Process for the production of a foam sheet for the production of a foamed film
By removing the outer skin of the foam block and cutting it into foam boards of a specific thickness, the problems of debris and heat damage during foam film cutting in the prior art are solved, enabling the production of high-quality foam films suitable for applications such as smartphone speakers.
Patent Information
- Application Number
- CN202180073140.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-10-29
- Filing Date
- 2021-10-12
- Publication Date
- 2026-05-15
- Estimated Expiration
- 2041-10-12
AI Technical Summary
Existing technologies struggle to cut foam films less than 3 mm thick without debris, and suffer from thermal damage and material loss, particularly pinholes and insufficient elongation at break.
The foam block is cut by removing its outer skin and cutting the remaining part into foam boards with a thickness between 10 and 135 mm using a laser, band knife, or band saw. The polymer with a glass transition temperature (Tg) of at least 100 °C, an average cell diameter between 20 μm and 250 μm, and an elongation at break between 4% and 13% is selected.
It achieves chip-free cutting, avoids thermal damage and material loss, and produces high-quality foam films suitable for film production with a thickness of less than 3mm. It has excellent mechanical properties and a uniform cell structure.
Abstract
Description
Technical Field
[0001] This invention relates to a method for preparing a foam board for producing a foam film, wherein the foam film is formed from a material with a glass transition temperature T. g The polymer composition is at least 100°C, characterized in that the average cell diameter, as measured according to standard ASTM D 3576, is between 20 μm and 250 μm, and there are fewer than 20 cells per square meter with a diameter >260 μm, and the elongation at break of the foam, as measured according to ASTM D 638, is 4%-13%. Background Technology
[0002] Similar to other foams, rigid foams, such as those named after the product... The polymethacrylamide sold can be cut using different methods. In such cases, the standard method for performing this operation is by sawing. This involves horizontally slicing thick blocks of foam using a band saw, thus producing a significant amount of sawdust. Furthermore, it is virtually impossible to obtain thin or very thin sheets or films from rigid foam by this method. Very thin films are simply not achievable due to the thickness of the saw blade and the relatively high mechanical stress on the area of rigid foam to be cut during sawing. Thin sheets between 3 and 10 mm thick are only possible with significant material loss and substantial dust formation, as the saw blade used for sawing has a significant thickness of at least 2 mm, resulting in corresponding material loss. If the saw blade is particularly thin, it will sag, leading to large thickness variations in the cut product and / or making film cutting virtually impossible. Similarly, problems arise during sawing when slicing thicker sheets exceeding 10 mm, as the bending of the area to be cut due to the thickness of the saw blade causes it to break during slicing. This is a problem particularly prevalent with very rigid and therefore somewhat brittle foams.
[0003] Flexible foams, such as flexible polyurethane foam, can also be cut using a belt cutter without producing sawdust as waste.
[0004] Many types of foam (rigid and flexible) can also be cut using heated tension wire. However, there is a possibility of thermal damage to the material due to the hot wire. Additionally, there is a risk of material loss or sheet breakage due to the limited thickness of the wire.
[0005] US 10,556,357 describes a method for planar segmentation of rigid foam suitable for obtaining films or sheets. This method is characterized by first softening the rigid foam and then cutting it with a knife. Due to the presence of multiple pinholes, the foam film described in this intellectual property exhibits insufficient elongation at break. Summary of the Invention
[0006] Technical problems to be solved
[0007] In the context of the prior art discussed, the problem addressed by the present invention is to provide a method for preparing a foam board from which a thin foam film can be provided, which is formed by the glass transition temperature T. g Made of polymers heated to at least 100°C, it has small pore diameters and almost no pinholes.
[0008] The method for preparing the foam boards should be particularly suitable for preparing foam films with a thickness of less than 3 mm from these foam boards. The slitting of the foam boards should be carried out without the formation of debris.
[0009] Other issues not explicitly discussed herein may be derived from the prior art, the specification, the claims, or exemplary embodiments.
[0010] Solution
[0011] This problem is solved by providing a method for preparing a foam board for producing a foam film, wherein the foam film has a glass transition temperature T g The foam board is composed of a polymer with a temperature of at least 100°C, and has an average cell diameter between 20 μm and 250 μm as measured according to standard ASTM D3576, and fewer than 20 cells per square meter with a diameter >260 μm, and an elongation at break between 4% and 13% as measured according to ASTM D 638.
[0012] A) Remove the foam skin from the foam block, and
[0013] B) Cut the remaining portion of the foam block into foam boards with a thickness between 10 and 135 mm.
[0014] The foam board according to the invention is prepared from a polymer having a glass transition temperature T of at least 100°C, preferably at least 140°C, as measured according to DIN EN ISO 11357-2. g The standard for plastics, DIN EN ISO 11357-2 (dated July 2014), describes differential scanning calorimetry (DSC) – Part 2: determination of glass transition temperature and activation energy of glass transition.
[0015] The polymer is selected from polyethersulfone, polyphenylsulfone, polyetheretherketone, poly(meth)acrylimide, poly(meth)methyl acrylate, polyetherimide, polysulfone, polyurethane, polyethylene terephthalate and mixtures thereof, as well as copolymers thereof.
[0016] The term "poly(meth)acrylimide" (P(M)I) is understood below to mean polymethacrylimide (PMI), polyacrylimide (PI), or mixtures thereof. A similar interpretation applies, for example, to poly(methyl methacrylate). Therefore, the term "poly(methyl methacrylate)" should be understood to mean not only polymethyl methacrylate but also polymethyl methacrylate and mixtures thereof.
[0017] The preferred material for the foam core is P(M)I, with PMI being particularly preferred. Such P(M)I foam is also known as rigid foam and exhibits exceptional strength. The preparation of P(M)I foam is described, for example, in EP 3221101. The P(M)I foam is typically prepared in a two-stage process: a) preparing a casting polymer, and b) foaming this casting polymer.
[0018] The casting polymer is prepared by first preparing a monomer mixture comprising (meth)acrylic acid and (meth)acrylonitrile in a molar ratio preferably of 2:3 to 3:2 as the main components. Additionally, other comonomers may be used, such as esters of acrylic acid or methacrylic acid, styrene, maleic acid or itaconic acid or their anhydrides, or vinylpyrrolidone. However, the proportion of the comonomer should not exceed 30% by weight. A small amount of crosslinking monomer, such as allyl acrylate, may also be used. However, the amount should preferably be at most 0.05 to 2.0% by weight.
[0019] The mixture used for copolymerization further contains a foaming agent that either decomposes or evaporates to form a gas phase at a temperature of about 150 to 250°C. Polymerization occurs below this temperature, thus the cast polymer contains a potential foaming agent. The polymerization advantageously occurs in block form between two glass plates. To prepare a foamed sheet, the cast polymer is then foamed at a suitable temperature in a second step according to existing techniques. The preparation of these P(M)I foams is known in principle to those skilled in the art and can be found, for example, in EP 1 444 293, EP 1678 244 or WO 2011 / 138060. Examples of PMI foams include those from Evonik Industries AG, Germany. In terms of preparation and processing, acrylamide foam can be considered similar to PMI foam. However, for toxicological reasons, these materials are generally less preferred compared to other foam materials.
[0020] The density of the rigid foam material can be selected relatively freely. P(M)I foam can range from, for example, 20 to 320 kg / m³. 3 Preferred weight is 25 to 250 kg / m³. 3 Use within the density range. Particularly preferred is a density between 30 and 200 kg / m³. 3 The PMI bubble between them.
[0021] The foam described here is prepared in the form of foam blocks. These foam blocks have different thicknesses depending on the polymer used and the density achieved.
[0022] It has been found that using only a specific area of foam derived from the foam block is particularly advantageous. It has also been found that removing the foam skin / surface from the foam block results in foam boards with excellent mechanical properties.
[0023] Preferably, 3 mm, particularly 5 mm, very particularly preferred 10 mm, and especially preferred 15 mm of the surface / foam skin of the foam block are removed. The remaining material has better cell size uniformity and elongation at break, and is therefore suitable for processing into foam boards.
[0024] The remaining portion of the foam block is cut into foam boards with a thickness between 10 and 135 mm, preferably between 60 and 125 mm, and particularly preferably 75 mm thick.
[0025] Various methods for cutting foam boards from foam blocks are known. Laser, band knife, or band saw are preferred methods for cutting.
[0026] The foam board prepared according to the present invention is particularly suitable for the production of foam films.
[0027] The foam board can be used to produce foam films with particularly low thickness. Thin foam films with a thickness between 0.05 and 3 mm can be produced. Preferably, foam films with a thickness between 0.15 and 1 mm are obtained.
[0028] A particular problem in foam film production is pinholes. In this document, the term "pinhole" refers to a relatively large pore that appears on the surface of the film and causes a reduction in strength. In extreme cases, the pore size is larger than the thickness of the film, thus resulting in voids within the film.
[0029] According to the invention, the foam film has an average cell diameter between 20 μm and 250 μm, preferably between 50 μm and 220 μm, and particularly preferably between 80 μm and 200 μm, as measured according to standard ASTM D 3576. Standard ASTM D 3576 (2015 edition) is used to determine the cell size of rigid foams.
[0030] To achieve the desired mechanical properties, particularly elongation at break, there should be fewer than 20 cells per square meter with a diameter >260 μm. Preferably, there should be fewer than 15 cells per square meter with a diameter >260 μm.
[0031] The preferred foam film has an elongation at break between 4% and 30%, particularly preferably between 5% and 10%, as measured according to ASTM D 638 (2014 edition). ASTM D 638 corresponds to ISO 527-1 and is the standard test method for determining the tensile properties of plastics.
[0032] Specifically, particularly rigid foams with high stiffness and brittleness, such as rigid P(M)I foam, may encounter problems with thick plates breaking during cutting, especially because the blade has a wedge-shaped cross-section.
[0033] Foams with specific properties, such as high elongation at break and a cellular structure, are suitable for splitting into thin layers. Splitting rigid foam is a very efficient method for preparing thin layers, for example, those used in smartphone speakers. The high elongation at break of the foam benefits process stability and achievable layer thicknesses due to the mechanical requirements of the splitting method (deflection of the cut film at the cutter bar). Since the cut foam film is bonded to a very thin layer of aluminum foil, relatively rough and uneven cellular structures become readily visible, thus requiring the finest and most uniform cellular structure possible.
[0034] In a variation of the method, the still-heated rigid foam is split directly after the foaming operation in an oven or a heated press.
[0035] There are also multiple implementation schemes for the arrangement of the knives.
[0036] In a preferred embodiment, the rigid foam plate moves at a right angle to the cutting surface of the blade, while the blade moves only at a right angle to the transport direction of the rigid foam plate. Alternatively, although less preferred, the blade moves along a fixed rigid foam during the cutting operation. The blade and the rigid foam can also have opposite directions of movement, in which case, in the latter two variations, the blade can effectively move at a right angle to the rigid foam, in addition to the support body for the cutting operation.
[0037] When the blade moves at a right angle, there are also two variations. First, the blade can move reciprocally. However, a belt blade is preferred. This type of belt blade moves in a loop in a direction perpendicular to the cutting direction and is typically guided and driven by at least two deflecting rollers. Belt blade systems are commercially available.
[0038] In one particular implementation, several workpieces, such as films or sheets, are cut from rigid foam in a single motion using multiple blades arranged sequentially. These can be, in particular, several belt blades arranged in series. Thus, multiple workpieces can be cut from a single block in a very efficient manner in a single operation.
[0039] Alternatively or additionally, the film can then be covered with at least one outer layer. These outer layers can be, for example, composite materials, metals, or wood. This allows for the use of sandwich materials, for example, in lightweight constructions. Alternatively, the outer layer can simply be a protective film or decorative layer that can be removed again. In particular, the application of very thin aluminum foil is of particular interest.
[0040] A significant advantage of this invention is that it virtually eliminates the generation of waste in the form of sawdust during the cutting of rigid foam and eliminates thermal damage to the surface of the rigid foam. This allows for limited material loss and makes the method more economical overall than prior art methods.
[0041] Thin foam films have a very wide range of applications. For example, they can be used as membranes, particularly in speakers, portable music players, or headphones. They can also be considered for decorative purposes, such as surface finishing of articles.
Claims
1. A method for preparing a foam board for producing a foam film, wherein the foam film has a glass transition temperature T g The foam board is composed of a polymer with a temperature of at least 100°C, and has an average cell diameter between 20 µm and 250 µm as measured according to standard ASTM D 3576, with fewer than 20 cells per square meter having a diameter > 260 µm, and an elongation at break between 4% and 13% as measured according to ASTM D 638. A) Remove the foam skin from the foam block, and B) Cut the remaining portion of the foam block into foam boards with a thickness between 60 and 135 mm.
2. The method of claim 1, wherein the polymer has a glass transition temperature of at least 140°C.
3. The method according to claim 1 or 2, wherein the polymer is selected from polyethersulfone, polyphenylsulfone, polyetheretherketone, poly(meth)acrylimide, poly(meth)acrylate, polyetherimide, polysulfone, polyurethane, polyethylene terephthalate and mixtures thereof, and copolymers thereof.
4. The method according to claim 1 or 2, wherein the average cell diameter of the foam board is between 50 µm and 220 µm.
5. The method of claim 4, wherein the average cell diameter of the foam board is between 80 µm and 200 µm.
6. The method according to claim 1 or 2, wherein there are fewer than 15 cells per square meter of foam board with a cell diameter > 260 μm.
7. The method according to claim 1 or 2, wherein the elongation at break of the foam board is 5%-10% as measured according to ASTM D 638.
8. The method according to claim 1 or 2, wherein the foam skin of the foam block in step A) has a thickness of 3 mm.
9. The method according to claim 1 or 2, wherein the foam board in step B) is cut using a band cutter or band saw.