Synthesis method of corn protein powder zymolyte chelated zinc
Through gelatinization, saccharification and enzymatic hydrolysis of corn gluten meal, combined with zinc sulfate for chelation reaction, the problem of low zinc content and chelation rate of corn gluten hydrolysis method in the existing technology is solved, and efficient and safe corn gluten is obtained. Powder enzymatic hydrolyzate chelated zinc product improves the zinc absorption efficiency of animals.
Patent Information
- Application Number
- CN202410846046.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-06-21
- Filing Date
- 2024-06-27
- Publication Date
- 2024-10-11
AI Technical Summary
When preparing chelated zinc using the corn protein hydrolysis method in the prior art, the zinc content is low, the chelation rate is low, and the use of strong acid or strong alkali leads to the destruction of amino acids, reducing the nutritional value of corn protein.
Corn gluten powder is used to undergo gelatinization, saccharification, enzymatic hydrolysis, combined with calcium chloride dihydrate and α-amylase treatment, and then undergoes a chelation reaction with zinc sulfate, and a solid powdered corn gluten powder with high chelation rate is obtained through spray drying. Enzymatic hydrolyzate chelated zinc product.
Achieved the production of chelated zinc from corn gluten meal enzymatic hydrolyzate with high chelation rate (≥95%), avoided the use of harmful solvents, increased the metal content of the product (≥15%), enhanced the zinc absorption efficiency of animals, and was safe. Environmental friendly.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of chelated zinc processing, in particular to a method for synthesizing chelated zinc of corn protein powder enzymatic hydrolysate. Background Art
[0002] Zinc is an essential trace element for animals. Zinc plays a variety of important physiological functions in animals and is essential for their health and growth and development. In addition, zinc is involved in the composition and activity of a variety of enzymes in animals, which play an important role in cell metabolism. For example, zinc is a component or enzyme activator of many metalloenzymes, such as dehydrogenase and carbonic anhydrase, which play a key role in tissue respiration and material metabolism. Therefore, zinc plays a vital role in enzyme activity, growth and development, reproductive function, and immune response in animals.
[0003] The zinc content of animals can be increased by adding zinc to feed to promote their growth and development and improve production efficiency. Inorganic zinc or organic zinc can be added to feed.
[0004] Inorganic zinc sources: Commonly used inorganic zinc sources include zinc sulfate (ZnSO4) and zinc oxide. Zinc sulfate is the most common zinc source with high bioavailability and low cost. Zinc oxide can be used at higher concentrations (up to 1600 mg / kg) in specific stages (such as the first two weeks after weaning of piglets).
[0005] Organic zinc sources: Organic zinc sources such as zinc methionine chelate and zinc glycinate chelate have significantly higher liver deposition and less impact on other minerals such as manganese and copper.
[0006] The bioavailability of organic zinc is higher than that of inorganic zinc. Adding organic zinc to animal feed can significantly improve the production performance of animals. For example, in the study of production performance and egg quality of laying hens in the later stage of egg production, adding organic zinc has more advantages than inorganic zinc.
[0007] Corn gluten meal is a by-product of corn kernels after starch is extracted. It is composed of corn protein, is rich in protein, and also contains a small amount of starch and fiber. It has a special taste and color. It can be used as a raw material for protein feed. It has obvious resource advantages and high feeding value. Therefore, it can be used to replace soybean meal, fish meal and other protein feeds in the feed market where soybean meal and fish meal are in short supply.
[0008] Since the protein in corn protein powder is a large molecular protein, the internal groups are stably bound to each other and cannot directly combine with zinc to form a chelate. In order to produce corn protein chelated zinc, the corn protein must first be hydrolyzed or enzymatically hydrolyzed to convert the corn protein into small peptides or amino acids, and then reacted with zinc to produce a chelate.
[0009] The hydrolysis method usually uses strong acid (sulfuric acid or hydrochloric acid) or strong alkali (sodium hydroxide or potassium hydroxide) to break the chemical bonds between amino acids in the protein under high temperature and high pressure conditions. However, in this process, some amino acids are usually destroyed, resulting in a decrease in the original nutritional value of corn protein.
[0010] At present, there are technologies for preparing chelated zinc products by reacting corn protein hydrolysate with zinc chloride, and there are technologies for preparing chelated zinc products by reacting soybean corn protein hydrolysate with zinc sulfate. However, the products obtained by such methods have disadvantages such as low zinc content and low chelation rate. Summary of the invention
[0011] The purpose of the present invention is to provide a method for synthesizing corn gluten meal enzymatic hydrolysate chelated zinc in view of the problems existing in the current prior art. In the method, corn gluten meal is gelatinized, saccharified and enzymatically hydrolyzed to obtain corn gluten meal enzymatic hydrolysate, which is subjected to chelation reaction with zinc to produce protein zinc product which can be used as feed additive, provide zinc and amino acids for animals, and promote the healthy growth of animals.
[0012] In order to achieve the above invention object, the technical solution of the present invention is as follows:
[0013] A method for synthesizing corn protein meal enzymatic hydrolysate chelated zinc comprises the following steps:
[0014] 1) Corn gluten powder starch gelatinization
[0015] The corn gluten powder is placed in a container, and then water is added to the corn gluten powder and stirred evenly, and then the pH is adjusted and the temperature is increased to react, and during this process, calcium chloride dihydrate and α-amylase are added, and the reaction is carried out for more than 4 hours (specifically 4-12 hours) to gelatinize the corn gluten powder starch;
[0016] 2) Corn gluten meal starch saccharification
[0017] After the corn gluten powder starch is completely gelatinized in step 1), the pH and temperature are adjusted, and the reaction is stirred for more than 4 hours (specifically 4-12 hours) to perform saccharification of the corn gluten powder starch;
[0018] 3) Enzymatic hydrolysis of corn protein
[0019] After saccharification is complete, the pH is adjusted and alcalase protease is added for enzymatic hydrolysis;
[0020] 4) Corn protein chelates metal elements
[0021] After the enzymatic hydrolysis is completed, zinc sulfate monohydrate or zinc sulfate heptahydrate is continuously added to the container, the pH is adjusted to carry out a chelating reaction, and the protein zinc solution is collected and spray-dried to obtain a solid powdery corn protein powder enzymatic hydrolyzate chelated zinc product (referred to as protein zinc).
[0022] As a better embodiment of the present application, in step 1) of the synthesis method of corn protein meal enzymatic hydrolysate chelated zinc, the relationship between the mass g of corn protein meal and the volume L of water is 100-200:1; the pH is adjusted to 5-6, the temperature is raised to 100±5°C, and the reaction is carried out at this temperature for 1 hour.
[0023] As a better embodiment of the present application, in step 1) of the synthesis method of corn gluten meal enzymatic hydrolyzate chelated zinc, the addition amount of calcium chloride dihydrate is 0.1%-0.2% of the corn gluten meal; the addition amount of α-amylase is 0.5-1% of the corn gluten meal.
[0024] As a better embodiment of the present application, in step 2) of the method for synthesizing corn protein meal enzymatic hydrolysate chelated zinc, 1+1 hydrochloric acid is used to adjust the pH to 4.0-4.5, and the temperature is 60±5°C.
[0025] As a better embodiment of the present application, in step 3) of the method for synthesizing chelated zinc from corn protein powder enzymatic hydrolysate, sodium hydroxide solution is used to adjust the pH to 8-9; the concentration of the sodium hydroxide solution is 5 mol / L; the amount of alcalase protease added is 0.1%-0.2% of the raw corn protein powder; the pH continues to decrease during the reaction, and 1 mol / L sodium hydroxide solution is added at any time to maintain the pH at 8-9, and the total reaction time is 2-6 hours, more preferably 4 hours.
[0026] As a better embodiment of the present application, in step 4) of the method for synthesizing corn protein powder enzymatic hydrolyzate chelated zinc, before adding zinc sulfate monohydrate, the enzymatic protein solution needs to be heated and stirred to 55±5°C, and the pH value is adjusted to 8±0.5; the amount of zinc sulfate monohydrate added is 75-80:100 based on the raw material corn protein powder.
[0027] As a better embodiment of the present application, in step 4) of the method for synthesizing chelated zinc from corn protein meal enzymatic hydrolysate, after the zinc sulfate monohydrate is added, it is necessary to stir evenly and keep the temperature at 60°C±5°C for 1-2h, more preferably 90min, and adjust the pH to 6-7 with 5mol / L sodium hydroxide solution during the process.
[0028] As a better embodiment of the present application, in step 4) of the method for synthesizing a corn protein powder enzymatic hydrolysate chelated zinc, the spray drying conditions are: setting the inlet temperature at 170-180°C, adjusting the feed rate, controlling the outlet temperature at 50-60°C, and controlling the moisture content of the finished product to ≤10%.
[0029] The present application also protects the corn protein meal enzymatic hydrolysate chelated zinc which can be synthesized by using any of the above methods or a combination of method steps.
[0030] Another invention objective of the present application is to protect the use of the above-mentioned corn protein meal enzymatic hydrolysate chelated zinc in animal feed additives.
[0031] Compared with the prior art, the present invention has the following beneficial effects:
[0032] (I) The raw material is corn protein powder, which has a wide source and low cost. It adopts a wet reaction method, has a sufficient reaction, and a high chelation rate (≥95%). The synthesis process does not involve organic solvents such as ethanol and ether, which is safe and environmentally friendly.
[0033] (II) Excessive chloride ion will have a serious impact on pigs. Excessive chloride ion will cause excessive metabolic burden on pigs, thereby inducing a variety of diseases, including gastrointestinal diseases and osteoporosis. At the same time, when chloride ion is >700mg / L in circulating water for a long time, it has extremely high polarity and promotes corrosion reaction. It also has strong penetrability and can easily penetrate the protective film on the metal surface, causing crevice corrosion and pitting corrosion. In particular, it causes cracking and great harm to austenitic stainless steel, which can make production equipment scrapped in a short period of time. Therefore, this method uses safer sulfate as a zinc source to produce feed additives. The product obtained by this method has a higher metal content (≥15%), which can reduce the amount of additives used to achieve the same zinc supplementation effect.
[0034] (III) This method moderately enzymatically hydrolyzes corn protein powder, and most of the enzymatic hydrolysis products are small peptides, and a small part are amino acids. The enzymatic hydrolysis products can fully react with zinc element to generate chelated zinc products.
[0035] (iv) In the present application, the enzymatic hydrolysis products of corn gluten powder are not separated, but all react with zinc, so that the product components are diversified, which promotes faster absorption by animals. DETAILED DESCRIPTION
[0036] All features disclosed in this specification, or steps in all methods or processes disclosed, except mutually exclusive features and / or steps, can be combined in any manner.
[0037] Any feature disclosed in this specification (including claims and abstract), unless otherwise stated, may be replaced by other equivalent or alternative features having similar purposes. That is, unless otherwise stated, each feature is only an example of a series of equivalent or similar features.
[0038] The features and performance of the present invention are further described in detail below in conjunction with the embodiments.
[0039] Embodiment 1:
[0040] A method for synthesizing corn protein meal enzymatic hydrolysate chelated zinc comprises the following steps:
[0041] 1) Corn gluten powder starch gelatinization
[0042] Add 1 L of deionized water and 100 g of corn gluten powder to a 2 L container, place in a magnetic stirrer, and stir evenly.
[0043] Adjust the pH to about 5.5, raise the temperature to 100°C, keep warm for 1 hour, add 0.1 g of calcium chloride dihydrate, add 0.5 g of α-amylase, and react for 4 hours.
[0044] 2) Corn gluten meal starch saccharification
[0045] After detecting the absence of starch with iodine solution, add 1+1 hydrochloric acid to adjust the pH to 4..2, control the reaction temperature to 60°C, start stirring, and react for 6 hours.
[0046] 3) Enzymatic hydrolysis of corn protein
[0047] After the saccharification is complete as detected by the kit, 5 mol / L sodium hydroxide solution is added to adjust the pH to about 8.5, and 0.2 g of alcalase protease (commercially available product) is added. As the reaction proceeds, the pH continues to decrease, and 1 mol / L sodium hydroxide solution is added at any time to maintain the pH at about 8.5. The reaction is carried out for 4 hours to obtain an enzymatic protein solution.
[0048] 4) Corn protein chelates metal elements
[0049] Heat and stir the enzymatic protein solution to 55°C, pH 7.88, slowly add 75.7 g of zinc sulfate monohydrate, stir evenly, maintain the temperature at 60°C for 120 minutes, adjust the pH to 6.21 with 5 mol / L sodium hydroxide solution during the process, collect the protein zinc solution and wait for spray drying.
[0050] 5) Spray drying: set the inlet temperature to 170° C., adjust the feed rate to 400 ml / h, and control the outlet temperature to 55° C. to obtain a solid powdered corn protein meal enzymatic hydrolysate chelated zinc product.
[0051] Embodiment 2:
[0052] A method for synthesizing corn protein meal enzymatic hydrolysate chelated zinc comprises the following steps:
[0053] 1) Corn gluten powder starch gelatinization
[0054] Add 1 L of deionized water and 150 g of corn gluten powder to a 2 L beaker, place in a magnetic stirrer and stir.
[0055] The pH was adjusted to about 5.5, the temperature was raised to 100°C, kept warm for 1 hour, 0.2 g of calcium chloride dihydrate and 0.8 g of α-amylase were added, and the reaction was continued for 6 hours.
[0056] 2) Corn gluten meal starch saccharification
[0057] After detecting the absence of starch with iodine solution, add 1+1 hydrochloric acid to adjust the pH to 4.3, the temperature to 60°C, start stirring, and react for 4 hours.
[0058] 3) Enzymatic hydrolysis of corn protein
[0059] After the saccharification is complete as detected by the kit, 5 mol / L sodium hydroxide solution is added to adjust the pH to about 8.5, and 0.2 g of alcalase protease is added. As the reaction proceeds, the pH continues to decrease, and 1 mol / L sodium hydroxide solution is added at any time to maintain the pH at about 8.5. The reaction is continued for 4 hours to obtain an enzymatic protein solution.
[0060] 4) Corn protein chelates metal elements
[0061] Heat and stir the enzymatic protein solution to 55°C, pH 7.88, slowly add 172 g of zinc sulfate heptahydrate, stir evenly, maintain the temperature at 65°C for 90 minutes, adjust the pH to 6.21 with 5 mol / L sodium hydroxide solution during the process, collect the protein zinc solution and wait for spray drying.
[0062] 5) Spray drying: set the inlet temperature to 175° C., adjust the feed rate to 450 ml / h, and control the outlet temperature to 56° C. to obtain a solid powdered corn protein meal enzymatic hydrolysate chelated zinc product.
[0063] Embodiment 3:
[0064] A method for synthesizing corn protein meal enzymatic hydrolysate chelated zinc comprises the following steps:
[0065] 1) Corn gluten powder starch gelatinization
[0066] Add 1 L of deionized water and 180 g of corn gluten powder to a 2 L beaker, place in a magnetic stirrer and stir.
[0067] The pH was adjusted to 5.5, the temperature was raised to 100°C, kept warm for 1 hour, 0.1 g of calcium chloride dihydrate and 0.5 g of α-amylase were added, and the reaction was continued for 8 hours.
[0068] 2) Corn gluten meal starch saccharification
[0069] After detecting the absence of starch with iodine solution, add 1+1 hydrochloric acid to adjust the pH to 4.2, the temperature to 60°C, start stirring, and react for 8 hours.
[0070] 3) Enzymatic hydrolysis of corn protein
[0071] After the saccharification is complete as detected by the kit, 5 mol / L sodium hydroxide solution is added to adjust the pH to 8.5, and 0.2 g of alcalase protease is added. As the reaction proceeds, the pH continues to decrease, and 1 mol / L sodium hydroxide solution is added at any time to maintain the pH at around 8.5. The reaction is continued for 4 hours to obtain an enzymatic protein solution.
[0072] 4) Corn protein chelates metal elements
[0073] Heat and stir the enzymatic protein solution to 55°C, pH 7.82, slowly add 136.26 g of zinc sulfate monohydrate, stir evenly, maintain the temperature at 62°C for 100 min, adjust the pH to 6.21 with 5 mol / L sodium hydroxide solution during the process, collect the protein zinc solution and wait for spray drying.
[0074] 5) Spray drying: set the inlet temperature to 180° C., adjust the feed rate to 500 ml / h, and control the outlet temperature to 58° C. to obtain a solid powdered corn protein meal enzymatic hydrolysate chelated zinc product.
[0075] Comparative Example 1: Direct Chelation Reaction
[0076] Weigh 100g corn protein powder into a beaker, add 1L of water, stir evenly and heat to 60°C, slowly add 80g of zinc sulfate monohydrate, stir evenly, keep the temperature at about 60°C and react for 60min, collect the corn protein chelated zinc slurry, and obtain the product by spray drying.
[0077] Comparative Example 2: Direct enzymatic hydrolysis without starch hydrolysis
[0078] 1) Weigh 100g corn gluten powder into a beaker, add 1L of water, stir evenly, heat to 60°C, and slowly add 5mol / L sodium hydroxide solution to adjust the pH to 9.0.
[0079] 2) Weigh 0.2 g of alcalase (2‰ corn protein) into a beaker, stir for enzymatic reaction, pH value slowly decreases, add 1 mol / L sodium hydroxide solution to maintain pH=8.5, and enzymatic reaction for 1 hour. The end point pH value is 7.60.
[0080] 3) Heat and stir the enzymatic protein solution to 55° C., pH 7.81, slowly add 80 g of zinc sulfate monohydrate, stir evenly, the pH value drops to 4.83, keep the temperature at about 60° C. and react for 60 min, the end point pH is 4.95, collect the corn protein chelated zinc slurry, and obtain the product by spray drying.
[0081] Comparative Example 3: Direct enzymatic hydrolysis without hydrolyzing starch
[0082] 1) Weigh 100g corn protein powder into a beaker, add 1L of water, stir evenly and heat to 60°C, pH value is 3.78, the solution is bright yellow, slowly add 5mol / L sodium hydroxide solution to adjust the pH to 9.0.
[0083] 2) Weigh 0.2g of alcalase (2‰ corn protein) into a beaker, stir for enzymatic reaction, pH value slowly decreases, add 1mol / L sodium hydroxide solution to maintain pH=8.5, and enzymatic reaction for 1h. The end point pH value is 7.95.
[0084] 3) Heat and stir the enzymatic protein solution to 55° C., pH 7.81, slowly add 80 g of zinc sulfate monohydrate, stir evenly, the pH value drops to 5.26, adjust the pH to about 5.5 with 1 mol / L sodium hydroxide solution, maintain the temperature at about 60° C. for 60 min, the end point pH is 5.54, collect the zein chelated zinc slurry, and obtain the product by spray drying.
[0085] Comparative Example 4:
[0086] A method for synthesizing corn protein meal enzymatic hydrolysate chelated zinc comprises the following steps:
[0087] 1) Corn gluten powder starch gelatinization
[0088] Add 1 L of deionized water and 150 g of corn gluten powder to a 2 L beaker, place in a magnetic stirrer and stir.
[0089] The pH was adjusted to 5.5, the temperature was raised to 100°C, kept warm for 1 hour, 0.1 g of calcium chloride dihydrate and 0.5 g of α-amylase were added, and the reaction was continued for 6 hours.
[0090] 2) Corn gluten meal starch saccharification
[0091] After detecting the absence of starch with iodine solution, add 1+1 hydrochloric acid to adjust the pH to 4.2, the temperature to 60°C, start stirring, and react for 6 hours.
[0092] 3) Enzymatic hydrolysis of corn protein
[0093] After the saccharification is complete as detected by the kit, 5 mol / L sodium hydroxide solution is added to adjust the pH to 8.5, and 0.2 g of alcalase protease is added. As the reaction proceeds, the pH continues to decrease, and 1 mol / L sodium hydroxide solution is added at any time to maintain the pH at around 8.5. The reaction is continued for 4 hours to obtain an enzymatic protein solution.
[0094] 4) Corn protein chelates metal elements
[0095] Heat and stir the enzymatic protein solution to 55°C, pH 7.82, slowly add 51.50 g of zinc oxide, stir evenly, maintain the temperature at 62°C for 120 min, there is a large amount of precipitate in the solution, the reaction is not obvious, collect the protein zinc solution and insoluble matter and spray dry.
[0096] 5) Spray drying: set the inlet temperature to 180° C., adjust the feed rate to 500 ml / h, and control the outlet temperature to 58° C. to obtain a solid powdered corn protein meal enzymatic hydrolysate chelated zinc product.
[0097] The protein zinc obtained in Examples 1 to 3 and the product obtained in the comparative example were tested. The specific test results are shown in Table 1:
[0098] Table 1: Detection data of protein zinc in each embodiment
[0099] Zinc -% Free zinc -% Chelation rate-% protein-% Example 1 15.70 0.16 98.98 30.35 Example 2 15.60 0.47 96.99 31.00 Example 3 15.10 0.50 96.69 31.28 Comparative Example 1 15.5 10.6 31.61 22.94 Comparative Example 2 17.2 5.6 67.44 26.94 Comparative Example 3 14.5 1.2 91.72 32.01 Comparative Example 4 14.88 14.26 4.16 34.22
[0100] The above-mentioned embodiments only express the specific implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the protection scope of the present application. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the technical solution concept of the present application, and these all belong to the protection scope of the present application.
[0101] This background section is provided to generally present the context of the invention, and the work of the presently named inventors, the work to the extent described in this background section, and aspects of this section that did not constitute prior art at the time of application are neither explicitly nor implicitly admitted to be prior art to the present invention.
Claims
1. A method for synthesizing chelated zinc from corn protein meal enzymatic hydrolysate, characterized in that The following steps are involved: 1) Corn gluten powder starch gelatinization The corn gluten powder is placed in a container, and then water is added to the corn gluten powder and stirred evenly, and then the pH is adjusted and the temperature is increased to react, and during this process, calcium chloride dihydrate and α-amylase are added, and the reaction is carried out for more than 4 hours to gelatinize the corn gluten powder starch; 2) Corn gluten meal starch saccharification After the corn gluten powder starch is completely gelatinized in step 1), the pH and temperature are adjusted, and the reaction is stirred for more than 4 hours to perform saccharification of the corn gluten powder starch; 3) Enzymatic hydrolysis of corn protein After saccharification is complete, the pH is adjusted and alcalase protease is added for enzymatic hydrolysis; 4) Corn protein chelates metal elements After the enzymatic hydrolysis is completed, zinc sulfate monohydrate or zinc sulfate heptahydrate is continuously added to the container, the pH is adjusted to carry out a chelating reaction, and the protein zinc solution is collected and spray-dried to obtain a solid powdery corn protein powder enzymatic hydrolyzate chelated zinc product.
2. The method for synthesizing chelated zinc from corn gluten meal enzymolysate according to claim 1, characterized in that: In step 1), the relationship between the mass g of corn protein powder and the volume L of water is 100-200:1; the pH is adjusted to 5-6, the temperature is raised to 100±5°C, and the reaction is carried out at this temperature for 1 hour.
3. The method for synthesizing chelated zinc from corn gluten meal enzymolysate according to claim 1, characterized in that: In step 1), the addition amount of calcium chloride dihydrate is 0.1% to 0.2% of the corn gluten meal; the addition amount of α-amylase is 0.5% to 1% of the corn gluten meal.
4. The method for synthesizing chelated zinc from corn gluten meal enzymolysate according to claim 1, characterized in that: In step 2), 1+1 hydrochloric acid is used to adjust the pH to 4.0-4.5, and the temperature is 60±5°C.
5. The method for synthesizing chelated zinc from corn gluten meal enzymolysate according to claim 1, characterized in that: In step 3), sodium hydroxide solution is used to adjust the pH to 8-9; the concentration of the sodium hydroxide solution is 5 mol / L; the amount of alcalase protease added is 0.1%-0.2% of the raw corn protein powder; the pH value continues to decrease during the reaction, and 1 mol / L sodium hydroxide solution is added at any time to maintain the pH value at 8-9, and the total reaction time is 2-6 hours.
6. The method for synthesizing chelated zinc from corn gluten meal enzymolysate according to claim 1, characterized in that: In step 4), before adding zinc sulfate monohydrate, the enzymatic protein solution needs to be heated and stirred to 55±5° C., and the pH value is adjusted to 8±0.5; the amount of zinc sulfate monohydrate added is 75-80:100 based on the raw material corn protein powder.
7. The method for synthesizing chelated zinc from corn gluten meal enzymolysate according to claim 1, characterized in that In step 4), after the zinc sulfate monohydrate is added, it is necessary to stir evenly and keep the temperature at 60°C ± 5°C for 1 to 2 hours. During the process, the pH is adjusted to 6-7 with 5 mol / L sodium hydroxide solution.
8. The method for synthesizing chelated zinc from corn gluten meal enzymolysate according to claim 1, characterized in that: The spray drying conditions in step 4) are: setting the inlet temperature at 170-180°C, adjusting the feed rate, controlling the outlet temperature at 50-60°C, and controlling the moisture content of the finished product to ≤10%.
9. The corn gluten meal enzymatic hydrolysate chelated zinc synthesized according to any one of claims 1 to 8.
10. Use of the corn protein meal enzymolysate chelated zinc according to claim 9 in animal feed additives.