Method for purifying crude ammonium fluoride

By combining the electrochemical exchange method with anhydrous ethanol, the problem of difficulty in removing hydrogen fluoride impurities in ammonium fluoride is solved, and efficient and low-energy purification of ammonium fluoride is achieved, reaching a purity of more than 99.6 wt% and nearly 100% Recovery rate.

CN117165960BActive Publication Date: 2024-10-11FUJIAN TIANFU ELECTRONIC MATERIAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310470921.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-04-27
Publication Date
2024-10-11
Estimated Expiration
2043-04-27

AI Technical Summary

Technical Problem

The hydrogen fluoride impurity that is difficult to remove in the existing ammonium fluoride preparation process results in low product purity, and the traditional multiple recrystallization method consumes high energy and has low efficiency.

Method used

An electrolytic cell is used for electrochemical exchange, and a basic alkali metal compound aqueous solution and a copper electrode are used for electrolysis. Through ion exchange and solubility difference, hydrogen fluoride impurities are removed, and the use of absolute ethanol and calcium oxide is combined to achieve efficient purification of ammonium fluoride.

Benefits of technology

It achieves an ultra-high purity of ammonium fluoride of more than 99.6 wt% and a recovery rate of nearly 100%, reduces energy consumption, simplifies the process flow, and is suitable for industrial production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
Patent Text Reader

Abstract

The present invention belongs to the field of chemical technology, and in particular, relates to a method for purifying crude ammonium fluoride. The method comprises: (1) providing an electrolytic cell, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane, wherein an inert cathode is provided in the cathode region, and an alkaline alkali metal compound aqueous solution and a copper electrode are provided in the anode region; (2) the crude ammonium fluoride solution is used as the cathode region electrolyte, and an electric current is applied for electrolysis treatment; (3) the electrolysis treatment is carried out until the potential rises to a threshold value, and the cathode region electrolyte is recovered; (4) the recovered cathode region electrolyte is mixed with excess anhydrous ethanol, and then calcium oxide is added to remove water and dry, and the precipitate is filtered and removed, and then crystallized under low temperature conditions to obtain a purified ammonium fluoride product. The present invention adopts an electrochemical exchange method to directly and effectively remove impurities that are usually difficult to remove by crystallization or distillation processes, thereby greatly improving the purity of the product; compared with traditional purification methods, the present invention has the characteristics of simplicity, high efficiency and low energy consumption, and is adapted to the needs of industrial production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of chemical engineering, and in particular relates to a method for purifying crude ammonium fluoride. Background Art

[0002] Ammonium fluoride is a white crystal with the molecular formula NH4F. It is easily deliquescent and decomposes into ammonia and hydrogen fluoride when heated or exposed to hot water. It can corrode glass. Ammonium fluoride can be obtained by neutralizing hydrofluoric acid and ammonia water and then concentrating and crystallizing.

[0003] In the actual production process, the properties of ammonium fluoride are extremely unstable, and usually the reaction temperature and reaction materials need to be relatively strictly controlled. Usually, an excess of hydrogen fluoride and ammonia are reacted in a liquid phase or a gas phase to prepare a mixture of ammonium fluoride and hydrogen fluoride, and then a relatively high-purity product of ammonium fluoride is prepared through multiple crystallization processes.

[0004] However, due to the actual existence of NH-F hydrogen bonds in ammonium fluoride, the hydrogen bonding effect causes a certain amount of unavoidable and almost difficult to remove hydrogen fluoride impurities to still exist in the purified product actually obtained, and the impurities may exist in the form of ammonium bifluoride and the like. Summary of the invention

[0005] In order to solve the problem that most of the existing ammonium fluoride preparation processes use excessive hydrofluoric acid to increase the output and actual industrial benefits, resulting in the presence of hydrofluoric acid impurities that are difficult to remove in the ammonium fluoride product, the present invention provides a method for purifying crude ammonium fluoride.

[0006] The main purposes of the present invention are: first, to be able to efficiently and thoroughly remove a small amount of hydrogen fluoride remaining in the ammonium fluoride product; second, the removal effect is simple and efficient, and the energy consumption is relatively low.

[0007] To achieve the above objectives, the present invention adopts the following technical solutions.

[0008] A method for purifying crude ammonium fluoride comprises: (1) providing an electrolytic cell, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane, wherein an inert cathode is provided in the cathode region, and an alkaline alkali metal compound aqueous solution and a copper electrode are provided in the anode region; (2) placing a crude ammonium fluoride solution in the cathode region as a cathode region electrolyte, and applying power to perform electrolytic treatment; (3) performing the electrolytic treatment until the potential rises to a threshold value, terminating the electrolytic process and recovering the cathode region electrolyte; and (4) mixing the recovered cathode region electrolyte with excess anhydrous ethanol, adding calcium oxide, removing water, and drying, filtering to remove precipitates, and then crystallizing under low temperature conditions to obtain a purified ammonium fluoride product.

[0009] The present invention adopts the method of ion directional exchange, so that the hydrogen fluoride in the crude ammonium fluoride solution is fully converted. In the specific process, in the anode area, the selected alkaline alkali metal compound aqueous solution can generally adopt sodium hydroxide aqueous solution and / or potassium hydroxide aqueous solution. In the actual industrial production process, a saturated solution can be directly used or sodium hydroxide and / or potassium hydroxide with at least 1.3 times the hydrogen fluoride content in the crude solution can be used to prepare an aqueous solution according to the characterization results of the crude solution. During the electrolysis process, the copper electrode loses electrons and oxidizes into the alkaline alkali metal compound aqueous solution and complexes and precipitates to avoid copper ions entering the cathode area to cause loss of ammonium ions. During the electrolysis process, the hydrogen ions in the cathode area are reduced to hydrogen. In order to maintain the electrical neutrality of the electrolysis system, the cationic alkali metal ions in the anode area, that is, sodium ions and / or potassium ions are exchanged and enter the cathode area. After the electrolysis treatment is completed, the components in the cathode area electrolyte recovered are converted into ammonium fluoride and sodium fluoride and / or potassium fluoride, and instead of the traditional method of removing hydrogen fluoride by multiple recrystallizations, the present invention uses solubility differences to directly separate sodium fluoride and potassium fluoride. In anhydrous ethanol, ammonium fluoride still maintains a certain solubility, but sodium fluoride and potassium fluoride are insoluble, and since the fluorine content in the solution increases after the ammonium fluoride is dissolved, the dissolution of sodium fluoride and potassium fluoride is actually further limited. Therefore, after dehydration and drying, the present invention uses a special recrystallization method to directly, effectively and thoroughly remove excess fluoride impurities, thereby obtaining an ultra-high purity ammonium fluoride product with a purity of more than 99.6 wt%, and the recovery rate of ammonium fluoride is close to 100%, and no loss of ammonium fluoride will occur.

[0010] Preferably, in step (1), the inert cathode is a carbon electrode.

[0011] The carbon electrode is reactive and inert in the system of the present invention, and can avoid the introduction of impurities.

[0012] Preferably, during the constant current electrolysis treatment in step (2), the starting voltage is controlled to be 1.23 V, and the potential voltage threshold in step (3) is 1.32 V.

[0013] During the constant current electrolysis process, as the solution systems in the anode and cathode regions change, the electrolysis potential will change. In the actual production and preparation process, after rising to the above voltage threshold, it can be basically determined that the hydrogen fluoride in the cathode electrolyte has been completely reacted.

[0014] Preferably, when the cathode electrolyte recovered in step (4) is mixed with excess anhydrous ethanol, at least 48 times the volume of anhydrous ethanol is added to the cathode electrolyte.

[0015] A large amount of anhydrous ethanol is used to ensure that the ammonium fluoride in the cathode electrolyte can be effectively recovered to improve the recovery rate of the product.

[0016] Preferably, the amount of calcium oxide used in step (4) is controlled so that its loose volume is at least 0.8 times the recovered cathode electrolyte.

[0017] The present invention uses excessive calcium oxide to remove residual water in the cathode electrolyte because water and anhydrous ethanol are miscible and the presence of water will affect the impurity content in the final product.

[0018] Preferably, the purified ammonium fluoride product obtained in step (4) is slowly dissolved in anhydrous ethanol until the purified ammonium fluoride product no longer dissolves, followed by solid-liquid separation to remove solid matter, and the anhydrous ethanol solution of ammonium fluoride is crystallized again to obtain an ultra-high purity ammonium fluoride product.

[0019] The purified product is subjected to dropwise purification again to further remove a very small amount of residual impurities, so that the purity of the ammonium fluoride product is further improved.

[0020] The beneficial effects of the present invention are: (1) the present invention adopts the electrochemical exchange method to directly and effectively remove impurities that are usually difficult to remove by crystallization or distillation processes, thereby greatly improving the purity of the product; (2) compared with traditional purification methods, the present invention is simple, efficient and low in energy consumption, and is suitable for industrial production needs. DETAILED DESCRIPTION

[0021] The present invention is further described in detail below in conjunction with specific embodiments. Those of ordinary skill in the art will be able to implement the present invention based on these descriptions. In addition, the embodiments of the present invention involved in the following description are generally only embodiments of a part of the present invention, rather than all embodiments. Therefore, based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without making creative work should fall within the scope of protection of the present invention.

[0022] Unless otherwise specified, the raw materials used in the examples of the present invention are all commercially available or available to those skilled in the art; unless otherwise specified, the methods used in the examples of the present invention are all methods known to those skilled in the art.

[0023] Unless otherwise specified, the crude ammonium fluoride solution used in the embodiments of the present invention is prepared by dissolving the currently industrially produced ammonium fluoride product in water. The purity of the industrially produced ammonium fluoride is 93-95%, and the impurity components are hydrogen fluoride and / or ammonium bifluoride.

[0024] Embodiment 1: A method for purifying crude ammonium fluoride comprises: (1) providing an electrolytic cell, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane), wherein a carbon electrode is provided in the cathode region, and a saturated sodium hydroxide aqueous solution is provided in the anode region as an electrolyte in the anode region, wherein the sodium hydroxide equivalent in the saturated sodium hydroxide aqueous solution used is about 2.0 Eq, and a copper electrode is used as an anode electrode; (2) placing a crude ammonium fluoride solution in the cathode region as an electrolyte in the cathode region, applying power for electrolysis, and controlling the starting voltage to be 1.23 V; (3) performing the electrolysis treatment until the potential rises to a threshold value of 1.32 V, terminating the electrolysis process and recovering the electrolyte in the cathode region; (4) mixing the recovered electrolyte in the cathode region with 48 times the volume of anhydrous ethanol, adding industrial quicklime with a loose volume of 0.8 times the volume of the electrolyte in the cathode region, dehydrating and drying, filtering to remove the precipitate, evaporating under low pressure at 20° C., recovering the anhydrous ethanol, and recovering the crystalline product to obtain a purified ammonium fluoride product.

[0025] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery amount is calculated. The purity and ammonium fluoride content of the purified ammonium fluoride product obtained in step (4) are characterized, and the actual recovery amount is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery amount and the actual recovery amount.

[0026] The specific calculation formula for the recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%; through characterization and calculation, the purity of the purified ammonium fluoride product obtained in this embodiment is 99.7%, and the recovery rate is accurate to one decimal place, and the calculated result is 100.0%.

[0027] Example 2: A method for purifying crude ammonium fluoride, comprising: (1) providing an electrolytic cell, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane), wherein a carbon electrode is provided in the cathode region, and a saturated potassium hydroxide aqueous solution is provided in the anode region as an electrolyte in the anode region, wherein the potassium hydroxide equivalent in the saturated potassium hydroxide aqueous solution used is about 2.1 Eq, and a copper electrode is used as an anode electrode; (2) placing a crude ammonium fluoride solution in the cathode region as an electrolyte in the cathode region, applying power for electrolysis, and controlling the starting voltage to be 1.23 V; (3) performing the electrolysis until the potential rises to a threshold value of 1.32 V, terminating the electrolysis process and recovering the electrolyte in the cathode region; (4) mixing the recovered electrolyte in the cathode region with 48 times the volume of anhydrous ethanol, adding industrial quicklime with a bulk volume of 0.8 times that of the electrolyte in the cathode region, dehydrating and drying, filtering to remove the precipitate, evaporating under low pressure at 20° C., recovering the anhydrous ethanol, and recovering the crystalline product to obtain a purified ammonium fluoride product.

[0028] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery amount is calculated. The purity and ammonium fluoride content of the purified ammonium fluoride product obtained in step (4) are characterized, and the actual recovery amount is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery amount and the actual recovery amount.

[0029] The specific calculation formula for the recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%; through characterization and calculation, the purity of the purified ammonium fluoride product obtained in this embodiment is 99.6%, and the recovery rate is accurate to one decimal place, and the calculated result is 99.9%.

[0030] Example 3: A method for purifying crude ammonium fluoride, comprising: (1) providing an electrolytic cell, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane), a carbon electrode is provided in the cathode region, a saturated sodium hydroxide aqueous solution is provided in the anode region as the anode region electrolyte, the sodium hydroxide equivalent in the saturated sodium hydroxide aqueous solution used is about 2.0 Eq, and a copper electrode is used as the anode electrode; (2) placing a crude ammonium fluoride solution in the cathode region as the cathode region electrolyte, applying power for electrolysis, and controlling the starting voltage to be 1.23 V; (3) performing the electrolysis until the potential rises to a threshold value of 1.35 V, terminating the electrolysis process and recovering the cathode region electrolyte; (4) mixing the recovered cathode region electrolyte with 48 times the volume of anhydrous ethanol, adding industrial quicklime with a loose volume of 0.8 times the volume of the cathode region electrolyte, dehydrating and drying, filtering to remove the precipitate, evaporating under low pressure at 20° C., recovering the anhydrous ethanol, and recovering the crystalline product to obtain a purified ammonium fluoride product.

[0031] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery amount is calculated. The purity and ammonium fluoride content of the purified ammonium fluoride product obtained in step (4) are characterized, and the actual recovery amount is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery amount and the actual recovery amount.

[0032] The specific calculation formula of recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%;

[0033] Through characterization and calculation, the purity of the purified ammonium fluoride product obtained in this example is 99.6%, and the recovery rate is accurate to one decimal place, and the calculated result is 99.9%.

[0034] Example 4: A method for purifying crude ammonium fluoride, comprising: (1) providing an electrolytic cell, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane), a carbon electrode is provided in the cathode region, and a saturated sodium hydroxide aqueous solution is provided in the anode region as the anode region electrolyte, wherein the sodium hydroxide equivalent in the saturated sodium hydroxide aqueous solution used is about 2.0 Eq, and a copper electrode is used as the anode electrode; (2) placing a crude ammonium fluoride solution in the cathode region as the cathode region electrolyte, applying power for electrolysis, and controlling the starting voltage to be 1.23 V; (3) performing the electrolysis until the potential rises to a threshold value of 1.32 V, terminating the electrolysis process and recovering the cathode region electrolyte; (4) mixing the recovered cathode region electrolyte with anhydrous ethanol having a volume of 48 times that of the recovered cathode region electrolyte, and then adding 0.8 times the volume of the cathode region electrolyte to the recovered cathode region electrolyte; (5) at least 50 kg of purified ammonium fluoride product is slowly dissolved in anhydrous ethanol, and the rate of adding anhydrous ethanol is controlled to add 15 mL of anhydrous ethanol per minute per gram of purified ammonium fluoride product, until the purified ammonium fluoride product no longer dissolves within 2 minutes, and then vacuum filtration is performed to separate and remove insoluble matter, and the anhydrous ethanol solution of ammonium fluoride is placed at 20 ° C. The evaporation is carried out at a low pressure, the anhydrous ethanol is recovered, and the crystallized product is recovered to obtain an ultra-high purity ammonium fluoride product.

[0035] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery amount is calculated. The purity and ammonium fluoride content of the ultra-high purity ammonium fluoride product obtained in step (5) are characterized, and the actual recovery amount is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery amount and the actual recovery amount.

[0036] The specific calculation formula for the recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%; through characterization and calculation, the purity of the purified ammonium fluoride product obtained in this embodiment is 99.9%, and the recovery rate is accurate to one decimal place, and the calculated result is 99.9%.

[0037] Example 5: A method for purifying crude ammonium fluoride, comprising: (1) providing an electrolytic cell, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane), a carbon electrode is provided in the cathode region, and a saturated potassium hydroxide aqueous solution is provided in the anode region as the anode region electrolyte, wherein the potassium hydroxide equivalent in the saturated potassium hydroxide aqueous solution used is about 2.1 Eq, and a copper electrode is used as the anode electrode; (2) placing a crude ammonium fluoride solution in the cathode region as the cathode region electrolyte, applying power for electrolysis, and controlling the starting voltage to be 1.23 V; (3) performing the electrolysis until the potential rises to a threshold value of 1.32 V, terminating the electrolysis process and recovering the cathode region electrolyte; (4) mixing the recovered cathode region electrolyte with anhydrous ethanol having a volume of 48 times that of the recovered cathode region electrolyte, and then adding 0.8 times the volume of the cathode region electrolyte to the recovered cathode region electrolyte; (5) at least 50 kg of purified ammonium fluoride product is slowly dissolved in anhydrous ethanol, and the rate of adding anhydrous ethanol is controlled to add 15 mL of anhydrous ethanol per minute per gram of purified ammonium fluoride product, until the purified ammonium fluoride product no longer dissolves within 2 minutes, and then vacuum filtration is performed to separate and remove insoluble matter, and the anhydrous ethanol solution of ammonium fluoride is placed at 20 ° C. The evaporation is carried out at a low pressure, the anhydrous ethanol is recovered, and the crystallized product is recovered to obtain an ultra-high purity ammonium fluoride product.

[0038] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery amount is calculated. The purity and ammonium fluoride content of the ultra-high purity ammonium fluoride product obtained in step (5) are characterized, and the actual recovery amount is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery amount and the actual recovery amount.

[0039] The specific calculation formula of recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%;

[0040] Through characterization and calculation, the purity of the purified ammonium fluoride product obtained in this example is 99.9%, and the recovery rate is accurate to one decimal place, and the calculated result is 99.9%.

[0041] Comparative Example 1: A method for purifying crude ammonium fluoride, comprising: (1) providing an electrolytic cell, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane), a carbon electrode is provided in the cathode region, a sodium hydroxide aqueous solution is provided in the anode region as the anode region electrolyte, and a copper electrode is used as the anode electrode; (2) placing a crude ammonium fluoride solution in the cathode region as the cathode region electrolyte, applying power for electrolysis, and controlling the starting voltage to be 1.23 V; (3) performing the electrolysis treatment until the potential rises to a threshold value of 1.32 V, terminating the electrolysis process and recovering the cathode region electrolyte; (4) mixing the recovered cathode region electrolyte with 48 times the volume of anhydrous ethanol, adding industrial quicklime with a loose volume of 0.8 times that of the cathode region electrolyte, dehydrating and drying, filtering to remove the precipitate, evaporating under low pressure at 20°C, recovering the anhydrous ethanol, and recovering the crystalline product to obtain a purified ammonium fluoride product.

[0042] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery amount is calculated. The purity and ammonium fluoride content of the purified ammonium fluoride product obtained in step (4) are characterized, and the actual recovery amount is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery amount and the actual recovery amount.

[0043] The specific calculation formula of the recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%; the amount of sodium hydroxide in the sodium hydroxide aqueous solution in step (1) is recorded in equivalent (Eq), where 1 Eq means that 1.0 times the content of hydrogen fluoride in the crude product solution is used to prepare the aqueous solution. The preparation results of different equivalents are shown in the following table.

[0044] In the table: product recovery rate is the ammonium fluoride recovery rate.

[0045] It can be seen from the above characterization test results that the equivalent of the alkali metal hydroxide used in the anode electrolyte in the technical solution of the present invention has little practical effect on the recovery rate of ammonium fluoride, but has a greater impact on the purity. The use of low equivalents of sodium hydroxide will limit the ion exchange process to a certain extent, resulting in a decrease in the degree of removal of hydrogen fluoride. In order to ensure the production of ammonium fluoride products with a purity of 99.5%, which is a high industrial standard, at least 1.3 Eq of alkali metal hydroxide such as sodium hydroxide should be used.

[0046] Comparative Example 2: A method for purifying crude ammonium fluoride, comprising: (1) providing an electrolytic cell, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane), a carbon electrode is provided in the cathode region, and a saturated sodium hydroxide aqueous solution is provided in the anode region as an electrolyte in the anode region, wherein the sodium hydroxide equivalent in the saturated sodium hydroxide aqueous solution used is about 2.0 Eq, and a copper electrode is used as an anode electrode; (2) placing a crude ammonium fluoride solution in the cathode region as an electrolyte in the cathode region, applying power for electrolysis, and controlling the starting voltage to be 1.23 V; (3) performing the electrolysis until the potential rises to threshold values ​​of 1.30 V and 1.35 V, performing two sets of experimental verifications, terminating the electrolysis process and recovering the electrolyte in the cathode region; (4) mixing the recovered electrolyte in the cathode region with anhydrous ethanol 48 times its volume, adding industrial quicklime with a loose volume of 0.8 times that of the electrolyte in the cathode region, dehydrating and drying, filtering to remove the precipitate, and then heating at 20 After low-pressure evaporation at ℃ and recovery of anhydrous ethanol, the crystalline product is recovered to obtain a purified ammonium fluoride product.

[0047] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery amount is calculated. The purity and ammonium fluoride content of the purified ammonium fluoride product obtained in step (4) are characterized, and the actual recovery amount is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery amount and the actual recovery amount.

[0048] The specific calculation formula of recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%;

[0049] Through characterization and calculation, the purity of the purified ammonium fluoride product obtained in this example is 99.7%, and the recovery rate is accurate to one decimal place, and the calculated result is 100.0%.

[0050] The verification results show that when the control threshold is 1.30 V, the purity of ammonium fluoride in the obtained product is 99.3%, and the recovery rate is 100.0%. When the control threshold is 1.35 V, the purity of ammonium fluoride in the obtained product is 99.5%, and the recovery rate is 100.0%. It can be seen that lowering the threshold potential used to judge the electrolysis process will lead to a more obvious decrease in the purity of the ammonium fluoride product. Characterization of the product also found that this is a manifestation caused by incomplete removal of hydrogen fluoride. Increasing the threshold will greatly increase energy consumption, and the purity and recovery rate of the actual product have not been significantly improved. Compared with the 1.32 V threshold, the energy consumption of the electrolysis process increased by about 12% at the 1.35 V threshold. Therefore, in order to control costs, a 0.01 V gradient test was carried out, and the optimal threshold control range should be 1.32-1.34 V.

[0051] Comparative Example 3: Take the crude ammonium fluoride liquid, perform recrystallization treatment 5 times with the existing conventional process, and characterize the purity and calculate the recovery rate of the product. The specific calculation formula of the recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%, where the actual recovery amount is the actual recovery amount obtained by product characterization, and the theoretical maximum recovery amount is characterized and calculated according to the content of ammonium fluoride in the crude ammonium fluoride liquid. The characterization settlement results show that the product purity is 97.8% and the recovery rate is 96.3%. And compared with the process of Example 1 of the present invention, the actual industrial production cycle of multiple recrystallization treatments is extended by about 3 h, and the energy consumption is increased by about 6%.

[0052] It can be seen that compared with the existing recrystallization process, the process of the present invention has been comprehensively improved in many aspects such as improving production efficiency, reducing energy consumption, and improving product quality and recovery rate.

[0053] Comparative Example 4: A method for purifying crude ammonium fluoride, comprising: (1) providing an electrolytic cell, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane N2050WX (Nafion ion exchange membrane), a carbon electrode is provided in the cathode region, and a saturated sodium hydroxide aqueous solution is provided in the anode region as an electrolyte in the anode region, wherein the sodium hydroxide equivalent in the saturated sodium hydroxide aqueous solution used is about 2.0 Eq, and a copper electrode is used as an anode electrode; (2) industrial ammonium fluoride crystals of different purities are dissolved in water to prepare a crude product solution, which is placed in the cathode region as an electrolyte in the cathode region, and an electric current is applied for electrolysis treatment, and the starting voltage is controlled to be 1.23 V; (3) the electrolysis treatment is carried out until the potential rises to a threshold value of 1.32 V, the electrolysis process is terminated, and the cathode region electrolyte is recovered; (4) the recovered cathode region electrolyte is mixed with 48 times the volume of anhydrous ethanol, and then industrial quicklime with a loose volume of 0.8 times that of the cathode region electrolyte is added to remove water and dry, and after filtering to remove the precipitate, the solution is heated at 20 After low-pressure evaporation at ℃ and recovery of anhydrous ethanol, the crystalline product is recovered to obtain a purified ammonium fluoride product.

[0054] The content of ammonium fluoride in the crude ammonium fluoride liquid of step (2) is characterized, and the theoretical maximum recovery amount is calculated. The purity and ammonium fluoride content of the purified ammonium fluoride product obtained in step (4) are characterized, and the actual recovery amount is calculated. The recovery rate of ammonium fluoride is calculated based on the theoretical maximum recovery amount and the actual recovery amount.

[0055] The specific calculation formula of recovery rate is: recovery rate = (actual recovery amount / theoretical maximum recovery amount) × 100%;

[0056] The corresponding preparation effects of industrial crystals of ammonium fluoride with different purities are shown in the following table. In the table: crystal purity refers to the purity of ammonium fluoride in the industrial crystal product of ammonium fluoride; product recovery rate refers to the recovery rate of ammonium fluoride.

[0057] The industrial crystals of ammonium fluoride used were characterized, and the characterization results showed that in the products with a crystal purity of 87.2% and 89.3%, the impurities were mainly composed of hydrogen fluoride and / or ammonium bifluoride, but also contained other copper ion compound impurities, which the process of the present invention could not effectively and thoroughly remove. Therefore, for the applicability of the purification method of the present invention, it should be applicable to crude products whose main impurities are composed of hydrogen fluoride and / or ammonium bifluoride.

Claims

1. A method for purifying crude ammonium fluoride, It is characterized in that The method comprises: (1) providing an electrolytic cell, wherein the electrolytic cell is divided into a cathode region and an anode region by a cation exchange membrane, an inert cathode is provided in the cathode region, and an alkaline alkali metal compound aqueous solution and a copper electrode are provided in the anode region; The alkaline alkali metal compound aqueous solution is a sodium hydroxide aqueous solution and / or a potassium hydroxide aqueous solution; (2) placing the crude ammonium fluoride solution in the cathode region as the cathode region electrolyte and applying power for electrolysis; (3) The electrolysis process is continued until the potential reaches a threshold value, the electrolysis process is terminated, and the cathode electrolyte is recovered; (4) recovering the cathode electrolyte, mixing it with excess anhydrous ethanol, adding calcium oxide to remove water and dry it, filtering to remove the precipitate, and then crystallizing it under low temperature conditions to obtain a purified ammonium fluoride product; In step (1), the inert cathode is a carbon electrode; During the constant current electrolysis treatment in step (2), the starting voltage is controlled to be 1.23 V, and the potential voltage threshold in step (3) is 1.32 V; The purified ammonium fluoride product obtained in step (4) is slowly dissolved in anhydrous ethanol until the purified ammonium fluoride product no longer dissolves, and then the solid matter is removed by solid-liquid separation. The anhydrous ethanol solution of ammonium fluoride is crystallized again to obtain an ultra-high purity ammonium fluoride product.

2. A method for purifying crude ammonium fluoride according to claim 1, It is characterized in that When the cathode electrolyte recovered in step (4) is mixed with excess anhydrous ethanol, at least 48 times the volume of anhydrous ethanol is added to the anode electrolyte.