A method for determining the morphology and displacement evolution of shale particles under simulated gravity

Through the HA-YXZB-II core preparation instrument and multi-scale multi-view scanning electron microscope technology, combined with Image J software, the morphology and displacement evolution of shale particles are measured under simulated gravity, which solves the difficulty of analyzing shale particles with existing technologies. The shortcomings of simulation experiments enable precise evaluation of shale reservoirs and support shale oil and gas production.

CN115508399BActive Publication Date: 2024-10-29CHENGDU UNIVERSITY OF TECHNOLOGY
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202210783323.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-05
Publication Date
2024-10-29
Estimated Expiration
2042-07-05

AI Technical Summary

Technical Problem

Existing shale particle simulation experiments are difficult to directionally characterize the morphological characteristics, displacement evolution, and changes in directional arrangement of particles. It is especially difficult to accurately analyze changes in microstructure under simulated overlying gravity.

Method used

Using the HA-YXZB-II core preparation instrument combined with multi-scale multi-view scanning electron microscopy technology and Image J software, the morphology and displacement evolution of shale particles under the action of gravity was simulated through drying, dehydration and layer-by-layer pressurization. Determination, calculation of geometric parameters and degree of arrangement of particles, using epoxy adhesive as cement, simulating the impact of overlying pressure on fine-grained rocks.

Benefits of technology

It achieves accurate measurement of shale particle morphology and displacement evolution process, reveals the mechanical mechanism of the directional arrangement of fine-grained rock particles caused by overlying rock pressure, provides precise evaluation of shale reservoirs, and helps shale oil and gas production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115508399B_ABST
    Figure CN115508399B_ABST
Patent Text Reader

Abstract

The present invention belongs to the field of geological experiment technology, and discloses a method for measuring the morphology and displacement evolution process of shale particles under simulated gravity, extracting kerogen from shale core as organic component experimental material, selecting inorganic component experimental material; selecting experimental equipment; drying and dehydrating the mineral particles, and uniformly stirring them with a mixing agitator; loading the mixed mineral particle layered samples into a mold until the mold is filled; taking out the samples after compacting; and calculating the morphological characteristics and particle arrangement degree of the shale sample particles. The present invention analyzes the geomechanical environment during the diagenesis of fine-grained rock particles, analyzes the changing laws of the morphological characteristics, arrangement characteristics, and pore structure characteristics of the particles under the pressure of the overlying rock, analyzes the influence of stress differences on the directional arrangement of fine-grained rock particles, and reveals the mechanical mechanism of the directional arrangement of fine-grained rock particles.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of geological experiments, and in particular relates to a method for measuring the morphology and displacement evolution process of shale particles under simulated gravity. Background Art

[0002] Fine-grained rock is well developed in my country, containing huge oil and gas resources, and has broad prospects for development. With the continuous advancement of unconventional oil and gas exploration technology, fine-grained rock has been considered to be the source rock and reservoir of tight and shale oil and gas, and is closely related to oil and gas resources. Compared with conventional reservoirs, fine-grained rock has small grain size and complex arrangement structure, and is a trinity of "source-reservoir-cap". In addition, fine-grained rock reservoirs have strong heterogeneity, which manifests itself as anisotropy of physical and mechanical properties at the macro level, and mainly manifests itself as variability, complexity and randomness of particle structure and arrangement combination at the micro level. At present, fine-grained rock particles are affected by various external forces during diagenesis, the most important of which is the overburden pressure. Overburden rock pressure, also known as overburden load and geostatic pressure, refers to the pressure generated by the sum of the mass of the matrix of the overburden formation and the mass of the fluid (oil, gas, water) in the pores of the overburden formation, and the direction is vertically downward. During the process of diagenesis and compaction, a certain point in the formation will be subjected to the force caused by the compaction of the upper rock. The overlying rock strata at a certain point of fine-grained rock in the formation are equal to the sum of the total weight of the overlying strata.

[0003] Compaction has a distorting and squeezing effect. Some sediments rich in clay minerals and organic matter can be compacted to one-quarter or even one-eighth of their initial deposition thickness. Plastic minerals such as clay minerals and organic matter are more easily compressed and deformed under the action of overburden pressure, while brittle particles such as quartz feldspar are not easy to deform, and the orientation of mineral particles is difficult to change. Therefore, overburden rock pressure plays a key role in the evolution of fine-grained sedimentary rocks.

[0004] The experiment used the "cold pressing method" to simulate the compaction process of mudstone, and adopted the principle of a single variable. Through artificial rock pressing simulation experiments, the evolution of mudstone particle morphology and displacement under overburden stress can be analyzed more accurately and intuitively. Artificial cores can eliminate the interference of external factors and accurately control mineral composition, overburden pressure and other conditions.

[0005] Through the above analysis, the problems and defects of the existing technology are as follows: the existing shale particle simulation experiment can only simulate the macroscopic morphological characteristics of the rock under the overlying gravity, and it is difficult to characterize the morphological characteristics, displacement evolution and changes in directional arrangement of the particles. Summary of the invention

[0006] In view of the problems existing in the prior art, the present invention provides a method for measuring the morphology and displacement evolution process of shale particles under simulated gravity.

[0007] The present invention is implemented as follows: a method for measuring the morphology and displacement evolution of shale particles under simulated gravity comprises:

[0008] Step 1: extract kerogen from shale core as organic component experimental material, and select brittle mineral and clay mineral powder with purity of more than 90% as inorganic component experimental material;

[0009] Step 2: Select HA-YXZB-II core preparation instrument as the experimental equipment;

[0010] Step 3, drying and dehydrating the mineral particles, and uniformly stirring them using a mixing agitator;

[0011] Step 4: Load the mixed mineral particle layered samples into the mold, press each layer under an overburden pressure of 10 MPa for 10 minutes, and then load the next layer of mineral particles until the mold is filled;

[0012] Step 5: After compacting the sample for 20 hours, take the sample out of the mold;

[0013] Step six, based on the multi-scale and multi-view scanning electron microscopy identification technology (7×7), combined with Image J software, the morphological characteristics and particle arrangement degree of the shale sample particles were calculated respectively.

[0014] Furthermore, in step 1, quartz, feldspar, calcite and pyrite are used as brittle mineral experimental materials, and illite, montmorillonite, kaolinite and chlorite are selected as clay mineral experimental materials. The proportion of specific minerals refers to the simulated shale lithofacies type, and there is no fixed proportion.

[0015] Furthermore, the experimental equipment in step 2 is divided into two parts: an automatic pressure control system and a hydraulic press. The applied pressure range is 0-60 MPa. The rock mold is composed of a base, a cavity, a pressure-bearing layer, etc. The cavity is a cylinder. After the mixed mineral particles are loaded into the mold layer by layer, the overburden pressure value is set.

[0016] Furthermore, in the drying and dehydration treatment in step 3, the drying is carried out at a constant temperature of 60°C to 80°C for 24 hours, and the stirring time of the mixing stirrer is 30 minutes. The dehydration treatment is to eliminate the influence of water on the surface of the mineral particles on the experiment, making the simulation experiment more reasonable.

[0017] Furthermore, when the sample is loaded into the mold in layers in step 4, the specific steps include:

[0018] (1) adding a cementing material to the mixed mineral particles;

[0019] (2) screening the particles of the uniformly mixed cement;

[0020] (3) Loading the mineral particles after the above steps into a pressing mold, using a layer-by-layer loading and gradual pressurization method.

[0021] Furthermore, the binder in step (1) is A / B series epoxy adhesive YY4250A / B, the content of the binder is maintained at about 5% of the weight of the mineral, and the binder is fully adhered to the surface of the mineral particles.

[0022] Furthermore, in step (2), the particles are passed through a 1000-mesh sieve.

[0023] Furthermore, in step (3), when the samples are loaded into the mold layer by layer, the pressure is increased to 10 MPa and pressed for 10 minutes after each loading, and this cycle is repeated until the mold is filled.

[0024] Furthermore, in step 5, during the compaction of multiple groups of samples for different periods of time, the overburden pressure is calculated according to the following formula:

[0025] P r =Hρg

[0026] Where P r is the overlying stratum pressure, in MPa; H is the burial depth, in m; g is the gravitational acceleration, which is 9.8 m / s 2 ; ρ is the average density of the formation, which is 2.16~2.65g / cm 3 .

[0027] Further, the operation process of the Image J image processing software in step six is ​​as follows:

[0028] ① Grayscale transformation: import the target image into the software and transform the image into grayscale;

[0029] ② Grayscale threshold setting: adjust the image threshold according to the grayscale value of the image, so that the image presents a complete geometric shape of the particle size, keep the threshold concentrated in a stable range, and extract the particles according to the threshold;

[0030] ③ Automatic denoising: manually correct the image, or remove the noise by filtering and smoothing the image, and use automatic denoising for analysis;

[0031] ④ Acquisition of geometric parameters: Set an appropriate scale for the image according to the magnification of the scanning electron microscope; calculate the geometric parameters of the particles, including particle size, flatness, perimeter, equivalent elliptical perimeter, convexity, and calibrate and count the particles;

[0032] ⑤ Export data: export and transform data, save all data output in Excel, and obtain particle geometry information after data processing; the identified information values ​​are divided into particle area, pixel value, X and Y coordinate position, particle circumference, width, length, height and angle, particle Feret diameter, particle roundness, particle sphericity and convexity parameters.

[0033] Furthermore, the calculation model of the particle arrangement degree in step 6 is:

[0034] Based on the influence of pore arrangement structure, the directional entropy of fine-grained rock structure is regarded as a function of particle size entropy, particle arrangement entropy and pore arrangement entropy, which is expressed by the following formula:

[0035]

[0036] In the formula, E di is the particle arrangement entropy, which represents the particle orientation fractal dimension value; E pd is the particle size entropy, which indicates the value of the particle size fractal dimension; E bi is the pore arrangement entropy, which represents the value of the pore orientation fractal dimension.

[0037] The fine-grained rock value is equivalent to the average of the particle arrangement entropy, grain size entropy and pore arrangement entropy, and the weight coefficient is 1 / 3, as shown below:

[0038]

[0039] in, The larger the value, the higher the degree of disorder, the more chaotic the arrangement, the more chaotic the arrangement, the more irregular the arrangement, and the more unstable the system. The smaller the value, the lower the degree of disorder, the more directional the arrangement, and the more stable the system.

[0040] Furthermore, the multi-scale and multi-viewing field scanning electron microscope identification technology in step six adopts a method of splicing 7×7 scanning electron microscope images end to end.

[0041] In combination with the above technical solutions and the technical problems solved, please analyze the advantages and positive effects of the technical solutions to be protected by the present invention from the following aspects:

[0042] First, in view of the technical problems existing in the above-mentioned prior art and the difficulty of solving the problems, the technical solutions to be protected by the present invention and the results and data during the research and development process are closely combined to analyze in detail and deeply how the technical solutions of the present invention solve the technical problems, and some creative technical effects brought about after solving the problems. The specific description is as follows:

[0043] The present invention analyzes the geomechanical environment during the diagenesis of fine-grained rock particles, simulates the action mechanism of overlying gravity on its microstructure through artificial rock compression experiments, analyzes the changing laws of the morphological characteristics, arrangement characteristics, and pore structure characteristics of the particles under the pressure of the overlying rocks, analyzes the influence of stress differences on the directional arrangement of fine-grained rock particles, and reveals the mechanical mechanism of the directional arrangement of fine-grained rock particles.

[0044] Second, considering the technical solution as a whole or from the perspective of the product, the technical effects and advantages of the technical solution to be protected by the present invention are described in detail as follows:

[0045] The morphological characteristics and directional arrangement of mineral particles in shale can control the migration of oil and gas. Therefore, it is of great significance to characterize the influence of the morphological characteristics and directional arrangement of different shale mineral particles on seepage. By simulating the directional arrangement of particles under different gravity, it is beneficial to the fine evaluation of shale reservoirs, so the present invention can serve shale oil and gas exploitation more accurately. BRIEF DESCRIPTION OF THE DRAWINGS

[0046] Figure 1 It is a flow chart of a method for measuring the morphology and displacement evolution process of shale particles under simulated gravity provided by an embodiment of the present invention;

[0047] Figure 2 This is a rendering of the mineral powder provided by an embodiment of the present invention;

[0048] Figure 3 It is a FE-SEM rendering of artificially compacted shale and shale in a formation provided by an embodiment of the present invention.

[0049] Figure 4 These are the renderings of artificial shale cores under different overburden pressures provided by the embodiments of the present invention (#G1-#G8).

[0050] Figure 5 This is a multi-scale and multi-view FE-SEM stitching effect diagram of the #G1-#G8 shale samples provided in an embodiment of the present invention (a. 25MPa; b. 30MPa; c. 35MPa; d. 40MPa; e. 45MPa; f. 50MPa; g. 55MPa; h. 60MPa).

[0051] Figure 6 It is a line graph of average pore size changes under different overburden pressures and lithofacies provided by an embodiment of the present invention.

[0052] Figure 7 It is a line graph of pore flatness variation under different overburden pressures provided by an embodiment of the present invention.

[0053] Figure 8 It is a schematic diagram of the change in particle size shape under different overlying pressures provided by an embodiment of the present invention.

[0054] Fig. 9 It is a diagram of the dominant direction of shale particle arrangement under overlying rock pressure provided by an embodiment of the present invention.

[0055] Fig.10 It is a numerical line graph of particle size, particle and pore orientation fractal dimension under different overburden pressures provided by an embodiment of the present invention.

[0056] Fig.11 It is a histogram of directional entropy of different overlying stress structures provided by an embodiment of the present invention.

[0057] Fig.12 It is a diagram of the evolution pattern of particle microstructure under the pressure of overlying rock provided by an embodiment of the present invention. DETAILED DESCRIPTION

[0058] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0059] 1. Explanatory Examples In order to enable those skilled in the art to fully understand how to implement the present invention, this section provides an illustrative example that expands and describes the technical solution of the claims.

[0060] like Figure 1 As shown, the method for measuring the morphology and displacement evolution of shale particles under simulated gravity provided by the embodiment of the present invention includes:

[0061] S101, selection of experimental samples: extract kerogen from shale core as organic component, select brittle mineral experimental materials and clay mineral experimental materials with a purity of 90%;

[0062] S102, select HA-YXZB-II core preparation instrument as the experimental equipment;

[0063] S103, drying and dehydrating the mineral particles, and uniformly stirring them using a mixing agitator;

[0064] S104, loading the mixed mineral particle layered samples into a mold, pressing each layer under an overburden pressure of 10 MPa for 10 min, and then loading the next layer of mineral particles until the mold is filled;

[0065] S105, after compacting the sample for 20 hours, take the sample out of the mold;

[0066] S106, based on the multi-scale and multi-view scanning electron microscopy identification technology (7×7), combined with Image J software, the morphological characteristics and particle arrangement degree of shale sample particles were calculated respectively.

[0067] (1) Experimental samples

[0068] Kerogen in shale is the main body of organic matter, accounting for about 80% to 90% of the total organic matter. More than 80% of petroleum hydrocarbons are converted from kerogen. The composition and structure of kerogen are complex. It is a high molecular polymer with no fixed structural expression. Kerogen was extracted from shale core as an organic component. Quartz, feldspar, calcite, and pyrite were selected as brittle mineral experimental materials, and illite, montmorillonite, kaolinite, and chlorite were selected as clay mineral experimental materials (such as Figure 2 Specific parameter values ​​of mineral powder are shown in Table 1.

[0069] Table 1 Statistics of mineral particle parameters

[0070]

[0071] (2) Experimental equipment

[0072] The present invention adopts the "cold pressing method" to simulate the influence of overburden pressure on the directional arrangement of fine-grained rock particles during diagenetic evolution. The instrument model is HA-YXZB-II. The instrument is divided into two parts: an automatic pressure control system and a hydraulic press. The applied pressure range is 0-60MPa. The rock grinding tool is composed of a base, a cavity, a pressure-bearing layer, etc., and the cavity is a cylinder.

[0073] (3) Experimental process

[0074] According to the mineral composition of shale, 8 different overburden pressure experiments were set. Before the minerals were mixed, the mineral particles were dried and dehydrated, and dried at a constant temperature of 60°C for 24 hours. In order to make the various minerals mixed evenly, a mixing agitator was used to stir them evenly for 30 minutes. After stirring, the mineral particles were uniform in color and loose, without agglomeration.

[0075] During the diagenetic evolution process, the cement plays the role of bonding granular minerals and consolidating diagenesis, and is an indispensable link in the diagenetic process. Therefore, the embodiment of the present invention adopts the addition of artificial binders to replace the cementing effect, and the type of binder is A / B series epoxy adhesive YY4250A / B. First, add YY4250A / B cement to the mixed mineral particles, keep the content of the cement to be about 5% of the weight of the mineral, and make the binder fully adhere to the surface of the mineral particles. Secondly, screen the particles of the uniformly mixed cement so that they can fully pass through the 1000 mesh sieve. The mineral particles after the above steps are loaded into the pressing mold, and the method of "loading layer by layer and gradually pressurizing" is adopted. In order to maintain the consistency of pressure, the sample is loaded into the mold in layers, and the pressure is increased to 10MPa and pressed for 10min after each loading, and the cycle is repeated until the mold is filled.

[0076] (4) Experimental plan

[0077] The present invention analyzes the influence of overburden pressure and mineral composition on particle orientation. However, in the long geological evolution process, time is a particularly critical factor. Therefore, the reasonable determination of compaction time should be the first step of the experimental plan. The experimental process is as follows: Figure 3 shown.

[0078] ① Determination of compaction time

[0079] The sample depth in the embodiment of the present invention is 1235m, and the overlying gravity value is P r =Hρg=1235×2.55×9.8=30.86MPa, so the compaction stress is approximately equal to 31MPa. The experiment selected 8h, 12h, 16h, 20h, 24h, 28h, 32h, 36h, 40h, 44h, 48h, 52h, 56h, and 60h as the compaction time to observe the changes in the microstructure of fine-grained rock under different compaction times. The specific experimental parameters are shown in Table 2.

[0080] The results show that under different compaction times, the particle size, geometric shape, arrangement structure and other parameters of fine-grained rock fluctuate less, especially when the compaction time is greater than 20 hours. Therefore, the compaction time parameter is set to 20 hours in the embodiment of the present invention.

[0081] Table 2 Microstructural parameters of fine-grained rock at different compaction times

[0082]

[0083]

[0084] ② Setting of mineral composition and pressure

[0085] In terms of pressure setting, the overburden pressure calculated according to the following formula is approximately 30-60 MPa (Hu Huafeng et al., 2018).

[0086] P r =Hρg

[0087] Where P r is the overlying stratum pressure, MPa; H is the burial depth, m; g is the gravitational acceleration, 9.8 m / s 2 ; ρ is the average density of the formation, 2.16~2.65g / cm 3 .

[0088] Therefore, the embodiment of the present invention sets eight groups of experiments to analyze the influence of overburden pressure on the microstructure of fine-grained rock (#G1-8), and the pressure is set to 25MPa, 30MPa, 35MPa, 40MPa, 45MPa, 50MPa, 55MPa and 60MPa. In order to explore the influence of different rock phases on the directional arrangement of particles under the same overburden pressure, five groups of experiments (#G4, #G9-12) are set to explore the influence of different rock phases on the directional arrangement of particles (#G4, #G11-12), as shown in Table 3.

[0089] Table 3 Experimental table of the effects of overburden pressure and mineral composition on the microstructure of fine-grained rocks

[0090]

[0091] (5) Particle microstructure comparison

[0092] like Figure 3 The following are FE-SEM images of artificially compacted shale and shale in the formation. From the images, we can see that the microstructural characteristics of artificially compacted shale are highly similar to those of shale in the formation, both in the vertical direction and in the parallel direction.

[0093] 2. Application Examples: In order to prove the creativity and technical value of the technical solution of the present invention, this section provides application examples of the technical solution of the claims on specific products or related technologies.

[0094] First, the method for determining the morphology and displacement evolution of shale particles under simulated gravity provided by the embodiment of the present invention is applied to the evaluation of shale reservoirs, and the changes and evolution stages of the morphology and directional arrangement characteristics of mud shale particles under overlying gravity are clarified, providing analog support materials for the characterization of the internal structure of underground shale reservoirs. Secondly, the test results divide the morphology and displacement evolution process of shale particles, clarify the morphology and arrangement characteristics of mud shale particles at different evolutionary stages and their changing laws, etc.

[0095] 3. Evidence of the effects of the embodiments. The embodiments of the present invention have achieved some positive effects during the development or use process, and indeed have great advantages over the prior art. The following content is described in conjunction with the data, charts, etc. of the test process.

[0096] 1. The influence of overlying rock pressure on the pores and particle shape of fine-grained rocks.

[0097] The artificial core is a column with a diameter of 25 mm and a length of 20 mm. The direction of the arrow in the figure is perpendicular to the bedding plane ( Figure 3 ). The direction of the straight bedding plane was sampled and multi-scale and multi-viewing field scanning electron microscope experiments were carried out. The magnification of the FE-SEM photos was fixed at 5000×, and the splicing field was 7×7. The multi-scale and multi-viewing field splicing photos of the experimental groups #G1 to #G8 are shown in Figure 5 , a total of 392 FE-SEM photos were taken.

[0098] (1) Pore shape

[0099] The experimental results show that the overburden pressure has a negative correlation with the average pore size. As the overburden pressure increases, the average pore size shows a trend of gradually decreasing, and the magnitude of the decrease gradually slows down ( Figure 6 ). When the pressure is initially increased, the average pore diameter changes greatly, with significant fluctuation characteristics, but as the pressure increases further, the change in the average pore diameter tends to be gentle.

[0100] In the early stage of compaction, the pore flatness does not change significantly and fluctuates; in the later stage of compaction, the pore flatness shows a trend of gradual increase, and the pores gradually evolve in a narrow and long direction. This phenomenon may be due to the fact that the fine-grained rock particles were not fully compacted in the early stage, and the particle skeleton has not been destroyed. At this time, the pore changes are small, and the particles are mostly in point-to-face, edge-to-edge, and edge-to-face contact. The pores generated under this contact relationship have various forms. Therefore, the pore flatness value shows irregular changes. With the further increase of the overburden pressure, the particles gradually come into full contact, and the particles are mostly in face-to-face contact. The face-to-face contact structure is conducive to the preservation of narrow and long pores.

[0101] (2) Particle shape

[0102] Table 4 shows the particle size and shape parameter values ​​under different overburden pressures and mineral compositions. The results show that when the overburden pressure is less than 45 MPa, the shape parameters of the particles do not change significantly and are irregular; when the overburden pressure is greater than 45 MPa, the flatness of the particles increases, the roundness decreases, and the angularity weakens.

[0103] In the early stage of compaction, the pore structure changes to adapt to the changes in external pressure. When the pore changes to the limit, the particles will displace and deform to resist the increased pressure. In the early stage of compaction, the change in particle oblateness is less sensitive to pressure and there is almost no significant change. Only when the pressure reaches a certain value, the particle evolution tends to increase flatness, decrease roundness, and reduce angularity ( Figure 8 ).

[0104] Table 4 Particle shape parameters under different overburden pressures and mineral compositions

[0105]

[0106] 2. The influence of overlying rock pressure on the directional arrangement of fine-grained rock particles.

[0107] (1) Directionality of particle arrangement

[0108] In the early stage of compaction, the pore structure bears most of the pressure, while fine-grained rock particles are less sensitive to pressure. When the pore changes are not enough to resist the changes in external pressure, the fine-grained rock particles begin to displace and deform. At this time, the fine-grained rock particles do not show the characteristics of preferential orientation ( Fig. 9 As the overburden pressure increases further, the interaction between particles increases, the reduction of pores restricts the rotation of particles, the aggregation slows down, and the orientation of particles gradually tends to be consistent, showing a directional arrangement distribution feature ( Fig. 9 dh in.

[0109] (2) Structural directional entropy

[0110] a. Granularity fractal dimension

[0111] As the overburden pressure increases, the fractal dimension of the particle size of fine-grained rock shows a trend of gradually decreasing. As the compaction degree of shale increases, the particle size gradually becomes uniform. Under the action of external pressure, the specific gravity of relatively stable particles will gradually increase (rigid particles), while the number of variable particles will relatively decrease (plastic particles), thus forming a relatively stable particle grading pattern that is adapted to the external pressure ( Fig.10 ).

[0112] b. Particle orientation fractal dimension

[0113] With the increase of overburden pressure in the experimental test, the oriented fractal dimension of fine-grained rock particles shows a trend of gradual decrease ( Fig.10 ), the orderliness of particle arrangement is enhanced. In the early stage of compaction, the change range of particle orientation fractal dimension is very significant, and as the overburden pressure increases further, the fractal dimension value begins to decrease slightly.

[0114] c. Pore orientation fractal dimension

[0115] As the overburden pressure increases in the experimental test, the pore orientation fractal dimension fluctuates and generally has a decreasing trend ( Fig.10 The results show that the orientation of the pores gradually tends to be consistent, forming a directional structure perpendicular to the load direction. However, with the increase of overburden stress, the rate of change of the numerical value of the pore orientation fractal dimension is not the same, and the curve shows obvious stages. In the early stage of compaction, the effective stress of the particle skeleton is constantly changing, the fine-grained rock particles have not been destroyed, and the pore structure and orientation change little. In the later stage of compaction, the microstructure of the particles is destroyed under the action of pressure, the pore orientation changes significantly, and the main axis direction of the pore gradually becomes perpendicular to the load direction.

[0116] Based on the values ​​of the above three fractal dimensions, the orientation entropy of the particle structure was calculated. The results show that with the increase of the overburden stress, the orientation of the particles is constantly adjusted, gradually showing the characteristics of preferential orientation, the orientation entropy of the structure decreases, and the degree of directional arrangement increases. In the early stage of compaction, the contact mode between particles is constantly adjusted, resulting in a large change in the orientation of the particles; with the further increase of pressure, the particles are arranged gradually in the same direction, the edge-face connection mode between particles is continuously reduced, and is replaced by a stable face-face connection mode, and the directional arrangement structure is further enhanced, showing the characteristics of preferential orientation.

[0117] During the compaction process, as the effective stress increases, the speed of change of the orientation of the particle arrangement is different, with significant stages. When the overburden pressure is <35MPa, the effective stress acting on the particles is constantly changing, causing their arrangement direction to constantly change and adjust, so the orientation has increased significantly, with a change rate of 3.72 / kPa. When the overburden pressure is >35MPa, as the distance between particles decreases, the pore volume decreases, and the interaction between particles is strengthened, which limits the rotation of the particles. Therefore, the change of the orientation of the particle arrangement slows down, and the result value changes with the pressure change at a rate of 1.08 / kPa ( Fig.11 ).

[0118] 3. Evolution of particle orientation under overburden pressure

[0119] During the compaction process, the influence of overburden pressure on particle microstructure is mainly reflected in the shape of pores and particles and the orientation of particle arrangement. Combined with the above experimental results, the evolution of fine-grained rock can be roughly divided into three stages: pore reduction stage, particle deformation and displacement stage, and slow adjustment stage.

[0120] In the early stage of compaction, when the overburden pressure is small, the pores and particles share the external stress. Compared with the particle skeleton, the pores are more easily compressed and deformed. Therefore, the pores share most of the external stress, and the particles only bear a small part of the stress and undergo slight deformation. At this time, the volume of the pores continues to change, the average pore size and porosity continue to decrease, and the pore shape gradually tends to be flat. In the middle stage of compaction, when the overburden stress increases to the yield stress of the particles, the particle structure is gradually destroyed, resulting in alternating agglomerates or fragmentation, which increases the complexity of the shape. The evolution of this stage is mainly reflected in the changes in the particle shape and the direction of the main axis. At the same time, the morphology of pores and cracks also changes accordingly with the evolution of the particles. With the further increase of the overburden stress, the flatness of the particles increases, and the angularity decreases, but the particles gradually show the characteristics of preferential orientation, and the arrangement tends to be directional. In the late stage of compaction, the porosity is very low, and the particles are difficult to displace and rotate. They adjust slowly or remain basically unchanged (such as Fig.12 shown).

[0121] The above description is only a specific implementation mode of the present invention, but the protection scope of the present invention is not limited thereto. Any modifications, equivalent substitutions and improvements made by any technician familiar with the technical field within the technical scope disclosed by the present invention and within the spirit and principle of the present invention should be covered by the protection scope of the present invention.

Claims

1. A method for measuring the morphology and displacement evolution of shale particles under simulated gravity, characterized in that: The method for determining the shale particle morphology and displacement evolution process under simulated gravity includes: Step 1: extract kerogen from shale core as organic component experimental material, and select brittle mineral and clay mineral powder with purity of more than 90% as inorganic component experimental material; Step 2: Select HA-YXZB-II core preparation instrument as the experimental equipment; Step 3, drying and dehydrating the mineral particles, and uniformly stirring them using a mixing agitator; Step 4: Load the mixed mineral particle layered samples into the mold, press each layer under an overburden pressure of 10 MPa for 10 minutes, and then load the next layer of mineral particles until the mold is filled; Step 5: After compacting the sample for 20 hours, take the sample out of the mold; Step 6: Based on the multi-scale and multi-view scanning electron microscope identification technology, combined with Image J software, the morphological characteristics and particle arrangement degree of the shale sample particles are calculated respectively; The operation process of the Image J software in step 6 is as follows: ① Grayscale transformation: import the target image into the software and transform the image into grayscale; ② Grayscale threshold setting: adjust the image threshold according to the grayscale value of the image, so that the image presents a complete geometric shape of the particle size, keep the threshold concentrated in a stable range, and extract the particles according to the threshold; ③ Automatic denoising: manually correct the image, or remove the noise by filtering and smoothing the image, and use automatic denoising for analysis; ④ Acquisition of geometric parameters: Set an appropriate scale for the image according to the magnification of the scanning electron microscope; calculate the geometric parameters of the particles, including particle size, flatness, perimeter, equivalent elliptical perimeter, convexity, and calibrate and count the particles; ⑤ Export data: export and transform data, save all data output in Excel, and obtain particle geometry information after data processing; the identified information values ​​are divided into particle area, pixel value, X and Y coordinate position, particle perimeter, width, length, height and angle, particle Feret diameter, particle roundness, particle sphericity and convexity parameters; The calculation model of the particle arrangement degree in step 6 is: Based on the influence of pore arrangement structure, the directional entropy of fine-grained rock structure is regarded as a function of particle size entropy, particle arrangement entropy and pore arrangement entropy, which is expressed by the following formula: In the formula, E di is the particle arrangement entropy, which represents the particle orientation fractal dimension value; E pd is the particle size entropy, which indicates the value of the particle size fractal dimension; E bi is the pore arrangement entropy, which represents the value of the pore orientation fractal dimension; The fine-grained rock value is equivalent to the average of the particle arrangement entropy, grain size entropy and pore arrangement entropy, and the weight coefficient is 1 / 3, as shown below: in, The larger the value, the higher the degree of disorder, the more chaotic the arrangement, the more chaotic the arrangement, the more irregular the arrangement, and the more unstable the system. The smaller the value, the lower the degree of disorder, the more directional the arrangement, and the more stable the system.

2. The method for measuring the morphology and displacement evolution of shale particles under simulated gravity as claimed in claim 1, characterized in that: In the step 1, quartz, feldspar, calcite and pyrite are used as brittle mineral experimental materials, and illite, montmorillonite, kaolinite and chlorite are selected as clay mineral experimental materials.

3. The method for measuring the morphology and displacement evolution of shale particles under simulated gravity as claimed in claim 1, characterized in that: The experimental equipment in step 2 is divided into two parts: an automatic pressure control system and a hydraulic press. The applied pressure range is 0-60 MPa. The rock grinding tool consists of a base, a cavity, and a pressure-bearing layer, and the cavity is a cylinder.

4. The method for measuring the morphology and displacement evolution of shale particles under simulated gravity as claimed in claim 1, characterized in that: In the drying and dehydration treatment in step 3, a constant temperature of 60° C. to 80° C. is used for drying for 24 hours.

5. The method for measuring the morphology and displacement evolution of shale particles under simulated gravity as claimed in claim 1, characterized in that: The stirring time of the mixing agitator in step 3 is 30 min.

6. The method for measuring the morphology and displacement evolution of shale particles under simulated gravity as claimed in claim 1, characterized in that: When the sample is loaded into the mold in layers in step 4, the specific steps include: (1) adding a cementing material to the mixed mineral particles; (2) screening the particles of the uniformly mixed cement; (3) Loading the mineral particles after the above steps into a pressing mold, using a layer-by-layer loading and gradual pressurization method.

7. The method for measuring the morphology and displacement evolution of shale particles under simulated gravity as claimed in claim 6, characterized in that: The binder in step (1) is an A / B series epoxy adhesive, the content of the binder is maintained at 5% of the weight of the mineral, and the binder is fully adhered to the surface of the mineral particles.

8. The method for measuring the morphology and displacement evolution of shale particles under simulated gravity as claimed in claim 6, characterized in that: In step (2), the particles are passed through a 1000 mesh sieve.

9. The method for measuring the morphology and displacement evolution of shale particles under simulated gravity as claimed in claim 6, characterized in that: In step (3), when the samples are loaded into the mold layer by layer, the pressure is increased to 10 MPa and pressed for 10 minutes after each loading, and this cycle is repeated until the mold is filled.

10. The method for measuring the morphology and displacement evolution of shale particles under simulated gravity as claimed in claim 1, characterized in that: In step 5, during the compaction of multiple groups of samples for different periods of time, the overburden pressure is calculated according to the following formula: P r =Hρg Where P r is the overlying stratum pressure, in MPa; H is the burial depth, in m; g is the gravitational acceleration, which is 9.8 m / s 2 ; ρ is the average density of the formation, which is 2.16~2.65g / cm 3 .

Citation Information

Patent Citations

  • Experimental method for simulating shale organic pore evolution process

    CN110726655A

  • Shale pore quantitative structure complexity determination method, system, medium and equipment

    CN114371187A