Line scanning fast interferometric detection device for surface shape and subsurface defects in the grinding process of large-aperture optical components
Through the line scanning fast interference detection device, the line scanning technology and frequency division multiplexing data processing algorithm are used to solve the problem of inconvenient application of surface shape detection and high cost of subsurface defect detection in the grinding stage of large-diameter optical components, and the high efficiency is achieved. Accurate surface shape and defect detection provide richer grinding and processing guidance information.
Patent Information
- Application Number
- CN202411237522.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-05
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-09-05
AI Technical Summary
The prior art has problems such as inconvenient application, harsh optical detection conditions and limited range in the surface shape detection of large-diameter optical components, and the cost of subsurface defect detection is high and the efficiency is poor.
The line scanning fast interference detection device is adopted to realize the surface shape and subsurface defect detection of line scanning through light sources, signal transmission channels, dispersion elements, galvanometer systems and telecentric scanning field mirrors, and use wide spectrum low coherence light sources and frequency divisions. Multiplexing technology, synchronous detection of surface shape and defect information.
It realizes high-precision surface shape detection and subsurface defect synchronization detection in the grinding stage of large-diameter optical components, improves detection efficiency, reduces costs, has in-situ detection capabilities, has more comprehensive detection information, is applicable and flexible, and is easy to install and adjust.
Smart Images

Figure CN118758960B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of optical interference measurement, and in particular to a line scanning type rapid interference detection device for surface shape and sub-surface defects in a grinding process of a large-caliber optical element. Background Art
[0002] Currently, there is a relatively mature detection theoretical system for parameters such as surface shape and roughness during the fine polishing stage of large-aperture optical components. However, research on surface shape and sub-surface defect detection of optical components during the grinding / rough polishing stage is still insufficient, especially for sub-surface defect detection of meter-level aperture complex curved optical components, which are rarely reported at home and abroad.
[0003] Large-aperture optical surface processing usually goes through three stages: milling, grinding, and polishing. The surface deviation PV value in milling is usually more than 100 microns. The surface deviation must be converged to about 1-2 microns in grinding, and finally the optical surface processing with nanometer precision is completed through polishing. Whether it is conventional processing under the existing processing flow, or process improvement for rapid convergence of surface deviation, or more advanced processing technology research, achieving accurate and efficient surface detection under a large dynamic range is the key to promoting the manufacturing and application of large-aperture optical components.
[0004] Corresponding to different processing stages, the surface detection method used to guide processing usually transitions from contour detection with micron-level accuracy to interference detection with nanometer-level accuracy. As far as the grinding stage is concerned, due to the high surface roughness during processing (several microns to tens of microns), it is difficult to form effective optical reflection, and there is no effective non-contact optical detection method. Therefore, surface detection is mostly achieved through contour detection in which the detection mechanism is in contact with the surface. The existing technologies include three-coordinate contour detection, laser tracking contour detection, and swing arm contour detection. Among them, swing arm contour detection can also be achieved using a non-contact probe. For some components that can form a certain optical reflection on the surface at the end of the grinding process, some optical detection methods can also be used for surface detection. The existing methods include the Shack-Hartmann detection method, the infrared light interference detection method, and the fringe reflection detection method. However, the above-mentioned methods for surface shape detection in the grinding stage of optical components also have the following shortcomings. The three optical detection technologies, namely, the Shack-Hartmann detection method, the infrared light interference detection method, and the fringe reflection detection method, are only applicable to the situation where the surface has a certain optical reflection at the end of the grinding process, and cannot cover the entire grinding process cycle. The application conditions are harsh and the application scope is limited. In the three-coordinate contour detection technology, a three-coordinate measuring machine is generally used to measure the geometric morphology of large-diameter optical components. However, for optical components with a diameter of 1m or even larger, the detection accuracy of the traditional three-coordinate measurement method is only at the order of 20μm, and the large-diameter optical components must be transported to the detection machine tool, which cannot realize the in-situ rapid detection of three-dimensional morphology. Although laser tracking contour detection can realize in-situ online detection, like three-coordinate contour detection, both are contact detection, which not only brings potential surface scratches, but also the wear problem of the probe or the reflective ball itself also leads to increased detection costs. The swing-arm contour detection technology using non-contact displacement sensors requires precise adjustment of the system so that the measurement trajectory is on the closest spherical surface to the measured surface. The mutual coupling errors between the components of the system will also affect the detection accuracy. The system adjustment is difficult and the error impact is complex. At the same time, in the detection of large-caliber components, large swing-arm contour detection mechanisms occupy a large space, have high driving costs, low device flexibility, and low detection efficiency. Affected by this, during the large-caliber complex surface grinding stage, the number of quantitative full-aperture surface shape detection is reduced, and processing personnel often rely on empirical evaluation to complete the surface grinding process. The possible "under-processing" or "over-processing" caused by this will affect the subsequent surface polishing stage processing and detection, resulting in reduced component production efficiency.
[0005] In addition, modern optical systems have increasingly higher requirements on the quality of optical components. Examining only the surface quality and surface accuracy of optical components cannot meet the growing performance requirements of optical systems. Sub-surface defects have become another important parameter for evaluating the quality of optical components.
[0006] At present, the sub-surface defect detection technology of optical components is still immature. According to whether the test piece is damaged or not, the sub-surface defect detection technology can be divided into destructive detection technology and non-destructive detection technology. Destructive detection technology refers to the partial or complete destruction of the test piece, exposing the defects to be detected, and obtaining the detection results through appropriate microscopic observation technology. Representative technologies include chemical etching, cross-sectional microscopy, and angle polishing. Non-destructive detection technology uses the difference in the response of internal defects of the material to light, sound, and electricity to detect abnormalities and defects inside the material. Representative technologies include optical microscopy, ultrasonic imaging, and optical coherence tomography. However, the sub-surface defect detection technologies of these optical components also have the following shortcomings. Among them, the destructive detection methods such as chemical etching, cross-sectional microscopy, and angle polishing are only suitable for comparative experiments. In component processing inspection, the processed parts and the same type of tested parts need to be processed in the same batch, and the detection cost is extremely high. In order to cooperate with the processing progress, the detection process is extremely cumbersome; the lateral and axial detection ranges of optical microscopy technology and high-frequency scanning ultrasonic imaging technology are only up to hundreds of microns. Although optical coherence tomography technology has a millimeter-level detection range, the same point scanning imaging method makes the detection time-consuming and difficult to meet the rapid detection needs of sub-surface defects of large-diameter optical components. Summary of the invention
[0007] The present invention aims to solve the technical problems of the inconvenience of applying the existing contour detection technology in the surface shape detection of large-aperture optical components in the grinding stage, the harsh application conditions and limited application scope of optical detection technology, and the high detection cost and poor detection efficiency in sub-surface defect detection in the prior art, and provide a line scanning fast interference detection device for the surface shape and sub-surface defects of large-aperture optical components in the grinding processing stage.
[0008] In order to solve the above technical problems, the technical solutions of the present invention are as follows:
[0009] A line scanning fast interference detection device for surface shape and sub-surface defects in the grinding process of a large-aperture optical element, characterized in that the detection device replaces the traditional point scanning method with a line scanning method, and comprises: a light source, a signal transmission channel, a sample arm containing a dispersion element to generate a scanning line, a reference arm, and a spectrum detector;
[0010] The sample arm includes, in the direction of the optical path, a dispersion element, a galvanometer system, and a telecentric scanning field lens; the measured element is arranged at a position close to the telecentric scanning field lens; a beam splitter is arranged in the signal transmission channel;
[0011] in:
[0012] The light beam output by the light source is split by the beam splitter and reaches the reference arm and the sample arm respectively; the complex illumination light entering the sample arm is dispersed in one direction after passing through the dispersion element, and light waves of different frequencies enter the galvanometer system at different deflection angles; after being emitted from the galvanometer system, it is converged to the measured element by the telecentric scanning field mirror;
[0013] After illumination light of different frequencies irradiates the measured element, the generated backscattered light field returns along the original path, is combined into a complex light beam after passing through the telecentric scanning field mirror and the dispersion element, and returns to the signal transmission channel as the sample arm light signal;
[0014] In the signal transmission channel, the light signal of the sample arm interferes with the reference light signal reflected by the reference arm, and the interference spectrum signal is received by the spectrum detector and then processed.
[0015] After calculation and processing, the vector height change information of the surface of the measured component and the tomographic image from the surface to the bottom of the surface of the measured component are obtained; the surface vector height change information will be used for surface shape fitting to realize the detection of the surface shape of the measured component; the tomographic image from the surface to the bottom of the surface is used for sub-surface defect analysis to realize the detection of sub-surface defects of the measured component.
[0016] In the above technical solution, the light source is a low-coherence light source with a wide spectrum, and the output band range is selected according to the material of the component to be measured.
[0017] In the above technical solution, the spectral bandwidth of the light source is and central wavelength By axial resolution Requirements must be determined; the incident light power is determined based on the scattering characteristics of the component being measured.
[0018] In the above technical solution, the focal points of light waves of different frequencies converged on the measured element are arranged in parallel to form a spectral line, and the line length is Determined by the dispersion element parameters, the line width Determined by the parameters of the telecentric scanning field lens and the incident light beam parameters.
[0019] In the above technical solution, the spectral detector is a spectrometer.
[0020] In the above technical solution, the dispersion element is a dispersion prism, a prism or a grating.
[0021] In the above technical solution, the interference spectrum signal is processed after being received by the spectrum detector as follows:
[0022] The interference spectrum signal data is windowed and the interference spectrum is divided into m equally spaced segments, where m is an even number, corresponding to m sampling positions in the slow axis scanning direction, and the spacing of the corresponding segments is Scanning step length in fast axis scanning direction x is equal to, during the scanning sampling process, the scanning step length in the slow axis scanning direction , the m-segment interference spectrum obtained by the k-th slow axis scan comes from m consecutive sampling positions in the slow axis scan direction, , , ,……, In the continuous slow-axis scanning process, the same sampling position will correspond to m / 2 different interference spectrum segments in chronological order. These interference spectrum segments are spliced in chronological order and processed to obtain the axial depth information of the corresponding sampling point.
[0023] The present invention has the following beneficial effects:
[0024] 1) Synchronous detection of surface shape and defect information: The detection device of the present invention can realize synchronous detection of surface shape and surface / sub-surface defects of the measured component while completing high-precision surface shape detection in the grinding stage of large-aperture optical components. Unlike the traditional point scanning method, the line scanning method expands the scanning field of view and improves the detection efficiency by at least one time. In addition, the line scanning method proposed in the present invention does not require an increase in camera cost, but only requires an additional dispersion element to the sample arm. The parallel data of the scanning line is processed by the data processing algorithm of the present invention, and the detection results can be displayed in an intuitive high-contrast image. The detection information of the detection device is more comprehensive, and can provide richer guidance information for the grinding process.
[0025] 2) Flexible application and in-situ detection capability: The detection device of the present invention adopts a modular design, the probe part can be integrated and packaged separately, and the signal transmission is realized by optical fiber through a reserved interface. In terms of surface shape detection of large-aperture optical components, compared with the swing arm profilometer, the detection device of the present invention does not involve large mechanical moving components, and has a small size and light weight. At the same time, since the probe does not involve complex motion trajectory transmission, the motion drive of the probe will be more flexible and free, and parallel in-situ detection can be realized in conjunction with the grinding process.
[0026] 3) Low cost and easy installation and adjustment: Compared with the prior art, the detection device of the present invention greatly reduces the detection cost in the application of synchronous detection of surface shape and defects; at the same time, the various parts of the detection device have simple structures and high stability. It only needs to add a dispersion element to the traditional point scanning system. The installation and adjustment process only involves lateral or axial distance deviations. The error impact is relatively single and no coupling occurs, and the system installation and adjustment is relatively simple.
[0027] 4) Fast and efficient: The detection device of the present invention uses linear beam scanning to complete sampling detection. The operating frequency of the galvanometer that generates beam scanning can reach up to 100 kHz. At the same time, the line scanning sampling adopted by the system reduces the deflection step number required in the slow axis direction of the galvanometer by half compared with the point scanning sampling, further improving the sampling efficiency. For large-aperture optical components of about 1m, it is expected to complete the synchronous detection of surface shape and defects in the full aperture range within 30 minutes. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] The present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments.
[0029] Figure 1 The present invention is a flow chart of data collection and processing of a line scanning rapid interference detection device for surface shape and sub-surface defects in the grinding process of a large-aperture optical element.
[0030] Figure 2 The present invention is a block diagram of the composition of the line scanning type rapid interference detection device for surface shape and sub-surface defects in the grinding process stage of a large-aperture optical element.
[0031] Figure 3 It is a schematic diagram of point scanning and extended spectrum line scanning of the line scanning fast interference detection device for surface shape and sub-surface defects in the grinding process stage of a large-aperture optical element of the present invention.
[0032] Figure 4 The figure is a schematic diagram of interference spectrum separation processing of the line scanning type rapid interference detection device for surface shape and sub-surface defects in the grinding process stage of a large-aperture optical element of the present invention.
[0033] Figure 5 It is a schematic diagram of the frequency flow data acquisition principle of the line scanning fast interference detection device for surface shape and sub-surface defects in the grinding process stage of large-aperture optical elements of the present invention.
[0034] Figure 6 The present invention is a data splicing process flow chart of the line scanning type rapid interference detection device for surface shape and sub-surface defects in the grinding process stage of large-aperture optical elements.
[0035] Figure 7 The present invention is a schematic structural diagram of a specific implementation of a line scanning fast interference detection device for surface shape and sub-surface defects in the grinding process of a large-aperture optical element.
[0036] Figure 8 Schematic diagram of the Michelson interferometer principle. DETAILED DESCRIPTION
[0037] The inventive concept of the present invention is:
[0038] The line scanning type fast interference detection device for surface shape and sub-surface defects in the grinding process of large-caliber optical elements of the present invention realizes accurate and fast detection of the whole process of grinding process of large-caliber optical elements through line scanning technology and frequency division multiplexing data processing algorithm: adopting line scanning sampling can more efficiently realize in-situ surface shape detection in parallel with the grinding process, and synchronously display the sub-surface structure information of the measured area through tomography, and realize non-destructive online real-time detection of sub-surface defects such as cracks, cavities, stress deformation, etc. that may be generated during the grinding process. It is beneficial to improve the grinding efficiency of large-caliber optical elements and realize high-precision and high-quality connection with polishing, and is more conducive to the reasonable evaluation of grinding process and process improvement research.
[0039] The line scanning rapid interference detection device for surface shape and sub-surface defects of large-aperture optical elements in the grinding process stage of the present invention applies frequency division multiplexing line scanning interference tomography technology based on low-coherence wide-spectrum light source to rapid interference detection of surface shape and sub-surface defects of large-aperture optical elements.
[0040] The invention discloses a line scanning rapid interference detection device for surface shape and sub-surface defects in the grinding process of a large-aperture optical element. The device is used to realize the linear expansion of the illumination beam in the sample space in a spectrally separated manner and the normal collection of scattered light in different spectral bands. This function is realized by a dispersion element.
[0041] The line scanning fast interference detection device for surface shape and sub-surface defects in the grinding process of large-aperture optical elements of the present invention is used for the "frequency flow" information processing mechanism of the line scanning optical coherence tomography system. For different sampling positions, the spectrum segments of the corresponding positions are extracted from the multi-frame interference spectrum data arranged in time sequence, and then sequentially spliced, and the axial depth (A-scan) interference spectrum data at the corresponding different sampling positions are synthesized and the related information is solved, so as to expand the lateral field of view without sacrificing the axial resolution, scanning density and signal-to-noise ratio.
[0042] The detection principle of the line scanning fast interference detection device of the present invention is based on Figure 8 The Michelson interferometer principle shown in Figure 8 Only some component names are shown in the figure). Light field emitted by a low-correlation light source After passing through the spectroscope, the light is transmitted to the reference arm, the reflector, the sample arm, and the measured element respectively. The light field reflected by the reflector and the light field backscattered by different depth layers of the measured element return along the original path and then aliased to form an interference light field after passing through the spectroscope. , for the interference light field Detection and solution can be performed to obtain the optical path differences along the optical axis of the sample arm. Corresponding interference intensity information. After obtaining the interference intensity information of different lateral and axial positions of the measured component through two-dimensional scanning by the galvanometer, the three-dimensional structural information of the measured component can be extracted.
[0043] Since the traditional low-coherence interference detection device adopts a point scanning method, the lateral field of view increases in the detection of large-aperture components. If you want to ensure the sampling timeliness, you need to sacrifice the sampling density. If you want to ensure the sampling density, you need to sacrifice the sampling timeliness. The line scanning type fast interference detection device proposed in the present invention adopts line scanning sampling. Compared with the point scanning method, it can ensure higher sampling timeliness under the premise of the same sampling density. At the same time, the device is based on frequency division multiplexing sampling. Different from the general line scanning sampling, each sampling point is synchronously irradiated by the same wide-spectrum light wave. During the operation of this device, each sampling point will be irradiated in sequence by a series of different narrow-spectrum light waves within the wide spectrum range, and then the total spectral irradiation of each sampling point is guaranteed to be consistent through sequential splicing. Compared with the general line scanning method, the signal-to-noise ratio of the sampling result is higher.
[0044] The line scanning type rapid interference detection device for surface shape and sub-surface defects in the grinding process of large-aperture optical elements of the present invention is described in detail below with reference to the accompanying drawings.
[0045] The invention discloses a line scanning fast interference detection device for surface shape and sub-surface defects of large-aperture optical elements in the grinding process. The detection device replaces the traditional point scanning method with a line scanning method. Figure 2 As shown, it includes: a light source, a signal transmission channel, a sample arm with a dispersion element to generate a scan line, a reference arm, and a spectrum detector. In the sample arm, in the direction of the light path, it includes: a dispersion element, a galvanometer system, and a telecentric scanning field lens; the measured element is set at a position close to the telecentric scanning field lens; and a beam splitter is provided in the signal transmission channel.
[0046] The light source is a low-coherence light source with a wide spectrum. The output band range can be selected according to the material of the component to be tested. Generally, the infrared band with a larger penetration depth is selected; spectral bandwidth and central wavelength By axial resolution Requirements are determined by the formula Description. The incident light power is determined according to the scattering characteristics of the measured element. Due to the regular changes in the irradiation spectrum corresponding to different sampling positions during the frequency division multiplexing sampling process, compared with the traditional scanning method, since different spectrum bands correspond to different positions, the light power of a single spectrum band is greater, so each sampling position has a higher signal-to-noise ratio.
[0047] The light signal output by the light source reaches the reference arm and the sample arm through the signal transmission channel. The complex illumination light ( Figure 2The middle line A shows that after passing through the dispersion element (dispersion prism, prism or grating, etc.), unidirectional dispersion is generated. Light waves of different frequencies enter the galvanometer system at different deflection angles. After exiting, they are focused by the telecentric scanning field mirror toward the measured element. The focusing points of light waves of different frequencies are arranged in parallel to form Figure 2 A spectral line is shown in Determined by the dispersion element parameters, the line width It is determined by the parameters of the telecentric scanning field mirror and the parameters of the incident light beam. Through the high-speed two-dimensional deflection of the light beam by the galvanometer system, the lateral two-dimensional scanning of the spectrum line on the measured element can be achieved.
[0048] When illumination light of different frequencies irradiates the measured element, the generated backscattered light field returns along the original path, and then is combined into a complex light beam after passing through the telecentric scanning field mirror and the dispersion element ( Figure 2 The light from the sample arm is reflected by the reference arm (shown as line A in the middle), and returns to the signal transmission channel as the sample arm light signal. In the channel, the sample arm light signal interferes with the reference light signal reflected by the reference arm, and the interference spectrum signal is received by the spectrum detector. It is then read to the computer through the information acquisition card to complete the corresponding information solution. Finally, after data processing, the vector height change information on the surface of the measured component and the tomographic image from the surface to below the surface of the measured component will be obtained. The surface vector height change information will be used for surface shape fitting to detect the surface shape of the measured component; the tomographic image from the surface to below the surface will be used for sub-surface defect analysis to detect sub-surface defects of the measured component.
[0049] like Figure 3 As shown in the figure, the sampling process of the line scanning fast interference detection device of the present invention is similar to the point scanning sampling process, both of which adopt a grid scanning method that moves along the X direction and the Y direction with a certain step length. Different from the point scanning sampling, in the extended spectrum line scanning sampling of the present invention, the scanning step length in the slow axis scanning direction is Scan step length in the fast axis scanning direction twice, that is .
[0050] At the same time, since the sampling lines are spread out in the form of spectra in the sample space, the system will adopt a "frequency flow" information processing mechanism. For the spectral lines that are broadened in the slow axis scanning direction, the backscattered light in the coverage area interferes with the reference light and is collected and recorded by the spectrometer as interference spectrum data. Figure 4 As shown in the figure, the interference spectrum data can be divided into m (m is an even number) equally spaced spectral segments by windowing, corresponding to the sampling positions in the m slow axis scanning direction, and the spacing of the corresponding spectral segments is Scanning step length in fast axis scanning direction x is equal, that is x. During the scanning sampling process, the scanning step length in the slow axis scanning direction , the m interference spectra obtained from the k-th slow-axis scan come from m consecutive sampling positions in the slow-axis scan direction, that is , , , ……, . Correspondingly, during consecutive slow-axis scans, the same sampling position will correspond to m / 2 different interference spectrum segments in chronological order. By splicing these interference spectrum segments in chronological order and performing arithmetic processing, the axial depth (A-scan) information of the corresponding sampling point can be obtained.
[0051] Only when the number of slow-axis scan times k and the number of interference spectrum segment separations m satisfy the relationship , can the data processing of spectral splicing start from the sampling positions corresponding to the two end spectra in the first scan. As Figure 6 shown, for the sampling points with the slow-axis direction position coordinate value j < m - 1, due to insufficient spliced data, the complete spectral splicing of the corresponding sampling points cannot be achieved. Only the sampling points with the slow-axis direction position coordinate value j ≥ m - 1 can obtain complete spectral data through splicing.
[0052] When it is determined that j is odd, the current scan order number is determined, the segmented spectral data of the i-th fast-axis scan and the k-th to k + m / 2 - 1-th frames of slow-axis scans are extracted, and then the m - 1-th segment of the k-th frame of slow-axis scan spectrum, the m - 3-th segment of the (k + 1)-th frame of slow-axis scan spectrum... the 1-st segment of the (k + m / 2 - 1)-th frame of slow-axis scan spectrum are extracted in sequence. The above segments of spectra are spliced in order to form the axial depth (A-scan) interference spectral data at the sampling point with the coordinate value (i, j).
[0053] When it is determined that j is even, the current scan order number is determined, the segmented spectral data of the i-th fast-axis scan and the k-th to k + m / 2 - 1-th frames of slow-axis scans are extracted, and then the m-th segment of the k-th frame of slow-axis scan spectrum, the m - 2-th segment of the (k + 1)-th frame of slow-axis scan spectrum... the 2-nd segment of the (k + m / 2 - 1)-th frame of slow-axis scan spectrum are extracted in sequence. The above segments of spectra are spliced in order to form the axial depth (A-scan) interference spectral data at the sampling point with the coordinate value (i, j).
[0054] In summary, the m / 2 different interference spectrum segments corresponding to the sampling points where complete spectral data splicing can be achieved are spliced in chronological order and expressed as: In the formula,
[0055]
[0056]
[0057] where is the sampling point The interference spectrum data is formed by splicing in chronological order. It represents the xth segment of the m-segment interference spectrum obtained by the i-th fast-axis scan and the n-th slow-axis scan; k is the slow-axis scan order number, which is 1, 2, 3, 4, ..., and the value of k increases by 1 every time j increases by 2 from the initial value.
[0058] For example, Figure 5 The figure shows that the interference spectrum is divided into m=14 spectral segments after windowing. As the scanning order in the slow axis direction increases to the 7th time, the sampling position in the slow axis direction can be The spectral segment splicing process starts at The interference spectrum after splicing is "the 13th segment of the 1st frame data + the 11th segment of the 2nd frame data + the 9th segment of the 3rd frame data + the 7th segment of the 4th frame data + the 5th segment of the 5th frame data + the 3rd segment of the 6th frame data + the 1st segment of the 7th frame data". The interference spectrum after splicing is "the 14th segment of the 2nd frame data + the 12th segment of the 3rd frame data + the 10th segment of the 4th frame data + the 8th segment of the 5th frame data + the 6th segment of the 6th frame data + the 4th segment of the 7th frame data + the 2nd segment of the 8th frame data". And so on. According to this frequency division multiplexing method, the axial depth (A-scan) interference spectrum data at different sampling positions can be obtained, and the axial depth (A-scan) tomography results of the corresponding sampling positions can be obtained after further solution. During the scanning process, the interference spectra of different frequency bands corresponding to different sampling positions are spliced and solved in turn, and finally the vector height change information and three-dimensional tomographic images of the surface of the measured component are obtained.
[0059] Figure 7 FIG. 1 is a schematic structural diagram of a specific embodiment of a line scanning type fast interference detection device for surface shape and sub-surface defects in the grinding process of a large-aperture optical element of the present invention. The data acquisition and data splicing processing processes of the line scanning type fast interference detection device of the present invention are respectively as follows: Figure 1 and 6 As shown, the following is a specific description:
[0060] 1) The line scanning fast interference detection device of the present invention comprises:
[0061] The line scanning fast interference detection device for surface shape and sub-surface defects of large-aperture optical elements during the grinding process of the present invention is a frequency division multiplexing line scanning bright and dark field synchronous interference measurement system, which adopts a Michelson interferometer structure, such as Figure 7As shown, it includes: a broadband light source, a signal transmission channel, a sample arm, a reference arm and a spectrometer; wherein, in the sample arm, in the direction of the light path, it includes: a dispersion prism, an X-direction galvanometer and a Y-direction galvanometer, and a telecentric scanning field mirror in sequence; wherein, the broadband light source is the light source, the dispersion prism is the dispersion element, and the galvanometer system includes: an X-direction galvanometer and a Y-direction galvanometer. The component to be measured is set at a position close to the telecentric scanning field mirror;
[0062] The signal transmission channel is provided with a beam splitter, an optical fiber jumper and a polarization controller. In the signal transmission channel, a collimating lens and a polarization controller are provided on the optical path between the beam splitter and the sample arm and the reference arm, respectively; a collimating lens is provided on the optical path between the beam splitter and the light source and the spectrum detector, respectively.
[0063] The light beam emitted by the broadband light source is collimated by the collimating lens and then divided into two parts by the beam splitter. One part enters the reference arm through the collimating lens and polarization controller, and the other part is introduced into the sample arm through the collimating lens, fiber jumper, and polarization controller. In the sample arm, the illumination beam is dispersed in one direction after passing through the dispersion prism. The light beams of different spectral bands pass through the two-dimensional scanning galvanometer (X-direction galvanometer and Y-direction galvanometer) and enter the telecentric scanning field mirror and finally converge at the measured element. The scattered light of each spectral band generated returns along the original transmission path of the illumination beam of each spectral band, and after being combined by the dispersion prism, it is coupled into the fiber jumper again and continues to propagate, and finally interferes with the reference light reflected from the reference arm. The interference spectrum signal is transmitted to the spectrometer for reception.
[0064] In the device, the sample arm part can be encapsulated as a movable sample arm probe so as to be fixed on a mechanical arm or other motion mechanism, thereby realizing sub-aperture splicing detection of surface shape and sub-surface defects of large-aperture optical elements.
[0065] 2) Working principle of the line scanning fast interference detection device of the present invention:
[0066] The interference spectrum signal involved in the device is generated by a Michelson interferometer. Since the time delay of the reflected light signals of the reference arm and the sample arm is related to the structural information of the surface and the subsurface of the measured element, it is manifested as different frequency modulations generated on the broadband spectrum. For the line scanning fast interference detection device of the present invention, the interference spectrum signal received by the spectrometer is not directly used, but the interference spectrum data after splicing processing according to the time sequence is used (the splicing processing flow is as follows Figure 6 As shown), if a sampling position corresponds to the interference spectrum By n-segment spectrum ( ), which can be expressed as:
[0067]
[0068] In the formula, Represents the sample arm length corresponding to different layers of the measured component, represents the back reflection coefficient of different layers of the measured element, is the reference arm length, the back reflection coefficient at the reference arm reflector is a(R), S(k) is the light source power spectral density, k is the wave number ( , is the angular frequency, is the speed of light), Representative index , Represents the imaginary part of the complex number. Assuming that the amplitude and phase of the light source are not modulated after entering the reference arm, set a(R)=1. At the same time, assume that the common reference plane with the reference arm in the sample arm space is at the position of the reference arm reflector, so R=0, and the distance between different layers of the measured element and the common reference plane is Z (reference mirror virtual image position), and the following simplified interference spectrum signal can be obtained:
[0069] in, The inverse Fourier transform of A(k) is the axial reflectivity distribution a(Z) of different layers of the measured element.
[0070] After performing the following inverse Fourier transform on the above spectral signal, we get:
[0071]
[0072] in, is the envelope of the autocorrelation function of the light source, that is, the power spectral density of the light source The inverse Fourier transform of .
[0073] In the above formula, It is the DC term at zero optical path z=0, which is the autocorrelation term of the reference arm and accounts for most of the spectral signal intensity; is the autocorrelation item of the sample's depth information, which is distributed near the zero optical path and has a relatively small amplitude. After filtering out the DC term and the sample autocorrelation term, the axial distribution structural information a(z) and a(-z) at a certain sampling position of the measured element is obtained. They are a set of mirror images symmetrical relative to the zero optical path position. In order to prevent aliasing, the position of the measured element is usually adjusted to one side of the zero optical path during detection, that is, a quantitative offset is introduced relative to the zero optical path. According to the systematic sampling process, after combining the axial distribution structural information of the above series of sampling positions, the transverse and axial structural information of the sample can be obtained.
[0074] 3) Data collection and processing:
[0075] The data collection and processing will be realized by software. The data collection and processing flow of the line scanning fast interference detection device for surface shape and sub-surface defects in the grinding process of large-aperture optical elements of the present invention is as follows: Figure 1 shown.
[0076] During the test, the software will first determine the sampling area size and sampling point size through human-computer interaction, and then determine the scanning step length and the spectral window size and the number of spectral windows m. The generated control parameters will be confirmed and input by the personnel to start line scanning sampling. The driving electrical signal command is issued to control the X-direction galvanometer and Y-direction galvanometer in the galvanometer system to perform two-dimensional stepping deflection movement. During the movement of the X-direction galvanometer and the Y-direction galvanometer, the driving electrical signal also triggers the spectral detector to be exposed, so that the spectrometer can obtain the interference spectrum data of the corresponding position with the galvanometer step scanning. In the same period, the data acquisition card receives the command, reads out the data of the spectral detector in sequence and transmits it to the computer memory for sequential storage. The above process is repeated until the line scanning sampling is completed, and finally an interference spectrum database corresponding to different sampling positions is formed.
[0077] During the data acquisition process, when the computer determines that the slow axis scanning order p≥m / 2, the computer CPU will start to read the relevant frame data from the interference spectrum database in parallel according to the program design, and form multi-frame separated spectrum data through window separation processing, and perform spectrum splicing and calculation processing on the corresponding series of sampling points. Specifically, if a total of p (p>m / 2) slow axis step scans are required to complete the sampling of a certain area, and each slow axis scan corresponds to q fast axis step scans, the data splicing processing of the A-scan interference spectrum segment will be carried out after the acquisition of the first fast axis scan interference data corresponding to the m / 2 slow axis scan is completed, that is, from the sampling point , Start along the sampling point , After the q fast-axis scans corresponding to the m / 2th slow-axis scan are completed, the q fast-axis scans corresponding to the m / 2+1th slow-axis scan are continued, and the scanning points are scanned in the same direction. , The multi-spectral data of each sampling point are spliced in the same direction. This process is repeated until the scanning sampling of the entire sampling area and the splicing and calculation of the interference spectrum of the corresponding sampling points are completed, and the axial depth (A-scan) data of the series of sampling positions are obtained and stored in sequence, and finally a coherent tomography database of the sampling area is formed for subsequent detection result analysis.
[0078] In the above process, the software interface will display the spliced spectral data and the tomographic images processed by GPU acceleration in real time, which can be used to evaluate the quality of the collected data online. After saving the test data, the software can continue to be used to complete the surface fitting calculation and offline image processing and analysis.
[0079] The detection device of the present invention can not only complete the high-precision surface shape detection of large-diameter optical components during the grinding stage, but also realize the surface / sub-surface defect detection of the measured components, and the detection results can be presented in an intuitive high-contrast image. The detection information of the device is more comprehensive and can provide richer guidance information for grinding processing.
[0080] The detection device of the present invention adopts a modular design, the probe part is separately integrated and packaged, and the signal transmission is realized by optical fiber through a reserved interface. In terms of the surface shape detection of large-aperture optical components, compared with the swing arm profilometer, the detection device of the present invention does not involve large mechanical moving components, and has a small size and light weight. At the same time, since the probe does not involve complex motion trajectory transmission, the motion drive of the probe will be more flexible and free, and parallel in-situ detection can be realized in conjunction with the grinding process.
[0081] Compared with the existing technical solutions, the detection device of the present invention greatly reduces the detection cost in the application of simultaneous detection of surface shape and defects; at the same time, the various parts of the detection device have simple structures and high stability. It only needs to add a dispersion element to the traditional point scanning system. The adjustment process only involves lateral or axial distance deviations. The error impact is relatively single and no coupling occurs, and the device adjustment is relatively simple.
[0082] The detection device of the present invention uses linear beam scanning to complete sampling detection. The operating frequency of the galvanometer that generates beam scanning can reach up to 100 kHz. At the same time, the line scanning sampling adopted by the device reduces the deflection step number required in the slow axis direction of the galvanometer by half compared with the point scanning sampling, further improving the sampling efficiency. For large-aperture optical components of about 1m, it is expected to complete the synchronous detection of surface shape and defects in the full aperture range within 30 minutes.
[0083] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the invention.
Claims
1. A line scanning fast interference detection device for surface shape and sub-surface defects in the grinding process of large-aperture optical components, characterized in that: The detection device replaces the traditional point scanning method with a line scanning method, and includes: a light source, a signal transmission channel, a sample arm containing a dispersion element to generate a scanning line, a reference arm, and a spectrum detector; The sample arm includes, in the direction of the optical path, a dispersion element, a galvanometer system, and a telecentric scanning field lens; the measured element is arranged at a position close to the telecentric scanning field lens; a beam splitter is arranged in the signal transmission channel; in: The light beam output by the light source is split by the beam splitter and reaches the reference arm and the sample arm respectively; the complex illumination light entering the sample arm is dispersed in one direction after passing through the dispersion element, and light waves of different frequencies enter the galvanometer system at different deflection angles; after being emitted from the galvanometer system, it is converged to the measured element by the telecentric scanning field mirror; After illumination light of different frequencies irradiates the measured element, the generated backscattered light field returns along the original path, is combined into a complex light beam after passing through the telecentric scanning field mirror and the dispersion element, and returns to the signal transmission channel as the sample arm light signal; In the signal transmission channel, the light signal of the sample arm interferes with the reference light signal reflected by the reference arm, and the interference spectrum signal is received by the spectrum detector and then processed. After calculation and processing, the surface vector height change information of the measured component and the tomographic image from the surface to the bottom of the surface of the measured component are obtained; the surface vector height change information will be used for surface shape fitting to realize the detection of the surface shape of the measured component; the tomographic image from the surface to the bottom of the surface is used for sub-surface defect analysis to realize the detection of sub-surface defects of the measured component; The interference spectrum signal is received by the spectrum detector and then processed as follows: The interference spectrum signal data is windowed and the interference spectrum is divided into m equally spaced spectrum segments, where m is an even number and corresponds to m sampling positions in the slow axis scanning direction. The spacing S of the corresponding spectrum segments is equal to the scanning step length Δx in the fast axis scanning direction. During the scanning sampling process, the scanning step length Δy in the slow axis scanning direction is 2Δx. The m interference spectrum segments obtained by the kth slow axis scanning come from m consecutive sampling positions in the slow axis scanning direction, 2(k-1)+1, 2(k-1)+2, 2(k-1)+3, ..., 2(k-1)+m. During the continuous slow axis scanning process, the same sampling position will correspond to m / 2 different interference spectrum segments in chronological order. These interference spectrum segments are sequentially spliced in chronological order and processed to obtain the axial depth information of the corresponding sampling points.
2. The line scanning rapid interference detection device for surface shape and sub-surface defects in the grinding process of large-aperture optical elements according to claim 1 is characterized in that: The light source is a low-coherence light source with a wide spectrum, and the output waveband range is selected according to the material of the component to be tested.
3. The line scanning rapid interference detection device for surface shape and sub-surface defects in the grinding process of large-aperture optical elements according to claim 2, characterized in that: The spectral bandwidth Δλ and the central wavelength λ0 of the light source are determined by the axial resolution δz requirement; the incident light power is determined according to the scattering characteristics of the measured element.
4. The line scanning rapid interference detection device for surface shape and sub-surface defects in the grinding process of large-aperture optical elements according to claim 1, characterized in that: The focal points of light waves of different frequencies converging toward the measured element are arranged side by side to form a spectral line. The line length l is determined by the dispersion element parameters, and the line width w is determined by the telecentric scanning field lens parameters and the incident light beam parameters.
5. The line scanning rapid interference detection device for surface shape and sub-surface defects in the grinding process of large-aperture optical elements according to claim 1, characterized in that: The spectrum detector is a spectrometer.
6. The line scanning fast interference detection device for surface shape and sub-surface defects in the grinding process of large-aperture optical elements according to claim 1, characterized in that: The dispersion element is a dispersion prism, a prism or a grating.