Lithium supplement agent and preparation method and application thereof

By using a combination of lithium oxalate, carbon materials, catalysts and modifiers in lithium-ion batteries to prepare hollow spherical particle lithium replenishing agents, the problems of high decomposition voltage and low decomposition efficiency of lithium oxalate are solved, and the energy density and energy density of the battery are improved. cycle life.

CN118763219AActive Publication Date: 2024-10-11NINGBO RONBAY LITHIUM BATTERY MATERIAL CO LTD

Patent Information

Application Number
CN202411216012.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-02
Publication Date
2024-10-11
Estimated Expiration
2044-09-02

AI Technical Summary

Technical Problem

Lithium oxalate has high decomposition voltage, low decomposition efficiency, and small application range in lithium-ion batteries, which limits its application as a lithium supplement additive for the cathode.

Method used

A combination of lithium oxalate, carbon materials, catalysts and modifiers is used to prepare hollow spherical particle lithium supplementation agents through ultrasonic dispersion and spray drying processes. Fast ion conductors and lithiophilic agents are added to reduce the initial decomposition voltage of lithium oxalate and increase lithium ions. migration rate.

Benefits of technology

Significantly reduces the decomposition voltage of lithium oxalate, improves the transmission efficiency of lithium ions, enhances the energy density and cycle life of the battery, and improves the contact area with the electrode material and the wettability of the electrolyte through the hollow rupture structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118763219A_ABST
    Figure CN118763219A_ABST
Patent Text Reader

Abstract

The invention provides a lithium supplement agent and a preparation method and application thereof, the lithium supplement agent comprises lithium oxalate, a carbon material, a catalyst and a modifier, and the modifier comprises at least one of a fast ion conductor and / or a lithium affinity agent; wherein the mass ratio of the lithium oxalate to the carbon material to the catalyst to the modifier is (70-95): (2.5-14): (2.5-14): (0.1-1). Through the synergistic effect of lithium oxalate, a carbon material, a catalyst and a modifier, the initial decomposition voltage and the average decomposition voltage of lithium oxalate are remarkably reduced, meanwhile, the lithium supplementing effect of lithium oxalate is improved, the initial decomposition voltage of lithium oxalate can be assisted to be reduced by adding a fast ion conductor and / or a lithium-philic agent, and the lithium supplementing effect of lithium oxalate is improved. Therefore, lithium ions can be separated from lithium oxalate more quickly, migration of the lithium ions on the surface of the electrode material is accelerated, and internal resistance is reduced. The lithium supplement agent provided by the invention is high in electrochemical activity, the decomposition voltage is as low as 4.14 V, and the lithium supplement agent has a relatively large specific surface area and can be in good contact with an electrode material and an electrolyte.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of lithium-ion batteries, and in particular to a lithium supplement agent and a preparation method and application thereof. Background Art

[0002] Pre-lithiation technology plays an important role in the development of lithium-ion batteries with high energy density and long cycle life. At present, pre-physical and chemical technologies are mainly divided into positive electrode and negative electrode pre-lithiation. Compared with positive electrode pre-lithiation, negative electrode pre-lithiation faces the problems of high reaction activity and poor stability of active lithium sources. However, the lithium sources of positive electrode lithium replenishment reagents such as Li3P, Li2S and Li5FeO4 also have reaction residues and poor stability in humid air, which seriously limits their application scenarios and scale. Therefore, the development direction of positive electrode lithium replenishers is low reaction residue, high lithium replenishment capacity and high air stability.

[0003] After lithium oxalate (Li2C2O4) is fully decomposed in the battery, it produces carbon dioxide (CO2). During the battery formation process, this CO2 is completely discharged from the battery system, leaving no residue. Furthermore, lithium oxalate is highly air-stable and safe. Therefore, its zero residue, high capacity, and high air-stability make it an ideal lithium supplement.

[0004] However, the actual decomposition potential of unmodified lithium oxalate is as high as 4.7 V, which severely limits its application as a positive electrode lithium supplement. Therefore, there is an urgent need to provide a modified lithium oxalate lithium supplement to address the problems of high decomposition voltage, low decomposition efficiency, and limited application range of lithium oxalate in the existing technology. Summary of the Invention

[0005] The technical problems to be solved by the present invention are the high decomposition voltage, low decomposition efficiency and small application range of lithium oxalate.

[0006] To solve the above problems, the present invention provides a lithium supplement agent, which includes lithium oxalate, a carbon material, a catalyst and a modifier, and the modifier includes at least one of a fast ion conductor and / or a lithium-philic agent; wherein the mass ratio of lithium oxalate, carbon material, catalyst and modifier is (70-95): (2.5-14): (2.5-14): (0.1-1).

[0007] The lithium supplement provided by the present invention includes lithium oxalate, a carbon material, a catalyst and a modifier. Among them, lithium oxalate is used as the core component of the lithium supplement and is used in the battery to replenish the active lithium ions consumed when the SEI film is formed, thereby improving the cycle performance and energy density of the battery; the carbon material is used to improve the conductivity and structural stability of the electrode, which helps the battery maintain performance during the charge and discharge process; the catalyst can reduce the reaction activation energy, thereby reducing the initial decomposition voltage of lithium oxalate and accelerating the decomposition reaction of lithium oxalate; the modifier includes a fast ion conductor and / or a lithium affinity agent. The modifier can significantly increase the migration rate of lithium ions on the surface of the lithium supplement, accelerate the release of lithium ions, and thus optimize the transmission efficiency of lithium ions.

[0008] The present invention significantly improves the energy density and cycle life of batteries through the synergistic effects of lithium oxalate, carbon materials, catalysts, and modifiers. The addition of a fast ion conductor and / or a lithiophile allows lithium ions to escape from the surface of the lithium oxalate material more quickly, increasing the rate of lithium ion migration and thus reducing the decomposition voltage of lithium oxalate, leading to faster decomposition.

[0009] In any of the above technical solutions, the lithium supplement agent is a hollow spherical particle, and some of the particles have a hollow fracture structure.

[0010] Hollow spherical particles refer to the hollow spherical structure formed during the preparation process of the lithium supplement. This structure gives the particles a low physical density and a large specific surface area, allowing them to better contact with the electrode material. The rupture or collapse of the hollow spherical particles increases the contact area with the electrode material and the wettability with the electrolyte, which can provide a better lithium supplement effect.

[0011] In any of the above technical solutions, the proportion of particles with hollow fracture structures to the total number of particles is 10%-99%.

[0012] Particles with a hollow fracture structure have a higher proportion, which can increase the surface area and porosity of the material, thereby increasing the contact area with the electrode material and the wettability of the electrolyte, thereby improving the lithium replenishment effect of the lithium replenisher.

[0013] In any of the above technical solutions, the specific surface area of ​​the lithium supplement is 60m 2 / g-170m 2 / g.

[0014] The lithium supplement agent provided by the present invention has a hollow rupture structure, which enables the lithium supplement agent to have a higher specific surface area, which not only increases the contact area with the electrode material, but also improves the wettability with the electrolyte, thereby ensuring a better lithium supplement effect.

[0015] In any of the above technical solutions, the fast ion conductor includes Li4Ti5O 12, Li3PO4, Li2Zr2(PO4)3, LiPO2F2, LiF, LiNO3, LiAlO2; and / or the lithium-philic agent includes at least one of Si, S, P; and / or the catalyst includes at least one of a transition metal element and a transition metal compound; and / or the carbon material includes at least one of Ketjen black, Super-P conductive carbon black, CNTs, redox graphene, polyvinyl pyrrolidone, and tannic acid.

[0016] Fast ion conductors have excellent ion transport capabilities and structural stability. When added in appropriate amounts, they can improve the surface conductivity of the material and accelerate the release of lithium ions without reducing the performance of the material itself. LiPO2F2 has a three-dimensional structure in its crystal structure. Free lithium ions can diffuse freely in multiple directions in three-dimensional space, further enriching the diffusion path of lithium ions and reducing impedance, thereby achieving the purpose of reducing the decomposition voltage of lithium oxalate and promoting the decomposition of lithium oxalate; Li4Ti5O 12 As a fast ion conductor, it not only improves the conductivity, but also has the characteristic of "zero strain". + When the lattice constant and volume of the crystal change very little, it can stably promote the decomposition reaction of lithium oxalate, and its chemical properties are stable and it does not react with the electrolyte.

[0017] Transition metals, such as iron, cobalt, and nickel, are effective catalyzers of a wide variety of chemical reactions due to their unique electronic structures and variable oxidation states. The use of transition metal catalysts can significantly increase the rate of chemical reactions, allowing them to be completed quickly under milder conditions, thereby saving energy and time. Transition metal compounds, such as molybdenum trioxide and cobalt oxide, exhibit high efficiency and specific activity in catalyzing specific reactions. These compounds possess high chemical reactivity and selectivity.

[0018] Ketjen black (KB) is a highly structured conductive carbon black with a high specific surface area and electrical conductivity. Super-P conductive carbon black is an ultrafine carbon black with excellent electrical conductivity and stability. Carbon nanotubes (CNTs) have ultra-high strength and electrical conductivity and are used to strengthen composite materials, conductive channels in electronic devices, etc. Redox graphene has a unique two-dimensional structure and excellent electronic conductivity. Polyvinylpyrrolidone (PVP) is added as a stabilizer and dispersant together with other carbon sources to improve the processability and compatibility of the material and reduce agglomeration. Tannic acid has an excellent coating effect and can be immediately coated on the surface of the material under neutral conditions, achieving controllable and uniform coating of the material. The above-mentioned carbon materials can provide excellent electrical conductivity and thermal stability, and enhance the overall performance of the final product.

[0019] The present invention also provides a method for preparing a lithium supplement, which is used to prepare the lithium supplement as described above, and comprises the following steps: S100: dissolving lithium oxalate, and then adding a carbon material, a catalyst, and a modifier to obtain a mixed solution; S200: sequentially subjecting the mixed solution to ultrasonic dispersion, spray drying, and crushing to obtain the lithium supplement; wherein the mass fraction of lithium oxalate in the mixed solution is 1%-5.5%.

[0020] The present invention provides a method for preparing a lithium supplement. The method involves first dissolving lithium oxalate in a suitable solvent, followed by the addition of a carbon material, a catalyst, and a modifier. This step aims to reduce the initial and average decomposition voltages of lithium oxalate, thereby enhancing its lithium supplementation efficacy. The resulting mixed solution is then ultrasonically dispersed to ensure uniform distribution of the components. The solution is then converted to a powder using spray drying technology, and finally crushed to obtain a fine-grained lithium supplement.

[0021] In this preparation method, the content of lithium oxalate is controlled at a mass fraction of 1%-5.5%. By reducing the concentration of lithium oxalate in the slurry, the lithium supplement particles after spray drying have an irregular spherical shape and form a hollow structure. The hollow structure increases the specific surface area of ​​the material, allowing the material to better contact with the electrode material.

[0022] In any of the above technical solutions, the ultrasonic dispersion treatment time is 1.5h-2.5h; and / or the inlet air temperature of the spray drying is 200°C-260°C; and / or the feed rate of the spray drying is 35r / min-45r / min.

[0023] In this embodiment, the ultrasonic dispersion treatment time is set between 1.5h-2.5h to achieve the optimal dispersion effect of each component in the solution and avoid the degradation of material performance that may be caused by over-treatment. The inlet air temperature of the spray drying is set between 200℃-260℃. This temperature range is determined based on the comprehensive consideration of the thermal stability of the chemical substances involved and the spray drying efficiency to ensure that the material maintains chemical and structural integrity during the conversion into dry powder. The feed rate of the spray drying is set to 35r / min-45r / min, which helps to ensure uniform drying of the material and avoid agglomeration while maintaining high efficiency. The special preparation technology spray drying process is used to make the generated lithium supplement particles have a hollow structure, which not only increases the contact area with the electrode material, but also improves the wettability with the electrolyte.

[0024] The present invention also provides a positive electrode material, which includes the lithium supplement agent described above.

[0025] The present invention also provides a lithium-ion battery, which includes a positive electrode sheet, a separator and a negative electrode sheet, and the positive electrode sheet includes the positive electrode material described above.

[0026] After adopting the technical solution of the present invention, the following technical effects can be achieved: The lithium supplement provided by the present invention includes lithium oxalate, a carbon material, a catalyst and a modifier. Through the synergistic effect of lithium oxalate, the carbon material, the catalyst and the modifier, the initial decomposition voltage and average decomposition voltage of lithium oxalate are significantly reduced, while the lithium supplement effect of lithium oxalate is improved. Among them, the addition of a fast ion conductor and / or a lithium affinity agent can help reduce the initial decomposition voltage of lithium oxalate, allowing lithium ions to be released from lithium oxalate more quickly, accelerating the migration of lithium ions on the surface of the electrode material, and reducing internal resistance. The lithium supplement provided by the present invention has high electrochemical activity, a decomposition voltage as low as 4.14V, and a large specific surface area, and can be in good contact with the electrode material and the electrolyte. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] The above and / or additional aspects and advantages of the present invention will become apparent and readily understood from the following description of the embodiments with reference to the accompanying drawings, in which: Figure 1 This is an electron microscope image of the lithium supplement provided in Example 1 of the present invention; Figure 2 This is an electron microscope image of the lithium supplement provided in Example 3 of the present invention; Figure 3 This is an electron microscope image of the lithium supplement provided in Example 4 of the present invention. DETAILED DESCRIPTION

[0028] To make the above-mentioned objects, features, and advantages of the present invention more clearly understood, the technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only some embodiments of the present invention, not all embodiments. All other embodiments obtained by persons of ordinary skill in the art based on the embodiments of the present invention without creative effort shall fall within the scope of protection of the present invention.

[0029] An embodiment of the present invention provides a lithium supplement agent, which includes lithium oxalate, a carbon material, a catalyst and a modifier, wherein the modifier includes at least one of a fast ion conductor and / or a lithium-philic agent; wherein the mass ratio of lithium oxalate, carbon material, catalyst and modifier is (70-95): (2.5-14): (2.5-14): (0.1-1).

[0030] The lithium supplement provided by the present invention includes lithium oxalate, a carbon material, a catalyst and a modifier. Among them, lithium oxalate is used as the core component of the lithium supplement and is used in the battery to replenish the active lithium ions consumed when the SEI film is formed, thereby improving the cycle performance and energy density of the battery; the carbon material is used to improve the conductivity and structural stability of the electrode, which helps the battery maintain performance during the charge and discharge process; the catalyst can reduce the reaction activation energy, thereby reducing the initial decomposition voltage of lithium oxalate and accelerating the decomposition reaction of lithium oxalate; the modifier includes a fast ion conductor and / or a lithium affinity agent. The modifier can significantly increase the migration rate of lithium ions on the surface of the lithium supplement, accelerate the release of lithium ions, and thus optimize the transmission efficiency of lithium ions.

[0031] The present invention significantly improves the energy density and cycle life of batteries through the synergistic effects of lithium oxalate, carbon materials, catalysts, and modifiers. The addition of a fast ion conductor and / or a lithiophile allows lithium ions to escape from the surface of the lithium oxalate material more quickly, increasing the rate of lithium ion migration and thus reducing the decomposition voltage of lithium oxalate, leading to faster decomposition.

[0032] In some embodiments of the present application, the lithium supplement is in the form of hollow spherical particles, and some of the particles have a hollow fracture structure.

[0033] Hollow spherical particles refer to the lithium supplement agent that forms a hollow spherical structure during the preparation process. This structure gives the particles a physically low density and a large specific surface area, enabling them to better contact with the electrode material. The rupture or collapse of the hollow spherical particles increases the contact area with the electrode material and the wettability with the electrolyte, thereby providing a better lithium supplement effect. It should be noted that the spherical structure of the particles is irregular in shape.

[0034] In some embodiments of the present application, the proportion of particles having a hollow fracture structure to the total number of particles is 10%-99%.

[0035] Particles with a hollow fracture structure have a higher proportion, which can increase the surface area and porosity of the material, thereby increasing the contact area with the electrode material and the wettability of the electrolyte, thereby improving the lithium replenishment effect of the lithium replenisher.

[0036] It should be noted that the statistical method for the crushing ratio of lithium supplement particles is to compare them with uncrushed materials, count the number of crushed materials and the number of uncrushed materials, and the ratio of the number of crushed materials to the sum of the number of crushed materials and the number of uncrushed materials is the crushing ratio; among them, the number of crushed materials is the number of crushed materials observed from the electron microscope image, and the number of uncrushed materials is the number of uncrushed materials observed from the electron microscope image. Each group is counted three times and the average value is taken.

[0037] In some embodiments of the present application, the specific surface area of ​​the lithium supplement is 60m 2 / g-170m 2 / g.

[0038] The lithium supplement agent provided by the present invention has a hollow rupture structure, which enables the lithium supplement agent to have a higher specific surface area, which not only increases the contact area with the electrode material, but also improves the wettability with the electrolyte, thereby ensuring a better lithium supplement effect.

[0039] In some embodiments of the present application, the fast ion conductor includes Li4Ti5O 12 , Li3PO4, Li2Zr2(PO4)3, LiPO2F2, LiF, LiNO3, LiAlO2; and / or the lithium-philic agent includes at least one of Si, S, P; and / or the catalyst includes at least one of a transition metal element and a transition metal compound; and / or the carbon material includes at least one of Ketjen black, Super-P conductive carbon black, CNTs, redox graphene, polyvinyl pyrrolidone, and tannic acid.

[0040] Fast ion conductors have excellent ion transport capabilities and structural stability. When added in appropriate amounts, they can improve the surface conductivity of the material and accelerate the release of lithium ions without reducing the performance of the material itself. LiPO2F2 has a three-dimensional structure in its crystal structure. Free lithium ions can diffuse freely in multiple directions in three-dimensional space, further enriching the diffusion path of lithium ions and reducing impedance, thereby achieving the purpose of reducing the decomposition voltage of lithium oxalate and promoting the decomposition of lithium oxalate; Li4Ti5O 12 As a fast ion conductor, it not only improves the conductivity, but also has the characteristic of "zero strain". + When the lattice constant and volume of the crystal change very little, it can stably promote the decomposition reaction of lithium oxalate, and its chemical properties are stable and it does not react with the electrolyte.

[0041] Transition metals, such as iron, cobalt, and nickel, are effective catalyzers of a wide variety of chemical reactions due to their unique electronic structures and variable oxidation states. Using transition metal catalysts can significantly increase the rate of chemical reactions, allowing reactions to be completed quickly and under milder conditions, thereby saving energy and time. Transition metal compounds, such as molybdenum trioxide and cobalt oxide, exhibit high efficiency and specific activity in catalyzing specific reactions. Molybdenum trioxide is preferred due to its high chemical reactivity and selectivity.

[0042] Ketjen black (KB) is a highly structured conductive carbon black with a high specific surface area and electrical conductivity. Super-P conductive carbon black is an ultrafine carbon black with excellent electrical conductivity and stability. Carbon nanotubes (CNTs) have ultra-high strength and electrical conductivity and are used to strengthen composite materials, conductive channels in electronic devices, etc. Redox graphene has a unique two-dimensional structure and excellent electronic conductivity. Polyvinylpyrrolidone (PVP) is added as a stabilizer and dispersant together with other carbon sources to improve the processability and compatibility of the material and reduce agglomeration. Tannic acid has an excellent coating effect and can be immediately coated on the surface of the material under neutral conditions, achieving controllable and uniform coating of the material. The above-mentioned carbon materials can provide excellent electrical conductivity and thermal stability, and enhance the overall performance of the final product.

[0043] An embodiment of the present invention further provides a method for preparing a lithium supplement, which is used to prepare the lithium supplement as described above, and the preparation method comprises the following steps: S100: dissolving lithium oxalate, and then adding a carbon material, a catalyst, and a modifier to obtain a mixed solution; S200: sequentially performing ultrasonic dispersion, spray drying, and crushing on the mixed solution to obtain a lithium supplement; wherein the mass fraction of lithium oxalate in the mixed solution is 1%-5.5%.

[0044] The present invention provides a method for preparing a lithium supplement. The method involves first dissolving lithium oxalate in a suitable solvent, followed by the addition of a carbon material, a catalyst, and a modifier. This step aims to reduce the initial and average decomposition voltages of lithium oxalate, thereby enhancing its lithium supplementation efficacy. The resulting mixed solution is then ultrasonically dispersed to ensure uniform distribution of the components. The solution is then converted to a powder using spray drying technology, and finally crushed to obtain a fine-grained lithium supplement.

[0045] The atomizer used in the spray drying process is either centrifugal or two-fluid, preferably a two-fluid atomizer. Liquid droplets are transported into the atomizer cavity via a high-pressure airflow. The droplets evaporate instantaneously under high-temperature conditions, resulting in dry solid particles. The lithium supplement particles obtained under the airflow have a hollow, cracked, or collapsed structure. Crushing methods include, but are not limited to, steel mills, juicers, and rollers.

[0046] In this preparation method, the content of lithium oxalate is controlled at a mass fraction of 1%-5.5%. By reducing the concentration of lithium oxalate in the slurry, the lithium supplement particles after spray drying have an irregular spherical shape and form a hollow structure. The hollow structure increases the specific surface area of ​​the material, allowing the material to better contact with the electrode material.

[0047] In some embodiments of the present application, the ultrasonic dispersion treatment time is 1.5h-2.5h; and / or the inlet air temperature of the spray drying is 200°C-260°C; and / or the feed rate of the spray drying is 35r / min-45r / min.

[0048] In this embodiment, the ultrasonic dispersion treatment time is set between 1.5h-2.5h to achieve the optimal dispersion effect of each component in the solution and avoid the degradation of material performance that may be caused by over-treatment. The inlet air temperature of the spray drying is set between 200℃-260℃. This temperature range is determined based on the comprehensive consideration of the thermal stability of the chemical substances involved and the spray drying efficiency to ensure that the material maintains chemical and structural integrity during the conversion into dry powder. The feed rate of the spray drying is set to 35r / min-45r / min, which helps to ensure uniform drying of the material and avoid agglomeration while maintaining high efficiency. The special preparation technology spray drying process is used to make the generated lithium supplement particles have a hollow structure, which not only increases the contact area with the electrode material, but also improves the wettability with the electrolyte.

[0049] By precisely controlling the ultrasonic dispersion time and the spray drying temperature and speed, the uniformity and performance stability of the final lithium supplement can be maximized. By controlling the parameters of these key process steps, the optimal performance of the lithium supplement in the battery can be ensured, thereby improving the battery's energy density and cycle life.

[0050] An embodiment of the present invention further provides a positive electrode material, which includes the lithium supplement agent described above.

[0051] An embodiment of the present invention further provides a lithium-ion battery, which includes a positive electrode sheet, a separator, and a negative electrode sheet, wherein the positive electrode sheet includes the positive electrode material described above.

[0052] The positive electrode sheet can be prepared using conventional techniques in the art. Specifically, the lithium oxalate supplement, positive electrode active material, conductive agent, and binder can be uniformly dispersed in a solvent to obtain a positive electrode active layer slurry. The positive electrode active layer slurry is then applied to at least one functional surface of the positive electrode current collector and dried to obtain the positive electrode sheet of the present invention. In addition to the positive electrode sheet, the lithium-ion battery of the present invention also includes a separator, a negative electrode sheet, and an electrolyte. The composition of the negative electrode sheet can refer to conventional negative electrode sheets in the art, and the separator can also use separators commonly used in the art, such as PP film, PE film, etc.

[0053] An embodiment of the present invention further provides a method for preparing a lithium-ion battery, which is used to prepare the lithium-ion battery described above. The method comprises the following steps: stacking a positive electrode sheet, a separator, and a negative electrode sheet in sequence, and packaging them to obtain a lithium-ion battery.

[0054] The lithium-ion battery of the present invention can be prepared by conventional methods in the art. Specifically, the positive electrode sheet, the separator and the negative electrode sheet can be stacked in sequence, and then a battery cell can be obtained through a lamination or winding process. The battery cell can then be obtained through baking, liquid injection, formation, packaging and other processes.

[0055] Example 1 S1, 80g lithium oxalate, 9.5g molybdenum trioxide, 0.5g LiPO2F2, 10g Ketjen black were added to water, wherein the mass fraction of lithium oxalate in the above mixed solution was 1wt%, and ultrasonic equipment was turned on for ultrasonic dispersion for 1 h to form a uniform suspension; S2. Drying is performed using a spray drying device, which is a two-fluid atomizer. The inlet air temperature of the spray drying device is 240° C. and the feed rate is 40 r / min.

[0056] S3. After spraying is completed, the mixture is crushed and then vacuum dried at 200° C. to obtain a modified lithium oxalate lithium supplement.

[0057] Examples 2-28 and Comparative Examples 1-5 were prepared using the same method as Example 1. The differences are shown in Table 1.

[0058] Test conditions: The prepared lithium oxalate supplement was subjected to constant current and constant voltage charging tests on button-type half-cells at a test current of 0.1C (nominal capacity 525 mAh / g), a cutoff voltage of 4.35V, and a constant voltage cutoff current of 0.05C. The resulting charge specific capacity was the decomposition capacity of the lithium oxalate. The starting decomposition voltage was read from the charge curve, and the resulting average charge voltage was the average decomposition voltage of the lithium oxalate. Specific test results are shown in Table 1.

[0059] Table 1 Preparation parameters and test results of Examples 1-28 and Comparative Examples 1-5 Table 2 Test results of crushing ratio and specific surface area of ​​Examples 1-28 and Comparative Examples 1-5 Figure 1 This is an electron microscope image of the lithium supplement provided in Example 1; Figure 2 This is an electron microscope image of the lithium supplement provided in Example 3; Figure 3 This is an electron microscope image of the lithium supplement provided in Example 4.

[0060] According to the comparison of Examples 1-4, by reducing the concentration of lithium oxalate in the feed solution during the preparation process, the particles of the lithium supplement agent have irregular spherical shapes, and after crushing, a hollow fracture structure is formed. As the concentration decreases from 5.5% to 1%, the concentration of the lithium oxalate solution decreases, and the degree of crushing gradually increases. After crushing, the specific surface area of ​​the material is increased, so that the material can better contact with the electrode material. Figure 1-3 As shown, the lithium supplements of Examples 1, 3, and 4 all have a hollow rupture structure, but the lithium supplement in Example 1 has a higher degree of breakage and a higher decomposition capacity.

[0061] According to the comparison of Examples 1, 27 and Comparative Example 1, it can be seen that as the proportion of lithium oxalate changes, the decomposition capacity of the material is proportional to the proportion of lithium oxalate, but the lower carbon content and catalyst will make the decomposition voltage of the material higher, which is not suitable for mainstream battery systems.

[0062] According to the comparison between Examples 1 and 4, the maximum solubility of lithium oxalate is 5.5% in the solution. If excessive addition is made, lithium oxalate will not dissolve, resulting in uneven spraying and affecting the subsequent crushing effect.

[0063] According to the comparison of Examples 1-4, it can be seen that the morphology after crushing is different when the concentration of lithium oxalate in the slurry is different. The degree of crushing is higher at low concentrations, which greatly increases the contact area with the electrode material and the wettability of the electrolyte. It decomposes more completely during the formation and can better provide lithium replenishment effect.

[0064] According to the comparison between Example 1 and Comparative Example 2, a fast ion conductor and / or a lithium-philic agent is added during the preparation process. The modifier has a high ionic conductivity, can improve the lithium ion release performance, and reduce the initial decomposition voltage of lithium oxalate delithiation.

[0065] According to the comparison between Example 1 and Example 28, in the spray drying process, the atomizer used is preferably a two-fluid atomizer, and the droplets are transported into the sprayer cavity by a high-pressure airflow. The droplets evaporate instantly under high temperature conditions to obtain dry solid particles. The lithium supplement particles obtained under the airflow have a hollow rupture structure.

[0066] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the various embodiments of the present invention.

Claims

1. A lithium supplement, characterized in that: The lithium supplement agent comprises lithium oxalate, a carbon material, a catalyst and a modifier, wherein the modifier comprises at least one of a fast ion conductor and / or a lithium affinity agent; Wherein, the mass ratio of the lithium oxalate, the carbon material, the catalyst and the modifier is (70-95): (2.5-14): (2.5-14): (0.1-1).

2. The lithium supplement according to claim 1, characterized in that: The lithium supplement agent is hollow spherical particles, and some of the particles have a hollow rupture structure.

3. The lithium supplement according to claim 2, characterized in that: The proportion of the particles having the hollow fracture structure to the total amount of the particles is 10%-99%.

4. The lithium supplement according to claim 1, characterized in that: The specific surface area of ​​the lithium supplement is 60m 2 / g-170m 2 / g.

5. The lithium supplement according to claim 1, characterized in that: The fast ion conductor includes Li4Ti5O 12 , at least one of Li3PO4, Li2Zr2(PO4)3, LiPO2F2, LiF, LiNO3, LiAlO2; and / or The lithium-philic agent comprises at least one of Si, S, and P; and / or The catalyst comprises at least one of a transition metal element and a transition metal compound; and / or The carbon material includes at least one of Ketjen black, Super-P conductive carbon black, CNTs, redox graphene, polyvinyl pyrrolidone, and tannic acid.

6. A method for preparing a lithium supplement, characterized in that: The preparation method is used to prepare the lithium supplement according to any one of claims 1 to 5, and the preparation method comprises the following steps: S100: dissolving the lithium oxalate, and then adding the carbon material, the catalyst and the modifier to obtain a mixed solution; S200: subjecting the mixed solution to ultrasonic dispersion, spray drying, and crushing treatments in sequence to obtain the lithium supplement; Wherein, the mass fraction of the lithium oxalate in the mixed solution is 1%-5.5%.

7. The preparation method according to claim 6, characterized in that: The ultrasonic dispersion treatment time is 1.5h-2.5h; and / or The inlet air temperature of the spray drying is 200°C-260°C; and / or The feed rate of the spray drying is 35r / min-45r / min.

8. A positive electrode material, characterized in that The positive electrode material includes the lithium supplement agent according to any one of claims 1 to 5.

9. A lithium ion battery, characterized in that: The lithium-ion battery comprises a positive electrode sheet, a separator and a negative electrode sheet, and the positive electrode sheet comprises the positive electrode material as claimed in claim 8.

Citation Information

Patent Citations

  • Preparation method of composite coated ternary positive electrode material

    CN112794372A

  • Lithium metal negative plate, preparation method thereof and secondary battery

    CN113871575A

  • Modified lithium oxalate as well as preparation method and application thereof

    CN114300680A

  • Lithium-philic carbon skeleton composite material as well as preparation method and application thereof

    CN114335540A

  • Lithium metal negative electrode with interface modification layer and preparation method of lithium metal negative electrode

    CN115132958A

Cited By

  • Composite, composite lithium supplement agent, and preparation method and application of composite lithium supplement agent

    CN119050369A

  • Composite material, composite lithium supplement, preparation method and application thereof

    CN119050369B

  • Nanoscale lithium oxalate / carbon composite lithium supplement agent, preparation method and application of nanoscale lithium oxalate / carbon composite lithium supplement agent in lithium ion battery

    CN119674077A