A control method, device and system for a battery plate silver plating production line

Through high-definition camera analysis and real-time monitoring of the cleaning and plating solution parameters of battery plates, the problem of low cleaning efficiency and uneven plating in the existing technology has been solved, and the efficient and stable production of the battery plate hanging silver plating production line has been achieved, improving the efficiency of the battery plate hanging silver plating production line. Production efficiency and product quality.

CN118497875BActive Publication Date: 2024-10-11NANTONG ANAIHUA TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410969040.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-10-11
Estimated Expiration
2044-07-19

AI Technical Summary

Technical Problem

The existing battery plate rack silver plating production line lacks flexibility and accuracy in cleaning and plating solution flow rate control, resulting in low cleaning efficiency, uneven plating, and lack of real-time monitoring and evaluation, affecting production efficiency and product quality.

Method used

High-definition cameras are used for image analysis to monitor and regulate the cleaning time and plating solution parameters in real time. By monitoring and regulating the temperature and flow rate of the plating solution in different areas, a production line operation quality evaluation system is established to form a closed-loop monitoring.

Benefits of technology

It improves cleaning efficiency and coating quality consistency, reduces resource waste and production costs, and improves production efficiency and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118497875B_ABST
    Figure CN118497875B_ABST
Patent Text Reader

Abstract

The present invention belongs to the technical field of silver plating production of battery plates, and discloses a control method, equipment and system for a production line of silver plating of battery plates. The present invention uses a high-definition camera to collect images of battery plates before and after cleaning in the production process of silver plating of battery plates, analyzes the dirtiness coefficient, and then determines and adjusts the cleaning time, which is conducive to improving the cleaning efficiency of battery plates, and can carry out targeted immersion cleaning for a single battery plate, avoiding waste of resources or insufficient cleanliness caused by inaccuracy of cleaning time. The present invention monitors and regulates the parameters of the plating solution in the plating pool by different regions, which is conducive to targeted adjustment of specific plating solution parameters of the plating pool, avoiding waste of resources and affecting production efficiency, while maintaining the uniformity and stability of the plating layer of the battery plates to the greatest extent. The present invention analyzes the abnormal index of the production line and judges the production status of the production line, which is conducive to judging the maintenance needs of the production line.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of battery plate rack silver plating production, and relates to a battery plate rack silver plating production line control method, equipment and system. Background Art

[0002] Battery plates are one of the core components of batteries. Silver plating of battery plates can improve the performance, corrosion resistance, contact performance and heat dissipation performance of batteries, thereby optimizing the overall performance of batteries. A reasonable battery plate silver plating production line is of great significance in improving product performance, extending service life, reducing maintenance costs, increasing product added value, and environmental protection and energy saving.

[0003] The battery plate silver plating production line includes processes such as racking, cleaning, silver plating and quality inspection. Among them, efficient and standardized cleaning and plating processes have an important impact on the quality of battery plate coating.

[0004] Existing battery plate silver plating production lines generally use a fixed cleaning time when cleaning the battery plates and then immerse the battery plates for cleaning. This determination of the cleaning time may result in the cleaning time being insufficient or excessive, reducing the efficiency of the cleaning work, causing waste of resources, aggravating equipment wear, and lack of flexibility. At the same time, insufficient cleaning may occur, affecting subsequent production steps and reducing product quality.

[0005] The existing battery plate silver plating production line uses a control device to perform overall control in the event of abnormal parameters. This method, which does not perform regional monitoring and control on the plating pool, will affect production efficiency, reduce the overall capacity of the production line, cause waste of resources, and even cause uneven thickness of the coating on the surface of the battery plate due to affecting the overall stability of the plating solution, thereby reducing the stability of the battery plate electroplating quality. In addition, a fixed flow rate method is usually used when setting the plating solution flow rate. This method ignores the relationship between the electroplating process and the plating solution flow rate, which will affect product production efficiency and the stability of the coating, thereby reducing product quality.

[0006] The existing battery plate silver plating production line lacks analysis of the production line's operating quality, lacks real-time monitoring and evaluation of the production line, has not formed a production closed loop, and is unable to promptly detect abnormalities in the production line's operation. As a result, production line operation quality issues may be ignored or delayed, making it difficult to promptly identify improvement points and optimization opportunities, affecting the continuous improvement and enhancement of the production line. Summary of the invention

[0007] In view of this, in order to solve the problems raised in the above background technology, a control method, equipment and system for a battery plate silver plating production line are proposed.

[0008] The purpose of the present invention can be achieved through the following technical solutions: The first aspect of the present invention provides a control method for a battery plate silver plating production line, including: S1, cleaning process operation: using a high-definition camera to obtain the surface image of the battery plate before cleaning, analyzing the dirtiness of the battery plate before cleaning and calculating the initial immersion time, and then starting the machine to immerse the battery plate for cleaning.

[0009] S2. Cleaning process monitoring: Use a high-definition camera to obtain the surface image of the battery plate after cleaning, and analyze the dirtiness of the battery plate after cleaning, and then determine whether the battery plate needs to be immersed in water for cleaning again. When it is determined that re-cleaning is necessary, execute the cleaning process control steps, otherwise execute the rack plating process operation steps.

[0010] S3. Cleaning process control: based on the dirtiness after cleaning, the immersion time is adjusted and re-immersion cleaning is performed. After re-immersion cleaning, the cleaning process monitoring step is performed.

[0011] S4, rack plating process operation: the rack plating pool is divided into a plurality of rack plating areas, and the battery plate is immersed in the plating solution for electroplating.

[0012] S5. Rack plating process monitoring: From the beginning of electroplating, the electroplating process is divided into several detection time points at equal intervals, and a temperature sensor and a flow rate sensor are set in each rack plating area to obtain the actual plating solution parameters of each rack plating area at each detection time point in the rack plating process operation, and the deviation of the plating solution parameters corresponding to each rack plating area at each detection time point is analyzed, where the plating solution parameters include plating solution temperature and plating solution flow rate.

[0013] S6. Control of the rack plating process: a temperature control device and a stirring device are set on the mobile control device, and based on the deviation of the plating solution parameters, it is determined whether the actual plating solution parameters need to be adjusted in each rack plating area at each detection time point. If necessary, the mobile control device is used to adjust the plating solution parameters until the appropriate plating solution parameters are reached.

[0014] S7. Production line operation quality evaluation: Statistics and analysis of the adjustment frequency and adjustment range in the cleaning process and the rack plating process, and then analysis of the production line abnormality index.

[0015] In an optional manner, the steps of analyzing the contamination of the battery plates before cleaning and calculating the initial immersion time are as follows: using edge detection processing technology to identify the dirty areas in the surface image of the battery plates before cleaning obtained by a high-definition camera to obtain the contours of the dirty areas, and then importing them into image processing software to obtain the area of ​​the dirty areas.

[0016] Import the contour image of the battery plate into the image processing software to obtain the surface area of ​​the battery plate, and then substitute the dirty area area into the analysis formula Get the dirtiness coefficient of the battery plate before cleaning, where Represents a natural constant.

[0017] Substitute the dirtiness coefficient of the battery plate before cleaning into the calculation formula The initial immersion time is obtained, wherein the standard immersion time refers to the immersion cleaning time required for the standard dirtiness coefficient, and the standard dirtiness coefficient is the dirtiness coefficient of the battery plate under a preset standard state.

[0018] In an optional manner, the determination of whether the battery plate needs to be immersed again for cleaning is as follows: Substituting the dirt coefficient of the battery plate after cleaning into the judgment model Get the judgment result whether it is necessary to immerse and clean again. Indicates the preset allowable dirtiness coefficient after cleaning. Indicates that the battery plates do not need to be immersed in water for cleaning again. Indicates that the battery plates need to be immersed and cleaned again.

[0019] In an optional manner, the plating area division of the plating pool is specifically as follows: a number of longitudinal dividing lines are obtained by equidistantly dividing the outer wall of the plating pool, and adjacent longitudinal dividing lines and the central axis of the plating pool divide the space of the plating pool into a number of areas, which are recorded as plating areas, and each plating area is numbered.

[0020] In an optional manner, the analysis of the deviation of the plating solution parameters corresponding to each rack plating area at each detection time point is specifically as follows: the actual plating solution temperature of each rack plating area at each detection time point is and suitable bath temperature Substitute into the calculation formula of bath temperature deviation Get the first Detection time point Deviation of plating solution temperature in the rack plating area ,in Indicates the detection time point number, , Indicates the plating area number. .

[0021] Locate the appropriate plating solution flow rate corresponding to each detection time point from the standard plating solution flow rate change trend chart .

[0022] The actual plating solution flow rate of each rack plating area at each detection time point and appropriate bath flow rate Substitute into the calculation formula of plating solution flow rate deviation Get the first Detection time point Deviation of plating solution flow rate in the rack plating area .

[0023] The temperature deviation of the plating solution in each rack plating area at each detection time point and the deviation of plating solution flow rate Substitute into the calculation formula Get the first Detection time point Deviation of plating bath parameters in the rack plating area ,in They respectively represent the weights of the deviation of plating solution temperature and the deviation of plating solution flow rate.

[0024] In an optional manner, the step of judging whether the actual plating solution parameters of each plating area at each detection time point need to be adjusted is as follows: comparing the deviation of the plating solution parameters of each plating area at each detection time point with the preset allowable deviation of the plating solution parameters; if the deviation of the plating solution parameters of a certain plating area at a certain detection time point is less than or equal to the preset allowable deviation of the plating solution parameters, then the actual plating solution parameters corresponding to the plating area at this detection time point do not need to be adjusted; if the deviation of the plating solution parameters of a certain plating area at a certain detection time point is greater than the preset allowable deviation of the plating solution parameters, then the actual plating solution parameters corresponding to the plating area at this detection time point need to be adjusted, and then the detection time point is taken as an abnormal detection time point, and the plating area is taken as an abnormal plating area.

[0025] In an optional manner, the steps of adjusting the plating solution parameters using the mobile control device are as follows: identifying the abnormal direction of the abnormal plating area; if the plating solution temperature deviation corresponding to a certain abnormal plating area at a certain abnormal detection time point is greater than the allowable plating solution temperature deviation, then the abnormal detection time point corresponds to the abnormal plating area with a plating solution temperature abnormality; if the plating solution flow rate deviation corresponding to a certain abnormal plating area at a certain abnormal detection time point is greater than the allowable plating solution flow rate deviation, then the abnormal detection time point corresponds to the abnormal plating area with a plating solution flow rate abnormality.

[0026] When the plating solution temperature is abnormal in a certain abnormal plating area, the mobile control device is used to move to the abnormal plating area and then the temperature control device is used to adjust the plating solution temperature of the plating area until the appropriate plating solution temperature is reached.

[0027] When there is an abnormal plating solution flow rate in a certain abnormal hanging plating area, substitute the actual plating solution flow rate and the appropriate plating solution flow rate into the stirring device frequency calculation formula The stirring frequency of the stirring device is obtained, and then the mobile control device is used to move to the abnormal plating area and the plating solution flow rate of the plating area is adjusted by the stirring device according to the calculated stirring frequency.

[0028] In an optional manner, the step of analyzing the abnormal index of the production line is as follows: Substitute the immersion time adjustment frequency and the immersion time adjustment amplitude into the formula Get the immersion time anomaly index .

[0029] Substitute the bath parameter adjustment frequency and bath parameter adjustment amplitude into the formula Get the abnormal index of plating bath parameters .

[0030] Then, the immersion time abnormality index and the plating solution parameter abnormality index are summed and calculated to obtain the production line abnormality index.

[0031] The second aspect of the present invention provides a battery plate silver plating production line control system, comprising the following modules: a cleaning process operation module, which is used to use a high-definition camera to obtain the surface image of the battery plate before cleaning, analyze the dirtiness of the battery plate before cleaning and calculate the initial immersion time, and then start the machine to immerse the battery plate for cleaning.

[0032] The cleaning process monitoring module is used to use a high-definition camera to obtain the surface image of the battery plate after cleaning, and analyze the dirtiness of the battery plate after cleaning to determine whether the battery plate needs to be immersed in water for cleaning again. When it is determined that re-cleaning is required, the cleaning process control is executed, otherwise the plating process operation is executed.

[0033] The cleaning process control module is used to adjust the immersion time based on the dirtiness after cleaning and perform re-immersion cleaning, and perform cleaning process monitoring after re-immersion cleaning.

[0034] The rack plating process operation module is used to divide the rack plating pool into several rack plating areas, immerse the battery plate in the plating solution for electroplating, wherein the plating solution parameters include the plating solution temperature and the plating solution flow rate.

[0035] The rack plating process monitoring module is used to divide the electroplating time into equally spaced time periods to obtain a number of detection time points. A temperature sensor and a flow rate sensor are set in each rack plating area to obtain the actual plating solution parameters of each rack plating area at each detection time point in the rack plating process operation and analyze the deviation of the plating solution parameters of each rack plating area corresponding to each detection time point.

[0036] The rack plating process control module is used to set a temperature control device and a stirring device on the mobile control device, and judge whether the actual plating solution parameters need to be adjusted in each rack plating area at each detection time point based on the deviation of the plating solution parameters. If necessary, the mobile control device is used to adjust the plating solution parameters until the appropriate plating solution parameters are reached.

[0037] The production line operation quality evaluation module is used to count and analyze the adjustment frequency and adjustment range in the cleaning process and the rack plating process, and then analyze the production line abnormality index.

[0038] A third aspect of the present invention provides a device, which includes any one of the above-mentioned magnetic pole plate silver plating production line control methods or battery pole plate silver plating production line control systems.

[0039] Compared with the prior art, the beneficial effects of the present invention are as follows: (1) The present invention uses a high-definition camera to collect multiple images of the battery plates before and after cleaning, and then analyzes the initial immersion time and the adjusted immersion time of the battery plates. This cleaning time analysis method can improve the cleaning efficiency of the battery plates on the growth line, is more targeted, and can reduce the waste of resources and machine wear caused by excessively long cleaning time. At the same time, it can avoid the occurrence of low battery plate cleanliness caused by insufficient cleaning time, thereby improving cleaning efficiency and cleaning quality, and improving production efficiency and capacity.

[0040] (2) The present invention divides the plating pool into plating areas and then monitors and controls the plating solution parameters in each area. This method can more accurately monitor and control the changes in the plating solution parameters in different areas of the plating pool, so that the plating solution parameters in each area are in the best state, ensuring the stability and consistency of the coating quality, reducing resource waste and costs, and improving product production efficiency.

[0041] (3) The present invention sets different suitable plating solution flow rates based on different plating time periods during the silver plating process of battery plates, which can improve the efficiency of plating solution utilization during the plating process, thereby ensuring the overall quality and consistency of the battery plate coating while improving production efficiency.

[0042] (4) The present invention provides an operation quality evaluation function for a battery plate silver plating production line, which can analyze the operation status of the production line in real time to form a closed production loop. By real-time monitoring of abnormal conditions that may occur during the production process, the production line process can be targetedly improved and improved, which is conducive to optimizing product quality, thereby reducing production costs and improving the economic benefits of the production line. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for describing the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.

[0044] Figure 1 It is a schematic diagram of the steps for implementing the method of the present invention.

[0045] Figure 2 It is a schematic diagram of system module connection of the present invention.

[0046] Figure 3 It is a schematic diagram of the division of the rack plating area of ​​the present invention.

[0047] Figure numerals: 1 - plating area, 2 - longitudinal dividing line, 3 - central axis. DETAILED DESCRIPTION

[0048] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0049] See also Figure 1 As shown, the first aspect of the present invention provides a control method for a battery plate silver plating production line, the method comprising: S1, cleaning process operation: using a high-definition camera to obtain a surface image of the battery plate before cleaning, analyzing the dirtiness of the battery plate before cleaning and calculating the initial immersion time, and then starting the machine to immerse the battery plate for cleaning.

[0050] It should be noted that when collecting the surface image of the battery plate, it is necessary to set up opposite high-definition cameras to collect the surface images of both sides of the battery plate at the same time.

[0051] Preferably, edge detection processing technology is used to identify dirty areas in the surface image of the battery plate before cleaning obtained by a high-definition camera to obtain the contour of the dirty area, which is then imported into image processing software to obtain the area of ​​the dirty area.

[0052] It should be noted that the dirty area is the sum of the dirty areas on both sides of the battery plates.

[0053] Import the contour image of the battery plate into the image processing software to obtain the surface area of ​​the battery plate, and then substitute the dirty area area into the analysis formula Get the dirtiness coefficient of the battery plate before cleaning, where Represents a natural constant.

[0054] Substitute the dirtiness coefficient of the battery plate before cleaning into the calculation formula The initial immersion time is obtained, wherein the standard immersion time refers to the immersion cleaning time required for the standard dirtiness coefficient, and the standard dirtiness coefficient is the dirtiness coefficient of the battery plate under a preset standard state.

[0055] S2. Cleaning process monitoring: Use a high-definition camera to obtain the surface image of the battery plate after cleaning, and analyze the dirtiness of the battery plate after cleaning, and then determine whether the battery plate needs to be immersed in water for cleaning again. When it is determined that re-cleaning is necessary, execute the cleaning process control steps, otherwise execute the rack plating process operation steps.

[0056] Preferably, the dirt coefficient of the battery plate after cleaning is substituted into the judgment model Get the judgment result whether it is necessary to immerse and clean again. Indicates the preset allowable dirtiness coefficient after cleaning. Indicates that the battery plates do not need to be immersed in water for cleaning again. Indicates that the battery plates need to be immersed and cleaned again.

[0057] For example, .

[0058] It should be noted that the reason for using the dirtiness coefficient as the basis for judging whether the battery plates need to be re-immersed for cleaning is that the dirtiness coefficient can quantitatively describe the degree of contamination on the surface of the battery plates, which enables a more accurate assessment of the surface cleanliness and avoids subjective errors that may be caused by visual inspection alone; contamination on the surface of the battery plates may affect the quality and performance of the final product. By re-immersing and cleaning according to the dirtiness coefficient, it can be ensured that the surface of the battery plates meets the required cleanliness standards, thereby ensuring consistency in product quality.

[0059] S3. Cleaning process control: based on the dirtiness after cleaning, the immersion time is adjusted and re-immersion cleaning is performed. After re-immersion cleaning, the cleaning process monitoring step is performed.

[0060] It should be noted that the present invention utilizes a high-definition camera to perform multiple image acquisitions on the battery plates before and after cleaning, and then analyzes the initial immersion time and the adjusted immersion time of the battery plates. This cleaning time analysis method can improve the cleaning efficiency of the growth line battery plates, is more targeted, can reduce resource waste and machine wear caused by excessively long cleaning time, and can avoid the occurrence of low battery plate cleanliness caused by insufficient cleaning time, thereby improving the cleaning efficiency and cleaning quality and thus improving production efficiency and capacity.

[0061] Preferably, the dirtiness coefficient of the battery plate after cleaning is substituted into the calculation formula Get adjusted immersion time.

[0062] S4, rack plating process operation: the rack plating pool is divided into a plurality of rack plating areas, and the battery plate is immersed in the plating solution for electroplating.

[0063] Preferably, see Figure 3 As shown, a number of longitudinal dividing lines are equally spaced on the outer wall of the plating pool, and adjacent longitudinal dividing lines and the central axis of the plating pool divide the space of the plating pool into a number of areas, which are recorded as plating areas, and each plating area is numbered.

[0064] It should be noted that the method of dividing the plating pool into plating areas in the present invention can ensure that each plating area includes the plating pool wall, thereby facilitating the installation of temperature sensors and flow rate sensors. On the other hand, it can ensure that the size and spatial layout of each plating area are similar, thereby ignoring the impact on the monitoring of plating solution parameters.

[0065] S5. Rack plating process monitoring: From the beginning of electroplating, the electroplating process is divided into several detection time points at equal intervals, and a temperature sensor and a flow rate sensor are set in each rack plating area to obtain the actual plating solution parameters of each rack plating area at each detection time point in the rack plating process operation, and the deviation of the plating solution parameters corresponding to each rack plating area at each detection time point is analyzed, where the plating solution parameters include plating solution temperature and plating solution flow rate.

[0066] It should be noted that the reasons for selecting the plating solution temperature and plating solution flow rate as the plating solution parameters for analysis are as follows: changes in temperature will affect the physical properties of the plating solution, such as conductivity, ion activity, and solution viscosity, and thus affect the efficiency and quality of the electroplating process. Increasing the temperature can reduce cathode polarization and promote the formation of a coarse-grained coating, but it may also cause instability in the plating solution components, so the temperature needs to be controlled within an appropriate range; appropriate temperature can increase the diffusion rate of ions, reduce concentration polarization, and reduce electrochemical polarization, thereby increasing current density and improving electroplating efficiency; the plating solution flow rate directly affects the uniformity of the coating on the workpiece surface. Too fast a flow rate may cause the coating to be too thin or uneven, while too slow a flow rate may cause the coating to be too thick or impurities to appear. An appropriate plating solution flow rate can promote the uniform distribution of ions in the plating solution on the cathode surface, reduce concentration polarization, and improve the uniformity and quality of the coating. At the same time, too fast a flow rate can also prevent the sediment in the plating solution from depositing on the cathode surface, keeping the plating solution clean and stable.

[0067] Preferably, the actual plating solution temperature of each rack plating area at each detection time point is and suitable bath temperature Substitute into the calculation formula of bath temperature deviation Get the first Detection time point Deviation of plating solution temperature in the rack plating area ,in Indicates the detection time point number, , Indicates the plating area number. .

[0068] Locate the appropriate plating solution flow rate corresponding to each detection time point from the standard plating solution flow rate change trend chart .

[0069] It should be added that the suitable plating solution temperature refers to the temperature corresponding to the pre-set ideal electroplating environment, and the suitable plating solution flow rate refers to the standard plating solution flow rate corresponding to each hanging plating time.

[0070] It should be noted that the standard plating solution flow rate change trend chart uses the plating time as the horizontal axis and the plating solution flow rate as the vertical axis. The specific change trend is based on the optimal plating solution flow rate required for the appropriate coating thickness corresponding to each time length collected during the historical plating process.

[0071] It should be noted that the reasons why different plating times correspond to different plating solution flow rates are as follows: 1. During the electroplating process, as the plating time increases, the current density on the workpiece surface may change. This is because the coating will gradually thicken during the electroplating process, and the resistance will also increase, resulting in a decrease in current density. In order to maintain the uniformity and efficiency of electroplating, the plating solution flow rate needs to be adjusted according to the change in current density to ensure that the ions in the plating solution can reach the workpiece surface evenly and quickly; 2. As the electroplating time increases, the effective ingredients in the plating solution will gradually be consumed, and some by-products or impurities may be produced. These changes will affect the conductivity, ion activity and other properties of the plating solution, and thus affect the electroplating process. Therefore, the plating solution flow rate needs to be adjusted according to the changes in the plating solution composition to maintain the stability of the electroplating process and the quality of the coating; 3. An appropriate plating solution flow rate helps to maintain the stability of the electroplating process and reduce failures and downtime. At the same time, by optimizing the plating solution flow rate, energy consumption, plating solution consumption and wastewater treatment costs can be reduced, thereby improving the economy of the electroplating process.

[0072] It should be added that, during the silver plating process of battery plates, the present invention sets different suitable plating solution flow rates based on different plating time periods, which can improve the efficiency of plating solution utilization during the plating process, thereby ensuring the overall quality and consistency of the battery plate coating while improving production efficiency.

[0073] The actual plating solution flow rate of each rack plating area at each detection time point and appropriate bath flow rate Substitute into the calculation formula of plating solution flow rate deviation Get the first Detection time point Deviation of plating solution flow rate in the rack plating area .

[0074] The temperature deviation of the plating solution in each rack plating area at each detection time point and the deviation of plating solution flow rate Substitute into the calculation formula Get the first Detection time point Deviation of plating bath parameters in the rack plating area ,in They respectively represent the weights of the deviation of plating solution temperature and the deviation of plating solution flow rate.

[0075] For example, .

[0076] S6. Control of the rack plating process: a temperature control device and a stirring device are set on the mobile control device, and based on the deviation of the plating solution parameters, it is determined whether the actual plating solution parameters need to be adjusted in each rack plating area at each detection time point. If necessary, the mobile control device is used to adjust the plating solution parameters until the appropriate plating solution parameters are reached.

[0077] Preferably, the deviation of the plating liquid parameters of each plating area at each detection time point is compared with the preset allowable deviation of the plating liquid parameters. If the deviation of the plating liquid parameters of a certain plating area at a certain detection time point is less than or equal to the preset allowable deviation of the plating liquid parameters, then the actual plating liquid parameters corresponding to the plating area at this detection time point do not need to be adjusted. If the deviation of the plating liquid parameters of a certain plating area at a certain detection time point is greater than the preset allowable deviation of the plating liquid parameters, then the actual plating liquid parameters corresponding to the plating area at this detection time point need to be adjusted, and then the detection time point is taken as an abnormal detection time point, and the plating area is taken as an abnormal plating area.

[0078] Exemplarily, the allowable deviation of the plating solution parameters can be .

[0079] It should be noted that the present invention divides the plating pool into plating areas and then monitors and controls the plating solution parameters in each area. This method can more accurately monitor and control the changes in plating solution parameters in different areas of the plating pool, so that the plating solution parameters in each area are in the best state, ensuring the stability and consistency of the coating quality, reducing resource waste and costs, and improving product production efficiency.

[0080] Further preferably, the abnormal direction of the abnormal plating area is identified. If the deviation of the plating solution temperature in a certain abnormal plating area corresponding to a certain abnormal detection time point is greater than the allowable deviation of the plating solution temperature, then the abnormal detection time point corresponds to the abnormal plating area with an abnormal plating temperature abnormality. If the deviation of the plating solution flow rate in a certain abnormal detection time point corresponds to the abnormal plating area with an abnormal detection time point is greater than the allowable deviation of the plating solution flow rate, then the abnormal detection time point corresponds to the abnormal plating area with an abnormal flow rate abnormality.

[0081] When the plating solution temperature is abnormal in a certain abnormal plating area, the mobile control device is used to move to the abnormal plating area and then the temperature control device is used to adjust the plating solution temperature of the plating area until the appropriate plating solution temperature is reached.

[0082] It should be added that when the temperature of an abnormal plating area is adjusted, the mobile control device is moved to the center of the abnormal plating area, and the temperature control device is used to adjust the plating area, while monitoring the real-time plastic temperature until the temperature reaches the operating plating solution temperature and then stopping the temperature adjustment.

[0083] When there is an abnormal plating solution flow rate in a certain abnormal hanging plating area, substitute the actual plating solution flow rate and the appropriate plating solution flow rate into the stirring device frequency calculation formula The stirring frequency of the stirring device is obtained, and then the mobile control device is used to move to the abnormal plating area and the plating solution flow rate of the plating area is adjusted by the stirring device according to the calculated stirring frequency.

[0084] It should be explained that the above stirring frequency can be negative, and the positive or negative stirring frequency indicates the stirring direction. When the stirring frequency is positive, it means that the stirring direction is consistent with the flow direction of the plating solution. When the stirring frequency is negative, it means that the stirring direction is opposite to the flow direction of the plating solution.

[0085] It should be noted that the reason for providing a stirring device and controlling the flow rate of the plating solution by adjusting the frequency of the stirring device is to be able to quickly and timely adjust the flow rate of the plating solution to avoid causing instability in product quality and affecting product quality.

[0086] It should be noted that the cleaning process and the rack plating process are of great significance in the production process of rack silver plating of battery plates: the cleaning process can remove oil, oxides and other impurities on the surface of the battery plates, and provide a clean and pollution-free substrate surface for the subsequent rack plating process, which helps to ensure that the coating can be evenly and tightly adhered to the substrate, thereby improving the quality and performance of the coating; the rack plating process is the core link in the silver plating process of battery plates. A uniform silver coating is formed on the surface of the battery plates by electrochemical methods. This coating not only has excellent conductivity and corrosion resistance, but also improves the performance and life of the battery plates.

[0087] S7. Production line operation quality evaluation: Statistics and analysis of the adjustment frequency and adjustment range in the cleaning process and the rack plating process, and then analysis of the production line abnormality index.

[0088] It should be added that the analysis of the adjustment frequency and adjustment range in the cleaning process and the rack plating process includes the following steps: wherein the cleaning process adjustment refers to the immersion time adjustment, the adjusted immersion time corresponding to each immersion time adjustment operation is averaged to obtain the average adjusted immersion time, and the average adjusted immersion time is substituted into the formula The average immersion time adjustment amplitude is obtained.

[0089] For example, the reference duration is .

[0090] The rack plating process adjustment includes plating solution temperature adjustment and plating solution flow rate adjustment. The actual plating solution temperature and the appropriate plating solution temperature of each plating solution temperature adjustment operation are substituted into the calculation formula The plating solution temperature adjustment amount of each plating solution temperature adjustment operation is obtained, and then the average adjustment plating solution temperature is obtained by performing mean calculation.

[0091] Substitute the actual plating solution flow rate of each plating solution flow rate adjustment operation and the appropriate plating solution flow rate corresponding to the adjustment moment into the calculation formula The plating solution flow rate adjustment amount of each plating solution flow rate adjustment operation is obtained, and then the average adjustment plating solution flow rate is obtained by performing mean calculation.

[0092] Substitute the average regulated bath temperature and the average regulated bath flow rate into the formula Get the average bath parameter adjustment range, where They respectively represent the weights of the average adjusted plating solution temperature and the average adjusted plating solution flow rate.

[0093] For example, , see the plating solution temperature , the reference plating solution flow rate is .

[0094] It should be supplemented that the average immersion time adjustment range and the average plating solution parameter adjustment range are respectively used as the immersion time adjustment range and the plating solution parameter adjustment range.

[0095] Preferably, the immersion time adjustment frequency and the immersion time adjustment amplitude are substituted into the formula Get the immersion time anomaly index .

[0096] Substitute the bath parameter adjustment frequency and bath parameter adjustment amplitude into the formula Get the abnormal index of plating bath parameters .

[0097] Then, the immersion time abnormality index and the plating solution parameter abnormality index are summed and calculated to obtain the production line abnormality index.

[0098] It should be noted that the present invention provides an operation quality evaluation function for a battery plate silver plating production line, which can analyze the operation status of the production line in real time to form a closed production loop. By real-time monitoring of abnormal situations that may occur during the production process, the production line process can be specifically improved and improved, which is conducive to optimizing product quality, thereby reducing production costs and improving the economic benefits of the production line.

[0099] See also Figure 2As shown, the second aspect of the present invention provides a battery plate silver plating production line control system, including a cleaning process operation module, a cleaning process monitoring module, a cleaning process control module, a rack plating process operation module, a rack plating process monitoring module, a rack plating process control module and a production line operation quality evaluation module, wherein the cleaning process operation module is connected to the cleaning process monitoring module, the cleaning process monitoring module is respectively connected to the cleaning process control module and the rack plating process operation module, the cleaning process control module is connected to the cleaning process control module, the rack plating process operation module is connected to the rack plating process monitoring module, the rack plating process monitoring module is connected to the rack plating process control module, and the rack plating process control module and the cleaning process control module are both connected to the production line operation quality evaluation module.

[0100] The cleaning process operation module is used to use a high-definition camera to obtain the surface image of the battery plate before cleaning, analyze the dirtiness of the battery plate before cleaning and calculate the initial immersion time, and then start the machine to immerse and clean the battery plate.

[0101] The cleaning process monitoring module is used to use a high-definition camera to obtain the surface image of the battery plate after cleaning, and analyze the dirtiness of the battery plate after cleaning to determine whether the battery plate needs to be immersed in water for cleaning again. When it is determined that re-cleaning is required, the cleaning process control is executed, otherwise the plating process operation is executed.

[0102] The cleaning process control module is used to obtain and adjust the immersion time based on the dirtiness after cleaning and perform re-immersion cleaning, and perform cleaning process monitoring after re-immersion cleaning.

[0103] The rack plating process operation module is used to divide the rack plating pool into a plurality of rack plating areas, immerse the battery plate in a plating solution for electroplating, wherein the plating solution parameters include the plating solution temperature and the plating solution flow rate.

[0104] The rack plating process monitoring module is used to divide the electroplating time into equally spaced time periods to obtain a number of detection time points, and set a temperature sensor and a flow rate sensor in each rack plating area to obtain the actual plating solution parameters of each rack plating area at each detection time point in the rack plating process operation and analyze the deviation of the plating solution parameters of each rack plating area corresponding to each detection time point.

[0105] The plating process control module is used to set a temperature control device and a stirring device on the mobile control device, and judge whether the actual plating solution parameters need to be adjusted in each plating area at each detection time point based on the deviation of the plating solution parameters. If necessary, the mobile control device is used to adjust the plating solution parameters until the appropriate plating solution parameters are reached.

[0106] The production line operation quality evaluation module is used to count and analyze the adjustment frequency and adjustment range in the cleaning process and the rack plating process, and then analyze the production line abnormality index.

[0107] A third aspect of the present invention provides a device, which includes any one of the above-mentioned magnetic pole plate silver plating production line control methods or battery pole plate silver plating production line control systems.

[0108] The above contents are merely examples and explanations of the concept of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the concept of the invention or exceed the scope defined by the present invention, they shall all fall within the protection scope of the present invention.

Claims

1. A control method for a battery plate silver plating production line, It is characterized in that The method comprises the following steps: S1. Cleaning process operation: using a high-definition camera to obtain the surface image of the battery plate before cleaning, analyzing the dirtiness of the battery plate before cleaning and calculating the initial immersion time, and then starting the machine to immerse and clean the battery plate; S2, cleaning process monitoring: using a high-definition camera to obtain the surface image of the battery plate after cleaning, and analyzing the dirtiness of the battery plate after cleaning, and then judging whether the battery plate needs to be immersed again for cleaning, and executing the cleaning process control step when it is judged that it needs to be cleaned again, otherwise executing the rack plating process operation step; S3, cleaning process control: based on the dirtiness after cleaning, the immersion time is adjusted and re-immersion cleaning is performed, and after re-immersion cleaning, the cleaning process monitoring step is performed; S4, rack plating process operation: the rack plating pool is divided into a plurality of rack plating areas, and the battery plate is immersed in the plating solution for electroplating; S5, rack plating process monitoring: from the beginning of electroplating, the electroplating process is divided into several detection time points according to equal intervals, and a temperature sensor and a flow rate sensor are set in each rack plating area to obtain the actual plating solution parameters of each rack plating area at each detection time point in the rack plating process operation, and the deviation of the plating solution parameters corresponding to each rack plating area at each detection time point is analyzed, wherein the plating solution parameters include plating solution temperature and plating solution flow rate; S6, rack plating process control: a temperature control device and a stirring device are arranged on the mobile control device, and based on the deviation of the plating solution parameters, it is determined whether the actual plating solution parameters need to be adjusted in each rack plating area at each detection time point, and if necessary, the plating solution parameters are adjusted by the mobile control device until the appropriate plating solution parameters are reached; S7. Production line operation quality evaluation: Statistics and analysis of the adjustment frequency and adjustment range in the cleaning process and the rack plating process, and then analysis of the production line abnormality index.

2. A battery plate silver plating production line control method as claimed in claim 1, Features: The steps of analyzing the dirtiness of the battery plates before cleaning and calculating the initial immersion time are as follows: The dirty area in the surface image of the battery plate before cleaning obtained by the high-definition camera is identified by edge detection processing technology to obtain the outline of the dirty area, and then the dirty area is obtained by importing it into the image processing software; Import the contour image of the battery plate into the image processing software to obtain the surface area of ​​the battery plate, and then substitute the dirty area area into the analysis formula Get the dirtiness coefficient of the battery plate before cleaning, where represents a natural constant; Substitute the dirtiness coefficient of the battery plate before cleaning into the calculation formula The initial immersion time is obtained, wherein the standard immersion time refers to the immersion cleaning time required for the standard dirtiness coefficient, and the standard dirtiness coefficient is the dirtiness coefficient of the battery plate under a preset standard state.

3. A battery plate silver plating production line control method as claimed in claim 1, Features: The determination of whether the battery plate needs to be immersed and cleaned again is as follows: Substitute the dirty coefficient of the battery plate after cleaning into the judgment model Get the judgment result whether it is necessary to immerse and clean again. Indicates the preset allowable dirtiness coefficient after cleaning. Indicates that the battery plates do not need to be immersed in water for cleaning again. Indicates that the battery plates need to be immersed and cleaned again.

4. A battery plate silver plating production line control method as claimed in claim 1, Features: The specific division of the rack plating area of ​​the rack plating pool is as follows: A number of longitudinal dividing lines are equally spaced on the outer wall of the plating pool, and the adjacent longitudinal dividing lines and the central axis of the plating pool divide the space of the plating pool into a number of areas, which are recorded as plating areas, and each plating area is numbered.

5. A battery plate silver plating production line control method as claimed in claim 1, Features: The analysis of the deviation of the plating solution parameters corresponding to each rack plating area at each detection time point is as follows: The actual bath temperature of each rack plating area at each detection time point and suitable bath temperature Substitute into the calculation formula of bath temperature deviation Get the first Detection time point Deviation of plating solution temperature in the rack plating area ,in Indicates the detection time point number, , Indicates the plating area number. ; Locate the appropriate plating solution flow rate corresponding to each detection time point from the standard plating solution flow rate change trend chart ; The actual plating solution flow rate of each rack plating area at each detection time point and appropriate bath flow rate Substitute into the calculation formula of plating solution flow rate deviation Get the first Detection time point Deviation of plating solution flow rate in the rack plating area ; The temperature deviation of the plating solution in each rack plating area at each detection time point and the deviation of plating solution flow rate Substitute into the calculation formula Get the first Detection time point Deviation of plating bath parameters in the rack plating area ,in They respectively represent the weights of the deviation of plating solution temperature and the deviation of plating solution flow rate.

6. A battery plate silver plating production line control method as claimed in claim 5, Features: The steps of judging whether the actual plating solution parameters need to be adjusted in each rack plating area at each detection time point are as follows: The deviation of the plating liquid parameters of each plating area at each detection time point is compared with the preset allowable deviation of the plating liquid parameters. If the deviation of the plating liquid parameters of a certain plating area at a certain detection time point is less than or equal to the preset allowable deviation of the plating liquid parameters, then the actual plating liquid parameters corresponding to the plating area at this detection time point do not need to be adjusted; if the deviation of the plating liquid parameters of a certain plating area at a certain detection time point is greater than the preset allowable deviation of the plating liquid parameters, then the actual plating liquid parameters corresponding to the plating area at this detection time point need to be adjusted, and then the detection time point is taken as an abnormal detection time point, and the plating area is taken as an abnormal plating area.

7. A battery plate silver plating production line control method as claimed in claim 6, Features: The steps of adjusting the parameters of the plating solution by using the mobile control device are as follows: Identify the abnormal direction of the abnormal plating area. If the deviation of the plating solution temperature of the abnormal plating area corresponding to a certain abnormal detection time point is greater than the allowable deviation of the plating solution temperature, then the abnormal plating area corresponding to the abnormal detection time point has a plating solution temperature abnormality. If the deviation of the plating solution flow rate of the abnormal plating area corresponding to a certain abnormal detection time point is greater than the allowable deviation of the plating solution flow rate, then the abnormal plating area corresponding to the abnormal detection time point has a plating solution flow rate abnormality. When the temperature of the plating solution in a certain abnormal plating area is abnormal, the mobile control device is used to move to the abnormal plating area and then the temperature of the plating solution in the plating area is adjusted by the temperature control device until the appropriate plating solution temperature is reached; When there is an abnormal plating solution flow rate in a certain abnormal hanging plating area, substitute the actual plating solution flow rate and the appropriate plating solution flow rate into the stirring device frequency calculation formula The stirring frequency of the stirring device is obtained, and then the mobile control device is used to move to the abnormal plating area and the plating solution flow rate of the plating area is adjusted by the stirring device according to the calculated stirring frequency.

8. A battery plate silver plating production line control method as claimed in claim 1, Features: The steps of analyzing the abnormal index of the production line are as follows: Substitute the immersion time adjustment frequency and immersion time adjustment amplitude into the formula Get the immersion time anomaly index ; Substitute the bath parameter adjustment frequency and bath parameter adjustment amplitude into the formula Get the abnormal index of plating bath parameters ; Then, the immersion time abnormality index and the plating solution parameter abnormality index are summed and calculated to obtain the production line abnormality index.

9. A battery plate silver plating production line control system, It is characterized in that The system includes: A cleaning process operation module is used to use a high-definition camera to obtain the surface image of the battery plate before cleaning, analyze the dirtiness of the battery plate before cleaning and calculate the initial immersion time, and then start the machine to immerse and clean the battery plate; The cleaning process monitoring module is used to use a high-definition camera to obtain the surface image of the battery plate after cleaning, and analyze the dirtiness of the battery plate after cleaning to determine whether the battery plate needs to be immersed in the water for cleaning again. When it is determined that cleaning is required again, the cleaning process control is performed, otherwise the rack plating process operation is performed; A cleaning process control module is used to adjust the immersion time based on the dirtiness after cleaning and perform re-immersion cleaning, and perform cleaning process monitoring after re-immersion cleaning; The rack plating process operation module is used to divide the rack plating pool into a plurality of rack plating areas, immerse the battery plate in the plating solution for electroplating, wherein the plating solution parameters include the plating solution temperature and the plating solution flow rate; The rack plating process monitoring module is used to divide the electroplating time into equal intervals to obtain a number of detection time points, set a temperature sensor and a flow rate sensor in each rack plating area to obtain the actual plating solution parameters of each rack plating area at each detection time point in the rack plating process operation, and analyze the deviation of the plating solution parameters of each rack plating area corresponding to each detection time point; The rack plating process control module is used to set a temperature control device and a stirring device on the mobile control device, and judge whether the actual plating solution parameters need to be adjusted in each rack plating area at each detection time point based on the deviation of the plating solution parameters. If necessary, the mobile control device is used to adjust the plating solution parameters until the appropriate plating solution parameters are reached; The production line operation quality evaluation module is used to count and analyze the adjustment frequency and adjustment range in the cleaning process and the rack plating process, and then analyze the production line abnormality index.