Aerosol generating device, preparation method thereof and aerosol generating system
By using a combination of tobacco segment and non-tobacco segment aerosol matrix in the heat-not-burn cigarette device, using the porous matrix to absorb the smoking agent and optimizing the atomization structure, the problem of glycerin smoking agent penetration is solved, and the appearance and use of the cigarette are improved. experience.
Patent Information
- Application Number
- CN202411123908.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-10-01
AI Technical Summary
The high content of glycerol smoke agent in existing heat-not-burn cigarette devices causes penetration problems, affecting the appearance quality and consumption experience of cigarettes.
Design an aerosol generating device that uses a combination of a tobacco segment aerosol matrix and a non-tobacco segment aerosol matrix. The latter contains a porous matrix to absorb high-content smoking agents, reduce the smoking agent content in the tobacco segment matrix, and pass The groove and channel structure optimizes the atomization effect.
While achieving good atomization effect, it also reduces the penetration problem of smoke-generating agent and improves the appearance quality of cigarettes and consumer experience.
Smart Images

Figure CN118716686A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of aerosol generation, and in particular to an aerosol generating device and a preparation method thereof, and an aerosol generating system. Background Art
[0002] An aerosol generator is a device that can convert liquid or solid substances into aerosols. Heat-not-burn cigarettes are a special type of aerosol generator. The heating temperature of heat-not-burn cigarettes is usually 200℃~400℃, which is much lower than the combustion temperature of traditional cigarettes. The harmful components produced by heating are greatly reduced, so they have been rapidly developed. In order to simulate the "smoking" effect of traditional cigarettes, it is necessary to add a smoke-generating agent to the aerosol matrix of the non-tobacco segment of the heated cigarette.
[0003] Commonly used smoke-generating agents are glycerin or mixed solvents containing glycerin, and their mass content is usually 20% to 40%. In order to pursue a stronger smoking effect, the glycerin content will be higher. The high content of glycerin in the aerosol matrix of heat-not-burn cigarettes will penetrate to the outside of the wrapping material layer, resulting in patches of spots, which seriously affects the appearance quality of the cigarettes and the consumer experience.
[0004] Therefore, it is necessary to improve the traditional technology so as to reduce the problem of smoke agent penetration while obtaining a good atomization effect. Summary of the invention
[0005] Based on this, it is necessary to provide an aerosol generating device and a preparation method thereof and an aerosol generating system, which can reduce the problem of smoke agent penetration while achieving a good atomization effect.
[0006] In a first aspect of the present application, an aerosol generating device is provided, comprising a wrapping material layer, a filter body, a hollow device and an aerosol matrix; the wrapping material layer is wrapped around the outer sides of the filter body, the hollow device and the aerosol matrix which are connected in sequence; the aerosol matrix comprises a tobacco segment aerosol matrix and a non-tobacco segment aerosol matrix, the non-tobacco segment aerosol matrix comprises a porous matrix and a smoke generating agent, and the smoke generating agent is adsorbed in the porous matrix.
[0007] Thus, the above-mentioned aerosol generating device, its aerosol matrix includes a tobacco segment aerosol matrix and a non-tobacco segment aerosol matrix, wherein the tobacco segment aerosol matrix can provide tobacco satisfaction as a tobacco functional segment, and the non-tobacco segment aerosol matrix can adsorb a higher content of smoke-generating agent due to its porous matrix structure, and can be used as the main smoke-generating functional area, so that the content of smoke-generating agent in the tobacco segment aerosol matrix can be reduced, and its smoke-generating agent penetration problem can be reduced. In this way, the tobacco segment aerosol matrix and the non-tobacco segment aerosol matrix give full play to their respective advantages, and can reduce penetration problems while obtaining a good atomization effect, thereby improving the appearance quality of cigarettes and consumers' experience.
[0008] In some embodiments, the non-tobacco segment aerosol matrix is located at one end of the tobacco segment aerosol matrix close to the hollow device. Compared with the structure in which the non-tobacco segment aerosol matrix is located at one end of the tobacco segment aerosol matrix away from the hollow device, the non-tobacco segment aerosol matrix is located at one end of the tobacco segment aerosol matrix close to the hollow device, so that the non-tobacco segment aerosol matrix is closer to the filter body and the utilization rate of the atomizer is higher; in addition, the tobacco segment aerosol matrix is located on the outside, which is convenient for the heating component to act on the tobacco segment aerosol matrix to achieve heating. Compared with the heating component acting on the non-tobacco segment aerosol matrix to achieve heating, it is cleaner when used and easier to adjust the product design.
[0009] In some of the embodiments, the side wall of the non-tobacco segment aerosol substrate is provided with a groove, and the groove runs from one end of the non-tobacco segment aerosol substrate close to the hollow device to the other end, and a channel is formed between the area where the side wall of the non-tobacco segment aerosol substrate is provided with the groove and the wrapping material layer.
[0010] In this way, the side wall of the non-tobacco segment aerosol matrix is provided with a penetrating groove, and a channel is formed between the area where the side wall of the non-tobacco segment aerosol matrix is provided with the groove and the wrapping material layer. When the non-tobacco segment aerosol matrix is heated and atomized, the smoke formed by the atomization of the non-tobacco segment aerosol matrix near the central area is more likely to diffuse toward the groove of the side wall. At the same time, the penetrating channel also facilitates the transmission of the smoke formed by atomization, thereby improving the smoke release efficiency and obtaining a good atomization effect.
[0011] In some of the embodiments, the area of the side wall of the non-tobacco segment aerosol substrate where the groove is provided accounts for 1 / 5 to 4 / 5 of the total area of the side wall of the non-tobacco segment aerosol substrate.
[0012] In some of the embodiments, the area of the side wall of the non-tobacco segment aerosol substrate where the groove is provided accounts for 1 / 4 to 3 / 4 of the total area of the side wall of the non-tobacco segment aerosol substrate.
[0013] In some of the embodiments, the area of the side wall of the non-tobacco segment aerosol substrate where the groove is provided accounts for 1 / 3 to 2 / 3 of the total area of the side wall of the non-tobacco segment aerosol substrate.
[0014] In some of the embodiments, the area of the side wall of the non-tobacco segment aerosol substrate not provided with the groove is in contact with the wrapping material layer.
[0015] In some of the embodiments, the non-tobacco aerosol matrix is a cylindrical structure, and the total arc length of the side wall of the non-tobacco aerosol matrix in contact with the wrapping material layer accounts for 1 / 5 to 4 / 5 of the total inner circumference of the wrapping material layer.
[0016] In some embodiments, the cross-sectional shape of the groove is fan-shaped, polygonal or irregular.
[0017] In some of the embodiments, the number of the grooves on the side wall of the non-tobacco segment aerosol substrate is 1 to 50.
[0018] In some of the embodiments, on the radial cross section of the non-tobacco segment aerosol matrix, the total area of the hollow region including the groove accounts for 5% to 40% of the inner cross section formed by the wrapping material layer.
[0019] In some of the embodiments, the interior of the non-tobacco segment aerosol matrix is provided with a channel extending from one end close to the hollow device to the other end.
[0020] In some embodiments, the number of the channels is 1 to 10.
[0021] In some of the embodiments, the cross-sectional shape of the channel is circular, elliptical, fan-shaped, polygonal or irregular.
[0022] In some of the embodiments, based on the volume of the non-tobacco segment aerosol matrix, the total volume of the grooves and the pores accounts for 5% to 40%.
[0023] In some embodiments, one or more of the following conditions are met:
[0024] (1) In the direction in which the hollow device extends toward the aerosol matrix, the length of the non-tobacco segment aerosol matrix is 2 mm to 15 mm;
[0025] (2) In the direction in which the hollow device extends toward the aerosol matrix, the length of the tobacco segment aerosol matrix is 5 mm to 35 mm.
[0026] In some of the embodiments, both the non-tobacco segment aerosol matrix and the tobacco segment aerosol matrix are adsorbed with smoking agent.
[0027] In some embodiments, one or more of the following conditions are met:
[0028] (1) The porous matrix is a porous granular material matrix, and the smoke generating agent is adsorbed in the porous granular material matrix;
[0029] (2) The smoking agent in the non-tobacco segment aerosol matrix and the tobacco segment aerosol matrix both comprises at least one of glycerin, propylene glycol, ethylene glycol, xylitol and erythritol;
[0030] (3) Based on the total mass of the smoke-generating agent in the non-tobacco segment aerosol matrix and the tobacco segment aerosol matrix, the mass proportion of the smoke-generating agent in the non-tobacco segment aerosol matrix is 40% to 65%.
[0031] The porous particle material matrix is different from the traditional non-tobacco aerosol matrix made of plant fiber materials. Since the porous particle material matrix is a porous particle material, it can adsorb a higher content of smoke-generating agents without external leakage, thereby reducing the penetration of smoke-generating agents such as glycerin.
[0032] In some embodiments, one or more of the following conditions are met:
[0033] (1) The porous granular material of the porous granular material matrix includes at least one of natural porous mineral materials, metal oxides, hydroxides, carbonates, sulfates, activated carbon and molecular sieves;
[0034] (2) The average particle size of the porous granular material of the porous granular material matrix is between 200 μm and 600 μm;
[0035] (3) The smoking agent in the non-tobacco segment aerosol matrix and the tobacco segment aerosol matrix both include glycerin;
[0036] (4) The mass of the smoke generating agent in the non-tobacco aerosol matrix is 20 mg to 50 mg per cigarette;
[0037] (5) The mass of the smoke generating agent in the tobacco segment aerosol matrix is 30 mg to 40 mg per cigarette.
[0038] In some embodiments, one or more of the following conditions are met:
[0039] (1) The natural porous mineral material includes at least one of diatomaceous earth, montmorillonite, sepiolite and kaolin;
[0040] (2) The tobacco segment aerosol matrix also includes one or more of tobacco leaves, tobacco shreds, tobacco stem shreds, tobacco flakes, tobacco particles and tobacco extracts.
[0041] The second aspect of the present application further provides a method for preparing the aerosol generating device provided in the first aspect of the present application, comprising the following steps:
[0042] The filter body, the hollow device, the non-tobacco segment aerosol matrix and the tobacco segment aerosol matrix are arranged in sequence, and the wrapping material layer is used to wrap the outer sides of the filter body, the hollow device, the non-tobacco segment aerosol matrix and the tobacco segment aerosol matrix connected in sequence to obtain an aerosol generating device.
[0043] In some of these embodiments, the step of preparing the non-tobacco segment aerosol matrix is also included;
[0044] The preparation of the non-tobacco segment aerosol matrix comprises the following steps: allowing the porous material to absorb the smoke agent; granulating the porous material absorbed with the smoke agent; extruding the porous granular material obtained by granulation to obtain the non-tobacco segment aerosol matrix; or,
[0045] The preparation of the non-tobacco segment aerosol matrix comprises the following steps: granulating a porous material to obtain a porous granular material; allowing the porous granular material to adsorb a smoke generating agent, and extruding the porous granular material adsorbing the smoke generating agent to obtain the non-tobacco segment aerosol matrix.
[0046] In a third aspect of the present application, an aerosol generating system is provided, comprising the aerosol generating device provided in the first aspect of the present application and a heating device for heating the aerosol generating device.
[0047] In some embodiments, the heating device includes a heating component, a battery component, a control component and a shell, the battery component is a battery component for powering the heating device, the control component is used to control the battery component, and the heating component, the battery component and the control component are housed in the shell. BRIEF DESCRIPTION OF THE DRAWINGS
[0048] FIG1 is a schematic cross-sectional view of an aerosol generating device according to an embodiment of the present application;
[0049] FIG2 is a schematic diagram of a radial cross-sectional structure of an exemplary non-tobacco segment aerosol substrate in an aerosol generating device according to an embodiment of the present application;
[0050] Figure 3 This is a schematic diagram of the radial cross-sectional structure of another exemplary non-tobacco segment aerosol substrate in the aerosol generating device according to one embodiment of the present application;
[0051] Figure 4 This is a schematic cross-sectional structure diagram of an aerosol generating device according to another embodiment of the present application.
[0052] Description of reference numerals:
[0053] 10. filter body; 20. hollow device; 30. aerosol matrix; 31. tobacco segment aerosol matrix; 32. non-tobacco segment aerosol matrix; 321. groove; 322. channel; 40. wrapping material layer. DETAILED DESCRIPTION
[0054] In order to facilitate the understanding of the present invention, the present invention will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present invention are given in the drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. It should be understood that the purpose of providing these embodiments is to make the understanding of the disclosure of the present invention more thorough and comprehensive.
[0055] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which the present invention belongs. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more of the related listed items.
[0056] In the description of the present invention, it should be understood that the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0057] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.
[0058] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0059] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0060] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" or "below" a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.
[0061] The terms "vertical", "horizontal", "upper", "lower", "left", "right" and similar expressions used herein are for illustrative purposes only and do not represent the only implementations.
[0062] It should be noted that when an element is referred to as being "fixed to" another element, it may be directly on the other element or there may be an intermediate element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be an intermediate element at the same time.
[0063] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which the present invention belongs. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more of the related listed items.
[0064] As described in the background technology, increasing the content of the smoke agent can improve the atomization effect, but it will increase the problem of smoke agent penetration. In order to reduce the penetration phenomenon, one technology is to add an anti-permeation layer to the wrapping material layer, but it increases the cost. Based on this, the present application provides an aerosol generating device, which can reduce the problem of smoke agent penetration while achieving a good atomization effect, and improve the appearance quality of aerosol generating devices such as cigarettes and the consumer experience.
[0065] Please refer to Figures 1 and 2. An embodiment of the present application provides an aerosol generating device, including a filter body 10, a hollow device 20, an aerosol matrix 30 and a wrapping material layer 40; the wrapping material layer 40 is wrapped around the outer sides of the filter body 10, the hollow device 20 and the aerosol matrix 30 which are connected in sequence.
[0066] The aerosol matrix 30 includes a tobacco-segment aerosol matrix 31 and a non-tobacco-segment aerosol matrix 32. The non-tobacco-segment aerosol matrix 32 includes a porous matrix and a smoke generating agent, wherein the smoke generating agent is adsorbed in the porous matrix.
[0067] Thus, the above-mentioned aerosol generating device, its aerosol matrix 30 includes a tobacco segment aerosol matrix 31 and a non-tobacco segment aerosol matrix 32, wherein the tobacco segment aerosol matrix 31 can provide tobacco satisfaction as a tobacco functional segment, and the non-tobacco segment aerosol matrix 32 can be used as the main smoking functional area because of its porous matrix structure that can adsorb a higher content of smoke-generating agent, thereby reducing the content of smoke-generating agent in the tobacco segment aerosol matrix 31 and reducing its smoke-generating agent penetration problem. In this way, the tobacco segment aerosol matrix 31 and the non-tobacco segment aerosol matrix 32 give full play to their respective advantages, and can reduce penetration problems while obtaining a good atomization effect, thereby improving the appearance quality of aerosol generating devices such as cigarettes and the consumer experience.
[0068] In some of the embodiments, the non-tobacco segment aerosol matrix 32 is located at one end of the tobacco segment aerosol matrix 31 close to the hollow device 20. In other embodiments, the non-tobacco segment aerosol matrix 32 may also be located at one end of the tobacco segment aerosol matrix 31 away from the hollow device 20. In other words, the non-tobacco segment aerosol matrix 32 and the tobacco segment aerosol matrix 31 may be sequentially arranged in any order in the extension direction from the filter 10 to the hollow device 20.
[0069] Compared with the structure in which the non-tobacco segment aerosol matrix 32 can also be located at the end of the tobacco segment aerosol matrix 31 away from the hollow device 20, the non-tobacco segment aerosol matrix 32 is located at the end of the tobacco segment aerosol matrix 31 close to the hollow device 20, so that the non-tobacco segment aerosol matrix is closer to the filter body and the utilization rate of the atomizer is higher; in addition, the tobacco segment aerosol matrix is located on the outside, which is convenient for the heating component to act on the tobacco segment aerosol matrix to achieve heating. Compared with the heating component acting on the non-tobacco segment aerosol matrix to achieve heating, it is cleaner to use and easier to adjust the product design.
[0070] In some of the embodiments, the side wall of the non-tobacco segment aerosol matrix 32 is provided with a groove 321, and the groove 321 runs from one end of the non-tobacco segment aerosol matrix 32 close to the hollow device 20 to the other end, and a channel is formed between the area where the groove 321 is provided on the side wall of the non-tobacco segment aerosol matrix 32 and the wrapping material layer 40.
[0071] In this way, the above-mentioned aerosol generating device has a side wall of the non-tobacco section aerosol matrix 32 provided with a penetrating groove 321, and a channel is formed between the area where the side wall of the non-tobacco section aerosol matrix 32 is provided with the groove 321 and the wrapping material layer 40. When the non-tobacco section aerosol matrix 32 is heated and atomized, the smoke formed by the atomization of the non-tobacco section aerosol matrix 32 near the central area is more likely to diffuse toward the groove 321 of the side wall. At the same time, the penetrating channel also facilitates the transmission of the smoke formed by atomization, thereby improving the smoke release efficiency and obtaining a good atomization effect.
[0072] In addition, because it can achieve high atomization release efficiency, in some examples, the usage of the non-tobacco segment aerosol matrix 32 can be reduced, thereby reducing penetration problems and improving the appearance quality of aerosol generating devices such as cigarettes and the consumer experience.
[0073] When the non-tobacco aerosol matrix 32 is located at one end of the tobacco aerosol matrix 31 close to the hollow device 20, the hollow device 20 further has a hollow portion, and the channel formed between the area where the groove 321 is provided on the side wall of the non-tobacco aerosol matrix 32 and the wrapping material layer 40 is connected to the hollow portion. In this way, smoke can be transmitted from the channel to the hollow portion of the hollow device 20 very quickly, thereby improving smoke release efficiency.
[0074] In some of the embodiments, the area of the region where the groove 321 is provided on the side wall of the non-tobacco segment aerosol matrix 32 accounts for 1 / 5 to 4 / 5 of the total area of the side wall of the non-tobacco segment aerosol matrix 32; as an example, the area ratio can be 1 / 5, 1 / 4, 30%, 1 / 3, 35%, 2 / 5, 1 / 2, 55%, 60%, 2 / 3, 70%, 3 / 4, 4 / 5, or within the range formed by any two of the above point values.
[0075] It can be understood that the total side wall area of the non-tobacco segment aerosol matrix 32 refers to the side wall area of the non-tobacco segment aerosol matrix 32 without the groove 321; taking the cylindrical structure of the non-tobacco segment aerosol matrix 32 as an example in the following text, the total side wall area of the non-tobacco segment aerosol matrix 32 is based on the side wall area of the non-tobacco segment aerosol matrix 32 as a whole presenting a cylindrical structure.
[0076] Furthermore, the area of the side wall of the non-tobacco segment aerosol substrate 32 where the groove 321 is provided accounts for 1 / 4 to 3 / 4 of the total area of the side wall of the non-tobacco segment aerosol substrate 32 .
[0077] Furthermore, the area of the side wall of the non-tobacco segment aerosol substrate 32 where the groove 321 is provided accounts for 1 / 3 to 2 / 3 of the total area of the side wall of the non-tobacco segment aerosol substrate 32 .
[0078] In some embodiments, the area of the side wall of the non-tobacco aerosol matrix 32 where the groove 321 is not provided contacts the wrapping material layer 40. In this way, the area where the side wall of the non-tobacco aerosol matrix 32 contacts the wrapping material layer 40 can ensure the heating efficiency of the heating device for heating the aerosol generating device, so as to promote the non-tobacco aerosol matrix 32 to be heated and atomized, thereby producing an atomization effect.
[0079] In some embodiments, the non-tobacco aerosol matrix 32 is a cylindrical structure. Further, the filter 10 and the hollow device 20 are also cylindrical structures, and the wrapping material layer 40 is surrounded to form a cylindrical structure, which is wrapped around the outer side of the filter 10, the hollow device 20, and the non-tobacco aerosol matrix 32 of the cylindrical structure.
[0080] Furthermore, the non-tobacco aerosol matrix 32 is a cylindrical structure, and the groove 321 runs from one end of the non-tobacco aerosol matrix 32 close to the hollow device 20 to the other end; that is, the groove 321 runs from one axial end of the non-tobacco aerosol matrix 32 to the other end.
[0081] Further, the cross-sectional shapes of any two locations of the groove 321 extending from one axial end to the other end of the non-tobacco segment aerosol substrate 32 may be the same or different. In a specific example, the cross-sectional shapes of any two locations of the groove 321 extending from one axial end to the other end of the non-tobacco segment aerosol substrate 32 are the same, and further, the cross-sectional shapes are not only the same but also overlap each other.
[0082] Further, the total arc length of the side wall of the non-tobacco segment aerosol matrix 32 in contact with the wrapping material layer 40 accounts for 1 / 5 to 4 / 5 of the total inner circumference of the wrapping material layer 40; as an example, the proportion can be 1 / 5, 1 / 4, 30%, 1 / 3, 35%, 2 / 5, 1 / 2, 55%, 60%, 2 / 3, 70%, 3 / 4, 4 / 5, or within the range of any two of the above point values. Further, the proportion can be 1 / 4 to 3 / 4, and further 1 / 3 to 2 / 3. Please continue to refer to Figure 2, the total inner circumference of the wrapping material layer 40 is the same as the outer circumference of the non-tobacco segment aerosol matrix 32 (the outermost solid line and dotted line The ring formed by the circle); the total arc length of the side wall of the non-tobacco segment aerosol matrix 32 in contact with the wrapping material layer 40 is the total length of the outer solid line area in Figure 2.
[0083] In some embodiments, the cross-sectional shape of the groove 321 is fan-shaped, polygonal or irregular.
[0084] Further, the sector shape includes a semicircle, a sector shape smaller than 180°, or a sector shape larger than 180°; the following is similar.
[0085] Furthermore, polygons include but are not limited to triangles, quadrilaterals, pentagons or hexagons, etc. Quadrilaterals include but are not limited to squares, rectangles, trapezoids, parallelograms, etc. In the example shown in FIG2 , the cross-sectional shape of the groove 321 is a triangle.
[0086] In some of the embodiments, the number of the grooves 321 on the side wall of the non-tobacco segment aerosol substrate 32 is at least one, for example, 1 to 50, and can be optionally 3 to 30; further, it can be optionally 4 to 20, or it can be in the range of any two integers from 1 to 50.
[0087] In some of the embodiments, on any radial cross section of the non-tobacco segment aerosol matrix 32, the total area of the hollow area including the groove 321 accounts for 5% to 40% of the inner cross section formed by the wrapping material layer 40. As an example, the area proportion of the channel 322 can be 5%, 8%, 10%, 15%, 20%, 25%, 30%, 35%, 40%, or within the range formed by any two of the above point values as end values. Further, the area proportion can be 10% to 30%, and is optimized to be 15% to 25%.
[0088] In some of the embodiments, the non-tobacco aerosol matrix 32 is provided with a hole 322 near one end of the hollow device 20 and through the other end. The hole 322 can also be used for the transmission of smoke formed by atomization. The smoke-generating agent in the non-tobacco aerosol matrix 32 can diffuse to the outer groove 321 or to the inner hole 322, thereby improving the smoke release efficiency and obtaining a good atomization effect. The setting of the hole 322 is also conducive to reducing the adsorption of the aerosol released by the tobacco aerosol matrix; on the other hand, in some examples, the hole 322 can be conducive to the operation of central heating, avoiding the heating needle or heating plate of the central heating from hitting the non-tobacco aerosol matrix.
[0089] Further, the number of the channels 322 inside the non-tobacco segment aerosol matrix 32 is at least one, for example, 1 to 10, for example, 1 to 3. Further, at least one channel 322 is located at the axis of the non-tobacco segment aerosol matrix 32.
[0090] In some embodiments, the cross-sectional shape of the channel 322 is circular, elliptical, fan-shaped, polygonal or irregular. Further, the polygon includes but is not limited to a triangle, a quadrilateral, a pentagon or a hexagon, etc. The quadrilateral includes but is not limited to a square, a rectangle, a trapezoid, a parallelogram, etc.
[0091] In some of the embodiments, on the radial cross section of the non-tobacco aerosol matrix 32, the total area of the groove 321 and the channel 322 accounts for 5% to 40% of the inner cross section formed by the wrapping material layer 40; as an example, the area proportion of the channel 322 can be 5%, 8%, 10%, 15%, 20%, 25%, 30%, 35%, 40%, or a range formed by any two of the above point values as end values. Further, the area proportion can be 10% to 30%, and is optimized to be 15% to 25%.
[0092] In some of the embodiments, based on the volume of the non-tobacco segment aerosol matrix 32, the total volume of the groove 321 and the pore 322 accounts for 5% to 40%; as an example, the total volume of the groove 321 and the pore 322 can be 5%, 8%, 10%, 15%, 20%, 25%, 30%, 35%, 40%, or within the range of any two of the above point values as end values. Further, the volume share can be 30% to 40%. Further, the volume share of the pore 322 is 2% to 20%, and the rest is the volume share of the groove 321. As an example, the volume share of the pore 322 is 2%, 3%, 5%, 8%, 10%, 12%, 15%, 18%, 20%, or within the range of any two of the above point values as end values.
[0093] See also Figure 3 In other embodiments, the non-tobacco segment aerosol matrix 32 has no pores 322 disposed therein, and is a solid structure from a macroscopic perspective.
[0094] In some embodiments, in the direction in which the hollow device 20 extends toward the aerosol substrate 30, the length of the non-tobacco segment aerosol substrate 32 is 2 mm to 15 mm; as an example, it can be 2 mm, 3 mm, 5 mm, 8 mm, 10 mm, 12 mm, 15 mm, or within the range formed by any two of the above point values as end values. Further, it can be 3 mm to 12 mm; preferably 5 mm to 10 mm.
[0095] In some of the embodiments, in the direction in which the hollow device 20 extends toward the aerosol matrix 30, the length of the tobacco segment aerosol matrix 31 is 5 mm to 35 mm; as an example, it can be 5 mm, 8 mm, 10 mm, 15 mm, 20 mm, 25 mm, 30 mm, 35 mm, or within the range formed by any two of the above point values as end values.
[0096] In some embodiments, smoke generating agent is adsorbed in both the tobacco segment aerosol matrix 31 and the non-tobacco segment aerosol matrix 32. The smoke generating agent is used to generate an atomization effect when heated.
[0097] Traditional aerosol matrices are all based on plant fibers. Plant fibers include but are not limited to tobacco, wood pulp and other plant fibers. However, these plant fibers have low saturated adsorption capacity for smoke-generating agents such as glycerin. For example, when the mass content of glycerin exceeds 20%, the surface of the aerosol matrix will become moist, which can easily lead to penetration and agglomeration. For heat-not-burn cigarettes, taking the smoke-generating agent glycerin as an example, glycerin can be evaporated and released above 150°C, but due to the poor thermal conductivity of the aerosol matrix made of plant fiber material, the central heating type heating component is usually set at a temperature of about 350°C, and the circumferential heating type heating component is set at a temperature of about 250°C. Usually, only the heated material close to the heat source can be heated to a temperature close to the set temperature, while the temperature of the heated material in most areas is far below the set temperature range. Therefore, the efficiency of glycerin release atomization is actually not high. Glycerin released by heat in the high-temperature area will be adsorbed and absorbed by the aerosol matrix in the low-temperature area, which also reduces the efficiency of glycerin release atomization. In addition, excessively high heating temperatures will cause glycerin to pyrolyze and produce harmful substances such as acetaldehyde and acrolein. Therefore, the present application further improves the structure of the non-tobacco segment aerosol matrix 32 .
[0098] In some embodiments, the tobacco segment aerosol matrix 31 is based on plant fibers as carriers and can be prepared using known processes. Plant fibers include but are not limited to tobacco, wood pulp and other plant fibers. Further, in addition to the smoke-generating agent, the tobacco segment aerosol matrix 31 also includes one or more of tobacco leaves, tobacco shreds, tobacco stem shreds, tobacco flakes, tobacco particles and tobacco extracts. Further, the tobacco segment aerosol matrix 31 also includes flavoring agents, which include but are not limited to one or more of coffee flavor, mint flavor, orange flavor, strawberry flavor, cantaloupe flavor and mango flavor. Further, the tobacco segment aerosol matrix 31 and the inner wall of the wrapping material layer 40 are mutually attached. Further, the tobacco segment aerosol matrix 31 is a cylindrical structure.
[0099] In some of the embodiments, the smoke-generating agent in the non-tobacco segment aerosol matrix 32 is adsorbed in the porous material in the porous granular material matrix. Further, the porous material is a porous granular material. In some of the embodiments, the porous matrix in the non-tobacco segment aerosol matrix 32 is a porous granular material matrix, and the smoke-generating agent is adsorbed in the porous granular material matrix. The porous granular material matrix is different from the traditional aerosol matrix of plant fiber material. Since the porous granular material matrix is a porous granular material, it can adsorb a higher content of smoke-generating agent without extravasation, thereby reducing the penetration problem of smoke-generating agents such as glycerin. Furthermore, the above-mentioned non-tobacco segment aerosol matrix 32 using a porous granular material matrix, combined with the groove 321 structural design of the non-tobacco segment aerosol matrix 32, is conducive to the atomization release efficiency of the smoke-generating agent with a high adsorption amount.
[0100] Furthermore, the porous particle material matrix is a heat-conducting material. The good heat-conducting property of the porous particle material matrix can improve the heat conduction of the non-tobacco aerosol matrix 32, improve its heating uniformity, and improve the atomization release efficiency of the smoking agent such as glycerin.
[0101] Further, the porous granular material of the porous granular material matrix includes at least one of natural porous mineral materials, metal oxides, hydroxides, carbonates, sulfates, activated carbon and molecular sieves. Further, the natural porous mineral material includes at least one of diatomaceous earth, montmorillonite, sepiolite and kaolin.
[0102] Furthermore, the average particle size of the porous granular material is between 200 μm and 600 μm; as an example, it may be 200 μm, 300 μm, 400 μm, 500 μm, 600 μm, or within a range consisting of any two of the above point values as end values.
[0103] Further, the smoke generating agent in the tobacco segment aerosol matrix 31 and the non-tobacco segment aerosol matrix 32 includes at least one of glycerin, propylene glycol, ethylene glycol, xylitol and erythritol. Further, the smoke generating agent in the tobacco segment aerosol matrix 31 and the non-tobacco segment aerosol matrix 32 both includes glycerin; further, it may also include at least one of propylene glycol, ethylene glycol, xylitol and erythritol, such as propylene glycol.
[0104] In some of the embodiments, based on the total mass of the smoke-generating agent in the non-tobacco aerosol matrix 32 and the tobacco aerosol matrix 31, the mass proportion of the smoke-generating agent in the non-tobacco aerosol matrix 32 is 40% to 65%; as an example, it can be 40%, 42%, 45%, 48%, 50%, 52%, 55%, 60%, 62.5%, 65%, or within the range formed by any two of the above point values as end values. Optionally, the mass proportion can be 50% to 60% or 60% to 65%. Within this range, when the total amount of smoke-generating agent added is the same, the release amount and release efficiency of the smoke-generating agent are both high.
[0105] In some of the embodiments, the mass of glycerin in the non-tobacco segment aerosol matrix 32 is 20 mg / stick to 50 mg / stick; as an example, it can be 20 mg / stick, 25 mg / stick, 30 mg / stick, 35 mg / stick, 40 mg / stick, 45 mg / stick, 50 mg / stick, or within the range consisting of any two of the above point values as end values.
[0106] In some of the embodiments, the mass of glycerin in the tobacco segment aerosol matrix 31 is 30 mg / stick to 40 mg / stick. As an example, it can be 30 mg / stick, 35 mg / stick, 40 mg / stick, or within the range consisting of any two of the above point values as end values.
[0107] In some of these embodiments, the non-tobacco segment aerosol matrix 32 may also include one or more of green tea extract, black tea extract, coffee flavor, mint flavor, orange flavor, strawberry flavor, cantaloupe flavor, and mango flavor.
[0108] In some embodiments, there may be a distance between the tobacco segment aerosol matrix 31 and the non-tobacco segment aerosol matrix 32, as shown in FIG. 1 ; or they may be directly connected, that is, without a distance; Figure 4 There is a certain distance between the two mainly to avoid the influence of the high content of atomizer in the aerosol matrix of the non-tobacco segment on the tobacco segment.
[0109] Furthermore, the spacing length is 2 mm to 5 mm.
[0110] An embodiment of the present application provides a method for preparing any of the above-mentioned aerosol generating devices, comprising the following steps:
[0111] The filter body 10, the hollow device 20, the non-tobacco segment aerosol matrix 32 and the tobacco segment aerosol matrix 31 are arranged in sequence, and a wrapping material layer 40 is used to wrap the outer sides of the filter body 10, the hollow device 20, the non-tobacco segment aerosol matrix 32 and the tobacco segment aerosol matrix 31 connected in sequence to obtain an aerosol generating device.
[0112] In some of the embodiments, the preparation of the non-tobacco segment aerosol matrix 32 comprises the following steps:
[0113] The porous material is made to absorb the smoke generating agent, and then the porous material absorbed with the smoke generating agent is extruded to obtain the non-tobacco segment aerosol matrix 32 .
[0114] The preparation method of the above-mentioned non-tobacco segment aerosol matrix 32 is to make the porous material absorb the smoke agent first, and then extrude and mold it into a porous material matrix, so that the smoke agent is absorbed in the porous material in the porous material matrix, so that the non-tobacco segment aerosol matrix 32 can absorb more smoke agent and is not easy to leak.
[0115] Understandably, in the process of extruding the porous material adsorbed with the smoke-generating agent, an adhesive may be added or not added according to the viscosity requirements of the porous material. Some porous materials are sticky in themselves, so no adhesive is needed; while some porous materials have low viscosity, adhesives can be added to improve viscosity and facilitate molding. Further, the adhesive includes at least one of gum, cellulose adhesive, polysaccharide, organic acid and conjugate alkali salt of organic acid, including but not limited to at least one of carboxymethyl cellulose, sodium carboxymethyl cellulose, chitosan, starch, modified starch, polyacrylic acid, and sodium silicate. Among them, the most commonly used adhesive is carboxymethyl cellulose (sodium), with an amount of 0.5wt%~2wt%, based on the weight of the porous material adsorbed with the smoke-generating agent; as an example, the amount ratio of the adhesive can be 0.5wt%, 0.8wt%, 1wt%, 1.2wt%, 1.5wt%, 2wt%, or within the range of any two of the above point values.
[0116] In some of the embodiments, the preparation of the non-tobacco segment aerosol matrix 32 includes the following steps: allowing the porous material to adsorb the smoke-generating agent; then granulating the porous material adsorbing the smoke-generating agent; and extruding the porous granular material obtained by granulation to obtain the non-tobacco segment aerosol matrix 32.
[0117] Furthermore, the porous material can be made to absorb the smoke agent by one of the following methods: dipping, stirring and mixing, spraying, etc. Furthermore, the adsorption time is controlled to reach a saturated adsorption amount.
[0118] Furthermore, before the porous material is subjected to the adsorption of the smoke generating agent or the granulation, a pretreatment step is further included: the material is crushed to an average diameter less than or equal to 80 microns.
[0119] Furthermore, after granulation and before extrusion molding, the porous granular material obtained by granulation is sequentially dried, sized, screened, etc., wherein the drying temperature is lower than the evaporation temperature of the smoke generating agent, so as to obtain a porous granular material with an average particle size of 200 microns to 600 microns.
[0120] Alternatively, in some other embodiments, the preparation of the non-tobacco segment aerosol matrix 32 includes the following steps: granulating the porous material to obtain a porous granular material; then allowing the porous granular material to adsorb a smoke-generating agent, and extruding the porous granular material adsorbed with the smoke-generating agent to obtain the non-tobacco segment aerosol matrix 32.
[0121] Furthermore, the porous granular material can be made to absorb the smoke agent by one of the methods of impregnation, stirring and mixing, spraying, etc. Furthermore, the adsorption time is controlled to reach the saturated adsorption amount.
[0122] Furthermore, after the porous granular material is obtained by granulation and before the porous granular material adsorbs the smoke-generating agent, the porous granular material obtained by granulation is sequentially subjected to drying, granulation, sieving and other steps, wherein the drying temperature is lower than the evaporation temperature of the smoke-generating agent. In this way, a porous granular material with an average particle size of 200 microns to 600 microns is obtained.
[0123] Furthermore, the extrusion molding can be performed by using a corresponding mold to extrude into a corresponding shape according to the diameter of the heated cigarette; the corresponding mold can be used to extrude into a corresponding shape according to the shape of the groove and other requirements; the corresponding mold can be used to extrude into a corresponding shape according to the shape of the channel and other requirements.
[0124] Another embodiment of the present application further provides an aerosol generating system, comprising any of the above-mentioned aerosol generating devices and a heating device for heating the aerosol generating device.
[0125] In some embodiments, the heating device includes a heating component, a battery component, a control component and a shell, the battery component is used to power the heating device, the control component is used to control the battery component, and the heating component, the battery component and the control component are housed in the shell.
[0126] Further, the heating component may be a central heating type heating component or a circumferential heating type heating component.
[0127] In order to make the purpose, technical solutions and advantages of the present invention more concise and clear, the present invention is described with the following specific embodiments, but the present invention is by no means limited to these embodiments. The embodiments described below are only preferred embodiments of the present invention, which can be used to describe the present invention and cannot be understood as limiting the scope of the present invention. It should be pointed out that any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
[0128] In order to better illustrate the present invention, the present invention is further described below in conjunction with the embodiments. The following are specific embodiments.
[0129] Example 1
[0130] (1) Preparation of tobacco segment aerosol matrix.
[0131] The aerosol matrix is formed by tobacco flakes, and glycerol is adsorbed on the tobacco segment aerosol matrix. The glycerol content is shown in Table 1, in mg / stick, which refers to the mass of glycerol contained in the tobacco segment aerosol matrix in each aerosol device. The following is similar.
[0132] (2) Preparation of non-tobacco aerosol matrix.
[0133] The porous material montmorillonite is adsorbed with glycerol as a smoke generating agent; the porous material adsorbed with the smoke generating agent is then granulated; the porous granular material montmorillonite obtained by granulation is mixed with a sodium carboxymethyl cellulose aqueous solution, and extruded through a mold, wherein the amount of sodium carboxymethyl cellulose used is 1wt% of the porous granular material (water in the sodium carboxymethyl cellulose aqueous solution is removed by heating during the extrusion molding), to obtain a cylindrical non-tobacco segment aerosol matrix.
[0134] The extrusion molding simultaneously forms grooves on the side wall of the smoke-generating body; specifically, five grooves penetrating along the axial direction are formed on the side wall, and the cross-sectional shape of the grooves is fan-shaped.
[0135] The non-tobacco segment aerosol matrix includes a porous matrix (i.e., a montmorillonite matrix) and glycerol, a smoke generating agent, adsorbed in the montmorillonite of the porous matrix. The mass of glycerol contained in the non-tobacco segment aerosol matrix is shown in Table 1.
[0136] It is understandable that different porous materials are used to form different porous matrices. If the porous material used is sepiolite, a sepiolite matrix is formed, as shown in Example 3. Other embodiments are similar.
[0137] (3) Preparation of aerosol generating device (i.e., cigarette stick).
[0138] As shown in Figure 1, the filter body, the hollow device, the non-tobacco segment aerosol matrix and the tobacco segment aerosol matrix are arranged in sequence, and the wrapping material layer is wrapped on the outer sides of the filter body, the hollow device, the non-tobacco segment aerosol matrix and the tobacco segment aerosol matrix connected in sequence to obtain an aerosol generating device.
[0139] Wherein, in Example 1, no pores are provided, and in the non-tobacco segment aerosol matrix, the total volume proportion of each groove is referred to as the total pore volume proportion in Table 1, %.
[0140] Embodiments 2 to 16
[0141] Examples 2 to 16 are substantially the same as Example 1, except that in step (2), at least one of the type of porous material in the preparation of the non-tobacco segment aerosol matrix, the glycerol content in the non-tobacco segment aerosol matrix, and whether or not a pore is provided and the shape of the pore is different, as shown in Table 1.
[0142] The pores can be formed synchronously by using a mold during extrusion molding. The shape of the pores and the volume ratio of the pores in the non-tobacco segment aerosol matrix are shown in Table 1. In this embodiment, the pores provided are all 1 central hole. Taking Example 2 as an example, a circular pore penetrating through the axis of the non-tobacco segment aerosol matrix is provided by an extrusion molding process. The total volume ratio of each groove and pore in Example 2 is referred to as the total pore volume ratio in Table 1; others are similar.
[0143] Comparative Example 1
[0144] It is basically the same as Example 1, except that a tobacco segment aerosol matrix of the same length is used to replace the non-tobacco segment aerosol matrix in Example 1; at the same time, the mass of total glycerol contained in the tobacco segment aerosol matrix is the same as the mass of total glycerol in Example 1.
[0145] Comparative Example 2
[0146] It is basically the same as Example 2, except that a tobacco segment aerosol matrix of the same length is used to replace the non-tobacco segment aerosol matrix in Example 2; at the same time, the mass of total glycerol contained in the tobacco segment aerosol matrix is the same as the mass of total glycerol in Example 2.
[0147] The aerosol generating devices (cigarettes) prepared in the examples and comparative examples were subjected to ambient heating, with the heating temperature set at 220° C., and the glycerin release amount, glycerin release rate and cigarette appearance were tested. The cigarette appearance was tested by visual observation.
[0148] The process of testing the glycerol release amount and glycerol release rate is as follows:
[0149] The heat-not-burn cigarettes were smoked using a linear smoking machine, and the smoking parameters of the cigarettes were:
[0150] Puffing capacity: 55mL; Puffing time: 2s; Puffing interval: 30s; Number of puffs: 8; Preheating time: 18s; Puffing curve: bell-shaped. A 44 mm Cambridge filter was used to capture the particulate matter in the heat-not-burn cigarette aerosol, and each filter captured the particulate matter of 5 cigarette samples.
[0151] The GC-TCD method was used to test the released glycerol content, with reference to the literature "Wang Kang, Liu Jun, Xiao Shaohong, et al. Simultaneous detection of moisture in heat-not-burn cigarette aerosols and the release of nicotine, glycerol, 1,2-propylene glycol, triacetin and menthol by GC-TCD [J]. Tobacco Science & Technology, 2019, 52 (3): 63-68."
[0152] Glycerol release rate = glycerol release mass / (glycerol in aerosol matrix + total mass of glycerol in independent smoke body) × 100%.
[0153] Table 1
[0154]
[0155] From the test results in Table 1, we can see that:
[0156] 1. By comparing Example 1 with Examples 1, 3, 5 and other examples with the same total amount of glycerol, as well as comparing Example 2 with Examples 2, 4, 6 and other examples with the same total amount of glycerol, it can be seen that when the aerosol matrix of the two-stage structure of the non-tobacco segment aerosol matrix of the present application and the traditional tobacco segment aerosol matrix is used, when the total amount of glycerol in the cigarette is the same, the amount of glycerol released increases and the glycerol release rate also increases.
[0157] 2. When other conditions remain unchanged, the total glycerin content of the cigarette increases from 50 mg to 80 mg, and the amount of glycerin released also increases; but the release rate of glycerin decreases.
[0158] 3. By comparing Examples 10 to 12, it can be seen that appropriately increasing the mass ratio of glycerol in the non-tobacco segment aerosol matrix to the total glycerol content in the aerosol matrix can increase the release amount and release rate of glycerol.
[0159] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0160] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the invention patent. It should be pointed out that for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be based on the attached claims, and the description and drawings can be used to interpret the content of the claims.
Claims
1. An aerosol generating device, characterized in that: It comprises a wrapping material layer, a filter body, a hollow device and an aerosol matrix; the wrapping material layer wraps the outer sides of the filter body, the hollow device and the aerosol matrix which are connected in sequence; the aerosol matrix comprises a tobacco segment aerosol matrix and a non-tobacco segment aerosol matrix, the non-tobacco segment aerosol matrix comprises a porous matrix and a smoke generating agent, and the smoke generating agent is adsorbed in the porous matrix.
2. The aerosol generating device according to claim 1, characterized in that: The non-tobacco segment aerosol matrix is located at one end of the tobacco segment aerosol matrix close to the hollow device.
3. The aerosol generating device according to claim 1, characterized in that: The side wall of the non-tobacco segment aerosol substrate is provided with a groove, and the groove runs from one end of the non-tobacco segment aerosol substrate close to the hollow device to the other end, and a channel is formed between the area of the side wall of the non-tobacco segment aerosol substrate where the groove is provided and the wrapping material layer.
4. The aerosol generating device according to claim 3, characterized in that: The area of the side wall of the non-tobacco segment aerosol substrate where the groove is provided accounts for 1 / 5 to 4 / 5 of the total area of the side wall of the non-tobacco segment aerosol substrate.
5. The aerosol generating device according to claim 1, characterized in that: The area of the side wall of the non-tobacco segment aerosol substrate not provided with the groove contacts the wrapping material layer.
6. The aerosol generating device according to claim 5, characterized in that: The non-tobacco segment aerosol matrix is a cylindrical structure, and the total arc length of the side wall of the non-tobacco segment aerosol matrix in contact with the wrapping material layer accounts for 1 / 5 to 4 / 5 of the total inner circumference of the wrapping material layer.
7. The aerosol generating device according to claim 1, characterized in that: The cross-sectional shape of the groove is fan-shaped, polygonal or irregular.
8. The aerosol generating device according to any one of claims 1 to 7, characterized in that: The number of the grooves on the side wall of the non-tobacco segment aerosol substrate is 1 to 50.
9. The aerosol generating device according to any one of claims 1 to 7, characterized in that: On the radial cross section of the non-tobacco segment aerosol matrix, the total area of the hollow region including the groove accounts for 5% to 40% of the inner cross section formed by the wrapping material layer.
10. The aerosol generating device according to any one of claims 1 to 7, characterized in that: The interior of the non-tobacco segment aerosol matrix is provided with a channel which is close to one end of the hollow device and penetrates the other end.
11. The aerosol generating device according to claim 10, characterized in that: The cross-sectional shape of the pores is circular, elliptical, sector-shaped, polygonal or irregular.
12. The aerosol generating device according to claim 10, characterized in that: Based on the volume of the non-tobacco segment aerosol matrix, the total volume of the grooves and the pores accounts for 5% to 40%.
13. The aerosol generating device according to any one of claims 1 to 7, characterized in that: One or more of the following conditions are met: (1) In the direction in which the hollow device extends toward the aerosol matrix, the length of the non-tobacco segment aerosol matrix is 2 mm to 15 mm; (2) In the direction in which the hollow device extends toward the aerosol matrix, the length of the tobacco segment aerosol matrix is 5 mm to 35 mm.
14. The aerosol generating device according to claim 1, characterized in that: The non-tobacco segment aerosol matrix and the tobacco segment aerosol matrix are both adsorbed with smoke generating agents.
15. The aerosol generating device according to claim 14, characterized in that: One or more of the following conditions are met: (1) The porous matrix is a porous granular material matrix, and the smoke generating agent is adsorbed in the porous granular material matrix; (2) The smoking agent in the non-tobacco segment aerosol matrix and the tobacco segment aerosol matrix both comprises at least one of glycerin, propylene glycol, ethylene glycol, xylitol and erythritol; (3) Based on the total mass of the smoke-generating agent in the non-tobacco segment aerosol matrix and the tobacco segment aerosol matrix, the mass proportion of the smoke-generating agent in the non-tobacco segment aerosol matrix is 40% to 65%.
16. The aerosol generating device according to claim 15, characterized in that: One or more of the following conditions are met: (1) The porous granular material of the porous granular material matrix includes at least one of natural porous mineral materials, metal oxides, hydroxides, carbonates, sulfates, activated carbon and molecular sieves; (2) The average particle size of the porous granular material of the porous granular material matrix is between 200 μm and 600 μm; (3) The smoking agent in the non-tobacco segment aerosol matrix and the tobacco segment aerosol matrix both include glycerin; (4) The mass of the smoke generating agent in the non-tobacco aerosol matrix is 20 mg to 50 mg per cigarette; (5) The mass of the smoke generating agent in the tobacco segment aerosol matrix is 30 mg to 40 mg per cigarette.
17. The aerosol generating device according to claim 16, characterized in that: One or more of the following conditions are met: (1) The natural porous mineral material includes at least one of diatomaceous earth, montmorillonite, sepiolite and kaolin; (2) The tobacco segment aerosol matrix also includes one or more of tobacco leaves, tobacco shreds, tobacco stem shreds, tobacco flakes, tobacco particles and tobacco extracts.
18. A method for preparing an aerosol generating device according to any one of claims 1 to 17, characterized in that: The steps include: The filter body, the hollow device, the non-tobacco segment aerosol matrix and the tobacco segment aerosol matrix are arranged in sequence, and the wrapping material layer is used to wrap the outer sides of the filter body, the hollow device, the non-tobacco segment aerosol matrix and the tobacco segment aerosol matrix connected in sequence to obtain an aerosol generating device.
19. The preparation method according to claim 18, characterized in that: Also included is the step of preparing the non-tobacco segment aerosol matrix; The preparation of the non-tobacco segment aerosol matrix comprises the following steps: allowing the porous material to absorb the smoke agent; granulating the porous material absorbed with the smoke agent; extruding the porous granular material obtained by granulation to obtain the non-tobacco segment aerosol matrix; or, The preparation of the non-tobacco segment aerosol matrix comprises the following steps: granulating a porous material to obtain a porous granular material; allowing the porous granular material to adsorb a smoke generating agent, and extruding the porous granular material adsorbing the smoke generating agent to obtain the non-tobacco segment aerosol matrix.
20. An aerosol generating system, characterized in that: It comprises the aerosol generating device according to any one of claims 1 to 17 and a heating device for heating the aerosol generating device.
21. The aerosol generating system according to claim 20, characterized in that: The heating device comprises a heating component, a battery component, a control component and a shell, the battery component is used to supply power to the heating device, the control component is used to control the battery component, and the heating component, the battery component and the control component are accommodated in the shell.
Citation Information
Patent Citations
Three-section heating nonflammable cigarette containing adsorbing material
CN107752123A
Heat-not-burn cigarette, preparation method thereof and heat-not-burn system
CN113940447A
Smoke agent, smoke material and heat-not-burn cigarette
CN114532577A
Aerosol-generating article having porous aerosol-generating substrate rod-form closure
CN115413817A
Aerosol-generating substrate and preparation method thereof
CN117481383A
Cited By
Aerosol-generating article, aerosol-generating system, and manufacturing method for aerosol-generating section
WO2026098326A1