Seesaw accelerometer and preparation method thereof

Through the silicon-glass composite cover plate and anode bonding process, the problems of insufficient preparation accuracy and sealing of the mass block in the seesaw accelerometer are solved, the miniaturization and high precision of the device are achieved, and the sealing and performance are improved.

CN115343503BActive Publication Date: 2024-10-11INST OF SEMICONDUCTORS - CHINESE ACAD OF SCI
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202110531763.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-05-14
Publication Date
2024-10-11
Estimated Expiration
2041-05-14

AI Technical Summary

Technical Problem

Existing seesaw accelerometers have process accuracy problems and insufficient sealing in mass preparation and lead methods, which affects device miniaturization.

Method used

The silicon-glass composite cover plate preparation method is used, and the anodic bonding process and indium tin oxide mask etching technology are used to form vertical leads and fixed capacitor plates, reducing lead width and bonding width, and improving sealing and accuracy.

Benefits of technology

It achieves the miniaturization and high precision of the seesaw accelerometer, improves the sealing and performance of the device, simplifies the preparation process of the mass block, and reduces signal feedthrough and crosstalk.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115343503B_ABST
    Figure CN115343503B_ABST
Patent Text Reader

Abstract

The present invention provides a seesaw accelerometer and a preparation method thereof, the preparation method comprising: using an anodic bonding process to bond a silicon-glass composite cover plate to the surface where the first groove of a fourth low-resistance silicon wafer is located, to obtain a second bonding sheet; using a patterned ITO as a mask or using a patterned ITO and a photoresist as a mask, corresponding to the position of a fixed capacitor plate, etching a "convex"-shaped mass block on the surface where the fourth low-resistance silicon wafer is located after thinning, to obtain a third bonding sheet containing a structural layer, wherein the mass block includes a first capacitor plate and a second capacitor plate of different sizes. The seesaw accelerometer preparation method of the present invention obtains a mass block by etching once, and the process is simple, efficient and high in precision. Using a silicon-glass composite cover plate, including a vertical lead and a fixed plate at the same time, and using an anodic bonding process to achieve sealed packaging, effectively improves the sealing performance of the device, reduces the lateral area of ​​the chip, and is conducive to improving the miniaturization of the device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of capacitive accelerometer design and manufacturing, and in particular to a seesaw accelerometer and a preparation method thereof. Background Art

[0002] Capacitive accelerometers are sensors that reflect changes in acceleration values ​​by changes in the distance between capacitor plates. Seesaw accelerometers are sensitive mass blocks that generate unbalanced torques at both ends of the mass block under the action of acceleration, causing the mass block to flip around the support beam, similar to a seesaw. The mass block, as the movable plate of the capacitor, flips, and the distance between it and the fixed plate of the capacitor changes, causing the capacitance to change.

[0003] The preparation of mass in the existing seesaw accelerometer usually adopts etching of the mass block or deposition of materials on the mass block to change the mass of different plates of the mass block. These two methods are greatly affected by the process accuracy, and the error between the prepared mass block and the design value is large. In addition, the existing seesaw accelerometer adopts the horizontal lead method, which will affect the sealing of the device, and the reserved lead width and bonding width are not conducive to the miniaturization of the device. Summary of the invention

[0004] 1. Technical issues to be resolved

[0005] In view of the existing technical problems, the present invention provides a seesaw accelerometer and a preparation method thereof, which are used to at least partially solve the above technical problems.

[0006] (II) Technical solution

[0007] The present invention provides a method for preparing a silicon-glass composite cover plate, comprising: etching a first low-resistance silicon wafer with a patterned photoresist or silicon oxide as a mask to obtain a second low-resistance silicon wafer including a silicon column and a silicon groove; bonding a first glass sheet to the surface of the second low-resistance silicon wafer where the silicon groove is located with an anodic bonding process to obtain a first bonding sheet; heating the first bonding sheet to soften the first glass sheet and fill the silicon groove; grinding the first bonding sheet to obtain a silicon-glass composite cover plate 5 in which the silicon column is isolated by glass, wherein the silicon column includes a vertical lead 6 and a fixed capacitor plate 7, and the vertical lead 6 is used to lead out an electrical signal in a sealed cavity of a sensor.

[0008] Optionally, the bonding gas pressure of the anodic bonding process is 10 -3 mbar~1bar; bonding the first glass sheet and the second low-resistance silicon wafer to form a first sealed cavity, the air pressure of the first sealed cavity is 1mbar~1bar.

[0009] The present invention provides a method for preparing a seesaw accelerometer, wherein a silicon-glass composite cover plate 5 is prepared by the method for preparing a silicon-glass composite cover plate according to an embodiment of the present invention, comprising: etching a third low-resistance silicon wafer using a patterned photoresist or silicon oxide as a mask to obtain a fourth low-resistance silicon wafer including a first groove 4; bonding the silicon-glass composite cover plate 5 to the surface of the fourth low-resistance silicon wafer where the first groove 4 is located using an anodic bonding process to obtain a second bonding sheet; grinding and thinning the surface of the second bonding sheet where the fourth low-resistance silicon wafer is located; and Using patterned ITO as a mask or using patterned ITO and photoresist as a mask, a "convex"-shaped mass block 3 is etched on the surface of the thinned fourth low-resistance silicon wafer corresponding to the position of the fixed capacitor plate 7 to obtain a third bonding sheet including a structural layer, wherein the mass block 3 includes a first capacitor plate 31 and a second capacitor plate 32 of different sizes; using patterned metal as a mask, the second glass sheet is corroded to obtain a cover plate 11 including a second groove 12; and the cover plate 11 and the structural layer are bonded using an anodic bonding process.

[0010] Optionally, the method for preparing the seesaw accelerometer also includes: using patterned photoresist or silicon oxide as a mask, etching a frame 1 and a cantilever beam 2 on the surface of the thinned fourth low-resistance silicon wafer, wherein the mass block 3 is torsionally connected to the frame 1 through the cantilever beam 2.

[0011] Optionally, the bonding gas pressure of the anodic bonding process is 10 -3 The bonding structure layer and the cover plate 11 form a sealed cavity, and the air pressure of the sealed cavity is 1 mbar to 1 bar.

[0012] On the other hand, the present invention provides a seesaw accelerometer, comprising: a cover plate 11, a structural layer and a silicon-glass composite cover plate 5 stacked in sequence; wherein the structural layer comprises a "convex"-shaped mass block 3, the mass block 3 comprises a first capacitor plate 31 and a second capacitor plate 32 of different sizes; the silicon-glass composite cover plate 5 comprises two fixed capacitor plates 7 arranged in parallel and isolated, and the two fixed capacitor plates 7 are respectively arranged in a non-contact manner corresponding to the first capacitor plate 31 and the second capacitor plate 32.

[0013] Optionally, the structural layer also includes: a frame 1 and a cantilever beam 2; wherein the mass block 3 is torsionally connected to the frame 1 through the cantilever beam 2; the mass block 3 is axially symmetrical along a direction perpendicular to the cantilever beam 2, and the first capacitor plate 31 and the second capacitor plate 32 are respectively located on both sides of the cantilever beam 2.

[0014] Optionally, the silicon-glass composite cover plate 5 also includes: a vertical lead 6 and an isolation ring 8, one end of the vertical lead 6 is connected to the structural layer, and the isolation ring 8 is used to isolate the vertical lead 6 and the fixed capacitor plate 7; the other end of the vertical lead 6 is provided with a first metal electrode 9, and the end of the fixed capacitor plate 7 away from the mass block 3 is provided with a second metal electrode 10; the cover plate 11 includes: a second groove 12, and the second groove 12 is used to provide a movable space for the mass block 3.

[0015] Optionally, the upper and lower surfaces of the cover plate 11 and / or the structural layer and / or the silicon-glass composite cover plate 5 are parallel; and the surface roughness of the cover plate 11 and / or the structural layer and / or the silicon-glass composite cover plate 5 is less than 50 nm.

[0016] Optionally, the material of the structural layer and / or the fixed capacitor plate 7 and / or the vertical lead 6 is low-resistance silicon; the material of the isolation ring 8 and / or the cover plate 11 is glass; the thickness of the cover plate 11 is 20-500 μm. The material of the first metal electrode 9 and / or the second metal electrode 10 includes: any one of aluminum, copper, titanium, gold, nickel, platinum, chromium, molybdenum, polycrystalline silicon and single crystal silicon with a resistivity lower than 0.001 Ω·cm and their combinations.

[0017] (III) Beneficial effects

[0018] The present invention provides a silicon-glass composite cover plate and a method for preparing a seesaw accelerometer comprising the silicon-glass composite cover plate. By using a silicon on glass (SOG) wafer etching process and an indium tin oxide (ITO) mask, a low-resistance silicon wafer is etched to obtain a silicon-glass composite cover plate in which silicon columns are isolated by glass. The silicon columns can be used as vertical leads and fixed capacitor plates. The vertical leads are used to lead out electrical signals in a sealed cavity of a sensor. There is no need to reserve a lateral lead position for a sensor device packaged using the silicon-glass composite cover plate, thereby reducing the lead width and bonding width of the device and greatly increasing the miniaturization space of the device.

[0019] The method for preparing a seesaw accelerometer provided by the present invention uses a single low-resistance silicon wafer as a structural layer, and uses chemical mechanical polishing to precisely control the thickness and surface roughness of the device layer, without using an SOI wafer. A "convex"-shaped mass block including a first capacitor plate and a second capacitor plate of different sizes is obtained by etching the low-resistance silicon wafer in one step, without requiring extra steps to change the mass at different ends of the mass block, and the preparation process is simple and accurate, thereby improving the performance of the seesaw accelerometer.

[0020] The silicon-glass composite cover plate and the method for preparing a seesaw accelerometer including the silicon-glass composite cover plate provided by the present invention adopt an anodic bonding process and improve the sealing of the device and the quality of the sensor device by adjusting the bonding air pressure and the sealing cavity air pressure of the bonding sheet.

[0021] On the other hand, the present invention provides a seesaw accelerometer, which adopts a "convex"-shaped mass block, that is, by changing the shape of the mass block to obtain a mass block with different masses at both ends, and has a delicate structure. A vertical lead is used to derive the electrical signal of the sealed cavity, and the lead and bonding width are low, which greatly reduces the size of the seesaw accelerometer. At the same time, the vertical lead does not have the step coverage problem in the bonding process, and can achieve a good airtight packaging. Compared with the silicon direct bonding packaging process, it does not require an excessively high temperature. Using glass as an isolation ring can effectively control parasitic capacitance and reduce signal feedthrough and crosstalk. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] The above and other objects, features and advantages of the present invention will become more apparent through the following description of the embodiments of the present invention with reference to the accompanying drawings, in which:

[0023] Figure 1 a- Figure 1 b schematically shows a structural diagram of a seesaw accelerometer according to an embodiment of the present invention;

[0024] Figure 2 a- Figure 2 c schematically shows a structural diagram of a structural layer according to an embodiment of the present invention;

[0025] Figure 3 a- Figure 3 c schematically shows a structural diagram of a silicon-glass composite cover plate according to an embodiment of the present invention;

[0026] Figure 4 a- Figure 4 c schematically shows a structural diagram of a cover plate according to an embodiment of the present invention;

[0027] Figure 5 A flow chart of a method for preparing a silicon-glass composite cover plate according to an embodiment of the present invention is schematically shown;

[0028] Figure 6 a- Figure 6 f schematically shows a structural change diagram of a silicon-glass composite cover plate preparation process according to an embodiment of the present invention;

[0029] Figure 7 A flowchart of a method for preparing a seesaw accelerometer according to an embodiment of the present invention is schematically shown;

[0030] Figure 8 a- Figure 8 i schematically shows a structural change diagram of a seesaw accelerometer preparation process according to an embodiment of the present invention.

[0031] [Description of Reference Numerals]

[0032] 1-Border

[0033] 2-Cantilever beam

[0034] 3-Mass Block

[0035] 31- first capacitor plate

[0036] 32- Second capacitor plate

[0037] 4-First groove

[0038] 5-Silicon-glass composite cover

[0039] 6-Vertical lead

[0040] 7-Fixed capacitor plates

[0041] 8-Isolation ring

[0042] 9-First metal electrode

[0043] 10- Second metal electrode

[0044] 11-Cover

[0045] 12-Second groove DETAILED DESCRIPTION

[0046] In order to make the objectives, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with specific embodiments and with reference to the accompanying drawings.

[0047] It should be noted that in the drawings or descriptions, similar or identical parts use the same figure numbers. The technical features in the various embodiments exemplified in the specification can be freely combined to form a new solution without conflict. In addition, each claim can be used as an embodiment alone or the technical features in each claim can be combined as a new embodiment. In the drawings, the shape or thickness of the embodiment can be expanded and simplified or conveniently indicated. Furthermore, the elements or implementations not shown or described in the drawings are in a form known to a person of ordinary skill in the art. In addition, although demonstrations of parameters containing specific values ​​may be provided herein, it should be understood that the parameters do not need to be exactly equal to the corresponding values, but can be approximated to the corresponding values ​​within an acceptable error tolerance or design constraint.

[0048] Unless there are technical obstacles or contradictions, the above-mentioned various embodiments of the present invention can be freely combined to form other embodiments, and these other embodiments are all within the protection scope of the present invention.

[0049] Although the present invention is described in conjunction with the accompanying drawings, the embodiments disclosed in the drawings are intended to exemplify the preferred embodiments of the present invention and should not be construed as limiting the present invention. The size ratios in the drawings are merely illustrative and should not be construed as limiting the present invention.

[0050] Although some embodiments of the present general inventive concept have been shown and described, it will be appreciated by those skilled in the art that changes may be made to these embodiments without departing from the principles and spirit of the present general inventive concept, the scope of which is defined by the claims and their equivalents.

[0051] Figure 1 a- Figure 1 b schematically shows a structural diagram of a seesaw accelerometer according to an embodiment of the present invention. Figure 1 a and Figure 1 b schematically shows, for example, a left view and a front view after cutting open the mass block 3 and the fixed capacitor plate 7 . Figure 2 a- Figure 2 c schematically shows a structural layer structure diagram according to an embodiment of the present invention. Figure 3 a- Figure 3 c schematically shows the structure of a silicon-glass composite cover plate according to an embodiment of the present invention.

[0052] According to an embodiment of the present invention, Figure 1 a- Figure 1 As shown in FIG. 2 , the seesaw accelerometer includes, for example, a cover plate 11, a structural layer and a silicon-glass composite cover plate 5 stacked in sequence. Figure 2 As shown in a, the structural layer includes a "convex" shaped mass block 3, which includes a first capacitor plate 31 and a second capacitor plate 32 of different sizes and a damping hole between the first capacitor plate 31 and the second capacitor plate 32, and the damping hole is used to adjust the system damping. Figure 3 a or Figure 3 As shown in Fig. 3, the silicon-glass composite cover plate 5 includes, for example, two fixed capacitor plates 7 that are arranged in parallel and isolated, and the two fixed capacitor plates 7 are arranged non-contactly corresponding to the first capacitor plate 31 and the second capacitor plate 32, respectively. The distance between the first capacitor plate 31 and the second capacitor plate 32 and the fixed capacitor plate 7 by the first groove 4 can be used as the initial capacitor plate spacing. The "convex"-shaped mass block 3 has different sizes at both ends, namely the first capacitor plate 31 and the second capacitor plate 32, and the first capacitor plate 31 and the second capacitor plate 32 belong to the same structural layer of material, so the masses at both ends of the mass block 3 are also different, which can constitute a "seesaw" structure of a seesaw accelerometer.

[0053] According to an embodiment of the present invention, Figure 2As shown in a, the structural layer also includes, for example, a frame 1 and a cantilever beam 2. Among them, the mass block 3 is torsionally connected to the frame 1 through the cantilever beam 2. The mass block 3 is axially symmetrical along a direction perpendicular to the cantilever beam 2, and the first capacitor plate 31 and the second capacitor plate 32 are respectively located on both sides of the cantilever beam 2. One of the surfaces of the mass block 3 can be flush with one of the surfaces of the frame 1 and the cantilever beam 2, and the other surface of the mass block 3 can be lower than the other surface of the frame 1, that is, the thickness of the mass block 3 is less than the thickness of the frame 1. The thickness of the cantilever beam 2 can be, for example, the same as the thickness of the mass block 3, the width of the cantilever beam 2 can be, for example, 10-100 μm, and the length of the cantilever beam 2 can be, for example, 100-300 μm. When the acceleration changes, the mass block 3 can be twisted with the cantilever beam 2 as the axis, and then the spacing between the mass block 3 and the fixed capacitor plate 7 changes, and the change in the spacing between the capacitor plates can reflect the change in acceleration. The material of the frame 1, the cantilever beam 2 and the mass block 3 can be, for example, low-resistance silicon.

[0054] According to an embodiment of the present invention, Figure 3 a or Figure 3 As shown in b, the silicon-glass composite cover plate 5, for example, also includes: a vertical lead 6 and an isolation ring 8. One end of the vertical lead 6 is connected to the structural layer, and the electrical signal in the sealed cavity of the seesaw accelerometer can be guided out of the seesaw accelerometer. The connection between the vertical lead 6 and the structural layer does not have the problem of step coverage during the bonding and pressing process, and a good airtight package can be achieved. Compared with the silicon direct bonding packaging process, it does not require an excessively high temperature. The isolation ring 8 is used to isolate the vertical lead 6 and the fixed capacitor plate 7. The isolation ring 8 is made of glass, for example, and can effectively control parasitic capacitance and reduce signal feedthrough and crosstalk. The other end of the vertical lead 6 is provided with a first metal electrode 9, and the end of the fixed capacitor plate 7 away from the mass block 3 is provided with a second metal electrode 10. The material of the vertical lead 6 and the fixed capacitor plate 7 can be, for example, low-resistance silicon. The material of the first metal electrode 9 and the second metal electrode 10 is a conductive material, for example, including: any one of aluminum, copper, titanium, gold, nickel, platinum, chromium, molybdenum, polysilicon, heavily doped single crystal silicon, for example, single crystal silicon with a resistivity lower than 0.001Ω·cm, and a combination thereof.

[0055] Figure 4 a- Figure 4 c schematically shows a structural diagram of a cover plate according to an embodiment of the present invention.

[0056] According to an embodiment of the present invention, Figure 4 a- Figure 4 As shown in c, the cover plate 11 includes, for example: a first groove 12, the first groove 12 is used to provide a movable space for the mass block 3. Figure 2As shown in FIG. 1 , when the left side of the mass block 3 is not flush with the frame 1, the cover plate 11 may not be provided with a groove and may be directly bonded to the left side of the mass block 3. In this case, the mass block 3 also has sufficient space for movement. The material of the cover plate 11 may be glass, such as Pyrex 7740 or BF33, which are commonly used glass types for anodic bonding. The thickness of the glass raw material may be, for example, 100-500 μm. The thickness of the cover plate 11 obtained by thinning may be, for example, 20-500 μm.

[0057] According to the embodiment of the present invention, the upper and lower surfaces of the cover plate 11 and / or the structural layer and / or the silicon-glass composite cover plate 5 are parallel; the surface roughness of the cover plate 11 and / or the structural layer and / or the silicon-glass composite cover plate 5 is less than 50 nm. That is, the upper and lower surfaces of each layer of material need to be parallel and smooth as much as possible to maximize the measurement accuracy of the seesaw accelerometer.

[0058] Figure 5 The flowchart of the method for preparing a silicon-glass composite cover plate according to an embodiment of the present invention is schematically shown.

[0059] Figure 6 a- Figure 6 f schematically shows the structural changes during the preparation process of the silicon-glass composite cover plate according to an embodiment of the present invention.

[0060] Another aspect of the present invention provides a method for preparing a silicon-glass composite cover plate, such as Figure 5 As shown, the method for preparing the silicon-glass composite cover plate includes, for example:

[0061] S501, using patterned photoresist or silicon oxide as a mask, etching the first low-resistance silicon wafer to obtain a second low-resistance silicon wafer including silicon pillars and silicon trenches.

[0062] According to an embodiment of the present invention, Figure 6 a- Figure 6 As shown in FIG. 2 , for example, a 300 nm thick silicon oxide film can be prepared on the surface of a 4-inch low-resistance silicon wafer, for example, by a chemical vapor deposition process. The etching area is defined by patterned photolithography, for example, a DRIE etching process is used to perform deep silicon etching on the low-resistance silicon wafer, and a 300 μm deep silicon groove is obtained by etching, and the etched silicon column can be used as a vertical lead 6 and a capacitor fixed plate 7. Then, for example, sulfuric acid, hydrogen peroxide, hydrochloric acid and other solutions are used to perform standard cleaning on the etched wafer to remove particles and organic matter remaining on the wafer surface.

[0063] S502, using an anodic bonding process, bonding the first glass sheet to the surface of the second low-resistance silicon wafer where the silicon grooves are located, to obtain a first bonding sheet.

[0064] According to an embodiment of the present invention, Figure 6c, for example, an anodic bonding process is used to bond a glass sheet to a wafer, and a silicon groove is sealed inside the bonding sheet. The upper surface of the resulting bonding sheet is glass, and the lower surface is silicon. During the bonding process, a high vacuum chamber must be ensured. That is, the bonding pressure of the anodic bonding process is, for example, 10 -3 The first glass sheet and the second low-resistance silicon wafer are bonded to form a first sealed cavity, and the air pressure of the first sealed cavity is, for example, 1 mbar to 1 bar.

[0065] S503, heating the first bonding wafer to soften the first glass wafer and fill the silicon groove.

[0066] According to an embodiment of the present invention, Figure 6 As shown in FIG. 4 , for example, a glass reflow process is used to place the bonding sheet in a high-temperature annealing furnace, for example, at a high temperature above 821°C to soften the glass in the bonding sheet and make it fluid. Under pressure and other conditions, the glass flows into the silicon groove until the silicon groove is completely filled. After the glass is cooled and shaped, it is taken out of the high-temperature annealing furnace.

[0067] S504, grinding the first bonding wafer to obtain a silicon-glass composite cover plate 5 in which silicon pillars are separated by glass, wherein the silicon pillars include vertical leads 6 and fixed capacitor plates 7, and the vertical leads 6 are used to lead out electrical signals in the sealed cavity of the sensor.

[0068] According to an embodiment of the present invention, Figure 6 e- Figure 6 As shown in FIG. 5 , the upper glass surface of the bonding sheet is ground and polished by, for example, a chemical mechanical grinding and polishing process, with the lower surface of the bonding sheet as a reference, until the silicon pillar on the upper surface of the bonding sheet is exposed. Then, with the polished glass surface as a reference, the lower silicon surface of the bonding sheet is chemically mechanically polished until the glass is exposed on the lower surface of the bonding sheet. The upper and lower planes of the polished bonding sheet are both surrounded by glass to electrically isolate the silicon pillar, and the silicon pillar can be used for vertical lead electrical connection and fixed capacitor plates.

[0069] Figure 7 A flow chart of a method for preparing a seesaw accelerometer according to an embodiment of the present invention is schematically shown.

[0070] Figure 8 a- Figure 8 i schematically shows a structural change diagram of a seesaw accelerometer preparation process according to an embodiment of the present invention.

[0071] Another aspect of the present invention provides a method for preparing a seesaw accelerometer, such as Figure 7 As shown, the method for preparing the seesaw accelerometer includes, for example:

[0072] S701 , using the patterned photoresist or silicon oxide as a mask, etching the third low-resistance silicon wafer to obtain a fourth low-resistance silicon wafer including the first groove 4 .

[0073] According to an embodiment of the present invention, Figure 8 As shown in a, on the surface of a low-resistance silicon wafer, a 300nm thick silicon oxide film is prepared, for example, by a chemical vapor deposition process, and a patterned photoresist, silicon oxide or other materials are used as a mask to etch a groove of, for example, 2μm on the surface of the low-resistance silicon wafer to serve as a gap between the fixed plate and the movable plate of the capacitor.

[0074] S702 , using an anodic bonding process, bonding the silicon-glass composite cover plate 5 to the surface of the fourth low-resistance silicon wafer where the first groove 4 is located, to obtain a second bonding wafer.

[0075] According to an embodiment of the present invention, Figure 8 As shown in FIG. 2 , for example, an anodic bonding process is used to bond the upper surface of the low-resistance silicon to the silicon-glass composite cover plate 5 prepared in the above embodiment through alignment photolithography, and the upper surface of the low-resistance silicon wafer and the lower surface of the silicon-glass cover plate are the bonding interface. For example, the bonding sheet can be turned over, and at this time, the lower surface of the original low-resistance silicon wafer is the upper surface of the bonding sheet, and the upper surface of the silicon-glass composite cover plate is the lower surface of the bonding sheet.

[0076] S703, grinding and thinning the surface of the second bonding wafer where the fourth low-resistance silicon wafer is located.

[0077] According to an embodiment of the present invention, Figure 8 As shown in c, the low-resistance silicon on the upper surface of the bonding wafer is thinned and polished with the lower surface of the bonding wafer as the reference. For example, a 400 μm thick silicon wafer is thinned to, for example, 80 μm, and the remaining low-resistance silicon thickness of 80 μm is the thickness of the seesaw structure layer.

[0078] S704, using patterned ITO as a mask or patterned ITO and photoresist as a mask, corresponding to the position of the fixed capacitor plate 7, a "convex"-shaped mass block 3 is etched on the surface of the thinned fourth low-resistance silicon wafer to obtain a third bonding sheet including a structural layer, wherein the mass block 3 includes a first capacitor plate 31 and a second capacitor plate 32 of different sizes.

[0079] According to an embodiment of the present invention, Figure 8 As shown in FIG. d, on the polished low-resistance silicon surface, for example, a 300 nm thick silicon oxide is deposited by chemical vapor deposition as a mask, and the etching area is defined by patterned photolithography, and for example, a dry etching process is used to perform deep silicon etching on the thinned structural layer until the low-resistance silicon layer is completely etched, thereby completing the release of the seesaw mass block 3. For example, the structural layer can also be etched simultaneously to obtain the frame 1 and the cantilever beam 2, and the mass block 3 is torsionally connected to the frame 1 through the cantilever beam 2.

[0080] S705 , using the patterned metal as a mask, etching the second glass sheet to obtain a cover plate 11 including a second groove 12 .

[0081] According to an embodiment of the present invention, Figure 8 As shown in Figure e, for example, 20 nm thick chromium and 20 nm thick gold are evaporated by electron beam on the surface of the glass sheet, and the etching area is defined by patterned photoresist to pattern the metal mask. Under the protection of the patterned metal mask, for example, a 20 μm deep groove is etched on the glass surface by a wet etching process to serve as the active area of ​​the seesaw mass block. Then, for example, a wet etching process is used to remove metal, photoresist and other substances on the glass surface, and standard cleaning is performed. The etched glass sheet is used as a glass cover.

[0082] S706, bonding the cover plate 11 and the structural layer by using an anodic bonding process.

[0083] According to an embodiment of the present invention, Figure 8 h, for example, the side of the glass cover plate with the groove is the lower surface, and the flat side is the upper surface. The glass cover plate and the structural layer of the bonding sheet are bonded together by using the anodic bonding process. The lower surface of the glass cover plate and the upper surface of the bonding sheet are the bonding interface, so as to realize the three-layer bonding of the glass cover plate, the structural layer and the silicon-glass composite cover plate. The bonding gas pressure of the anodic bonding process is, for example, 10 -3 mbar~1bar. The bonding structure layer and the cover plate 11 form a sealed cavity, and the air pressure of the sealed cavity is, for example, 1mbar~1bar. Then, for example, 200nm thick aluminum is deposited on the surface of the silicon-glass composite cover plate 5 by magnetron sputtering process, and PAD is defined by graphic lithography, that is, the area of ​​the electrode on the surface of the cover plate and the lead routing. The PAD covers the surface of the vertical lead 6 and the fixed plate 7 of the capacitor respectively. Finally, the device based on the low-resistance silicon wafer is diced according to the size required by the seesaw accelerometer to obtain a seesaw accelerometer.

[0084] In summary, the embodiment of the present invention proposes a seesaw accelerometer and a preparation method thereof, which adopts a silicon-glass composite cover plate, includes vertical leads and a fixed electrode plate, and adopts an anodic bonding process to achieve sealed packaging, effectively improving the sealing performance of the device, reducing the lateral area of ​​the chip, and is conducive to improving the reliability and miniaturization of the device.

[0085] Any details not included in the method / product embodiment section are similar to those in the device / method embodiment section. Please refer to the device / method embodiment section and will not be repeated here.

[0086] It should be understood that the specific order or hierarchy of steps in the disclosed process is an example of an exemplary method. Based on design preferences, it should be understood that the specific order or hierarchy of steps in the process can be rearranged without departing from the scope of protection of the present disclosure. The attached method claims present the elements of the various steps in an exemplary order and are not intended to be limited to a specific order or hierarchy.

[0087] It should also be noted that the directional terms mentioned in the embodiments, such as "upper", "lower", "front", "back", "left", "right", etc., are only reference directions of the drawings and are not intended to limit the scope of protection of the present disclosure. Throughout the drawings, the same elements are represented by the same or similar reference numerals. Conventional structures or configurations will be omitted when they may cause confusion in the understanding of the present disclosure. In addition, the shapes, sizes, and positional relationships of the components in the drawings do not reflect the actual sizes, proportions, and actual positional relationships.

[0088] In the above detailed description, various features are grouped together in a single embodiment to simplify the disclosure. This method of disclosure should not be interpreted as reflecting an intention that the embodiments of the claimed subject matter require more features than are clearly stated in each claim. On the contrary, as reflected in the appended claims, the invention is in a state of having less than all the features of the disclosed individual embodiments. Therefore, the appended claims are hereby expressly incorporated into the detailed description, with each claim standing on its own as a separate preferred embodiment of the invention.

[0089] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "multiple" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined. With respect to the term "comprising" used in the specification or claims, the word is covered in a manner similar to the term "including", just as "including," is explained as a transitional word in the claims. Any term "or" used in the specification of the claims is intended to mean "non-exclusive or".

[0090] The specific embodiments described above further illustrate the objectives, technical solutions and beneficial effects of the present invention in detail. It should be understood that the above description is only a specific embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for preparing a silicon-glass composite cover plate, characterized in that: include: Using patterned photoresist or silicon oxide as a mask, etching the first low-resistance silicon wafer to obtain a second low-resistance silicon wafer including silicon pillars and silicon trenches; Adopting an anodic bonding process, bonding the first glass sheet to the surface of the second low-resistance silicon wafer where the silicon groove is located, to obtain a first bonding sheet; heating the first bonding sheet to soften the first glass sheet and fill the silicon groove; The first bonding sheet is ground to obtain the silicon-glass composite cover plate (5) in which the silicon pillars are isolated by glass, wherein the silicon pillars include vertical leads (6) and fixed capacitor plates (7), and the vertical leads (6) are used to lead out electrical signals in the sealed cavity of the sensor.

2. The method for preparing a silicon-glass composite cover plate according to claim 1, characterized in that: The bonding gas pressure of the anodic bonding process is 10 -3 mbar~1bar; The first glass sheet and the second low-resistance silicon wafer are bonded to form a first sealed cavity, and the air pressure of the first sealed cavity is 1 mbar~1 bar.

3. A method for preparing a seesaw accelerometer, characterized in that: A silicon-glass composite cover plate (5) prepared by the method for preparing a silicon-glass composite cover plate according to claim 1, comprising: Using patterned photoresist or silicon oxide as a mask, etching the third low-resistance silicon wafer to obtain a fourth low-resistance silicon wafer including a first groove (4); Using an anodic bonding process, the silicon-glass composite cover plate (5) is bonded to the surface of the fourth low-resistance silicon wafer where the first groove (4) is located, thereby obtaining a second bonding sheet; Grinding and thinning the surface of the second bonding wafer where the fourth low-resistance silicon wafer is located; Using patterned ITO as a mask or using patterned ITO and photoresist as a mask, a "convex"-shaped mass block (3) is etched on the surface of the thinned fourth low-resistance silicon wafer corresponding to the position of the fixed capacitor plate (7), thereby obtaining a third bonding sheet including a structural layer, wherein the mass block (3) includes a first capacitor plate (31) and a second capacitor plate (32) of different sizes; Using the patterned metal as a mask, etching the second glass sheet to obtain a cover plate (11) including a second groove (12); The cover plate (11) and the structural layer are bonded using an anodic bonding process.

4. The method for preparing a seesaw accelerometer according to claim 3, characterized in that: The method for preparing the seesaw accelerometer further comprises: Using patterned photoresist or silicon oxide as a mask, a frame (1) and a cantilever beam (2) are etched on the surface of the thinned fourth low-resistance silicon wafer, wherein the mass block (3) is torsionally connected to the frame (1) via the cantilever beam (2).

5. The method for preparing a seesaw accelerometer according to claim 3, characterized in that: The bonding gas pressure of the anodic bonding process is 10 -3 mbar~1bar; The structural layer and the cover plate (11) are bonded to form a sealed cavity, wherein the air pressure of the sealed cavity is 1 mbar to 1 bar.

6. A seesaw accelerometer, characterized in that: include: A cover plate (11), a structural layer and a silicon-glass composite cover plate (5) stacked in sequence; The structural layer comprises a mass block (3) in a "convex" shape, and the mass block (3) comprises a first capacitor plate (31) and a second capacitor plate (32) of different sizes; The silicon-glass composite cover plate (5) comprises two fixed capacitor plates (7) arranged in parallel and in isolation, and the two fixed capacitor plates (7) are arranged in a non-contact manner corresponding to the first capacitor plate (31) and the second capacitor plate (32), respectively.

7. The seesaw accelerometer according to claim 6, characterized in that: The structural layer also includes: A frame (1) and a cantilever beam (2); Wherein, the mass block (3) is torsionally connected to the frame (1) via the cantilever beam (2); The mass block (3) is axisymmetric along a direction perpendicular to the cantilever beam (2), and the first capacitor plate (31) and the second capacitor plate (32) are respectively located on two sides of the cantilever beam (2).

8. The seesaw accelerometer according to claim 6, characterized in that: The silicon-glass composite cover plate (5) further comprises: A vertical lead (6) and an isolation ring (8), one end of the vertical lead (6) being connected to the structural layer, and the isolation ring (8) being used to isolate the vertical lead (6) from the fixed capacitor plate (7); A first metal electrode (9) is provided at the other end of the vertical lead (6), and a second metal electrode (10) is provided at one end of the fixed capacitor plate (7) away from the mass block (3); The cover plate (11) comprises: A second groove (12), wherein the second groove (12) is used to provide a movable space for the mass block (3).

9. The seesaw accelerometer according to claim 6, characterized in that: The upper and lower surfaces of the cover plate (11) and / or the structural layer and / or the silicon-glass composite cover plate (5) are parallel; The surface roughness of the cover plate (11) and / or the structural layer and / or the silicon-glass composite cover plate (5) is less than 50 nm.

10. The seesaw accelerometer according to claim 8, characterized in that The material of the structural layer and / or the fixed capacitor plate (7) and / or the vertical lead (6) is low-resistance silicon; The material of the isolation ring (8) and / or the cover plate (11) is glass; The thickness of the cover plate (11) is 20-500 μm; The material of the first metal electrode (9) and / or the second metal electrode (10) includes: Any one of aluminum, copper, titanium, gold, nickel, platinum, chromium, molybdenum, polycrystalline silicon and single crystal silicon with a resistivity lower than 0.001Ω•cm, and any combination thereof.

Citation Information

Patent Citations

  • Z axis structure of accelerometer

    CN104614553A

  • Triaxial capacitive MEMS acceleration sensor and preparation method

    CN104714050A

  • Preparation method of low-stress acceleration meter

    CN105137121A

  • Capacitive compound sensor and manufacturing method thereof

    CN106290985A

  • Low-stress Z-axis MEMS accelerometer based on rigidity coupling

    CN111766404A