Quantum dot film, method for making quantum dot film, and display device

By setting and limiting the quantum dot positions in the first quantum hole and the second quantum hole in the quantum dot film, the problem of low white light purity in the traditional quantum dot film is solved, and the color accuracy and color gamut coverage of the display device are improved .

CN118630118BActive Publication Date: 2024-12-06HKC CORP LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411089097.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-09
Publication Date
2024-12-06
Estimated Expiration
2044-08-09

AI Technical Summary

Technical Problem

After the first primary color light in a conventional quantum dot film passes through the quantum dot film, the purity of the second primary color light and the third primary color light formed by excitation is insufficient, resulting in the purity of the final mixed white light.

Method used

The first quantum hole and the second quantum hole are arranged in the quantum dot film, and the positions of the first quantum dot and the second quantum dot are restricted through the first quantum hole and the second quantum dot to ensure that there is no intersection in the light exit direction of the display device stack to reduce unnecessary interactions between the third primary color light and the first quantum dot and the second quantum dot, avoid spectral overlap, and improve the ray purity of the second primary color light and the third primary color light.

Benefits of technology

By reducing spectral overlap, the color accuracy of the display device and the purity of the white light are improved, and the color gamut coverage and color expression are enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118630118B_ABST
    Figure CN118630118B_ABST
Patent Text Reader

Abstract

A quantum dot film, a method for making the quantum dot film, and a display device, wherein the quantum dot film is provided with a first quantum hole and a second quantum hole, wherein the first quantum dot is provided in the first quantum hole, and the first quantum dot is used to excite and form a first primary color light; wherein the second quantum dot is provided in the second quantum hole, and the second quantum dot is used to excite and form a second primary color light, and along the thickness direction of the quantum dot film, the projected overlapping area of ​​the second quantum dot and the first quantum dot is 0. The technical solution of the present application is to provide the first quantum hole and the second quantum hole in the quantum dot film, and to limit the positions of the first quantum dot and the second quantum dot by the first quantum hole and the second quantum hole, so as to ensure that the first quantum dot and the second quantum dot are provided in the quantum dot film without overlap in the light emitting direction of the display device. In this way, unnecessary interactions between the third primary color light and the first quantum dot and the second quantum dot when passing through the quantum dot film are reduced, and the color accuracy of the display device is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of quantum dot films, and in particular to a quantum dot film, a method for manufacturing the quantum dot film, and a display device. Background Art

[0002] Quantum dots, also known as nanocrystals, are semiconductor particles composed of II-VI or III-V elements, with a particle size generally between 1 and 10 nm. These semiconductor particles have a unique property, that is, whenever stimulated by light or electricity, they emit light of a specific frequency, and the frequency of the light changes with the size of the semiconductor.

[0003] In a traditional quantum dot film, a first quantum dot and a second quantum dot are usually provided, and the diameters of the first quantum dot and the second quantum dot are different. When the third primary color light of the light source is irradiated into the quantum dot film, the third primary color light emitted by the light source can interact with the first quantum dot and the second quantum dot in the quantum dot film, and excite the first quantum dot to form the first primary color light, and excite the second quantum dot to form the second primary color light. The first primary color light, the second primary color light and the third primary color light of the light source are mixed with each other to produce high-quality white light. This unique process not only significantly improves the color gamut coverage of the display, but also can restore colors more realistically, meeting users' needs for high color expression.

[0004] However, in the related art, after the first primary color light passes through the quantum dot film, the purity of the second primary color light and the third primary color light excited and formed is insufficient, resulting in low purity of the final mixed white light. Summary of the invention

[0005] The purpose of the present application is to provide a quantum dot film, a method for manufacturing a quantum dot film, and a display device, aiming to solve the problem of low purity of white light generated by the quantum dot film in the related art.

[0006] To achieve the purpose of the present application, in a first aspect, the present application provides a quantum dot film, wherein the quantum dot film is provided with a first quantum hole and a second quantum hole, wherein the first quantum hole is provided with a first quantum dot, and the first quantum dot is used to excite and form a first primary color light;

[0007] The second quantum hole is provided with a second quantum dot, and the second quantum dot is used for exciting to form a second primary color light. Along the thickness direction of the quantum dot film, the projected overlapping area of ​​the second quantum dot and the first quantum dot is 0.

[0008] In one possible implementation, the quantum dot film includes a plurality of first quantum holes and a plurality of second quantum holes; along the thickness direction of the quantum dot film, the projections of the first quantum holes and the projections of the second quantum holes are alternately arranged in sequence along the length direction of the quantum dot film and / or the width direction of the quantum dot film.

[0009] In a possible implementation, the aperture of the first quantum hole is A, the aperture of the second quantum hole is B, the distance between each adjacent first quantum hole and second quantum hole is C, and A>C>B.

[0010] In a possible implementation, in each of the first quantum holes, the number of the first quantum dots is N, and in each of the second quantum holes, the number of the second quantum dots is M, where N=M.

[0011] In a second aspect, the present application further proposes a method for manufacturing a quantum dot film, the method for manufacturing the quantum dot film comprising the following steps:

[0012] Forming a first quantum hole and a second quantum hole in the quantum dot film;

[0013] The first quantum hole is filled with a first quantum dot, and the second quantum hole is filled with a second quantum dot.

[0014] In a possible implementation, the diameter of the first quantum dot is greater than the diameter of the second quantum dot, the aperture of the first quantum hole is greater than the aperture of the second quantum hole, and the filling of the first quantum dot into the first quantum hole and the filling of the second quantum dot into the second quantum hole comprises the following steps:

[0015] Filling the first quantum hole with a first substance;

[0016] coating a second substance on the second quantum dot, wherein the second substance and the first substance repel each other;

[0017] The first quantum dots and the second quantum dots are coated on the quantum dot film, so that the first quantum holes are filled with the first quantum dots and the second quantum holes are filled with the second quantum dots.

[0018] In a possible implementation, before coating the first quantum dots and the second quantum dots on the quantum dot film, the method further includes the following steps:

[0019] The second quantum hole is filled with a third substance, and the third substance and the second substance attract each other.

[0020] In a possible implementation manner, the first substance and the third substance are positively charged substances; and the second substance is negatively charged substance.

[0021] In a possible implementation manner, the charge amount of the second substance is smaller than the charge amount of the third substance.

[0022] In a third aspect, the present application further provides a display device, the display device comprising a quantum dot film, the quantum dot film being provided with a first quantum hole and a second quantum hole, the first quantum hole being provided with a first quantum dot, the first quantum dot being used to excite and form a first primary color light;

[0023] The second quantum hole is provided with a second quantum dot, and the second quantum dot is used for exciting to form a second primary color light. Along the thickness direction of the quantum dot film, the projected overlapping area of ​​the second quantum dot and the first quantum dot is 0.

[0024] The technical solution of the present application is to set the first quantum hole and the second quantum hole in the quantum dot film, and limit the positions of the first quantum dot and the second quantum dot by the first quantum hole and the second quantum hole, so as to ensure that the first quantum dot and the second quantum dot are set in the quantum dot film without overlapping in the light emitting direction of the display device. In this way, unnecessary interaction between the third primary color light and the first quantum dot and the second quantum dot when passing through the quantum dot film is reduced, color distortion and brightness reduction caused by spectral overlap between the first quantum dot and the second quantum dot are avoided, the light purity of the second primary color light and the third primary color light is improved, and the color accuracy of the display device is improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] In order to more clearly illustrate the implementation methods of the present application or the technical solutions in the prior art, the drawings required for use in the implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0026] Figure 1 A cross-sectional view of an embodiment of a display device provided in the present application;

[0027] Figure 2 is a cross-sectional view of a quantum dot film in the related art;

[0028] Figure 3 for Figure 1 A cross-sectional view of a first embodiment of a quantum dot film;

[0029] Figure 4 A schematic diagram of a process for manufacturing a quantum dot film provided in the present application in a first embodiment;

[0030] Figure 5A schematic diagram of a process of forming a first quantum hole and a second quantum hole in a quantum dot film according to an embodiment of the present application;

[0031] Figure 6 It is a schematic diagram of forming the first quantum hole and the second quantum hole in the first embodiment;

[0032] Figure 7 for Figure 3 A schematic diagram of the structure of an implementation method of a quantum dot film during the manufacturing process;

[0033] Figure 8 for Figure 3 A schematic structural diagram of another embodiment of a quantum dot film during the manufacturing process;

[0034] Fig. 9 It is a schematic diagram of a process of charging the first quantum dot and the second quantum dot into the first quantum hole and the second quantum hole in one embodiment under the first implementation mode;

[0035] Fig.10 It is a schematic diagram of the structure in which the first quantum dot and the second quantum dot are filled into the first quantum hole and the second quantum hole in the first implementation mode;

[0036] Fig.11 A schematic flow chart of another method for manufacturing the quantum dot film provided in the present application under the first embodiment;

[0037] Fig.12 for Figure 1 A cross-sectional view of a second embodiment of a quantum dot film;

[0038] Fig.13 A schematic flow chart of a method for manufacturing a quantum dot film provided in the present application under a second embodiment;

[0039] Fig.14 for Fig.13 Continuation of ;

[0040] Fig.15 is a schematic diagram of forming a second quantum hole in the first embodiment;

[0041] Fig.16 is a schematic diagram of forming a first quantum hole in the second embodiment;

[0042] Fig.17 for Figure 1 A cross-sectional view of a third embodiment of a quantum dot film;

[0043] Fig.18 A schematic flow chart of a method for manufacturing a quantum dot film provided in the present application in a third embodiment;

[0044] Fig.19is a schematic diagram of forming the first quantum hole and the second quantum hole in the third embodiment;

[0045] Fig. 20 for Figure 1 A cross-sectional view of a fourth embodiment of a quantum dot film;

[0046] Fig.21 A schematic flow chart of a method for manufacturing a quantum dot film provided in the present application in a fourth embodiment;

[0047] Fig. 22 FIG. 4 is a schematic diagram of forming the first quantum hole and the second quantum hole in the fourth embodiment.

[0048] Description of related technical reference numerals:

[0049] 10'-Quantum dot film;

[0050] 1'-first quantum dot, 2'-second quantum dot.

[0051] Description of the accompanying drawings in this application:

[0052] 1000-display device;

[0053] 100-optical film;

[0054] 10-Quantum dot film;

[0055] 1-substrate layer, 2-water and oxygen barrier layer, 21-first water and oxygen barrier layer, 22-second water and oxygen barrier layer, 3-sealing layer, 31-first sealing layer, 32-second sealing layer, 4-first quantum hole, 5-second quantum hole, 6-first quantum dot, 7-second quantum dot;

[0056] 20-diffusion film, 30-brightness enhancement film, 40-reflection film;

[0057] 200-backlight assembly, 210-light source, 220-light guide plate;

[0058] 300-back panel;

[0059] 400-display screen;

[0060] 2000-light shielding plate, 2000a-first light shielding plate, 2000b-second light shielding plate, 2100-exposure hole, 2100a-first exposure hole, 2100b-second exposure hole;

[0061] 3000 - photoresist layer, 3100 - first photoresist layer, 3200 - second photoresist layer;

[0062] 4000-shading layer;

[0063] 5000-first substance, 6000-second substance, 7000-third substance. DETAILED DESCRIPTION

[0064] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0065] It should be noted that when a component is said to be "fixed to" another component, it can be directly on the other component or there can be a central component. When a component is said to be "connected to" another component, it can be directly connected to the other component or there can be a central component at the same time.

[0066] Unless otherwise defined, all technical and scientific terms used in this application have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used in this application and in the specification are only for the purpose of describing specific implementations and are not intended to limit this application. The term "and / or" used in this application includes any and all combinations of one or more of the related listed items.

[0067] Some embodiments of the present application are described in detail below in conjunction with the accompanying drawings. In the absence of conflict, the following embodiments and features in the embodiments can be combined with each other.

[0068] Please refer to Figure 1 The present application proposes a display device 1000, which includes a back plate 300, a backlight assembly 200, and a display screen 400. The back plate 300 serves as a supporting frame of the display device 1000, and is used to provide support and connection for the various component assemblies of the display device 1000. The back plate 300 is formed with an installation cavity with an opening on one side, the display screen 400 is arranged at the opening, and the backlight assembly 200 is installed in the installation cavity.

[0069] The display screen 400 is used to display images or information. It receives signals from a video source (such as a computer, a TV signal receiver, a game console, etc.), converts these signals into visible images, and presents them through a screen. The display screen 400 can be a liquid crystal display screen 400 or an OLED display screen 400, and this application does not limit this.

[0070] The backlight assembly 200 is used to provide backlight for the display screen 400. The backlight assembly 200 includes a light source 210, a light guide plate 220, and an optical film 100 disposed on the light-emitting side of the light guide plate 220. The light source 210 is used to generate light. The light source 210 can be an incandescent lamp or an LED lamp, which is not limited in this application. The light provided by the light source 210 can be blue light, yellow light, or white light, which is not limited in this application.

[0071] The light guide plate 220 is used to convert the point light source 210 or line light source 210 provided by the light source 210 component into a surface light source 210, thereby improving the uniformity of light output from the display device 1000. The light guide plate 220 can be made of acrylic plate (PMMA) or polycarbonate (PC), and this application does not impose any restrictions on this.

[0072] The optical film 100 is used to improve the quality of light, and the optical film 100 includes a brightness enhancement film 30, a diffusion film 20, a reflective sheet 40, and a quantum dot film 10. The brightness enhancement film 30 is used to recycle and gather light to increase the intensity of light emitted from the backlight assembly 200. The diffusion film 20 is used to refract and diffract light to improve the uniformity of light. The reflective sheet 40 is used to reflect the light irradiated from the light source 210 and the light guide plate 220 to the back plate 300 back to the display screen 400, thereby improving the utilization rate of light by the backlight module.

[0073] The quantum dot film 10 is provided with quantum dots, which can also be called nanocrystals, and are semiconductor particles composed of II-VI or III-V elements, and the particle size of the particles is generally between 1 and 10 nm. Such semiconductor particles have a unique characteristic, that is, whenever stimulated by light or electricity, these semiconductor particles will emit light of a specific frequency, and the frequency of the light will change with the change of the size of the semiconductor.

[0074] Please refer to Figure 2 In a conventional quantum dot film 10', a first quantum dot 1' and a second quantum dot 2' are usually provided, and the diameters of the first quantum dot 1' and the second quantum dot are different. When the third primary color light of the light source is irradiated into the quantum dot film 10', the third primary color light emitted by the light source can interact with the first quantum dot 1' and the second quantum dot 2' in the quantum dot film 10', and excite the first quantum dot 1' to form the first primary color light, and excite the second quantum dot 2' to form the second primary color light. The first primary color light, the second primary color light and the third primary color light of the light source are mixed with each other to produce high-quality white light. This unique process not only significantly improves the color gamut coverage of the display, but also can restore colors more realistically, meeting users' needs for high color expression.

[0075] However, if Figure 2As shown, in the related art, the first quantum dots 1' and the second quantum dots 2' are chaotically and disorderly stacked in the quantum dot film 10'. When the third primary color light of the light source is irradiated into the quantum dot film 10', due to the disordered arrangement of the first quantum dots 1' and the second quantum dots 2', the propagation path of the light in the film becomes complicated and difficult to control. This causes the interaction between the third primary color light emitted by the light source and the first quantum dots 1' and the second quantum dots 2' in the quantum dot film 10' to become uneven and unpredictable. This uneven interaction will weaken the purity of the first primary color light and the second primary color light excited by the first quantum dots 1' and the second quantum dots 2', thereby affecting the quality of the white light finally formed by the mixture, and ultimately affecting the color accuracy of the display device.

[0076] Please refer to Figure 3 In order to solve the above problems, in the present application, the quantum dot film 10 is provided with a first quantum hole 4 and a second quantum hole 5. The first quantum hole 4 is provided with a first quantum dot 6, and the first quantum dot 6 is used to excite and form a first primary color light; the second quantum hole 5 is provided with a second quantum dot 7, and the second quantum dot 7 is used to excite and form a second primary color light. Along the thickness direction of the quantum dot film 10, the projected overlapping area of ​​the second quantum dot 7 and the first quantum dot 6 is 0.

[0077] The technical solution of the present application is to set the first quantum hole 4 and the second quantum hole 5 in the quantum dot film 10, and limit the positions of the first quantum dot 6 and the second quantum dot 7 by the first quantum hole 4 and the second quantum hole 5, so as to ensure that the first quantum dot 6 and the second quantum dot 7 are arranged in the quantum dot film 10 without overlapping in the light emitting direction of the display device. In this way, unnecessary interaction between the third primary color light and the first quantum dot 6 and the second quantum dot 7 when passing through the quantum dot film 10 is reduced, color distortion and brightness reduction caused by spectral overlap between the first quantum dot 6 and the second quantum dot 7 are avoided, the light purity of the second primary color light and the third primary color light is improved, and the color accuracy of the display device is improved.

[0078] Hereinafter, the quantum dot film provided in the present application will be described in detail with reference to the accompanying drawings.

[0079] The quantum dot film 10 has a functional layer, which serves as the main structure of the quantum dot film 10 and is used to support other structures of the quantum dot film 10 and refract light incident into the quantum dot film 10 .

[0080] The functional layer is provided with a first quantum hole 4 and a second quantum hole 5, the first quantum hole 4 is provided with a first quantum dot 6, and the second quantum hole 5 is provided with a second quantum dot 7. The first quantum dot 6 and the second quantum dot 7 are semiconductor particles composed of II-VI group or III-V group elements, and the semiconductor particles are made of ZnS and PbS as shell materials, and one or more nanomaterials composed of CdS, CdSe, CdTe, ZnSe, GaN, and InAs containing cadmium and zinc are added to the shell materials.

[0081] When the third primary color light of the light source 210 is irradiated into the quantum dot film 10, the third primary color light emitted by the light source 210 can interact with the first quantum dot 6 and the second quantum dot 7, and excite the first quantum dot 6 to form the first primary color light, and excite the second quantum dot 7 to form the second primary color light. The first primary color light, the second primary color light and the third primary color light of the light source 210 are mixed with each other to generate high-quality white light, thereby improving the color gamut coverage of the display device 1000.

[0082] It should be noted that in the above-mentioned excitation process, the third primary color light emitted by the light source 210 can be red light, green light, or blue light, and the present application does not impose specific restrictions on this. After being excited by the third primary color light, the first primary color light excited by the first quantum dot 6 and the second primary color light excited by the second quantum dot 7 can also be blue light, red light, or green light, depending on the characteristics of the quantum dot material and the excitation conditions. The present application also does not impose specific restrictions on this. In theory, as long as the quantum dot material is excited by light sources 210 of different wavelengths to produce a combination of different color lights, no matter what form these color light combinations are in (for example, a combination of red light and green light, a combination of blue light and red light, a combination of green light and blue light, etc.), as long as a specific display effect can be achieved or specific application requirements can be met, they should be within the scope of protection of the present application.

[0083] For example, in the present application, the first quantum dot 6 is a red quantum dot with a diameter between 5-6 mm, the second quantum dot 7 is a green quantum dot with a diameter between 3-4 mm, and the light source 210 is an LED blue light source 210. When the blue light of the LED light source 210 is irradiated into the functional layer, under the refraction of the functional layer, the blue light interacts with the red quantum dot to form red light, and interacts with the green quantum dot to form green light. Finally, the blue light, the red light, and the green light are mixed with each other and finally form white light, thereby improving the color gamut coverage of the display device 1000.

[0084] In this process, the first quantum hole 4 and the second quantum hole 5 provided in the functional layer can limit the position of the first quantum dot 7, so as to ensure that the first quantum dot 6 and the second quantum dot 7 are provided in the quantum dot film 10 without overlapping in the light emitting direction of the display device 1000. In this way, unnecessary interaction between the third primary color light and the first quantum dot 6 and the second quantum dot 7 when passing through the quantum dot film 10 is reduced, color distortion and brightness reduction caused by spectral overlap between the first quantum dot 6 and the second quantum dot 7 are avoided, the light purity of the second primary color light and the third primary color light is improved, and the color accuracy of the display device 1000 is improved.

[0085] In order to improve the purity of white light of the quantum dot film 10, in the first possible implementation mode of the present application, the quantum dot film 10 includes a plurality of first quantum holes 4 and a plurality of second quantum holes 5; along the thickness direction of the quantum dot film 10, the projections of the first quantum holes 4 and the projections of the second quantum holes 5 are alternately arranged in sequence along the length direction of the quantum dot film 10 and / or the width direction of the quantum dot film 10, so as to ensure that the first quantum dots 6 and the second quantum dots 7 can be evenly distributed on the quantum dot film 10, thereby ensuring that the amount of the first primary color light and the second primary color light formed by the excitation in the first quantum holes 4 and the second quantum holes 5 remains equal, thereby improving the uniformity of the mixing of the first primary color light, the second primary color light and the third primary color light, improving the purity of the white light formed by the quantum dot film 10, and improving the color accuracy of the display device 1000.

[0086] There are many structural arrangements of the functional layer. In the first embodiment of the present application, the functional layer includes a sealing layer 3, a water and oxygen barrier layer 2, and a substrate layer 1 stacked in sequence. The substrate layer 1 is made of polyethylene terephthalate (PET) or polymethyl methacrylate (PMMA) or polycarbonate (PC) or a UV-cured acrylic film with a light transmittance of ≥90% and a refractive index of ≥1.45, and its purpose is to provide support for the entire quantum dot film 10 to improve the support strength of the quantum dot film 10.

[0087] The water-oxygen barrier layer 2 is provided with a first quantum hole 4 and a second quantum hole 5, and the first quantum dot 6 and the second quantum dot 7 are provided in the water-oxygen barrier layer 2 through the first quantum hole 4 and the second quantum hole 5. The water-oxygen barrier layer 2 is used to isolate the first quantum dot 6 and the second quantum dot 7 from the influence of water vapor and oxygen in the external environment, thereby protecting the first quantum dot 6 and the second quantum dot 7 located inside it from damage. The material of the water-oxygen barrier layer 2 can be fluororesin, can be high Tg (glass transition temperature) methacrylate to epoxy resin, can be a hydrophobic coating formed by modifying polyurethane or acrylic acid, and this application does not limit this.

[0088] The sealing layer 3 is used to seal the first quantum hole 4 and the second quantum hole 5, thereby preventing external water vapor from entering the water and oxygen barrier layer 2 through the first quantum hole 4 and the second quantum hole 5, and protecting the safety of the first quantum dot 6 and the second quantum dot 7. The material of the sealing layer 3 can be epoxy resin or silicone resin, which is not limited in this application.

[0089] Please refer to Figure 4 , the present application also proposes a method for manufacturing a quantum dot film based on the first embodiment, the method for manufacturing a quantum dot film comprises the following steps;

[0090] S10a, forming a first quantum hole and a second quantum hole in the quantum dot film.

[0091] There are many ways to form the first quantum hole and the second quantum hole in the quantum dot film. Please refer to Figure 5 In one embodiment of the present application, forming the first quantum hole and the second quantum hole in the quantum dot film includes the following steps:

[0092] S101a, forming a water and oxygen barrier layer on one side of the substrate layer.

[0093] The water and oxygen barrier layer can be coated on the substrate layer, or laminated on the substrate layer by heating or pressurizing. The material of the substrate layer can be selected from at least one of polyethylene terephthalate (PET), polymethyl methacrylate (PMMA), polycarbonate (PC) or UV-cured acrylic film. The material of the water and oxygen barrier layer can be selected from at least one of hydrophobic coatings formed by modifying epoxy resin, polyurethane or acrylic acid with fluororesin, high Tg (glass transition temperature) methacrylate.

[0094] S102a, coating a photoresist layer on the side of the water and oxygen barrier layer facing away from the substrate layer.

[0095] The photoresist layer can be coated on the water and oxygen barrier layer, or laminated on the water and oxygen barrier layer by heating or pressurizing, and this application does not impose any limitation on this.

[0096] S103a, exposing, developing and etching the photoresist layer to form a first quantum hole and a second quantum hole in the water and oxygen barrier layer.

[0097] Please refer to Figure 6Before this step, a shading plate 2000 is prefabricated, and an exposure hole 2100 is provided on the shading plate 2000. The distribution positions of the exposure holes 2100 on the shading plate 2000 correspond to the distribution positions of the first quantum hole 4 and the second quantum hole 5 on the water and oxygen barrier layer 2. Subsequently, the shading plate 2000 is shielded between the photoresist layer 3000 and the exposure source for exposure operation. During exposure, the light emitted by the exposure source irradiates the photoresist layer 3000 through the exposure hole 2100 on the shading plate 2000, causing a chemical reaction in a specific area of ​​the photoresist layer 3000. After the exposure is completed, the photoresist layer 3000 is developed using an appropriate developer to remove the photoresist portion that has not undergone a chemical reaction, exposing the water and oxygen barrier layer 2. Finally, the portion of the water and oxygen barrier layer 2 protected by the photoresist layer 3000 is removed by an etching process (such as wet etching or dry etching) to form the first quantum hole 4 and the second quantum hole 5. The specific parameters of the etching process (such as etching time, etching solution concentration, etc.) should be adjusted according to the material and thickness of the water and oxygen barrier layer 2 to ensure that the size and shape of the hole meet the design requirements.

[0098] S104a, cleaning the photoresist layer.

[0099] The photoresist layer can be cleaned by spraying photoresist liquid, or removed by other chemical or mechanical methods, which is not limited in this application.

[0100] It can be understood that in other embodiments of the present application, the first quantum hole and the second quantum hole can also be directly shaped by chemical etching or 3D printing. Compared with other shaping methods, the shaping precision of the first quantum hole and the second quantum hole shaped by photolithography is higher, and the shaping depth of the first quantum hole and the second quantum hole can be adjusted according to the exposure time. At the same time, due to the presence of the light shielding layer, the exposure of the first surface and the second surface of the substrate layer can be carried out simultaneously, thereby improving the production efficiency of the quantum dot film.

[0101] S20a, filling the first quantum hole with a first quantum dot, and filling the second quantum hole with a second quantum dot.

[0102] It can be understood that for the quantum dot film structure of the first embodiment, since the openings of the first quantum hole and the second quantum hole are located on the same plane, when the first quantum dots and the second quantum dots are filled in a coating manner (i.e., the first quantum dot liquid and the second quantum dot liquid are pre-configured and coated on the surface of the water and oxygen barrier layer), the following may occur: Figure 7 As shown, the first quantum dot and the second quantum dot enter the first quantum hole at the same time. Figure 8 As shown, the first quantum dot blocks the second quantum hole, thereby causing holes to appear in the quantum dot film.

[0103] Please refer to Fig. 9 To avoid the above situation, in one possible implementation of the present application, the diameter of the first quantum dot is greater than the diameter of the second quantum dot, the aperture of the first quantum hole is greater than the aperture of the second quantum hole, the first quantum hole is filled with the first quantum dot, and the second quantum hole is filled with the second quantum dot, including the following steps:

[0104] S201a, filling the first quantum hole with a first substance.

[0105] S202a, coating the second quantum dot with a second substance, wherein the second substance and the first substance repel each other.

[0106] S203a, coating the first quantum dot and the second quantum dot on the quantum dot film, so that the first quantum hole is filled with the first quantum dot, and the second quantum hole is filled with the second quantum dot.

[0107] Please refer to Fig.10 In this embodiment, the first quantum hole 4 is filled with the first substance 5000, and the second quantum dot 7 is coated with the second substance 6000 that can repel the first substance 5000, and the first quantum dot 6 is not processed. When the first quantum liquid and the second quantum liquid are simultaneously coated on the functional layer of the quantum dot film, for the first quantum dot 6, since the diameter of the first quantum dot 6 is larger than the diameter of the second quantum hole 5, when the first quantum dot liquid is coated on the functional layer, the first quantum dot 6 can only enter the first quantum hole 4, but cannot enter the second quantum hole 5. For the second quantum dot 7, although the diameter of the first quantum dot 6 is smaller than the diameter of the first quantum hole 4, due to the presence of the first substance 5000, when the second quantum dot 7 reaches the first quantum hole 4, the second substance 6000 on the second quantum dot 7 will repel the first substance 5000 in the first quantum dot 6, and then be repelled from the first quantum hole 4. In this way, the first quantum dot 6 and the second quantum dot 7 can enter the first quantum hole 4 and the second quantum hole 5 according to the preset requirements, thereby improving the uniformity of the light of the quantum dot film.

[0108] To further improve, in one embodiment of the present application, before coating the first quantum dots and the second quantum dots on the quantum dot film, the following steps are further included:

[0109] The third substance is filled into the second quantum hole, and the third substance and the second substance attract each other.

[0110] In this embodiment, the third substance 7000 is filled into the second quantum hole 5, and the third substance 7000 and the second substance 6000 of the second quantum dot 7 attract each other. In this embodiment, the first substance 5000 is filled into the first quantum hole 4, and the second substance 6000 that can repel the first substance 5000 is coated on the second quantum dot 7, and the first quantum is not processed. When the first quantum liquid and the second quantum liquid are simultaneously coated on the functional layer of the quantum dot film, for the first quantum dot 6, since the diameter of the first quantum dot 6 is greater than the diameter of the second quantum hole 5, when the first quantum dot liquid is coated on the functional layer, the first quantum dot 6 can only enter the first quantum hole 4, but cannot enter the second quantum hole 5. For the second quantum dot 7, although the diameter of the first quantum dot 6 is smaller than the diameter of the first quantum hole 4, due to the presence of the first substance 5000, when the second quantum dot 7 reaches the first quantum hole 4, the second substance 6000 on the second quantum dot 7 will repel the first substance 5000 in the first quantum dot 6, and then be repelled from the first quantum hole 4. In this way, the first quantum dot 6 and the second quantum dot 7 can enter the first quantum hole 4 and the second quantum hole 5 according to the preset requirements, thereby improving the uniformity of the light of the quantum dot film.

[0111] To further improve, in one embodiment of the present application, before coating the first quantum dots 6 and the second quantum dots 7 on the quantum dot film, the following steps are further included:

[0112] The third substance 7000 is filled into the second quantum hole 5, and the third substance 7000 and the second substance 6000 attract each other.

[0113] In this embodiment, the third substance 7000 is filled into the second quantum hole 5, and the third substance 7000 and the second substance 6000 of the second quantum dot 7 attract each other, thereby prompting the second quantum dot 7 to flow into the second quantum hole 5 quickly, increasing the flow rate of the second quantum dot 7, and improving the coating efficiency of the second quantum dot 7 on the functional layer. At the same time, the faster flow rate of the second quantum dot 7 can also make the second quantum dot 7 reach the opening of the second quantum hole 5 faster than the first quantum dot 6 and enter the second quantum hole 5, so as to reduce the possibility of the first quantum dot 6 blocking the second quantum hole 5 and causing holes in the quantum dot film, and improve the production yield of the quantum dot film.

[0114] There are many possibilities for the first substance 5000, the second substance 6000 and the third substance 7000. In one embodiment of the present application, the first substance 5000 and the third substance 7000 are positively charged substances; the second substance 6000 is a negatively charged substance. For example, the first substance 5000 is a negatively charged non-metallic oxide or metal sulfide, which is filled into the first quantum hole 4 by coding printing. The second substance 6000 is thioglycolic acid. Before being coated on the functional layer, the second quantum dot liquid is mixed with thioglycolic acid and is negatively charged under the modification of thioglycolic acid. The third substance 7000 is a positively charged metal oxide or metal hydroxide, which is filled into the second quantum hole 5 by coding printing.

[0115] In addition to positive and negative charges, in other possible implementations of the present application, the first substance 5000, the second substance 6000 and the third substance 7000 may also be some positive and negative magnetic pole particles, or some chemical functional groups that can produce adsorption and repulsion reactions, and the present application does not impose any restrictions on this.

[0116] When the first substance 5000, the second substance 6000 and the third substance 7000 are positively charged substances, in one embodiment of the present application, the charge of the second substance 6000 is less than the charge of the third substance 7000. In this way, when the second quantum dot 7 enters the second quantum hole 5 under the attraction of the third substance 7000, the negative charge on the second quantum dot 7 will be neutralized by the positive charge of the third substance 7000, and after neutralization, the positive charge of the third substance 7000 in the second quantum hole 5 will be transferred to the second quantum dot 7, so that the surface of the second quantum dot 7 is positively charged, and then the second quantum dot 7 outside the second quantum hole 5 is continuously attracted to enter the second quantum hole 5, thereby increasing the attraction of the second quantum hole 5 to the second quantum dot 7, increasing the flow rate of the second quantum dot 7, increasing the coating efficiency of the second quantum dot 7 on the functional layer, and increasing the production yield of the quantum dot film.

[0117] Understandably, in addition to the above production steps, please refer to Fig.11 In other possible implementations of the present application, the method for manufacturing the quantum dot film may further include:

[0118] S30a, forming a sealing layer on the water and oxygen barrier layer.

[0119] The sealing layer is used to seal the first quantum hole and the second quantum hole, thereby preventing external water vapor from entering the water-oxygen barrier layer through the first quantum hole and the second quantum hole, and protecting the safety of the first quantum dot and the second quantum dot. The material of the sealing layer can be epoxy resin or silicone resin, and this application does not limit this.

[0120] In addition to the above structure, please refer to Fig.12 In the second embodiment of the present application, the functional layer includes a first sealing layer 31, a first water and oxygen barrier layer 21, a second sealing layer 32, a second water and oxygen barrier layer 22 and a substrate layer 1 stacked in sequence. In this embodiment, the material, structure and function of the sealing layer, the water and oxygen barrier layer and the substrate layer 1 are the same as those in the previous embodiment.

[0121] Different from the previous embodiment, in this embodiment, the first quantum hole 4 is arranged on the second water and oxygen barrier layer 22, and the second quantum hole 5 is arranged on the first water and oxygen barrier layer 21. It is also due to the above arrangement that in this embodiment, the first quantum dot and the second quantum dot can be filled in the first quantum hole and the second quantum hole on different planes. In this way, the difficulty of forming the quantum dot film 10 is reduced and the forming rate of the quantum dot film 10 is improved.

[0122] Please refer to Fig.13 and Fig.14 , in the second embodiment, the method for making a quantum dot film includes the following steps;

[0123] S10b, forming a second water and oxygen barrier layer on the substrate layer.

[0124] The second water and oxygen barrier layer can be coated on the substrate layer, or laminated on the substrate layer by heating or pressurizing. The material of the substrate layer can be selected from at least one of polyethylene terephthalate (PET), polymethyl methacrylate (PMMA), polycarbonate (PC) or UV-cured acrylic film. The material of the second water and oxygen barrier layer can be selected from at least one of hydrophobic coatings formed by modifying epoxy resin, polyurethane or acrylic acid with fluororesin or methacrylate with high Tg (glass transition temperature).

[0125] S20b, coating a first photoresist layer on the side of the second water and oxygen barrier layer facing away from the substrate layer.

[0126] The first photoresist layer can be coated on the second water and oxygen barrier layer, or laminated on the second water and oxygen barrier layer by heating or pressurizing, and this application does not impose any limitation on this.

[0127] S30b, exposing, developing and etching the first photoresist layer to form a first quantum hole in the second water and oxygen barrier layer.

[0128] Please refer to Fig.15Before this step begins, a first light shielding plate 2000a is prefabricated, and a first exposure hole 2100a is provided on the first light shielding plate 2000a. The distribution position of the first exposure hole 2100a on the first light shielding plate 2000a corresponds to the distribution position of the first quantum hole 4 on the second water and oxygen barrier layer 22. Subsequently, the first light shielding plate 2000a is shielded between the first photoresist layer 3100 and the exposure source to perform an exposure operation. During exposure, the light emitted by the exposure source irradiates the first photoresist layer 3100 through the first exposure hole 2100a on the first light shielding plate 2000a, causing a chemical reaction to occur in a specific area of ​​the photoresist layer. After the exposure is completed, the first photoresist layer 3100 is developed using an appropriate developer to remove the photoresist portion that has not undergone a chemical reaction, exposing the second water and oxygen barrier layer 22. Finally, the portion of the water and oxygen barrier layer protected by the photoresist layer is removed by an etching process (such as wet etching or dry etching) to form a first quantum hole 4 .

[0129] S40b, cleaning the first photoresist layer.

[0130] The first photoresist layer can be cleaned by spraying photoresist liquid, or removed by other chemical or mechanical methods, which is not limited in the present application.

[0131] S50b, filling the first quantum dot into the first quantum hole.

[0132] Before the manufacture of the quantum dot film begins, the first quantum dot liquid and the second quantum dot liquid (i.e., a mixture of the first quantum dots, the second quantum dots 7 and water or an organic solvent) are pre-configured. When the functional layer of the quantum dot film is the functional layer structure under the second embodiment, the first quantum dot liquid is coated on the second water and oxygen barrier layer, and the second quantum dot liquid is coated on the first water and oxygen barrier layer, so that the first quantum dots can be filled into the first quantum holes and the second quantum dots can be filled into the second quantum holes.

[0133] S60b, forming a second sealing layer on the side of the second water and oxygen barrier layer facing away from the substrate layer.

[0134] The second sealing layer can be coated on the second water and oxygen barrier layer, or laminated on the second water and oxygen barrier layer by heating or pressurizing. The material of the second sealing layer can be epoxy resin or silicone resin, which is not limited in this application.

[0135] S70b, forming a first water and oxygen barrier layer on the side of the second sealing layer away from the second water and oxygen barrier layer.

[0136] The first water and oxygen barrier layer can be coated on the second sealing layer, or laminated on the second sealing layer by heating or pressurizing. The material of the first water and oxygen barrier layer can be selected from at least one of fluororesin, high Tg (glass transition temperature) methacrylate to modify epoxy resin, polyurethane or acrylic acid to form a hydrophobic coating.

[0137] S80b, coating a second photoresist layer on the side of the first water and oxygen barrier layer facing away from the second sealing layer.

[0138] The photoresist layer can be coated on the first water and oxygen barrier layer, or laminated on the first water and oxygen barrier layer by heating or pressurizing, which is not limited in the present application.

[0139] S90b, exposing, developing and etching the second photoresist layer to form a second quantum hole in the first water and oxygen barrier layer.

[0140] Please refer to Fig.16 Before this step begins, a second light shielding plate 2000b is prefabricated, and a second exposure hole 2100b is provided on the second light shielding plate 2000b. The distribution position of the second exposure hole 2100b on the second light shielding plate 2000b corresponds to the distribution position of the second quantum hole 5 on the first water and oxygen barrier layer 21. Subsequently, the second light shielding plate 2000b is shielded between the second photoresist layer 3200 and the exposure source to perform an exposure operation. During exposure, the light emitted by the exposure source irradiates the second photoresist layer 3200 through the second exposure hole 2100b on the second light shielding plate 2000b, causing a chemical reaction to occur in a specific area of ​​the second photoresist layer 3200. After the exposure is completed, the photoresist layer is developed using an appropriate developer to remove the photoresist portion that has not undergone a chemical reaction, exposing the first water and oxygen barrier layer 21. Finally, the portion of the water and oxygen barrier layer protected by the photoresist layer is removed by an etching process (such as wet etching or dry etching) to form a second quantum hole 5 .

[0141] S100b, cleaning the second photoresist layer.

[0142] The second photoresist layer can be cleaned by spraying photoresist liquid, or removed by other chemical or mechanical methods, which is not limited in the present application.

[0143] S110b, forming a first sealing layer on the first water and oxygen barrier layer.

[0144] The first sealing layer can be coated on the first water and oxygen barrier layer, or laminated on the first water and oxygen barrier layer by heating or pressurizing. The material of the first sealing layer can be epoxy resin or silicone resin, which is not limited in the present application.

[0145] The functional layer also has other implementation methods. For details, please refer to Fig.17 In the third embodiment of the present application, the functional layer includes a first sealing layer 31, a water and oxygen barrier layer 2, a second sealing layer 32 and a substrate layer 1 stacked in sequence. In this embodiment, the material, structure and function of the sealing layer 3, the water and oxygen barrier layer 2 and the substrate layer 1 are the same as those in the previous embodiment.

[0146] Different from the previous embodiment, in this embodiment, the water and oxygen barrier layer 2 has a first surface and a second surface arranged opposite to each other, the opening of the first quantum hole 4 is arranged on the first surface, and the opening of the second quantum hole 5 is arranged on the second surface. In this way, the difficulty of forming the quantum dot film 10 is reduced and the forming rate of the quantum dot film 10 is improved. Compared with the second embodiment, this embodiment removes a water and oxygen barrier layer 2, reduces the thickness of the quantum dot film 10, and improves the space utilization rate of the quantum dot film 10 for the display device 1000.

[0147] Please refer to Fig.18 , in the third embodiment, the method for making a quantum dot film includes the following steps;

[0148] S10c, coating a light shielding layer on the first surface of the water and oxygen barrier layer, and forming a first photoresist layer on the side of the light shielding layer away from the first surface.

[0149] The shading layer can be coated on the first surface or laminated on the first surface by heating or pressurizing. The first photoresist layer can be coated on the shading layer or laminated on the shading layer by heating or pressurizing. This application does not impose any restrictions on this.

[0150] The material of the water and oxygen barrier layer can be selected from at least one of the hydrophobic coatings formed by modifying epoxy resin, polyurethane or acrylic acid with fluororesin, high Tg (glass transition temperature) methacrylate. The light-shielding layer can be a light-shielding tape or a light-shielding ink, which is not limited in this application.

[0151] S20c, forming a second photoresist layer on the second surface of the water and oxygen barrier layer. The second photoresist layer can be coated on the second surface, or laminated on the second surface by heating or pressurizing, which is not limited in the present application.

[0152] S30c, exposing, developing and etching the first photoresist layer and the second photoresist layer to form a first quantum hole on the first surface and a second quantum hole on the second surface.

[0153] Please refer to Fig.19Before this step, a first light shielding plate 2000a and a second light shielding plate 2000b are prefabricated. The first light shielding plate 2000a is provided with a first exposure hole 2100a, and the second light shielding plate 2000b is provided with a second exposure hole 2100b. The distribution positions of the first exposure holes 2100a on the first light shielding plate 2000a correspond to the distribution positions of the first quantum holes 4 on the first surface. The distribution positions of the second exposure holes 2100b on the second light shielding plate 2000b correspond to the distribution positions of the second quantum holes 5 on the second surface. During exposure, the light emitted by the exposure source is irradiated onto the first photoresist layer 3100 through the first exposure hole 2100a on the first light shielding plate 2000a, and is irradiated onto the second photoresist layer 3200 through the second exposure hole 2100b on the second light shielding plate 2000b. Due to the existence of the light shielding layer 4000, the light of the first photoresist layer 3100 and the second photoresist layer 3200 will not affect each other. The light of the exposure source will cause a chemical reaction to occur in specific areas of the first photoresist layer 3100 and the second photoresist layer 3200. After the exposure is completed, the first photoresist layer 3100 and the second photoresist layer 3200 are developed using an appropriate developer to remove the photoresist portion that has not undergone a chemical reaction, exposing the water-oxygen barrier layer. Finally, the portion of the water-oxygen barrier layer protected by the photoresist layer is removed by an etching process (such as wet etching or dry etching) to form a first quantum hole 4 and a second quantum hole 5 on the first surface and the second surface of the water-oxygen barrier layer, respectively.

[0154] S40c, cleaning the first photoresist layer and the second photoresist layer.

[0155] The first photoresist layer and the second photoresist layer can be cleaned by spraying photoresist liquid, or removed by other chemical or mechanical methods, which is not limited in the present application.

[0156] S50c, forming a first sealing layer on the first surface of the water and oxygen barrier layer, and forming a second sealing layer on the second surface of the water and oxygen barrier layer.

[0157] The first sealing layer can be coated on the first surface, or laminated on the first surface by heating or pressurizing. The material of the first sealing layer can be epoxy resin, or silicone resin. The second sealing layer can be coated on the second surface, or laminated on the second surface by heating or pressurizing. The material of the second sealing layer can be epoxy resin, or silicone resin, and this application does not limit this.

[0158] Please refer to Fig. 20 In the fourth embodiment of the present application, the functional layer includes a first sealing layer 31, a substrate layer 1, and a second sealing layer 32 stacked in sequence. In this embodiment, the sealing layer and the substrate layer 1 have the same material, structure, and function as the above embodiment.

[0159] Different from the previous embodiment, in this embodiment, the substrate layer 1 has a first surface and a second surface arranged opposite to each other, the opening of the first quantum hole 4 is arranged on the first surface, and the opening of the second quantum hole 5 is arranged on the second surface. Compared with the first embodiment, in this embodiment, the first quantum hole 4 and the second quantum hole 5 are arranged on two different surfaces of the water and oxygen barrier layer 2, so as to reduce the difficulty of forming the quantum dot film 10 and improve the forming rate of the quantum dot film 10. Compared with the second embodiment and the third embodiment, the present embodiment removes two water and oxygen barrier layers 2, reduces the thickness of the quantum dot film 10, and improves the space utilization rate of the quantum dot film 10 for the display device 1000.

[0160] Please refer to Fig.21 , in the fourth embodiment, the method for manufacturing the quantum dot film includes the following steps;

[0161] S10d, forming a light shielding layer on the first surface of the substrate layer, and forming a first photoresist layer on the side of the light shielding layer away from the first surface.

[0162] The light-shielding layer can be coated on the first surface or bonded to the first surface. The first photoresist layer can be coated on the light-shielding layer or laminated on the light-shielding layer by heating or pressurizing. This application does not impose any restrictions on this.

[0163] The material of the substrate layer can be selected from at least one of polyethylene terephthalate (PET), polymethyl methacrylate (PMMA), polycarbonate (PC) or UV-cured acrylic film. The light-shielding layer can be a light-shielding tape or a light-shielding ink, which is not limited in this application.

[0164] S20d, forming a second photoresist layer on the second surface of the substrate layer.

[0165] The second photoresist layer can be coated on the second surface, or laminated on the second surface by heating or pressurizing, which is not limited in the present application.

[0166] S30d, exposing, developing and etching the first photoresist layer and the second photoresist layer to form a first quantum hole on the first surface and a second quantum hole on the second surface.

[0167] Please refer to Fig. 22Before this step, a first light shielding plate 2000a and a second light shielding plate 2000b are prefabricated. The first light shielding plate 2000a is provided with a first exposure hole 2100a, and the second light shielding plate 2000b is provided with a second exposure hole 2100b. The distribution positions of the first exposure holes 2100a on the first light shielding plate 2000a correspond to the distribution positions of the first quantum holes 4 on the first surface of the substrate layer 1. The distribution positions of the second exposure holes 2100b on the second light shielding plate 2000b correspond to the distribution positions of the second quantum holes 5 on the second surface of the substrate layer 1. During exposure, the light emitted by the exposure source is irradiated onto the first photoresist layer 3100 through the first exposure hole 2100a on the first light shielding plate 2000a, and onto the second photoresist layer 3200 through the second exposure hole 2100b on the second light shielding plate 2000b. Due to the existence of the light shielding layer 4000, the light of the first photoresist layer 3100 and the second photoresist layer 3200 will not affect each other. The light of the exposure source will cause a chemical reaction to occur in specific areas of the first photoresist layer 3100 and the second photoresist layer 3200. After the exposure is completed, the first photoresist layer 3100 and the second photoresist layer 3200 are developed using an appropriate developer to remove the photoresist portion that has not undergone a chemical reaction, exposing the substrate layer 1. Finally, the portion of the substrate layer 1 protected by the photoresist layer is removed by an etching process (such as wet etching or dry etching) to form a first quantum hole 4 and a second quantum hole 5 on the first surface and the second surface of the substrate layer 1, respectively.

[0168] S40d, cleaning the first photoresist layer and the second photoresist layer.

[0169] The first photoresist layer and the second photoresist layer can be cleaned by spraying photoresist liquid, or removed by other chemical or mechanical methods, which is not limited in the present application.

[0170] S50d, forming a first sealing layer on the first surface of the substrate layer, and forming a second sealing layer on the second surface of the substrate layer.

[0171] The first sealing layer can be coated on the first surface, or laminated on the first surface by heating or pressurizing. The material of the first sealing layer can be epoxy resin, or silicone resin. The second sealing layer can be coated on the second surface, or laminated on the second surface by heating or pressurizing. The material of the second sealing layer can be epoxy resin, or silicone resin, and this application does not limit this.

[0172] In the manufacturing method of the present application, the overlapping area of ​​the first quantum dot and the second quantum dot along the thickness direction of the quantum dot film is 0. In this way, the unnecessary interaction between the third primary color light of the light source and the first quantum dot and the second quantum dot when passing through the quantum dot film is reduced, the color distortion and brightness reduction caused by the spectral overlap between the first quantum dot and the second quantum dot are avoided, the light purity of the second primary color light and the third primary color light is improved, and the color accuracy of the display device is improved.

[0173] Please refer to Figure 3 In order to further improve the uniformity of the mixing of the first primary color light, the second primary color light and the third primary color light, in one embodiment of the present application, the spacing between adjacent first quantum holes 4 and second quantum holes 5 is set to be the same, and the aperture of the first quantum hole 4 is A, the aperture of the second quantum hole 5 is B, and the spacing between each adjacent first quantum hole 4 and second quantum hole 5 is C, A>C>B. In this way, it is ensured that the amount of the third primary color light transmitted from the gap between the first quantum hole 4 and the second quantum hole 5 can be kept equal to the first primary color light and the second primary color light, thereby improving the uniformity of the mixing of the first primary color light, the second primary color light and the third primary color light, improving the purity of the white light formed by the quantum dot film 10, and improving the color accuracy of the display device 1000.

[0174] The number of quantum dots in the first quantum hole 4 and the second quantum hole 5 is also set to be the same, or it can be set to be different, and the present application does not limit this. In one possible implementation mode of the present application, the number of first quantum dots 6 in each first quantum hole 4 is N, and the number of second quantum dots 7 in each second quantum hole 5 is M, N=M. In this way, the number of quantum dots in each first quantum hole 4 and the second quantum hole 5 is ensured to remain equal, thereby ensuring that the amount of light of the first primary color light and the second primary color light formed by the excitation in the first quantum hole 4 and the second quantum hole 5 remains equal, thereby improving the uniformity of the mixing of the first primary color light, the second primary color light and the third primary color light, improving the purity of the white light formed by the quantum dot film 10, and improving the color accuracy of the display device 1000.

[0175] In the description of the implementation methods of the present application, it should be noted that the orientation or positional relationship of terms such as "center", "up", "down", "left", "right", "vertical", "horizontal", "inside" and "outside" are based on the orientation or positional relationship described in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present application.

[0176] What is disclosed above is only a preferred implementation of the present application, and it certainly cannot be used to limit the scope of rights of the present application. Ordinary technicians in this field can understand that all or part of the processes of implementing the above implementation and equivalent changes made according to the claims of the present application are still within the scope covered by the present application.

Claims

1. A quantum dot film, characterized in that: The quantum dot film is provided with a first quantum hole and a second quantum hole, the first quantum hole is provided with a first quantum dot, the first quantum dot is used for exciting to form a first primary color light; the first quantum hole is filled with a first substance; The second quantum hole is provided with a second quantum dot, which is used to excite and form a second primary color light. Along the thickness direction of the quantum dot film, the projected overlapping area of ​​the second quantum dot and the first quantum dot is 0; the second quantum dot is coated with a second substance, the second substance and the first substance repel each other, and the diameter of the first quantum dot is greater than the diameter of the second quantum hole.

2. The quantum dot film according to claim 1, characterized in that The quantum dot film includes a plurality of first quantum holes and a plurality of second quantum holes; Along the thickness direction of the quantum dot film, the projection of the first quantum hole and the projection of the second quantum hole are alternately arranged in sequence along the length direction of the quantum dot film and / or the width direction of the quantum dot film.

3. The quantum dot film according to claim 2, characterized in that: The aperture of the first quantum hole is A, the aperture of the second quantum hole is B, the distance between each adjacent first quantum hole and second quantum hole is C, and A>C>B.

4. The quantum dot film according to claim 1, characterized in that In each of the first quantum holes, the number of the first quantum dots is N, and in each of the second quantum holes, the number of the second quantum dots is M, where N=M.

5. A method for preparing a quantum dot film, characterized in that: The method for preparing the quantum dot film comprises the following steps: Forming a first quantum hole and a second quantum hole in the quantum dot film, wherein the aperture of the first quantum hole is larger than the aperture of the second quantum hole; The first quantum hole is filled with a first quantum dot, and the second quantum hole is filled with a second quantum dot, wherein the diameter of the first quantum dot is greater than the diameter of the second quantum dot; and the forming of the first quantum hole and the second quantum hole in the quantum dot film comprises: Filling the first quantum hole with a first substance; coating a second substance on the second quantum dot, wherein the second substance and the first substance repel each other; The first quantum dots and the second quantum dots are coated on the quantum dot film, so that the first quantum holes are filled with the first quantum dots and the second quantum holes are filled with the second quantum dots.

6. The method for making a quantum dot film according to claim 5, characterized in that: Before coating the first quantum dots and the second quantum dots on the quantum dot film, the method further comprises the following steps: The second quantum hole is filled with a third substance, and the third substance and the second substance attract each other.

7. The method for preparing a quantum dot film according to claim 6, characterized in that: The first substance and the third substance are positively charged substances; the second substance is negatively charged substance.

8. The method for preparing a quantum dot film according to claim 7, characterized in that: The charge amount of the second substance is smaller than the charge amount of the third substance.

9. A display device, characterized in that: Comprising the quantum dot film as described in any one of claims 1-4.

Citation Information

Patent Citations

  • Optical filter, production method thereof, display substrate and display device

    CN105204104A

  • Substrate structure for improving light emitting purity of quantum dot color film

    CN108845448A

  • Multi-layer optical construction of quantum dot films for improved conversion efficiency and color gamut

    CN110800112A

  • Color film substrate, preparation method thereof and display panel

    CN111258111A

  • Quantum dot pixelated thin film layer, preparation method thereof and full-color Micro LED display device

    CN117677214A