Light board forming method, backlight module and display device
Through the lens mounting part and optical part of the curable hot melt silicone integrated molding, the problem of long assembly process cycle and low yield of Micro LED lamp panels is solved, and more efficient preparation and more reliable positioning are achieved, and product quality is improved.
Patent Information
- Application Number
- CN202111144226.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-09-28
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2041-09-28
AI Technical Summary
The assembly process cycle of existing Micro LED lamp panels is long and has low yield, which is prone to problems of unstable bonding or misalignment.
The lens mounting part and optical part that is integrally formed with curable hot melt silicone is covered on the light emitting element and the reflective layer. It is cured by heating and cooling treatment to achieve corresponding position and reliable positioning of the optical part and the light emitting element, and shorten the preparation period. And improve assembly yield.
The preparation cycle of the lamp plate is shortened, the assembly yield is improved, the correct correspondence and positioning of the optical part and the light-emitting element are ensured, and the incidence of lens installation errors is reduced.
Smart Images

Figure CN115877607B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of display technology, and in particular to a lamp panel molding method, a backlight module and a display device. Background Art
[0002] Micro-Light Emitting Diode (Micro LED) display technology refers to a display technology that uses self-luminous micron-sized Micro LED chips as light-emitting pixel units and assembles them on a substrate to form a high-density Micro LED array.
[0003] The Micro LED light board includes a substrate, a Micro LED chip array and a micro lens array. The Micro LED chip array is mounted on the substrate, the micro lens array covers the Micro LED chip array, and the micro lenses cover the Micro LED chips one by one. In the related art, each micro lens is independently prepared and formed by a glue dripping process, and each formed micro lens is then bonded to the substrate by a pre-applied glue on the substrate surrounding the circumference of the Micro LED chip, and covers the outer surface of the Micro LED chip one by one.
[0004] However, the lamp panel assembly method in the above technical solution has a long preparation process cycle and a low assembly yield. Summary of the invention
[0005] In view of the above problems, the embodiments of the present invention provide a lamp board molding method, a backlight module and a display device, which shorten the lamp board preparation cycle and improve the assembly yield of the lamp board.
[0006] In order to achieve the above purpose, the embodiment of the present invention provides the following technical solutions:
[0007] A first aspect of an embodiment of the present invention provides a method for forming a light board, wherein the light board includes a board body, a light-emitting element, and a lens, wherein the lens includes a mounting portion and an optical portion, wherein the mounting portion is used to be connected to the board body, and the method for forming the light board includes:
[0008] The liquid curable hot-melt silicone is heated to obtain a cured optical part; the liquid curable hot-melt silicone is coated on the light incident side of the optical part, and the liquid curable hot-melt silicone is cooled to obtain a mounting part in an intermediate state, wherein the mounting part in the intermediate state is connected to the optical part; the mounting part is covered on the reflective layer of the plate body, so that the optical part and the plate body are respectively located on both sides of the mounting part, and the optical part corresponds to the light-emitting element; the mounting part is heated to be liquefied by the heat and deposited on the reflective layer and then solidified.
[0009] In this way, the optical part and the mounting part of the lens are integrally formed, and the mounting part covers and adheres to the light-emitting element and the reflective layer, so that the position of the optical part corresponds to the position of the light-emitting element, thereby realizing the assembly of the optical part and the light-emitting element and shortening the preparation cycle; and the contact area between the mounting part and the reflective layer is large, the lens can be reliably positioned by relying on the mounting part, and defects such as lens installation misalignment or inadequate installation are not likely to occur, thereby improving the product yield.
[0010] In some embodiments, the heating of the liquid curable hot-melt silicone to obtain a cured optical part includes: heating to 150°C-200°C under vacuum conditions and maintaining the temperature for 20 minutes-120 minutes to cure the optical part. The vacuum conditions can degas the curable hot-melt silicone to avoid affecting the refractive index of the lens.
[0011] The cooling of the liquid curable hot-melt silicone to obtain a mounting portion in an intermediate state includes: cooling to 50°C-130°C and maintaining a constant temperature for 6 minutes-8 minutes to reduce the flow rate of the curable hot-melt silicone and obtain a mounting portion in an intermediate state; so as to facilitate the transfer of the mounting portion and the optical portion as a whole.
[0012] The mounting portion is heated to liquefy the mounting portion and solidify after being deposited on the reflective layer, comprising: heating to 150°C-200°C under vacuum conditions to liquefy the mounting portion, and maintaining the temperature for 20 minutes-120 minutes to solidify the mounting portion. The vacuum conditions can degas the curable hot-melt silicone to avoid affecting the refractive index of the lens.
[0013] In some embodiments, the reflective layer is formed by curing reflective ink, a avoidance area is provided on the reflective layer, and the light-emitting element is located in the avoidance area. In this way, by spraying reflective ink on the board body, a reflective layer can be formed on the board body for reflecting light, which is easy to shape, and the production cost of the light board is low and the production cycle is short.
[0014] In some embodiments, the reflective layer includes a plurality of sub-reflective layers, and the plurality of sub-reflective layers are stacked and arranged, and the reflectivity of the reflective layer is relatively high.
[0015] In some embodiments, the plurality of sub-reflection layers include a first sub-reflection layer and a second sub-reflection layer, the first sub-reflection layer is coated on the plate body, and the second sub-reflection layer is coated on the surface of the first sub-reflection layer; the first sub-reflection layer is provided with a first avoidance area, and the second sub-reflection layer is provided with a second avoidance area, and the radial dimension of the second avoidance area is greater than the radial dimension of the first avoidance area. In this way, a preset reflectivity can be achieved with a smaller number of sub-reflection layers, thereby reducing the manufacturing cost.
[0016] In some embodiments, the curable hot-melt silicone includes an organosilicon polymer and an associating agent, and the mass ratio of the organosilicon polymer to the associating agent is 8:1-15:1, wherein the organosilicon polymer and the associating agent can form the curable hot-melt silicone by a catalyst.
[0017] In some embodiments, the thickness of the mounting portion is 0.01 mm-1.5 mm to be suitable for different types of light emitting elements.
[0018] In some embodiments, the light emitting element comprises a micron-sized light emitting diode element, and the micron-sized light emitting diode element is welded and fixed to the plate, that is, the light emitting element can be a micron-sized light emitting diode chip or a micron-sized light emitting diode element with a package structure.
[0019] In some embodiments, the light-emitting element includes a sub-millimeter light-emitting diode element and a packaging colloid, the sub-millimeter light-emitting diode element is welded on the board, the packaging colloid covers and is bonded to the outer surface of the sub-millimeter light-emitting diode element, and particles for reducing the relative density of light intensity are bonded to the packaging colloid corresponding to the top surface of the sub-millimeter light-emitting diode element. The light-emitting element can select a packaged sub-millimeter light-emitting diode element.
[0020] A second aspect of an embodiment of the present invention provides a backlight module, which includes a back plate for support and protection.
[0021] The backlight module further includes a reflector; a light board assembly, the light board assembly includes a plurality of light boards made by the light board molding method described in the first aspect, and the plurality of light boards are arranged in parallel on the front side of the backboard; the reflector includes a first reflector and a second reflector, the first reflector is arranged between two adjacent light boards, and the second reflector is arranged on the outer side of the light board assembly in the circumferential direction, so as to avoid light leakage at the joint between two adjacent light boards and at the edge of the light board assembly in the circumferential direction.
[0022] In some embodiments, the reflective element is a reflective sheet with a relatively simple structure.
[0023] And / or, the reflective element is a reflective coating formed by curing reflective ink, which is easy to shape.
[0024] A third aspect of the embodiments of the present invention provides a display device, which includes the backlight module described in the second aspect. By adopting the backlight module, the assembly cycle of the light board and the display device can be reduced and the assembly yield can be improved.
[0025] In addition to the technical problems solved by the embodiments of the present invention described above, the technical features that constitute the technical solutions, and the beneficial effects brought about by the technical features of the technical solutions, other technical problems that can be solved by the lamp board forming method, backlight module and display device provided by the embodiments of the present invention, other technical features included in the technical solutions, and the beneficial effects brought about by these technical features will be further described in detail in the specific implementation methods. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] In order to more clearly illustrate the technical solutions in the embodiments of the present invention or related technologies, the following briefly introduces the drawings required for use in the embodiments or related technical descriptions. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0027] Figure 1 A process flow chart of a method for forming a light panel provided by an embodiment of the present invention;
[0028] Figure 2 A schematic diagram of a method for forming a light board according to an embodiment of the present invention;
[0029] Figure 3 for Figure 2 A cross-sectional view of the center light panel;
[0030] Figure 4 A schematic diagram of curing principle of curable hot-melt silicone provided in an embodiment of the present invention;
[0031] Figure 5 A graph showing the storage modulus and loss modulus of a curable hot-melt silicone rubber provided in an embodiment of the present invention;
[0032] Figure 6 A graph showing the surface adhesion and peel strength characteristics of the curable hot-melt silicone provided in an embodiment of the present invention;
[0033] Figure 7 for Figure 2 Another structural diagram of the middle light board;
[0034] Figure 8 for Figure 7 Schematic diagram of the forming process of the middle light board;
[0035] Fig. 9 for Figure 7 Schematic diagram of reflected light from the middle reflective layer;
[0036] Fig.10 for Figure 2 A schematic diagram of the structure of the light emitting element;
[0037] Fig.11for Figure 2 Another structural schematic diagram of the light emitting element;
[0038] Fig.12 An exploded view of a backlight module provided by an embodiment of the present invention;
[0039] Fig.13 for Fig.12 A cross-sectional view of the backlight module;
[0040] Fig.14 for Fig.13 The structural diagram of part A in the figure;
[0041] Fig.15 for Fig.12 Another structural schematic diagram of the backlight module;
[0042] Fig.16 for Fig. 9 A schematic diagram of the structure of the light board assembly;
[0043] Fig.17 for Fig. 9 Another structural schematic diagram of the light board assembly in FIG.
[0044] Fig.18 Another structural schematic diagram of a backlight module provided by an embodiment of the present invention;
[0045] Fig.19 Another structural schematic diagram of a backlight module provided by an embodiment of the present invention;
[0046] Fig. 20 Another structural schematic diagram of a backlight module provided by an embodiment of the present invention.
[0047] Reference numerals:
[0048] 100: light board;
[0049] 110: plate body; 111: positioning hole; 112: support pillar; 113: pad;
[0050] 120: light emitting element; 121: micron-sized light emitting diode element; 1211: P electrode; 1212: N electrode; 1213: P-type gallium nitride; 1214: N-type gallium nitride; 1215: light emitting area; 1216: sapphire; 1217: chip bump; 122: sub-millimeter light emitting diode element; 123: packaging colloid;
[0051] 130: lens; 131: mounting part; 1311: sticky solid glue; 1312: liquid glue; 1313: hardened solid glue; 132: optical part; 1321: lens mold; 1322: glue barrel; 1323: glue scraper; 1324: anti-stick lining;
[0052] 140: electrical connector; 141: solder pin; 142: plug interface;
[0053] 150: reflective layer;
[0054] 151: sub-reflection layer; 1511: avoidance area;
[0055] 15a: first sub-reflection layer; 15a1: first avoidance area; 15b: second sub-reflection layer; 15b1: second avoidance area;
[0056] 200: backlight module;
[0057] 210: back plate; 211: receiving portion; 2111: positioning column; 212: wire receiving portion; 213: clamping portion;
[0058] 220: display component; 221: diffusion plate; 222: membrane; 223: display panel;
[0059] 230: reflective element; 231: first reflective portion; 232: second reflective portion. DETAILED DESCRIPTION
[0060] In order to make the above-mentioned purposes, features and advantages of the embodiments of the present invention more obvious and understandable, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work belong to the scope of protection of the present invention.
[0061] In the related art, the Micro LED light board includes a substrate, a Micro LED chip array and a micro lens array. During assembly, glue is applied around each Micro LED chip on the substrate; each prepared micro lens covers the corresponding Micro LED chip, and each micro lens is bonded to the surface of the substrate by glue. This assembly method is inefficient and prone to defects such as weak bonding or misaligned bonding.
[0062] The embodiments of the present application provide a method for molding a light board, a backlight module, and a display device, which are applicable to micron-level light emitting diode (Micro-Light Emitting Diode, Micro LED) light boards and sub-millimeter light emitting diode (Mini-Light Emitting Diode, Mini LED) light boards. Among them, the mounting portion and the optical portion of the lens on the light board are integrally molded by curable hot-melt silicone, and the mounting portion covers and adheres to the light-emitting element and the reflective layer, so that the position of the optical portion corresponds to the position of the light-emitting element, and the optical portion and the light-emitting element are assembled, shortening the preparation cycle; and the contact area between the mounting portion and the reflective layer is large, and the lens can be reliably positioned by relying on the mounting portion, and it is not easy to have defects such as lens installation misalignment or inadequate installation, thereby improving the product yield.
[0063] See also Figures 1 to 6 as well as Fig.12 The present embodiment provides a method for forming a lamp board, and the method for forming a lamp board is used to make a lamp board 100. The lamp board 100 is applied to a display device. The display device has a display panel 223, and the display panel 223 is used to display information such as images and texts.
[0064] The display panel 223 may be a liquid crystal display panel, which itself does not emit light, wherein the light board 100 may serve as a backlight source to illuminate the liquid crystal display panel.
[0065] The display device has a top side, a bottom side, a left side, a right side, a front side, and a back side. Specifically, when a user uses the display device, the user faces the display panel 223 of the display device. At this time, the left side of the user is the left side of the display device, the right side of the user is the right side of the display device, the side of the display device facing the user is the front side of the display device, and the side of the display device away from the user is the back side of the display device.
[0066] In some embodiments, the light board 100 includes a plurality of light emitting elements 120, which are used as backlight sources to emit light. The arrangement of the plurality of light emitting elements 120 can be set as required, for example, the plurality of light emitting elements 120 are arranged vertically and horizontally.
[0067] In some embodiments, the light board 100 further includes a board body 110, and a plurality of light emitting elements 120 are disposed on the board body 110. Specifically, the light emitting elements 120 are disposed on the front side of the board body 110. The board body 110 may be an aluminum substrate, a fiberglass board, or a glass board.
[0068] An electrical connection line (not shown) is provided on one side of the board 110 where the light emitting element 120 is provided, and the electrical connection line may be a wire coated on the board 110. The light emitting element 120 may be fixed to the board 110 by welding and electrically connected to the electrical connection line, and the other end of the electrical connection line is connected to a power source through a conductive adhesive or other components to supply power to the light emitting element 120.
[0069] The light board 100 includes a lens 130 , which can disperse the light emitted by the light emitting element 120 , so that the light board 100 has good optical properties. The lens 130 includes a mounting portion 131 and an optical portion 132 , and the mounting portion 131 is used to connect with the board body 110 .
[0070] In some embodiments, a method for forming a light panel includes:
[0071] S101, heating the liquid curable hot-melt silicone to obtain a cured optical part.
[0072] Among them, hot melt polymer refers to a material that is solid at a lower temperature and melts into a fluid at a higher temperature. And hot melt polymer can also be cured under heating conditions, that is, the curable hot melt polymer can be cured again.
[0073] In some embodiments, the curable hot-melt silicone includes an organosilicon polymer and an associating agent. The organosilicon polymer and the associating agent undergo an addition reaction with a catalyst at a mass ratio of 8:1-15:1 to obtain the curable hot-melt silicone.
[0074] The organosilicon polymer may be a methyl organosilicon polymer, such as methyl vinyl silicone resin, or a phenyl organosilicon polymer, such as phenyl vinyl silicone resin. The correlation agent may be methyl hydrogenated silicone oil, phenyl hydrogenated silicone oil, and phenyl hydrogenated silicone resin. The catalyst may be a platinum catalyst, such as platinum black, an alcohol solution of chloroplatinic acid, or the like.
[0075] This embodiment does not limit the component contents of the organosilicon polymer, the associating agent, and the catalyst. In some embodiments, the mass ratio of the organosilicon polymer to the associating agent is 10:1.
[0076] In some embodiments, during the addition reaction, additives such as fluorescent powder and pigment may be added as needed to prepare curable hot-melt silicone.
[0077] The curable hot melt silicone is solid at a relatively low temperature (eg, room temperature), and can melt and convert into a fluid as the temperature rises (eg, greater than 150° C.), and the curable hot melt silicone can be cured by heating.
[0078] That is to say, Figure 4 As shown, the curable hot melt type silicone can have three forms: viscous solid glue 1311, liquid glue 1312 and hardened solid glue 1313. Among them, the viscous solid glue 1311 is an intermediate state between the liquid glue 1312 and the hardened solid glue 1313, and the viscous solid glue 1311 is a viscous semi-solid state. Figure 5 As shown, when the curable hot melt silicone is in a sticky solid glue 1311 state, the curable hot melt silicone is heated at a temperature of 120° C. for 6-8 minutes, and the sticky solid glue 1311 has moderate viscosity and peel strength.
[0079] like Figure 6 As shown, the ordinate only represents the magnitude relationship between the relative pressure values P of the storage modulus and the loss modulus, and is not limited to specific values. The farther from the origin, the greater the pressure value P of the storage modulus and the loss modulus.
[0080] When the storage modulus is much larger than the loss modulus, the curable hot-melt silicone mainly undergoes elastic deformation and is in the state of hardened solid glue 1313; when the loss modulus is much larger than the storage modulus, the curable hot-melt silicone mainly undergoes viscous deformation and is in the state of liquid glue 1312; when the storage modulus and the loss modulus are equivalent, the curable hot-melt silicone is semi-solid and is in the state of viscous solid glue 1311.
[0081] In this way, when the curable hot melt silicone is in the state of viscous solid glue 1311 and the state of liquid glue 1312, the two can be converted to each other under different temperature conditions, that is, when the temperature and other conditions change, the curable hot melt silicone in the state of viscous solid glue 1311 can be converted to the curable hot melt silicone in the state of liquid glue 1312, or the curable hot melt silicone in the state of liquid glue 1312 can be converted to the curable hot melt silicone in the state of viscous solid glue 1311. When the curable hot melt silicone is made into the state of hardened solid glue 1313, it is no longer reversible. At this time, when the temperature and other conditions change, the curable hot melt silicone always maintains the state of hardened solid glue 1313.
[0082] With reference to the above-mentioned characteristics of the curable hot-melt silicone, the curable hot-melt silicone generated by the addition reaction can be heated and liquefied into liquid glue 1312 , and then the lens 130 can be prepared on the lens mold 1321 by controlling the temperature of the liquid glue 1312 .
[0083] The liquid glue 1312 can be stored in the glue barrel 1322 for standby use. The lens mold 1321 is a metal part, and the lens mold 1321 is provided with a molding surface, and the molding surface is used to prepare the mounting part 131, and the molding surface has a molding cavity with a set tolerance to the outer size of the optical part 132, and the open end of the molding cavity corresponds to the light-incoming side of the optical part 132, and the inner wall surface of the molding cavity is adapted to the light-emitting surface of the optical part 132.
[0084] The shape of the inner wall of the molding cavity can be set according to the preset light distribution requirements. For example, see Figure 3 The top of the optical part 132 has a concave curved surface, and the circumference of the concave curved surface is connected to the mounting part 131 through the peripheral connecting curved surface, and the optical part 132 is flat as a whole. In this way, the light emitted by the light emitting element is refracted by the concave curved surface and the peripheral connecting curved surface, and diffuses from the center of the top surface to the circumference, thereby reducing the luminous intensity at the center of the top surface of the light emitting element, increasing the luminous intensity around the center of the top surface, and avoiding the situation of uniform distribution of light and dark.
[0085] When preparing the optical part 132, the liquid glue 1312 in the glue bucket 1322 is poured into the molding cavity, and the curable hot-melt silicone remaining on the molding surface is scraped off by the scraper 1323, so that the curable hot-melt silicone is flush with the molding surface. Then, the curable hot-melt silicone in the molding cavity is heated by heating the lens mold 1321.
[0086] In some embodiments, heating the liquid curable hot-melt silicone to obtain a cured optical part 132 includes: heating to 150°C-200°C under vacuum conditions and maintaining the temperature for 20 minutes-120 minutes, converting the liquid glue 1312 in the molding cavity into a hardened solid glue 1313 to cure the optical part 132.
[0087] The vacuum treatment can remove bubbles from the curable hot-melt silicone to avoid affecting the refractive index of the lens 130. For example, the lens mold 1321 can be placed in a laminator for vacuum treatment.
[0088] After obtaining the optical part 132, other structures or materials may be provided on the surface of the optical part 132, thereby forming an installation or fixing structure for assembling or fixing the optical part 132. Specifically, after step S101, the lamp panel forming method further includes:
[0089] S102, coating liquid curable hot-melt silicone on the light incident side of the optical part, and cooling the liquid curable hot-melt silicone to obtain a mounting part in an intermediate state, wherein the mounting part in the intermediate state is connected to the optical part.
[0090] The light incident side of the optical part 132 is coated with liquid curable hot melt silicone, that is, the liquid glue 1312 in the glue barrel 1322 is poured onto the molding surface, and the liquid glue 1312 simultaneously covers the cured optical part 132. The thickness of the covering layer is controlled by the distance between the scraper 1323 and the molding surface.
[0091] In some embodiments, the thickness of the mounting portion 131 is 0.01 mm-1.5 mm to be suitable for different types of light emitting elements 120 .
[0092] The liquid curable hot-melt silicone is cooled to obtain the mounting portion 131 in an intermediate state, and the mounting portion 131 is connected to the optical portion 132 .
[0093] The mold can be cooled to reduce the temperature of the covering layer to 50°C-130°C, for example, 120°C, and the temperature can be kept constant for 6 minutes to 8 minutes to reduce the flow rate of the curable hot-melt silicone rubber and obtain the mounting portion 131 in the intermediate state. At this time, the mounting portion 131 in the intermediate state is a viscous solid glue 1311, which has moderate viscosity and is fixedly connected to the optical portion 132. At the same time, the mounting portion 131 in the intermediate state has moderate peeling strength to be easily peeled off from the lens mold 1321.
[0094] Considering the stickiness of the sticky solid glue 1311, during the process of transferring the mounting portion 131 and the optical portion 132 to the board 110, a release liner 1324 may be mounted on the mounting portion 131 to prevent dust from being picked up by hand and damaging the mounting portion 131. When mounting the release liner 1324, air bubbles between the release liner 1324 and the mounting portion 131 may be removed by a scraper 1323.
[0095] After the mounting portion 131 is arranged on the optical portion 132, the mounting portion can be used as a reference to subsequently install the optical portion. Specifically, after step S102, the method for installing the light board further includes the following steps:
[0096] S103, covering the mounting part on the reflective layer of the board body, so that the optical part and the board body are respectively located on two sides of the mounting part, and the optical part corresponds to the light emitting element.
[0097] The mounting portion 131 and the optical portion 132 can be removed from the lens mold 1321 by a fixture such as a suction cup and transferred to the position of the board 110, and then the mounting portion 131 is covered on the reflective layer 150 of the board 110, so that the optical portion 132 and the board 110 are respectively located on both sides of the mounting portion 131, and the optical portion 132 corresponds to the light emitting element 120. The optical portion 132 can be aligned with the light emitting element 120 by aligning the fixture with the board 110.
[0098] After step S103, in order to further fix the mounting portion 131 and the optical portion 132 in the aligned position, the lamp panel mounting method specifically further includes:
[0099] S104, heating the mounting portion so that the mounting portion is liquefied by the heat and solidified after being deposited on the reflective layer.
[0100] Among them, since the optical part 132 is in the state of hardened solid glue 1313, when the mounting part 131 is heated, the optical part 132 in the state of hardened solid glue 1313 will not change its state, that is, the optical part 132 will maintain its own size unchanged to avoid affecting the optical effect.
[0101] The plate body 110 may be heated to 150° C.-200° C. under vacuum conditions to liquefy the mounting portion 131, that is, the mounting portion 131 in the state of viscous solid glue 1311 is converted into the mounting portion 131 in the state of liquid glue 1312. At this time, the mounting portion 131 in the state of liquid glue 1312 has fluidity and can be deposited on the reflective layer 150 and the light emitting element 120.
[0102] The board 110 is continuously heated and kept at a constant temperature for 20 minutes to 120 minutes to solidify the mounting portion 131. That is, the mounting portion 131 in the state of liquid glue 1312 is converted into the mounting portion 131 in the state of hardened solid glue 1313. At this time, the mounting portion 131 is integrally connected with the optical portion 132, and the mounting portion 131 is fixedly connected with the reflective surface on the board 110 and the light-emitting element 120.
[0103] The vacuum treatment can remove bubbles from the curable hot-melt silicone rubber to avoid affecting the refractive index of the lens 130 .
[0104] In this way, the mounting portion 131 of the lens 130 is integrally formed with the optical portion 132, and the mounting portion 131 covers and adheres to the light emitting element 120 and the reflective layer 150, so that the position of the optical portion 132 corresponds to the position of the light emitting element 120, and the optical portion 132 and the light emitting element 120 are assembled, which shortens the preparation cycle. At this time, the light emitted by the light emitting element 120 is emitted sequentially through the portion of the mounting portion 131 corresponding to the optical portion 132 and the optical portion 132. In addition, the contact area between the mounting portion 131 and the reflective layer 150 is large, and the lens 130 can be reliably positioned by relying on the mounting portion 131, and it is not easy to have defects such as misalignment or inadequate installation of the lens 130, thereby improving the product yield.
[0105] Furthermore, since the optical portion 132 is prefabricated in the molding cavity, the shape of the optical portion 132 is not affected during the shape change of the mounting portion 131 , and the optical portion 132 can always have a preset light emitting surface shape.
[0106] In some embodiments, there are multiple light emitting elements 120, which are spaced apart on the board 110. Accordingly, there are multiple optical parts 132, and the mounting part 131 is connected to multiple optical parts 132 at the same time to form a lens array.
[0107] Considering the small size of Micro LED and Mini LED, the number of light emitting elements 120 on the light board 100 is large. When the light board 100 uses a reflector, it is necessary to open holes in the reflector, and the number of holes is the same as the number of light emitting elements 120, which is a lot of work. Figure 7 The reflective layer 150 is formed by curing the reflective ink.
[0108] The reflective ink may contain titanium dioxide or barium sulfate white pigment particles, the particle size of the pigment particles may be 0.2-1.5um, and reflect light of different colors through the concave spherical reflection principle. Since the submicron pigment particles are randomly distributed, different particles can reflect light in different directions, that is, the reflective layer 150 can diffusely reflect light.
[0109] The color of the reflective ink may be green, white, red, or black. In some embodiments, the color of the reflective ink may be white to reduce light loss and increase the reflectivity of the reflective layer 150 .
[0110] Compared with the method of making holes in the reflective sheet, the production cycle of the reflective layer 150 is shorter, which reduces the production cycle of the light board 100. It can also protect the electrical connection wires on the board body 110 to prevent collision damage or corrosion short circuit of the electrical connection wires.
[0111] In some embodiments, a avoidance area 1511 is provided on the reflective layer 150, and the light emitting element 120 is located in the avoidance area 1511. During the coating of the reflective ink, the location of the avoidance area 1511 can be shielded, so that after the reflective layer 150 is formed, the electrical connection line at the location thereof can be exposed through the avoidance area 1511.
[0112] In some embodiments, the reflective layer 150 includes a plurality of sub-reflective layers 151 , and the plurality of sub-reflective layers 151 are stacked.
[0113] When the number of the sub-reflection layer 151 is one layer, the reflectivity of the reflective layer 150 can be 85%-87%. The reflection efficiency of diffuse reflection increases with the thickness of the sub-reflection layer 151. Figures 7 to 9 , multiple layers of sub-reflective layers 151 are stacked, the thickness of the reflective layer 150 increases, the number of submicron pigment particles increases, the reflective layer 150 absorbs less light, and the reflectivity of the reflective layer 150 increases. At this time, after the sub-reflective layer 151 is cured, the reflective ink can be coated again on the cured sub-reflective layer 151 and cured. By providing multiple layers of sub-reflective layers 151, the reflectivity of the reflective layer 150 can be greater than 92%.
[0114] In some embodiments, the avoidance area 1511 may be a cylindrical hole, that is, the cross-sectional dimensions of the avoidance area 1511 are the same everywhere.
[0115] In some embodiments, the radial dimension of the avoidance area 1511 at one end close to the plate body 110 is smaller than the radial dimension of the avoidance area 1511 at one end away from the plate body 110, that is, the avoidance area 1511 is an approximately conical hole, and the small-diameter end of the avoidance area 1511 is connected to the plate body 110, and the large-diameter end of the avoidance area 1511 is an open end.
[0116] When assembling the light board 100, the light emitting element 120 can extend into the avoidance area 1511 through the large-diameter end of the avoidance area 1511 and be welded to the board body 110. Since the open end of the avoidance area 1511 has a large diameter, it can be avoided that the light emitting element 120 and the reflective layer 150 interfere with each other during the assembly of the light board 100, and the welding end of the light emitting element 120 cannot fully contact with the board body 110, resulting in the light emitting element 120 being poorly welded.
[0117] Furthermore, during the lens preparation process, during the deposition of the mounting portion 131 in the state of liquid glue 1312 , it can be deposited and filled in the avoidance area 1511 to cover the light emitting element 120 .
[0118] In some embodiments, when the light board 100 is working, part of the light emitted by the light emitting element 120 can be directly directed toward the front side of the display device and emitted through the lens. Part of the light emitted by the light emitting element 120 is emitted toward the side wall surface of the avoidance area 1511. At this time, the part of the light passes through the mounting portion 131 in the avoidance area 1511, and is reflected by the side wall surface of the avoidance area 1511 and then emitted through the mounting portion 131 and the optical portion 132, so that the light loss of the light emitting element 120 is small.
[0119] It is understandable that the height of the LED can be 200μm-500μm, and the height of the Mini LED can be 90μm-120μm. The thickness of the sub-reflection layer 151 can be 20μm-25μm. To prevent the reflective layer 150 from blocking the light-emitting element 120, the thickness of the reflective layer 150 can be less than half the height of the light-emitting element 120. In other words, the number of layers of the sub-reflection layer 151 can be two or three.
[0120] Taking the number of two sub-reflection layers 151 as an example, in some embodiments, the multiple sub-reflection layers 151 include a first sub-reflection layer 15a and a second sub-reflection layer 15b, that is, the preset reflectivity can be achieved with a smaller number of sub-reflection layers 151, and the production cost of the light board 100 is lower.
[0121] The first sub-reflection layer 15a is coated on the plate body 110, and the first sub-reflection layer 15a is provided with a first avoidance area 15a1. That is, during the molding process of the light board 100, reflective ink can be coated on the plate body 110, and the reflective ink can be dried to solidify the first sub-reflection layer 15a. The location of the first avoidance area 15a1 can be shielded, so that during the molding process of the first sub-reflection layer 15a, the location of the first avoidance area 15a1 is not coated with reflective ink, so that the electrical connection line is exposed in the first avoidance area 15a1.
[0122] The second sub-reflection layer 15b is coated on the surface of the first sub-reflection layer 15a. The second sub-reflection layer 15b is provided with a second avoidance area 15b1. The radial dimension of the second avoidance area 15b1 is greater than the radial dimension of the first avoidance area 15a1.
[0123] After the first sub-reflection layer 15a is solidified, reflective ink is further coated on the surface of the first sub-reflection layer 15a, and the ink is dried to solidify the second sub-reflection layer 15b. The second avoidance area 15b1 can be shielded so that the reflective ink is not coated on the second avoidance area 15b1 during the molding process of the second sub-reflection layer 15b.
[0124] In some embodiments, when the reflective layer 150 includes a third sub-reflective layer, a radial dimension of the third avoidance region on the third sub-reflective layer may be smaller than or equal to a radial dimension of the second avoidance region 15 b 1 .
[0125] In some embodiments, the first avoidance area 15a1 and the second avoidance area 15b1 may have the same shape, for example, the first avoidance area 15a1 and the second avoidance area 15b1 are both circular holes, or the first avoidance area 15a1 and the second avoidance area 15b1 are both rectangular holes.
[0126] In some embodiments, the center lines of the first avoidance area 15a1 and the second avoidance area 15b1 can be staggered, or the first avoidance area 15a1 and the second avoidance area 15b1 can be set at the same position on the surface of the relative plate 110, so as to simplify the shape of the avoidance area 1511 and reduce the manufacturing cost. In this case, the avoidance area 1511 is approximately a stepped tapered hole.
[0127] In some embodiments, the gap between the inner wall surface of the first avoidance area 15a1 and the outer wall surface of the light emitting element 120 may be 10 μm-20 μm. The radial dimension difference between the first avoidance area 15a1 and the second avoidance area 15b1 may be 0.5 mm-1 mm.
[0128] In some embodiments, the light emitting element 120 includes a micron-sized light emitting diode element 121 , and the micron-sized light emitting diode element 121 is fixed to the board 110 by welding.
[0129] When the light emitting element 120 is applied to a Micro LED light panel, the light emitting element 120 uses a micron-sized light emitting diode chip or a micron-sized light emitting diode element 121 with a package structure.
[0130] For example, Fig.10 As shown, the micron-scale light-emitting diode chip is a flip-chip RGB three-color light-emitting chip, including a P electrode 1211, an N electrode 1212, a P-type gallium nitride 1213, an N-type gallium nitride 1214, a light-emitting area 1215 and sapphire 1216. Its specific structure is the same as that of the related technology and will not be repeated here.
[0131] The P electrode 1211 and the N electrode 1212 are respectively connected by welding to the electrical connection wires on the board 110. Two pads 113 are provided on the board 110, and chip bumps 1217 are respectively provided at the P electrode 1211 and the N electrode 1212. Silver glue or solder paste is pre-sprayed on the chip bumps 1217, and rosin is sprayed on the pads 113, so that the corresponding pads 113 and chip bumps 1217 are welded to each other.
[0132] In some embodiments, the light-emitting element 120 includes a sub-millimeter light-emitting diode element 122 and a packaging colloid 123. The sub-millimeter light-emitting diode element 122 is welded on the board 110. The packaging colloid 123 covers and is bonded to the outer surface of the sub-millimeter light-emitting diode element 122. Particles for reducing the relative density of light intensity are bonded to the packaging colloid 123 corresponding to the top surface of the sub-millimeter light-emitting diode element 122.
[0133] When the light emitting element 120 is applied to a Mini LED light board, the light emitting element 120 uses a sub-millimeter light emitting diode element 122 , and a packaging colloid 123 is disposed on the outer surface of the sub-millimeter light emitting diode element 122 .
[0134] For example, Fig.11 As shown, the sub-millimeter light-emitting diode element 122 is in a square box shape, and the bottom surface of the sub-millimeter light-emitting diode element 122 is welded to the board 110 through the pad 113. The outer surface of the sub-millimeter light-emitting diode element 122 is wrapped with a packaging colloid 123, and the packaging colloid 123 is made of silicone. Considering that the luminous intensity of the sub-millimeter light-emitting diode element 122 is uneven, in order to weaken the light intensity of its top surface, the packaging colloid 123 corresponding to the top surface of the sub-millimeter light-emitting diode element 122 is coated with glue, and the glue is doped with 15%-20% by mass of titanium dioxide, which is used to reduce the relative density of light intensity particles.
[0135] In some embodiments, Fig.16 and Fig.17 As shown, a connection hole is provided on the board 110 , the light emitting element 120 is connected to one end of an electrical connection line, and the other end of the electrical connection line is connected to the connection hole.
[0136] The light board 100 also includes an electrical connector 140 for connecting a wiring harness. The electrical connector 140 is disposed at the connection hole. A welding foot 141 on one side of the electrical connector 140 is located on the side of the board body 110 where the light-emitting element 120 is disposed. The welding foot 141 is connected to the electrical connection wire in a one-to-one correspondence. The middle portion of the electrical connector 140 is located in the connection hole. A plug interface 142 on the other side of the electrical connector 140 is located on the side of the board body 110 away from the light-emitting element 120. The wiring harness is connected through the plug interface 142, and the power supply is connected. Placing a portion of the electrical connector 140 in the connection hole reduces the space occupied by the electrical connector 140 and reduces the thickness of the light board 100.
[0137] See also Figures 12 to 20 The present embodiment provides a backlight module 200 , which includes a back plate 210 to provide support and protection for a light board assembly, a display assembly, etc., wherein the rear side of the light board assembly corresponds to the front side of the back plate 210 .
[0138] In some embodiments, the backlight module 200 further includes a light board assembly, which includes a plurality of light boards 100 made by the above-mentioned light board forming method, and the plurality of light boards 100 are arranged in parallel on the front side of the back plate 210. The process and beneficial effects of the light board forming method have been described in the above-mentioned embodiments, and will not be described in detail in this embodiment.
[0139] A plurality of light panels 100 may be arranged in the longitudinal and transverse directions, wherein each light panel 100 may be fixed to the back panel 210 by means of threaded fasteners, and the threaded fasteners are white to reduce the light consumption of the threaded fasteners.
[0140] The back plate 210 is provided with a receiving portion 211, which includes a receiving port and a receiving space formed by a receiving wall surface communicating with the receiving port, and a plurality of positioning posts 2111 are provided on the receiving wall surface of the receiving portion 211 opposite to the receiving port. The plate body 110 is provided with a plurality of positioning holes 111, which are used to be sleeved on the positioning posts 2111 to fix the light board assembly on the back plate 210. The positioning holes 111 can be any shape such as circular, triangular, etc.
[0141] In some embodiments, there are four positioning holes 111, and the connection line of the four positioning holes 111 is a rhombus, and the center of the rhombus is the same point as the center of the board 110. A connection hole is provided near the center of the board 110 for installing the electrical connector 140.
[0142] In some embodiments, the backlight module 200 also includes a display component 220 familiar to those skilled in the art. The display component 220 includes a diffuser plate 221, a membrane 222 and a display panel 223 stacked in sequence. The diffuser plate 221 is located on one side of the membrane 222 close to the light board assembly.
[0143] In some embodiments, a plurality of protruding pillars 112 are provided on the front side of the plate body 110, and the pillars 112 abut against the diffuser plate 221. A clamping portion 213 is provided at the edge of the back plate 210, and the diffuser plate 221, the membrane 222 and the display panel 223 are overlapped at the clamping portion 213 after being stacked, so that the connection method is simple and reliable, and the assembly efficiency is high.
[0144] In some embodiments, there are four pillars 112 , and the line connecting the four pillars 112 is a rectangle, and the center of the rectangle is the same point as the center of the plate body 110 .
[0145] The clamping portion 213 can be optionally set to a three-step stepped structure, and is a structure that gradually closes toward the inner side of the back plate 210. Then the diffuser plate 221, the membrane 222 and the display panel 223 can also be correspondingly set to a three-step stepped structure, and is a structure that gradually closes toward the side of the diffuser plate 221.
[0146] The bottom surface of the groove of the clamping portion 213 is flush with the top surface of the pillar 112 on the lamp panel assembly, so that the side of the diffusion plate 221 close to the bottom surface of the groove abuts against the top of the pillar 112 .
[0147] The support 112 can be configured to be a truncated cone or a trapezoidal cone with a cross-sectional area that is smaller at the top and larger at the bottom, so as to improve the stability of the connection with the board 110 and reduce the contact area with the display assembly 220.
[0148] In some embodiments, the back panel 210 is provided with a wire accommodating portion 212 for accommodating the wire harness, and the wire accommodating portion 212 is also a rectangular groove structure, and the back panel 210 is provided with a wire passing hole (not shown) connecting the wire accommodating portion 212 and the outside; the plug interface 142 is connected to the first end of the wire harness, part of the wire harness is located in the wire accommodating portion 212, and the second end of the wire harness passes through the wire passing hole and extends out of the wire accommodating portion 212.
[0149] In some embodiments, the backlight module 200 further includes a reflector 230, which includes a first reflector 231, which is disposed between two adjacent light boards 100 to avoid light leakage at the joint of the two adjacent light boards 100. Since the size of the backboard 210 is larger than the distribution size of the light board assembly, the reflector 230 further includes a second reflector 232, which is disposed on the outer side of the light board assembly in the circumferential direction to avoid light leakage at the outer edge of the light board assembly in the circumferential direction.
[0150] Positioning holes may be provided between the light board 100 and the diffuser 221 and between the light board 100 and the back plate 210 for positioning the light board 100 and the diffuser 221. In some embodiments, the reflector 230 may further include a third reflective portion, which covers the positioning holes and the portion of the threaded fasteners exposed on the front side of the light board, so as to avoid uneven brightness of the display panel 223 due to reduced reflectivity at the locations of the positioning holes and the threaded fasteners.
[0151] In some embodiments, the reflective member 230 is a reflective sheet. The reflective sheet may be made of polyethylene terephthalate (PET). The reflective sheet has a white reflective surface for emitting light toward the front side of the display device.
[0152] When the reflective sheet is disposed at the joint position between two adjacent light panels 100 , the reflective sheet is in a strip shape, and the reflective sheet can be mounted and fixed on the reflective layer 150 by an adhesive.
[0153] When the reflective sheet is arranged outside the circumference of the light board assembly, the reflective sheet can be annular, the inner edge of the reflective sheet is attached to the reflective layer 150 of the light board 100, and the outer edge of the reflective sheet is attached to the back plate 210. Of course, at this time, the reflective sheet can be strip-shaped and spliced into an annular shape.
[0154] In some embodiments, the reflective member 230 is a reflective coating formed by curing reflective ink, and the reflective coating includes a plurality of sub-reflective coatings, and the plurality of sub-reflective coatings are formed by successively curing solder resist ink. The molding process of the reflective coating is similar to that of the reflective layer 150, and both achieve a preset reflectivity by successively curing multiple layers of ink.
[0155] When the reflective coating is disposed at the joint position between two adjacent light panels 100, the reflective coating at least fills the joint position of the two light panels 100. Of course, the distribution area of the reflective coating can also be larger than the area of the joint, in which case the reflective coating is coated on the reflective layer 150.
[0156] When the reflective coating is arranged on the outer side of the circumference of the light panel assembly, the reflective coating is spliced with the reflective layer 150 or the reflective coating is partially coated on the reflective layer 150 to avoid a light leakage gap between the reflective coating and the reflective layer 150, resulting in uneven brightness of the display panel 223.
[0157] In some embodiments, the reflector 230 may include a reflective sheet and a reflective coating. Exemplarily, the reflective sheet is disposed at the joint position of two adjacent light panels 100, and the reflective coating is disposed on the outer side of the light panel assembly in the circumferential direction.
[0158] In some embodiments, the back panel 210 includes a back panel body and a folded edge arranged at the edge of the back panel body, and the second reflective portion 232 is arranged on both the back panel body and the folded edge, resulting in the side of the display panel 223 being brighter than other positions of the display panel 223, that is, the brightness at different positions of the display panel 223 is uneven.
[0159] Correspondingly, a light leakage structure is provided on the second reflective portion 232 to reduce the intensity of light reflected toward the front side of the back plate 210, so as to reduce the brightness at the side of the display panel 223 and avoid uneven brightness of the display panel 223. The light leakage structure is usually provided at the middle of the folded edge.
[0160] In some embodiments, when the reflector 230 is a reflective sheet, the light leakage structure is a through hole that penetrates the reflective sheet, and the through hole can be a circular hole, a bar hole, etc., and the structure is relatively simple. The aperture and number of the through hole can be set as needed.
[0161] In some embodiments, when the reflective element 230 is a reflective coating formed by curing solder resist ink, the light leakage structure is a recessed portion formed on the reflective coating, the recessed portion is open, and the recessed depth of the recessed portion is less than the thickness of the reflective coating, and is easy to form.
[0162] Exemplarily, when the reflective coating includes a first sub-reflective coating and a second sub-reflective coating, a recess is formed on the second sub-reflective coating to reduce the brightness at the side of the display panel 223 by reducing the reflectivity of the reflective coating at the location of the recess.
[0163] The cross-sectional shape of the recessed portion can be a circular hole, a strip hole, etc., and the structure is relatively simple. The aperture of the recessed portion and the number of the recessed portions can be set as required.
[0164] This embodiment provides a display device (not shown), which includes the above-mentioned backlight module 200. The structure, function and working principle of the backlight module 200 have been described in the above-mentioned embodiment, and will not be repeated in this embodiment.
[0165] By adopting the backlight module 200, the assembly cycle of the light panel 100 and the display device can be reduced and the assembly yield can be improved.
[0166] The various embodiments or implementation methods in this specification are described in a progressive manner. Each embodiment focuses on the differences from other embodiments, and the same or similar parts between the various embodiments can be referenced to each other.
[0167] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials, or characteristics described in conjunction with the embodiments or examples are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials, or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.
[0168] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A method for molding a lamp panel, the lamp panel comprising a panel body, a light emitting element and a lens, the lens comprising a mounting portion and an optical portion, the mounting portion being used to be connected to the panel body, the lens being prepared on a lens mold, the lens mold being provided with a molding surface, the molding surface having a molding cavity having a set tolerance with respect to an outer dimension of the optical portion, characterized in that: The molding method of the lamp panel comprises: The liquid curable hot-melt silicone is poured into the molding cavity, and the liquid curable hot-melt silicone is heated to obtain a cured optical part; the curable hot-melt silicone has three forms: viscous solid glue, liquid glue and hardened solid glue; the viscous solid glue is an intermediate state between the liquid glue and the hardened solid glue; the cured optical part is the hardened solid glue; Coating a liquid curable hot-melt silicone on the light incident side of the optical part, pouring the liquid curable hot-melt silicone on the molding surface, and cooling the liquid curable hot-melt silicone to obtain a mounting part in an intermediate state, wherein the mounting part in the intermediate state is connected to the optical part, the mounting part in the intermediate state is a viscous solid glue, and the viscous solid glue is in a viscous semi-solid state; removing the mounting portion and the optical portion from the lens mold; The mounting portion is covered on the reflective layer of the plate body, so that the optical portion and the plate body are respectively located on both sides of the mounting portion, and the optical portion corresponds to the light-emitting element, the reflective layer is formed by curing reflective ink, an avoidance area is provided on the reflective layer, and the light-emitting element is located in the avoidance area; The mounting portion is heated so that the mounting portion is liquefied by the heat and solidified after being deposited on the reflective layer.
2. The method for forming a lamp panel according to claim 1, characterized in that: The step of heating the liquid curable hot-melt silicone to obtain a cured optical part comprises: heating to 150° C.-200° C. under vacuum conditions and maintaining the temperature for 20 minutes-120 minutes to cure the optical part; The step of cooling the liquid curable hot-melt silicone to obtain the mounting portion in the intermediate state includes: cooling the temperature to 50° C.-130° C. and maintaining the temperature for 6 minutes-8 minutes to reduce the flow rate of the curable hot-melt silicone and obtain the mounting portion in the intermediate state; The step of heating the mounting portion to liquefy the mounting portion and solidify the mounting portion after being deposited on the reflective layer comprises: heating to 150° C.-200° C. under vacuum conditions to liquefy the mounting portion, and maintaining the temperature for 20 minutes-120 minutes to solidify the mounting portion.
3. The method for forming a lamp panel according to claim 1, characterized in that: The reflective layer includes a plurality of sub-reflective layers, and the plurality of sub-reflective layers are stacked.
4. The method for forming a lamp panel according to claim 3, characterized in that: The multiple sub-reflection layers include a first sub-reflection layer and a second sub-reflection layer, the first sub-reflection layer is coated on the plate body, and the second sub-reflection layer is coated on the surface of the first sub-reflection layer; The first sub-reflection layer is provided with a first avoidance area, and the second sub-reflection layer is provided with a second avoidance area, and the radial dimension of the second avoidance area is greater than the radial dimension of the first avoidance area.
5. The method for forming a lamp panel according to any one of claims 1 to 4, characterized in that: The curable hot-melt silicone comprises an organic silicon polymer and an associating agent, and the mass ratio of the organic silicon polymer to the associating agent is 8:1-15:
1.
6. The method for forming a lamp panel according to any one of claims 1 to 4, characterized in that: The thickness of the mounting portion is 0.01 mm-1.5 mm.
7. The method for forming a lamp panel according to any one of claims 1 to 4, characterized in that: The light emitting element comprises a micron-sized light emitting diode element, and the micron-sized light emitting diode element is welded and fixed to the plate.
8. The method for forming a lamp panel according to any one of claims 1 to 4, characterized in that: The light-emitting element includes a sub-millimeter light-emitting diode element and a packaging colloid. The sub-millimeter light-emitting diode element is welded on the board. The packaging colloid covers and is bonded to the outer surface of the sub-millimeter light-emitting diode element. Particles for reducing the relative density of light intensity are bonded to the packaging colloid corresponding to the top surface of the sub-millimeter light-emitting diode element.
9. A backlight module, applied to a display device, characterized in that: The backlight module comprises: Back panel; Reflective parts; A light board assembly, the light board assembly comprising a plurality of light boards made by the light board forming method according to any one of claims 1 to 8, wherein the plurality of light boards are arranged in parallel on the front side of the back board; The reflector includes a first reflective portion and a second reflective portion, wherein the first reflective portion is disposed between two adjacent lamp boards, and the second reflective portion is disposed on the outer side of the lamp board assembly in the circumferential direction.
10. A display device, characterized in that: Including the backlight module described in claim 9.