Arsenic removal process for producing 105% polyphosphoric acid from phosphoric acid by hot method
Through a two-step arsenic removal process, polyvinylpyrrolidone and phosphorus pentasulfide are used to prepare arsenic removal agent solution and microspheres, which successfully reduces the arsenic content in thermal phosphoric acid, solves the problem of difficulty in reducing arsenic content in the existing technology, and meets the requirements of high-end arsenic removal. Purity phosphoric acid has strict requirements on arsenic content, which improves product quality and filtration efficiency.
Patent Information
- Application Number
- CN202410991049.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-23
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-07-23
AI Technical Summary
In the existing thermal phosphoric acid production, it is difficult to reduce the arsenic content in 105% polyphosphoric acid to below 0.5PPM, which affects the quality of downstream products, especially the needs of lithium hexafluorophosphate electrolyte, drug synthesis, electronics and food industries.
A two-step arsenic removal process is adopted. First, arsenic removal agent solution is prepared from polyvinylpyrrolidone and phosphorus pentasulfide. Then, arsenic removal agent microspheres are prepared. The arsenic content is reduced through the primary and secondary arsenic removal processes and passed through a plate and frame filter press and Oxidation treatment yields low arsenic 105% polyphosphoric acid.
It has successfully reduced the arsenic content in thermal phosphoric acid to less than 0.5PPM, meeting the strict requirements of lithium hexafluorophosphate electrolyte, drug synthesis, electronics and food industries, improving the clarity and transparency of the product, and reducing the difficulty of filtration.
Smart Images

Figure BDA0004958887050000091
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of phosphoric acid production, and in particular to a dearsenicating process for producing 105% polyphosphoric acid by thermal phosphoric acid. Background Art
[0002] Arsenic belongs to the nitrogen family in the periodic table. In 105% polyphosphoric acid, due to its high density, high viscosity and dense chain length, elemental arsenic is the most difficult to remove. There is no consensus on the form of arsenic in thermal phosphoric acid, but elemental arsenic, as a primary poison, is highly toxic, and its compounds arsenic trisulfide and arsenic pentasulfide are even more toxic. The arsenic content has a great impact on the quality of downstream products. The higher the content, the worse the quality of downstream products. At present, the arsenic content of 105% polyphosphoric acid produced by domestic fine phosphorus chemical companies using thermal process in accordance with industry standards is maintained between 50PPM and 100PPM. 105% polyphosphoric acid is mainly used in special industries such as lithium hexafluorophosphate electrolyte, drug synthesis, electronics, and food, and its requirements for arsenic are more stringent, generally requiring it to be below 0.5PPM.
[0003] At present, the arsenic removal methods of polyphosphoric acid mainly include the low-arsenic method of raw yellow phosphorus and the arsenic removal method of arsenic removal agent. Among them, in the low-arsenic method of raw yellow phosphorus, the arsenic content of 105% polyphosphoric acid produced by thermal method mainly comes from raw yellow phosphorus. In my country, the main yellow phosphorus manufacturers are concentrated in Yunnan, Guizhou, Sichuan and other provinces. The phosphate mines in these provinces have different origins and arsenic contents, and the arsenic content of the produced yellow phosphorus is also different; according to the national standard yellow phosphorus quality analysis report, the arsenic content of yellow phosphorus in Yunnan is between 130PPM and 200PPM, the arsenic content of yellow phosphorus in Guizhou is between 310PPM and 450PPM, and the arsenic content of yellow phosphorus in Sichuan is between 250PPM and 380PPM; according to actual production experience, the recovery rate of 105% polyphosphoric acid is calculated as 2.944, and the arsenic content of 105% polyphosphoric acid produced by yellow phosphorus in most production areas does not meet the food-grade low-arsenic 105% polyphosphoric acid standard. If the arsenic is reduced by the low-arsenic method of raw yellow phosphorus, the arsenic content of the phosphate rock resources used to produce yellow phosphorus is required to be less than 0.001%. However, due to the limitation of national phosphate rock resources, no yellow phosphorus manufacturer in China has reduced the arsenic content of arsenic yellow phosphorus through technical transformation and other production means. In the arsenic removal method, the arsenic removal agent mainly includes sulfide, etc. However, due to the characteristics of high density, high viscosity, and dense chain length of polyphosphoric acid, the arsenic removal reaction is not completely removed by directly adding sulfide as the arsenic removal agent, and the subsequent filtration process is difficult, the filtration time is too long, and the finished product is not clear and transparent, which affects the product quality. Summary of the invention
[0004] The purpose of the present invention is to solve the above problems existing in the prior art and provide a dearsenicization process for producing 105% polyphosphoric acid by thermal phosphoric acid. The dearsenicization process of the present invention can reduce the arsenic content in the 105% polyphosphoric acid produced by thermal method to less than 0.5PPM. The low-arsenic 105% polyphosphoric acid of the present invention can meet the needs of special industries such as lithium hexafluorophosphate electrolyte, drug synthesis, electronics, food, etc. in the domestic and foreign markets.
[0005] In order to achieve the above object, the technical solution of the present invention is as follows:
[0006] The arsenic removal process for producing 105% polyphosphoric acid by thermal phosphoric acid comprises the following steps:
[0007] (1) Preparation of arsenic removal agent solution: adding polyvinyl pyrrolidone to water and mixing evenly, then adding phosphorus pentasulfide and mixing evenly to obtain a arsenic removal agent solution, wherein the mass ratio of polyvinyl pyrrolidone, phosphorus pentasulfide and water is 0.01-0.05:2-3:10;
[0008] (2) Primary arsenic removal: 107% polyphosphoric acid is injected into a arsenic removal reaction tower, and then the prepared arsenic removal agent solution is added into the arsenic removal reaction tower for arsenic removal reaction, wherein the amount of the arsenic removal agent solution added is 3-4 L / ton of polyphosphoric acid;
[0009] (3) Preparation of arsenic removal agent microspheres: sodium hydroxide is added to water to dissolve to obtain a mixed solution, metakaolin and rice bran are added to the mixed solution and mixed evenly to obtain a suspension; white oil is heated to 80-90° C. and stirred, and the suspension is dropped into the white oil while stirring to obtain a mixture; the temperature of the mixture is controlled to 60-70° C., and allowed to stand for 1-2 hours, filtered, and the filter residue is washed with boiling water, dried, roasted, and sieved to obtain arsenic removal agent microspheres;
[0010] (4) Secondary arsenic removal: the temperature of the polyphosphoric acid after the primary arsenic removal in step (2) is controlled at 85-95° C., the arsenic removal agent microspheres prepared in step (3) are added, and the reaction is stirred at a speed of 100-150 rpm for 20-40 min;
[0011] (5) Filtration: The polyphosphoric acid after the secondary arsenic removal in step (4) is filtered through a plate and frame filter press, and the filtrate is collected. Compressed air is introduced into the filtrate for aeration, oxidation, and blowing. Then, process water is added to adjust the acid concentration to 105% to obtain arsenic-free 105% polyphosphoric acid, wherein the element arsenic content of the arsenic-free 105% polyphosphoric acid is less than 0.5 PPM.
[0012] Furthermore, in step (2), the conditions of the dearsenicization reaction are controlled as follows: the reaction temperature is 95-110° C., the reaction time is 1-3 h, and the stirring speed is 70-80 rpm.
[0013] Furthermore, in step (3), the mass ratio of sodium hydroxide, water, metakaolin and rice bran is 0.5-3:5-10:0.5-1:0.1-0.5.
[0014] Furthermore, in step (3), the stirring speed is 350-400 rpm; the roasting temperature is 350-450° C., the roasting time is 3-5 h; and the sieving mesh size is 60-80 mesh.
[0015] Furthermore, in step (3), the amount of the suspension added is 0.5-1 times the volume of the white oil.
[0016] Furthermore, in step (3), the white oil is No. 100 white oil.
[0017] Furthermore, in step (4), the amount of the arsenic removal agent microspheres added is 0.1-0.3 times the weight of the polyphosphoric acid.
[0018] Furthermore, in step (5), hydrogen sulfide gas is continuously released during the aeration process of the filtrate, and the released hydrogen sulfide gas is introduced into the exhaust fan pipeline. Under the action of the exhaust fan, the hydrogen sulfide gas is sent to the hydrogen sulfide absorption tower, sprayed with industrial phosphoric acid for absorption, and then discharged into the atmosphere through the exhaust pipe after washing in the alkaline washing tower.
[0019] The beneficial effects of the present invention are as follows:
[0020] The arsenic removal process of the present invention can reduce the arsenic content in 105% polyphosphoric acid produced by a thermal method to less than 0.5 PPM. The low-arsenic 105% polyphosphoric acid obtained after arsenic removal can meet the needs of special industries such as lithium hexafluorophosphate electrolyte, drug synthesis, electronics, and food in the domestic and foreign markets, and can better serve the society.
[0021] The present invention is a two-step arsenic removal method. In the first arsenic removal, a arsenic removal agent solution is first prepared, and phosphorus pentasulfide and polyvinyl pyrrolidone are used to prepare a liquid arsenic removal agent. The phosphorus pentasulfide liquid arsenic removal agent can decompose and heat the arsenic element of orthophosphoric acid in polyphosphoric acid, and hydrogen sulfide can react and precipitate with the arsenic element better, and polyvinyl pyrrolidone plays an auxiliary role in arsenic removal; in the second arsenic removal, arsenic removal agent microspheres are first prepared, and then the polyphosphoric acid after the first arsenic removal is further treated with the arsenic removal agent microspheres, so that the purpose of thorough arsenic removal and a final arsenic content of less than 0.5 PPM can be achieved. At the same time, since the arsenic removal agent microspheres are used for treatment in the early stage, they play a filtering aid role in the subsequent filtration, reduce the filtration difficulty of the filtration section, shorten the filtration time, and the chromaticity of the finished product is low, clear and transparent, and the product quality is effectively improved. DETAILED DESCRIPTION
[0022] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with embodiments.
[0023] Example 1
[0024] The arsenic removal process for producing 105% polyphosphoric acid by thermal phosphoric acid comprises the following steps:
[0025] (1) Preparation of arsenic removal agent solution: polyvinyl pyrrolidone with a molecular weight of 10,000 is added to water and mixed evenly, and then phosphorus pentasulfide is added and mixed evenly to obtain a arsenic removal agent solution, wherein the mass ratio of polyvinyl pyrrolidone, phosphorus pentasulfide and water is 0.02:2.5:10.
[0026] (2) Primary arsenic removal: After the concentration of industrial phosphoric acid is increased to 107% polyphosphoric acid in the phosphorus burning process, the 107% polyphosphoric acid is pumped into the arsenic removal reaction tower through a circulating acid pump, and then the prepared arsenic removal agent solution is added to the arsenic removal reaction tower through a metering pump for arsenic removal reaction. The amount of the arsenic removal agent solution added is 3.5 L / ton of polyphosphoric acid, and the conditions of the arsenic removal reaction are controlled as follows: the reaction temperature is 105° C., the reaction time is 2 h, and the stirring speed is 75 rpm.
[0027] (3) Preparation of arsenic removal agent microspheres: Sodium hydroxide is added to water and dissolved to obtain a mixed solution, and kaolin and 100-mesh rice bran are added to the mixed solution and mixed evenly to obtain a suspension, wherein the mass ratio of the sodium hydroxide, water, kaolin and rice bran is 1:8:0.7:0.3; No. 100 white oil is heated to 85°C and stirred at a speed of 400 rpm, and the suspension is dripped into the No. 100 white oil while stirring, wherein the dripping volume of the suspension is 0.6 times the volume of the white oil, to obtain a mixture; the temperature of the mixture is controlled to be 65°C and allowed to stand for 1.5 hours, filtered, and the filter residue is washed twice with boiling water, dried, and then roasted at 400°C for 4 hours, and passed through an 80-mesh sieve to obtain arsenic removal agent microspheres.
[0028] (4) Secondary arsenic removal: The temperature of the polyphosphoric acid after the primary arsenic removal in step (2) was controlled at 90° C. The arsenic removal agent microspheres prepared in step (3) were added, wherein the weight of the arsenic removal agent microspheres added was 0.2 times that of the polyphosphoric acid, and the reaction was stirred at a speed of 120 rpm for 30 min.
[0029] (5) Filtration: The polyphosphoric acid after the secondary arsenic removal in step (4) is filtered through a plate and frame filter press, and the filtrate after filtration is collected in a collecting tank and finally flows into an acid collecting tank, and compressed air is introduced into the filtrate for aeration, oxidation, and blowing. The filtrate continuously releases hydrogen sulfide gas in the acid collecting tank, and the filtrate gradually becomes clear and transparent, and then process water is added to adjust the acid concentration to 105% to obtain 105% polyphosphoric acid after arsenic removal, which is a colorless, transparent, viscous liquid. Because the arsenic removal agent solution will reduce the concentration of part of the polyphosphoric acid, the concentration of the polyphosphoric acid should be increased to 107% in production to achieve the required concentration. The elemental arsenic content of the 105% polyphosphoric acid after arsenic removal is less than 0.5PPM, and it is pumped into a 100-ton storage tank by a finished product pump; the hydrogen sulfide gas released from the phosphoric acid in the acid collecting tank is introduced into the exhaust fan pipeline, and the hydrogen sulfide gas is sent to the hydrogen sulfide absorption tower under the action of the fan, sprayed with industrial phosphoric acid for absorption, and then washed in the alkali washing tower and discharged into the atmosphere through the exhaust pipe.
[0030] Example 2
[0031] The arsenic removal process for producing 105% polyphosphoric acid by thermal phosphoric acid comprises the following steps:
[0032] (1) Preparation of arsenic removal agent solution: polyvinyl pyrrolidone with a molecular weight of 10,000 is added to water and mixed evenly, and then phosphorus pentasulfide is added and mixed evenly to obtain a arsenic removal agent solution, wherein the mass ratio of polyvinyl pyrrolidone, phosphorus pentasulfide and water is 0.05:2:10.
[0033] (2) Primary arsenic removal: 107% polyphosphoric acid is pumped into a arsenic removal reaction tower through a circulating acid pump via a flow meter, and then the prepared arsenic removal agent solution is added to the arsenic removal reaction tower for arsenic removal reaction. The amount of the arsenic removal agent solution added is 4 L / ton of polyphosphoric acid. The conditions of the arsenic removal reaction are controlled as follows: the reaction temperature is 110° C., the reaction time is 1 h, and the stirring speed is 70 rpm.
[0034] (3) Preparation of arsenic removal agent microspheres: Sodium hydroxide is added to water and dissolved to obtain a mixed solution, and metakaolin and 100-mesh rice bran are added to the mixed solution and mixed evenly to obtain a suspension, wherein the mass ratio of the sodium hydroxide, water, metakaolin and rice bran is 0.5:5:0.5:0.1; No. 100 white oil is heated to 90° C. and stirred at a speed of 350 rpm, and the suspension is dripped into the No. 100 white oil while stirring, wherein the dripping volume of the suspension is 0.5 times the volume of the white oil, to obtain a mixture; the temperature of the mixture is controlled to 70° C. and allowed to stand for 1 hour, filtered, and the filter residue is washed twice with boiling water, dried, and then roasted at 350° C. for 5 hours, and passed through a 60-mesh sieve to obtain arsenic removal agent microspheres.
[0035] (4) Secondary arsenic removal: The temperature of the polyphosphoric acid after the primary arsenic removal in step (2) is controlled at 95° C. The arsenic removal agent microspheres prepared in step (3) are added, wherein the added weight of the arsenic removal agent microspheres is 0.3 times that of the polyphosphoric acid, and the reaction is stirred at a speed of 100 rpm for 40 min.
[0036] (5) Filtration: The polyphosphoric acid after the secondary arsenic removal in step (4) is filtered through a plate and frame filter press, and the filtrate is collected. Compressed air is introduced into the filtrate for aeration, oxidation, and blowing. Then, process water is added to adjust the acid concentration to 105% to obtain arsenic-free 105% polyphosphoric acid, which is a colorless, transparent, viscous liquid. The element arsenic content of the arsenic-free 105% polyphosphoric acid is less than 0.5 PPM.
[0037] Example 3
[0038] The arsenic removal process for producing 105% polyphosphoric acid by thermal phosphoric acid comprises the following steps:
[0039] (1) Preparation of arsenic removal agent solution: polyvinyl pyrrolidone with a molecular weight of 10,000 is added to water and mixed evenly, and then phosphorus pentasulfide is added and mixed evenly to obtain a arsenic removal agent solution, wherein the mass ratio of polyvinyl pyrrolidone, phosphorus pentasulfide and water is 0.01:3:10.
[0040] (2) Primary arsenic removal: 107% polyphosphoric acid is pumped into a arsenic removal reaction tower through a circulating acid pump via a flow meter, and then the prepared arsenic removal agent solution is added to the arsenic removal reaction tower for arsenic removal reaction. The amount of the arsenic removal agent solution added is 3.5 L / ton of polyphosphoric acid. The conditions of the arsenic removal reaction are controlled as follows: the reaction temperature is 95° C., the reaction time is 3 h, and the stirring speed is 80 rpm.
[0041] (3) Preparation of arsenic removal agent microspheres: Sodium hydroxide is added to water and dissolved to obtain a mixed solution, and metakaolin and 100-mesh rice bran are added to the mixed solution and mixed evenly to obtain a suspension, wherein the mass ratio of the sodium hydroxide, water, metakaolin and rice bran is 3:10:1:0.5; No. 100 white oil is heated to 80°C and stirred at a speed of 400 rpm, and the suspension is dripped into the No. 100 white oil while stirring, and the dripping volume of the suspension is 1 times the volume of the white oil to obtain a mixture; the temperature of the mixture is controlled to be 60°C and allowed to stand for 2 hours, filtered, and the filter residue is washed twice with boiling water, dried, and then roasted at 450°C for 3 hours, and passed through an 80-mesh sieve to obtain arsenic removal agent microspheres.
[0042] (4) Secondary arsenic removal: The temperature of the polyphosphoric acid after the primary arsenic removal in step (2) was controlled at 85° C. The arsenic removal agent microspheres prepared in step (3) were added, wherein the weight of the arsenic removal agent microspheres added was 0.1 times that of the polyphosphoric acid, and the reaction was stirred at a speed of 150 rpm for 20 min.
[0043] (5) Filtration: The polyphosphoric acid after the secondary arsenic removal in step (4) is filtered through a plate and frame filter press, and the filtrate is collected. Compressed air is introduced into the filtrate for aeration, oxidation, and blowing. Then, process water is added to adjust the acid concentration to 105% to obtain arsenic-free 105% polyphosphoric acid, which is a colorless, transparent, viscous liquid. The element arsenic content of the arsenic-free 105% polyphosphoric acid is less than 0.5 PPM.
[0044] Example 4
[0045] The arsenic removal process for producing 105% polyphosphoric acid by thermal phosphoric acid comprises the following steps:
[0046] (1) Preparation of arsenic removal agent solution: polyvinyl pyrrolidone with a molecular weight of 10,000 is added to water and mixed evenly, and then phosphorus pentasulfide is added and mixed evenly to obtain a arsenic removal agent solution, wherein the mass ratio of polyvinyl pyrrolidone, phosphorus pentasulfide and water is 0.01:3:10.
[0047] (2) Primary arsenic removal: 107% polyphosphoric acid is pumped into a arsenic removal reaction tower through a circulating acid pump via a flow meter, and then the prepared arsenic removal agent solution is added to the arsenic removal reaction tower for arsenic removal reaction. The amount of the arsenic removal agent solution added is 3 L / ton of polyphosphoric acid. The conditions of the arsenic removal reaction are controlled as follows: the reaction temperature is 95° C., the reaction time is 3 h, and the stirring speed is 80 rpm.
[0048] (3) Preparation of arsenic removal agent microspheres: Sodium hydroxide is added to water and dissolved to obtain a mixed solution, and metakaolin and 100-mesh rice bran are added to the mixed solution and mixed evenly to obtain a suspension, wherein the mass ratio of the sodium hydroxide, water, metakaolin and rice bran is 3:10:1:0.5; No. 10 white oil is heated to 80°C and stirred at a speed of 400 rpm, and the suspension is dripped into the No. 10 white oil while stirring, wherein the dripping volume of the suspension is 0.8 times that of the white oil, to obtain a mixture; the temperature of the mixture is controlled to be 60°C and allowed to stand for 2 hours, filtered, and the filter residue is washed twice with boiling water, dried, and then roasted at 450°C for 3 hours, and passed through an 80-mesh sieve to obtain arsenic removal agent microspheres.
[0049] (4) Secondary arsenic removal: The temperature of the polyphosphoric acid after the primary arsenic removal in step (2) was controlled at 85° C. The arsenic removal agent microspheres prepared in step (3) were added, wherein the weight of the arsenic removal agent microspheres added was 0.1 times that of the polyphosphoric acid, and the reaction was stirred at a speed of 150 rpm for 20 min.
[0050] (5) Filtration: The polyphosphoric acid after the secondary arsenic removal in step (4) is filtered through a plate and frame filter press, and the filtrate is collected. Compressed air is introduced into the filtrate for aeration, oxidation, and blowing. Then, process water is added to adjust the acid concentration to 105% to obtain arsenic-free 105% polyphosphoric acid, which is a colorless, transparent, viscous liquid. The element arsenic content of the arsenic-free 105% polyphosphoric acid is less than 0.5 PPM.
[0051] Comparative Example 1
[0052] The arsenic removal process for producing 105% polyphosphoric acid by thermal phosphoric acid comprises the following steps:
[0053] (1) Preparation of arsenic removal agent solution: polyvinyl pyrrolidone with a molecular weight of 10,000 is added to water and mixed evenly, and then phosphorus pentasulfide is added and mixed evenly to obtain a arsenic removal agent solution, wherein the mass ratio of polyvinyl pyrrolidone, phosphorus pentasulfide and water is 0.02:2.5:10.
[0054] (2) Primary arsenic removal: 107% polyphosphoric acid is pumped into a arsenic removal reaction tower through a circulating acid pump, and then the prepared arsenic removal agent solution is added to the arsenic removal reaction tower through a metering pump for arsenic removal reaction. The amount of the arsenic removal agent solution added is 5 L / ton of polyphosphoric acid. The conditions of the arsenic removal reaction are controlled as follows: the reaction temperature is 105° C., the reaction time is 2 h, and the stirring speed is 75 rpm.
[0055] (3) Filtration: The polyphosphoric acid after the arsenic removal in step (2) is filtered through a plate-frame filter press, and the filtrate is collected in a collecting tank and finally flows into an acid collecting tank, and compressed air is introduced into the filtrate for aeration, oxidation, and blowing. The filtrate continuously removes hydrogen sulfide gas in the acid collecting tank, and then process water is added to adjust the acid concentration to 105% to obtain 105% polyphosphoric acid after arsenic removal. According to experimental comparison, since the arsenic removal agent microspheres are not used in this comparative example, the filtration time is about twice that of Example 1.
[0056] Comparative Example 2
[0057] The arsenic removal process for producing 105% polyphosphoric acid by thermal phosphoric acid comprises the following steps:
[0058] (1) Preparation of arsenic removal agent microspheres: Sodium hydroxide is added to water and dissolved to obtain a mixed solution, and metakaolin and 100-mesh rice bran are added to the mixed solution and mixed evenly to obtain a suspension, wherein the mass ratio of the sodium hydroxide, water, metakaolin and rice bran is 1:8:0.7:0.3; No. 100 white oil is heated to 85°C and stirred at a speed of 400 rpm, and the suspension is dripped into the No. 100 white oil while stirring, wherein the dripping volume of the suspension is 0.6 times the volume of the white oil, to obtain a mixture; the temperature of the mixture is controlled to be 65°C and allowed to stand for 1.5 hours, filtered, and the filter residue is washed twice with boiling water, dried, and then roasted at 400°C for 4 hours, and passed through an 80-mesh sieve to obtain arsenic removal agent microspheres.
[0059] (2) Primary arsenic removal: The temperature of 107% polyphosphoric acid was controlled at 90° C., and the arsenic removal agent microspheres prepared in step (1) were added, wherein the weight of the arsenic removal agent microspheres added was 0.2 times that of the polyphosphoric acid, and the mixture was stirred at a speed of 120 rpm for 30 min.
[0060] (3) Filtration: The polyphosphoric acid after the arsenic removal in step (2) is filtered through a plate and frame filter press, and then process water is added to adjust the acid concentration to 105% to obtain 105% polyphosphoric acid after arsenic removal.
[0061] Comparative Example 3
[0062] The arsenic removal process for producing 105% polyphosphoric acid by thermal phosphoric acid comprises the following steps:
[0063] (1) Preparation of arsenic removal agent solution: phosphorus pentasulfide is added into water and mixed to obtain a arsenic removal agent solution, wherein the mass ratio of phosphorus pentasulfide to water is 2.5:10.
[0064] (2) Primary arsenic removal: After the concentration of industrial phosphoric acid is increased to 107% polyphosphoric acid in the phosphorus burning process, the 107% polyphosphoric acid is pumped into the arsenic removal reaction tower through a circulating acid pump, and then the prepared arsenic removal agent solution is added to the arsenic removal reaction tower through a metering pump for arsenic removal reaction. The amount of the arsenic removal agent solution added is 3.5 L / ton of polyphosphoric acid, and the conditions of the arsenic removal reaction are controlled as follows: the reaction temperature is 105° C., the reaction time is 2 h, and the stirring speed is 75 rpm.
[0065] (3) Preparation of arsenic removal agent microspheres: Sodium hydroxide is added to water and dissolved to obtain a mixed solution, and kaolin and 100-mesh rice bran are added to the mixed solution and mixed evenly to obtain a suspension, wherein the mass ratio of the sodium hydroxide, water, kaolin and rice bran is 1:8:0.7:0.3; No. 100 white oil is heated to 85°C and stirred at a speed of 400 rpm, and the suspension is dripped into the No. 100 white oil while stirring, wherein the dripping volume of the suspension is 0.6 times the volume of the white oil, to obtain a mixture; the temperature of the mixture is controlled to be 65°C and allowed to stand for 1.5 hours, filtered, and the filter residue is washed twice with boiling water, dried, and then roasted at 400°C for 4 hours, and passed through an 80-mesh sieve to obtain arsenic removal agent microspheres.
[0066] (4) Secondary arsenic removal: The temperature of the polyphosphoric acid after the primary arsenic removal in step (2) was controlled at 90° C. The arsenic removal agent microspheres prepared in step (3) were added, wherein the weight of the arsenic removal agent microspheres added was 0.2 times that of the polyphosphoric acid, and the reaction was stirred at a speed of 120 rpm for 30 min.
[0067] (5) Filtration: The polyphosphoric acid after the secondary arsenic removal in step (4) is filtered through a plate and frame filter press. The filtrate after filtration is collected in a collecting tank and finally flows into an acid collecting tank. Compressed air is introduced into the filtrate for aeration, oxidation and blowing. The filtrate continuously releases hydrogen sulfide gas in the acid collecting tank, and the filtrate gradually becomes clear and transparent. Then, process water is added to adjust the acid concentration to 105% to obtain 105% polyphosphoric acid after arsenic removal.
[0068] The comparison of arsenic removal experimental data of Examples 1-4 and Comparative Examples 1-3 is shown in Table 1.
[0069] Table 1
[0070] Group Original concentration, % Arsenic value before arsenic removal, PPM Arsenic value after arsenic removal, PPM Concentration after arsenic removal, % Example 1 107.54 88 0.092 105.15 Example 2 107.01 92 0.090 105.08 Example 3 107.63 89 0.095 105.24 Example 4 107.52 88 0.484 105.17 Comparative Example 1 107.77 90 5.178 105.49 Comparative Example 2 107.05 90 66.50 105.04 Comparative Example 3 107.13 87 0.899 105.10
[0071] From the comparison of the data in Table 1, it can be seen that the arsenic content of Examples 1-4 after arsenic removal is all less than 0.5PPM, which can meet the requirements of special industries such as lithium hexafluorophosphate electrolyte, drug synthesis, electronics, and food; the white oil used in Example 4 is No. 10 white oil, which has a poor arsenic removal effect compared with No. 100 white oil; Comparative Examples 1 and 2 both use a one-time arsenic removal process, and do not use arsenic removal agent microspheres or arsenic removal agent solution for arsenic removal, and the arsenic content of the final product is greatly increased, which is far from meeting the requirements of special industries such as food; Comparative Example 3 does not use polyvinyl pyrrolidone in the arsenic removal agent solution, which also causes the arsenic content of the final product to rise to>0.5PPM, which also does not meet the requirements of special industries such as food.
[0072] The analysis report of 105% polyphosphoric acid after the arsenic removal process of Examples 1-4 and Comparative Examples 1-3 is shown in Table 2.
[0073] Table 2
[0074]
[0075] It can be seen from the data in Table 2 that the various indicators of 105% polyphosphoric acid after arsenic removal by the arsenic removal process of Examples 1-4 meet the relevant standards, while the arsenic content of polyphosphoric acid after arsenic removal by the arsenic removal process of Comparative Examples 1-3 does not meet the requirements of special industries such as food. In summary, the two-step arsenic removal method adopted by the present invention can cooperate with each other to achieve the purpose of thorough arsenic removal, low chromaticity, clear and transparent finished products, and a final arsenic content of less than 0.5PPM.
[0076] Although the present invention has been disclosed as above with preferred embodiments, it is not intended to limit the present invention. Any person skilled in the art may make some modifications and improvements without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention shall be based on the definition of the claims.
Claims
1. Arsenic removal process for producing 105% polyphosphoric acid by thermal phosphoric acid, It is characterized in that The steps include: (1) Preparation of arsenic removal agent solution: adding polyvinyl pyrrolidone to water and mixing evenly, then adding phosphorus pentasulfide and mixing evenly to obtain a arsenic removal agent solution, wherein the mass ratio of polyvinyl pyrrolidone, phosphorus pentasulfide and water is 0.01-0.05:2-3:10; (2) Primary arsenic removal: 107% polyphosphoric acid is injected into a arsenic removal reaction tower, and then the prepared arsenic removal agent solution is added into the arsenic removal reaction tower for arsenic removal reaction, wherein the amount of the arsenic removal agent solution added is 3-4 L / ton of polyphosphoric acid; (3) Preparation of arsenic removal agent microspheres: sodium hydroxide is added to water to dissolve to obtain a mixed solution, metakaolin and rice bran are added to the mixed solution and mixed evenly to obtain a suspension; white oil is heated to 80-90° C. and stirred, and the suspension is dropped into the white oil while stirring to obtain a mixture; the temperature of the mixture is controlled to 60-70° C., and allowed to stand for 1-2 hours, filtered, and the filter residue is washed with boiling water, dried, roasted, and sieved to obtain arsenic removal agent microspheres; (4) Secondary arsenic removal: the temperature of the polyphosphoric acid after the primary arsenic removal in step (2) is controlled at 85-95° C., the arsenic removal agent microspheres prepared in step (3) are added, and the reaction is stirred at a speed of 100-150 rpm for 20-40 min; (5) Filtration: The polyphosphoric acid after the secondary arsenic removal in step (4) is filtered through a plate and frame filter press, and the filtrate is collected. Compressed air is introduced into the filtrate for aeration, oxidation, and blowing. Then, process water is added to adjust the acid concentration to 105% to obtain arsenic-free 105% polyphosphoric acid, wherein the element arsenic content of the arsenic-free 105% polyphosphoric acid is less than 0.5 PPM.
2. The arsenic removal process for producing 105% polyphosphoric acid by thermal phosphoric acid according to claim 1, It is characterized in that In step (2), the conditions of the arsenic removal reaction are controlled as follows: reaction temperature is 95-110° C., reaction time is 1-3 h, and stirring speed is 70-80 rpm.
3. The arsenic removal process for producing 105% polyphosphoric acid by thermal phosphoric acid as claimed in claim 1, Features: In step (3), the mass ratio of sodium hydroxide, water, metakaolin and rice bran is 0.5-3:5-10:0.5-1:0.1-0.
5.
4. The arsenic removal process for producing 105% polyphosphoric acid by thermal phosphoric acid according to claim 1, Features: In step (3), the stirring speed is 350-400 rpm; the roasting temperature is 350-450° C., the roasting time is 3-5 h; and the sieving mesh size is 60-80 mesh.
5. The arsenic removal process for producing 105% polyphosphoric acid by thermal phosphoric acid according to claim 1, Features: In step (3), the white oil is No. 100 white oil.
6. The arsenic removal process for producing 105% polyphosphoric acid by thermal phosphoric acid according to claim 1, Features: In step (4), the amount of the arsenic removal agent microspheres added is 0.1-0.3 times the weight of the polyphosphoric acid.
7. The arsenic removal process for producing 105% polyphosphoric acid by thermal phosphoric acid as claimed in claim 1, Features: In step (5), hydrogen sulfide gas is continuously removed during the aeration process of the filtrate, and the removed hydrogen sulfide gas is introduced into the exhaust fan pipeline. Under the action of the exhaust fan, the hydrogen sulfide gas is sent to the hydrogen sulfide absorption tower, sprayed with industrial phosphoric acid for absorption, and then washed in the alkaline washing tower and discharged into the atmosphere through the exhaust pipe.
Citation Information
Patent Citations
Arsenic removing method of phosphoric acid
CN102431982A
Arsenic-removing filtering method for high-concentration polyphosphoric acid
CN102515125A
Method for producing high-quality polyphosphoric acid
CN103818890A
Device for efficiently removing arsenic by purifying phosphoric acid through wet process
CN214299293U
Method for purification of phosphoric acid high purity polyphosphoric acid
US6861039B1