reinforcements 123 and thus serves as a predetermined breaking point 124. By introducing an eccentric tool 125 between the two wall reinforcements 123, the chill mold 100 can be "rocked" along the predetermined breaking point 124, so that the chill mold 100 is separated from the hardened mixture 200 therein.
[0104] The mixed material 200 hardened to the final hardness required for the dental molding 210 is obtained from Figure 8The finished molded part 210 is obtained in the form of a cold casting mold 100 which is designed as a test body. The molded part 210 has a wall thickness in the range of 0.3 mm to 10 mm. The lower tip section of the molded part 210 is designed with a recess 211, the shape of which corresponds to the shape of an abutment for fitting the dental molded part 210, for example a crown. The inner wall 122 (see FIG. 1 ) of the cold casting mold 100 is penetrated by a sieve-like structure. Figure 2 ), the inwardly directed wall of the recess 211 is provided with a knob-like surface 212. The knob-like surface 212 improves the support between the dental molding 210, such as a crown and, for example, an abutment.
[0105] exist Fig. 9 Shown in cross-sectional view Figure 4 The cold casting mold 100 in the embodiment of the present invention is shown in FIG. The cavity 110 of the cold casting mold 100 is filled with different mixed materials 201, 202, 203, 204 via a filling device 400. The mixed materials 201, 202, 203, 204 each contain an additive, which is suitable for coloring and / or creating opacity for the finished molded part 210. Each mixed material 201, 202, 203, 204 is preferably filled into the cavity 110 via its own filling channel 130 and the first opening 111 respectively connected thereto.
[0106] Fig.10 and 11 Schematic cross-sectional views of the mold cavity 110 filled with different mixtures 201, 202, 203, 204 are shown. For example, the lower tip section of the mold cavity 110 can be filled with the third mixture 203, the two outer, occlusal sections can be filled with the first mixture 201 or the fourth mixture 204, and the occlusal section located therebetween can be filled with the second mixture 202. After hardening and / or curing to the final hardness, the dental molding 210 produced then has regions or sections of different coloring or tooth color and / or different opacity or transparency.
[0107] Fig.12A flow chart of an exemplary process of the method according to the invention for producing a dental molding 210 is shown. Here, first, a cold casting mold 100 is provided or produced (1). The cold casting mold 100 is produced by means of an additive manufacturing method, for example by means of a 3D printer, wherein the cold casting mold 100 has at least one opening 111 and at least one second opening 112. As the raw material 150, preferably a plastic that can be thermally decomposed and / or thermally decomposed by respiration is used. Optionally, the cold casting mold 100 can already be configured to have one or more preset fracture sites 124 during production. Optionally, the cold casting mold 100 can be coated with a coating agent 220 before it is filled with the mixture 200 (1.1). For example, petroleum is suitable as the coating agent 220, wherein the cold casting mold 100 is preferably inserted into a basin with petroleum. Subsequently, the cold casting mold 100 is filled with the mixture 200 (2). Depending on the desired molding 210, the mixture 200 includes a ceramic or metal powder 209, which is suitable for producing a dental molding. Preferably, the corresponding powder 209 is stirred into a slurry or paste with the aid of a diluent 205, such as water or an organic solvent, mixed with a binder 206 and pre-treated before use. The mixture 200 is filled into the cavity 110 of the cold casting mold 100 via at least one first opening 111. During the filling, the fluid 207 contained in the mixture 200, in particular the diluent 205 or air inclusions 208, can already escape via at least one second opening 112. After filling, the mixture 200 is hardened or solidified inside the cold casting mold 100, more precisely in its cavity 110 (3). In order to accelerate the hardening or solidification, the cold casting mold 100 is placed, for example, in a drying cabinet or an air-conditioning cabinet to set the desired air humidity of the environment and is subjected to heat 230, so that the liquid components of the mixture 200 are dried or volatilized more quickly. Here, fluid 207, diluent 205 or air inclusions 208 can also escape via at least one second opening 112 and optionally additionally via at least one first opening 111. In order to produce a dental molding 210 from plastic, the cold casting mold 100 is designed to be transparent and acted upon with light 231, in particular UV light. In the case of dental plastics, hardening to the final hardness in the cold casting mold 100 is possible. In order to produce a ceramic or metallic dental molding 210, hardening in the cold casting mold 100 is preferably carried out to the green body hardness. The stability of the green body can be achieved by the adhesive 206 used.
[0108] After hardening, the cold casting mold 100 is plasticized (3.1). For this purpose, the cold casting mold 100 is placed in a sintering furnace together with the hardened mixed material 200 located therein and a temperature in the range of 35° C. to 300° C., in particular 50° C. to 300° C., is set inside the sintering furnace. The plastic of the cold casting mold 100 softens and can be "blown" and separated from the mixed material 200, for example by blowing in compressed air 232. In the case of a dental plastic molding 210, the cold casting mold 100 is separated by mechanical force along one or more predetermined breaking points 124 formed during production (4.B) and the finished dental molding 210 is removed.
[0109] In order to produce a ceramic or metallic dental molding 210, the cold casting mold 100 is thermally or thermochemically decomposed (4.A) before or during the hardening of the mixture 200 to the final hardness. For this purpose, the cold casting mold 100 is placed in a sintering furnace together with the mixture 200 located therein and the thermal decomposition or pyrolysis is started in the absence of oxygen or the thermochemical decomposition or combustion is carried out with the aid of oxygen at a temperature in the temperature range of 200° C. to 650° C., wherein the raw material 150 is completely or nearly completely melted. At a temperature in the temperature range of 650° C. to 1300° C., the mixture 200 can optionally be pre-sintered (5.1), wherein the binder 206 is volatilized. During the final final sintering or densification sintering (5), the mixture 200 is compacted to the final hardness at a temperature in the temperature range of 900° C. to 2500° C. and can be removed from the sintering furnace as a finished dental molding 210. Possible remnants of the chill mold 100 which have not yet completely decomposed are also decomposed during the pre-sintering or final sintering.
[0110] Fig.13 Show Figure 2The invention relates to a possible filling of a chill mold 100 in a mold by means of electrophoresis, in particular electrofiltration. The filling device 400 is designed in the form of an electrophoresis device. For electrofiltration, it is necessary that the mixture 200 is conductive, for example, it includes metal powder, and the chill mold 100 is optionally an insulator, for example, made of plastic or also conductively made of conductive polymer. At least one first opening 111 of the chill mold 100 is connected to the cathode 430 of the filling device 400 in a conductive manner via the mixture 200. A plurality of second openings 112 are also connected to the anode 431 of the filling device 400 in a conductive manner via the conductive mixture 200. By applying a voltage via a voltage source 432, an electric current can be generated, which causes the particle transfer from the cathode 430 to the anode 431. It has been confirmed in experiments that about 80% of the diluent 205 escapes from the mixture 200 during the electrophoretic filling of the chill mold 100, which results in a significantly shortened process time. The remaining water content remaining in the mixed material 200 escapes, as described in detail above with respect to the plurality of second openings 112, in particular with respect to the porous and / or water-absorbing surface formed by the second openings, until the mixed material 200 hardens and / or solidifies. Preferably, the first opening 111 arranged in the region of the cathode 430 or the filling channel 130 connected thereto is provided with a siphon 433, which in the water-containing mixed material 200 allows the hydrogen formed there to escape, in order to ensure the homogeneity of the mixed material 200.
[0111] Fig.14 Show Figure 1 and 2 Schematic cross-sectional view of a chill casting mold 100 in FIG. 1 , which is pneumatically filled with a mixture 200 under pressure. The method is particularly suitable for mixing and filling powdered mixtures 200, but is also suitable for slurries or pastes. For filling, the chill casting mold 100 or its cavity 110 is used in the form of a vacuum bag, wherein the pressure prevailing in the cavity 110 is less than the ambient pressure. This can be achieved, wherein the mixture 200 is delivered to the cavity 110 via a conveying line 440 under pressure of a filling device 400 configured as a pressure device. The introduction of the mixture 200 into the conveying line 440 can be achieved by means of a rotary valve, a pressure vessel and / or a pressure conveying facility.
[0112] Alternatively or additionally, a vacuum can also be generated in the cavity 110 of the cold casting mold 100, thereby realizing vacuum conveying or also suction conveying of the mixed material 200. A vacuum is generated centrally or dispersedly by means of a vacuum generator 441 so that the mixed material 200 is sucked and transported into the cavity 110 of the cold casting mold 100 via at least one first opening 111. The mixed material 200 is retained inside the cavity 110 via a plurality of second openings 112 or wall sections located therebetween. The conveying air 442 for conveying the mixed material 200 passes through a plurality of second openings 112 and is input from the environment via a particle filter 443. The control of the filling is simplified via a bypass channel 444, which is connected to the filling channel 130 in a fluid-conducting manner.
[0113] at last, Fig.15 An exemplary embodiment of the invention is shown, in which a cold casting mold 100 has a cavity 110 which corresponds to the geometry of a dental molding 210. Also schematically indicated in the illustration is a pressure nozzle 310 of a 3D printer 300, by means of which the cold casting mold 100 is additively manufactured in one piece from a raw material 150. The cold casting mold 100 comprises a first opening 111 which is connected to a filling channel 130 in a fluid-conducting manner via a valve-controlled compensation volume 131. The cavity 110 is filled with a mixture 200 via the filling channel 130 by means of a filling device 400, here by way of example a syringe 420. The fluid 207 contained in the mixture 200 or the air inclusions 208 produced during the filling are discharged from the cavity 110 via a plurality of second openings 112. The second openings 112 are designed here as capillaries or holes in an outer wall 121 and are therefore not visible to the naked eye. A porous or water-absorbent surface is produced by the plurality of second openings 112 , which conducts fluid 207 or moisture contained in the mixture 200 out of the mold cavity into the external environment.
[0114] Reference numerals list
[0115] 100 Cold Casting Mold
[0116] 110 Cavity or tool mold
[0117] 111 First Opening
[0118] 112 Second Opening
[0119] 120 Wall
[0120] 121 External wall
[0121] 122 Internal wall
[0122] 123 Wall reinforcement / wall protrusion
[0123] 124 Preset fracture location
[0124] 125 Eccentric tool
[0125] 130 Filling channel
[0126] 131 Compensation volume
[0127] 132 Transmission and / or mixing mechanisms
[0128] 140 Support structure
[0129] 150 raw materials
[0130] 200 Mixture 201, 202,
[0132] 203, 204 Mixtures with additives
[0133] 205 Thinner
[0134] 206 Adhesive
[0135] 207 Fluid
[0136] 208 Air inclusions
[0137] 209 Powder
[0138] 210 Molded parts
[0139] 211 Notch
[0140] 220 coating agent
[0141] 230 Heat / Air Moisture
[0142] 231 Light
[0143] 232 Compressed air
[0144] 300 3D Printer
[0145] 310 Pressure Nozzle
[0146] 400 Filling mechanism
[0147] 410 Hose
[0148] 420 Syringes, especially low-pressure syringes
[0149] 430 Cathode
[0150] 431 Anode
[0151] 432 Voltage Source
[0152] 433 Siphon
[0153] 440 Transmission pipeline
[0154] 441 Vacuum generator
[0155] 442 Air Transmission
[0156] 443 Particle Filter
[0157] 444 Bypass channel
[0158] Method steps:
[0159] 1 Provide and / or manufacture cold casting molds
[0160] 1.1 Coating of chill casting molds
[0161] 2 Fill the cold casting mold with the mixture
[0162] 3 Harden and / or solidify the mixture in the cold casting mold
[0163] 3.1 Plasticizing the cold casting mold
[0164] 4.A Thermal or thermochemical decomposition of the cold casting mold
[0165] 4.B Mechanical separation of the cold casting mold from the mixture
[0166] 5.1 Pre-sintering
[0167] 5 Sintering
Claims
1. A method for producing a chill casting mold (100), wherein the chill casting mold (100) is used to produce a molded part (210) from a mixed material (200), wherein the chill casting mold (100) has a cavity (110) corresponding to the geometry of the molded part (210), the chill casting mold (100) is additively manufactured from a raw material (150) based on a digital data record by means of an additive manufacturing method, and the chill casting mold (100) has at least one first opening (111) leading into the cavity (110) for filling with the mixed material (200), characterized in that Additively manufactured and one-piece manufactured cold casting mold (100), the cold casting mold having at least one second opening (112) leading into the mold cavity (110) and / or leading out of the mold cavity (110), the second opening (112) being used to discharge gas (208) and / or liquid (205), and having a filling channel (130) adjacent to at least one of the first openings (111) in a fluid-conducting manner, wherein the filling channel (130) is connected in a fluid-conducting manner to at least one compensation volume (131) for storing a mixed material (200).
2. The method according to claim 1, It is characterized in that At least one wall portion (120) of the cold casting mold (100) that limits the mold cavity (110) is constructed completely or partially by additive manufacturing, and the wall portion has a plurality of second openings (112) that extend into the mold cavity (110) and pass through the wall portion (120), and the second openings are used to discharge gas (208) and / or liquid (205).
3. The method according to claim 2, It is characterized in that A plurality of second openings (112) are formed in the form of pores and / or capillaries extending through the wall (120), so that the wall (120) completely or partially has porous and / or water-absorbing properties.
4. The method according to any one of claims 1 to 3, It is characterized in that The cold casting mold (100) is additively manufactured and has two or more first openings (111) respectively leading into the mold cavity (110), wherein the first openings are used to be filled with a mixed material (200) simultaneously or at a time offset.
5. The method according to claim 1, It is characterized in that An organic material is used as a raw material (150) for additively manufacturing a chill casting mold (100), so that the chill casting mold (100) can be plasticized and / or thermally decomposed and / or thermochemically decomposed.
6. The method according to claim 5, It is characterized in that The organic material used for additive manufacturing of the chill casting mold (100) has a melting point or a decomposition temperature in the temperature range of 40°C to 300°C.
7. The method according to claim 5, It is characterized in that The organic material used for additive manufacturing of the cold casting mold (100) can be plasticized or softened by heat when the temperature is in the range of 35°C to 300°C.
8. The method according to claim 5, It is characterized in that The organic material used for additive manufacturing of the chill casting mold (100) can be thermally decomposed by pyrolysis and / or thermochemically decomposed by combustion at a temperature in the range of 200° C. to 650° C. by the action of heat.
9. The method according to claim 1, It is characterized in that At least one wall portion (120) that delimits a cavity (110) of the chill casting mold (100) is additively manufactured, the wall portion having a predetermined breaking point (124).
10. The method according to claim 1, It is characterized in that The digital data record for the geometrical design of the cavity (110) of the chill mold (100) based on a spatial model of the patient's oral cavity includes the volume shrinkage of the mixed material (200) due to sintering and / or hardening.
11. A chill casting mold (100) for producing a molded part (210) from a mixed material (200), the chill casting mold (100) being produced in one piece by means of a method according to claim 1, wherein the chill casting mold (100) has a cavity (110) and at least one first opening (111) leading into the cavity (110) for filling with the mixed material (200), wherein the cavity (110) corresponds geometrically to the molded part (210) and is created according to a digital data record, It is characterized in that The cold casting mold (100) has at least one second opening (112) leading to the mold cavity (110), the second opening being used to discharge gas (208) and / or liquid (205), and has a filling channel (130) adjacent to the at least one first opening (111) in a fluid-conducting manner, wherein the filling channel (130) is connected to at least one compensation volume (131) for storing a mixed material (200) in a fluid-conducting manner.
12. The chill casting mold (100) according to claim 11, It is characterized in that The cold casting mold (100) has an organic material, which has a melting point or a decomposition temperature in the temperature range of 40°C to 300°C, so that the cold casting mold (100) can be plasticized when the temperature is in the temperature range of 35°C to 300°C and / or can be thermally decomposed and / or thermochemically decomposed when the temperature is in the temperature range of 200°C to 650°C.
13. The chill casting mold (100) according to claim 12, It is characterized in that The linear thermal expansion of the chill casting mold (100) is up to 10% based on the initial geometry, wherein the maximum thermal expansion of the chill casting mold (100) is at a temperature less than or equal to 240°C.
14. The chill casting mold (100) according to claim 11, It is characterized in that One or more walls (120) delimiting the cavity (110) of the chill mold (100) are transparent and / or transparent to ultraviolet radiation.