Oxidation and rust prevention treatment method and system for cutting tools

By dividing the monitoring area on the surface of the blade blank, collecting and analyzing the thickness data in real time, dynamically adjusting the argon gas usage and sputtering speed, and adjusting the argon gas supplementation based on the sputtering influence factors, the uniformity of titanium film deposition and the problem in the traditional PVD process are solved. The thickness is difficult to control, which improves production efficiency and product quality consistency.

CN118600375BActive Publication Date: 2024-10-15GUANGDONG OUYOU HOME FURNISHING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411034936.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-10-15
Estimated Expiration
2044-07-31

AI Technical Summary

Technical Problem

The lack of real-time monitoring and feedback adjustment mechanisms in the traditional PVD process makes it difficult to accurately control the uniformity and thickness of titanium film deposition, resulting in waste of resources and large differences in product quality. It relies on worker experience and has low production efficiency.

Method used

Divide the monitoring area on the surface of the tool blank, collect thickness data in real time, establish the first and second thickness data sets, dynamically adjust the argon gas usage and sputtering speed, and compare the sputtering influence factors with historical data to replenish the argon gas. Adjust to ensure the film thickness meets the requirements.

Benefits of technology

It improves the accuracy and consistency of titanium film deposition, reduces resource waste and dependence on workers' operating experience, ensures the stability and consistency of product quality, and provides a reliable reference for subsequent process optimization.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118600375B_ABST
    Figure CN118600375B_ABST
Patent Text Reader

Abstract

The present invention relates to the technical field of tool rust prevention, and discloses an oxidation rust prevention treatment method and system for tools, the method comprising: dividing a plurality of monitoring areas on the surface of a tool blank, collecting the average thickness of the tool blank to determine the amount of argon used and the sputtering speed; collecting the thickness data of the tool blank after processing to establish a second thickness data set, and comparing to determine whether the sputtering deposition is qualified; when the sputtering deposition is determined to be unqualified, collecting the sputtering distance of the titanium target from the tool blank, and calculating the sputtering influence factor according to the second thickness data set and the sputtering distance, comparing the sputtering influence factor with historical data, and determining the amount of argon supplement according to the comparison result; storing the data of the sputtering influence factor and the amount of argon supplement. The present invention improves the durability and working performance of the tool through film monitoring and adjustment and film deposition, and improves the consistency of the product.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of tool rust prevention, and in particular to an oxidation rust prevention treatment method and system for tools. Background Art

[0002] In modern manufacturing, the performance and life of cutting tools have a vital impact on production efficiency and product quality. In order to improve the wear resistance and corrosion resistance of cutting tools, physical vapor deposition (PVD) technology is widely used to deposit titanium films on the surface of cutting tools. However, the deposition quality of titanium films is directly affected by multiple process parameters, such as argon usage, sputtering speed, sputtering distance, etc. Therefore, how to accurately control these parameters to ensure that the uniformity and thickness of the titanium film meet the requirements has become an important issue in process optimization.

[0003] In the traditional PVD process, titanium film deposition is usually performed by setting fixed sputtering parameters, and then the tool surface is inspected to determine the film thickness. If the film thickness does not meet the requirements, the tool becomes a defective product and is scrapped. This method is inefficient and wastes a lot of resources. The lack of a feedback adjustment mechanism during the processing makes it impossible to improve the processing conditions according to the actual processing situation, and the parameter setting often relies on the workers' operating experience, which requires a high level of technical skills and easily causes large differences in product quality.

[0004] Therefore, it is necessary to design an oxidation anti-rust treatment method and system for cutting tools to solve the problems existing in the current technology. Summary of the invention

[0005] In view of this, the present invention proposes an oxidation anti-rust treatment method and system for cutting tools, aiming to solve the problems existing in the current cutting tool PVD processing technology, such as fixed parameters, lack of feedback adjustment mechanism, heavy reliance on workers' experience, resulting in large product differences and low production efficiency.

[0006] In one aspect, the present invention provides an oxidation anti-rust treatment method for a cutting tool, comprising:

[0007] Dividing the surface of the blade blank into several monitoring areas, collecting the thickness data of the blade blank in each of the monitoring areas to establish a first thickness data set, obtaining the average thickness of the blade blank according to the first thickness data set, and determining the amount of argon gas used and the sputtering speed according to the average thickness, wherein the argon gas is used to sputter a titanium target so that the surface of the blade blank is covered with a titanium film;

[0008] The blade blank after sputtering coating is deposited and annealed, and the thickness data of the blade blank after processing is collected to establish a second thickness data set, and each thickness data in the second thickness data set is compared with the thickness threshold, and whether the sputtering deposition is qualified is judged according to the comparison result; when the sputtering deposition is judged to be unqualified, the sputtering distance between the titanium target and the blade blank is collected, and the sputtering influence factor is calculated according to the second thickness data set and the sputtering distance, and the sputtering influence factor is compared with the historical data, and the argon gas supplement amount is determined according to the comparison result;

[0009] When the sputtering influence factor is different from the sputtering influence factor in the historical data, a supplementary area is determined and the first thickness data and the second thickness data of the supplementary area are compared to determine the initial argon gas supplement amount, and supplementary sputtering, deposition and annealing are performed; the third thickness data of the supplementary area after the supplementary sputtering is completed is collected, the data of the supplementary area in the second thickness data set is replaced with the third thickness data, and the second average thickness is calculated, and the second average thickness is compared with the thickness threshold value, and it is determined whether to adjust the initial argon gas supplement amount according to the comparison result, and the argon gas supplement amount is determined;

[0010] The data of the sputtering influence factor and the argon gas supplement amount are stored.

[0011] Further, when determining the amount of argon gas used and the sputtering speed according to the average thickness, it includes:

[0012] The average thickness is compared with a first preset thickness and a second preset thickness respectively, and the amount of argon gas used and the sputtering speed are determined according to the comparison results; the first preset thickness is less than the second preset thickness;

[0013] When the average thickness is less than or equal to the first preset thickness, the argon usage is determined to be the first preset usage, and the sputtering speed is determined to be the first preset sputtering speed; when the average thickness is greater than the first preset thickness and less than or equal to the second preset thickness, the argon usage is determined to be the second preset usage, and the sputtering speed is determined to be the second preset sputtering speed; when the average thickness is greater than the second preset thickness, the argon usage is determined to be the third preset usage, and the sputtering speed is determined to be the third preset sputtering speed;

[0014] Among them, the first preset usage is smaller than the second preset usage, the second preset usage is smaller than the third preset usage, the first preset sputtering speed is smaller than the second preset sputtering speed, and the second preset sputtering speed is smaller than the third preset sputtering speed.

[0015] Furthermore, after determining the argon gas usage and the sputtering speed, the method further includes:

[0016] The blade blank is placed in a vacuum chamber and fixed;

[0017] After the vacuum chamber is evacuated, the blade blank is heated to 200-400° C.;

[0018] applying a negative bias voltage to the blade blank;

[0019] The DC power supply is turned on, and the argon ions are controlled to bombard the titanium target material according to the argon gas usage and sputtering speed.

[0020] Further, judging whether the sputtering deposition is qualified according to the comparison result includes:

[0021] When each thickness data in the second thickness data set is greater than or equal to the thickness threshold, it is determined that the sputtering deposition is qualified;

[0022] When there is thickness data in the second thickness data set that is less than the thickness threshold, it is determined that the sputtering deposition is unqualified, and the monitoring area corresponding to the low thickness data is recorded.

[0023] Further, when calculating the sputtering influence factor according to the second thickness data set and the sputtering distance, it includes:

[0024] The sputtering influence factor is calculated by the following formula:

[0025] ;

[0026] Among them, I represents the sputtering influence factor, k represents the adjustment coefficient, N represents the number of unqualified areas, Hi represents the thickness of the i-th unqualified area after processing, T represents the thickness threshold, d represents the sputtering distance, and t represents the sputtering time.

[0027] Further, when determining the amount of argon gas to be supplemented according to the comparison result, it includes:

[0028] When the historical data contains data identical to the sputtering influencing factor, performing supplementary sputtering with the recorded argon gas supplementary amount;

[0029] When the historical data does not contain data identical to the sputtering influence factor, the data of the sputtering influence factor is stored, and the first thickness data and the second thickness data of the supplementary area are compared to determine the initial argon gas supplementation amount.

[0030] Furthermore, comparing the first thickness data and the second thickness data of the supplementary area to determine the initial argon supplement amount includes:

[0031] Obtaining a thickness difference value according to the first thickness data and the second thickness data, wherein the thickness difference value is the difference between the second thickness data and the first thickness data, comparing the thickness difference value with a first preset thickness difference value and a second preset thickness difference value respectively, wherein the first preset thickness difference value is smaller than the second preset thickness difference value, and determining an initial argon gas replenishment amount according to the comparison result;

[0032] When the thickness difference is less than or equal to a first preset thickness difference, determining the argon gas replenishment amount of the replenishment area to be the first preset replenishment amount;

[0033] When the thickness difference is greater than the first preset thickness difference and less than or equal to the second preset thickness difference, determining the argon gas replenishment amount of the replenishment area to be the second preset replenishment amount;

[0034] When the thickness difference is greater than the second preset thickness difference, determining the argon supplement amount of the supplement area to be a third preset supplement amount;

[0035] Wherein, the first preset replenishment amount is less than the second preset replenishment amount, and the second preset replenishment amount is less than the third preset replenishment amount;

[0036] The initial argon gas replenishment amount is obtained by determining the argon gas replenishment amount in each replenishment area and summing the amounts.

[0037] Further, judging whether to adjust the initial argon gas replenishment amount according to the comparison result includes:

[0038] When the second average thickness is greater than or equal to the thickness threshold, using the initial argon gas supplement amount as the argon gas supplement amount, and storing data of the argon gas supplement amount;

[0039] When the second average thickness is less than the thickness threshold, it is determined that the initial argon gas supplement amount is adjusted to obtain the argon gas supplement amount.

[0040] Further, the initial argon gas replenishment amount is adjusted to obtain the argon gas replenishment amount, including:

[0041] A supplementary thickness difference is obtained based on the second average thickness and the thickness threshold, an adjustment factor is determined based on the supplementary thickness difference to adjust the initial argon supplement amount, the argon supplement amount is obtained, and the data of the argon supplement amount is stored; the adjustment factor is proportional to the supplementary thickness difference.

[0042] Compared with the prior art, the beneficial effects of the present invention are: by dividing a number of monitoring areas on the surface of the blade blank, the thickness data is collected and analyzed in real time to dynamically adjust the argon usage and sputtering speed to ensure the uniformity and thickness of the titanium film deposition. By establishing a first thickness data set and a second thickness data set, the deposition process is feedback controlled to judge the qualification of the sputtering deposition, and when it is unqualified, the sputtering influence factor is calculated and the argon supplement amount is adjusted to perform supplementary sputtering, ultimately achieving the purpose of accurately controlling the film thickness. The accuracy and consistency of the titanium film deposition process are improved, the waste of resources and the dependence on the workers' operating experience are reduced, and the consistency and stability of the product quality are guaranteed. At the same time, through data storage and historical comparison, a reliable reference is provided for subsequent process optimization.

[0043] On the other hand, the present application also provides an oxidation anti-rust treatment system for cutting tools, which is used to apply the above oxidation anti-rust treatment method for cutting tools, comprising:

[0044] A collection unit is configured to divide a surface of a blade blank into a plurality of monitoring areas, collect thickness data of the blade blank in each of the monitoring areas to establish a first thickness data set, obtain an average thickness of the blade blank according to the first thickness data set, and determine an argon usage amount and a sputtering speed according to the average thickness, wherein the argon gas is used to sputter a titanium target so that the surface of the blade blank is covered with a titanium film;

[0045] A judgment unit is configured to perform deposition and annealing treatment on the blade blank after sputtering coating, collect thickness data of the blade blank after processing to establish a second thickness data set, compare each thickness data in the second thickness data set with the thickness threshold, and judge whether the sputtering deposition is qualified according to the comparison result; when the sputtering deposition is judged to be unqualified, collect the sputtering distance between the titanium target and the blade blank, calculate the sputtering influence factor according to the second thickness data set and the sputtering distance, compare the sputtering influence factor with the historical data, and determine the argon gas supplement amount according to the comparison result;

[0046] The adjustment unit is configured to, when the sputtering influence factor is different from the sputtering influence factor in the historical data, determine the supplementary area and compare the first thickness data and the second thickness data of the supplementary area, determine the initial argon gas supplement amount, and perform supplementary sputtering, deposition and annealing; collect the third thickness data of the supplementary area after the supplementary sputtering is completed, replace the data of the supplementary area in the second thickness data set with the third thickness data, calculate the second average thickness, compare the second average thickness with the thickness threshold, determine whether to adjust the initial argon gas supplement amount according to the comparison result, and determine the argon gas supplement amount;

[0047] The storage unit is configured to store the data of the sputtering influence factor and the argon gas supplement amount.

[0048] It is understandable that the above-mentioned oxidation anti-rust treatment method and system for cutting tools have the same beneficial effects, which will not be described in detail here. BRIEF DESCRIPTION OF THE DRAWINGS

[0049] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the detailed description of the preferred embodiments below. The accompanying drawings are only for the purpose of illustrating the preferred embodiments and are not to be considered as limiting the present invention. Moreover, the same reference symbols are used throughout the accompanying drawings to represent the same components. In the accompanying drawings:

[0050] Figure 1 A flow chart of an oxidation and rust prevention method for a cutting tool provided in an embodiment of the present invention;

[0051] Figure 2 This is a structural block diagram of an oxidation and rust prevention system for cutting tools provided in an embodiment of the present invention. DETAILED DESCRIPTION

[0052] Exemplary embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. Although exemplary embodiments of the present disclosure are shown in the accompanying drawings, it should be understood that the present disclosure can be implemented in various forms and should not be limited by the embodiments described herein. On the contrary, these embodiments are provided in order to enable a more thorough understanding of the present disclosure and to fully convey the scope of the present disclosure to those skilled in the art. It should be noted that, in the absence of conflict, the embodiments of the present invention and the features described in the embodiments can be combined with each other. The present invention will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.

[0053] In modern manufacturing, the performance and life of cutting tools have a crucial impact on production efficiency and product quality. In order to improve the wear resistance and corrosion resistance of cutting tools, physical vapor deposition technology is widely used to deposit titanium films on the surface of cutting tools. However, the deposition quality of titanium films is directly affected by multiple process parameters, such as argon usage, sputtering speed, sputtering distance, etc. Therefore, how to accurately control these parameters to ensure that the uniformity and thickness of the titanium film meet the requirements has become an important issue in process optimization.

[0054] In the traditional PVD process, titanium film deposition is usually performed by setting fixed sputtering parameters, and then the tool surface is inspected to determine the film thickness. If the film thickness does not meet the requirements, the tool becomes a defective product and is scrapped. This method is inefficient and there is a large waste of resources. In addition, parameter settings often rely on the workers' operating experience, which requires a high level of technical skills and easily causes large differences in product quality. This not only increases production costs, but also affects the consistency and reliability of products.

[0055] In the current technology, there is a lack of a PVD process that can be monitored and feedback controlled in real time, which makes it difficult to accurately control the film thickness and uniformity. Therefore, it is necessary to design an oxidation anti-rust treatment method and system for cutting tools to solve the problems existing in the current technology.

[0056] Therefore, it is necessary to design an oxidation anti-rust treatment method and system for cutting tools to solve the problems existing in the current technology.

[0057] In some embodiments of the present application, see Figure 1 As shown, a method for oxidation anti-rust treatment of a cutting tool comprises:

[0058] S100: Divide the surface of the blade blank into several monitoring areas, collect the thickness data of the blade blank in each monitoring area to establish a first thickness data set, obtain the average thickness of the blade blank according to the first thickness data set, determine the amount of argon gas used and the sputtering speed according to the average thickness, and use argon gas to sputter the titanium target so that the surface of the blade blank is covered with a titanium film.

[0059] S200: Deposition and annealing treatment are performed on the blade blank after sputtering coating, and the thickness data of the blade blank after processing is collected to establish a second thickness data set, and each thickness data in the second thickness data set is compared with the thickness threshold, and whether the sputtering deposition is qualified is judged according to the comparison result; when the sputtering deposition is judged to be unqualified, the sputtering distance of the titanium target from the blade blank is collected, and the sputtering influence factor is calculated according to the second thickness data set and the sputtering distance, and the sputtering influence factor is compared with the historical data, and the argon gas supplement amount is determined according to the comparison result.

[0060] S300: When the sputtering influence factor is different from the sputtering influence factor in the historical data, determine the supplementary area and compare the first thickness data and the second thickness data of the supplementary area to determine the initial argon gas supplement amount, and perform supplementary sputtering, deposition and annealing treatment; collect the third thickness data of the supplementary area after the supplementary sputtering is completed, replace the data of the supplementary area in the second thickness data set with the third thickness data, calculate the second average thickness, compare the second average thickness with the thickness threshold, and determine whether to adjust the initial argon gas supplement amount based on the comparison result, and determine the argon gas supplement amount.

[0061] S400: storing data of the sputtering influence factor and the argon gas supplement amount.

[0062] Specifically, in S100, the surface of the blade blank is divided into several monitoring areas, and the blade blank thickness data in each monitoring area is collected and a first thickness data set is established. The average thickness of the blade blank is calculated according to the first thickness data set, and the amount of argon used and the sputtering speed are determined based on the average thickness. Ensure that during the initial sputtering process, the amount of argon used and the sputtering speed can evenly cover the surface of the blade blank with a layer of titanium film. In S200, the blade blank that has been sputtered and coated is deposited and annealed, and the thickness data of the blade blank after the treatment is collected to establish a second thickness data set. Each thickness data in the second thickness data set is compared with a preset thickness threshold, and whether the sputtering deposition is qualified is determined based on the comparison result. If the sputtering deposition is determined to be unqualified, the sputtering distance between the titanium target and the blade blank is collected, and the sputtering influence factor is calculated based on the second thickness data set and the sputtering distance. The sputtering influence factor is compared with the historical data to determine the amount of argon that needs to be supplemented. In S300, if the current sputtering influence factor is different from the sputtering influence factor in the historical data, the area that needs to be supplemented with sputtering is determined, and the first thickness data and the second thickness data of the area are compared to determine the initial argon gas replenishment amount. After supplementary sputtering, deposition and annealing, the third thickness data of the supplementary area after the supplementary sputtering is completed is collected. The data of the supplementary area in the second thickness data set is replaced with the third thickness data, and a new second average thickness is calculated. The new second average thickness is compared with the thickness threshold, and it is determined whether the initial argon gas replenishment amount needs to be adjusted based on the comparison result to finally determine the argon gas replenishment amount. In S400, the sputtering influence factor and the argon gas replenishment amount data are stored. Provide a reference for subsequent process optimization to further improve the stability and controllability of the deposition process.

[0063] It is understandable that by real-time monitoring and feedback control of the thickness data of the blade blank during the sputtering process, the argon usage and sputtering speed are dynamically adjusted to ensure that the uniformity and thickness of the titanium film meet the requirements. By collecting and comparing thickness data multiple times and using the sputtering influencing factors for supplementary adjustments, the accuracy and consistency of sputtering deposition are improved, resource waste and dependence on worker experience are reduced, and product quality and stability are guaranteed. At the same time, through data storage and analysis, a reliable reference is provided for subsequent process optimization, which is conducive to improving the corrosion resistance and wear resistance of the tool and extending the service life of the tool.

[0064] In some embodiments of the present application, when determining the amount of argon gas used and the sputtering speed according to the average thickness, the method includes: comparing the average thickness with a first preset thickness and a second preset thickness respectively, and determining the amount of argon gas used and the sputtering speed according to the comparison results; the first preset thickness is less than the second preset thickness;

[0065] Specifically, when the average thickness is less than or equal to the first preset thickness, the argon usage is determined to be the first preset usage, and the sputtering speed is determined to be the first preset sputtering speed; when the average thickness is greater than the first preset thickness and less than or equal to the second preset thickness, the argon usage is determined to be the second preset usage, and the sputtering speed is determined to be the second preset sputtering speed; when the average thickness is greater than the second preset thickness, the argon usage is determined to be the third preset usage, and the sputtering speed is determined to be the third preset sputtering speed; wherein the first preset usage is less than the second preset usage, the second preset usage is less than the third preset usage, the first preset sputtering speed is less than the second preset sputtering speed, and the second preset sputtering speed is less than the third preset sputtering speed.

[0066] It can be understood that by measuring and controlling the average thickness of the blade blank to dynamically adjust the argon usage and sputtering speed, the uniformity and stability of the coating are ensured. Dynamic adjustment improves the quality and consistency of the coating and reduces the performance instability caused by uneven coating. In addition, through the reasonable setting of preset thickness and preset parameters, the entire sputtering deposition process is more automated and intelligent, effectively reducing production costs and process complexity.

[0067] In some embodiments of the present application, after determining the amount of argon gas used and the sputtering speed, it also includes: loading the knife blank into a vacuum chamber and fixing it; after evacuating the vacuum chamber, heating the knife blank to 200-400°C; applying a negative bias voltage to the knife blank; turning on a DC power supply to control the argon ion bombardment of the titanium target according to the amount of argon gas used and the sputtering speed.

[0068] Specifically, the blade blank is placed in a vacuum chamber and fixed to ensure that the position of the blade blank remains stable during subsequent processing. The vacuum chamber is evacuated to reduce the influence of gas impurities. The blade blank is heated to 200-400°C to improve the adhesion and uniformity of the titanium film. A negative bias voltage (-100V to -200V) is applied to the blade blank to enhance the bombardment effect of argon ions and improve the sputtering efficiency. The DC power supply is turned on, and the bombardment of argon ions is controlled using the previously determined argon usage and sputtering speed, so that the argon ions bombard the titanium target, sputter out titanium atoms and form a titanium film on the surface of the blade blank.

[0069] It is understandable that deposition is carried out in a vacuum environment, which reduces the interference of gas impurities. Heating the blade blank allows the titanium film to better adhere to the surface of the blade blank and improves the uniformity of the film. Applying a negative bias enhances the bombardment effect of argon ions, improves the sputtering efficiency, and makes the deposition process more efficient. The DC power supply precisely controls the bombardment of argon ions on the titanium target, ensuring the stability and controllability of the sputtering process. By setting specific parameters and steps, the dependence on the worker's operating experience is reduced, ensuring the consistency and stability of the product.

[0070] In some embodiments of the present application, judging whether the sputtering deposition is qualified according to the comparison result includes:

[0071] When all thickness data in the second thickness data set are greater than or equal to the thickness threshold, the sputtering deposition is determined to be qualified; when there is thickness data in the second thickness data set that is less than the thickness threshold, the sputtering deposition is determined to be unqualified, and the monitoring area corresponding to the low thickness data is recorded.

[0072] It is understandable that the control accuracy and production efficiency of the blade blank lamination process are improved through clear qualification criteria and unqualified area recording mechanism. By timely identifying and handling unqualified areas, the scrap rate caused by unqualified lamination quality is reduced, and production costs are reduced. Quantitative thickness data comparison and recording also enhances the traceability and management efficiency of the production process.

[0073] In some embodiments of the present application, when calculating the sputtering influence factor according to the second thickness data set and the sputtering distance, it includes:

[0074] The sputtering influence factor is calculated by the following formula:

[0075] ;

[0076] Among them, I represents the sputtering influence factor, k represents the adjustment coefficient, N represents the number of unqualified areas, Hi represents the thickness of the i-th unqualified area after processing, T represents the thickness threshold, d represents the sputtering distance, and t represents the sputtering time.

[0077] It is understandable that by calculating the sputtering influence factor, the degree of influence of each unqualified area on the coating quality can be quantitatively evaluated, which helps to accurately determine the priority and amplitude of adjusting the sputtering parameters. Quantitative analysis based on actual data improves the efficiency of diagnosing and solving coating quality problems, reduces resource waste and increased production costs caused by unqualified coating. The calculation method of the sputtering influence factor also enhances the controllability and predictability of the production process.

[0078] In some embodiments of the present application, when determining the amount of argon gas replenishment based on the comparison results, it includes: when there is data identical to the sputtering influence factor in the historical data, supplementary sputtering is performed with the recorded argon gas replenishment amount; when there is no data identical to the sputtering influence factor in the historical data, the data of the sputtering influence factor is stored, and the first thickness data and the second thickness data of the replenishment area are compared to determine the initial argon gas replenishment amount.

[0079] In some embodiments of the present application, when comparing the first thickness data and the second thickness data of the replenishment area to determine the initial argon replenishment amount, the method includes: obtaining a thickness difference according to the first thickness data and the second thickness data, where the thickness difference is the difference between the second thickness data and the first thickness data, comparing the thickness difference with a first preset thickness difference and a second preset thickness difference respectively, where the first preset thickness difference is less than the second preset thickness difference, and determining the initial argon replenishment amount according to the comparison result;

[0080] Specifically, when the thickness difference is less than or equal to the first preset thickness difference, the argon supplementary amount of the supplementary area is determined to be the first preset supplementary amount; when the thickness difference is greater than the first preset thickness difference and less than or equal to the second preset thickness difference, the argon supplementary amount of the supplementary area is determined to be the second preset supplementary amount; when the thickness difference is greater than the second preset thickness difference, the argon supplementary amount of the supplementary area is determined to be the third preset supplementary amount; wherein the first preset supplementary amount is less than the second preset supplementary amount, and the second preset supplementary amount is less than the third preset supplementary amount; after determining the argon supplementary amount of each supplementary area, the sum is performed to obtain the initial argon supplementary amount.

[0081] It can be understood that through the comparison and calculation process, the amount of argon gas replenishment in each replenishment area is effectively determined to ensure the consistency and stability of the coating quality. The calculation method based on actual data and preset values ​​improves the efficiency and accuracy of the replenishment process and avoids unnecessary waste caused by excessive or insufficient replenishment. Through the comparison and recording of historical data, the traceability and manageability of coating quality control in the production process are enhanced.

[0082] In some embodiments of the present application, whether to adjust the initial argon gas supplement amount is determined based on the comparison result, including: when the second average thickness is greater than or equal to the thickness threshold, the initial argon gas supplement amount is used as the argon gas supplement amount, and the data of the argon gas supplement amount is stored; when the second average thickness is less than the thickness threshold, it is determined to adjust the initial argon gas supplement amount to obtain the argon gas supplement amount.

[0083] In some embodiments of the present application, the initial argon gas replenishment amount is adjusted to obtain the argon gas replenishment amount, including: obtaining the replenishment thickness difference based on the second average thickness and the thickness threshold, determining the adjustment factor based on the replenishment thickness difference to adjust the initial argon gas replenishment amount, obtaining the argon gas replenishment amount, and storing the data of the argon gas replenishment amount; the adjustment factor is proportional to the replenishment thickness difference.

[0084] Specifically, for example, the second average thickness measurement result is 400nm, and the thickness threshold is 450nm. The supplementary thickness difference is 50nm. According to the set proportional relationship, the adjustment factor is 0.1 times the supplementary thickness difference, so the adjustment factor is 5. The initial argon gas replenishment amount is set to 100 units. Under the effect of the adjustment factor, the adjusted argon gas replenishment amount is 105 units. This argon gas replenishment amount data is stored to provide a basis for the next process adjustment.

[0085] It can be understood that by dynamically adjusting the amount of argon gas replenishment, the amount of argon gas used during the coating process is ensured based on the comparison between the actual measurement results and the preset threshold, thereby improving the stability and consistency of the coating quality, optimizing production efficiency, and reducing resource waste and costs.

[0086] In the above embodiment, several monitoring areas are divided on the surface of the blade blank to collect and analyze thickness data in real time, so as to dynamically adjust the amount of argon used and the sputtering speed to ensure the uniformity and thickness of the titanium film deposition. By establishing a first thickness data set and a second thickness data set, the deposition process is feedback controlled to judge the qualification of the sputtering deposition, and when it is unqualified, the sputtering influence factor is calculated and the argon supplement amount is adjusted to perform supplementary sputtering, so as to finally achieve the purpose of accurately controlling the film thickness. The accuracy and consistency of the titanium film deposition process are improved, the waste of resources and the dependence on the workers' operating experience are reduced, and the consistency and stability of the product quality are ensured. At the same time, through data storage and historical comparison, a reliable reference is provided for subsequent process optimization.

[0087] In another preferred embodiment based on the above embodiment, refer to Figure 2 As shown, this embodiment provides an oxidation anti-rust treatment system for a tool, which is used to apply the above oxidation anti-rust treatment method for a tool, including:

[0088] A collection unit is configured to divide a surface of a blade blank into a plurality of monitoring areas, collect thickness data of the blade blank in each monitoring area to establish a first thickness data set, obtain an average thickness of the blade blank according to the first thickness data set, determine an argon usage amount and a sputtering speed according to the average thickness, and use the argon gas to sputter a titanium target so that the surface of the blade blank is covered with a titanium film;

[0089] The judgment unit is configured to perform deposition and annealing treatment on the blade blank after sputtering coating, collect thickness data of the blade blank after processing to establish a second thickness data set, compare each thickness data in the second thickness data set with the thickness threshold, and judge whether the sputtering deposition is qualified according to the comparison result; when the sputtering deposition is judged to be unqualified, collect the sputtering distance between the titanium target and the blade blank, calculate the sputtering influence factor according to the second thickness data set and the sputtering distance, compare the sputtering influence factor with the historical data, and determine the argon gas supplement amount according to the comparison result;

[0090] The adjustment unit is configured to determine the supplementary area and compare the first thickness data and the second thickness data of the supplementary area when the sputtering influence factor is different from the sputtering influence factor in the historical data, determine the initial argon gas supplement amount, and perform supplementary sputtering, deposition and annealing; collect the third thickness data of the supplementary area after the supplementary sputtering is completed, replace the data of the supplementary area in the second thickness data set with the third thickness data, calculate the second average thickness, compare the second average thickness with the thickness threshold, determine whether to adjust the initial argon gas supplement amount according to the comparison result, and determine the argon gas supplement amount;

[0091] The storage unit is configured to store data of the sputtering influence factor and the argon gas supplement amount.

[0092] It is understandable that by dividing the surface of the blade blank into several monitoring areas, the thickness data is collected and analyzed in real time to dynamically adjust the argon usage and sputtering speed to ensure the uniformity and thickness of the titanium film deposition. By establishing the first thickness data set and the second thickness data set, the deposition process is feedback controlled to judge the qualification of the sputtering deposition, and when it is unqualified, the sputtering influence factor is calculated and the argon supplement amount is adjusted for supplementary sputtering, ultimately achieving the purpose of accurately controlling the film thickness. The accuracy and consistency of the titanium film deposition process are improved, the waste of resources and the dependence on the workers' operating experience are reduced, and the consistency and stability of product quality are ensured. At the same time, through data storage and historical comparison, a reliable reference is provided for subsequent process optimization.

[0093] Those skilled in the art will appreciate that the embodiments of the present application may be provided as methods, systems or computer program products. Therefore, the present application may take the form of a complete hardware embodiment, a complete software embodiment, or an embodiment combining software and hardware. Moreover, the present application may take the form of a computer program product implemented on one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) containing computer-usable program codes.

[0094] The present application is described with reference to the flowcharts and / or block diagrams of the methods, devices (systems) and computer program products according to the embodiments of the present application. It should be understood that each process and / or box in the flowchart and / or block diagram, as well as the combination of processes and / or boxes in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor or other programmable data processing device to produce a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.

[0095] These computer program instructions may also be stored in a computer-readable memory capable of directing a computer or other programmable data processing device to operate in a specific manner, so that the instructions stored in the computer-readable memory produce an article of manufacture comprising an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.

[0096] These computer program instructions can also be loaded onto a computer or other programmable data processing device so that a series of operating steps are executed on the computer or other programmable device to produce a computer-implemented process, thereby providing instructions for implementing the process. Figure 1 A process or multiple processes and / or boxes Figure 1 The steps for the functions specified in one or more boxes.

[0097] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the above embodiments, ordinary technicians in the relevant field should understand that the specific implementation methods of the present invention can still be modified or replaced by equivalents. Any modification or equivalent replacement that does not depart from the spirit and scope of the present invention should be covered within the scope of protection of the claims of the present invention.

Claims

1. A method for oxidation rust prevention of cutting tools, characterized in that: include: Dividing the surface of the blade blank into several monitoring areas, collecting the thickness data of the blade blank in each of the monitoring areas to establish a first thickness data set, obtaining the average thickness of the blade blank according to the first thickness data set, and determining the amount of argon gas used and the sputtering speed according to the average thickness, wherein the argon gas is used to sputter a titanium target so that the surface of the blade blank is covered with a titanium film; The blade blank after sputtering coating is deposited and annealed, and the thickness data of the blade blank after processing is collected to establish a second thickness data set, and each thickness data in the second thickness data set is compared with the thickness threshold, and whether the sputtering deposition is qualified is judged according to the comparison result; when the sputtering deposition is judged to be unqualified, the sputtering distance between the titanium target and the blade blank is collected, and the sputtering influence factor is calculated according to the second thickness data set and the sputtering distance, and the sputtering influence factor is compared with the historical data, and the argon gas supplement amount is determined according to the comparison result; When the sputtering influence factor is different from the sputtering influence factor in the historical data, a supplementary area is determined and the first thickness data and the second thickness data of the supplementary area are compared to determine the initial argon gas supplement amount, and supplementary sputtering, deposition and annealing are performed; the third thickness data of the supplementary area after the supplementary sputtering is completed is collected, the data of the supplementary area in the second thickness data set is replaced with the third thickness data, and the second average thickness is calculated, and the second average thickness is compared with the thickness threshold value, and it is determined whether to adjust the initial argon gas supplement amount according to the comparison result, and the argon gas supplement amount is determined; Storing the data of the sputtering influence factor and the argon gas supplement amount; When calculating the sputtering influence factor according to the second thickness data set and the sputtering distance, it includes: The sputtering influence factor is calculated by the following formula: ; Among them, I represents the sputtering influence factor, k represents the adjustment coefficient, N represents the number of unqualified areas, Hi represents the thickness of the i-th unqualified area after processing, T represents the thickness threshold, d represents the sputtering distance, and t represents the sputtering time.

2. The oxidation anti-rust treatment method for cutting tools according to claim 1, characterized in that: When determining the amount of argon gas used and the sputtering speed according to the average thickness, it includes: The average thickness is compared with a first preset thickness and a second preset thickness respectively, and the amount of argon gas used and the sputtering speed are determined according to the comparison results; the first preset thickness is less than the second preset thickness; When the average thickness is less than or equal to the first preset thickness, the argon usage is determined to be the first preset usage, and the sputtering speed is determined to be the first preset sputtering speed; when the average thickness is greater than the first preset thickness and less than or equal to the second preset thickness, the argon usage is determined to be the second preset usage, and the sputtering speed is determined to be the second preset sputtering speed; when the average thickness is greater than the second preset thickness, the argon usage is determined to be the third preset usage, and the sputtering speed is determined to be the third preset sputtering speed; Among them, the first preset usage is smaller than the second preset usage, the second preset usage is smaller than the third preset usage, the first preset sputtering speed is smaller than the second preset sputtering speed, and the second preset sputtering speed is smaller than the third preset sputtering speed.

3. The oxidation anti-rust treatment method for cutting tools according to claim 2, characterized in that: After determining the argon gas usage and sputtering speed, the process further includes: The blade blank is placed in a vacuum chamber and fixed; After the vacuum chamber is evacuated, the blade blank is heated to 200-400° C.; applying a negative bias voltage to the blade blank; The DC power supply is turned on, and the argon ions are controlled to bombard the titanium target material according to the argon gas usage and sputtering speed.

4. The oxidation anti-rust treatment method for cutting tools according to claim 1, characterized in that: When judging whether the sputtering deposition is qualified based on the comparison results, it includes: When each thickness data in the second thickness data set is greater than or equal to the thickness threshold, it is determined that the sputtering deposition is qualified; When there is thickness data in the second thickness data set that is less than the thickness threshold, it is determined that the sputtering deposition is unqualified, and the monitoring area corresponding to the low thickness data is recorded.

5. The oxidation anti-rust treatment method for cutting tools according to claim 1, characterized in that: When determining the amount of argon gas to be added based on the comparison results, it includes: When the historical data contains data identical to the sputtering influencing factor, performing supplementary sputtering with the recorded argon gas supplementary amount; When the historical data does not contain data identical to the sputtering influence factor, the data of the sputtering influence factor is stored, and the first thickness data and the second thickness data of the supplementary area are compared to determine the initial argon gas supplementation amount.

6. The oxidation anti-rust treatment method for cutting tools according to claim 5, characterized in that: The first thickness data and the second thickness data of the supplementary area are compared to determine the initial argon supplement amount, including: Obtaining a thickness difference value according to the first thickness data and the second thickness data, wherein the thickness difference value is the difference between the second thickness data and the first thickness data, comparing the thickness difference value with a first preset thickness difference value and a second preset thickness difference value respectively, wherein the first preset thickness difference value is smaller than the second preset thickness difference value, and determining an initial argon gas replenishment amount according to the comparison result; When the thickness difference is less than or equal to a first preset thickness difference, determining the argon gas replenishment amount of the replenishment area to be the first preset replenishment amount; When the thickness difference is greater than the first preset thickness difference and less than or equal to the second preset thickness difference, determining the argon gas replenishment amount of the replenishment area to be the second preset replenishment amount; When the thickness difference is greater than the second preset thickness difference, determining the argon supplement amount of the supplement area to be a third preset supplement amount; Wherein, the first preset replenishment amount is less than the second preset replenishment amount, and the second preset replenishment amount is less than the third preset replenishment amount; The initial argon gas replenishment amount is obtained by determining the argon gas replenishment amount in each replenishment area and summing the amounts.

7. The oxidation anti-rust treatment method for cutting tools according to claim 6, characterized in that: When judging whether to adjust the initial argon gas replenishment amount according to the comparison result, it includes: When the second average thickness is greater than or equal to the thickness threshold, using the initial argon gas supplement amount as the argon gas supplement amount, and storing data of the argon gas supplement amount; When the second average thickness is less than the thickness threshold, it is determined that the initial argon gas supplement amount is adjusted to obtain the argon gas supplement amount.

8. The oxidation anti-rust treatment method for cutting tools according to claim 7, characterized in that: The initial argon gas replenishment amount is adjusted to obtain the argon gas replenishment amount, comprising: A supplementary thickness difference is obtained based on the second average thickness and the thickness threshold, an adjustment factor is determined based on the supplementary thickness difference to adjust the initial argon supplement amount, the argon supplement amount is obtained, and the data of the argon supplement amount is stored; the adjustment factor is proportional to the supplementary thickness difference.

9. An oxidation anti-rust treatment system for cutting tools, used for applying the oxidation anti-rust treatment method for cutting tools as claimed in any one of claims 1 to 8, characterized in that: include: A collection unit is configured to divide a surface of a blade blank into a plurality of monitoring areas, collect thickness data of the blade blank in each of the monitoring areas to establish a first thickness data set, obtain an average thickness of the blade blank according to the first thickness data set, and determine an argon usage amount and a sputtering speed according to the average thickness, wherein the argon gas is used to sputter a titanium target so that the surface of the blade blank is covered with a titanium film; A judgment unit is configured to perform deposition and annealing treatment on the blade blank after sputtering coating, collect thickness data of the blade blank after processing to establish a second thickness data set, compare each thickness data in the second thickness data set with the thickness threshold, and judge whether the sputtering deposition is qualified according to the comparison result; when the sputtering deposition is judged to be unqualified, collect the sputtering distance between the titanium target and the blade blank, calculate the sputtering influence factor according to the second thickness data set and the sputtering distance, compare the sputtering influence factor with the historical data, and determine the argon gas supplement amount according to the comparison result; The adjustment unit is configured to, when the sputtering influence factor is different from the sputtering influence factor in the historical data, determine the supplementary area and compare the first thickness data and the second thickness data of the supplementary area, determine the initial argon gas supplement amount, and perform supplementary sputtering, deposition and annealing; collect the third thickness data of the supplementary area after the supplementary sputtering is completed, replace the data of the supplementary area in the second thickness data set with the third thickness data, calculate the second average thickness, compare the second average thickness with the thickness threshold, determine whether to adjust the initial argon gas supplement amount according to the comparison result, and determine the argon gas supplement amount; The storage unit is configured to store the data of the sputtering influence factor and the argon gas supplement amount.