Vapor chamber, preparation method thereof and battery
By arranging a reinforcing structure in the inner cavity of the vapor chamber, including bending sections and reinforcing rib groups, the problem of insufficient pressure-bearing and anti-expansion capabilities of the vapor chamber during the bending process is solved, and the structural strength and service life are improved.
Patent Information
- Application Number
- CN202411047801.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-10-11
AI Technical Summary
Existing vapor chambers have weak pressure-bearing and anti-expansion capabilities during the bending process, and are prone to deformation or breakage.
A vapor chamber is designed that includes a plate body and a first reinforcing structure. The first reinforcing structure is located in the inner cavity of the plate body and has a curved section. Through the arrangement of the reinforcing rib group and the reinforced bottom plate, the structural strength and strength of the plate body are improved. Compression resistance to avoid breakage when bending.
The pressure-bearing capacity and expansion resistance of the vapor chamber are improved, the service life is extended, and the structural strength is enhanced without taking up additional space.
Smart Images

Figure CN118758093A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of batteries, and in particular to a vapor chamber and a preparation method thereof, and a battery. Background Art
[0002] A vapor chamber is a phase change heat transfer element that uses the latent heat of phase change of the working fluid to carry away heat. It is the most promising thermal management method to solve the heat dissipation problem of products and equipment. At present, vapor chambers are mainly used for heat dissipation of electronic equipment. They have excellent thermal conductivity, a large heat transfer area and good temperature uniformity; especially ultra-thin thickness, and the external dimensions can be adjusted according to actual heat dissipation needs. In related technologies, the vapor chamber can be bent and used in conjunction with the battery casing. The thickness of the vapor chamber is relatively thin, and during the bending process, the bend is prone to deformation or even breakage due to its weak pressure bearing capacity and internal anti-expansion capacity. Summary of the invention
[0003] The embodiments of the present invention provide a vapor chamber and a method for preparing the same, as well as a battery, which are intended to solve the technical problem that the existing vapor chamber has weak pressure bearing capacity and internal anti-expansion capacity at the bend, resulting in easy deformation or even fracture at the bend.
[0004] In a first aspect, an embodiment of the present invention provides a vapor chamber comprising:
[0005] A plate body is provided with an inner cavity, the plate body comprises a first plate body and a second plate body arranged opposite to each other, the first plate body comprises a first sub-plate body, a bent plate and a second sub-plate body, the bent plate is connected between the first sub-plate body and the second sub-plate body; and,
[0006] The first reinforcing structure is connected to the first plate body and is located in the inner cavity. The first reinforcing structure has a curved section corresponding to the bent plate.
[0007] In one embodiment, the first reinforcement structure includes a first reinforcement plate, which is bent, a first fluid channel is provided on a side of the first reinforcement plate close to the first plate body, and a second fluid channel is provided on a side of the first reinforcement plate close to the second plate body.
[0008] In one embodiment, the first reinforcement structure is disposed separately from the plate body; and / or,
[0009] The first reinforcing plate is integrally formed.
[0010] In one embodiment, the first reinforcing plate includes at least one of a concave portion and a convex portion.
[0011] In one embodiment, the first reinforcement structure further includes a first section and a second section, the bent section is connected between the first section and the second section, the first section corresponds to the first sub-plate body, and the second section corresponds to the second sub-plate body.
[0012] In one embodiment, in the extension direction of the first sub-plate body, the size of the first reinforcement structure in the bending section is L1, the size of the first reinforcement structure in the first section is L2, and the size of the first reinforcement structure in the second section is L3, wherein L1: (L1+L2+L3)=(0.1~0.3):1.
[0013] In one embodiment, the first reinforcement structure includes a plurality of reinforcement rib groups and a reinforcement base plate, the plurality of reinforcement rib groups are arranged on the reinforcement base plate at intervals along the width direction of the first sub-plate body, each of the reinforcement rib groups includes a plurality of first reinforcement ribs, and the plurality of first reinforcement ribs are arranged at intervals along the width direction of the first sub-plate body, and in the width direction of the first sub-plate body, the size of the reinforcement base plate is L4, and the size of the first reinforcement rib is L5, wherein L5:L4=(0.005~0.05):1.
[0014] In one embodiment, the first reinforcement structure includes a plurality of reinforcement rib groups, each of the reinforcement rib groups includes a plurality of first reinforcement ribs, the plurality of first reinforcement ribs are arranged at intervals along the width direction of the first sub-plate body, each of the first reinforcement ribs includes two first sub-reinforcement ribs and a plurality of second sub-reinforcement ribs, the two first sub-reinforcement ribs are respectively located in the first section and the second section, and the plurality of second sub-reinforcement ribs are arranged between the two first sub-reinforcement ribs and are located in the bending section.
[0015] In one embodiment, the number of the second sub-reinforcing ribs of each of the first reinforcing ribs is n1, and the number of the first reinforcing ribs of each of the reinforcing rib groups is n2, wherein n1=n2.
[0016] In one embodiment, a second reinforcing structure is further included, and the second reinforcing structure is arranged on the first sub-plate body and the second sub-plate body, and the second reinforcing structure is located in the inner cavity, and the second reinforcing structure includes a plurality of reinforcing sub-ribs, and the density of the plurality of the reinforcing sub-ribs on the plate body is V1, and the density of the plurality of the second sub-reinforcing ribs on the plate body is V2, wherein V1:V2=(2~6):1.
[0017] In one embodiment, in the length direction of the first sub-plate body, the size of the first reinforcing structure in the bending section is L1, the size of the first reinforcing structure in the first section is L2, the size of the first reinforcing structure in the second section is L3, and the size of each of the second sub-reinforcement ribs is L6, wherein L6: (L1+L2+L3)=(0.03~0.2):1.
[0018] In one embodiment, the first reinforcement structure is integrally formed with the plate body.
[0019] In one embodiment, the bending angle of the bending plate is α, and the bending angle of the bending section is β, wherein 90°≤α≤95°, 90°≤β≤95°, and α=β.
[0020] In one embodiment, the material of the plate body includes stainless steel; and / or,
[0021] The material of the first reinforcement structure includes stainless steel.
[0022] In a second aspect, the present invention further provides a battery, comprising the above-mentioned heat spreader.
[0023] In a third aspect, the present invention further provides a method for preparing a vapor chamber, which is used to prepare the vapor chamber, comprising the following steps:
[0024] bending the first plate and the second plate;
[0025] The first plate body, the liquid wick, the screen and the second plate body are stacked from bottom to top;
[0026] After the step of bending the first plate body and the second plate body, the first plate body and the second plate body are welded to obtain a heat spreader.
[0027] Beneficial effects of the embodiments of the present invention:
[0028] The vapor chamber provided by the present invention comprises a plate body, the plate body is formed with an inner cavity, the first reinforcing structure is arranged in the inner cavity, the first reinforcing structure can support the plate body, strengthen the structural strength of the plate body, thereby improving the pressure bearing capacity and anti-expansion capacity of the vapor chamber, improving the structural strength of the vapor chamber, avoiding the vapor chamber from breaking during the bending process, thereby improving the service life of the vapor chamber. At the same time, the first reinforcing structure is arranged in the inner cavity and does not occupy additional space. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative work.
[0030] Figure 1 It is a structural schematic diagram of an embodiment of a vapor chamber provided by the present invention;
[0031] Figure 2 yes Figure 1 A schematic structural diagram of the first plate body;
[0032] Figure 3 yes Figure 1 A schematic diagram of the structure of the second plate body;
[0033] Figure 4 yes Figure 1 A structural schematic diagram of an embodiment of the first reinforcement structure;
[0034] Figure 5 yes Figure 4 A is an enlarged schematic diagram;
[0035] Figure 6 yes Figure 5 The main view;
[0036] Figure 7 yes Figure 6 A magnified schematic diagram of B;
[0037] Figure 8 yes Figure 5 Side view of
[0038] Fig. 9 yes Figure 1 A schematic diagram of the partial structure of another embodiment of the first reinforcement structure.
[0039] Description of Figure Numbers
[0040] Label name Label name 100 Vapor Chamber 112 Strengthen the bottom plate 101 Board body 113 Reinforcement group 103 The first plate 114 First reinforcement 104 The second plate 115 First son reinforcement 105 The first sub-board 116 Second reinforcement 106 The second sub-board 117 Support column 107 Bending Plate 118 Wicking core installation channel 108 The first reinforcement structure 119 Liquid wick 109 Paragraph 1 120 Silk Screen 110 Curved segment 121 Liquid inlet 111 Paragraph 2 122 Second reinforcement structure 123 First reinforcement plate 124 First fluid channel 125 Second fluid channel 126 The third sub-board 127 Bending sub-plate 128 Fourth sub-board DETAILED DESCRIPTION
[0041] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present invention. In addition, it should be understood that the specific implementation methods described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention. In the present invention, unless otherwise specified, the directional words used, such as "upper" and "lower", generally refer to the upper and lower parts of the device in actual use or working state, specifically the drawing direction in the drawings; while "inside" and "outside" refer to the outline of the device.
[0042] In the related art, the heat spreader can be bent and used as the outer shell of the battery. The thickness of the heat spreader is relatively thin, and during the bending process, the bending part is prone to deformation or even breakage due to its weak pressure bearing capacity and internal anti-expansion capacity.
[0043] Example 1
[0044] The present invention provides a heat sink. Figures 1 to 8 This is a structural schematic diagram of an embodiment of a heat spreader provided by the present invention. The heat spreader provided by the present invention has strong structural strength and strong pressure bearing capacity, and will not affect the overall size of the battery module. The heat spreader will be described in detail below in conjunction with the main drawings.
[0045] See also Figure 1 , Figure 2 and Figure 3 The heat spreader 100 includes a plate body 101 and a first reinforcement structure 108. The plate body 101 is provided with an inner cavity, and the plate body 101 includes a first plate body 103 and a second plate body 104 arranged opposite to each other, and the first plate body 103 includes a first sub-plate body 105, a bending plate 107 and a second sub-plate body 106, and the bending plate 107 is connected between the first sub-plate body 105 and the second sub-plate body 106. The first reinforcement structure 108 is provided on the first plate body 103 and is located in the inner cavity, and the first reinforcement structure 108 has a bending section 110, and the bending section 110 corresponds to the bending plate 107.
[0046] The heat spreader 100 provided by the present invention has a simple structure, low manufacturing cost, and high efficiency in heat diffusion. The heat spreader 100 includes a plate body 101, the plate body 101 is formed with an inner cavity, and a first reinforcing structure 108 is arranged in the inner cavity. The first reinforcing structure 108 can support the plate body 101 and strengthen the structural strength of the plate body 101, thereby improving the pressure bearing capacity and anti-expansion capacity of the heat spreader 100, improving the structural strength of the heat spreader 100, avoiding the heat spreader 100 from breaking during the bending process, and improving the service life of the heat spreader 100. At the same time, the first reinforcing structure 108 is arranged in the inner cavity and does not occupy additional space.
[0047] In some embodiments, the cross-section of the curved section 110 is arc-shaped, which can disperse the force exerted on the vapor chamber 100 and increase the life of the vapor chamber 100 .
[0048] It should be noted that the compressive strength of the vapor chamber 100 is greater than or equal to 2.5 MPa. During use, the battery will generate heat and expand. When the compressive strength of the vapor chamber 100 is less than 2.5 MPa, the vapor chamber 100 will bend or even break due to the expansion force.
[0049] See also Figure 4 The first reinforcement structure 108 also includes a first section 109 and a second section 111, and the bending section 110 is connected between the first section 109 and the second section 111. The first section 109 corresponds to the first sub-plate body 105, and the second section 111 corresponds to the second sub-plate body 106. This arrangement increases the contact area between the first reinforcement structure 108 and the first plate body 103, and improves the connection strength between the two.
[0050] In some embodiments, see Figure 3 The second plate body 104 includes a third sub-plate body 126, a bent sub-plate 127 and a fourth sub-plate body 128. The bent sub-plate 127 is connected between the third sub-plate body 126 and the fourth sub-plate body 128, wherein the third sub-plate body 126 corresponds to the first sub-plate body 105, the fourth sub-plate body 128 corresponds to the second sub-plate body 106, and the bent sub-plate 127 corresponds to the bent plate 107.
[0051] In order to facilitate processing, the first plate body 103 and the second plate body 104 are both flat plates in their initial state, and the connection method of the first plate body 103 and the second plate body 104 is not limited. In some embodiments, the first plate body 103 and the second plate body 104 are first welded, and then the welded first plate body 103 and the second plate body 104 are bent. Such a configuration facilitates the welding operation and reduces the difficulty of welding. In another embodiment, the first plate body 103 and the second plate body 104 are first bent so that the third sub-plate body 126 corresponds to the first sub-plate body 105, the fourth sub-plate body 128 corresponds to the second sub-plate body 106, and the bent sub-plate 127 corresponds to the bent plate 107, and then the first plate body 103 and the second plate body 104 are welded together. Such a configuration can improve the heat generation performance at the bent plate 107 and the bent sub-plate 127, avoid the loss of heat transfer performance at the bent plate 107 and the bent sub-plate 127, and improve the overall performance of the heat spreader 100.
[0052] In some embodiments, see Figure 1 , the first plate body 103 is the lower shell plate, the second plate body 104 is the upper shell plate, the upper shell plate and the lower shell plate are respectively formed with a first receiving groove and a second receiving groove, the upper shell plate and the lower shell plate are welded and connected so that the first receiving groove and the second receiving groove are connected to form an inner cavity. It should be noted that the specific position of the first reinforcing structure 108 is not limited, it only needs to be located in the inner cavity. In the above embodiment, the first reinforcing structure 108 is provided on the first plate body 103. Of course, the first reinforcing structure 108 can also be provided on the second plate body 104. It can be selected according to the actual situation. Since the first plate body 103 is the lower shell plate, the first reinforcing structure 108 is provided on the first plate body 103, which is more convenient for the welding connection between the first plate body 103 and the second plate body 104.
[0053] In some embodiments, a working fluid is provided in the inner cavity, and the working fluid is used for heat exchange. It should be noted that the type of the working fluid in the above embodiments is not limited and can be selected according to the actual application. For example, the working fluid can be lubricating oil, water, cold air, alcohol compounds, etc.
[0054] In some embodiments, see Figure 8, in the extension direction of the first sub-plate 105, the size of the first reinforcing structure 108 in the curved section 110 is L1 (i.e., the length of the arc of the curved section 110), the size of the first reinforcing structure 108 in the first section 109 is L2 (i.e., the length of the first sub-reinforcing rib 115 in the first section 109), and the size of the first reinforcing structure 108 in the second section 111 is L3 (i.e., the length of the first sub-reinforcing rib 115 in the second section 111), wherein L1: (L1+L2+L3)=(0.1-0.3):1. It should be noted that when the ratio of L1 to (L1+L2+L3) is less than 0.1, the area of the curved section 110 is too small, the bending difficulty increases, the welding difficulty of the first plate 103 and the second plate 104 increases, the processing is difficult, and the processing sequence increases. When the ratio of L1 to (L1+L2+L3) is greater than 0.3, the area of the curved section 110 increases, and the wasted space increases.
[0055] See 4 and Figure 5 The first reinforcement structure 108 includes a reinforcement base plate 112 and a plurality of reinforcement rib groups 113. The reinforcement base plate 112 extends along the width direction of the first sub-plate body 105 and is disposed in the first section 109, the curved section 110 and the second section 111; the plurality of reinforcement rib groups 113 are disposed at intervals on the reinforcement base plate 112 along the width direction of the first sub-plate body 105 and are disposed in the first section 109, the curved section 110 and the second section 111. In this embodiment, the reinforcing bottom plate 112 and the plurality of reinforcing rib groups 113 are integrally formed. The provision of the reinforcing bottom plate 112 can facilitate the welding of the first reinforcing structure 108 on the first plate body 103. During the welding process, the reinforcing bottom plate 112 can be welded to the first plate body 103, thereby reducing the welding steps (when the reinforcing bottom plate 112 is not provided, the plurality of reinforcing rib groups 113 need to be welded to the first plate body 103 respectively, which increases the welding difficulty and the welding steps). Another function of the reinforcing bottom plate 112 is to increase the structural strength of the first plate body 103 so that the first plate body 103 will not break during the bending process. The function of the plurality of reinforcing rib groups 113 is to further increase the structural strength of the first plate body 103. At the same time, the purpose of providing the plurality of reinforcing rib groups 113 is to form a cavity between two adjacent reinforcing rib groups 113. During the bending process, the cavity can absorb a part of the bending force, thereby avoiding the concentration of the bending force, which causes the heat spreader 100 to deform or even break.
[0056] In some embodiments, see Figure 5Each reinforcing rib group 113 includes a plurality of first reinforcing ribs 114, and the plurality of first reinforcing ribs 114 are extended along the length direction of the first sub-plate body 105, and the plurality of first reinforcing ribs 114 are spaced apart along the width direction of the first sub-plate body 105, and a first gap is formed between two adjacent reinforcing rib groups 113, and the first gap is configured to allow the working fluid to flow, so that the first section 109 and the second section 111 are connected.
[0057] Further, in this embodiment, please refer to Figure 6 and Figure 7 , in the width direction of the first sub-plate body 105, the size of the reinforcing bottom plate 112 is L4, and the size of the first reinforcing rib 114 is L5, wherein L5:L4=(0.005-0.05):1. When the ratio of L5 to L4 is less than 0.005, the size of the first reinforcing rib 114 is too small, resulting in insufficient strength of the heat spreader 100, and the heat spreader 100 is easily damaged during use. When the ratio of L5 to L4 is greater than 0.05, the size of the first reinforcing rib 114 is too large, the occupied volume increases, the first gap decreases, the first section 109 and the second section 111 cannot be connected, and the heat dissipation capacity or thermal conductivity of the heat spreader 100 is reduced.
[0058] In some embodiments, the size of the first reinforcing rib 114 is 0.1 mm to 0.3 mm. Specifically, L4 can be 0.1 mm, 0.12 mm, 0.13 mm, 0.15 mm, 0.16 mm, 0.17 mm, 0.18 mm, 0.19 mm, 0.2 mm, 0.21 mm, 0.24 mm, 0.25 mm, 0.28 mm, 0.29 mm, 0.3 mm or other unspecified values.
[0059] In some embodiments, the width of the first gap is 0.8mm to 3mm. It should be noted that when the width of the first gap is less than 0.8mm, the size of the first gap is too small and is prone to blockage, resulting in the first section 109 and the second section 111 being unable to communicate. When the size of the first gap is greater than 3mm, the strength of the heat spreader 100 will be insufficient, and it will be prone to deformation or even breakage. Specifically, the size of the first gap can be 0.8mm, 0.85mm, 0.9mm, 0.92mm, 0.95mm, 0.98mm, 1mm, 1.1mm, 1.4mm, 1.5mm, 1.8mm, 2mm, 2.2mm, 2.5mm, 2.7mm, 3mm or other unspecified values.
[0060] The connection method of the first reinforcing structure 108 and the first plate 103 is not limited. In some embodiments, the first reinforcing structure 108 and the first plate 103 are bent separately and then connected together. In another embodiment, the first reinforcing structure 108 and the first plate 103 are first connected together and then bent at the same time.
[0061] In order to avoid stress concentration during the bending process, which may cause the first plate 103 or the second plate 104 to deform or even break. Figure 8 Each first reinforcing rib 114 includes two first sub-reinforcing ribs 115 and a plurality of second sub-reinforcing ribs 116. The two first sub-reinforcing ribs 115 are respectively located in the first section 109 and the second section 111. The plurality of second sub-reinforcing ribs 116 are arranged between the two first sub-reinforcing ribs 115 and are located in the bending section 110. Specifically, since the plurality of second sub-reinforcing ribs 116 are arranged in the bending section 110, the orientation of each second sub-reinforcing rib 116 is different. During the bending process, each sub-reinforcing rib 115 diffuses the stress in different directions, thereby avoiding stress concentration and preventing the heat spreader 100 from deforming or breaking. At the same time, the heat spreader 100 is also provided with a wire mesh 120 and a liquid wick 119. The plurality of second sub-reinforcing ribs 116 diffuse the stress in different directions, thereby avoiding squeezing of the wire mesh 120 or the liquid wick 119, causing wrinkles in the liquid wick 119 or the wire mesh 120, and blocking the inner cavity.
[0062] In some embodiments, the heat spreader also includes a second reinforcement structure 122, which is disposed on the first sub-plate body 105 and the second sub-plate body 106. The second reinforcement structure 122 is used to increase the strength of the first sub-plate body 105 and the second sub-plate body 106. The second reinforcement structure 122 is located in the inner cavity, and the second reinforcement structure 122 includes a plurality of reinforcement sub-ribs.
[0063] Furthermore, the density of the plurality of reinforcing sub-ribs on the plate body 101 is V1, the density of the plurality of second sub-reinforcing ribs 116 on the plate body 101 is V2, and the density of the plurality of second sub-reinforcing ribs 116 on the plate body is V2, wherein V1:V2=(2-6):1. It should be noted that when the ratio of V1 to V2 is less than 2, the number of reinforcing sub-ribs is small, the pressure bearing capacity and internal anti-expansion capacity of the first sub-plate body 105 and the second sub-plate body 106 are weak, resulting in easy deformation of the heat spreader; when the ratio of V1 to V2 is greater than 6, the density of the plurality of reinforcing sub-ribs is too dense, resulting in a reduction in the space of the inner cavity, the working fluid cannot flow smoothly, and blockage is easy to occur.
[0064] In some embodiments, see Figure 4, the number of the second sub-reinforcement ribs 116 of each first reinforcement rib 114 is n1, and the number of the first reinforcement ribs 114 of each reinforcement rib group 113 is n2, wherein n1=n2. It should be noted that during the bending process, the bending section 110 is generally bent, and during the bending process, the bending section 110 will receive a bending force, and the area near the bending section 110 will also be affected by the bending force (that is, the area of the first sub-plate body 105 corresponding to the first section 109 will be affected by the bending force, and the area of the second sub-plate body 106 corresponding to the second section 111 will also be affected by the bending force). In this embodiment, the second sub-reinforcement rib 116 is used to enhance the structural strength of the bending plate 107, and the first sub-reinforcement rib 115 is used to increase the first sub-plate body 105 and the second sub-plate body 106. The structural strength of the two sub-plate bodies 106 is such that since the first reinforcing rib 114 includes two second sub-reinforcing ribs 116, and the two second sub-reinforcing ribs 116 correspond to the first section 109 and the second section 111 respectively, in each reinforcing rib group 113, the number of second sub-reinforcing ribs located in the first section is also n2, and the number of second sub-reinforcing ribs located in the second section is also n2, wherein n1=n2. The purpose of such a setting is to ensure that the structural strengths of the first section 109, the curved section 110 and the second section 111 are the same, so that they are subjected to uniform force and local deformation is avoided.
[0065] In some embodiments, in the length direction of the first sub-plate body 105, the size of the first reinforcing structure 108 in the curved section 110 is L1, the size of the first reinforcing structure 108 in the first section 109 is L2, the size of the first reinforcing structure 108 in the second section 111 is L3, and the size of the second sub-reinforcing rib 116 is L6, wherein L6: (L1+L2+L3)=(0.03-0.2): 1. It should be noted that when the ratio of L6 to (L1+L2+L3) is less than 0.03, the size of the second sub-reinforcing rib 116 is small, and during the bending process, the second sub-reinforcing rib 116 itself is easily squeezed and deformed, thereby squeezing other parts (such as the screen 120 or the wick 119), causing other parts to bend and deform. When the ratio of L6 to (L1+L2+L3) is greater than 0.2, the size of the second sub-reinforcement rib 116 is too large, and a larger bending force is required to bend the first reinforcement structure 108 during the bending process, causing other parts to be affected and deformed or even broken.
[0066] Further, in some embodiments, the size of the second reinforcing rib L6 is 0.05-0.1 mm. Specifically, L6 can be 0.05 mm, 0.055 mm, 0.06 mm, 0.065 mm, 0.07 mm, 0.075 mm, 0.08 mm, 0.085 mm, 0.09 mm, 0.095 mm, 0.1 mm or other unspecified values.
[0067] In some embodiments, the heat sink 100 further includes a second reinforcement structure 122, the second reinforcement structure 122 includes a plurality of support columns 117, a plurality of first support columns 117 are located in the inner cavity, one end of the plurality of support columns 117 is connected to the first plate body 103, and the other end of the plurality of support columns 117 is connected to the second plate body 104, and the plurality of support columns 117 are used to support the first plate body 103 and the second plate body 104. It should be noted that the arrangement of the plurality of support columns 117 is not limited. In one embodiment, the plurality of first support columns 117 are regularly arranged. In some other implementations, the plurality of first support columns 117 are irregularly arranged.
[0068] Furthermore, in this embodiment, in order to prevent the heat spreader 100 from bending and deforming, the reinforcing bottom plate 112 and the reinforcing rib group 113 are connected between the first plate body 103 and the second plate body 104. The reinforcing bottom plate 112 is connected to the bending plate 107, and the reinforcing rib group 113 is connected to the bending sub-plate 127. The reinforcing bottom plate 112 and the reinforcing rib group 113 support the bending plate 107 and the bending sub-plate 127, thereby improving the structural strength of the bending section 110.
[0069] In some embodiments, see Figure 1 The heat spreader 100 further includes a plurality of wicks 119, which are arranged to extend along the length direction of the plate body 101, and are arranged in the inner cavity at intervals along the width direction of the plate body 101. Specifically, a wick installation channel 118 is formed between two adjacent reinforcing rib groups 113, and the wick installation channel 118 is arranged to extend along the length direction of the plate body 101, and is configured to install the wick 119. The wick 119 can absorb the working fluid and diffuse the working fluid into the inner cavity, so that the working fluid can fill the inner cavity and improve the heat dissipation capacity.
[0070] In some embodiments, the width of the wick installation channel 118 is 14-20 mm. More specifically, the width of the wick installation channel 118 can be 14 mm, 15 mm, 16 mm, 17 mm, 18 mm, 19 mm, 20 mm or other unspecified values.
[0071] In some embodiments, please refer to Figure 1 The heat spreader 100 further includes a wire mesh 120 , which is disposed in the inner cavity and located above the plurality of liquid wicks 119 .
[0072] In some embodiments, see Figure 2, the bending angle of the bending plate 107 is α, 90°≤α≤95°. When α is less than 90°, the space occupied by the bending plate 107 increases. When α is greater than 95°, the space between the two walls of the bending plate 107 cannot be used, and the space utilization rate is low. Specifically, α can be 90°, 91°, 92°, 93°, 94°, 95° or other unspecified values. As a preferred embodiment, α is 90°.
[0073] In some embodiments, see Figure 4 , the bending angle of the bending section is β, wherein 90°≤β≤95°. When β is less than 90°, the space occupied by the bending section 110 increases. When β is greater than 95°, the angle between the first section 109 and the second section 111 is too large, the space between the bending sections 110 cannot be utilized, and the space utilization rate is low. Specifically, β can be 90°, 91°, 92°, 93°, 94°, 95° or other unspecified values. As a preferred embodiment, β is 90°.
[0074] In some embodiments, see Figure 3 , the bending angle of the bending sub-plate is θ, 90°≤θ≤95°. When θ is less than 90°, the space occupied by the bending sub-plate 127 increases. When θ is greater than 95°, the space between the two walls of the bending sub-plate 127 cannot be used, and the space utilization rate is low. Specifically, θ can be 90°, 91°, 92°, 93°, 94°, 95° or other unspecified values. As a preferred embodiment, θ is 90°.
[0075] In this embodiment, α=β=θ. This configuration makes the first reinforcing structure 108 fit more closely with the first plate body 103 and the second plate body 106, thereby avoiding a gap between the three and improving the structural strength of the heat sink 100.
[0076] In some embodiments, see Figure 1 A liquid inlet 121 is also formed on the heat spreader 100. The liquid inlet 121 is connected to the inner cavity and is used to input the working fluid into the inner cavity.
[0077] In some embodiments, the material of the plate body 101 includes stainless steel, that is, the material of the first plate body 103 and the second plate body 104 are also stainless steel. At the same time, the material of the first reinforcement structure 108 is also stainless steel. The activity of stainless steel is poor, and it generally does not react with other substances, and has good corrosion resistance. At the same time, the structural strength of stainless steel is strong, and it is not easy to deform, which can increase the service life of the heat plate 100. In this embodiment, the model of the stainless steel material is preferably 304 stainless steel.
[0078] Of course, in some other embodiments, in order to improve the corrosion resistance of the plate body 101, a protective layer is often provided on the outside of the plate body 101. The protective layer is wrapped around the outside of the plate body 101 to isolate the plate body 101 from the outside world, prevent the plate body 101 from being corroded, and improve the service life of the plate body 101. More specifically, the protective layer includes any one of a nickel layer, a chromium layer and a zinc layer. The nickel layer, the chromium layer and the zinc layer have poor activity and basically do not react with other substances. The protective layer is wrapped around the outside of the plate body 101 to protect the plate body 101 and form a dense passivation film on the outer surface of the plate body 101, which effectively prevents the plate body 101 from reacting with other substances, thereby extending the service life of the heat spreader 100.
[0079] Similarly, in some embodiments, a protective layer may also be provided on the outer side of the first reinforcement structure 108 . The specific configuration method may refer to the configuration method of the plate body, and will not be described in detail here.
[0080] The present invention also provides a battery, which includes the above-mentioned vapor chamber 100. The specific structure of the vapor chamber 100 refers to the above-mentioned embodiment. Since the present battery adopts all the technical solutions of all the above-mentioned embodiments, it has at least all the beneficial effects brought by the technical solutions of the above-mentioned embodiments, which will not be described one by one here.
[0081] Specifically, in one embodiment, the battery further includes a battery housing, and the battery housing is composed of a heat spreader 100, that is, the six sides of the battery housing can be composed of a heat spreader 100, so that it can save space and improve space utilization. It should be noted that the six heat spreaders 100 can be interconnected or not, and the selection can be made according to the actual situation.
[0082] In some embodiments, the battery housing has six shell surfaces, and the heat spreader 100 can be applied to any shell surface of the battery housing, or can be applied to multiple shell surfaces at the same time, for example, the heat spreader 100 is applied to two adjacent shell surfaces of the battery housing. Specifically, the first section 109 of the heat spreader 100 corresponds to one shell surface, and the second section 111 of the heat spreader 100 corresponds to another shell surface, so that the heat spreader 100 can serve as two shell surfaces of the battery housing. The specific selection can be based on the size of the battery module.
[0083] In some other embodiments, the heat spreader 100 can also be used inside a battery, where the battery includes a battery shell and a core pack group, which is installed in the battery shell. The core pack group includes at least one core pack. Specifically, the first section 109 of the heat spreader 100 corresponds to one side of the core pack, and the second section 111 of the heat spreader 100 corresponds to the other side of the core pack. Furthermore, in order to even out the temperatures of adjacent core packs, a heat spreader 100 can also be arranged between two adjacent core packs to achieve temperature balance on multiple sides, thereby transferring the temperature of the high-temperature part to the low-temperature part directly cooled by the cooling plate, thereby improving the cooling efficiency and avoiding thermal runaway.
[0084] In some other embodiments, the heat spreader 100 can also be used in a battery module, which includes multiple batteries. The first section 109 of the heat spreader 100 corresponds to one side of the battery casing, and the second section 111 of the heat spreader 100 corresponds to the other side of the battery casing. Furthermore, in order to equalize the temperature of adjacent batteries, a heat spreader 100 can also be set between two adjacent batteries to achieve temperature balance on multiple sides, thereby transferring the temperature of the high-temperature part to the low-temperature part for direct cooling by the cooling plate.
[0085] Example 2
[0086] See also Figure 1 , Figure 2 and Figure 3 The heat spreader 100 includes a plate body 101 and a first reinforcement structure 108. The plate body 101 is provided with an inner cavity, and the plate body 101 includes a first plate body 103 and a second plate body 104 arranged opposite to each other, and the first plate body 103 includes a first sub-plate body 105, a bending plate 107 and a second sub-plate body 106, and the bending plate 107 is connected between the first sub-plate body 105 and the second sub-plate body 106. The first reinforcement structure 108 is provided on the first plate body 103 and is located in the inner cavity, and the first reinforcement structure 108 has a bending section 110, and the bending section 110 corresponds to the bending plate 107.
[0087] The heat spreader 100 provided by the present invention has a simple structure, low manufacturing cost, and high efficiency in heat diffusion. The heat spreader 100 includes a plate body 101, the plate body 101 is formed with an inner cavity, and a first reinforcing structure 108 is arranged in the inner cavity. The first reinforcing structure 108 can support the plate body 101 and strengthen the structural strength of the plate body 101, thereby improving the pressure bearing capacity and anti-expansion capacity of the heat spreader 100, improving the structural strength of the heat spreader 100, avoiding the heat spreader 100 from breaking during the bending process, and improving the service life of the heat spreader 100. At the same time, the first reinforcing structure 108 is arranged in the inner cavity and does not occupy additional space.
[0088] In some embodiments, the first reinforcing plate 123 includes a concave portion. In other embodiments, the first reinforcing plate 123 includes a convex portion. In yet another embodiment, the first reinforcing plate 123 includes a concave portion and a convex portion.
[0089] In this example, see Fig. 9 The first reinforcing structure 108 includes a convex portion and a concave portion. The first reinforcing structure 108 includes a first reinforcing plate 123. The first reinforcing plate 123 is arranged in a concave and convex manner. Figure 8 Take the first reinforcing plate 123 in the embodiment as an example, the part close to the first plate body 103 is a convex part, the part close to the second plate body 104 is a concave part, the concave part and the first plate body 103 enclose a first fluid channel 124, the convex part and the second plate body 104 enclose a second fluid channel 125, and the first fluid channel 124 and the second fluid channel 125 are separated. In this embodiment, by setting the first reinforcing plate 123 concave and convex, the space is reasonably utilized, the space occupied by the first reinforcing structure 108 is reduced, and the cooling efficiency is improved. More specifically, the traditional reinforcing structure often sets a plurality of reinforcing ribs in the inner cavity, and the plurality of reinforcing ribs are arranged at intervals, resulting in an increase in the space occupied by the reinforcing ribs, and the position where the reinforcing ribs are located cannot be used for the working fluid to pass through. In this embodiment, by setting the first reinforcing structure 108 concave and convex, a flow channel is formed between the first reinforcing plate 123 and the first plate body 103 and the second plate body 104, which can not only improve the structural strength of the heat spreader, but also avoid wasting the space of the inner cavity, and the working fluid is allowed to pass through the first fluid channel 124 and the second fluid channel 125, thereby improving the cooling efficiency.
[0090] Furthermore, in some embodiments, the first reinforcement structure 108 is separately provided from the plate body 101, and the first reinforcement structure 108 is stamped and formed integrally. Specifically, in actual operation, the first reinforcement structure 108 is first stamped and formed, and then the convex part of the first reinforcement structure 108 is welded to the first plate body 103, and the concave part of the first reinforcement structure 108 is welded to the second plate body 104, so as to fix the first reinforcement structure 108 on the plate body 101.
[0091] In one embodiment, the first reinforcement structure 108 may also be integrally formed by aluminum extrusion. The specific operation steps of the aluminum extrusion integrally formed may refer to conventional settings in the art and will not be described in detail here.
[0092] The first reinforcing structure 108 further includes a plurality of reinforcing rib groups 113 . The arrangement of the plurality of reinforcing rib groups 113 may be referred to in Example 1, and will not be described in detail herein.
[0093] The vapor chamber 100 further includes a second reinforcement structure 122 . The configuration of the second reinforcement structure 122 may be referred to in Example 1, and will not be described in detail herein.
[0094] Example 3
[0095] The present invention provides a method for preparing a vapor chamber 100, comprising the following steps:
[0096] S1, bending the first plate 103 and the second plate 104;
[0097] Materials are selected, the first plate body 103, the second plate body 104, the wire mesh 120, the liquid absorbent core 119 and the liquid injection tube are all made of stainless steel, and then the first plate body 103 and the second plate body 104 are placed on a punching machine, and a first groove is formed on the first plate body 103 and a second groove is formed on the second plate body 104 through stamping. The first plate body 103 and the second plate body 104 are bent by a bending machine, and the bending size can be determined according to specific process requirements. Subsequently, the bent first plate body 103, the bent second plate body 104, the wire mesh 120, the liquid absorbent core 119 and the liquid injection tube are ultrasonically cleaned.
[0098] S2, stacking the first plate 103, the wick 119, the screen 120 and the second plate 104 from bottom to top;
[0099] The first plate 103 and the second plate 104 are coated with a protective layer by vacuum ion plating. The first reinforcing structure 108 is then welded to the first plate 103. The first plate 103 is placed on the operating table, the liquid wick 119 is installed on the first plate 103, the screen 120 is placed on the liquid wick 119, and the second plate 104 is placed on the first plate 103.
[0100] S3. After the step of bending the first plate body 103 and the second plate body 104, the first plate body 103 and the second plate body 104 are welded to obtain a heat spreader.
[0101] The first plate 103 and the second plate 104 are welded together by laser welding for edge sealing. (It should be noted that in this step, the first plate 103 and the second plate 104 are welded together after being bent).
[0102] Then, the liquid injection tube is welded to the liquid inlet 121 , and pure water is injected into the inner cavity through the liquid injection tube. Subsequently, the inner cavity is evacuated (the vacuum is 0.08 torr), and then laser welding is used to weld and seal, thereby obtaining the heat spreader 100 .
[0103] An aging test is performed on the vapor chamber 100 (test conditions: 85±5° C., 12-24 h) to detect whether its performance is attenuated.
[0104] The vapor chamber 100 is subjected to an airtightness test (test conditions: helium pressure 0.16-0.6 MPa, 4 h) to detect whether its performance is attenuated.
[0105] It should be noted that the test methods and performance tests for the aging test and the airtight test may refer to the conventional settings in the field and will not be described in detail here.
[0106] The embodiments of the present invention are described in detail above. Specific examples are used herein to illustrate the principles and implementation methods of the present invention. The description of the above embodiments is only used to help understand the method of the present invention and its core idea. At the same time, for those skilled in the art, according to the idea of the present invention, there will be changes in the specific implementation methods and application scope. In summary, the content of this specification should not be understood as a limitation on the present invention.
Claims
1. A heat sink, characterized in that: include: A plate body is provided with an inner cavity, the plate body comprises a first plate body and a second plate body arranged opposite to each other, the first plate body comprises a first sub-plate body, a bent plate and a second sub-plate body, the bent plate is connected between the first sub-plate body and the second sub-plate body; and, The first reinforcing structure is connected to the first plate body and is located in the inner cavity. The first reinforcing structure has a curved section corresponding to the bent plate.
2. The vapor chamber according to claim 1, characterized in that: The first reinforcement structure includes a first reinforcement plate, which is bent, a first fluid channel is provided on a side of the first reinforcement plate close to the first plate body, and a second fluid channel is provided on a side of the first reinforcement plate close to the second plate body.
3. The heat sink according to claim 2, characterized in that: The first reinforcement structure is disposed separately from the plate body; and / or, The first reinforcing plate is integrally formed.
4. The heat sink according to claim 2, characterized in that: The first reinforcing plate includes at least one of a concave portion and a convex portion.
5. The vapor chamber according to claim 1, characterized in that: The first reinforcement structure further includes a first section and a second section, the bent section is connected between the first section and the second section, the first section corresponds to the first sub-plate body, and the second section corresponds to the second sub-plate body.
6. The vapor chamber according to claim 5, characterized in that: In the extension direction of the first sub-plate body, the size of the first reinforcement structure in the bending section is L1, the size of the first reinforcement structure in the first section is L2, and the size of the first reinforcement structure in the second section is L3, wherein L1: (L1+L2+L3)=(0.1~0.3):
1.
7. The vapor chamber according to claim 5, characterized in that: The first reinforcement structure includes a plurality of reinforcement rib groups and a reinforcement base plate. The plurality of reinforcement rib groups are arranged on the reinforcement base plate at intervals along the width direction of the first sub-plate body. Each of the reinforcement rib groups includes a plurality of first reinforcement ribs. The plurality of first reinforcement ribs are arranged at intervals along the width direction of the first sub-plate body. In the width direction of the first sub-plate body, the size of the reinforcement base plate is L4, and the size of the first reinforcement rib is L5, wherein L5:L4=(0.005~0.05):
1.
8. The vapor chamber according to claim 5, characterized in that: The first reinforcement structure includes a plurality of reinforcement rib groups, each of the reinforcement rib groups includes a plurality of first reinforcement ribs, the plurality of first reinforcement ribs are arranged at intervals along the width direction of the first sub-plate body, each of the first reinforcement ribs includes two first sub-reinforcement ribs and a plurality of second sub-reinforcement ribs, the two first sub-reinforcement ribs are respectively located in the first section and the second section, and the plurality of second sub-reinforcement ribs are arranged between the two first sub-reinforcement ribs and are located in the bending section.
9. The vapor chamber according to claim 8, characterized in that: The number of the second sub-reinforcing ribs of each of the first reinforcing ribs is n1, and the number of the first reinforcing ribs of each of the reinforcing rib groups is n2, wherein n1=n2.
10. The vapor chamber according to claim 8, characterized in that: It also includes a second reinforcement structure, which is arranged on the first sub-plate body and the second sub-plate body, and the second reinforcement structure is located in the inner cavity. The second reinforcement structure includes a plurality of reinforcing sub-ribs, and the density of the plurality of the reinforcing sub-ribs on the plate body is V1, and the density of the plurality of the second sub-reinforcing ribs on the plate body is V2, wherein V1:V2=(2~6):
1.
11. The vapor chamber according to claim 8, characterized in that: In the length direction of the first sub-plate body, the size of the first reinforcing structure in the bending section is L1, the size of the first reinforcing structure in the first section is L2, the size of the first reinforcing structure in the second section is L3, and the size of each of the second sub-reinforcement ribs is L6, wherein L6: (L1+L2+L3)=(0.03~0.2):
1.
12. The vapor chamber according to any one of claims 5 to 11, characterized in that: The first reinforcement structure is integrally formed with the plate body.
13. The vapor chamber according to any one of claims 1 to 11, characterized in that: The bending angle of the bending plate is α, and the bending angle of the bending section is β, wherein 90°≤α≤95°, 90°≤β≤95°, and α=β.
14. The vapor chamber according to any one of claims 1 to 11, characterized in that: The material of the plate body includes stainless steel; and / or, The material of the first reinforcement structure includes stainless steel.
15. A battery, characterized in that: Comprising a heat spreader as described in any one of claims 1-14.
16. A method for preparing a vapor chamber, for preparing the vapor chamber as claimed in any one of claims 1 to 14, characterized in that: The following steps are involved: bending the first plate and the second plate; The first plate body, the liquid wick, the screen and the second plate body are stacked from bottom to top; After the step of bending the first plate body and the second plate body, the first plate body and the second plate body are welded to obtain a heat spreader.
Citation Information
Patent Citations
Temperature plate and heat dissipation device
CN107529315A
Vapor chamber and manufacturing method
CN112325683A
Battery, electric device, and method and system for manufacturing battery
CN115885412A
Cooling plate, battery pack and electric equipment
CN117039255A
Liquid cooling plate and battery pack
CN217848100U
Cited By
Vapor chamber, battery and battery module
WO2026025959A1