A THz dual-band tunable circular dichroic metasurface based on a graphene-gold resonant ring.
By utilizing the combined structure of graphene and gold resonant rings and the Fermi level modulation, a THz dual-band circular dichroic metasurface was realized, solving the problems of complex structure and single frequency in the existing technology, and realizing the controllability of the device and the promotion of practical applications.
Patent Information
- Application Number
- CN202311159393.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-09-11
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2043-09-11
AI Technical Summary
Existing chiral metasurface structural units based on graphene materials are complex to design, operate at a single frequency, and are difficult to tune the Fermi level, which limits their development in practical applications.
A THz dual-band tunable circular dichroism metasurface based on graphene-gold resonant rings is designed. By modulating the Fermi levels of graphene on the left and right sides, and utilizing the combination structure of graphene micron strips and the top gold open rectangular resonant ring, symmetry is broken, resulting in a difference in circular dichroism.
The reconfigurable control of circular dichroism values was achieved in the THz dual-band, reducing the processing difficulty and enabling controllable adjustment of functions, thus promoting the development of chiral metasurfaces in practical applications.
Smart Images

Figure CN118348619B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of terahertz device technology, and in particular to a THz dual-band tunable circular dichroic metasurface based on a graphene-gold resonant ring. Background Technology
[0002] Metamaterials are a new type of artificial functional material that emerged in the early 21st century. These materials are mostly composed of periodically distributed subwavelength structural units. By designing parameters such as the geometry and arrangement of these structural units, the effective dielectric constant and permeability of metamaterials can be effectively controlled, potentially enabling the manipulation of electromagnetic waves by materials while breaking the optical diffraction limit. Therefore, metamaterials can exhibit extraordinary physical properties not found in natural materials, showing broad application prospects in polarization conversion, perfect absorption, and electromagnetic stealth. Metasurfaces are planar counterparts of metamaterials; their structures are simpler and easier to fabricate, making them a popular research area in metamaterials. Chirality refers to the property that an object or structure cannot be superimposed on its mirror image. When an object and its mirror image cannot be superimposed through translation or rotation, the structure is called a chiral structure. Due to the lack of mirror symmetry, electromagnetic coupling occurs when electromagnetic waves interact with chiral materials, resulting in unique electromagnetic properties. On a macroscopic scale, chiral optical effects occur when electromagnetic waves are transmitted or reflected through chiral materials, such as circular dichroism (CD) and asymmetric transmission (AT). A small number of naturally occurring chiral materials exist, but due to a significant mismatch between their geometric dimensions and the wavelength of light, the chiral phenomena observed in natural materials are extremely weak and cannot meet practical application requirements. Artificial metasurfaces can compensate for the weak chirality of natural materials. By rationally designing the structure of artificial chiral metasurfaces, it is hoped that the weak optical responses in natural materials can be amplified, making it possible to achieve strong chirality.
[0003] Chiral metasurfaces based on metallic structural units have been extensively studied and are widely used in optoelectronics. These metasurfaces typically require breaking three-dimensional spatial symmetry, thus placing stringent demands on the precise fabrication of the device's micro / nano structures. Furthermore, once the device is fabricated, its functionality is largely limited and cannot be adjusted, which significantly restricts its further development in practical applications. Therefore, designing chiral metasurfaces with simple structures and controllable performance is currently a hot research topic. Graphene is a two-dimensional material with excellent optical and electrical properties, exhibiting strong plasmon resonance characteristics in the THz frequency band, thus enabling the fabrication of optoelectronic devices in this band. Moreover, the Fermi level of graphene can be effectively tuned by the gate voltage, laying the foundation for the reconfigurable control of related device performance.
[0004] Existing reports on circular dichroic chiral metasurfaces based on graphene materials typically face challenges such as complex structural unit design, difficulty in tuning the graphene Fermi level, and limited operating frequency bands. This invention discloses a graphene strip-gold resonant ring-based metasurface that effectively solves these problems. By tuning the Fermi levels on both sides of the graphene layer, the metasurface achieves reconfigurable control of the CD value between -0.73 and 0.65 in both frequency bands of 8.45 THz and 9.75 THz. Related devices can be widely applied in near-field imaging, biological detection, and chiral sensors. Summary of the Invention
[0005] To address the challenges of complex structural unit design, single operating frequency, and difficulty in tuning the Fermi level of graphene-based chiral metasurfaces, this invention provides a THz dual-band tunable circular dichroism metasurface based on a graphene-gold resonant ring.
[0006] The THz dual-band tunable circular dichroic metasurface based on a graphene-gold resonant ring comprises, from bottom to top, a bottom metal reflector, a polyimide dielectric layer, a silicon dioxide dielectric layer, symmetrically distributed graphene micron strips with unequal Fermi levels, and a top gold open rectangular resonant ring structure. The layers are tightly bonded together. The bottom metal reflector is a gold thin film with a thickness of h1 = 0.2 μm, designed to completely reflect incident electromagnetic waves. The polyimide dielectric layer has a dielectric constant of 3.5 and a thickness of h2 = 1.6 μm. The silicon dioxide dielectric layer has a refractive index of 1.45 and a thickness of h3 = 1.4 μm. The graphene micron strips have a width W... g =3.2μm, the thickness of the graphene micron strip is 0.34nm, the spacing between two adjacent graphene micron strips is Δw = 0.4μm, and the Fermi level E of the graphene micron strip on the left is... f1 =1.0 eV, Fermi level E of graphene micron strip on the right. f2 =0.1eV, relaxation time is 1ps, thickness of top gold open rectangular resonator h4 = 0.3μm, ring width L1 = 1.4μm on both sides of top gold open rectangular resonator, ring width L2 = 1.2μm at the top and bottom ends of top gold open rectangular resonator, opening width S1 = 3.6μm, ring width W = 9μm, length L = 8μm. Top gold open rectangular resonator and graphene micron strips are typical C2 mirror symmetrical structures. They do not have circular dichroism in the THz band. When unequal gate voltages are applied to the symmetrically distributed graphene micron strips to change their Fermi levels, the original symmetry of the device is broken, thus realizing the response difference to circularly polarized light with different rotation directions.
[0007] Preferably, the metasurface has a periodicity P in the x-direction. x =13μm, y-direction period P y =10μm.
[0008] Preferably, the metasurface operates in the 7THz-10.5THz frequency band.
[0009] Preferably, the metasurface produces antisymmetric CD values of -0.73 and 0.65 at frequencies of 8.45 THz and 9.75 THz, respectively.
[0010] Compared with the prior art, the beneficial effects of the present invention are as follows:
[0011] The metasurface described in this invention achieves strong antisymmetric circular dichroism in two THz frequency bands (8.45THz and 9.75THz). Furthermore, this invention adds two symmetrically distributed graphene micron strips below the top gold open-ring resonator. By applying different gate voltages to these strips to change their Fermi levels, the circular dichroism of this metasurface is dynamically tunable.
[0012] This structure achieves circular dichroism simply by controlling the asymmetric distribution of the Fermi levels in graphene micron strips, avoiding the complex geometric designs of traditional metasurfaces and significantly reducing the fabrication difficulty. Furthermore, this control method is simple and manageable, avoiding the functional limitations and lack of adjustability issues that plague traditional metasurface devices once fabricated, thus greatly promoting the further development of chiral metasurfaces in practical applications. Attached Figure Description
[0013] Figure 1 This is a schematic diagram of the three-dimensional structural unit of a THz dual-band tunable circular dichroic metasurface device based on a graphene-gold resonant ring.
[0014] Figure 2 This is a top view of a THz dual-band tunable circular dichroic metasurface device unit based on a graphene-gold resonant ring.
[0015] Figure 3 This is the spectrum of the reflection coefficient when circularly polarized light is incident on the metasurface along the -z direction, where E f1 =E f2 =0.9eV;
[0016] Figure 4 The images show the absorption and CD values of right-hand circularly polarized light (RCP) and left-hand circularly polarized light (LCP) incident on the metasurface along the -z direction, respectively. Ec f1 =E f2 =0.9eV;
[0017] Figure 5This is a spectrum of the reflection coefficients when circularly polarized light is incident on the metasurface along the -z direction, where the graphene Fermi level E on the left is shown. f1 =1.0 eV, right-hand graphene Fermi level E f2 =0.1eV;
[0018] Figure 6 These are the absorption and CD spectra of right-handed circularly polarized light (RCP) and left-handed circularly polarized light (LCP) incident along the -z direction onto the metasurface, respectively. The graphene Fermi level E on the left is shown in the diagram. f1 =1.0 eV, right-hand graphene Fermi level E f2 =0.1eV;
[0019] Figure 7 It is to fix the Fermi level E of the right-side graphene f2 =0.1eV, the Fermi level of the graphene on the left is E f1 Two-dimensional CD spectrum as it changes from 0.4 eV to 1.0 eV;
[0020] Figure 8 It is a fixed right-side Fermi level E f2 =0.1eV, left Fermi level E f1 CD curves at 0.6 eV, 0.8 eV, and 0.98 eV, respectively. Detailed Implementation
[0021] The present invention will now be described in detail with reference to the accompanying drawings and specific embodiments:
[0022] See Figures 1 to 8 As shown, a THz dual-band tunable circular dichroic metasurface based on a graphene-gold resonant ring comprises, from bottom to top, a bottom metal reflector, a polyimide (PI) dielectric layer, a silicon dioxide (SiO2) dielectric layer, symmetrically distributed graphene micron strips with unequal Fermi levels, and a top gold open rectangular resonant ring structure. The layers are tightly bonded together. The bottom metal reflector is a gold thin film material with a thickness of h1 = 0.2 μm, its function being to completely reflect the incident electromagnetic waves. The polyimide (PI) dielectric layer has a dielectric constant of 3.5 and a thickness of h2 = 1.6 μm. The silicon dioxide (SiO2) dielectric layer has a refractive index of 1.45 and a thickness of h3 = 1.4 μm. The graphene micron strips have a width W... g =3.2μm, the thickness of the graphene micron strip is 0.34nm, the spacing between two adjacent graphene micron strips is Δw = 0.4μm, and the Fermi level E of the graphene micron strip on the left is... f1 =1.0 eV, Fermi level E of graphene micron strip on the right. f2=0.1eV, relaxation time is 1ps, the thickness of the top gold open rectangular resonator is h4 = 0.3μm, the ring width on both sides of the top gold open rectangular resonator is L1 = 1.4μm, the ring width at the top and bottom ends of the top gold open rectangular resonator is L2 = 1.2μm, the opening width of the top gold open rectangular resonator is S1 = 3.6μm, the ring width of the top gold open rectangular resonator is W = 9μm, and the length of the top gold open rectangular resonator is L = 8μm. The top gold open rectangular resonator and the graphene micron strip are typical C2 mirror symmetrical structures. It does not have circular dichroism in the THz band. When unequal gate voltages are applied to the symmetrically distributed graphene micron strips to change their Fermi levels, the original symmetry of the device is broken, thus realizing the response difference to circularly polarized light with different rotation directions, i.e., circular dichroism. This metasurface has a periodicity P in the x-direction. x =13μm, y-direction period P y =10μm.
[0023] Furthermore, a THz dual-band tunable circular dichroism metasurface based on a graphene-gold resonant ring operates in the 7THz-10.5THz frequency band, producing antisymmetric CD values of -0.73 and 0.65 at frequencies of 8.45THz and 9.75THz, respectively.
[0024] The working principle of this invention is as follows:
[0025] The structure consisting of a top-layer gold-aperture rectangular resonant ring and symmetrically distributed graphene micron strips is a typical C2 mirror-symmetric structure, which itself does not possess chiral optical properties in the THz frequency band. This invention breaks the original structural symmetry of the device by applying unequal gate voltages to the symmetrically distributed graphene micron strips to alter their Fermi levels, thereby achieving different responses to circularly polarized light with different rotational directions and generating strong circular dichroism.
[0026] Circular dichroism, or the dichroism of circularly polarized light, refers to the differential absorption phenomenon between left-handed circularly polarized light (LCP) and right-handed circularly polarized light (RCP). Assuming the light absorptivity of the material is A, its absorptivity for right-handed and left-handed circularly polarized light can be expressed as A0 and A1, respectively. RCP and A LCP Then A RCP and A LCP The difference ΔA = CD = A RCP -A LCPThis is represented by the circular dichroism of the material. When an electromagnetic wave is incident on a material, it produces absorption (A), transmission (T), and reflection (R), and the ratio between these three values satisfies A = 1 - TR. In this invention, a 0.2 μm thick gold layer is chosen as the substrate at the bottom of the structure. Its thickness is greater than the skin depth of the electromagnetic wave, allowing it to completely reflect the energy of the incident electromagnetic wave; that is, the transmittance T = 0 when the electromagnetic wave is incident on the metasurface of this invention. Therefore, the absorption rate A under circularly polarized light incident in this invention can be simplified to A = 1 - R.
[0027] The formula for calculating its circular dichroism is:
[0028] A RCP =1-R RCP
[0029] A LCP =1-R LCP
[0030] CD = A RCP -A LCP
[0031] Right-hand circularly polarized light (RCP) and left-hand circularly polarized light (LCP) are incident on the designed metasurface along the -z direction. RCP and LCP are defined as clockwise and counterclockwise directions when viewed along the propagation direction, respectively. Figure 5 This is a spectrum of reflection coefficients when a circularly polarized wave is incident on a metasurface along the -z direction. The left side shows the Fermi level E of the graphene micron strip. f1 =1.0 eV, Fermi level E of graphene micron strip on the right. f2 =0.1eV, R LL R RR R is the same polarization reflection coefficient. LR R RL Given the cross-polarization reflection coefficient, a perfectly reflective circular dichroic metasurface can selectively reflect a circularly polarized light while preserving its cycloidia. In other words, a reflective circular dichroic metasurface must satisfy the condition: R LL ≠R RR And R LR =R RL R LL and R RR The larger the difference, the larger the CD value of the metasurface will be. According to... Figure 5 As shown, the cross-polarization reflection coefficient R of the metasurface of the present invention LR =R RL The same polarization reflection coefficient R RR and R LL The significant difference at the dual frequencies of 8.45 THz and 9.75 THz demonstrates that the metasurface achieves good circular dichroism.
[0032] Figure 6The polarization-selective absorption of the metasurface can be visually observed, and the Fermi level E of the graphene micron-strips is... f1 =1.0 eV, E f2 At 0.1 eV, the present invention exhibits an absorption of nearly 1 for LCP at 8.45 THz, while the absorptivity of RCP at the same frequency is only 0.25. Therefore, the circular dichroism (CD1) of the metasurface at this frequency is -0.73. Conversely, at 9.75 THz, most of the LCP is reflected, with an absorptivity of only 0.2, while RCP is heavily absorbed, with an absorptivity of 0.85. The circular dichroism (CD2) at this frequency is 0.65. The selective absorption of circularly polarized light at both 8.45 THz and 9.75 THz results in strong circular dichroism at these frequencies.
[0033] For comparison, we observed the circular dichroism of the device when the Fermi levels of the two graphene micron strips were set to be equal (0.9 eV). Figure 3 and Figure 4 As shown, at this time, the reflection coefficient of the designed metasurface in the operating frequency band is: R LL =R RR R LR =R RL Therefore, it has the same absorbance for both LCP and RCP, and the metasurface has CD = 0, thus lacking circular dichroism. Figures 3 to 6 This demonstrates that by applying unequal gate voltages to symmetrically distributed graphene micron strips to alter their Fermi levels, the symmetry of the device structure can be effectively broken, resulting in circular dichroism.
[0034] Graphene micron-strips, as the tunable portion of the designed chiral metasurface, are an excellent material for dynamically tunable resonant frequencies in the THz band. Using the random phase approximation theory, the conductivity of graphene micron-strips can be expressed by the Kubo formula, which consists of interband conductivity and intraband conductivity:
[0035]
[0036] in It is a simplified Planck constant, ω is the angular frequency, and E is the angular frequency. f It is the Fermi level, τ = μE f / (eV f 2 ) is the carrier relaxation time, μ = 10 4 cm 2 / V is the carrier mobility, V f =10 6 m / s is the Fermi velocity.
[0037] Low-frequency limit in the THz band Under these conditions, conductivity is dominated by in-band response, and the weak interband response can be ignored. Therefore, conductivity can be simplified to:
[0038]
[0039] The conductivity of graphene micron strips is affected by E f Impact, E f The relationship between voltage V and voltage V can be expressed as:
[0040] Where ε₀ is the free space permittivity, ε r Let d be the relative permittivity and d be the PI thickness. The Fermi level E is altered by changing the gate voltage applied to the graphene micron strip. f To change its conductivity.
[0041] Figure 7 It is to fix the Fermi level E of the right-side graphene micron strip. f2 =0.1eV, Fermi level E of graphene micron strip on the left f1 A two-dimensional CD value spectrum as the voltage changes from 0.4 eV to 1.0 eV. Figure 7 and Figure 8 It can be seen that the Fermi level E of the graphene micron strip on the right side is fixed. f2 Subsequently, the overall CD value of the device changes with the Fermi level value E of the graphene micron strip on the left. f1 The change is due to variations in E. Specifically, the wavelengths corresponding to the two CD peaks change with E. f1 The value decreases with increasing E, resulting in a blue shift; while the CD peak size decreases with increasing E. f1 The value increases with the increase of the graphene micron strips. It should be noted that the Fermi level settings of the left and right graphene micron strips are not fixed; when the values are reversed, the properties of the metasurface device of this invention will also change. The numerical settings here are for representative reference only. The circular dichroism dynamic reconfigurable characteristics of the related metasurface device in this invention have great potential for development in practical applications.
Claims
1. A THz dual-band tunable circular dichroic metasurface based on a graphene-gold resonant ring, characterized in that: From bottom to top, the structure comprises a bottom metal reflector, a polyimide dielectric layer, a silicon dioxide dielectric layer, symmetrically distributed graphene micron strips with unequal Fermi levels, and a top gold open rectangular resonant ring structure. All layers are tightly bonded together. The bottom metal reflector is a gold thin film with a thickness of h1 = 0.2 μm, designed to completely reflect incident electromagnetic waves. The polyimide dielectric layer has a dielectric constant of 3.5 and a thickness of h2 = 1.6 μm. The silicon dioxide dielectric layer has a refractive index of 1.45 and a thickness of h3 = 1.4 μm. The graphene micron strips have a width of W... g =3.2μm, the thickness of the graphene micron strip is 0.34nm, the spacing between two adjacent graphene micron strips is Δw = 0.4μm, and the Fermi level E of the graphene micron strip on the left is... f1 =1.0 eV, Fermi level E of graphene micron strip on the right. f2 =0.1eV, relaxation time is 1ps, thickness of top gold open rectangular resonator h4 = 0.3μm, ring width L1 = 1.4μm on both sides of top gold open rectangular resonator, ring width L2 = 1.2μm at the top and bottom ends of top gold open rectangular resonator, opening width S1 = 3.6μm, ring width W = 9μm, length L = 8μm. Top gold open rectangular resonator and graphene micron strips are typical C2 mirror symmetrical structures. They do not have circular dichroism in the THz band. When unequal gate voltages are applied to the symmetrically distributed graphene micron strips to change their Fermi levels, the original symmetry of the device is broken, thus realizing the response difference to circularly polarized light with different rotation directions.
2. The THz dual-band tunable circular dichroic metasurface based on a graphene-gold resonant ring according to claim 1, characterized in that: The metasurface has a periodicity P in the x-direction. x =13μm, y-direction period P y =10μm.
3. The THz dual-band tunable circular dichroic metasurface based on a graphene-gold resonant ring according to claim 1, characterized in that: The metasurface operates in the 7THz-10.5THz frequency band.