Method and device for improving short-circuit welding waveform of fusion-type short-circuit gas shielded welding

By adjusting the short-circuit welding waveform and arc current duration, the problem of inaccurate arc sensing tracking in short-circuit welding is solved, and the accuracy of the welding process and the adaptability of complex working conditions are improved.

CN116000413BActive Publication Date: 2024-11-01PANASONIC WELDING SYST TANGSHAN
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202310145559.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-02-21
Publication Date
2024-11-01
Estimated Expiration
2043-02-21

AI Technical Summary

Technical Problem

During the melting electrode gas protection welding process, the arc sensing tracking is inaccurate due to complex workpieces and environment during short-circuit welding, which affects the welding effect.

Method used

By obtaining the initial current setting value and short-circuit waveform parameters, adjusting the short-circuit welding waveform, including adjusting the first and second rising slopes of the short-circuit, and adjusting the arc current duration according to the actual welding current to ensure the current setting during the welding process. Set value.

Benefits of technology

It significantly improves the tracking accuracy of arc sensing, stabilizes the welding arc state, improves the weld forming quality and adaptability to complex working conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116000413B_ABST
    Figure CN116000413B_ABST
Patent Text Reader

Abstract

The present invention relates to the field of welding technology, specifically to a method and device for improving the short-circuit welding waveform of a fusion electrode short-circuit gas shielded welding, the method comprising: obtaining an initial current setting value and initial short-circuit waveform parameters of a welding power source; before welding begins, after receiving an arc sensor signal, adjusting the short-circuit welding waveform under the current welding current setting value according to the initial current setting value and the initial short-circuit waveform parameters; welding is performed according to the current setting value and the short-circuit waveform parameters defined in the adjusted short-circuit welding waveform; during welding, obtaining the actual welding current, and adjusting the arc current duration in the short-circuit welding waveform according to the actual welding current and the current setting value. When using arc sensing, by adjusting the short-circuit welding waveform, the accuracy of arc sensor tracking is significantly improved, and during welding, the arc state is stable, the weld is well formed, and the adaptability to complex welding conditions is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of welding, in particular to a method and a device for improving the short-circuit welding waveform of fusion-type short-circuit gas shielded welding. Background Art

[0002] Arc sensing technology is gradually being widely used as an important means of implementing automated welding. Arc sensing technology uses the change in welding parameters caused by the change in the distance between the welding torch and the workpiece to detect the height and left and right deviation of the welding torch. In the constant speed wire feeding adjustment system, the wire feeding speed is constant, and the welding power supply generally adopts a flat or slow-down external characteristic. In this case, the welding current will change with the change of the arc length; the change in the arc position will cause the change in the arc length, and the welding current will also change accordingly, so that the relative position between the welding torch and the weld can be determined. Arc sensing uses this principle to achieve real-time tracking and automatic deviation correction of the weld position.

[0003] During the short-circuit welding process of gas metal arc welding, the complexity of the workpiece and the surrounding environment often leads to inaccurate tracking during the use of arc sensors, which in turn affects the tracking effect of the arc sensors. Summary of the invention

[0004] In view of the above problems, an embodiment of the present invention provides a method and device for improving the short-circuit welding waveform of fusion-type short-circuit gas shielded welding.

[0005] In one aspect of the present invention, a method for improving a short-circuit welding waveform of a fusion short-circuit gas shielded welding is provided, comprising:

[0006] Obtaining an initial current setting value and initial short-circuit waveform parameters of a welding power source;

[0007] Before welding starts, after receiving the arc sensor signal, the short-circuit welding waveform under the current welding current setting value is adjusted according to the initial current setting value and the initial short-circuit waveform parameters;

[0008] Welding is performed according to the current setting value and short-circuit waveform parameters defined in the adjusted short-circuit welding waveform;

[0009] During the welding process, the actual welding current is obtained, and the arc current duration in the short-circuit welding waveform is adjusted according to the actual welding current and the current setting value.

[0010] Optionally, the initial short-circuit waveform parameters include: arcing current SPI in the arcing stage, arcing current duration T in the arcing stage, short-circuit first rising slope L1 in the short-circuit stage, short-circuit second rising slope L2 and short-circuit current inflection point S1.

[0011] Optionally, the process of adjusting the short-circuit welding waveform at the current welding current setting value according to the initial current setting value and the initial short-circuit waveform parameters includes:

[0012] Adjust the short circuit first rising slope L1 and the short circuit second rising slope L2, and keep other parameters unchanged, while ensuring that the average current value in the adjusted short circuit welding waveform is equal to the initial current setting value.

[0013] Optionally, the process of adjusting the short-circuit first rising slope L1 and the short-circuit second rising slope L2 includes:

[0014] Adjust the short-circuit first rising slope L1 and the short-circuit second rising slope L2 according to the following expressions:

[0015] L1'=K1*S1+L1

[0016] L2'=K2*S1+L2

[0017] Wherein, L1' represents the adjusted short-circuit first rising slope, K1 is a preset positive value, L2' represents the adjusted short-circuit second rising slope, and K2 is a preset negative value.

[0018] Optionally, the process of adjusting the arc current duration in the short circuit welding waveform according to the actual welding current and the current setting value includes:

[0019] Compare the actual welding current with the current setting value. When the actual welding current is greater than the current setting value, reduce the arc current duration; when the actual welding current is less than the current setting value, increase the arc current duration; when the actual welding current is equal to the current setting value, keep the arc current duration unchanged.

[0020] Another aspect of the present invention is to provide a short-circuit welding waveform improvement device for fusion short-circuit gas shielded welding, comprising:

[0021] A data acquisition module, used to obtain an initial current setting value and an initial short-circuit waveform parameter of a welding power source;

[0022] A pre-welding adjustment module is used to adjust the short-circuit welding waveform under the current welding current setting value according to the initial current setting value and the initial short-circuit waveform parameters before welding starts after receiving the arc sensor signal;

[0023] A welding control module, for performing welding according to a current setting value and short-circuit waveform parameters defined in the adjusted short-circuit welding waveform;

[0024] The welding adjustment module is used to obtain the actual welding current during the welding process, and adjust the arc current duration in the short-circuit welding waveform according to the actual welding current and the current setting value.

[0025] Optionally, the initial short-circuit waveform parameters include: arcing current SPI in the arcing stage, arcing current duration T in the arcing stage, short-circuit first rising slope L1 in the short-circuit stage, short-circuit second rising slope L2 and short-circuit current inflection point S1.

[0026] Optionally, the pre-welding adjustment module is specifically used to adjust the short-circuit first rising slope L1 and the short-circuit second rising slope L2, and the other parameters remain unchanged, while ensuring that the average current value in the adjusted short-circuit welding waveform is equal to the initial current setting value.

[0027] Optionally, the pre-welding adjustment module is specifically used to adjust the short-circuit first rising slope L1 and the short-circuit second rising slope L2 according to the following expression:

[0028] L1'=K1*S1+L1

[0029] L2'=K2*S1+L2

[0030] Wherein, L1' represents the adjusted short-circuit first rising slope, K1 is a preset positive value, L2' represents the adjusted short-circuit second rising slope, and K2 is a preset negative value.

[0031] Optionally, a welding adjustment module is specifically used to compare the actual welding current and the current setting value. When the actual welding current is greater than the current setting value, the arc current duration is reduced; when the actual welding current is less than the current setting value, the arc current duration is increased; when the actual welding current is equal to the current setting value, the arc current duration is kept unchanged.

[0032] Compared with the prior art, the beneficial effects of the present invention are: when using arc sensing, by adjusting the short-circuit welding waveform, the accuracy of arc sensor tracking is significantly improved. During the welding process, the arc state is stable, the weld is well formed, and the adaptability to complex welding conditions is improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] The drawings described herein are used to provide a further understanding of the present invention, constitute a part of the present application, and do not constitute a limitation of the present invention. In the drawings:

[0034] Figure 1 A schematic flow chart of a method for improving a short-circuit welding waveform of a fusion-type short-circuit gas shielded welding machine provided in an embodiment of the present invention;

[0035] Figure 2 A comparison diagram of a short-circuit welding waveform before and after adjustment before welding is started provided by an embodiment of the present invention;

[0036] Figure 3A comparison diagram of a short-circuit welding waveform before and after adjustment when the actual welding current is greater than the current setting value in a welding process provided by an embodiment of the present invention;

[0037] Figure 4 A comparison diagram of a short-circuit welding waveform before and after adjustment when the actual welding current is less than the current setting value in a welding process provided by an embodiment of the present invention;

[0038] Figure 5 A schematic structural diagram of a short-circuit welding waveform improvement device for fusion-type short-circuit gas shielded welding provided in an embodiment of the present invention. DETAILED DESCRIPTION

[0039] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the embodiments and the accompanying drawings. Here, the illustrative embodiments of the present invention and their descriptions are used to explain the present invention, but are not intended to limit the present invention.

[0040] See also Figure 1 The present invention provides a method for improving the short-circuit welding waveform of a fusion-type short-circuit gas shielded welding, comprising:

[0041] S100, obtaining an initial current setting value and an initial short-circuit waveform parameter of a welding power source.

[0042] During implementation, before the arc sensor signal is identified, it is necessary to record the relevant initial welding parameters and initial short-circuit waveform parameters. The initial welding parameters include the initial current setting value, and the initial short-circuit waveform parameters include: the arc current SPI in the arcing stage, the arc current duration T in the arcing stage, the first short-circuit rising slope L1 in the short-circuit stage, the second short-circuit rising slope L2 and the short-circuit current inflection point S1.

[0043] S110, before welding starts, after receiving the arc sensor signal, the short-circuit welding waveform under the current welding current setting value is adjusted according to the initial current setting value and the initial short-circuit waveform parameters.

[0044] During implementation, the arc sensing device is connected to the welding system and starts to supply power. The arc sensing device will send an arc sensing signal to the welding power supply. After receiving the arc sensing signal, the welding power supply will adjust the short-circuit welding waveform under the current welding current setting value. The specific adjustment idea is: adjust the short-circuit first rising slope L1 and the short-circuit second rising slope L2, and keep the other parameters unchanged, while ensuring that the average current value in the adjusted short-circuit welding waveform is equal to the initial current setting value.

[0045] In a specific implementation, the short-circuit first rising slope L1 and the short-circuit second rising slope L2 may be adjusted according to the following expression:

[0046] L1'=K1*S1+L1

[0047] L2'=K2*S1+L2

[0048] Among them, L1' represents the adjusted short-circuit first rising slope, K1 is a preset positive value, L2' is the adjusted short-circuit second rising slope, and K2 is a preset negative value; after adjustment, the short-circuit first rising slope L1' increases, and the short-circuit second rising slope L2' decreases. The adjusted L1', L2' and other unadjusted parameters are recorded as the short-circuit waveform parameters of the adjusted short-circuit welding waveform. The adjustment effect is shown in FIG. Figure 2 shown.

[0049] S120, welding is performed according to the current setting value and short-circuit waveform parameters defined in the adjusted short-circuit welding waveform.

[0050] S130, during the welding process, obtaining the actual welding current, and adjusting the arc current duration in the short-circuit welding waveform according to the actual welding current and the current setting value.

[0051] In practice, after welding starts, due to the change of dry extension length and other reasons, the actual welding current will have a certain deviation from the current setting value. In order to ensure that the actual welding current is consistent with the current setting value, the arc current duration is adjusted to control it. Specifically, the actual welding current is compared with the current setting value. When the actual welding current is greater than the current setting value, the arc current duration is reduced. The adjustment effect is as follows: Figure 3 As shown; when the actual welding current is less than the current setting value, increase the arc current duration, the adjustment effect is as follows Figure 4 As shown in the figure, when the actual welding current is equal to the current setting value, the arc current duration is kept unchanged.

[0052] The above short-circuit welding waveform improvement method is adopted. After actual welding verification, when using arc sensing, the accuracy of arc sensor tracking is significantly improved. During the welding process, the arc state is stable, the weld is well formed, and the adaptability to complex welding conditions is improved.

[0053] See also Figure 5 , a short-circuit welding waveform improvement device for fusion-type short-circuit gas shielded welding provided by an embodiment of the present invention comprises:

[0054] The data acquisition module 500 is used to obtain the initial current setting value and initial short-circuit waveform parameters of the welding power source;

[0055] The pre-welding adjustment module 510 is used to adjust the short-circuit welding waveform under the current welding current setting value according to the initial current setting value and the initial short-circuit waveform parameters before welding starts after receiving the arc sensor signal;

[0056] A welding control module 520 for performing welding according to the current setting value and the short-circuit waveform parameters defined in the adjusted short-circuit welding waveform;

[0057] The welding adjustment module 530 is used to obtain the actual welding current during the welding process, and adjust the arc current duration in the short-circuit welding waveform according to the actual welding current and the current setting value.

[0058] In implementation, the initial short-circuit waveform parameters include: arcing current SPI in the arcing stage, arcing current duration T in the arcing stage, short-circuit first rising slope L1 in the short-circuit stage, short-circuit second rising slope L2 and short-circuit current inflection point S1.

[0059] In implementation, the pre-welding adjustment module 510 is specifically used to adjust the short-circuit first rising slope L1 and the short-circuit second rising slope L2, and the other parameters remain unchanged, while ensuring that the average current value in the adjusted short-circuit welding waveform is equal to the initial current setting value.

[0060] In implementation, the pre-welding adjustment module 510 is specifically used to adjust the short-circuit first rising slope L1 and the short-circuit second rising slope L2 according to the following expression:

[0061] L1'=K1*S1+L1

[0062] L2'=K2*S1+L2

[0063] Wherein, L1' represents the adjusted short-circuit first rising slope, K1 is a preset positive value, L2' represents the adjusted short-circuit second rising slope, and K2 is a preset negative value.

[0064] During implementation, the welding adjustment module 530 is specifically used to compare the actual welding current and the current setting value. When the actual welding current is greater than the current setting value, the arc current duration is reduced; when the actual welding current is less than the current setting value, the arc current duration is increased; when the actual welding current is equal to the current setting value, the arc current duration is kept unchanged.

[0065] The above description is only a preferred embodiment of the present invention and is not intended to limit the protection scope of the present invention. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention are included in the protection scope of the present invention.

Claims

1. A method for improving the short-circuit welding waveform of fusion short-circuit gas shielded welding, characterized in that: include: Obtaining an initial current setting value and initial short-circuit waveform parameters of a welding power source; Before welding starts, after receiving the arc sensor signal, the short-circuit welding waveform under the current welding current setting value is adjusted according to the initial current setting value and the initial short-circuit waveform parameters; Welding is performed according to the current setting value and short-circuit waveform parameters defined in the adjusted short-circuit welding waveform; During welding, the actual welding current is obtained, and the arc current duration in the short-circuit welding waveform is adjusted according to the actual welding current and the current setting value; The initial short-circuit waveform parameters include: arcing current SPI in the arcing stage, arcing current duration T in the arcing stage, short-circuit first rising slope L1 in the short-circuit stage, short-circuit second rising slope L2 and short-circuit current inflection point S1; The process of adjusting the short-circuit welding waveform under the current welding current setting value according to the initial current setting value and the initial short-circuit waveform parameters includes: Adjust the short circuit first rising slope L1 and the short circuit second rising slope L2, and keep other parameters unchanged, while ensuring that the average current value in the adjusted short circuit welding waveform is equal to the initial current setting value; The process of adjusting the short-circuit first rising slope L1 and the short-circuit second rising slope L2 includes: Adjust the short-circuit first rising slope L1 and the short-circuit second rising slope L2 according to the following expressions: L1'=K1*S1+L1 L2'=K2*S1+L2 Wherein, L1' represents the adjusted short-circuit first rising slope, K1 is a preset positive value, L2' represents the adjusted short-circuit second rising slope, and K2 is a preset negative value.

2. The method for improving the short-circuit welding waveform of the fusion short-circuit gas shielded welding according to claim 1, characterized in that: The process of adjusting the arc current duration in the short-circuit welding waveform according to the actual welding current and the current setting value includes: Compare the actual welding current with the current setting value. When the actual welding current is greater than the current setting value, reduce the arc current duration; when the actual welding current is less than the current setting value, increase the arc current duration; when the actual welding current is equal to the current setting value, keep the arc current duration unchanged.

3. A short-circuit welding waveform improvement device for fusion short-circuit gas shielded welding, characterized in that: include: A data acquisition module, used to obtain an initial current setting value and an initial short-circuit waveform parameter of a welding power source; A pre-welding adjustment module is used to adjust the short-circuit welding waveform under the current welding current setting value according to the initial current setting value and the initial short-circuit waveform parameters before welding starts after receiving the arc sensor signal; A welding control module, for performing welding according to a current setting value and short-circuit waveform parameters defined in the adjusted short-circuit welding waveform; The welding adjustment module is used to obtain the actual welding current during the welding process and adjust the arc current duration in the short-circuit welding waveform according to the actual welding current and the current setting value; The initial short-circuit waveform parameters include: arcing current SPI in the arcing stage, arcing current duration T in the arcing stage, short-circuit first rising slope L1 in the short-circuit stage, short-circuit second rising slope L2 and short-circuit current inflection point S1; The pre-welding adjustment module is specifically used to adjust the short-circuit first rising slope L1 and the short-circuit second rising slope L2, and the other parameters remain unchanged, while ensuring that the average current value in the adjusted short-circuit welding waveform is equal to the initial current setting value; The pre-welding adjustment module is specifically used to adjust the short-circuit first rising slope L1 and the short-circuit second rising slope L2 according to the following expression: L1'=K1*S1+L1 L2'=K2*S1+L2 Wherein, L1' represents the adjusted short-circuit first rising slope, K1 is a preset positive value, L2' represents the adjusted short-circuit second rising slope, and K2 is a preset negative value.

4. The short-circuit welding waveform improvement device for short-circuit gas shielded welding according to claim 3, characterized in that: The welding adjustment module is specifically used to compare the actual welding current with the current setting value, and when the actual welding current is greater than the current setting value, the arc current duration is reduced; when the actual welding current is less than the current setting value, the arc current duration is increased; When the actual welding current is equal to the current setting value, the arc current duration is kept unchanged.

Citation Information

Patent Citations

  • Arc welding method and arc welding device

    CN102123812A

  • Arc welding methods and arc welding equipment

    CN102271853A

  • Short-circuit transient welding method and system

    CN108057942A

  • Welding current waveform adjusting method and device

    CN114749766A

  • Direct current welding control method and device

    CN115041778A