Electrode assembly, manufacturing method and manufacturing system thereof, battery cell, battery and electrical device
By introducing the guide portion and opening structure of the bent section into the electrode assembly, the problem of lithium deposition caused by the deviation of the electrode assembly during the molding process is solved, and the electrochemical performance and safety are improved.
Patent Information
- Application Number
- CN202080102169.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-12-18
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2040-12-18
AI Technical Summary
In existing battery technology, electrode components tend to deviate from their predetermined positions during the molding process, leading to lithium precipitation and affecting electrochemical performance and safety.
An electrode assembly is designed, which includes a bending section with a guide part. The guide part guides the first pole piece to bend in a predetermined area during the bending process, ensuring the controllability and accuracy of the bending position and reducing lithium deposition. Risks are reduced, and the strength and stress concentration of the bending section are reduced through openings, providing enough space to reduce the extrusion force and reduce powder loss.
It effectively reduces the risk of lithium precipitation in the electrode assembly, improves electrochemical performance and safety, and ensures the stability and performance of the battery.
Smart Images

Figure CN115699398B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of battery technology, and more specifically, to an electrode assembly and a manufacturing method and system thereof, a battery cell, a battery, and an electrical device. Background Art
[0002] Rechargeable batteries, also known as secondary batteries, are batteries that can be recharged to activate the active material after the battery is discharged and continue to be used. Rechargeable batteries are widely used in electronic devices such as mobile phones, laptops, battery cars, electric cars, electric airplanes, electric boats, electric toy cars, electric toy boats, electric toy airplanes, and electric tools, etc.
[0003] In the development of battery technology, in addition to improving battery performance, safety is also an issue that cannot be ignored. If the safety of the battery cannot be guaranteed, the battery cannot be used. Therefore, how to enhance the safety of the battery is a technical problem that needs to be solved urgently in battery technology. Summary of the invention
[0004] The present application provides an electrode assembly and a manufacturing method and system thereof, a battery cell, a battery and an electrical device, which can reduce the risk of lithium plating and enhance the safety of the battery.
[0005] In the first aspect, the embodiment of the present application provides an electrode assembly, which includes: a first pole piece, including a plurality of bending sections and a plurality of first stacking sections arranged in layers, each bending section is used to connect two adjacent first stacking sections, and the bending section has a guide portion, and the guide portion is used to guide the bending section to bend during production; a plurality of second pole pieces, the second pole pieces have opposite polarity to the first pole pieces and include a second stacking section, and the second stacking section of each second pole piece is arranged between two adjacent first stacking sections; an isolation film, which is used to separate the first pole piece and the second pole piece, and the isolation film includes a plurality of isolation sections, and each isolation section is arranged between adjacent first stacking sections and second stacking sections. Wherein, in the stacking direction of the plurality of first stacking sections, the thickness of the first stacking section is Da, the thickness of the second stacking section is Dc, and the thickness of the isolation section is Ds; the size of the guide portion in the bending direction of the bending section is w, and w, Da, Dc and Ds satisfy the relationship: Dc+2Ds≤w≤2×(Dc+2Ds+Da).
[0006] In an embodiment of the present application, when the size w of the guide portion satisfies the relationship Dc+2Ds≤w≤2×(Dc+2Ds+Da), the guide portion can guide the first pole piece to bend in a predetermined area, thereby improving the controllability and accuracy of the bending position, reducing the risk of the first pole piece and the second pole piece deviating from the predetermined position, and reducing lithium plating; at the same time, the guide portion can also reduce the stress concentration of the first active material layer on the bending section, provide sufficient space for the second stacking section and the isolation membrane, reduce the extrusion force exerted by the bending section on the second stacking section and the isolation membrane, and reduce powder loss.
[0007] In some embodiments, the guide portion is arranged along a first direction, and the first direction is perpendicular to the bending direction of the bending section.
[0008] In some embodiments, the guide portion includes at least one opening. The opening can reduce the strength of the bending section, making the bending section easier to bend. By providing the opening, at least part of the first active material layer of the bending section is removed to reduce the stress concentration of the first active material layer on the bending section, provide space for the second stacking section and the isolation membrane, reduce the extrusion force applied by the bending section to the second stacking section and the isolation membrane, and reduce powder loss.
[0009] In some embodiments, the opening passes through the bent section. The opening can be formed by punching the first pole piece, and the forming process is simple. The through opening can also reduce the weight of the electrode assembly and improve the energy density of the electrode assembly. The electrolyte can also pass through the opening and infiltrate the second pole piece, thereby improving the wettability of the electrode assembly.
[0010] In some embodiments, the bending section includes a plurality of sub-bending sections, and the sub-bending sections and the openings are alternately arranged along the first direction. By increasing the number of sub-bending sections, the size of the sub-bending sections along the first direction can be reduced, making each sub-bending section easier to bend, which helps guide the folding of the first pole piece.
[0011] In some embodiments, the size of the opening along the first direction is L1, the size of the sub-bending section along the first direction is L2, and 2≤L1 / L2≤40. This can improve the bending effect of the sub-bending section while avoiding the sub-bending section from breaking.
[0012] In some embodiments, the guide portion includes a plurality of openings, and the plurality of openings are spaced apart.
[0013] In some embodiments, a plurality of openings are arranged at intervals along the first direction. Increasing the number of openings can correspondingly increase the number of sub-bending segments, reduce the size of the sub-bending segments along the first direction, make each sub-bending segment easier to bend, and help guide the folding of the first pole piece.
[0014] In some embodiments, the opening is circular, elliptical, racetrack-shaped or polygonal. Optionally, the corners of the polygon are rounded. The rounded corners can make the corners of the polygonal opening smoother and reduce burrs on the first pole piece when the opening is formed.
[0015] In some embodiments, the dimension of the guide portion along the first direction is L3, the dimension of the bending section along the first direction is L4, and 0.5≤L3 / L4≤0.99. This can improve the bending effect of the bending section and the guiding effect of the guide portion while reducing the risk of the bending section breaking.
[0016] In some embodiments, the dimension L4 of the bending section along the first direction is 200 mm-1200 mm. When the dimension L4 of the bending section is 200 mm-1200 mm, the bending effect of the bending section is better.
[0017] In some embodiments, the plurality of bending segments include a first bending segment and a second bending segment, the first bending segment and the second bending segment are respectively connected to two ends of the first stacking segment along the second direction, the spacing L5 between the guide portion on the first bending segment and the guide portion on the second bending segment along the second direction is 80 mm-200 mm, and the second direction is perpendicular to the first direction and the stacking direction. Setting the value of L5 to 80 mm-200 mm can improve the forming effect of the electrode assembly.
[0018] In some embodiments, the first electrode is a negative electrode, and the second electrode is a positive electrode. The first active material layer of the bent section can provide lithium insertion space for lithium ions, thereby reducing the risk of lithium plating.
[0019] In some embodiments, the first pole piece includes a first current collector and a first active material layer disposed on the surface of the first current collector, and the second pole piece includes a second current collector and a second active material layer disposed on the surface of the second current collector. In the stacking direction, the first active material layer of the first stacking section completely covers the second active material layer of the second stacking section. The first active material layer of the first stacking section can provide lithium insertion space for the lithium ions extracted and inserted from the second active material layer, thereby reducing lithium precipitation.
[0020] In some embodiments, in a direction perpendicular to the stacking direction, the first active material layer of the first stacking section exceeds the second active material layer of the second stacking section by at least 0.1 mm. The first active material layer of the first stacking section can provide sufficient lithium insertion space for lithium ions extracted from the second active material layer, thereby reducing the risk of lithium precipitation.
[0021] In some embodiments, each first stacking section has two opposite first edges, and after the bending section is guided to be bent during production, the first edges of two adjacent first stacking sections connected to the bending section are consistent.
[0022] In a second aspect, an embodiment of the present application provides a battery cell, comprising: a shell having a receiving cavity and an opening; at least one electrode assembly of the first aspect, received in the receiving cavity; and a cover plate for closing the opening of the shell.
[0023] In a third aspect, an embodiment of the present application provides a battery, comprising: a casing; and at least one battery cell according to the second aspect, the battery cell being accommodated in the casing.
[0024] In a fourth aspect, an embodiment of the present application provides an electric device, which is configured to receive electric power provided by the battery of the third aspect.
[0025] In a fifth aspect, an embodiment of the present application provides a method for manufacturing an electrode assembly, comprising: providing a first pole piece, the first pole piece comprising a plurality of bending sections and a plurality of first stacking sections, each bending section being used to connect two adjacent first stacking sections, the bending section having a guide portion, the guide portion being used to guide the bending section to bend during production; providing an isolation membrane, and fixing the isolation membrane to two surfaces of the first pole piece, the isolation membrane comprising a plurality of isolation sections; providing a plurality of second pole pieces, the second pole pieces having opposite polarity to the first pole pieces and comprising second stacking sections, and fixing the second pole pieces to the surface of the isolation membrane facing away from the first pole pieces; bending the bending sections under the guidance of the guide portion so that the plurality of first stacking sections are stacked, the second stacking section of each second pole piece is arranged between two adjacent first stacking sections, and each isolation section is arranged between adjacent first stacking sections and second stacking sections. Among them, in the stacking direction of multiple first stacking segments, the thickness of the first stacking segment is Da, the thickness of the second stacking segment is Dc, the thickness of the isolation segment is Ds, and the dimension of the guide portion in the bending direction of the bending section is w, and w, Da, Dc and Ds satisfy the relationship: Dc+2Ds≤w≤2×(Dc+2Ds+Da).
[0026] In a sixth aspect, an embodiment of the present application provides a manufacturing system for an electrode assembly, comprising: a first providing device for providing a first electrode sheet, the first electrode sheet comprising a plurality of bending segments and a plurality of first stacked segments, each bending segment being used to connect two adjacent first stacked segments, the bending segment having a guide portion, the guide portion being used to guide the bending segment to bend during production; a second providing device for providing an isolation membrane, the isolation membrane comprising a plurality of isolation segments; a first assembling device for fixing the isolation membrane to two surfaces of the first electrode sheet; a third providing device for providing a plurality of second electrode sheets, the second electrode sheets having opposite polarity to the first electrode sheets and comprising second stacked segments; a second assembling device for attaching the second electrode sheets to the electrodes; The sheet is fixed to the surface of the isolation membrane away from the first pole piece; a third assembling device is used to bend the bending section under the guidance of the guide part, so that multiple first stacking sections are stacked, the second stacking section of each second pole piece is arranged between two adjacent first stacking sections, and each isolation section is arranged between adjacent first stacking sections and second stacking sections; wherein, in the stacking direction of the multiple first stacking sections, the thickness of the first stacking section is Da, the thickness of the second stacking section is Dc, the thickness of the isolation section is Ds, the dimension of the guide part in the bending direction of the bending section is w, and w, Da, Dc and Ds satisfy the relationship: Dc+2Ds≤w≤2×(Dc+2Ds+Da). BRIEF DESCRIPTION OF THE DRAWINGS
[0027] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments of the present application will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on the drawings without paying creative work.
[0028] Figure 1 A schematic diagram of the structure of a vehicle according to an embodiment of the present application;
[0029] Figure 2 This is a schematic diagram of the structure of a battery according to an embodiment of the present application;
[0030] Figure 3 This is a schematic diagram of the structure of a battery module according to an embodiment of the present application;
[0031] Figure 4 A schematic diagram of the structure of a battery cell according to an embodiment of the present application;
[0032] Figure 5 A front view schematic diagram of an electrode assembly according to an embodiment of the present application;
[0033] Figure 6 for Figure 5 A schematic cross-sectional view of the electrode assembly shown along line AA;
[0034] Figure 7for Figure 5 A schematic cross-sectional view of the electrode assembly shown along line BB;
[0035] Figure 8 for Figure 6 An enlarged schematic diagram of the electrode assembly shown at box C;
[0036] Fig. 9 This is a schematic structural diagram of a first electrode sheet of an electrode assembly in a folded state according to an embodiment of the present application;
[0037] Fig.10 This is a schematic structural diagram of a first electrode sheet of an electrode assembly in an unfolded state according to an embodiment of the present application;
[0038] Fig.11 This is a schematic structural diagram of a first electrode sheet of an electrode assembly in another embodiment of the present application in an unfolded state;
[0039] Figures 12 to 16 A schematic diagram of an electrode assembly during a forming process according to an embodiment of the present application;
[0040] Fig.17 A partial cross-sectional schematic diagram of an electrode assembly according to an embodiment of the present application;
[0041] Fig.18 A partial cross-sectional schematic diagram of an electrode assembly according to an embodiment of the present application;
[0042] Fig.19 A schematic flow chart of a method for manufacturing an electrode assembly according to an embodiment of the present application;
[0043] Fig. 20 The present invention is a schematic block diagram of a battery cell manufacturing system according to an embodiment of the present application.
[0044] In the drawings, the drawings are not drawn to scale. DETAILED DESCRIPTION
[0045] In order to make the purpose, technical solution and advantages of the embodiments of the present application clearer, the technical solution in the embodiments of the present application will be clearly described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0046] Unless otherwise defined, all technical and scientific terms used in this application have the same meanings as those commonly understood by technicians in the technical field of this application; the terms used in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application; the terms "including" and "having" in the specification and claims of this application and the above-mentioned drawings and any variations thereof are intended to cover non-exclusive inclusions. The terms "first", "second", etc. in the specification and claims of this application or the above-mentioned drawings are used to distinguish different objects, rather than to describe a specific order or a primary and secondary relationship.
[0047] Reference to "embodiments" in this application means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described in this application may be combined with other embodiments.
[0048] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", and "attached" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0049] The term "and / or" in this application is only a description of the association relationship of associated objects, indicating that there can be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this application generally indicates that the associated objects before and after are in an "or" relationship.
[0050] The term "multiple" as used in the present application refers to more than two (including two). Similarly, "multiple groups" refers to more than two groups (including two groups), and "multiple sheets" refers to more than two sheets (including two sheets).
[0051] In the present application, the term "parallel" includes not only the absolutely parallel situation, but also the roughly parallel situation conventionally recognized in engineering; meanwhile, "vertical" includes not only the absolutely vertical situation, but also the roughly vertical situation conventionally recognized in engineering.
[0052] In the present application, battery cells may include lithium-ion secondary batteries, lithium-ion primary batteries, lithium-sulfur batteries, sodium-lithium-ion batteries, sodium-ion batteries or magnesium-ion batteries, etc., and the embodiments of the present application do not limit this. Battery cells may be cylindrical, flat, rectangular or other shapes, etc., and the embodiments of the present application do not limit this. Battery cells are generally divided into three types according to the packaging method: cylindrical battery cells, square battery cells and soft-pack battery cells, and the embodiments of the present application do not limit this.
[0053] The battery mentioned in the embodiments of the present application refers to a single physical module including one or more battery cells to provide higher voltage and capacity. For example, the battery mentioned in the present application may include a battery module or a battery pack. The battery generally includes a box for encapsulating one or more battery cells. The box can prevent liquid or other foreign matter from affecting the charging or discharging of the battery cells.
[0054] The battery cell includes an electrode assembly and an electrolyte. The electrode assembly is composed of a positive electrode sheet, a negative electrode sheet and a separator. The battery cell mainly relies on the movement of metal ions between the positive electrode sheet and the negative electrode sheet to work. The positive electrode sheet includes a positive current collector and a positive active material layer. The positive active material layer is coated on the surface of the positive current collector. The current collector not coated with the positive active material layer protrudes from the current collector coated with the positive active material layer. The current collector not coated with the positive active material layer serves as the positive electrode tab. Taking lithium-ion batteries as an example, the material of the positive current collector can be aluminum, and the positive active material can be lithium cobalt oxide, lithium iron phosphate, ternary lithium or lithium manganese oxide, etc. The negative electrode sheet includes a negative current collector and a negative active material layer. The negative active material layer is coated on the surface of the negative current collector. The current collector not coated with the negative active material layer protrudes from the current collector coated with the negative active material layer. The current collector not coated with the negative active material layer serves as the negative electrode tab. The material of the negative current collector can be copper, and the negative active material can be carbon or silicon, etc. In order to ensure that a large current can pass without melting, there are multiple positive electrode tabs stacked together, and multiple negative electrode tabs stacked together. The separator has a large number of through-holes, which can ensure the free passage of electrolyte ions and has good permeability to lithium ions. The material of the separator can be PP or PE. The development of battery technology must consider many design factors at the same time, such as performance parameters such as energy density, cycle life, discharge capacity, charge and discharge rate, and battery safety.
[0055] When a lithium-ion battery is charged, lithium ions are deintercalated from the positive electrode and embedded in the negative electrode. However, some abnormal situations may occur, such as insufficient lithium embedding space in the negative electrode, too much resistance for lithium ions to embed in the negative electrode, or too fast deintercalation of lithium ions from the positive electrode. The deintercalated lithium ions cannot be equally embedded in the negative electrode active material layer of the negative electrode. The lithium ions that cannot be embedded in the negative electrode can only obtain electrons on the surface of the negative electrode, thereby forming a silvery-white metallic lithium single substance. This is the lithium precipitation phenomenon. Lithium precipitation not only reduces the performance of lithium-ion batteries and greatly shortens the cycle life, but also limits the fast charging capacity of lithium-ion batteries. In addition, when lithium ion batteries undergo lithium precipitation, the precipitated lithium metal is very active and can react with the electrolyte at a lower temperature, causing the battery's self-heating starting temperature (Tonset) to decrease and the self-heating rate to increase, seriously endangering the safety of the battery. Furthermore, when lithium precipitation is severe, the deintercalated lithium ions can form lithium crystals on the surface of the negative electrode, and the lithium crystals can easily puncture the isolation membrane, causing the adjacent positive and negative electrode sheets to have the risk of short circuit.
[0056] After noticing the problem of poor electrochemical performance of existing battery cells, the inventors found that it was because at least one of the positive and negative pole pieces in the formed electrode assembly deviated from the predetermined position, thus affecting the electrochemical performance of the electrode assembly. The inventors further found that at least one of the positive and negative pole pieces in the formed electrode assembly deviated from the predetermined position, resulting in lithium precipitation in the electrode assembly, thereby affecting the electrochemical performance of the secondary battery. It is speculated that the reason may be that the negative active material layer cannot completely cover the positive active material layer, resulting in the inability of the deintercalated lithium ions to be equally embedded in the negative active material layer of the negative pole piece.
[0057] In view of this, the present application intends to provide an electrode assembly, which can place the positive electrode plate and the negative electrode plate in a predetermined position, reduce the risk of lithium plating, ensure that the electrode assembly has good electrochemical properties, and improve the safety of the battery.
[0058] The technical solutions described in the embodiments of the present application are applicable to various devices that use batteries, such as mobile phones, portable devices, laptop computers, electric vehicles, electric toys, electric tools, electric vehicles, ships and spacecraft, for example, spacecraft include airplanes, rockets, space shuttles and spacecraft, etc.
[0059] It should be understood that the technical solutions described in the embodiments of the present application are not limited to the devices described above, but can also be applied to all devices using batteries. However, for the sake of simplicity, the following embodiments are described using electric vehicles as examples.
[0060] For example, Figure 1As shown, it is a structural schematic diagram of a vehicle 1 according to an embodiment of the present application. The vehicle 1 may be a fuel vehicle, a gas vehicle or a new energy vehicle. The new energy vehicle may be a pure electric vehicle, a hybrid vehicle or an extended-range vehicle, etc. A battery 10, a controller 20 and a motor 30 may be arranged inside the vehicle 1, and the controller 20 is used to control the battery 10 to supply power to the motor 30. For example, a battery 10 may be arranged at the bottom, front or rear of the vehicle 1. The battery 10 may be used to power the vehicle 1. For example, the battery 10 may be used as an operating power source for the vehicle 1, for the circuit system of the vehicle 1, for example, for the working power requirements during the start-up, navigation and operation of the vehicle 1. In another embodiment of the present application, the battery 10 may not only be used as an operating power source for the vehicle 1, but also as a driving power source for the vehicle 1, replacing or partially replacing fuel or natural gas to provide driving power for the vehicle 1.
[0061] In order to meet different power requirements, the battery 10 may include a plurality of battery cells, wherein the plurality of battery cells may be connected in series, in parallel, or in a hybrid connection, wherein the hybrid connection refers to a mixture of series and parallel connections. The battery 10 may also be referred to as a battery pack. Optionally, a plurality of battery cells may be connected in series, in parallel, or in a hybrid connection to form a battery module, and a plurality of battery modules may be connected in series, in parallel, or in a hybrid connection to form the battery 10. In other words, a plurality of battery cells may directly form the battery 10, or may first form a battery module, and then the battery module may form the battery 10.
[0062] For example, Figure 2 As shown in FIG. 1 , it is a schematic diagram of the structure of a battery 10 according to an embodiment of the present application. The battery 10 may include a plurality of battery cells 40. The battery 10 may also include a box (or a cover), the interior of the box is a hollow structure, and the plurality of battery cells 40 are accommodated in the box. Figure 2 As shown, the box body may include two parts, which are respectively referred to as the first part 111 and the second part 112, and the first part 111 and the second part 112 are buckled together. The shapes of the first part 111 and the second part 112 may be determined according to the shapes of the combination of multiple battery cells 40, and the first part 111 and the second part 112 may both have an opening. For example, the first part 111 and the second part 112 may both be hollow cuboids and each has only one face as an opening face, the opening of the first part 111 and the opening of the second part 112 are arranged opposite to each other, and the first part 111 and the second part 112 are buckled together to form a box body with a closed chamber. Multiple battery cells 40 are connected in parallel, in series, or in a mixed combination and are placed in the box body formed by the buckling of the first part 111 and the second part 112.
[0063] Optionally, the battery 10 may also include other structures, which are not described one by one here. For example, the battery 10 may also include a busbar component, which is used to realize electrical connection between multiple battery cells 40, such as parallel connection, series connection or mixed connection. Specifically, the busbar component can realize electrical connection between battery cells 40 by connecting the electrode terminals of the battery cells 40. Further, the busbar component can be fixed to the electrode terminals of the battery cells 40 by welding. The electrical energy of multiple battery cells 40 can be further led out through the box through a conductive mechanism. Optionally, the conductive mechanism may also belong to the busbar component.
[0064] The number of battery cells 40 can be set to any value according to different power requirements. Multiple battery cells 40 can be connected in series, parallel or mixed to achieve a larger capacity or power. Since the number of battery cells 40 included in each battery 10 may be large, for ease of installation, the battery cells 40 can be grouped, and each group of battery cells 40 constitutes a battery module. The number of battery cells 40 included in the battery module is not limited and can be set according to requirements. For example, Figure 3 The battery 10 may include a plurality of battery modules, which may be connected in series, in parallel or in a mixed manner.
[0065] like Figure 4 As shown, it is a schematic diagram of the structure of a battery cell 40 of an embodiment of the present application. The battery cell 40 of the embodiment of the application includes an electrode assembly 50, a shell 60 and an end cap assembly 70, the shell 60 has a receiving cavity and an opening, and the electrode assembly 50 is received in the receiving cavity. The shell 60 is determined according to the shape of one or more electrode assemblies 50 after being combined. For example, the shell 60 can be a hollow cuboid or a cube or a cylinder, and one of the faces of the shell 60 has an opening so that one or more electrode assemblies 50 can be placed in the shell 60. For example, when the shell 60 is a hollow cuboid or a cube, one of the planes of the shell 60 is an open surface, that is, the plane does not have a wall body so that the shell 60 communicates with the inside and outside. The end cap assembly 70 includes a cover plate 71, which covers the opening and is connected to the shell 60, thereby closing the opening of the shell 60, so that the electrode assembly 50 is placed in the closed cavity. The shell 60 is filled with an electrolyte, such as an electrolyte.
[0066] The end cap assembly 70 may further include two electrode terminals 72, which may be disposed on the cover plate 71. The cover plate 71 is generally in the shape of a flat plate, and the two electrode terminals 72 are fixed on the flat surface of the cover plate 71, and the two electrode terminals 72 are respectively a positive electrode terminal and a negative electrode terminal. Each electrode terminal 72 is provided with a corresponding connecting member 73, or may also be referred to as a current collecting member, which is used to electrically connect the electrode assembly 50 and the electrode terminal 72.
[0067] Each electrode assembly 50 has a first pole tab 513 and a second pole tab 523. The polarities of the first pole tab 513 and the second pole tab 523 are opposite. For example, when the first pole tab 513 is a positive pole tab, the second pole tab 523 is a negative pole tab. The first pole tab 513 of one or more electrode assemblies 50 is connected to one electrode terminal 72 through a connecting member 73, and the second pole tab 523 of one or more electrode assemblies 50 is connected to another electrode terminal 72 through another connecting member 73. For example, the positive electrode terminal is connected to the positive pole tab through one connecting member 73, and the negative electrode terminal is connected to the negative pole tab through another connecting member 73.
[0068] In the battery cell 40 , the electrode assembly 50 can be provided as a single one or multiple ones according to actual use requirements.
[0069] like Figure 5 , which is a front view schematic diagram of an electrode assembly 50 according to an embodiment of the present application; Figure 6 for Figure 5 The electrode assembly 50 is shown as a cross-sectional schematic diagram taken along line AA; Figure 7 for Figure 5 The schematic cross-sectional view of the electrode assembly 50 shown is made along line BB; Figure 8 for Figure 6 An enlarged schematic diagram of the electrode assembly 50 at box C is shown.
[0070] like Figures 5 to 8 As shown, the electrode assembly 50 of the embodiment of the present application includes a first pole piece 51, a second pole piece 52 and a separator 53, and the separator 53 is used to separate the first pole piece 51 from the second pole piece 52. The second pole piece 52 has an opposite polarity to the first pole piece 51. For example, when the first pole piece 51 is a negative pole piece, the second pole piece 52 is a positive pole piece, and when the first pole piece 51 is a positive pole piece, the second pole piece 52 is a negative pole piece.
[0071] The first pole piece 51 includes a first current collector 51a and a first active material layer 51b disposed on the surface of the first current collector 51a. The first current collector 51a includes a first coating area and a first protruding area, the first coating area is coated with the first active material layer 51b, the first protruding area protrudes from the first coating area, and the first protruding area is at least partially not coated with the first active material layer 51b. The portion of the first protruding area that is not coated with the first active material layer 51b is used to connect to the connecting member 73, that is, the first protruding area serves as the first pole lug 513.
[0072] The second pole piece 52 includes a second current collector 52a and a second active material layer 52b disposed on the surface of the second current collector 52a. The second current collector 52a includes a second coating area and a second protruding area, the second coating area is coated with the second active material layer 52b, the second protruding area protrudes from the second coating area, and the second protruding area is at least partially uncoated with the second active material layer 52b. The portion of the second protruding area that is not coated with the second active material layer 52b is used to connect to the connecting member 73, that is, the second protruding area serves as a second pole lug 523.
[0073] The first pole tab 513 and the second pole tab 523 are usually formed by a cutting process. In some embodiments, the second pole piece 52 further includes a protective coating 52c, which is applied to the surface of the second current collector 52a and connected to the second active material layer 52b, and the protective coating 52c is located on the side of the second active material layer 52b close to the second protruding area. A portion of the protective coating 52c is applied to the second coating area, and another portion of the protective coating 52c is applied to the second protruding area. The area of the second protruding area not covered by the protective coating 52c is used to connect to the connecting member 73. The protective coating 52c can reduce the burrs at the cutting position during the cutting process of the second pole tab 523.
[0074] The first pole piece 51 includes a plurality of bending sections 511 and a plurality of first stacking sections 512 arranged in a stacked manner, and each bending section 511 is used to connect two adjacent first stacking sections 512. In this embodiment, the first pole piece 51 is a continuous extension structure as a whole, and is generally reciprocatingly bent in a Z-shape. The plurality of first stacking sections 512 are stacked in sequence along the stacking direction Z.
[0075] In the electrode assembly 50, the bending section 511 is at least partially in a bending state. In some examples, the bending section 511 is in a bending state as a whole, and the bending section 511 is generally arc-shaped, for example, it can be a circular arc. In other examples, the bending section 511 is only partially in a bending state; specifically, the bending section 511 has an arc region 5111 and a straight region 5112, the arc region 5111 is bent as a whole into an arc shape, for example, it can be a circular arc shape, and the straight region 5112 is in a flat plate shape and connects the arc region 5111 and the first stacked section 512.
[0076] In some embodiments, the first stacking section 512 is in the shape of a flat plate as a whole and is perpendicular to the stacking direction Z. In other embodiments, the end of the first stacking section 512 connected to the bending section 511 may also be in a bent state.
[0077] The second pole pieces 52 are provided in plurality. Each second pole piece 52 includes a second stacking section 522, and the second stacking section 522 of each second pole piece 52 is provided between two adjacent first stacking sections 512. The plurality of second pole pieces 52 are separated from each other. The second stacking section 522 is generally in the shape of a plate and is perpendicular to the stacking direction Z, and the stacking direction Z is parallel to the thickness direction of the first stacking section 512 and the thickness direction of the second stacking section 522.
[0078] The isolation film 53 includes a plurality of isolation segments 531, each of which is disposed between adjacent first stacking segments 512 and second stacking segments 522. The isolation segments 531 can insulate and separate the adjacent first stacking segments 512 and second stacking segments 522 to reduce the risk of short circuit. The isolation segments 531 are parallel to the first stacking segments 512 and second stacking segments 522, and the thickness direction of the isolation segments 531 is parallel to the stacking direction Z. In some embodiments, the isolation film 53 also includes a connecting segment 532 disposed on both inner and outer sides of each bending segment 511, and the connecting segment 532 is used to connect the two isolation segments 531. The connecting segment 532 can insulate and separate the bending segment 511 and the second stacking segment 522 to reduce the risk of short circuit. Optionally, there are two isolation films 53, and each isolation film 53 is reciprocally bent in a Z shape to form an isolation segment 531 and a connecting segment 532.
[0079] The first pole tabs 513 extend from the edge of the first stacked section 512, and the second pole tabs 523 extend from the edge of the second stacked section 522. In some examples, the number of first pole tabs 513 is the same as the number of first stacked sections 512, and the first pole tabs 513 and the first stacked sections 512 are arranged in a one-to-one correspondence. The number of second pole tabs 523 is the same as the number of second stacked sections 522, and the second pole tabs 523 and the second stacked sections 522 are arranged in a one-to-one correspondence.
[0080] By analyzing the forming process of the electrode assembly, the inventor further studied the lithium precipitation phenomenon and found that the first pole piece is a continuous structure as a whole, and it is difficult to bend along the predetermined area during the bending process, resulting in the first pole piece and the second pole piece After the electrode assembly is stacked, there is a situation where the negative electrode active material layer cannot completely cover the positive electrode active material layer, which is easy to cause lithium precipitation in the electrode assembly, thereby affecting the electrochemical performance and safety performance of the secondary battery. In addition, when the first pole piece is bent, the first active material layer on the bending section will produce stress concentration, causing the active material to fall off, which is called powdering. The space between the bending section and the second stacking section is limited, so there may be a situation where the bending section squeezes the edge of the second stacking section, which will also cause the second active material layer on the second stacking section to fall off; at the same time, the bending section may also squeeze the isolation membrane, causing the isolation membrane between the bending section and the second stacking section to wrinkle.
[0081] Based on the above problems found by the inventors, the inventors improved the structure of the first pole piece.
[0082] Specifically, in some embodiments, the bending section 511 has a guide portion 514, and the guide portion 514 is used to guide the bending section 511 to bend during production. During the production process of the electrode assembly 50, when an external force is applied to the first pole piece 51 to bend the first pole piece 51, the guide portion 514 can guide the first pole piece 51 to bend in a predetermined area to form the bending section 511, which is conducive to improving the controllability and accuracy of the bending position, thereby reducing the risk of the first pole piece 51 and the second pole piece 52 deviating from the predetermined position, reducing the possibility that the negative electrode active material layer in the first stacking section 512 and the second stacking section 522 cannot completely cover the positive electrode active material layer, reducing lithium plating, and improving the electrochemical performance of the electrode assembly 50.
[0083] In some embodiments, the number of guide portions 514 may be the same as the number of bending segments 511, and the guide portions 514 and the bending segments 511 are arranged in a one-to-one correspondence. Of course, in other embodiments, a portion of the bending segments 511 among all the bending segments 511 are provided with guide portions 514, while the other bending segments 511 may not be provided with guide portions 514.
[0084] The guide portion 514 may be a trace left by something. Optionally, the guide portion 514 may refer to a structure formed by removing part of the first active material layer 51b on the first pole piece 51 through a material removal component, or the guide portion 514 may refer to a structure formed by removing part of the first active material layer 51b and part of the first current collector 51a on the first pole piece 51 through a material removal component. By providing the guide portion 514, the strength of the bending section 511 can be reduced, so that the bending section 511 is easier to bend. The first active material layer 51b itself has a certain degree of brittleness, and there is a possibility of powder falling due to stress concentration during the bending process. By opening a guide portion 514 on the bending section 511, part of the first active material layer 51b on the bending section 511 can be removed, thereby reducing the stress concentration of the first active material layer 51b on the bending section 511; at the same time, by opening a guide portion 514 on the bending section 511, space can be provided for the second stacking section 522 and the isolation membrane 53, thereby reducing the extrusion force exerted by the bending section 511 on the second stacking section 522 and the isolation membrane 53, thereby reducing powder loss.
[0085] The bending section 511 extends between two adjacent first stacking sections 512. The bending section 511 is parallel to the first direction X, and the first direction X is perpendicular to the stacking direction Z. Specifically, the bending section 511 extends along the bending direction S shown in the figure, and the bending direction S can be understood as a direction parallel to the surface of the bending section 511. The bending direction S is perpendicular to the first direction X.
[0086] The guide portion 514 is conducive to improving the controllability and accuracy of the bending position, thereby reducing the risk of the first pole piece 51 and the second pole piece 52 deviating from the predetermined position. The inventors further found that the size of the guide portion 514 along the bending direction S has a direct impact on the bending position of the first pole piece 51.
[0087] Specifically, if the dimension of the guide portion 514 along the bending direction S is too small, then during the bending and stacking process of the first pole piece 51, the guiding effect of the guide portion 514 is limited, which increases the possibility that the first pole piece 51 is not bent in the predetermined area, causing the risk of the first stacked section 512 deviating from the predetermined position. In addition, the effect of the guide portion 514 in reducing the stress concentration of the first active material layer 51b of the bending section 511 is not obvious, and the bending section 511 still has the risk of powder falling. The space provided by the guide portion 514 for the second stacked section 522 and the isolation membrane 53 is relatively small, and the extrusion force applied by the bending section 511 to the second stacked section 522 and the isolation membrane 53 is relatively large, and the second stacked section 522 still has the risk of powder falling.
[0088] If the guide portion 514 is too large in the bending direction S, the easily bendable area of the first pole piece 51 is too large, which will increase the probability that the first pole piece 51 is not bent in the predetermined area, causing the risk of the first stacking section 512 deviating from the predetermined position, resulting in serious deformation of the electrode assembly 50. At the same time, if the guide portion 514 is too large in the bending direction S, the guide portion 514 may extend to one side of the second pole piece 52 along the stacking direction Z. At this time, the guide portion 514 cannot provide lithium insertion space for the lithium ions extracted from the first pole piece 51, causing the risk of lithium precipitation.
[0089] In view of this, the inventors further improved the structure of the first pole piece 51. Specifically, in the stacking direction Z, the thickness of the first stacking section 512 is Da, the thickness of the second stacking section 522 is Dc, and the thickness of the isolation section 531 is Ds; the size of the guide portion 514 in the bending direction S is w. Among them, w, Da, Dc and Ds satisfy the relationship: Dc+2Ds≤w≤2×(Dc+2Ds+Da). Optionally, the value of Da is 0.11mm-0.25mm, the value of Dc is 0.16mm-0.3mm, and the value of Ds is 0.009mm-0.02mm.
[0090] Through research and experiments, the inventors found that when the size w of the guide portion 514 satisfies the above relationship, the guide portion 514 can guide the first pole piece 51 to bend in a predetermined area, improve the controllability and accuracy of the bending position, reduce the risk of the first pole piece 51 and the second pole piece 52 deviating from the predetermined position, and reduce lithium plating; at the same time, the guide portion 514 can also reduce the stress concentration of the first active material layer 51b on the bending section 511, provide sufficient space for the second stacking section 522 and the isolation membrane 53, reduce the extrusion force exerted by the bending section 511 on the second stacking section 522 and the isolation membrane 53, and reduce powder loss.
[0091] In the bending direction S, the size of the bending section 511 is associated with the size w of the guide portion 514. Specifically, in some examples, in the bending direction S, the size w of the guide portion 514 is equal to the size of the bending section 511. In other words, the bending section 511 and the first stacking section 512 can be defined according to the edge of the guide portion 514 in the bending direction S.
[0092] In some embodiments, the first electrode sheet 51 is a negative electrode sheet, and the second electrode sheet 52 is a positive electrode sheet. The first active material layer 51b of the bent section 511 can provide lithium insertion space for lithium ions, thereby reducing the risk of lithium deposition.
[0093] In some embodiments, in the stacking direction Z, the first active material layer 51b of the first stacking section 512 completely covers the second active material layer 52b of the second stacking section 522. Here, "completely covering" means that in a plane perpendicular to the stacking direction Z, the orthographic projection of the second active material layer 52b of the second stacking section 522 is completely located within the orthographic projection of the first active material layer 51b of the first stacking section 512. At this time, the projection area of the second active material layer 52b of the second stacking section 522 is smaller than the projection area of the first active material layer 51b of the first stacking section 512.
[0094] The first active material layer 51 b of the first stacked section 512 can provide lithium insertion space for lithium ions extracted from the second active material layer 52 b , thereby reducing lithium plating.
[0095] In some embodiments, in a direction perpendicular to the stacking direction Z, the first active material layer 51b of the first stacking section 512 exceeds the second active material layer of the second stacking section 522 by at least 0.1 mm. Specifically, in the first direction X, the first active material layer 51b of the first stacking section 512 exceeds the second active material layer of the second stacking section 522 by at least 0.1 mm; in the second direction Y, the first active material layer 51b of the first stacking section 512 exceeds the second active material layer of the second stacking section 522 by at least 0.1 mm. The second direction Y is perpendicular to the first direction X and the stacking direction Z. At this time, the first active material layer 51b of the first stacking section 512 can provide sufficient lithium insertion space for the lithium ions extracted and inserted from the second active material layer 52b, thereby reducing lithium precipitation.
[0096] Fig. 9 This is a schematic structural diagram of a first electrode sheet 51 of an electrode assembly 50 in a folded state according to an embodiment of the present application; Fig.10 This is a schematic diagram of the structure of the first electrode sheet 51 of the electrode assembly 50 in an embodiment of the present application in an unfolded state. Fig.10 The dotted line in the figure does not represent a physical structure, but schematically shows the dividing line between the bending section 511 and the first stacking section 512 .
[0097] When the first pole piece 51 is in the unfolded state, the first pole piece 51 extends along its own length direction H, and the first stacked sections 512 and the bent sections 511 are alternately arranged along the length direction H. Each bent section 511 connects two adjacent first stacked sections 512. When the first pole piece 51 is in the folded state, the dimension w of the guide portion 514 along the bending direction S is: the dimension of the guide portion 514 along the length direction H when the first pole piece 51 is in the unfolded state. When the first pole piece 51 is in the unfolded state, the first direction X is parallel to the width direction of the first pole piece 51 itself.
[0098] In some embodiments, the guide portion 514 includes at least one opening 514a. The opening 514a is formed on the bending section 511 by removing a portion of the material of the bending section 511. The opening 514a can reduce the strength of the bending section 511, making the bending section 511 easier to bend. By providing the opening 514a, at least part of the first active material layer of the bending section 511 is removed to reduce the stress concentration of the first active material layer on the bending section 511, provide space for the second stacking section and the isolation membrane, reduce the extrusion force applied by the bending section 511 to the second stacking section and the isolation membrane, and reduce powder loss.
[0099] In some embodiments, the opening 514a may be a blind hole; in other words, the opening 514a is a groove that does not penetrate the bent section 511. In some examples, the opening 514a is recessed relative to the surface of the bent section 511 facing the second stacked section. Optionally, the opening 514a is formed by removing part of the first active material layer, and the opening 514a extends to the first current collector and exposes the first current collector.
[0100] In some embodiments, the opening 514a is a through hole and passes through the bending section 511. The opening 514a passes through the first current collector of the bending section 511 and the first active material layer on both sides of the first current collector. The opening 514a can be formed by punching the first pole piece 51, and the molding process is simple. The through opening 514a can reduce the stress concentration of the first active material layer on the bending section 511, provide sufficient space for the second stacking section and the isolation membrane, reduce the extrusion force applied by the bending section 511 to the second stacking section and the isolation membrane, and reduce powder loss. The through opening 514a can also reduce the weight of the electrode assembly and increase the energy density of the electrode assembly. The electrolyte can also pass through the opening 514a and infiltrate the second pole piece, thereby improving the wettability of the electrode assembly.
[0101] In some embodiments, the bending section 511 includes a plurality of sub-bending sections 511a, and the sub-bending sections 511a and the openings 514a are alternately arranged along the first direction X. Each sub-bending section 511a connects two adjacent first stacked sections 512. By increasing the number of sub-bending sections 511a, the size of the sub-bending sections 511a along the first direction X can be reduced, making each sub-bending section 511a easier to bend, which helps guide the folding of the first pole piece 51.
[0102] When the opening 514a is a through hole, the multiple sub-bending sections 511a are separated from each other. When the opening 514a is a blind hole, the bending section 511 also includes a sub-connecting section, which is the bottom wall of the opening 514a and connects two adjacent sub-bending sections 511a.
[0103] In some embodiments, the size of the opening 514a along the first direction X is L1, and the size of the sub-bending section 511a along the first direction X is L2. The size of the first pole piece 51 along the first direction X is constant. The larger the value of L1, the smaller the value of L2, and the easier it is for the sub-bending section 511a to bend. Correspondingly, the lower the strength of the sub-bending section 511a, the easier it is to break during the bending process; conversely, the smaller the value of L1, the larger the value of L2, the more difficult it is for the sub-bending section 511a to bend, and the worse the guiding effect of the sub-bending section 511a. The inventor comprehensively considered the bending effect and strength of the sub-bending section 511a, and after research and experiments, found that when 2≤L1 / L2≤40, the bending effect of the sub-bending section 511a can be improved while avoiding the sub-bending section 511a from breaking. Optionally, the values of L1 / L2 are 10, 20 and 30.
[0104] In some embodiments, the guide portion 514 includes a plurality of openings 514a, and the plurality of openings 514a are arranged at intervals. Optionally, the plurality of openings 514a are arranged at intervals along the first direction X. Increasing the number of openings 514a can correspondingly increase the number of sub-bending segments 511a, reduce the size of the sub-bending segments 511a along the first direction X, make each sub-bending segment 511a easier to bend, and help guide the folding of the first pole piece 51.
[0105] In some embodiments, the opening 514a is circular, elliptical, racetrack-shaped or polygonal. It is noted that the above-mentioned shape refers to the shape of the opening 514a when the first pole piece 51 is in the expanded state. In some examples, the corners of the polygonal opening 514a are rounded; the rounded corners can make the corners of the polygonal opening 514a smoother, and the burrs on the first pole piece 51 can be reduced when the opening 514a is formed. For example, the opening 514a is generally rectangular and has four rounded corners. When the first pole piece 51 is in the expanded state, the size of the opening 514a along the first direction X is greater than the size of the opening 514a along the length direction H.
[0106] The dimension of the guide portion 514 along the first direction X is L3. Specifically, when the guide portion 514 includes only one opening 514a, L3 is equal to L1. When the guide portion 514 includes multiple openings 514a, L3 is equal to the sum of the dimensions L1 of the multiple openings 514a along the first direction X.
[0107] The dimension of the bending section 511 along the first direction X is L4. The dimension L4 of the bending section 511 along the first direction X is equal to the dimension L4 of the first stacking section 512 along the first direction X. Each first stacking section 512 has two opposite first edges 5121, and the first edges 5121 are located at both ends of the first stacking section 512 along the first direction X. In the first direction X, the distance between the two first edges 5121 is equal to L4. When the first pole piece 51 is in the unfolded state, the value of L4 is the width of the first pole piece 51. The dimension L4 of the bending section 511 is equal to the sum of the dimensions L1 of all openings 514a and the dimensions L2 of all sub-bending sections 511a.
[0108] In some embodiments, the larger the value of L3 / L4, the easier the bending section 511 is to bend, the better the guiding effect, and the higher the risk of the bending section 511 breaking during the bending process; conversely, the smaller the value of L3 / L4, the more difficult the bending section 511 is to bend, the worse the guiding effect, and the higher the strength of the bending section 511, the less likely it is to break during the bending process. The inventors comprehensively considered the bending effect and strength of the sub-bending section 511a, and after research and experiments, found that when 0.5≤L3 / L4≤0.99, the bending effect of the bending section 511 and the guiding effect of the guiding part can be improved while reducing the risk of the bending section 511 breaking. Optionally, the values of L3 / L4 are 0.6, 0.7, 0.8 and 0.9.
[0109] The smaller L4 is, the lower the strength of the bending section 511 is; when L4 is too small, the guiding effect of the guide portion 514 is not obvious. The larger L4 is, the more difficult it is to ensure that both ends of the bending section 511 are bent synchronously along the first direction X. After research and experiments, the inventors found that when the size L4 of the bending section 511 is 200mm-1200mm, the bending effect of the bending section 511 is better.
[0110] In some embodiments, the plurality of bending segments 511 include a first bending segment and a second bending segment, the first bending segment and the second bending segment are respectively connected to the two ends of the first stacking segment 512 along the second direction Y, the spacing L5 between the guide portion 514 on the first bending segment and the guide portion 514 on the second bending segment along the second direction Y is 80mm-200mm, and the second direction Y is perpendicular to the first direction X and the stacking direction Z. When the first pole piece 51 is in the unfolded state, the spacing between the guide portions 514 of two adjacent bending segments 511 along the length direction H of the first pole piece 51 is L5. In some examples, the value of L5 is equal to the size of the first stacking segment 512 along the second direction Y.
[0111] During the folding process of the first pole piece 51, if a certain bending section 511 deviates slightly from the set position due to accident, the first stacking section 512 connected to the bending section 511 may be deflected. In this case, the first edge 5121 of the first stacking section 512 forms a certain angle with the second direction Y. The larger the value of L5, the greater the maximum value of the first edge 5121 deviating from the predetermined position in the first direction X. Under the premise that the capacity of the electrode assembly 50 is certain, the smaller L5 is, the more layers of the first pole piece 51 are folded, and the higher the possibility that the first stacking section 512 deviates from the set position. After research and experiments, the inventor set the value of L5 to 80mm-200mm, which can improve the molding effect of the electrode assembly 50.
[0112] In some embodiments, after the first pole piece 51 is bent under the guidance of the guide portion 514, the first edges 5121 of the two adjacent first stacking sections 512 connected to the bent section 511 are consistent. In a plane perpendicular to the stacking direction Z, the orthographic projections of the first edges 5121 of the same side of the two adjacent first stacking sections 512 coincide, and the first edges 5121 of the two adjacent first stacking sections 512 are considered to be consistent. Of course, due to process errors, in a plane perpendicular to the stacking direction Z, there may also be an angle between the orthographic projections of the first edges 5121 of the two adjacent first stacking sections 512. As long as the first active material layer 51b of the first stacking section 512 can completely cover the second active material layer 52b of the second stacking section 522 in the stacking direction Z, the first edges 5121 of the two adjacent first stacking sections 512 are considered to be consistent. This angle is called the allowable error angle.
[0113] Fig.11 FIG. 5 is a schematic structural diagram of a first electrode sheet 51 of an electrode assembly 50 in another embodiment of the present application in an unfolded state. Fig.11 As shown, in some embodiments, the bending section 511 includes two openings 514a and one sub-bending section 511a. The sub-bending section 511a connects two adjacent first stacking sections 512. The two openings 514a are respectively located on both sides of the sub-bending section 511a along the first direction X. The ends of each opening 514a along the first direction X are open. In other embodiments, the bending section 511 may also include only one opening 514a and one sub-bending section 511a, and the opening 514a and the sub-bending section 511a are arranged along the first direction X.
[0114] Hereinafter, the above aspects of the present disclosure are described in more detail with reference to examples. However, these examples are exemplary and the present disclosure is not limited thereto.
[0115] (Preparation of Electrode Assembly)
[0116] Example 1:
[0117] (i) Graphite, a negative electrode active material, or a mixture of graphite and other active materials in different mass ratios, acetylene black as a conductive agent, CMC as a thickener, and SBR as a binder are mixed in a mass ratio of 96.4:1:1.2:1.4, deionized water as a solvent is added, and the mixture is stirred in a vacuum mixer until the system is uniform to obtain a negative electrode slurry; the negative electrode slurry is evenly coated on a copper foil, dried at room temperature, and then transferred to an oven for further drying, and then cold pressed, slit, and cut to obtain a first electrode sheet 51. After the negative electrode slurry is dried and solidified, a first active material layer 51b is formed.
[0118] (ii) Using a laser or a die cutting tool, an opening 514 a is formed on the first pole piece 51 . The opening 514 a penetrates the first pole piece 51 . Fig.12FIG. 5 is a schematic diagram of the first pole piece 51 after the opening 514a is formed. Fig.12 As shown, the first pole piece 51 includes a first stacking section 512 and a bending section 511 alternately arranged along the length direction H, each bending section 511 includes four sub-bending sections 511a and three openings 514a, and the sub-bending sections 511a and the openings 514a are alternately arranged along the first direction X. The size L1 of each opening 514a along the first direction X is 160mm, and the size L2 of each sub-bending section 511a along the first direction X is 20mm. The size of the bending section 511 and the first stacking section 512 along the first direction X is 560mm. The size of the first stacking section 512 in the length direction H of the first pole piece 51 is 88mm. The size w of the bending section 511, the sub-bending section 511a and the opening 514a in the length direction H is 0.3mm. The thickness Da of the first stacking section 512 and the thickness of the bending section 511 are both 0.18mm. The first stacking section 512 has two first edges 5121 disposed opposite to each other along the first direction X and two second edges 5122 disposed opposite to each other in the length direction H. The opening 514a is disposed adjacent to the second edge 5122. Fig.12 The dotted line in the figure does not represent a physical structure, but can be schematically used as the second edge 5122 of the first stacking section 512. The first edge 5121 and the second edge 5122 are also the edges of the first active material layer 51b. The tab 513 extends from a first edge 5121. There are 41 first stacking sections 512 and 40 bending sections 511.
[0119] (iii) Two isolation films 53 are provided, and the two isolation films 53 are fixed to two surfaces of the first pole piece 51 respectively. Fig.13 Schematic diagram of the structure of the first pole piece 51 and the isolation film 53 fixed together. The isolation film 53 can be fixed to the first pole piece 51 by hot pressing, electrophoresis or bonding. The isolation film 53 is a polyethylene film. The thickness Ds of the isolation film 53 is 0.01 mm.
[0120] (iv) The positive electrode active material NCM523, the conductive agent acetylene black, and the binder PVDF are mixed in a mass ratio of 96:2:2, and the solvent NMP is added. The mixture is stirred in a vacuum mixer until the system is uniform to obtain a positive electrode slurry; the binder PVDF, the insulating material aluminum oxide, and the solvent are mixed together to prepare a protective slurry; the positive electrode slurry and the protective slurry are evenly coated on the aluminum foil, dried at room temperature, and then transferred to an oven for further drying, and then cold pressed, slit, and cut into pieces to obtain the second electrode sheet 52. After the positive electrode slurry is cured, the second active material layer 52b is formed, and after the protective slurry is cured, the protective coating 52c is formed.
[0121] (v) Fix the plurality of second pole pieces 52 onto the isolation film 53 . Fig.14FIG. 5 is a schematic diagram of a strip-shaped electrode assembly 50a, showing a first electrode sheet 51, a second electrode sheet 52 and a separator 53 fixed together. The plurality of second electrode sheets 52 may be arranged in accordance with Fig.14 The second pole piece 52 is arranged in the manner shown. The second pole piece 52 can be fixed to the isolation film 53 by heat pressing, electrophoresis or bonding. Fig.15 FIG. 1 is a partial top view of a strip-shaped electrode assembly 50a, which shows a first electrode sheet 51, a second electrode sheet 52 and a separator 53 fixed together. Fig.15 As shown, the second pole piece 52 includes a second stacking section 522 and a second pole ear 523 connected to the second stacking section 522. The second stacking section 522 includes a third edge 5221 and a fourth edge 5222 arranged opposite to each other along the first direction, and the second pole ear 523 extends from the fourth edge 5222. Along the first direction X, the size of the second stacking section 522 is 558.5 mm. Specifically, in the first direction X, one first edge 5121 of the first stacking section 512 exceeds the third edge by 1.5 mm, and the other first edge 5121 of the first stacking section 512 is flush with the fourth edge 5222. The size of the portion of the protective coating 52c on the second stacking section 522 along the first direction X is 1.5 mm. That is, in the first direction X, both first edges 5121 of the first stacking section 512 exceed the second active material layer by 1.5 mm. The size of the second stacked section 522 along the length direction H is 86 mm, and the second stacked section 522 has two fifth edges 5223 arranged opposite to each other in the length direction H. In the length direction H, the distance between the fifth edge 5223 and the second edge 5122 of the first stacked section 512 is 1 mm. The thickness Dc of the second stacked section 522 is 0.25 mm. There are 40 second pole pieces 52.
[0122] (vi) The strip-shaped electrode assembly 50a is folded. Fig.16 The schematic diagram of the strip electrode assembly 50a during the folding process is shown. For example, the strip electrode assembly 50a can be pulled above the forming mold 50b, and after entering the cavity of the forming mold 50b, the strip electrode assembly 50a is folded under the action of gravity. Other auxiliary components can also be used to help the strip electrode assembly 50a bend.
[0123] (vii) After folding, the formed electrode assembly is heat-pressed and fixed with tape.
[0124] Example 2: An electrode assembly was manufactured according to the same method as Example 1, except that the dimension w of the opening 514a in the length direction H was changed to 0.27 mm.
[0125] Example 3: An electrode assembly was manufactured according to the same method as Example 1, except that the dimension w of the opening 514a in the length direction H was changed to 0.4 mm.
[0126] Example 4: An electrode assembly was manufactured according to the same method as Example 1, except that the dimension w of the opening 514a in the length direction H was changed to 0.5 mm.
[0127] Example 5: An electrode assembly was manufactured according to the same method as Example 1, except that the dimension w of the opening 514a in the length direction H was changed to 0.6 mm.
[0128] Example 6: An electrode assembly was manufactured according to the same method as Example 1, except that the dimension w of the opening 514a in the length direction H was changed to 0.7 mm.
[0129] Example 7: An electrode assembly was manufactured according to the same method as Example 1, except that the dimension w of the opening 514a in the length direction H was changed to 0.8 mm.
[0130] Example 8: An electrode assembly was manufactured according to the same method as Example 1, except that the dimension w of the opening 514a in the length direction H was changed to 0.9 mm.
[0131] Comparative Example 1: An electrode assembly was manufactured according to the same method as Example 1, except that the dimension w of the opening 514a in the length direction H was changed to 0.1 mm.
[0132] Comparative Example 2: An electrode assembly was manufactured according to the same method as Example 1, except that the dimension w of the opening 514a in the length direction H was changed to 0.2 mm.
[0133] Comparative Example 3: An electrode assembly was manufactured according to the same method as Example 1, except that the dimension w of the opening 514a in the length direction H was changed to 1 mm.
[0134] Comparative Example 4: An electrode assembly was manufactured according to the same method as Example 1, except that the dimension w of the opening 514a in the length direction H was changed to 1.2 mm.
[0135] Evaluation example: Evaluate the relative position of an edge of a first stacked segment and an edge of a second stacked segment.
[0136] Electrode assemblies according to Examples 1 to 8 and Comparative Examples 1 to 4 were manufactured and evaluated.
[0137] The positions of the respective edges of the first laminated sections and the positions of the respective edges of the second laminated sections in Examples 1-8 and Comparative Examples 1-4 were detected using an X-ray CT scanner.
[0138] Fig.17 FIG. 1 is a partial cross-sectional schematic diagram of an electrode assembly according to an embodiment of the present application. Fig.17As shown, based on the image detected by the scanner, the minimum distance D11 between the third edge 5221 of each second stacking segment 522 and a first edge 5121 of the corresponding first stacking segment 512 in the first direction X is calculated. Wherein, D11 is the dimension of an edge of the first active material layer exceeding an edge of the second active material layer in the first direction X. Each second stacking segment 522 is compared with the first stacking segments 512 on both sides thereof to obtain 80 values.
[0139] According to the image detected by the scanner, the minimum distance D12a between the fourth edge 5222 of each second stacking segment 522 and the other first edge 5121 of the corresponding first stacking segment 512 in the first direction X is calculated. D12a plus 1.5 mm is the dimension D12 of the other edge of the first active material layer exceeding the other edge of the second active material layer in the first direction X. Each second stacking segment 522 is compared with the first stacking segments 512 on both sides thereof to obtain 80 values.
[0140] Fig.18 FIG. 1 is another partial cross-sectional schematic diagram of an electrode assembly according to an embodiment of the present application. Fig.18 As shown, based on the image detected by the scanner, the minimum distance D13 between the fifth edge 5223 of each second stacking segment 522 and the second edge 5122 of the corresponding first stacking segment 512 in the first direction X is calculated. Each second stacking segment 522 is compared with the first stacking segments 512 on both sides thereof to obtain 160 values.
[0141] Wherein, D11 is a positive value, which means that one edge of the first active material layer exceeds one edge of the second active material layer in the first direction X; D11 is a negative value, which means that one edge of the second active material layer exceeds one edge of the first active material layer in the first direction X. The same is true for D12 and D13.
[0142] The evaluation results of Examples 1-8 and Comparative Examples 1-4 are shown in Table 1.
[0143] w D11 minimum D12 minimum D13 minimum Example 1 0.3mm 0.23mm 0.25mm 0.68mm Example 2 0.27mm 0.19mm 0.20mm 0.70mm Example 3 0.4mm 0.37mm 0.35mm 0.61mm Example 4 0.5mm 0.54mm 0.56mm 0.52mm Example 5 0.6mm 0.76mm 0.71mm 0.45mm Example 6 0.7mm 0.56mm 0.53mm 0.34mm Example 7 0.8mm 0.33mm 0.34mm 0.26mm Example 8 0.9mm 0.20mm 0.22mm 0.20mm Comparative Example 1 0.1mm -0.03mm -0.01mm 0.81mm Comparative Example 2 0.2mm 0.09mm 0.07mm 0.74mm Comparison Example 3 1.0mm 0.08mm 0.09mm 0.09mm Comparison Example 4 1.2mm -0.01mm -0.02mm -0.03mm
[0144] As shown in Table 1, for the electrode assemblies of Examples 1-8, the value of w is within 0.27mm-09mm, which satisfies the relationship Dc+2Ds≤w≤2×(Dc+2Ds+Da), and the first active material layer of the first stacking section can exceed the predetermined size of the second active material layer of the second stacking section, and the first active material layer of the first stacking section can completely cover the second active material layer of the second stacking section, providing sufficient lithium insertion space for lithium ions and reducing lithium precipitation. In Comparative Examples 1-4, the value of w is too large or too small, which may prevent the first active material layer of the first stacking section from completely exceeding the second active material layer of the second stacking section, or the first active material layer of the first stacking section exceeds the second active material layer of the second stacking section by too small a size; compared with Examples 1-8, the electrode assembly in Comparative Examples 1-4 has a higher risk of lithium precipitation. Therefore, compared with the electrode assembly in Comparative Examples 1-4, the electrode assembly in Examples 1-8 has better electrochemical performance and higher safety.
[0145] Fig.19 FIG. 1 is a schematic flow chart of a method for manufacturing an electrode assembly according to an embodiment of the present application. Fig.19 As shown, the manufacturing method includes:
[0146] S810, providing a first pole piece, the first pole piece comprising a plurality of bending segments and a plurality of first stacked segments, each bending segment being used to connect two adjacent first stacked segments, the bending segment having a guide portion, the guide portion being used to guide the bending segment to bend during production;
[0147] S820, providing an isolation membrane, and fixing the isolation membrane to two surfaces of the first pole piece, wherein the isolation membrane includes a plurality of isolation segments;
[0148] S830, providing a plurality of second pole pieces, wherein the second pole pieces have opposite polarities to the first pole pieces and include second stacked sections, and fixing the second pole pieces to a surface of the isolation film that is away from the first pole pieces;
[0149] S840 Bend the bending section under the guidance of the guide part so that a plurality of first stacking sections are stacked, the second stacking section of each second pole piece is arranged between two adjacent first stacking sections, and each isolation section is arranged between adjacent first stacking sections and second stacking sections. Wherein, in the stacking direction of the plurality of first stacking sections, the thickness of the first stacking section is Da, the thickness of the second stacking section is Dc, the thickness of the isolation section is Ds, the dimension of the guide part in the bending direction of the bending section is w, and w, Da, Dc and Ds satisfy the relationship: Dc+2Ds≤w≤2×(Dc+2Ds+Da).
[0150] The relevant structure of the electrode assembly manufactured by the manufacturing method of this embodiment can refer to the aforementioned Figure 1-18 The relevant contents of the electrode assembly described in the corresponding embodiment will not be repeated here.
[0151] Fig. 20 FIG. 1 is a schematic block diagram of a battery cell manufacturing system according to an embodiment of the present application. Fig. 20 As shown, the manufacturing system 900 includes a first providing device 910, a second providing device 920, a first assembling device 930, a third providing device 940, a second assembling device 950 and a third assembling device 960. The first providing device 910 is used to provide a first pole piece, the first pole piece includes a plurality of bending segments and a plurality of first stacking segments, each bending segment is used to connect two adjacent first stacking segments, the bending segment has a guide portion, and the guide portion is used to guide the bending segment to bend during production. The second providing device 920 is used to provide an isolation membrane, the isolation membrane includes a plurality of isolation segments. The first assembling device 930 is used to fix the isolation membrane to the two surfaces of the first pole piece. The third providing device 940 is used to provide a plurality of second pole pieces, the second pole pieces have opposite polarity to the first pole pieces and include a second stacking segment. The second assembling device 950 is used to fix the second pole piece to the surface of the isolation membrane facing away from the first pole piece. The third assembly device 960 is used to bend the bending section under the guidance of the guide part, so that multiple first stacking sections are stacked, the second stacking section of each second pole piece is arranged between two adjacent first stacking sections, and each isolation section is arranged between adjacent first stacking sections and second stacking sections. Wherein, in the stacking direction of the multiple first stacking sections, the thickness of the first stacking section is Da, the thickness of the second stacking section is Dc, the thickness of the isolation section is Ds, the dimension of the guide part in the bending direction of the bending section is w, and w, Da, Dc and Ds satisfy the relationship: Dc+2Ds≤w≤2×(Dc+2Ds+Da).
[0152] The relevant structure of the electrode assembly manufactured by the manufacturing system of this embodiment can refer to the aforementioned Figure 1-18 The relevant contents of the electrode assembly described in the corresponding embodiment will not be repeated here.
[0153] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit it. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein, but these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present application.
Claims
1. An electrode assembly, characterized in that: include: A first pole piece, comprising a plurality of bending segments and a plurality of first stacked segments, each of the bending segments being used to connect two adjacent first stacked segments, the bending segments having a guide portion, the guide portion being used to guide the bending segments to bend during production; A plurality of second pole pieces, wherein the second pole pieces have opposite polarities to the first pole pieces and include second stacked sections, and the second stacked section of each second pole piece is disposed between two adjacent first stacked sections; An isolation film, used to separate the first pole piece from the second pole piece, the isolation film comprising a plurality of isolation segments, each isolation segment being arranged between adjacent first stacked segments and second stacked segments; Wherein, in the stacking direction of the plurality of first stacking segments, the thickness of the first stacking segment is Da, the thickness of the second stacking segment is Dc, and the thickness of the isolation segment is Ds; The dimension of the guide portion in the bending direction of the bending section is w, and w, Da, Dc and Ds satisfy the relationship: Dc+2Ds≤w≤2×(Dc+2Ds+Da).
2. The electrode assembly according to claim 1, characterized in that: The guide portion is arranged along a first direction, and the first direction is perpendicular to a bending direction of the bending section.
3. The electrode assembly according to claim 2, characterized in that: The guide portion includes at least one opening.
4. The electrode assembly according to claim 3, characterized in that: The opening passes through the bending section.
5. The electrode assembly according to claim 3 or 4, characterized in that: The bending section includes a plurality of sub-bending sections, and the sub-bending sections and the openings are alternately arranged along the first direction.
6. The electrode assembly according to claim 5, characterized in that: The size of the opening along the first direction is L1, the size of the sub-bending section along the first direction is L2, and 2≤L1 / L2≤40.
7. The electrode assembly according to claim 3, characterized in that: The guide portion includes a plurality of openings, and the plurality of openings are arranged at intervals.
8. The electrode assembly according to claim 7, characterized in that: The plurality of openings are spaced apart along the first direction.
9. The electrode assembly according to claim 3, characterized in that: The opening is circular, elliptical, racetrack-shaped or polygonal.
10. The electrode assembly according to claim 2, characterized in that: The dimension of the guide portion along the first direction is L3, the dimension of the bending section along the first direction is L4, and 0.5≤L3 / L4≤0.
99.
11. The electrode assembly according to claim 10, characterized in that: A dimension L4 of the bending section along the first direction is 200 mm-1200 mm.
12. The electrode assembly according to claim 2, characterized in that: The multiple bending sections include a first bending section and a second bending section, the first bending section and the second bending section are respectively connected to the two ends of the first stacking section along the second direction, the spacing L5 between the guide portion on the first bending section and the guide portion on the second bending section along the second direction is 80mm-200mm, and the second direction is perpendicular to the first direction and the stacking direction.
13. The electrode assembly according to claim 1, characterized in that: The first pole piece is a negative pole piece, and the second pole piece is a positive pole piece.
14. The electrode assembly according to claim 13, characterized in that: The first pole piece includes a first current collector and a first active material layer disposed on a surface of the first current collector, and the second pole piece includes a second current collector and a second active material layer disposed on a surface of the second current collector; In the stacking direction, the first active material layer of the first stacking section completely covers the second active material layer of the second stacking section.
15. The electrode assembly according to claim 14, characterized in that: In a direction perpendicular to the stacking direction, the first active material layer of the first stacking section exceeds the second active material layer of the second stacking section by at least 0.1 mm.
16. The electrode assembly according to claim 1, characterized in that Each of the first stacking sections has two opposite first edges. After the bending section is guided to be bent during production, the first edges of two adjacent first stacking sections connected to the bending section are consistent.
17. A battery cell, characterized in that: include: A housing having a receiving cavity and an opening; At least one electrode assembly according to any one of claims 1 to 16, accommodated in the accommodating cavity; as well as The cover plate is used to close the opening of the shell.
18. A battery, characterized in that: include: Box; At least one battery cell as claimed in claim 17, wherein the battery cell is accommodated in the box.
19. An electrical device, characterized in that: The power-consuming device is configured to receive power supplied from the battery of claim 18.
20. A method for manufacturing an electrode assembly, characterized in that: include: Providing a first pole piece, the first pole piece comprising a plurality of bending segments and a plurality of first stacked segments, each of the bending segments being used to connect two adjacent first stacked segments, the bending segment having a guide portion, the guide portion being used to guide the bending segment to bend during production; Providing an isolation film, and fixing the isolation film on two surfaces of the first pole piece, wherein the isolation film includes a plurality of isolation segments; Providing a plurality of second pole pieces, wherein the second pole pieces have opposite polarities to the first pole pieces and include second stacked sections, and fixing the second pole pieces to a surface of the isolation film that is away from the first pole pieces; Bend the bent section under the guidance of the guide portion, so that a plurality of first stacking sections are stacked, the second stacking section of each second pole piece is arranged between two adjacent first stacking sections, and each isolation section is arranged between adjacent first stacking sections and second stacking sections; Among them, in the stacking direction of multiple first stacking segments, the thickness of the first stacking segment is Da, the thickness of the second stacking segment is Dc, the thickness of the isolation segment is Ds, and the dimension of the guide portion in the bending direction of the bending segment is w, and w, Da, Dc and Ds satisfy the relationship: Dc+2Ds≤w≤2×(Dc+2Ds+Da).
21. A manufacturing system for an electrode assembly, characterized in that: include: A first providing device, used for providing a first pole piece, wherein the first pole piece comprises a plurality of bending segments and a plurality of first stacking segments, each of the bending segments is used for connecting two adjacent first stacking segments, and the bending segment has a guiding portion, and the guiding portion is used for guiding the bending segment to bend during production; A second providing device, for providing an isolation membrane, wherein the isolation membrane comprises a plurality of isolation segments; A first assembling device, used for fixing the isolation film to two surfaces of the first pole piece; A third providing device, for providing a plurality of second pole pieces, wherein the second pole pieces have opposite polarities to the first pole pieces and include second stacked sections; A second assembly device, used for fixing the second pole piece to a surface of the isolation film facing away from the first pole piece; The third assembly device is used to bend the bending section under the guidance of the guide part, so that multiple first stacking sections are stacked, the second stacking section of each second pole piece is arranged between two adjacent first stacking sections, and each isolation section is arranged between adjacent first stacking sections and second stacking sections; wherein, in the stacking direction of multiple first stacking sections, the thickness of the first stacking section is Da, the thickness of the second stacking section is Dc, the thickness of the isolation section is Ds, the dimension of the guide part in the bending direction of the bending section is w, and w, Da, Dc and Ds satisfy the relationship: Dc+2Ds≤w≤2×(Dc+2Ds+Da).
Citation Information
Patent Citations
Lithium ion battery and battery core thereof
CN103579684A
Lithium battery and preparation method thereof
CN110071331A