A kind of explosive bead for cigarettes coated with water-soluble flavor and preparation method thereof

By using a skin-core structure that combines wax materials and tricyclic diterpenoid compounds in cigarette popping beads, and an inner wall material of polysaccharide materials, the stability and sealing performance of cigarette popping beads in the existing technology are solved. It solves the problem of poor quality, achieves uniform release of aroma and improves production efficiency.

CN114847516BActive Publication Date: 2024-10-18WUYI UNIV
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202210353874.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-04-02
Publication Date
2024-10-18
Estimated Expiration
2042-04-02

AI Technical Summary

Technical Problem

Existing cigarette popping beads have problems such as stability risks, poor sealing performance and high process complexity when using single-layer, double-layer or three-layer structures. It is difficult to effectively cover water-soluble flavors, resulting in uneven aroma release and product production. Low efficiency.

Method used

Wax waterproof materials are used as outer wall materials, and tricyclic diterpenoids are added as supporting materials to form a skin-core structure. Polysaccharide materials are combined as inner wall materials to improve sealing and stability while simplifying process steps. .

Benefits of technology

It achieves an increase in the strength and sealing performance of wax materials, prevents water molecules from penetrating, extends the service life of the exploding beads, reduces production costs, and improves product stability and production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114847516B_ABST
    Figure CN114847516B_ABST
Patent Text Reader

Abstract

The present invention relates to a tobacco popping bead coated with a water-soluble flavor and a preparation method thereof, and belongs to the field of tobacco. The tobacco popping bead is provided with a skin-core structure, and the skin-core structure includes an outer wall material and a core liquid; the outer wall material includes wax and a tricyclic diterpenoid compound, and the core liquid includes a water-soluble flavor and an additive. This scheme uses a tricyclic diterpenoid compound as a supporting material to give the popping bead a certain strength, and further strengthens the sealing effect of the wall material on the core liquid to prevent the popping bead from becoming a hollow shell.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of tobacco, and particularly relates to a tobacco explosive bead coated with a water-soluble flavor and a preparation method thereof. Background Art

[0002] Adding popping beads to the filter of cigarettes can increase the tobacco flavor, smoking experience and rich taste. Usually, the contents of commercial popping beads are generally based on caprylic decanoic acid glyceride as the core material, and the flavor of the popping beads is adjusted by adding different oil-soluble flavors, and polysaccharide materials (animal gelatin, sodium alginate, carrageenan, etc.) are used as wall materials to achieve sealing, so as to achieve the packaging and sealing of oil-soluble flavors with different aromas. However, the water absorption and swelling characteristics of polysaccharide materials limit the use of water-soluble flavors as popping beads to add flavor.

[0003] In order to expand the application of water-soluble flavors in popping beads, the current methods and approaches for coating water-soluble flavors are mainly: (1) Single-layer structure: a) The core liquid is emulsified by reverse phase to form an oil-in-water microemulsion, and biomass glue or synthetic resin is used as the wall material; b) Non-water-soluble polymers and their monomers are polymerized by free radicals to form a film to coat the core liquid. c) The wall material is a composite of wax, long-chain lipid material and reinforcing material. (2) Double-layer structure: a) The inner layer is wax and the outer layer is photosensitive resin material; b) The inner layer is a hydrophobic hot melt adhesive film and the outer layer is biomass glue. (3) Three-layer structure: The inner layer is a wax layer, the middle layer is a coating powder layer, and the outer layer is a hydrophilic film layer.

[0004] In the above methods and approaches, the core liquid microemulsion in the single-layer structure has a hidden danger of stability. The wax layer in the double-layer structure has poor adhesion to the photosensitive resin, and it is difficult to evenly coat the surface of the wax layer; and the hydrophobic hot melt adhesive film generally has good vapor permeability, and the water molecules in the core liquid can easily evaporate from the inside through the hot melt adhesive film, causing the outer biomass adhesive to soften and fail. The process design process in the three-layer structure is more complicated and difficult to implement. Therefore, the art needs to develop a tobacco explosive bead with a simple preparation process, stable structure, and good sealing performance. Summary of the invention

[0005] The object of the present invention is to provide a tobacco popping bead coated with a water-soluble flavor and a preparation method thereof based on the above-mentioned deficiencies of the prior art.

[0006] The present invention is achieved through the following technical solutions:

[0007] The present invention provides a tobacco popping bead coated with a water-soluble flavor. The tobacco popping bead is provided with a skin-core structure, wherein the skin-core structure comprises an outer wall material and a core liquid; the outer wall material comprises wax and a tricyclic diterpene compound, and the weight ratio of the wax to the tricyclic diterpene compound is 1:(0.5-2).

[0008] The outer wall material of the cigarette popping bead of the present invention is based on a wax waterproof material, and tricyclic diterpenoid compounds are further added as supporting materials. Since the tricyclic diterpenoid compounds are hard and brittle, they can give the popping bead a certain strength, and a crisp sound is emitted when the popping bead is crushed; at the same time, the tricyclic diterpenoid compounds have good bonding and sealing properties, and can enhance the sealing effect of the wall material on the core liquid, preventing water molecules from penetrating from the wall material in the form of vapor, causing the popping bead to become hollow.

[0009] As a preferred embodiment of the tobacco explosive beads coated with water-soluble flavors of the present invention, the weight of the outer wall material is 55-80 parts, and the weight of the core liquid is 20-45 parts.

[0010] As a preferred embodiment of the water-soluble flavor-coated popping beads of the present invention, an inner wall material is provided between the outer wall material and the core liquid to avoid the mutual repulsion between the wax material and the aqueous core liquid when in contact, and further enhance the stability of the popping bead material. The inner wall material is a polysaccharide material; the polysaccharide material is at least one of sodium alginate, gelatin, and carrageenan.

[0011] As a preferred embodiment of the tobacco explosive beads coated with water-soluble flavors of the present invention, the inner wall material is 55-80 parts by weight, and the core liquid is 20-45 parts by weight.

[0012] As a preferred embodiment of the tobacco explosive beads coated with water-soluble flavors according to the present invention, the wax is at least one of beeswax, carnauba wax, solid paraffin, and insect wax; the tricyclic diterpenoid compound is at least one of rosin resin, hydrogenated rosin resin, glycerol rosin resin, maleic anhydride rosin resin, rosin-modified phenolic resin, rosin methyl ester, and rosin vinyl alcohol ester; the core liquid includes water-soluble flavors and additives, and the weight ratio of the water-soluble flavors and the additives is 1:(0.5-1); the water-soluble flavor is at least one of blended flavors and natural plant extracts; the additive is at least one of a stabilizer, a preservative, a defoamer, a thickener, and a bactericide.

[0013] Preferably, the water-soluble flavor is at least one of a blended flavor and a natural plant extract; such components can be released after the cigarette or the heat-not-burn electronic cigarette is crushed by a bursting bead or destroyed by other external forces, thereby giving or enhancing a certain style and flavor to the cigarette or the heat-not-burn electronic cigarette, such as mint flavor, milk flavor, fruit flavor, herbal flavor, tobacco flavor, etc.

[0014] Preferably, the blended essence is essential oils such as fennel oil and patchouli oil, absolute oils such as rosemary oil and rose absolute, alcohols such as lavender alcohol, menthol, isopulegol, ethers such as anisole and methyl phenethyl ether, aldehydes such as citronellal and benzaldehyde, ketones such as ionone and methyl propylene ketone, acids such as acetic acid and lactic acid, esters such as hexyl formate and isopentyl isovalerate, esters such as octanolactone and angelica lactone, and heterocyclics such as furfuryl alcohol and 3-ethylpyridine.

[0015] As a preferred embodiment of the tobacco popping beads coated with water-soluble flavors according to the present invention, the natural extract is at least one of monk fruit extract, cocoa extract, blueberry extract, naringin extract, licorice extract, coffee extract, Zimbabwe extract, and tobacco extract.

[0016] As a preferred embodiment of the tobacco exploding beads coated with water-soluble flavors of the present invention, the weight of the exploding beads is 50-100 mg, the diameter is 3-7 mm, and the crushing strength is 5-30N.

[0017] The present invention also provides a method for preparing the above-mentioned water-soluble flavored tobacco explosive beads, comprising the following steps:

[0018] (1) taking a water-soluble flavor and an additive and mixing them evenly to obtain a core liquid; the weight ratio of the water-soluble flavor to the core liquid is 1:(2.5-22); the weight ratio of the additive to the core liquid is 1:(5-22);

[0019] (2) mixing the wax and the tricyclic diterpenoid compound in the weight ratio, stirring, heating and melting to obtain an outer wall material glue;

[0020] (3) The core liquid obtained in step (1) and the outer wall material glue obtained in step (2) are respectively fed into the dripping holes, and the core liquid droplets and the outer wall material glue droplets are dripped out to form concentric spherical droplets; the protective liquid is dripped in to cool, separate and wash, and the result is obtained.

[0021] As a preferred embodiment of the method for preparing tobacco explosive beads coated with water-soluble flavors according to the present invention, in the step (2), the heating and melting temperature of the outer wall material glue is 80°C-140°C; in the step (3), when the glue is fed into the drip hole, the flow rate of the outer wall material glue: the flow rate of the core liquid = (1.2-2.5): 1; the temperature of the outer wall material glue is 80°C-140°C, the temperature at the drip hole is 80°C-110°C, and the temperature of the core liquid is 25°C-60°C; the protective liquid is dimethyl silicone oil, and the cooling temperature is 10°C-40°C.

[0022] The present invention also provides a method for preparing the above-mentioned tobacco popping beads with inner and outer double-layer wall materials coated with water-soluble flavors, comprising the following steps:

[0023] (1) taking a water-soluble flavor and an additive and mixing them evenly to obtain a core liquid; the weight ratio of the water-soluble flavor to the core liquid is 1:(2.5-22); the weight ratio of the additive to the core liquid is 1:(5-22);

[0024] (2) mixing the wax and the tricyclic diterpenoid compound in the weight ratio, stirring, heating and melting to obtain an outer wall material glue;

[0025] (3) dissolving the polysaccharide material in water under heating and stirring conditions to obtain an inner wall material glue solution; the mass percentage of the polysaccharide material in the inner wall material glue solution is 10% to 30%;

[0026] (4) feeding the core liquid obtained in step (1) and the inner wall material glue obtained in step (3) into the dripping holes respectively, and the core liquid droplets and the inner wall material glue droplets dripped out form core spherical droplets; dripping into the protective liquid for cooling, separation and washing, so as to obtain the inner layer structure of the popping bead for cigarettes;

[0027] (5) immersing the inner layer structure of the tobacco explosive beads obtained in step (4) in the outer layer wall material glue obtained in step (2) and cooling the mixture to obtain the product.

[0028] As a preferred embodiment of the method for preparing the tobacco explosive beads with inner and outer double-layer wall materials coated with water-soluble flavors according to the present invention, in the step (2), the heating melting temperature of the outer layer wall material glue is 80°C-140°C; in the step (3), the heating temperature of the inner layer wall material glue is 65°C-80°C; in the step (4), when the glue is fed into the drip hole, the flow rate of the inner layer wall material glue: the flow rate of the core liquid = (1.2-2.5): 1; the temperature of the inner layer wall material glue is 65°C-80°C, the temperature at the drip hole is 65°C-80°C, and the temperature of the core liquid is 25°C-60°C; the protective liquid is a calcium chloride aqueous solution with a mass fraction of 5%-20%, and the cooling temperature is 10°C-40°C.

[0029] The beneficial effects of the present invention are as follows: (1) Compared with the existing single-layer structure design scheme, tricyclic diterpenoid compounds are used as supporting materials on the basis of wax waterproof materials. On the one hand, the hard and brittle characteristics of tricyclic diterpenoid compounds are utilized to give the popping beads a certain strength, and a crisp sound is emitted when they are squeezed in use; on the other hand, the good bonding and sealing properties of tricyclic diterpenoid compounds can be utilized to further enhance the sealing effect of the wall material on the core liquid, prevent water molecules from penetrating from the wall material in the form of vapor, causing the popping beads to become hollow shells, and enhance the stability of the popping bead structure; in addition, tricyclic diterpenoid compounds also have certain medicinal effects, such as antitussive and expectorant, myogenic and analgesic, etc. (2) Compared with the use of other long-chain lipid materials and supporting materials, tricyclic diterpenoid compounds are not only derived from nature, and their use is in line with current environmental protection concepts and requirements, but also have low prices, which can further reduce the production cost of popping beads and increase product profit margins. (3) Compared with the three-layer structure, the structural design in this scheme simplifies the subsequent process steps, shortens the popping bead preparation cycle, and improves production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 Schematic diagram of the preparation of cigarette explosive beads with outer wall material covering core liquid;

[0031] Figure 2 Schematic diagram of the preparation of a cigarette-use explosive bead with an inner and outer double-layer core material injection syringe wall material coated with a core liquid;

[0032] Among them, 1-core material injection syringe, 2-wall material injection syringe, 3-injection pump, 4-coaxial double-layer dripper, 5-inner core delivery channel, 6-outer wall delivery channel, 7-protective liquid, 8-screen, 9-molten outer layer glue DETAILED DESCRIPTION

[0033] To better illustrate the purpose, technical solutions and advantages of the present invention, the present invention will be further described below in conjunction with specific embodiments. It should be understood by those skilled in the art that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.

[0034] Unless otherwise specified, the test methods used in the examples are all conventional methods; the materials and reagents used are all commercially available unless otherwise specified. The following "parts" are all parts by weight.

[0035] Example 1

[0036] A tobacco popping bead coated with a water-soluble flavor, the tobacco popping bead is provided with a skin-core structure, the skin-core structure comprises an outer wall material and a core liquid; the outer wall material comprises 100 parts of beeswax and 160 parts of rosin resin; the core liquid comprises 100 parts of water, 5 parts of a water-soluble flavor (Zimbabwe extract), 2.5 parts of a preservative (kathion), and 2.5 parts of a thickener (sodium alginate).

[0037] The preparation method of the above-mentioned tobacco popping beads coated with water-soluble flavor is as follows:

[0038] 1) mixing water, water-soluble flavor, preservative and thickener according to a formula to obtain a core liquid;

[0039] 2) Evenly mix the beeswax and rosin resin according to the formula ratio, heat to 120° C. under stirring, and melt to obtain the outer wall material glue; then repeatedly evacuate the outer wall material glue to remove bubbles in the glue.

[0040] 3) If Figure 1 The schematic diagram of the preparation of the cigarette explosion beads with the outer wall material covering the core liquid is shown in the figure. Figure 1 The dripping pill machine shown comprises a core material injection syringe 1, a wall material injection syringe 2, and a coaxial double-layer dripper 4; the coaxial double-layer dripper 4 is provided with an inner core delivery channel 5 and an outer wall delivery channel 6, the core material injection syringe 1 is connected to the inner core delivery channel 5 through the injection pump 3, the wall material injection syringe 2 is connected to the outer wall delivery channel 6 through the injection pump 3, and a structure containing a protective liquid 7 is provided below the coaxial double-layer dripper 4. The core liquid prepared in step 1) and the molten outer wall material glue in step 2) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump; wherein, the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the molten wall material glue flows out from the outer aperture of the coaxial double-layer needle at 120°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue liquid form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the molten wall material glue liquid. The droplets drip into the 25°C protective liquid (dimethyl silicone oil) under their own gravity to cool, forming popping beads with a certain hardness. After separation and washing by a sieve, the popping beads for cigarettes coated with water-soluble flavors can be obtained.

[0041] Among them: the flow rate of the outer wall material glue: the flow rate of the inner core liquid = 2.2:1.

[0042] The obtained tobacco explosive beads coated with water-soluble flavors have a weight of 60.7 mg, a diameter of 4.5 mm, a crushing strength of 15.2 N, and a water loss rate of <5.0% in 6 months.

[0043] Example 2

[0044] A tobacco popping bead coated with a water-soluble flavor, the tobacco popping bead is provided with a skin-core structure, the skin-core structure comprises an outer wall material and a core liquid; the outer wall material comprises 100 parts of beeswax and 100 parts of rosin resin; the core liquid comprises 100 parts of water, 5 parts of a water-soluble flavor (Zimbabwe extract), 4.75 parts of a preservative (Carbomer), and 0.25 parts of a thickener (Carbomer).

[0045] The preparation method of the above-mentioned tobacco popping beads coated with water-soluble flavor is as follows:

[0046] 1) Mix water, water-soluble flavor, preservative and thickener according to the formula to obtain core liquid.

[0047] 2) Evenly mix the beeswax and rosin resin according to the formula ratio, heat to 140° C. under stirring, and melt to obtain the outer wall material glue; then repeatedly evacuate the outer wall material glue to remove bubbles in the glue.

[0048] 3) If Figure 1 As shown, the core liquid prepared in step 1) and the molten outer wall material glue in step 2) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump; wherein, the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the molten wall material glue flows out from the outer aperture of the coaxial double-layer needle at 140°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the molten wall material glue. Under the action of their own gravity, the droplets are dripped into a protective liquid (dimethyl silicone oil) at 25°C to cool, forming bursting bead particles with a certain hardness. After separation and washing by a sieve, the tobacco bursting beads coated with water-soluble flavors can be obtained.

[0049] Among them: the flow rate of the outer wall material glue: the flow rate of the inner core liquid = 2:1.

[0050] The obtained tobacco explosive beads coated with water-soluble flavors have a weight of 80.4 mg, a diameter of 5.5 mm, a crushing strength of 20.4 N, and a water loss rate of <4.5% in 6 months.

[0051] Example 3

[0052] A tobacco popping bead coated with a water-soluble flavor, the tobacco popping bead is provided with a skin-core structure, the skin-core structure comprises an outer wall material and a core liquid; the outer wall material comprises 100 parts of beeswax and 120 parts of rosin resin; the core liquid comprises 100 parts of water, 20 parts of a water-soluble flavor (a mixture of fennel oil and patchouli oil), 4.75 parts of a preservative (carbomer), and 0.25 parts of a thickener (carbomer).

[0053] The preparation method of the above-mentioned tobacco popping beads coated with water-soluble flavor is as follows:

[0054] 1) Mix water, water-soluble flavor, preservative and thickener according to the formula to obtain core liquid.

[0055] 2) Evenly mix the beeswax and rosin resin according to the formula ratio, heat to 100° C. under stirring conditions, and melt to obtain the outer wall material glue; then repeatedly evacuate the outer wall material glue to remove bubbles in the glue.

[0056] 3) If Figure 1As shown, the core liquid prepared in step 1) and the molten outer wall material glue in step 2) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump; wherein, the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the molten wall material glue flows out from the outer aperture of the coaxial double-layer needle at 100°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the molten wall material glue. Under the action of their own gravity, the droplets are dripped into a protective liquid (dimethyl silicone oil) at 25°C to cool, forming bursting bead particles with a certain hardness. After separation and washing by a sieve, the tobacco bursting beads coated with water-soluble flavors can be obtained.

[0057] Among them: the flow rate of the outer wall material glue: the flow rate of the inner core liquid = 2:1.

[0058] The obtained tobacco explosive beads coated with water-soluble flavors have a weight of 70.5 mg, a diameter of 5.3 mm, a crushing strength of 22.3 N, and a water loss rate of <4.0% in 6 months.

[0059] Example 4

[0060] A tobacco popping bead coated with a water-soluble flavor, the tobacco popping bead is provided with a skin-core structure, the skin-core structure comprises an outer wall material and a core liquid; the outer wall material comprises 100 parts of carnauba wax and 80 parts of hydrogenated rosin resin; the core liquid comprises 100 parts of water, 100 parts of water-soluble flavor (tobacco extract), 2.5 parts of a preservative (kathon), and 2.5 parts of a defoaming agent (tributyl phosphate).

[0061] The preparation method of the above-mentioned tobacco popping beads coated with water-soluble flavor is as follows:

[0062] 1) Mix water, water-soluble flavor, preservative and defoamer according to the formula to obtain core liquid.

[0063] 2) The carnauba wax and hydrogenated rosin resin are uniformly mixed according to the formula ratio, heated to 80° C. under stirring conditions, and melted to obtain an outer wall material glue; then the outer wall material glue is repeatedly vacuumed to remove bubbles in the glue.

[0064] 3) If Figure 1As shown, the core liquid prepared in step 1) and the molten outer wall material glue in step 2) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump; wherein, the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the molten wall material glue flows out from the outer aperture of the coaxial double-layer needle at 80°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the molten wall material glue. Under the action of their own gravity, the droplets are dripped into a protective liquid (dimethyl silicone oil) at 25°C to cool, forming bursting bead particles with a certain hardness. After separation and washing by a sieve, the tobacco bursting beads coated with water-soluble flavors can be obtained.

[0065] Among them: the flow rate of the outer wall material glue: the flow rate of the inner core liquid = 1.8:1.

[0066] The obtained tobacco explosive beads coated with water-soluble flavors have a weight of 55.8 mg, a diameter of 4.3 mm, a crushing strength of 9.8 N, and a water loss rate of <4.7% in 6 months.

[0067] Example 5

[0068] A tobacco popping bead coated with a water-soluble flavor, the tobacco popping bead is provided with a skin-core structure, the skin-core structure comprises an outer wall material and a core liquid; the outer wall material comprises 100 parts of solid paraffin and 50 parts of glycerol rosin resin; the core liquid comprises 100 parts of water, 50 parts of a water-soluble flavor (a mixture of rosemary oil and ionone), 2.5 parts of a preservative (potassium sorbate), and 2.5 parts of a stabilizer (sorbitol).

[0069] The preparation method of the above-mentioned tobacco popping beads coated with water-soluble flavor is as follows:

[0070] 1) Mix water, water-soluble flavor, preservative and stabilizer according to the formula to obtain core liquid.

[0071] 2) Mix solid paraffin and glycerin rosin resin evenly according to the formula ratio, heat to 130° C. under stirring, and melt to obtain the outer wall material glue; then repeatedly evacuate the outer wall material glue to remove bubbles in the glue.

[0072] 3) If Figure 1As shown, the core liquid prepared in step 1) and the molten outer wall material glue in step 2) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump; wherein, the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the molten wall material glue flows out from the outer aperture of the coaxial double-layer needle at 130°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the molten wall material glue. Under the action of their own gravity, the droplets are dripped into a protective liquid (dimethyl silicone oil) at 25°C to cool, forming bursting bead particles with a certain hardness. After separation and washing by a sieve, the tobacco bursting beads coated with water-soluble flavors can be obtained.

[0073] Among them: the flow rate of the outer wall material glue: the flow rate of the inner core liquid = 1.6:1.

[0074] The obtained tobacco explosive beads coated with water-soluble flavors have a weight of 80.5 mg, a diameter of 6.3 mm, a crushing strength of 21.3 N, and a water loss rate of <5.5% in 6 months.

[0075] Example 6

[0076] A tobacco popping bead coated with a water-soluble flavor, the tobacco popping bead is provided with a skin-core structure, the skin-core structure comprises an outer wall material and a core liquid; the outer wall material comprises 100 parts of insect wax and 200 parts of rosin methyl ester; the core liquid comprises 100 parts of water, 20 parts of a water-soluble flavor (a mixture of tobacco extract and Zimbabwe tobacco extract), 1 part of a thickener (sodium alginate), and 4 parts of a stabilizer (sorbitol).

[0077] The preparation method of the above-mentioned tobacco popping beads coated with water-soluble flavor is as follows:

[0078] 1) Mix water, water-soluble flavor, thickener and stabilizer according to the formula to obtain core liquid.

[0079] 2) Evenly mix the insect wax and rosin methyl ester according to the formula ratio, heat to 110° C. under stirring, and melt to obtain the outer wall material glue; then repeatedly evacuate the outer wall material glue to remove bubbles in the glue.

[0080] 3) If Figure 1As shown, the core liquid prepared in step 1) and the molten outer wall material glue in step 2) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump; wherein, the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the molten wall material glue flows out from the outer aperture of the coaxial double-layer needle at 110°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the molten wall material glue. Under the action of its own gravity, the droplets are dripped into a protective liquid (dimethyl silicone oil) at 25°C to cool, forming bursting bead particles with a certain hardness. After separation and washing by a sieve, the tobacco bursting beads coated with water-soluble flavors can be obtained.

[0081] Among them: the flow rate of the outer wall material glue: the flow rate of the inner core liquid = 1.4:1.

[0082] The obtained tobacco explosive beads coated with water-soluble flavors have a weight of 61.2 mg, a diameter of 4.2 mm, a crushing strength of 9.2 N, and a water loss rate of <6.2% in 6 months.

[0083] Example 7

[0084] A tobacco popping bead coated with a water-soluble flavor, the tobacco popping bead is provided with a skin-core structure, the skin-core structure comprises an outer wall material and a core liquid; the outer wall material comprises 100 parts of carnauba wax and 200 parts of rosin vinyl alcohol ester; the core liquid comprises 100 parts of water, 40 parts of a water-soluble flavor (tobacco extract), 0.2 parts of a preservative (phenoxyethanol), and 0.3 parts of a defoaming agent (tributyl phosphate).

[0085] The preparation method of the above-mentioned tobacco popping beads coated with water-soluble flavor is as follows:

[0086] 1) Mix water, water-soluble flavor, preservative and defoamer according to the formula to obtain core liquid.

[0087] 2) Carnauba wax and rosin vinyl alcohol ester are uniformly mixed according to a formula ratio, heated to 90° C. under stirring conditions, and melted to obtain an outer wall material glue; then the outer wall material glue is repeatedly vacuumed to remove bubbles in the glue.

[0088] 3) If Figure 1As shown, the core liquid prepared in step 1) and the molten outer wall material glue in step 2) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump; wherein, the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the molten wall material glue flows out from the outer aperture of the coaxial double-layer needle at 90°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the molten wall material glue. Under the action of its own gravity, the droplets are dripped into a protective liquid (dimethyl silicone oil) at 25°C to cool, forming bursting bead particles with a certain hardness. After separation and washing by a sieve, the tobacco bursting beads coated with water-soluble flavors can be obtained.

[0089] Among them: the flow rate of the outer wall material glue: the flow rate of the inner core liquid = 1.2:1.

[0090] The obtained tobacco explosive beads coated with water-soluble flavor have a weight of 64.3 mg, a diameter of 3.8 mm, a crushing strength of 7.2 N, and a water loss rate of <6.5% in 6 months.

[0091] Example 8

[0092] A tobacco popping bead coated with a water-soluble flavor, the tobacco popping bead is provided with a skin-core structure, the skin-core structure comprises an outer wall material and a core liquid; the outer wall material comprises 100 parts of insect wax and 180 parts of rosin-modified phenolic resin; the core liquid comprises 100 parts of water, 15 parts of a water-soluble flavor (Zimbabwe tobacco extract), 0.4 parts of a stabilizer (sorbitol), and 0.1 parts of a defoaming agent (tributyl phosphate).

[0093] The preparation method of the above-mentioned tobacco popping beads coated with water-soluble flavor is as follows:

[0094] 1) Mix water, water-soluble flavor, stabilizer and defoamer according to the formula to obtain core liquid.

[0095] 2) The insect wax and rosin-modified phenolic resin are uniformly mixed according to the formula ratio, heated to 105° C. under stirring conditions, and melted to obtain an outer wall material glue solution; then the outer wall material glue solution is repeatedly vacuumed to remove bubbles in the glue solution.

[0096] 3) If Figure 1As shown, the core liquid prepared in step 1) and the molten outer wall material glue in step 2) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump; wherein, the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the molten wall material glue flows out from the outer aperture of the coaxial double-layer needle at 105°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the molten wall material glue. Under the action of their own gravity, the droplets are dripped into a protective liquid (dimethyl silicone oil) at 25°C to cool, forming bursting bead particles with a certain hardness. After separation and washing by a sieve, the tobacco bursting beads coated with water-soluble flavors can be obtained.

[0097] Among them: the flow rate of the outer wall material glue: the flow rate of the inner core liquid = 1.5:1.

[0098] The obtained tobacco explosive beads coated with water-soluble flavors have a weight of 70.2 mg, a diameter of 6.7 mm, a crushing strength of 18.4 N, and a water loss rate of <5.7% in 6 months.

[0099] Example 9

[0100] A tobacco popping bead coated with a water-soluble flavor, the tobacco popping bead is provided with a skin-core structure, the skin-core structure comprises an outer wall material and a core liquid; the outer wall material comprises 100 parts of beeswax and 160 parts of maleic anhydride rosin resin; the core liquid comprises 100 parts of water, 25 parts of a water-soluble flavor (a mixture of fennel oil and patchouli oil), 2.5 parts of a bactericide (phenoxyethanol), and 2.5 parts of a defoaming agent (tributyl phosphate).

[0101] The preparation method of the above-mentioned tobacco popping beads coated with water-soluble flavor is as follows:

[0102] 1) Mix water, water-soluble flavor, bactericide and defoamer according to the formula to obtain core liquid.

[0103] 2) beeswax and maleic anhydride rosin resin are uniformly mixed according to a formula ratio, heated to 115° C. under stirring conditions, and melted to obtain an outer wall material glue; then the outer wall material glue is repeatedly vacuumed to remove bubbles in the glue.

[0104] 3) If Figure 1As shown, the core liquid prepared in step 1) and the molten outer wall material glue in step 2) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump; wherein, the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the molten wall material glue flows out from the outer aperture of the coaxial double-layer needle at 115°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the molten wall material glue. Under the action of their own gravity, the droplets are dripped into a protective liquid (dimethyl silicone oil) at 25°C to cool, forming bursting bead particles with a certain hardness. After separation and washing by a sieve, the tobacco bursting beads coated with water-soluble flavors can be obtained.

[0105] Among them: the flow rate of the outer wall material glue: the flow rate of the inner core liquid = 1.7:1.

[0106] The obtained tobacco explosive beads coated with water-soluble flavors have a weight of 51.3 mg, a diameter of 3.6 mm, a crushing strength of 21.7 N, and a water loss rate of <5.5% in 6 months.

[0107] Comparative Example 1

[0108] A tobacco popping bead coated with a water-soluble flavor, the tobacco popping bead is provided with a skin-core structure, the skin-core structure comprises an outer wall material and a core liquid; the outer wall material comprises 100 parts of beeswax and 160 parts of rosin resin; the core liquid comprises 100 parts of water, 5 parts of a water-soluble flavor (Zimbabwe extract), 2.5 parts of a preservative (kathion), and 2.5 parts of a thickener (sodium alginate).

[0109] The preparation method of the above-mentioned tobacco popping beads coated with water-soluble flavor is as follows:

[0110] 1) Mix water, water-soluble flavor, preservative and thickener according to the formula to obtain core liquid.

[0111] 2) beeswax and rosin resin are mixed evenly according to a formula ratio, heated to 150° C. under stirring conditions, and melted to obtain an outer wall material glue liquid; then the outer wall material glue liquid is repeatedly vacuumed to remove bubbles in the glue liquid.

[0112] 3) If Figure 1As shown, the core liquid prepared in step 1) and the molten outer layer wall material glue in step 2) are respectively delivered into the dripping hole of the coaxial double-layer common needle through a metering pump; wherein, the core liquid flows out from the inner aperture of the coaxial double-layer needle, and the molten wall material glue flows out from the outer aperture of the coaxial double-layer needle. After the two solutions flow out from the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue form concentric spherical droplets, with the core liquid inside the droplets and the molten wall material glue on the outer layer. The droplets drip into the protective liquid under the action of their own gravity to cool, but no matter how the flow rate ratio between the wall material glue and the inner core liquid is adjusted, it is impossible to form explosive bead particles with a certain hardness and a concentric structure.

[0113] Comparative Example 2

[0114] A tobacco popping bead coated with a water-soluble flavor, the tobacco popping bead is provided with a skin-core structure, the skin-core structure comprises an outer wall material and a core liquid; the outer wall material comprises 100 parts of beeswax and 300 parts of rosin resin; the core liquid comprises 100 parts of water, 5 parts of a water-soluble flavor (Zimbabwe extract), 2.5 parts of a preservative (kathion), and 2.5 parts of a thickener (sodium alginate).

[0115] The preparation method of the above-mentioned tobacco popping beads coated with water-soluble flavor is as follows:

[0116] 1) Mix water, water-soluble flavor, preservative and thickener according to the formula to obtain core liquid.

[0117] 2) Evenly mix the beeswax and rosin resin according to the formula ratio, heat to 120° C. under stirring, and melt to obtain the outer wall material glue; then repeatedly evacuate the outer wall material glue to remove bubbles in the glue.

[0118] 3) If Figure 1 As shown, the core liquid prepared in step 1) and the molten outer wall material glue in step 2) are respectively fed into the dripping hole of the coaxial double-layer needle through a metering pump; wherein, the core liquid flows out from the inner aperture of the coaxial double-layer needle, and the molten wall material glue flows out from the outer aperture of the coaxial double-layer needle. The rosin resin content in the wall material glue is too high, which, on the one hand, leads to too high viscosity of the wall material glue, and the glue is extremely difficult to flow out from the outer aperture. On the other hand, the hardness of the beads formed after the glue is solidified is relatively high, and the crushing strength is 40N, which is extremely difficult to be crushed by hand.

[0119] Comparative Example 3

[0120] A tobacco popping bead coated with a water-soluble flavor, the tobacco popping bead is provided with a skin-core structure, the skin-core structure comprises an outer wall material and a core liquid; the outer wall material comprises 100 parts of beeswax and 160 parts of rosin resin; the core liquid comprises 100 parts of water, 5 parts of a water-soluble flavor (Zimbabwe extract), 2.5 parts of a preservative (kathion), and 2.5 parts of a thickener (sodium alginate).

[0121] The preparation method of the above-mentioned tobacco popping beads coated with water-soluble flavor is as follows:

[0122] 1) Mix water, water-soluble flavor, preservative and thickener according to the formula to obtain core liquid.

[0123] 2) Evenly mix the beeswax and rosin resin according to the formula ratio, heat to 120° C. under stirring, and melt to obtain the outer wall material glue; then repeatedly evacuate the outer wall material glue to remove bubbles in the glue.

[0124] 3) If Figure 1 As shown, the core liquid prepared in step 1) and the molten outer wall material glue in step 2) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump; wherein, the core liquid flows out from the inner aperture of the coaxial double-layer needle, and the molten wall material glue flows out from the outer aperture of the coaxial double-layer needle. The flow rate of the outer wall material glue: the flow rate of the inner core liquid = 3:1. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue cannot form concentric spherical droplets, or form spherical liquids with eccentric structures. The inside of the droplet is the core liquid, and the outer layer is the molten wall material glue.

[0125] More preferably, the embodiments and comparative examples of the water-soluble flavor bursting beads coated with inner and outer double-layer wall material structures are as follows:

[0126] Example 10

[0127] A water-soluble flavoring popping bead coated with inner and outer double-layer wall materials, the popping bead for tobacco comprises a double-layer skin-core structure, the double-layer skin-core structure comprises an outer wall material, an inner wall material and a core liquid; the outer wall material comprises 100 parts of beeswax and 160 parts of rosin resin; the inner wall material comprises 10 parts of sodium alginate, 20 parts of gelatin and 70 parts of water; the core liquid comprises 100 parts of water, 5 parts of water-soluble flavor (Zimbabwe extract), 2.5 parts of preservative (kathion) and 2.5 parts of thickener (sodium alginate).

[0128] The preparation method of the water-soluble essence bursting beads coated with the inner and outer double-layer wall materials is as follows:

[0129] 1) Mix water, water-soluble flavor, preservative and thickener according to the formula to obtain core liquid.

[0130] 2) Evenly mix the beeswax and rosin resin according to the formula ratio, heat to 120° C. under stirring, and melt to obtain the outer wall material glue; then repeatedly evacuate the outer wall material glue to remove bubbles in the glue.

[0131] 3) Evenly mix sodium alginate and gelatin according to the formula ratio, heat to 65° C. under stirring, and dissolve to obtain an inner wall material glue solution; then repeatedly evacuate the inner wall material glue solution to remove bubbles in the glue solution.

[0132] 4) If Figure 2 The schematic diagram of the preparation of the cigarette explosion beads with inner and outer double-layer wall materials covering the core liquid is shown in the figure. Figure 2 The dripping pill machine shown comprises a core material injection syringe 1, a wall material injection syringe 2, and a coaxial double-layer dripper 4; the coaxial double-layer dripper 4 is provided with an inner core delivery channel 5 and an outer wall delivery channel 6, the core material injection syringe 1 is connected to the inner core delivery channel 5 through an injection pump 3, and the wall material injection syringe 2 is connected to the outer wall delivery channel 6 through an injection pump 3, and a structure for containing a protective liquid 7 is provided below the coaxial double-layer dripper 4. Below the structure for containing the protective liquid 7 is a structure with a screen 8 as the upper layer and a molten outer layer glue 9 as the lower layer. The core liquid prepared in step 1) and the inner layer wall material glue in step 3) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump, wherein the core liquid flows out from the inner layer aperture of the coaxial double-layer needle at 25°C, and the inner layer wall material glue flows out from the outer layer aperture of the coaxial double-layer needle at 65°C. After the two solutions flow out from the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue liquid form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the wall material glue liquid. The droplets drip into the 25°C protective liquid (a 10% calcium chloride aqueous solution by mass) under the action of their own gravity to cool, forming bursting bead particles with a certain hardness. After separation and washing by a sieve, the inner layer structure of the tobacco bursting bead coated with water-soluble flavors can be obtained. Among them: the wall material glue liquid flow rate: the inner layer core liquid flow rate = 2.2:1.

[0133] 5) The inner layer structure of the tobacco popping beads obtained in step 4) is quickly immersed in the glue solution prepared in step 2), and taken out after staying for 2-5 seconds, and cooled at room temperature to obtain tobacco popping beads with inner and outer double-layer wall materials coated with water-soluble flavors.

[0134] The obtained tobacco explosive beads with inner and outer double-layer wall materials coated with water-soluble flavors have a weight of 60.3 mg, a diameter of 4.5 mm, a crushing strength of 15.2 N, and a water loss rate of <4.2% in 6 months.

[0135] Embodiment 11

[0136] A water-soluble flavoring popping bead coated with inner and outer double-layer wall materials, the popping bead for tobacco comprises a double-layer skin-core structure, the double-layer skin-core structure comprises an outer wall material, an inner wall material and a core liquid; the outer wall material comprises 100 parts of beeswax and 100 parts of rosin resin; the inner wall material comprises 10 parts of sodium alginate, 20 parts of carrageenan and 70 parts of water; the core liquid comprises 100 parts of water, 5 parts of water-soluble flavor (Zimbabwe extract), 4.75 parts of preservative (carbomer) and 0.25 parts of thickener (carbomer).

[0137] The preparation method of the water-soluble essence bursting beads coated with the inner and outer double-layer wall materials is as follows:

[0138] 1) Mix water, water-soluble flavor, preservative and thickener according to the formula to obtain core liquid.

[0139] 2) Evenly mix the beeswax and rosin resin according to the formula ratio, heat to 140° C. under stirring, and melt to obtain the outer wall material glue; then repeatedly evacuate the outer wall material glue to remove bubbles in the glue.

[0140] 3) Evenly mix sodium alginate and carrageenan according to the formula ratio, heat to 70° C. under stirring conditions, and dissolve to obtain an inner wall material glue solution; then repeatedly evacuate the inner wall material glue solution to remove bubbles in the glue solution.

[0141] 4) If Figure 2 As shown, the core liquid prepared in step 1) and the inner wall material glue liquid prepared in step 3) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump, wherein the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the inner wall material glue liquid flows out from the outer aperture of the coaxial double-layer needle at 70°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue liquid form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the wall material glue liquid. Under the action of its own gravity, the droplets are dripped into a 25°C protective liquid (a calcium chloride aqueous solution with a mass fraction of 15%) to cool, forming bursting bead particles with a certain hardness. After separation and washing by a screen, the inner layer structure of the tobacco bursting bead coated with a water-soluble flavor can be obtained. Among them: the wall material glue liquid flow rate: the inner layer core liquid flow rate = 2:1.

[0142] 5) The inner layer structure of the tobacco popping beads obtained in step 4) is quickly immersed in the glue solution prepared in step 2), and taken out after staying for 2-5 seconds, and cooled at room temperature to obtain tobacco popping beads with inner and outer double-layer wall materials coated with water-soluble flavors.

[0143] The obtained tobacco explosive beads with inner and outer double-layer wall materials coated with water-soluble flavors have a weight of 50.9 mg, a diameter of 3.7 mm, a crushing strength of 10.7 N, and a water loss rate of <3.7% in 6 months.

[0144] Example 12

[0145] A water-soluble flavoring popping bead coated with inner and outer double-layer wall materials, the popping bead for tobacco comprising a double-layer skin-core structure, the double-layer skin-core structure comprising an outer wall material, an inner wall material and a core liquid; the outer wall material comprises 100 parts of beeswax and 120 parts of rosin resin; the inner wall material comprises 10 parts of gelatin, 10 parts of carrageenan and 80 parts of water; the core liquid comprises 100 parts of water, 20 parts of water-soluble flavoring (a mixture of fennel oil and patchouli oil), 4.75 parts of a preservative (carbomer) and 0.25 parts of a thickener (carbomer).

[0146] The preparation method of the water-soluble essence bursting beads coated with the inner and outer double-layer wall materials is as follows:

[0147] 1) Mix water, water-soluble flavor, preservative and thickener according to the formula to obtain core liquid.

[0148] 2) Evenly mix the beeswax and rosin resin according to the formula ratio, heat to 100° C. under stirring conditions, and melt to obtain the outer wall material glue; then repeatedly evacuate the outer wall material glue to remove bubbles in the glue.

[0149] 3) The gelatin and carrageenan are uniformly mixed according to the formula ratio, heated to 70° C. under stirring conditions, and dissolved to obtain an inner wall material glue solution; then the inner wall material glue solution is repeatedly vacuumed to remove bubbles in the glue solution.

[0150] 4) If Figure 2 As shown, the core liquid prepared in step 1) and the inner wall material glue liquid prepared in step 3) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump, wherein the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the inner wall material glue liquid flows out from the outer aperture of the coaxial double-layer needle at 70°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue liquid form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the wall material glue liquid. Under the action of its own gravity, the droplets are dripped into a 25°C protective liquid (a calcium chloride aqueous solution with a mass fraction of 30%) to cool, forming bursting bead particles with a certain hardness. After separation and washing by a screen, the inner layer structure of the tobacco bursting bead coated with a water-soluble flavor can be obtained. Among them: the wall material glue liquid flow rate: the inner layer core liquid flow rate = 2:1.

[0151] 5) The inner layer structure of the tobacco popping beads obtained in step 4) is quickly immersed in the glue solution prepared in step 2), and taken out after staying for 2-5 seconds, and cooled at room temperature to obtain tobacco popping beads with inner and outer double-layer wall materials coated with water-soluble flavors.

[0152] The obtained tobacco explosive beads with inner and outer double-layer wall materials coated with water-soluble flavors have a weight of 70.3 mg, a diameter of 3.8 mm, a crushing strength of 13.6 N, and a water loss rate of <4.5% in 6 months.

[0153] Embodiment 13

[0154] A water-soluble flavoring popping bead coated with inner and outer double-layer wall materials, the popping bead for tobacco comprises a double-layer skin-core structure, the double-layer skin-core structure comprises an outer wall material, an inner wall material and a core liquid; the outer wall material comprises 100 parts of carnauba wax and 80 parts of hydrogenated rosin resin; the inner wall material comprises 20 parts of gelatin and 80 parts of water; the core liquid comprises 100 parts of water, 100 parts of water-soluble flavor (tobacco extract), 2.5 parts of preservative (kathion), and 2.5 parts of defoaming agent (tributyl phosphate).

[0155] The preparation method of the water-soluble essence bursting beads coated with the inner and outer double-layer wall materials is as follows:

[0156] 1) Mix water, water-soluble flavor, preservative and defoamer according to the formula to obtain core liquid.

[0157] 2) The carnauba wax and hydrogenated rosin resin are uniformly mixed according to the formula ratio, heated to 80° C. under stirring conditions, and melted to obtain an outer wall material glue; then the outer wall material glue is repeatedly vacuumed to remove bubbles in the glue.

[0158] 3) Evenly mix sodium alginate and carrageenan according to the formula ratio, heat to 70° C. under stirring conditions, and dissolve to obtain an inner wall material glue solution; then repeatedly evacuate the inner wall material glue solution to remove bubbles in the glue solution.

[0159] 4) If Figure 2 As shown, the core liquid prepared in step 1) and the inner wall material glue liquid prepared in step 3) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump, wherein the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the inner wall material glue liquid flows out from the outer aperture of the coaxial double-layer needle at 70°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue liquid form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the wall material glue liquid. Under the action of its own gravity, the droplets are dripped into a 25°C protective liquid (a calcium chloride aqueous solution with a mass fraction of 15%) to cool, forming bursting bead particles with a certain hardness. After separation and washing by a screen, the inner layer structure of the tobacco bursting bead coated with a water-soluble flavor can be obtained. Among them: the wall material glue liquid flow rate: the inner layer core liquid flow rate = 1.8:1.

[0160] 5) The inner layer structure of the tobacco popping beads obtained in step 4) is quickly immersed in the glue solution prepared in step 2), and taken out after staying for 2-5 seconds, and cooled at room temperature to obtain tobacco popping beads with inner and outer double-layer wall materials coated with water-soluble flavors.

[0161] The obtained tobacco explosive beads with inner and outer double-layer wall materials coated with water-soluble flavors have a weight of 60.3 mg, a diameter of 4.3 mm, a crushing strength of 15.4 N, and a water loss rate of <4.5% in 6 months.

[0162] Embodiment 14

[0163] A water-soluble flavoring popping bead coated with inner and outer double-layer wall materials, the popping bead for tobacco comprising a double-layer skin-core structure, the double-layer skin-core structure comprising an outer wall material, an inner wall material and a core liquid; the outer wall material comprises 100 parts of solid paraffin and 50 parts of glycerol rosin resin; the inner wall material comprises 20 parts of sodium alginate and 80 parts of water; the core liquid comprises 100 parts of water, 50 parts of water-soluble flavoring (a mixture of rosemary oil and ionone), 2.5 parts of a preservative (potassium sorbate) and 2.5 parts of a stabilizer (sorbitol).

[0164] The preparation method of the water-soluble essence bursting beads coated with the inner and outer double-layer wall materials is as follows:

[0165] 1) Mix water, water-soluble flavor, preservative and stabilizer according to the formula to obtain core liquid.

[0166] 2) Mix solid paraffin and glycerin rosin resin evenly according to the formula ratio, heat to 130° C. under stirring, and melt to obtain the outer wall material glue; then repeatedly evacuate the outer wall material glue to remove bubbles in the glue.

[0167] 3) Evenly mix sodium alginate and carrageenan according to the formula ratio, heat to 70° C. under stirring conditions, and dissolve to obtain an inner wall material glue solution; then repeatedly evacuate the inner wall material glue solution to remove bubbles in the glue solution.

[0168] 4) If Figure 2 As shown, the core liquid prepared in step 1) and the inner wall material glue liquid prepared in step 3) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump, wherein the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the inner wall material glue liquid flows out from the outer aperture of the coaxial double-layer needle at 70°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue liquid form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the wall material glue liquid. Under the action of its own gravity, the droplets are dripped into a 25°C protective liquid (a calcium chloride aqueous solution with a mass fraction of 20%) to cool, forming bursting bead particles with a certain hardness. After separation and washing by a screen, the inner layer structure of the tobacco bursting bead coated with a water-soluble flavor can be obtained. Among them: the wall material glue liquid flow rate: the inner layer core liquid flow rate = 1.6:1.

[0169] 5) The inner layer structure of the tobacco popping beads obtained in step 4) is quickly immersed in the glue solution prepared in step 2), and taken out after staying for 2-5 seconds, and cooled at room temperature to obtain tobacco popping beads with inner and outer double-layer wall materials coated with water-soluble flavors.

[0170] The obtained tobacco explosive beads with inner and outer double-layer wall materials coated with water-soluble flavors have a weight of 70.5 mg, a diameter of 4.3 mm, a crushing strength of 13.2 N, and a water loss rate of <4.2% in 6 months.

[0171] Embodiment 15

[0172] A water-soluble flavor popping bead coated with inner and outer double-layer wall materials, the popping bead for tobacco comprising a double-layer skin-core structure, the double-layer skin-core structure comprising an outer wall material, an inner wall material and a core liquid; the outer wall material comprises 100 parts of insect wax and 200 parts of rosin methyl ester; the inner wall material comprises 10 parts of carrageenan and 90 parts of water; the core liquid comprises 100 parts of water, 20 parts of water-soluble flavor (a mixture of tobacco extract and Zimbabwe tobacco extract), 1 part of thickener (sodium alginate) and 4 parts of stabilizer (sorbitol).

[0173] The preparation method of the water-soluble essence bursting beads coated with the inner and outer double-layer wall materials is as follows:

[0174] 1) Mix water, water-soluble flavor, thickener and stabilizer according to the formula to obtain core liquid.

[0175] 2) Evenly mix the insect wax and rosin methyl ester according to the formula ratio, heat to 110° C. under stirring, and melt to obtain the outer wall material glue; then repeatedly evacuate the outer wall material glue to remove bubbles in the glue.

[0176] 3) Evenly mix sodium alginate and carrageenan according to the formula ratio, heat to 70° C. under stirring conditions, and dissolve to obtain an inner wall material glue solution; then repeatedly evacuate the inner wall material glue solution to remove bubbles in the glue solution.

[0177] 4) If Figure 2 As shown, the core liquid prepared in step 1) and the inner wall material glue liquid prepared in step 3) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump, wherein the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the inner wall material glue liquid flows out from the outer aperture of the coaxial double-layer needle at 70°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue liquid form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the wall material glue liquid. Under the action of its own gravity, the droplets are dripped into a 25°C protective liquid (a calcium chloride aqueous solution with a mass fraction of 20%) to cool, forming bursting bead particles with a certain hardness. After separation and washing by a screen, the inner layer structure of the tobacco bursting bead coated with a water-soluble flavor can be obtained. Among them: the wall material glue liquid flow rate: the inner layer core liquid flow rate = 1.4:1.

[0178] 5) The inner layer structure of the tobacco popping beads obtained in step 4) is quickly immersed in the glue solution prepared in step 2), and taken out after staying for 2-5 seconds, and cooled at room temperature to obtain tobacco popping beads with inner and outer double-layer wall materials coated with water-soluble flavors.

[0179] The obtained tobacco explosive beads with inner and outer double-layer wall materials coated with water-soluble flavors have a weight of 55.4 mg, a diameter of 4.3 mm, a crushing strength of 12.8 N, and a water loss rate of <4.5% in 6 months.

[0180] Example 16

[0181] A water-soluble flavoring popping bead coated with inner and outer double-layer wall materials, the popping bead for tobacco comprising a double-layer skin-core structure, the double-layer skin-core structure comprising an outer wall material, an inner wall material and a core liquid; the outer wall material comprises 100 parts of carnauba wax and 200 parts of rosin vinyl alcohol ester; the inner wall material comprises 15 parts of gelatin, 5 parts of carrageenan and 80 parts of water; the core liquid comprises 100 parts of water, 40 parts of water-soluble flavor (tobacco extract), 0.2 parts of preservative (phenoxyethanol) and 0.3 parts of defoaming agent (tributyl phosphate).

[0182] The preparation method of the water-soluble essence bursting beads coated with the inner and outer double-layer wall materials is as follows:

[0183] 1) Mix water, water-soluble flavor, preservative and defoamer according to the formula to obtain core liquid.

[0184] 2) Carnauba wax and rosin vinyl alcohol ester are uniformly mixed according to a formula ratio, heated to 90° C. under stirring conditions, and melted to obtain an outer wall material glue; then the outer wall material glue is repeatedly vacuumed to remove bubbles in the glue.

[0185] 3) Evenly mix sodium alginate and carrageenan according to the formula ratio, heat to 75° C. under stirring conditions, and dissolve to obtain an inner wall material glue solution; then repeatedly evacuate the inner wall material glue solution to remove bubbles in the glue solution.

[0186] 4) If Figure 2 As shown, the core liquid prepared in step 1) and the inner wall material glue liquid prepared in step 3) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump, wherein the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the inner wall material glue liquid flows out from the outer aperture of the coaxial double-layer needle at 75°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue liquid form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the wall material glue liquid. Under the action of its own gravity, the droplets are dripped into a 25°C protective liquid (a calcium chloride aqueous solution with a mass fraction of 10%) to cool, forming bursting bead particles with a certain hardness. After separation and washing by a screen, the inner layer structure of the tobacco bursting bead coated with a water-soluble flavor can be obtained. Among them: the wall material glue liquid flow rate: the inner layer core liquid flow rate = 1.2:1.

[0187] 5) The inner layer structure of the tobacco popping beads obtained in step 4) is quickly immersed in the glue solution prepared in step 2), and taken out after staying for 2-5 seconds, and cooled at room temperature to obtain tobacco popping beads with inner and outer double-layer wall materials coated with water-soluble flavors.

[0188] The obtained tobacco explosive beads with inner and outer double-layer wall materials coated with water-soluble flavors have a weight of 90.2 mg, a diameter of 6.2 mm, a crushing strength of 15.8 N, and a water loss rate of <4.5% in 6 months.

[0189] Embodiment 17

[0190] A water-soluble flavoring popping bead coated with inner and outer double-layer wall materials, the popping bead for tobacco comprising a double-layer skin-core structure, the double-layer skin-core structure comprising an outer wall material, an inner wall material and a core liquid; the outer wall material comprises 100 parts of insect wax and 180 parts of rosin-modified phenolic resin; the inner wall material comprises 15 parts of gelatin and 85 parts of water; the core liquid comprises 100 parts of water, 15 parts of water-soluble flavor (Zimbabwe tobacco extract), 0.4 parts of a stabilizer (sorbitol) and 0.1 parts of a defoaming agent (tributyl phosphate).

[0191] The preparation method of the water-soluble essence bursting beads coated with the inner and outer double-layer wall materials is as follows:

[0192] 1) Mix water, water-soluble flavor, stabilizer and defoamer according to the formula to obtain core liquid.

[0193] 2) The insect wax and rosin-modified phenolic resin are uniformly mixed according to the formula ratio, heated to 105° C. under stirring conditions, and melted to obtain an outer wall material glue solution; then the outer wall material glue solution is repeatedly vacuumed to remove bubbles in the glue solution.

[0194] 3) Evenly mix sodium alginate and carrageenan according to the formula ratio, heat to 75° C. under stirring conditions, and dissolve to obtain an inner wall material glue solution; then repeatedly evacuate the inner wall material glue solution to remove bubbles in the glue solution.

[0195] 4) If Figure 2 As shown, the core liquid prepared in step 1) and the inner wall material glue liquid prepared in step 3) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump, wherein the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the inner wall material glue liquid flows out from the outer aperture of the coaxial double-layer needle at 75°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue liquid form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the wall material glue liquid. Under the action of its own gravity, the droplets are dripped into a 25°C protective liquid (a 5% calcium chloride aqueous solution) to cool, forming bursting bead particles with a certain hardness. After separation and washing by a screen, the inner layer structure of the tobacco bursting bead coated with a water-soluble flavor can be obtained. Among them: the wall material glue liquid flow rate: the inner layer core liquid flow rate = 1.5:1.

[0196] 5) The inner layer structure of the tobacco popping beads obtained in step 4) is quickly immersed in the glue solution prepared in step 2), and taken out after staying for 2-5 seconds, and cooled at room temperature to obtain tobacco popping beads with inner and outer double-layer wall materials coated with water-soluble flavors.

[0197] The obtained tobacco explosive beads with inner and outer double-layer wall materials coated with water-soluble flavors have a weight of 60.2 mg, a diameter of 3.9 mm, a crushing strength of 10.6 N, and a water loss rate of <4.0% in 6 months.

[0198] Embodiment 18

[0199] A water-soluble flavoring popping bead coated with inner and outer double-layer wall materials, the popping bead for tobacco comprises a double-layer skin-core structure, the double-layer skin-core structure comprises an outer wall material, an inner wall material and a core liquid; the outer wall material comprises 100 parts of beeswax and 160 parts of maleic anhydride rosin resin; the inner wall material comprises 20 parts of gelatin, 5 parts of sodium alginate and 75 parts of water; the core liquid comprises 100 parts of water, 25 parts of water-soluble flavoring (a mixture of fennel oil and patchouli oil), 2.5 parts of a bactericide (phenoxyethanol) and 2.5 parts of a defoaming agent (tributyl phosphate).

[0200] The preparation method of the water-soluble essence bursting beads coated with the inner and outer double-layer wall materials is as follows:

[0201] 1) Mix water, water-soluble flavor, bactericide and defoamer according to the formula to obtain core liquid.

[0202] 2) beeswax and maleic anhydride rosin resin are uniformly mixed according to a formula ratio, heated to 115° C. under stirring conditions, and melted to obtain an outer wall material glue; then the outer wall material glue is repeatedly vacuumed to remove bubbles in the glue.

[0203] 3) Evenly mix sodium alginate and carrageenan according to the formula ratio, heat to 75° C. under stirring conditions, and dissolve to obtain an inner wall material glue solution; then repeatedly evacuate the inner wall material glue solution to remove bubbles in the glue solution.

[0204] 4) If Figure 2 As shown, the core liquid prepared in step 1) and the inner wall material glue liquid prepared in step 3) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump, wherein the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the inner wall material glue liquid flows out from the outer aperture of the coaxial double-layer needle at 75°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue liquid form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the wall material glue liquid. Under the action of its own gravity, the droplets are dripped into a 25°C protective liquid (a calcium chloride aqueous solution with a mass fraction of 10%) to cool, forming bursting bead particles with a certain hardness. After separation and washing by a screen, the inner layer structure of the tobacco bursting bead coated with a water-soluble flavor can be obtained. Among them: the wall material glue liquid flow rate: the inner layer core liquid flow rate = 1.7:1.

[0205] 5) The inner layer structure of the tobacco popping beads obtained in step 4) is quickly immersed in the glue solution prepared in step 2), and taken out after staying for 2-5 seconds, and cooled at room temperature to obtain tobacco popping beads with inner and outer double-layer wall materials coated with water-soluble flavors.

[0206] The obtained tobacco explosive beads with inner and outer double-layer wall materials coated with water-soluble flavors have a weight of 70.3 mg, a diameter of 3.8 mm, a crushing strength of 12.9 N, and a water loss rate of <4.0% in 6 months.

[0207] Comparative Example 4

[0208] A water-soluble flavoring popping bead coated with inner and outer double-layer wall materials, the popping bead for tobacco comprises a double-layer skin-core structure, the double-layer skin-core structure comprises an outer wall material, an inner wall material and a core liquid; the outer wall material comprises 100 parts of beeswax and 160 parts of rosin resin; the inner wall material comprises 20 parts of gelatin, 5 parts of sodium alginate and 75 parts of water; the core liquid comprises 100 parts of water, 5 parts of water-soluble flavoring (Zimbabwe extract), 2.5 parts of preservative (kathion) and 2.5 parts of thickener (sodium alginate).

[0209] The preparation method of the water-soluble essence bursting beads coated with the inner and outer double-layer wall materials is as follows:

[0210] 1) Mix water, water-soluble flavor, preservative and thickener according to the formula to obtain core liquid.

[0211] 2) beeswax and rosin resin are mixed evenly according to a formula ratio, heated to 150° C. under stirring conditions, and melted to obtain an outer wall material glue liquid; then the outer wall material glue liquid is repeatedly vacuumed to remove bubbles in the glue liquid.

[0212] 3) Evenly mix sodium alginate and carrageenan according to the formula ratio, heat to 75° C. under stirring conditions, and dissolve to obtain an inner wall material glue solution; then repeatedly evacuate the inner wall material glue solution to remove bubbles in the glue solution.

[0213] 4) If Figure 2 As shown, the core liquid prepared in step 1) and the inner wall material glue liquid prepared in step 3) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump, wherein the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the inner wall material glue liquid flows out from the outer aperture of the coaxial double-layer needle at 75°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue liquid form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the wall material glue liquid. Under the action of its own gravity, the droplets are dripped into a 25°C protective liquid (a calcium chloride aqueous solution with a mass fraction of 10%) to cool, forming bursting bead particles with a certain hardness. After separation and washing by a screen, the inner layer structure of the tobacco bursting bead coated with a water-soluble flavor can be obtained. Among them: the wall material glue liquid flow rate: the inner layer core liquid flow rate = 1.7:1.

[0214] 5) The inner layer structure of the tobacco popping beads obtained in step 4) is quickly immersed in the glue solution prepared in step 2). No matter how long the inner layer structure of the tobacco popping beads stays in the outer layer glue solution, after being taken out and cooled at room temperature, popping beads particles with a certain hardness and a concentric structure cannot be obtained.

[0215] Comparative Example 5

[0216] A water-soluble flavoring popping bead coated with inner and outer double-layer wall materials, the popping bead for tobacco comprises a double-layer skin-core structure, the double-layer skin-core structure comprises an outer wall material, an inner wall material and a core liquid; the outer wall material comprises 100 parts of beeswax and 300 parts of rosin resin; the inner wall material comprises 15 parts of gelatin and 85 parts of water; the core liquid comprises 100 parts of water, 5 parts of water-soluble flavor (Zimbabwe extract), 2.5 parts of preservative (kathion) and 2.5 parts of thickener (sodium alginate).

[0217] The preparation method of the water-soluble essence bursting beads coated with the inner and outer double-layer wall materials is as follows:

[0218] 1) Mix water, water-soluble flavor, preservative and thickener according to the formula to obtain core liquid.

[0219] 2) Evenly mix the beeswax and rosin resin according to the formula ratio, heat to 120° C. under stirring, and melt to obtain the outer wall material glue; then repeatedly evacuate the outer wall material glue to remove bubbles in the glue.

[0220] 3) Evenly mix sodium alginate and carrageenan according to the formula ratio, heat to 75° C. under stirring conditions, and dissolve to obtain an inner wall material glue solution; then repeatedly evacuate the inner wall material glue solution to remove bubbles in the glue solution.

[0221] 4) If Figure 2 As shown, the core liquid prepared in step 1) and the inner wall material glue liquid prepared in step 3) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump, wherein the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the inner wall material glue liquid flows out from the outer aperture of the coaxial double-layer needle at 75°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue liquid form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the wall material glue liquid. Under the action of its own gravity, the droplets are dripped into a 25°C protective liquid (a 5% calcium chloride aqueous solution) to cool, forming bursting bead particles with a certain hardness. After separation and washing by a screen, the inner layer structure of the tobacco bursting bead coated with a water-soluble flavor can be obtained. Among them: the wall material glue liquid flow rate: the inner layer core liquid flow rate = 1.5:1.

[0222] 5) The inner layer structure of the tobacco popping beads obtained in step 4) is quickly immersed in the glue prepared in step 2), and after staying for 2-5 seconds, it is taken out and cooled at room temperature to obtain the tobacco popping beads with inner and outer double-layer wall materials coated with water-soluble flavors. Due to the high content of rosin resin in the wall material glue, on the one hand, the viscosity of the wall material glue is too high, and on the other hand, the hardness of the popping beads formed after the glue is solidified is relatively high, and the crushing strength is 45N, which is extremely difficult to be broken by hand.

[0223] Comparative Example 6

[0224] A water-soluble flavoring popping bead coated with inner and outer double-layer wall materials, the popping bead for tobacco comprises a double-layer skin-core structure, the double-layer skin-core structure comprises an outer wall material, an inner wall material and a core liquid; the outer wall material comprises 100 parts of beeswax and 40 parts of rosin resin; the inner wall material comprises 20 parts of sodium alginate and 80 parts of water; the core liquid comprises 100 parts of water, 5 parts of water-soluble flavor (Zimbabwe extract), 2.5 parts of preservative (kathion) and 2.5 parts of thickener (sodium alginate).

[0225] The preparation method of the water-soluble essence bursting beads coated with the inner and outer double-layer wall materials is as follows:

[0226] 1) Mix water, water-soluble flavor, preservative and thickener according to the formula to obtain core liquid.

[0227] 2) Evenly mix the beeswax and rosin resin according to the formula ratio, heat to 120° C. under stirring, and melt to obtain the outer wall material glue; then repeatedly evacuate the outer wall material glue to remove bubbles in the glue.

[0228] 3) Evenly mix sodium alginate and carrageenan according to the formula ratio, heat to 70° C. under stirring conditions, and dissolve to obtain an inner wall material glue solution; then repeatedly evacuate the inner wall material glue solution to remove bubbles in the glue solution.

[0229] 4) If Figure 2 As shown, the core liquid prepared in step 1) and the inner wall material glue liquid prepared in step 3) are respectively fed into the dripping hole of the coaxial double-layer common needle through a metering pump, wherein the core liquid flows out from the inner aperture of the coaxial double-layer needle at 25°C, and the inner wall material glue liquid flows out from the outer aperture of the coaxial double-layer needle at 70°C. After the two solutions flow out of the needle, under the action of surface tension, the dripping core liquid droplets and the dripping wall material glue liquid form concentric spherical droplets, the inside of the droplets is the core liquid, and the outer layer is the wall material glue liquid. Under the action of its own gravity, the droplets are dripped into a 25°C protective liquid (a calcium chloride aqueous solution with a mass fraction of 20%) to cool, forming bursting bead particles with a certain hardness. After separation and washing by a screen, the inner layer structure of the tobacco bursting bead coated with a water-soluble flavor can be obtained. Among them: the wall material glue liquid flow rate: the inner layer core liquid flow rate = 1.6:1.

[0230] 5) The inner layer structure of the tobacco popping beads obtained in step 4) is quickly immersed in the glue solution prepared in step 2), and taken out after staying for 2-5 seconds, and cooled at room temperature to obtain tobacco popping beads with inner and outer double-layer wall materials coated with water-soluble flavors, but the obtained popping beads are not brittle.

[0231] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit the scope of protection of the present invention. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the essence and scope of the technical solution of the present invention.

Claims

1. A tobacco popping bead coated with a water-soluble flavor, characterized in that: The tobacco explosive beads are provided with a skin-core structure, and the skin-core structure comprises an outer wall material and a core liquid; the outer wall material comprises wax and a tricyclic diterpenoid compound, and the weight ratio of the wax to the tricyclic diterpenoid compound is 1:(0.5-2); the tricyclic diterpenoid compound is rosin resin; by weight, the outer wall material is 55-80 parts, and the core liquid is 20-45 parts; The method for preparing the tobacco explosive beads coated with water-soluble flavor comprises the following steps: (1) taking a water-soluble flavor and an additive and mixing them evenly to obtain a core liquid; the weight ratio of the water-soluble flavor to the core liquid is 1:(2.5-22); the weight ratio of the additive to the core liquid is 1:(5-22); (2) mixing the wax and the tricyclic diterpenoid compound in the weight ratio, stirring, heating and melting to obtain an outer wall material glue; the heating and melting temperature of the outer wall material glue is 100° C.-140° C.; (3) The core liquid obtained in step (1) and the outer layer wall material glue obtained in step (2) are respectively fed into the dripping holes, and the core liquid droplets and the outer layer wall material glue are made into concentric spherical droplets, which are dripped into the protective liquid for cooling, separation and washing to obtain; when the core liquid droplets are fed into the dripping holes, the flow rate of the outer layer wall material glue: the flow rate of the core liquid droplets = (2 to 2.2):

1.

2. The tobacco-use explosive beads coated with water-soluble flavor according to claim 1, characterized in that: An inner wall material is provided between the outer wall material and the core liquid, and the inner wall material is a polysaccharide material; the polysaccharide material is at least one of sodium alginate, gelatin and carrageenan.

3. The tobacco explosive beads coated with water-soluble flavor according to claim 2, characterized in that: In terms of weight, the inner wall material accounts for 55-80 parts, and the core liquid accounts for 20-45 parts.

4. The tobacco explosive beads coated with water-soluble flavor according to any one of claims 1 to 3, characterized in that: The wax is at least one of beeswax, carnauba wax, solid paraffin, and insect wax; the core liquid includes water-soluble flavors and additives, and the weight ratio of the water-soluble flavors and additives is 1:(0.5-1); the water-soluble flavor is at least one of blended flavors and natural plant extracts; the additive is at least one of a stabilizer, a preservative, a defoamer, a thickener, and a bactericide.

5. The tobacco explosive beads coated with water-soluble flavor according to any one of claims 1 to 3, characterized in that: The weight of the explosive beads is 50-100 mg, the diameter is 3-7 mm, and the crushing strength is 5-30N.

6. The method for preparing the tobacco explosive beads coated with water-soluble flavors according to claim 1, characterized in that: The following steps are involved: (1) taking a water-soluble flavor and an additive and mixing them evenly to obtain a core liquid; the weight ratio of the water-soluble flavor to the core liquid is 1:(2.5-22); the weight ratio of the additive to the core liquid is 1:(5-22); (2) mixing the wax and the tricyclic diterpenoid compound in the weight ratio, stirring, heating and melting to obtain an outer wall material glue; the heating and melting temperature of the outer wall material glue is 100° C.-140° C.; (3) The core liquid obtained in step (1) and the outer layer wall material glue obtained in step (2) are respectively fed into the dripping holes, and the core liquid droplets and the outer layer wall material glue are made into concentric spherical droplets, which are dripped into the protective liquid for cooling, separation and washing to obtain; when the core liquid droplets are fed into the dripping holes, the flow rate of the outer layer wall material glue: the flow rate of the core liquid droplets = (2 to 2.2):

1.

7. The method for preparing the tobacco explosive beads coated with water-soluble flavor according to claim 6, characterized in that: In the step (3), the temperature of the outer wall material glue is 80°C-140°C, the temperature at the drip hole is 80°C-110°C, and the temperature of the core liquid is 25°C-60°C; the protective liquid is dimethyl silicone oil, and the cooling temperature is 10°C-40°C.

8. The method for preparing the tobacco explosive beads coated with water-soluble flavors according to claim 2 or 3, characterized in that: The following steps are involved: (1) taking a water-soluble flavor and an additive and mixing them evenly to obtain a core liquid; the weight ratio of the water-soluble flavor to the core liquid is 1:(2.5-22); the weight ratio of the additive to the core liquid is 1:(5-22); (2) mixing the wax and the tricyclic diterpenoid compound in the above weight ratio, stirring, heating and melting to obtain an outer wall material glue; (3) dissolving the polysaccharide material in water under heating and stirring conditions to obtain an inner wall material glue solution; the mass percentage of the polysaccharide material in the inner wall material glue solution is 10% to 30%; (4) feeding the core liquid obtained in step (1) and the inner wall material glue obtained in step (3) into the dripping holes respectively, and the core liquid droplets and the inner wall material glue droplets dripped out are made into concentric spherical droplets, dripped into the protective liquid for cooling, separated and washed, so as to obtain the inner layer structure of the popping bead for cigarettes; (5) immersing the inner layer structure of the tobacco explosive beads obtained in step (4) in the outer layer wall material glue obtained in step (2) and cooling the mixture to obtain the product.

9. The method for preparing the tobacco popping beads coated with water-soluble flavor according to claim 8, characterized in that: In the step (2), the heating melting temperature of the outer wall material glue is 80°C-140°C; In the step (3), the heating temperature of the inner wall material glue is 65°C-80°C; In the step (4), when the glue is fed into the drip hole, the flow rate of the inner wall material glue: the flow rate of the core liquid = (1.2-2.5): 1; the temperature of the inner wall material glue is 65°C-80°C, the temperature at the drip hole is 65°C-80°C, and the temperature of the core liquid is 25°C-60°C; the protective liquid is a calcium chloride aqueous solution with a mass fraction of 5%-20%, and the cooling temperature is 10°C-40°C.

Citation Information

Patent Citations

  • Water capsule for three-layer cigarette and preparation method of water capsule

    CN103815541A

  • Cigarette water capsule with water and hydrotropic substance as core materials and manufacturing method of cigarette water capsule with water and hydrotropic substance as core materials

    CN104305521A

  • Wax-in-water type cigarette explosive ball and preparation method thereof

    CN109222223A

  • Wax-encapsulated particles and method for making same

    EP0510761A1

  • Wax capsules containing hydrophilic cores

    US20090004337A1