A non-destructive separation method for lithium-ion battery interface impedance

The lithium-ion battery interface impedance is reconstructed through high-frequency inductive reactance and low-frequency diffusion models, and combined with relaxation time deconvolution technology and R//Q model, it solves the problem of early non-destructive diagnosis of the dynamic performance of the electrode interface and realizes the electrode interface Lossless separation of impedance and analysis of charge transfer internal resistance, suitable for dynamic diagnosis of electric vehicle batteries.

CN114976307BActive Publication Date: 2024-10-01BEIJING JIAOTONG UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210489917.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-05-07
Publication Date
2024-10-01
Estimated Expiration
2042-05-07

AI Technical Summary

Technical Problem

The existing technology lacks early non-destructive diagnosis technology for the dynamic performance of the electrode interface during the aging process of lithium-ion batteries. In particular, there is almost no research on the passivation film and charge transfer process. It is difficult to achieve non-destructive diagnosis of the dynamic impedance of the electrode interface from the full battery level. separation.

Method used

High-frequency inductive reactance and low-frequency diffusion models are used to reconstruct the interface impedance of lithium-ion batteries. Relaxation time deconvolution technology and R//Q model are used to identify the electrode reaction process, and the particle swarm optimization algorithm is combined to identify the internal resistance of the passivation film. , achieving lossless separation of electrode interface impedance.

Benefits of technology

The non-destructive separation of lithium-ion battery electrode interface impedance is achieved, and the evolution of characteristic parameters is analyzed through the transformation coefficient of charge transfer internal resistance, providing a reliable non-destructive diagnosis method for electric vehicle electrode interface dynamics.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114976307B_ABST
    Figure CN114976307B_ABST
Patent Text Reader

Abstract

The present invention discloses a non-destructive separation method for the interface impedance of a lithium-ion battery. The method reconstructs the real impedance reflecting the interface dynamics based on the total impedance and high-frequency inductive reactance and low-frequency diffusion model, uses relaxation time deconvolution technology and equivalent circuit to identify the model parameters of the interface, and realizes the non-destructive separation of the electrode interface dynamics model parameters through the impedance data of 50% and 5% SOC, and verifies the effectiveness of the technology in three-electrode impedance. At the same time, the charge transfer internal resistance of the separable SOC is transferred to the comparative SOC according to the conversion coefficient of the charge transfer internal resistance, realizing the analysis of the evolution law of the characteristic parameters at the same SOC point. The method has simple steps, is easy to operate, and has high reliability, and is suitable for non-destructive diagnosis of the electrode interface dynamics of electric vehicle power batteries.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of lithium-ion power battery safety, and in particular relates to a nondestructive diagnosis technology of electrode interface kinetic impedance of lithium-ion power batteries for electric vehicles. Background Art

[0002] In recent years, electric vehicles have developed rapidly. The development of electric vehicles is seen as an effective way to solve environmental pollution, reduce fuel consumption, and build green and environmentally friendly urban transportation. However, the kinetic performance of battery-powered vehicles is often the main reason for the sudden drop in mileage and power performance due to long-term use of batteries. The kinetic performance occurring at the solid / liquid interface is a comprehensive system of lithium ion and active material loss. Understanding the kinetic loss of a single electrode is an important means of identifying the mechanism of battery aging and early diagnosis. How to achieve lossless separation of the interface kinetics (passivation film and charge transfer process) of the electrode at the level of the entire battery is a very important technical issue.

[0003] Currently, most of the existing battery management systems focus on the analysis and identification of the battery's interface dynamics and lumped internal resistance, and most of the research on electrode performance degradation is also focused on post-disassembly and high-precision equipment testing. However, during the battery aging process, early non-destructive diagnosis technology for electrode interface dynamics is relatively scarce, especially the research on the passivation film and charge transfer process of the separated electrodes is almost blank. Summary of the invention

[0004] In view of the problems existing in the prior art, the present invention proposes a non-destructive separation method for the interface impedance of lithium-ion batteries. The method uses high-frequency inductive reactance and low-frequency diffusion model to reconstruct the interface impedance of the battery. To achieve the above purpose, the technical solution adopted by the present invention is:

[0005] A method for lossless separation of lithium-ion battery interface impedance, characterized in that:

[0006] The steps include:

[0007] Step 1: Perform an AC impedance test on a lithium-ion battery in an aging or temperature state at n% and m% (n, m are natural numbers) SOC;

[0008] Step 2: Subtract the high-frequency inductive reactance and the low-frequency diffusion impedance in the full frequency domain from the total impedance of the AC impedance test result to obtain the reconstructed interface impedance of n% and m% SOC;

[0009] Step 3: Deconvolution of the reconstructed interface impedance of n% and m% SOC is performed according to the relaxation time deconvolution technique (DRT) to obtain the DRT peaks of different interface reactions;

[0010] Step 4: According to the different responses of the positive and negative electrode charge transfer processes to low temperature and low SOC, the DRT peaks of different interface reactions are assigned to the reaction processes at the positive and negative electrode interfaces, and the relaxation times τcei and τsei across the positive electrode electrolyte membrane and the negative electrode solid electrolyte membrane are determined;

[0011] Step 5: Determine the optimal interval of relaxation time of the second-order R / / Q model according to the relaxation times τcei and τsei, and the sum of the reconstructed interface and charge transfer internal resistance Rct,total based on n% SOC;

[0012] Step 6: Based on the reconstructed interface impedance of n% SOC, the relaxation time τcei and τsei of the positive and negative electrode passivation films Rsei,total passing through the positive electrode electrolyte membrane and the negative electrode solid electrolyte membrane are calculated according to the lithium ion impedance, and the positive and negative electrode passivation films Rsei,total and the charge transfer internal resistance range of 90% to 110% Rct,total are used as the optimization interval, and the positive and negative electrode passivation film internal resistance Rcei and Rsei of the third-order R / / Q model and the total internal resistance Rct,total of the positive and negative electrode charge transfer are identified by an algorithm;

[0013] Step 7: At m% SOC, the total internal resistance Rct,total of the positive and negative electrode charge transfer is determined according to the positive and negative electrode passivation films Rsei,total, and the internal resistance range of 90% to 110% Rct,total is used as the optimization interval, and the 4th-order R / / Q model is used to identify the positive and negative electrode charge transfer internal resistance.

[0014] Preferably, the n% and m% SOC are 50% and 5% SOC.

[0015] In order to realize comparative analysis of the electrode reaction process, based on the above scheme, the following step 8 is also included:

[0016] Convert the internal resistance of the separable SOC point to the commonly used SOC point for comparative analysis, change the temperature or aging state, and return to step 1.

[0017] On the basis of the above scheme, the algorithm for identifying the internal resistances Rcei and Rsei of the positive and negative electrode passivation films of the third-order R / / Q model is a particle swarm optimization algorithm.

[0018] Based on the above scheme, the high-frequency inductive reactance and low-frequency diffusion impedance are specifically expressed as follows: the high-frequency inductive reactance model is a first-order R / / L model, and the low-frequency diffusion model is a combination of the solid-phase diffusion impedance expression of spherical particles and the liquid-phase diffusion impedance model characterized by the first-order R / / C.

[0019] The liquid phase diffusion impedance can be fitted by the first-order R / / C model, and the solid phase diffusion impedance model is an impedance response expression derived from the solid phase diffusion potential partial differential equation of the homogenized single particle model:

[0020]

[0021] Where DV is the ratio of the electrode equilibrium potential increment to the capacity increment, and τs is the solid phase diffusion time.

[0022] Furthermore, in steps 5 to 7, the objective function is defined as: the root mean square error between the impedance model simulation result and the actual test result within the test frequency range, that is:

[0023]

[0024] Where N is the number of test frequency points, Zm is the result of the test impedance data, and Zs is the result of the simulated impedance data.

[0025] Based on the above scheme, a series of independent radial basis functions are used to identify the electrochemical characteristic time constants in the interfacial impedance.

[0026] On the basis of the above scheme, a lithium ion testing device is provided, comprising a storage unit and an execution unit, for storing and executing the above lithium ion battery interface impedance lossless separation method.

[0027] Beneficial effects of the present invention:

[0028] The present invention realizes the non-destructive separation of the interface impedance of the lithium-ion battery electrode. At the same time, the charge transfer internal resistance of the separable SOC is transferred to the comparison SOC according to the conversion coefficient of the charge transfer internal resistance, realizing the analysis of the evolution law of characteristic parameters at the same SOC point. The method has simple steps, is easy to operate, and has high reliability, and is suitable for non-destructive diagnosis of electrode interface dynamics of electric vehicle power batteries. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] The present invention has the following accompanying drawings:

[0030] Figure 1 High frequency inductive reactance and low frequency diffusion models;

[0031] Among them, (a) is the high-frequency inductive reactance, and (b) is the low-frequency diffusion model;

[0032] Figure 2 Flow chart of the non-destructive separation method of the polarization process of the lithium-ion battery electrode interface;

[0033] Figure 3 Interface reaction relaxation time separation result diagram;

[0034] Figure 4Separation results of interfacial reaction internal resistance. DETAILED DESCRIPTION

[0035] The following combination Figure 1-4 The present invention is described in further detail.

[0036] The present invention is described in detail below in conjunction with a three-electrode battery experiment. In the embodiment, a soft-pack NMC111 lithium-ion power battery is used as an example, with a rated voltage of 3.75V and a nominal capacity of 8.5Ah. The correctness of the present invention is verified by using an assembled three-electrode battery. The experimental equipment used is: a Biologic electrochemical workstation with a Tianjin Tester SPX-150BX temperature control box.

[0037] like Figure 2 The steps shown are as follows:

[0038] The first step is to perform an AC impedance test on a lithium-ion battery in a certain aging or temperature state at 50% and 5% SOC, and record the experimental data of voltage and impedance;

[0039] In the second step, the impedance offset caused by OCV offset in the low frequency band is removed according to the static open circuit voltage in the first step, and the impedance data is corrected by the capacity change caused by the sinusoidal current to obtain the impedance data reflecting the real kinetic reaction:

[0040]

[0041] Where q, u, and i represent the battery's alternating capacity, alternating voltage, and alternating current, respectively; ω represents the battery's angular frequency, represents the phase angle, SOC0 represents the current SOC point, Qmax represents the maximum available capacity, Uoc represents the current open circuit voltage, and U represents the voltage signal of the original impedance.

[0042] Further, an impedance reflecting the real diffusion dynamics can be established:

[0043]

[0044] Due to the strong coupling effect of various electrochemical reactions, such as Figure 1 By establishing a high-frequency inductive reactance model and a low-frequency diffusion model, the influence of the two on the interface impedance data is completely decoupled, and the high-frequency inductive reactance and low-frequency diffusion impedance in the full frequency domain are subtracted from the total impedance to obtain the real impedance that can reflect the battery interface dynamics information. The specific expression is:

[0045] Z REIS =Z MEIS -Z SLM -Z RL (5)

[0046] Where SLM is the abbreviation of solid-liquid coexistence model, and RL stands for high-frequency inductive reactance model.

[0047] In the third step, the interface impedance of the two specific SOCs reconstructed in the second step is deconvolved according to the relaxation time deconvolution technique (DRT) to obtain the DRT peaks of different interface reactions, such as Figure 3 As shown. Figure 3 It can be seen that the relaxation time DRT of the passive film reaction of the electrode at two specific SOC points hardly changes, while the charge transfer reaction is greatly affected by the low temperature environment and low-end SOC, that is, at low temperatures, the slower charge transfer process of the negative electrode is easier to separate, and at low-end SOC, the slower charge transfer process of the positive electrode makes the charge transfer time of the electrode easier to separate. At the same time, after the three-electrode battery is operated from the first to the third steps as above, the DRT peak of the full battery has an obvious correspondence with the DRT peak of the electrode, and their relaxation times corresponding to the two specific SOCs are listed in Tables 1 and 2.

[0048] Table 1 Comparison of DRT results of full battery and electrode at the same SOC as step 5

[0049]

[0050] Table 2 Comparison of DRT results of full battery and electrode at another SOC

[0051]

[0052] In the fourth step, according to the different responses of the positive and negative charge transfer relaxation time to low temperature and low SOC, the DRT peak can be assigned to a single electrode interface reaction process from the whole battery level, and the relaxation time τ of each electrode reaction can be determined. The specific assignment is shown in Table 3. The combined analysis of two specific SOCs is used to determine the correctness of the separation of the positive electrode CEI and the negative electrode passivation film SEI. At 25°C and 10°C, the positive and negative charge transfers CT_CA and CT_AN are more easily separated at the low-end SOC, while at 0°C, the positive and negative charge transfers CT_CA and CT_AN are more easily separated at the same SOC as step five.

[0053] Table 3 Electrode reaction process corresponding to each DRT peak position

[0054]

[0055] The fifth step is to assign different DRT peaks to the reaction process at the positive and negative electrode interfaces according to the different responses of the positive and negative electrode charge transfer process to low temperature and low SOC. According to the relaxation time τ of the electrode passivation film and the charge transfer process determined in step 4, the optimization interval of the relaxation time of the second-order R / / Q model is determined, and the sum of the positive and negative electrode passivation film Rsei,total and the charge transfer internal resistance Rct,total is calculated based on the reconstructed interface impedance of 50% SOC.

[0056] In the sixth step, based on the interfacial impedance at the 50% SOC point reconstructed in the third step, the relaxation time τcei and τsei of lithium ions passing through the positive electrode electrolyte membrane and the negative electrode solid electrolyte membrane obtained in step 4, and the total passivation film Rsei,total and the charge transfer internal resistance of 90% to 110% Rct,total identified in the fifth step are used as the optimization range. The positive and negative passivation film internal resistances Rcei and Rsei of the third-order R / / Q model, as well as the total internal resistance Rct,total of the positive and negative charge transfer are identified by the particle swarm optimization algorithm. The identified passivation film internal resistance is shown in the attached figure. Figure 3 The results show that the technology described in the present invention can effectively reconstruct the internal resistance and time constant of the passivation film of the electrode under the following conditions;

[0057] Step 7: At 5% SOC, the total charge transfer impedance Rct,total can be preliminarily determined based on the total passivation film impedance Rsei,total determined in step 6, and 90% to 110% of Rct,total is used as the optimization range. The 4th-order R / / Q model is used to identify the positive and negative charge transfer internal resistances Rct_ca and Rct_an.

[0058] Step 8. In order to realize the comparative analysis of the electrode reaction process, the internal resistance at the separable SOC point needs to be converted to the commonly used 50% SOC point for comparative analysis. According to the Butler-Volmer equation, the conversion coefficient of the negative electrode charge transfer internal resistance is specifically expressed as:

[0059]

[0060] The negative electrode charge transfer resistance identified by the calculation model is converted to 50% SOC through the transfer coefficient, and the positive electrode charge transfer resistance is also calculated from the total charge transfer resistance and negative electrode charge transfer resistance calculated in step 7. The above results are compared with the positive and negative electrode charge transfer resistances identified by the three-electrode battery, as shown in Figure 2. Figure 4 shown.

[0061] The results show that the technology described in the present invention can effectively reconstruct the charge transfer internal resistance and time constant of the electrode at 25°C, 10°C, and 0°C.

[0062] The above implementation modes are only used to illustrate the present invention, but not to limit the present invention. Ordinary technicians in the relevant technical field can make various changes and modifications without departing from the essence and scope of the present invention. Therefore, all equivalent technical solutions also belong to the scope of the present invention, and the patent protection scope of the present invention should be defined by the claims. The contents not described in detail in this specification belong to the prior art known to professional and technical personnel in this field.

Claims

1. A method for lossless separation of interfacial impedance of lithium-ion batteries, characterized in that: The steps include: Step 1: Perform an AC impedance test on a lithium-ion battery in a certain aging or temperature state at n% and m% SOC; the n% is 50% and the m% is 5%; Step 2: Subtract the high-frequency inductive reactance and the low-frequency diffusion impedance in the full frequency domain from the total impedance of the AC impedance test result to obtain the reconstructed interface impedance of n% and m% SOC; Step 3: Deconvolute the reconstructed interface impedance of n% and m% SOC according to the relaxation time deconvolution technique DRT to obtain the DRT peaks of different interface reactions; Step 4: According to the different responses of the positive and negative electrode charge transfer processes to low temperature and low SOC, the DRT peaks of different interface reactions are assigned to the reaction processes at the positive and negative electrode interfaces, and the relaxation times τcei and τsei of lithium ions passing through the positive electrode electrolyte membrane and the negative electrode solid electrolyte membrane are determined; Step 5: According to the relaxation times τcei and τsei, determine the optimization interval of the relaxation time of the second-order R / / Q model, and calculate the sum of the total passivation film impedance Rsei,total of the positive and negative electrodes and the total charge transfer internal resistance Rct,total of the positive and negative electrodes based on the reconstructed interface impedance of 50% SOC; Step 6: Based on the reconstructed interface impedance of n% SOC, the relaxation time τcei and τsei of lithium ions passing through the positive electrode electrolyte membrane and the negative electrode solid electrolyte membrane, the total passivation film impedance Rsei,total of the positive and negative electrodes, and the internal resistance range of 90% to 110% Rct,total of the total charge transfer internal resistance of the positive and negative electrodes are used as the optimization interval, and the particle swarm optimization algorithm is used to identify the positive and negative electrode passivation film impedances Rcei and Rsei, as well as the total charge transfer internal resistance Rct,total of the positive and negative electrodes of the third-order R / / Q model; Step 7: At 5% SOC, the total positive and negative electrode charge transfer internal resistance Rct,total is preliminarily determined based on the total positive and negative electrode passivation film impedance Rsei,total determined in step 6, and 90% to 110% of Rct,total is used as the optimization range. The fourth-order R / / Q model is used to identify the positive and negative electrode charge transfer internal resistances Rct_ca and Rct_an.

2. A lithium-ion battery interface impedance lossless separation method as claimed in claim 1, characterized in that: The following steps are also included: Step 8: Convert the internal resistance at the separable SOC point to the commonly used 50% SOC point for comparative analysis of the positive and negative electrode charge transfer internal resistance.

3. A lithium-ion battery interface impedance lossless separation method as claimed in claim 1, characterized in that: The high-frequency inductive reactance and low-frequency diffusion impedance are specifically expressed as follows: The high-frequency inductive reactance model is a first-order R / / L model; The low-frequency diffusion model is a combination of the solid-phase diffusion impedance expression of spherical particles and the liquid-phase diffusion impedance model characterized by the first-order R / / C.

4. A method for lossless separation of lithium ion battery interface impedance as claimed in claim 1, characterized in that: A series of independent radial basis functions are used to identify the electrochemical characteristic time constants in the interfacial impedance.

5. A lithium ion testing device, characterized in that: It comprises a storage unit and an execution unit, which are used to store and execute a lithium-ion battery interface impedance lossless separation method as described in any one of claims 1 to 4.