Real-time evaluation method for evolution process of high-low cycle composite fatigue damage of steel structure

By defining the high-cycle-low-cycle composite fatigue criterion and the full-life fatigue model, the pre-damage-damage index of the steel structure is updated in real time, which solves the problem in the existing technology that the evolution process of high-cycle and low-cycle composite fatigue damage of the steel structure cannot be effectively evaluated. , achieving real-time evaluation and accurate calculation of steel structures, reducing calculation costs.

CN118747448APending Publication Date: 2024-10-08CHONGQING UNIV
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410644749.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-05-23
Publication Date
2024-10-08

AI Technical Summary

Technical Problem

Existing technology cannot effectively evaluate and real-time monitor the damage evolution process of steel structures under high-cycle and low-cycle composite fatigue, resulting in hidden dangers in structural life-cycle safety assessment and high calculation costs.

Method used

A real-time assessment method for the evolution process of high- and low-cycle composite fatigue damage of steel structures is proposed. By defining high-cycle-low-cycle composite fatigue criteria and a full-life fatigue model, state variables such as generalized stress, plastic rotation, and energy release rate are used to update the structure in real time. The pre-damage-damage index can automatically determine the fatigue action type and simulate the fatigue crack evolution process.

Benefits of technology

It achieves real-time assessment of the high and low cycle composite fatigue damage status of steel structures, reduces calculation costs, improves assessment accuracy, and provides a basis for structural reliability assessment and maintenance decisions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118747448A_ABST
    Figure CN118747448A_ABST
Patent Text Reader

Abstract

The invention discloses a real-time evaluation method for a high-low cycle composite fatigue damage evolution process of a steel structure, and belongs to the field of steel structure fatigue analys.The method comprises the steps that firstly, an inelastic hinge joint high-cycle-low cycle composite fatigue criterion is put forward, and structure pre-damage-damage indexes of a conventional service high-cycle fatigue stage and an accidental overload low-cycle fatigue stage are defined; then calculating a generalized stress amplitude, a plastic rotation amplitude and an energy release rate amplitude so as to update a fatigue structure pre-damage-damage index in real time; further establishing a full-life fatigue model of the steel structure, and carrying out real-time analysis on the whole process of crack evolution by automatically judging high-cycle or low-cycle fatigue; according to the invention, through automatic identification of a high-cycle or low-cycle fatigue loading process and through a method of nonlinear integration of a key variable in a time domain based on a high-cycle-low-cycle composite fatigue criterion, a convergence problem of structure full-life fatigue nonlinear process simulation is effectively overcome; and the damage evolution and performance mutation process of the bridge steel structure under full-life loading can be evaluated in real time.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of steel structure fatigue, and in particular relates to a real-time evaluation method for the evolution process of high- and low-cycle composite fatigue damage of a steel structure. Background Art

[0002] Steel structures have been widely used in infrastructure projects such as buildings, bridges, and offshore platforms because of their high strength, light weight, good seismic performance, resource reuse, and more eco-friendly advantages. These transportation and urban construction facilities mainly bear high-cycle loads such as vehicles and industrial cranes. At present, some transportation and building structures at home and abroad have entered the critical life period, that is, they have been in service for decades and have experienced decades of accumulated stress fatigue from load amplitudes. However, the impact of this part of stress fatigue on the residual performance of the structure is still unclear, which poses a hidden danger to the safety assessment of the structure life cycle. If they are not accurately assessed and reinforced in time, once these structures experience sudden earthquakes, impacts, overloads and other large-scale strain fatigue, it is very easy for key fatigue details to be damaged and fractured until the structure fails. The demand for full-life fatigue assessment technology for steel structures is becoming increasingly urgent, and there is currently no clear high-cycle stress-low-cycle strain fatigue composite assessment method.

[0003] Although the application demand of steel structures is increasing, fatigue problems are easily overlooked. The Shenyang Institute of Metal Research, Chinese Academy of Sciences and the American Society of Civil Engineering both mentioned that "nearly 90% of failures in metal structures are caused by fatigue damage", and fatigue damage often causes brittle failure, which is not easy to detect and is extremely harmful. At present, the fatigue performance evaluation of large structures over their entire life cycle mainly relies on on-site monitoring. There are two significant problems. First, the initial crack source of large bridge structures is difficult to locate, and the uniform arrangement of strain monitoring equipment throughout the bridge results in extremely high costs; more importantly, when the monitoring equipment senses a sudden change in structural performance, there is not enough time left for maintenance and reinforcement. The present invention proposes a real-time evaluation method for the evolution process of high- and low-cycle composite fatigue damage in steel structures, which is used for the fatigue performance evaluation of large-span steel structure bridges over their entire life cycle. Summary of the invention

[0004] In order to solve the problems that the existing evaluation methods cannot automatically determine the type of fatigue action, cannot update the damage status in real time, and cannot converge in the performance mutation stage when simulating the full-life fatigue nonlinear failure process of engineering-scale steel structures, the present invention proposes a real-time evaluation method for the evolution process of high- and low-cycle composite fatigue damage of steel structures. The real-time evolution of pre-damage and damage factors is used to characterize the process of high- and low-cycle fatigue crack initiation, expansion, and final failure at key nodes of steel structures.

[0005] The present invention is implemented by adopting the following technical scheme: a real-time evaluation method for the evolution process of high-low cycle composite fatigue damage of a steel structure, comprising the following steps:

[0006] Step A, proposing a high-cycle-low-cycle composite fatigue criterion for an inelastic hinge node, first defining a structural pre-damage-damage index in a conventional service high-cycle fatigue stage and an accidental overload low-cycle fatigue stage; the structural pre-damage-damage index includes a high-cycle fatigue pre-damage factor, a low-cycle fatigue pre-damage factor, and a high-cycle fatigue damage factor and a low-cycle fatigue damage factor;

[0007] The high cycle fatigue pre-damage factor is used to characterize the damage of the structure during the normal service period. 4 ~10 7 The crack initiation process caused by the accumulation of high-cycle loads, the low-cycle fatigue pre-damage factor is used to characterize the accelerated crack initiation process caused by the accumulation of plastic strain amplitude caused by accidental overload of the structure; when the pre-damage factor of the inelastic hinge node of the structure reaches the critical value, it indicates that the crack has initiated and entered the expansion stage; when the steel structure continues to be subjected to overload cycles, the high-cycle-low-cycle full-life fatigue model characterizes the expansion process after the initiation of the most unfavorable tensile section crack through the high-cycle fatigue damage factor and the low-cycle fatigue damage factor, and the fatigue life of the structure is determined to be terminated when the damage index reaches the critical value; specifically:

[0008] a) Steel structures are subjected to high-cycle cyclic loads during normal service. Before cracks are found, the high-cycle fatigue pre-damage factor ω H Characterize the crack initiation process of inelastic hinge nodes caused by high-cycle load accumulation:

[0009]

[0010] Where t represents the current moment of the life-cycle fatigue history of the steel structure, Delta is the loading time increment set in the life-cycle fatigue model of the steel structure, Δm(t) is the instantaneous generalized stress amplitude, and M cr Determined by the actual structure, γ is the high cycle fatigue index;

[0011] b) During the crack initiation process, the structure is subjected to low-cycle fatigue caused by overload, and the low-cycle fatigue pre-damage factor ω L Characterizes the accelerated crack initiation process caused by the accumulation of plastic strain amplitude when the structure is accidentally subjected to overload:

[0012]

[0013] Among them, Δφ P is the instantaneous plastic rotation amplitude, is the critical cracking plastic rotation, which is related to the cross-sectional size and material fatigue ductility coefficient, and β is the low-cycle fatigue index;

[0014] c) The crack growth process is expressed as the evolution of high-cycle and low-cycle fatigue damage indicators with the total loading time d(t), including the high-cycle fatigue damage factor d H (t) and low cycle fatigue damage factor d L (t):

[0015] d(t)=d L (t)+d H (t)

[0016] The accumulation process of high cycle fatigue damage factor can be described in the form of time increment Delta as follows:

[0017] d H (t) = d H (t-Delta)+(Q(DG(t)) R )·Delta

[0018] Among them, ΔG(t) is the instantaneous energy release rate amplitude, Q and R are the energy release coefficient and exponent of the node under stress cracking, respectively;

[0019] The accumulation process of low-cycle fatigue damage factors can be described as:

[0020]

[0021] Among them, α is the cross-sectional shape index, Δφ P is the instantaneous plastic rotation amplitude.

[0022] Step B: The structural pre-damage-damage index of the high-cycle-low-cycle full-life fatigue model is determined by key state variables such as generalized stress amplitude, plastic rotation amplitude and energy release rate amplitude. Based on the accumulation and difference of stress and deformation at the inelastic hinge node of the structure in the time domain, the generalized stress amplitude, plastic rotation amplitude and energy release rate amplitude are calculated, and the structural fatigue pre-damage-damage index is updated in real time; specifically:

[0023] a) Under high-cycle fatigue, the structure is in an elastic state, and the evolution of high-cycle fatigue pre-damage factor and high-cycle fatigue damage factor is controlled by stress amplitude; under low-cycle fatigue, the structure is in a plastic state, and the evolution of low-cycle fatigue pre-damage factor and low-cycle fatigue damage factor is controlled by strain amplitude;

[0024] b) The instantaneous generalized stress amplitude Δm(t) of the high-cycle fatigue pre-damage process is calculated based on the stress accumulation and difference criterion at the inelastic hinge node;

[0025] Superposition calculation of the cumulative generalized stresses at inelastic hinge nodes:

[0026] b i,j (t) = b i,j (t-Delta)+|m i,j(t)-m i,j (t-Delta)|

[0027] Among them, b i,j (t) is the cumulative generalized stress at the inelastic hinge node i or j subjected to cyclic load until time t, m i,j (t) is the generalized stress at the inelastic hinge node i or j at time t, m i,j (t-Delta) is the generalized stress before the unit time increment at the inelastic hinge node i or j at time t,

[0028] The instantaneous generalized stress amplitude at time t is calculated by the finite difference method:

[0029]

[0030] Where Δt is the time interval of the finite difference method;

[0031] c) The instantaneous energy release rate amplitude ΔG(t) of the high cycle fatigue damage process is calculated by the finite difference method based on the generalized stress at the inelastic hinge node of the structure:

[0032]

[0033] Among them, the cumulative energy release rate of node i or j subjected to cyclic load to time t is expressed as:

[0034] gg i,j (t) = gg i,j (t-Delta)+|G i,j (t)-G i,j (t-Delta)|

[0035] Among them, the energy release rate of the inelastic hinge node at each moment is expressed as:

[0036]

[0037] Where EI is the stiffness of the structural member, L is the actual length of the structural member, d(t-Delta) is the damage factor of the inelastic hinge node before the unit time increment at time t, m(t) is the generalized stress of the inelastic hinge node at time t, <m> + It means that only the generalized stress value in the positive direction, i.e. the cracking direction of the node, is calculated;

[0038] d) The structure is subjected to low-cycle fatigue caused by accidental overload. The low-cycle fatigue pre-damage factor and damage factor are both determined by the instantaneous plastic rotation amplitude Δφ P (t) is determined by the accumulation and difference criterion of plastic deformation at the inelastic hinge node:

[0039]

[0040] Among them, the accumulated plastic rotation of the inelastic hinge nodes i or j at both ends of the structural member is:

[0041]

[0042] in, and They represent the plastic rotation state of the inelastic hinge node i or j at the current time t and the time before the unit time increment, respectively.

[0043] Step C, establish a full-life fatigue model of the rod unit-inelastic hinge node of the steel structure, set boundary conditions, attribute constant parameters and analysis steps according to the actual loading process, and realize real-time analysis of the whole process of crack evolution of the inelastic hinge node of the structure by constructing control equations such as kinematic equations, mechanical equilibrium equations, and elastic-plastic damage constitutive equations;

[0044] Set the initial input conditions: including boundary conditions, attribute constant parameters and analysis steps. The boundary condition settings include node displacement constraints and loading time history. Constrain the horizontal and vertical translational degrees of freedom of the model boundary nodes. Apply displacement time histories of different amplitudes to the loading nodes to simulate full-life fatigue loading. Specifically:

[0045] The constant parameters of high-cycle fatigue properties of steel structures include the high-cycle fatigue base number M of the node crack incubation period cr and high cycle fatigue index γ, as well as the damage coefficient Q and index R during crack propagation; the low cycle fatigue property constants are set as: node critical cracking plastic rotation Low cycle fatigue index β and crack closure factor h when the node is under compression — ;

[0046] Establish the global coordinate system and the global coordinates of each node, define the state variables of the bar unit and the node, and establish the functional relationship between the relevant variables. The generalized deformation matrix of the steel structure bar {Φ} b It consists of three components: i-node rotation, j-node rotation, and rod axis expansion and contraction. The corresponding generalized stress matrix {M} b It is also composed of three components: i-node bending moment, j-node bending moment and rod axial force. The full-life fatigue process of the steel structure evaluated by this model is that the most unfavorable stress node of the structure first undergoes a high-cycle fatigue crack latent period, and then the accumulation of plastic rotation amplitude at the node under the action of low-cycle fatigue causes crack expansion and damage fracture.

[0047] where the generalized deformation {Φ} of the connecting node bar element b is b The kinematic equation between the global node displacement {U(t)} is defined as:

[0048] {Φ(t)} b =[B(U)] b {U(t)}

[0049] The length of the rod unit is L, and the angle between it and the X-axis of the global coordinate system is α. b , [B(U)] b is the overall coordination matrix between the rod element b and the corresponding nodes i and j;

[0050] The sum of the generalized stresses of all bar elements and the global node external forces satisfy the mechanical equilibrium equation, which is defined as:

[0051] {P(t)}=∑[B(U)] n T ·{M(t)} n

[0052] Under the action of high-cycle fatigue over a long period of time, the structure is in an elastic state, and the generalized deformation and generalized stress of the rod element satisfy the elastic constitutive equation {M(t)} n =[E]{Φ(t)} n At this time, the high cycle fatigue crack is in the latent period, and its stiffness matrix [E] remains unchanged, which can be described as,

[0053]

[0054] Among them, EI is the actual bending stiffness of the rod, and AE is the axial stiffness of the rod;

[0055] Furthermore, under low-cycle fatigue, the most unfavorable stress node of the structure forms an inelastic hinge, and it is necessary to consider the effects of plasticity and damage in the constitutive equation, that is, the elastic-plastic damage constitutive equation, which is described as

[0056]

[0057] Among them, {Φ p (t)} n is the state variable of the generalized plastic deformation of the rod element n evolving with time, F + (D) and F - (D) are the flexibility matrices for considering crack extension and closure when the inelastic hinge node is under tension and compression, respectively, and are described as:

[0058]

[0059] When the load is along the tensile cracking direction of the node, the flexibility matrix is ​​not modified, that is, h + =1.0, and when loading in the reverse direction, let h — =0.3, to describe the closure phenomenon of plastic damage cracks when the inelastic hinge node is under compression.

[0060] Based on the above three types of control equations, a full-life fatigue model of steel structure is established. The model automatically determines the type of fatigue action by analyzing the setting of the time increment step. When the time increment step Delta is less than 1.0, the analysis step is low-cycle fatigue loading, otherwise, the analysis step is high-cycle fatigue loading;

[0061] Through the iterative analysis of the full-life fatigue model of the steel structure, the generalized stress and plastic deformation of the inelastic hinge node at any time are obtained, and the key state variables of the inelastic hinge node, including the instantaneous generalized stress amplitude, instantaneous energy release rate amplitude and instantaneous plastic rotation amplitude, are calculated in real time. The pre-damage-damage index of the structure at the current moment is updated, and the elastic-plastic damage constitutive equation of the steel structure of the next incremental step model analysis is updated at the same time, so as to realize the real-time evaluation of the high-low cycle composite fatigue damage state of the steel structure.

[0062] Based on the high-cycle-low-cycle composite fatigue criterion of inelastic hinge nodes, the high-cycle or low-cycle fatigue effect is automatically identified through the full-life fatigue model of the steel structure, and the key state variables and damage indicators are updated in real time, overcoming the problem that the traditional model cannot converge when analyzing the performance mutation stage of the fatigue damage process of the steel structure.

[0063] Compared with the prior art, the advantages and positive effects of the present invention are:

[0064] In this scheme, when the steel structure is subjected to high-cycle and low-cycle combined fatigue, the plastic accumulation and damage cracking are concentrated on the inelastic hinge nodes. By comprehensively considering the elastic-plastic criterion and fatigue damage criterion of the steel structure throughout its life cycle, a full-life fatigue model of the steel structure that transcends the scale effect is established. By automatically identifying the high-cycle or low-cycle fatigue loading process, the fatigue damage evolution simulation of the whole life cycle is realized, which also greatly reduces the calculation cost.

[0065] In addition, the finite difference method is used to calculate the key state variables of the nodes in the high-low cycle composite fatigue loading process, so as to achieve the convergence of the fatigue crack evolution process of the simulated structure throughout its life cycle. Ultimately, the pre-damage index, damage index and the performance mutation process of the damaged structure node can be updated in real time. The high-low cycle composite fatigue damage evolution process of the steel structure is updated in real time, which provides a basis for the reliability assessment and maintenance decision-making of the in-service steel structure, so as to improve the calculation accuracy and reduce the cost. BRIEF DESCRIPTION OF THE DRAWINGS

[0066] Figure 1 It is a flow chart of the real-time evaluation method of high- and low-cycle combined fatigue damage evolution of the present invention;

[0067] Figure 2 A schematic diagram of the high-cycle-low-cycle full-life fatigue action borne by the inelastic hinge node according to an embodiment of the present invention;

[0068] Figure 3 A schematic diagram of a process for automatically identifying a model of high-cycle or low-cycle fatigue action according to an embodiment of the present invention;

[0069] Figure 4 This is a schematic diagram of the non-convergence of the full-life fatigue model of the steel structure caused by the 0.25 time interval in the embodiment of the present invention;

[0070] Figure 5 A comparison diagram of composite fatigue damage results of steel structures simulated at different time intervals according to an embodiment of the present invention;

[0071] Figure 6 The composite fatigue damage simulation result of the steel structure node calculated at a time interval of 0.50 in the embodiment of the present invention;

[0072] Figure 7 This is a comparison chart of the full-life damage evolution results of the steel structure under different high-cycle loading amplitudes according to the embodiment of the present invention. DETAILED DESCRIPTION

[0073] In order to more clearly understand the above-mentioned purpose, features and advantages of the present invention, the present invention is further described below in conjunction with the accompanying drawings and embodiments. In the following description, many specific details are set forth to facilitate a full understanding of the present invention, but the present invention can also be implemented in other ways different from those described herein, and therefore, the present invention is not limited to the specific embodiments disclosed below.

[0074] This embodiment proposes a real-time evaluation method for the evolution of high- and low-cycle composite fatigue damage in a common rigid connection node of a steel structure. Figure 1 As shown, the following steps are included:

[0075] Step A, in order to propose a high-cycle-low-cycle composite fatigue criterion for the full-life fatigue model of an inelastic hinge node, firstly, define the structural pre-damage-damage index in the conventional service high-cycle fatigue stage and the accidental overload low-cycle fatigue stage; the structural pre-damage-damage index includes a high-cycle fatigue pre-damage factor, a low-cycle fatigue pre-damage factor, and a high-cycle fatigue damage factor and a low-cycle fatigue damage factor;

[0076] (1) The high-cycle and low-cycle full-life fatigue effects on inelastic hinge joints of steel structures are as follows: Figure 2 As shown in the figure, the structural pre-damage index ω and damage index d in the conventional service high-cycle fatigue stage and the accidental overload low-cycle fatigue stage are defined as follows:

[0077] a) Steel structures are subjected to high-cycle cyclic loads during normal service. Before cracks can be found, the high-cycle-low-cycle full-life fatigue model uses the high-cycle fatigue pre-damage factor ω H Characterize the crack initiation process of inelastic hinge nodes caused by high-cycle load accumulation.

[0078]

[0079] Where t represents the current moment of the life-cycle fatigue history of the steel structure, Delta is the loading time increment set by the high-cycle-low-cycle life-cycle fatigue model, Δm(t) is the instantaneous generalized stress amplitude, and M cr Determined by the actual structure, γ is the high cycle fatigue index;

[0080] b) During the crack initiation process, the structure may be subjected to low-cycle fatigue caused by overload, and the accumulation of plastic strain amplitude accelerates the crack initiation process; the high-cycle-low-cycle full-life fatigue model uses the low-cycle fatigue pre-damage factor ω L Characterizes the accelerated crack initiation process caused by the accumulation of plastic strain amplitude when the structure is accidentally subjected to overload.

[0081]

[0082] Among them, Δφ P is the instantaneous plastic rotation amplitude, is the critical cracking plastic rotation, which is related to the cross-sectional size and material fatigue ductility coefficient, and β is the low-cycle fatigue index;

[0083] The critical state of crack initiation is the pre-damage value ω(t) = ω L (t)+ω H When (t) reaches 1.0, the pre-damage of the inelastic hinge node of the structure reaches the critical value, and the crack of the most unfavorable tensile section initiates and enters the crack propagation stage;

[0084] c) The crack growth process is expressed as the evolution of high- and low-cycle damage indicators with the total loading time d(t), including the high-cycle fatigue damage factor d H (t) and low cycle fatigue damage factor d L (t):

[0085] d(t)=d L (t)+d H (t)

[0086] The accumulation process of high cycle fatigue damage factor can be described in the form of time increment (Delta):

[0087] d H (t) = d H (t-Delta)+(Q(DG(t)) R )·Delta

[0088] Among them, ΔG(t) is the amplitude of the instantaneous energy release rate, Q and R are determined by the actual structure at the node and can be determined by high-cycle fatigue tests;

[0089] When a steel structure is subjected to overload or earthquake, although the cycle is short, it will aggravate the crack propagation of the inelastic hinge node, which is caused by further plastic cumulative damage. Therefore, the accumulation process of low-cycle fatigue damage factor can be described as:

[0090]

[0091] Among them, α is determined by the cross-sectional shape, Δφ P is the instantaneous plastic rotation amplitude,

[0092] In this process, the plastic rotation of the damaged section gradually increases, and ultimately fatigue failure is controlled by the damage index. The upper limit of crack extension is when the high and low cycle fatigue damage factor d(t) reaches 0.65, and the key inelastic hinge node of the steel structure fails.

[0093] Step B: The structural pre-damage-damage index of the high-cycle-low-cycle composite fatigue criterion is determined by key state variables such as generalized stress amplitude, plastic rotation amplitude and energy release rate amplitude. Based on the accumulation and difference of stress and deformation at the inelastic hinge node of the structure in the time domain, the generalized stress amplitude, plastic rotation amplitude and energy release rate amplitude are calculated, and the structural fatigue pre-damage-damage index is updated in real time.

[0094] a) Under high-cycle fatigue, the structure is in an elastic state, and the evolution of pre-damage and damage factors is controlled by the stress amplitude; under low-cycle fatigue, the structure is in a plastic state, and the evolution of pre-damage and damage factors is controlled by the strain amplitude;

[0095] b) The instantaneous generalized stress amplitude Δm(t) of the high-cycle fatigue pre-damage process is calculated based on the stress accumulation and difference criterion at the inelastic hinge node. First, the cumulative generalized stress of the inelastic hinge node is superimposed and calculated:

[0096] b i,j (t) = b i,j (t-Delta)+|m i,j (t)-m i,j (t-Delta)|

[0097] Among them, b i,j (t) is the cumulative generalized stress at the inelastic hinge node i or j subjected to cyclic load until time t, m i,j (t) is the generalized stress at the inelastic hinge node i or j at time t, m i,j (t-Delta) is the generalized stress before the unit time increment at the inelastic hinge node i or j at time t,

[0098] Next, the instantaneous generalized stress amplitude at time t is calculated by the finite difference method:

[0099]

[0100] Among them, the time interval Δt of the finite difference method is 0.5 or 1.0. If the interval is too short, it will be difficult for the results to converge to a steady state, and if the interval is too long, the real-time update of the damage state cannot be achieved;

[0101] c) The instantaneous energy release rate amplitude ΔG(t) of the high cycle fatigue damage process is also calculated by the finite difference method based on the generalized stress at the inelastic hinge node of the structure. The time interval Δt of the finite difference method is 0.5 or 1.0, expressed as:

[0102]

[0103] Among them, the cumulative energy release rate of node i or j subjected to cyclic load to time t is calculated as:

[0104] gg i,j (t) = gg i,j (t-Delta)+|G i,j (t)-G i,j (t-Delta)|

[0105] Among them, the energy release rate of the inelastic hinge node at each moment is calculated as:

[0106]

[0107] Where EI is the stiffness of the structural member, L is the actual length of the structural member, d(t-Delta) is the damage factor of the inelastic hinge node before the unit time increment at time t, m(t) is the generalized stress of the inelastic hinge node at time t, <m> + It means that only the generalized stress value in the positive direction, i.e. the cracking direction of the node, is calculated;

[0108] d) In addition, when the structure is subjected to low-cycle fatigue caused by accidental overload, both the low-cycle fatigue pre-damage factor and the damage factor are determined by the instantaneous plastic rotation amplitude Δφ P (t) is determined by the accumulation of plastic deformation at the inelastic hinge node and the calculation of the difference criterion. The time interval Δt of the finite difference method is 0.5 or 1.0.

[0109]

[0110] Among them, the accumulated plastic rotation of the inelastic hinge nodes i or j at both ends of the structural member is:

[0111]

[0112] in, and are the plastic rotation states of the inelastic hinge node i or j at the current time t and the increment time before the unit time increment respectively;

[0113] The high-cycle stress transient state variables Δm(t) and ΔG(t) and the low-cycle plastic strain transient state variable Δφ calculated above are P (t) is used to characterize the damage state of the inelastic hinge node in the full-life fatigue model of the steel structure in step C and to update the constitutive equation of the bar element.

[0114] Step C, establish a full-life fatigue model for steel structures, construct the elastic-plastic damage constitutive equations of the rod unit, and further propose an automatic recognition process for the type of fatigue action of the model to identify whether the current loading stage is high-cycle fatigue or low-cycle fatigue, thereby realizing real-time analysis of the entire process of crack evolution of the inelastic hinge node of the structure;

[0115] The initial input settings of the full-life fatigue model mainly include three parts: boundary conditions, attribute constant parameters and analysis steps. The boundary condition settings include node displacement constraints and loading time history, horizontal and vertical translational degrees of freedom constraints on support nodes, and full-life fatigue loading is simulated by applying displacement time histories of different amplitudes to the loading nodes. Specifically:

[0116] a) High cycle fatigue property constants of steel structures include the high cycle fatigue base M of the node crack incubation period cr =11115 kN·m and high cycle fatigue index γ = -3, as well as the damage coefficient Q = 0.01345 and index R = -0.1 during crack propagation, obtained from actual structural tests; according to the specific structural details, the low cycle fatigue property constants of steel structures are set as: critical crack plastic rotation is 0.03265, the low cycle fatigue index β is -1.67, and the crack closure factor h when the node is under pressure — is 0.3; the cross-sectional bending stiffness EI of the steel structure member is 19000 kN·m 2 , the cross-sectional axial stiffness EA is 1.321×10 6 kN, the cross-sectional shape factor α is 0.45, and the cross-sectional yield moment M y It is 307kN·m, and the strengthening coefficient c of the material is 16000;

[0117] b) Establish the global coordinate system of the steel structure full life fatigue model and the global coordinates of each node, define the state variables of the bar unit and the node, and establish the functional relationship between the relevant variables. The generalized deformation matrix of the steel structure bar {Φ} b It consists of three components: i-node rotation, j-node rotation, and rod axis expansion and contraction. The corresponding generalized stress matrix {M} b It is also composed of three components: i-node bending moment, j-node bending moment and rod axial force. The full-life fatigue failure process simulated by this model is that the most unfavorable stress node of the structure first undergoes a high-cycle fatigue crack latent period, and then the accumulation of plastic rotation amplitude at the node under the action of low-cycle fatigue causes crack expansion and damage fracture.

[0118] where the generalized deformation {Φ} of the connecting node bar element b is b The kinematic equation between the global node displacement {U(t)} is defined as:

[0119] {Φ(t)} b =[B(U)] b {U(t)}

[0120] The length of the rod unit is L, and the angle between it and the X-axis of the global coordinate system is α. b , [B(U)] b is the overall coordination matrix between the rod element b and the corresponding nodes i and j;

[0121] The sum of the generalized stresses of all bar elements and the global node external forces satisfy the mechanical equilibrium condition, which is defined as:

[0122] {P(t)}=∑[B(U)] n T ·{M(t)} n

[0123] Under the action of high-cycle fatigue over a long period of time, the structure is in an elastic state, and the generalized deformation and generalized stress of the rod element satisfy the elastic constitutive equation {M(t)} n =[E]{Φ(t)} n At this time, the high cycle fatigue crack is in the latent period, and its stiffness matrix [E] remains unchanged, which can be described as,

[0124]

[0125] Among them, EI is the actual bending stiffness of the rod, and AE is the axial stiffness of the rod;

[0126] Furthermore, under low-cycle fatigue, the most unfavorable stress node of the structure forms an inelastic hinge, and the plasticity and damage effects need to be considered in the constitutive equation, which is defined as Among them, {Φ p (t)} n is the state variable of the generalized plastic deformation of the rod element n evolving with time, F + (D) and F - (D) are the flexibility matrices for considering crack extension and closure when the inelastic hinge node is under tension and compression, respectively, and are described as:

[0127]

[0128] When the load is along the tensile cracking direction of the node, the flexibility matrix is ​​not modified, that is, h + =1.0, and when loading in the reverse direction, let h — =0.3, to describe the closure phenomenon of plastic damage cracks when the inelastic hinge node is under compression.

[0129] Based on the above-mentioned full-life fatigue model of the steel structure, the generalized stress and plastic deformation of the inelastic hinge node at the current moment are obtained, and the generalized stress amplitude, plastic rotation amplitude and energy release rate amplitude in step B are further calculated, as well as the high-cycle-low-cycle pre-damage index and damage index that describe the entire crack evolution process of the inelastic hinge node of the steel structure defined in the present invention, to form a fatigue damage matrix of the node at the current moment, and serve as an input of the full-life fatigue model at the next moment, for updating the elastic-plastic constitutive relationship at the next moment;

[0130] c) Determine whether the current analysis step is high-cycle fatigue loading or low-cycle fatigue loading by using the time increment Delta (e.g. Figure 3 ), specifically, when Delta is less than 1.0, the analysis step is low-cycle fatigue loading, otherwise, the analysis step is high-cycle fatigue loading. This is because the total time of low-cycle fatigue is short and there is strong material nonlinearity, so a small time increment is easy to converge, while the high-cycle fatigue action lasts for a long time, and the maximum time increment can be set to hundreds to thousands of times to save calculation time; the high-cycle pre-damage-low-cycle damage evolution criterion is also realized through iterative calculation of time increments;

[0131] When simulating the full-life fatigue failure of bridge steel structures, considering the order of magnitude difference between the high-cycle fatigue incubation period and the low-cycle fatigue crack growth period, different analysis steps are set. For high-cycle fatigue, the iterative time increment is 20,000; for low-cycle fatigue, the initial time increment is set to 0.013, the maximum time increment is set to 0.025; the total time is 10 6 (high cycle) + 13 (low cycle); the simulation program can automatically identify high-cycle or low-cycle fatigue effects according to whether the time increment is greater than 1, and output the bending moment, plastic rotation, pre-damage index and damage index of each increment of the hinge node.

[0132] d) In order to achieve the convergence of the high and low cycle full life fatigue model of steel structures, it is necessary to set an appropriate finite difference method time interval. When the interval set by the finite difference method is too short (Δt = 0.25), it will make it difficult for the results to converge to a steady state ( Figure 4 ), specifically,

[0133] Under constant amplitude high cycle fatigue and constant displacement amplitude low cycle fatigue overload, both high cycle pre-damage index and low cycle pre-damage index are theoretically linearly related to the loading cycle. However, in the process of simulating the evolution of high cycle-low cycle composite fatigue, the amplitude transition from conventional loading to overload will cause nonlinear fluctuations in the output value of the state variable. If the calculation cycle of the finite difference method is too small, such as Delta = 0.25, the output result will not converge when simulating the low cycle fatigue crack initiation stage caused by overload.

[0134] When the time interval Δt is 0.5 or 1.0, the whole process of simulated high-cycle-low-cycle composite fatigue cracking is basically the same ( Figure 5 ), which consists of the high-cycle fatigue crack incubation period, the low-cycle fatigue crack initiation period and the low-cycle fatigue crack propagation period;

[0135] When Δt is set to 0.5, this method is used to simulate Figure 2 Cyclic overload test of steel structure nodes with loading history, the load-displacement curve results are as follows Figure 6 As shown in the figure, the whole process of low-cycle fatigue failure can be simulated normally. The failure process and load-displacement curve simulated by the program are in good agreement with the actual structural node overload test, especially the fatigue performance degradation process caused by crack extension in the negative loading direction. The number of cycles at the final simulated failure is 10.75, and the number of cycles at the test node failure is 11.75. Furthermore, the low-cycle fatigue damage evolution analysis of steel structures under different high-cycle loading cycle histories was carried out. Figure 7 The comparison results show that the nodes have different pre-damage states after experiencing high-cycle fatigue loading cycles with different amplitudes. Then, under the same overload cycle, the nodes with large high-cycle fatigue loading amplitude enter the damage state faster and eventually fail due to fatigue at a shorter number of low-cycle cycles.

[0136] The present invention describes the full life real-time evolution process of the most unfavorable node of the steel structure from the stress amplitude accumulation in the conventional service stage to the cumulative plastic rotation and subsequent fracture failure under the action of accidental overload by proposing high-cycle fatigue pre-damage factor, damage factor, low-cycle fatigue pre-damage factor, damage factor and corresponding calculation criteria; an explicit calculation method for the key state variables of the inelastic hinge node of the structure is proposed, which is realized by the accumulation and difference of the generalized stress and deformation of the node in the time domain as the loading system changes. The time interval of the finite difference method is reasonably set to ensure the convergence of the simulation process, which overcomes the difficulty of commercial continuum finite element to converge when simulating sudden changes in structural states; the high-cycle-low-cycle automatic discrimination criterion realizes the continuous simulation process from the high-cycle fatigue crack incubation period to the low-cycle fatigue crack propagation period, which overcomes the key difficulty of fatigue performance evaluation of large-span steel structure bridges throughout their life cycle.

[0137] The above description is only a preferred embodiment of the present invention and does not limit the present invention in other forms. Any technician familiar with the profession may use the technical content disclosed above to change or modify it into an equivalent embodiment with equivalent changes and apply it to other fields. However, any simple modification, equivalent change and modification made to the above embodiment based on the technical essence of the present invention without departing from the content of the technical solution of the present invention still falls within the protection scope of the technical solution of the present invention.< / m> < / m>

Claims

1. A real-time evaluation method for the evolution of high-low cycle composite fatigue damage of steel structures, characterized in that: The following steps are involved: Step A: Propose a high-cycle-low-cycle composite fatigue criterion for inelastic hinge nodes, and define the structural pre-damage-damage index for the conventional service high-cycle fatigue stage and the accidental overload low-cycle fatigue stage; The structural pre-damage-damage index includes a high-cycle fatigue pre-damage factor, a low-cycle fatigue pre-damage factor, a high-cycle fatigue damage factor, and a low-cycle fatigue damage factor; Step B, the structural pre-damage-damage index is determined by the generalized stress amplitude, the plastic rotation amplitude and the energy release rate amplitude, and the generalized stress amplitude, the plastic rotation amplitude and the energy release rate amplitude are calculated based on the accumulation and difference of stress and deformation at the inelastic hinge node of the structure in the time domain, and the structural fatigue pre-damage-damage index is updated in real time; Step C: Establish a full-life fatigue model of the rod unit-inelastic hinge node of the steel structure, construct the elastic-plastic constitutive equation between the rod unit and the inelastic hinge node of the steel structure, and automatically identify whether the current loading stage is high-cycle fatigue or low-cycle fatigue, thereby realizing real-time analysis of the entire process of crack evolution of the inelastic hinge node of the structure.

2. The real-time evaluation method for the evolution of high-low cycle combined fatigue damage of steel structures according to claim 1 is characterized in that: In step A, the structural pre-damage index and damage index in the conventional service high-cycle fatigue stage and the accidental overload low-cycle fatigue stage are defined as follows: a) Steel structures are subjected to high-cycle cyclic loads during normal service. Before cracks are found, the high-cycle fatigue pre-damage factor ω H Characterize the crack initiation process of inelastic hinge nodes caused by high-cycle load accumulation: Where t represents the current moment of the life-cycle fatigue history of the steel structure, Delta is the loading time increment set in the life-cycle fatigue model of the steel structure, Δm(t) is the instantaneous generalized stress amplitude, and M cr Determined by the actual structure, γ is the high cycle fatigue index; b) During the crack initiation process, the structure is subjected to low-cycle fatigue caused by overload, and the low-cycle fatigue pre-damage factor ω L Characterizes the accelerated crack initiation process caused by the accumulation of plastic strain amplitude when the structure is accidentally subjected to overload: Among them, Δφ P is the instantaneous plastic rotation amplitude, is the critical cracking plastic rotation, which is related to the cross-sectional size and material fatigue ductility coefficient, and β is the low-cycle fatigue index; c) The crack growth process is expressed as the evolution of high-cycle and low-cycle fatigue damage indicators with the total loading time d(t), including the high-cycle fatigue damage factor d H (t) and low cycle fatigue damage factor d L (t): d(t)=d L (t)+d H (t) The accumulation process of high cycle fatigue damage factor can be described in the form of time increment Delta as follows: d H (t)=d H (t-Delta)+(Q(DG(t)) R )·Delta Among them, ΔG(t) is the instantaneous energy release rate amplitude, Q and R are the energy release coefficient and exponent of the node under stress cracking, respectively; The accumulation process of low-cycle fatigue damage factors can be described as: Among them, α is the cross-sectional shape index, Δφ P is the instantaneous plastic rotation amplitude.

3. The real-time evaluation method for the evolution of high-low cycle combined fatigue damage of steel structures according to claim 1 is characterized in that: The step B is specifically implemented in the following manner: a) The structure is in an elastic state under high cycle fatigue, and the evolution of high cycle fatigue pre-damage factor and high cycle fatigue damage factor is controlled by stress amplitude; Under low cycle fatigue, the structure is in a plastic state, and the evolution of low cycle fatigue pre-damage factor and low cycle fatigue damage factor is controlled by strain amplitude; b) The instantaneous generalized stress amplitude Δm(t) of the high-cycle fatigue pre-damage process is calculated based on the stress accumulation and difference criterion at the inelastic hinge node; Superposition calculation of the cumulative generalized stresses at inelastic hinge nodes: b i,j (t)=b i,j (t-Delta)+|m i,j (t)-m i,j (t-Delta)| Among them, b i,j (t) is the cumulative generalized stress at the inelastic hinge node i or j subjected to cyclic load until time t, m i,j (t) is the generalized stress at the inelastic hinge node i or j at time t, m i,j (t-Delta) is the generalized stress before the unit time increment at the inelastic hinge node i or j at time t, The instantaneous generalized stress amplitude at time t is calculated by the finite difference method: Where Δt is the time interval of the finite difference method; c) The instantaneous energy release rate amplitude ΔG(t) of the high cycle fatigue damage process is calculated by the finite difference method based on the generalized stress at the inelastic hinge node of the structure: Among them, the cumulative energy release rate of node i or j subjected to cyclic load to time t is expressed as: gg i,j (t)=gg i,j (t-Delta)+|G i,j (t)-G i,j (t-Delta)| Among them, the energy release rate of the inelastic hinge node at each moment is expressed as: Where EI is the stiffness of the structural member, L is the actual length of the structural member, d(t-Delta) is the damage factor of the inelastic hinge node before the unit time increment at time t, m(t) is the generalized stress of the inelastic hinge node at time t, <m> + It means that only the generalized stress value in the positive direction, i.e. the cracking direction of the node, is calculated;< / m> d) The structure is subjected to low-cycle fatigue caused by accidental overload. The low-cycle fatigue pre-damage factor and damage factor are both determined by the instantaneous plastic rotation amplitude Δφ P (t) is determined by the accumulation and difference criterion of plastic deformation at the inelastic hinge node: Among them, the accumulated plastic rotation of the inelastic hinge nodes i or j at both ends of the structural member is: in, and They represent the plastic rotation state of the inelastic hinge node i or j at the current time t and the time before the unit time increment, respectively.

4. The real-time evaluation method for the evolution of high-low cycle combined fatigue damage of a steel structure according to claim 1 is characterized in that: In the step C, a full-life fatigue model of the rod unit-inelastic hinge node of the steel structure is established, boundary conditions, attribute constant parameters and analysis steps are set according to the actual loading process, and the real-time analysis of the whole process of crack evolution of the inelastic hinge node of the structure is realized by constructing control equations such as elastic-plastic damage constitutive equations; (1) Boundary condition settings include node displacement constraints and loading time history. The horizontal and vertical translational degrees of freedom are constrained on the model boundary nodes. Displacement time histories of different amplitudes are applied to the loading nodes to simulate full-life fatigue loading. (2) Constant parameters of high-cycle fatigue properties of steel structures include: high-cycle fatigue base number M of node crack incubation period cr and high cycle fatigue index γ, as well as the damage coefficient Q and index R during crack propagation; the low cycle fatigue property constants are set as: node critical cracking plastic rotation Low cycle fatigue index β and crack closure factor h when the node is under compression — ; (3) Establish the global coordinate system and the global coordinates of each node, define the state variables of the rod unit and the node, and establish the functional relationship between the relevant variables; (4) Set different analysis steps and determine whether the current analysis step is high-cycle fatigue loading or low-cycle fatigue loading by the time increment Delta. When Delta is less than 1.0, the analysis step is low-cycle fatigue loading; otherwise, the analysis step is high-cycle fatigue loading. (5) Through the iterative analysis of the full-life fatigue model of the steel structure, the instantaneous generalized stress amplitude, instantaneous energy release rate amplitude, and instantaneous plastic rotation amplitude of the key state variables of the inelastic hinge node are calculated in real time, and the high-cycle fatigue and low-cycle fatigue damage factors are further obtained. At the same time, the elastic-plastic damage constitutive equation of the steel structure for the next incremental step model analysis is updated to realize the real-time evaluation of the high-low cycle composite fatigue damage evolution process of the steel structure.

Citation Information

Cited By

  • High-cycle fatigue strength evaluation method based on damage influence

    CN120651683A