SECONDARY BATTERY PROTECTION METHOD AND APPARATUS, SECONDARY BATTERY, battery module, battery pack, AND ELECTRIC DEVICE
Patent Information
- Application Number
- CN202280092627.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2022-06-16
- Publication Date
- 2024-10-11
AI Technical Summary
Existing secondary batteries lack effective protection at the welding point, resulting in short circuit and corrosion problems, affecting safety performance and production efficiency.
By forming a protective layer on the internal surface of the secondary battery, especially the welding joint, gas-solid interface reaction technology is used to select appropriate first and second reactants to form a uniform and dense protective layer to reduce the occurrence of corrosion and short circuits.
It effectively reduces the risk of short circuit and corrosion inside the secondary battery, improves the safety performance and the bonding strength of the protective layer, simplifies the manufacturing process, and reduces the probability of defects.
Smart Images

Figure CN118765464A_ABST
Abstract
Description
Secondary battery protection method and device, secondary battery, battery module, battery pack and power-consuming device Technical Field
[0001] The present application relates to the technical field of secondary batteries, and in particular to a secondary battery protection method and equipment, a secondary battery, a battery module, a battery pack, and an electrical device. Background Art
[0002] In recent years, the application of secondary batteries has become increasingly widespread. They are widely used in energy storage systems such as hydropower, thermal, wind, and solar power plants, as well as in power tools, electric bicycles, electric motorcycles, electric vehicles, military equipment, aerospace, and other fields. This rapid development of secondary batteries has led to higher demands for their energy density, cycle performance, and safety. However, the safety performance of existing secondary batteries needs further improvement.
[0003] Summary of the Invention
[0004] The present application is made in view of the above-mentioned problems, and its purpose is to provide a secondary battery protection method, which can simultaneously form a protective layer on the internal surface of the secondary battery, especially the welding point, thereby reducing the probability of internal corrosion and short circuit of the secondary battery.
[0005] In order to achieve the above-mentioned objectives, the present application provides a secondary battery protection method and equipment, a secondary battery, a battery module, a battery pack and an electrical device.
[0006] A first aspect of the present application provides a protection method for a secondary battery, wherein the secondary battery includes a liquid injection port, and the method includes:
[0007] Step (1): evacuating the secondary battery through the liquid injection port to within 100 kPa, optionally within 100 Pa;
[0008] Step (2): introducing a first reactant into the secondary battery through the injection port until the pressure rises by more than 1 Pa, optionally by more than 1 kPa, and is maintained for more than 1 ms, optionally for 0.1 s to 600 s; and optionally,
[0009] Step (3): evacuating the secondary battery through the injection port to within 100 kPa, optionally within 100 Pa; and
[0010] Step (4): introducing a second reactant into the secondary battery through the injection port until the pressure rises by more than 1 Pa, optionally by more than 1 kPa, and is maintained for more than 1 ms, optionally 0.1 s to 600 s;
[0011] thereby forming a protective layer on the inner surface of the secondary battery;
[0012] The second reactant can react with the first reactant to form the protective layer.
[0013] Therefore, the present application utilizes gas-solid interface reaction technology to protect the internal surface of the secondary battery, and performs integrated insulation protection treatment on the exposed surfaces inside the secondary battery, especially the surfaces of the welds produced during the subsequent assembly process, which can reduce the probability of internal corrosion and short circuit of the secondary battery, thereby improving the safety performance and corrosion resistance of the secondary battery.
[0014] In any embodiment, the first reactant includes at least one of a gaseous aluminum compound, a silicon compound, a tin compound, a germanium compound, a chromium compound, a boron compound, a titanium compound, a vanadium compound, a zinc element and a zinc compound, a zirconium compound, a hafnium compound and a tantalum compound; optionally includes gaseous AlCl3, trimethylaluminum, Al(CH3)2Cl, Al(C2H5)3, Al(OC2H5)3, (CH3)2AlOCH(CH3)2, (CH3CH2)2AlOC2H5, Al(CH3)2OC2H5, Al(N(C2H5)2)3, Al(N(CH3)2)3, SiCl4, SiCl2H2, Si2Cl6, Si(OC2H5)2H2, Si2H6, Si(OCH2CH3)4, Si(OCH3)4, SiH(OCH3)3, SiH(OC2H5)3 , (CH3)2Si(OCH3)2, Si(NCO)4, Si(OC2H5)4, H2N(CH2)3Si(OC2H5)3, CH2=CHSi(OCH3)3, (CH 2=CH)3SiOCH3, ((CH3)3CO)3SiOH, (CH3CH2C(CH3)2O)3SiOH, SiH[N(CH3)2]3, SiH2[N(CH3) 2]2, SiH2[NH(C4H9)]2, SiH2[N(C2H5)2]2, SiH2[NC2H5CH3]2, SiH3N(C4H9)2, [Si(NHC2H5) 3]2. Si(NHC2H5)4, SiH3N(C3H7)2, [SiH2N(C3H7)2]2, Si(N(CH3)2)4, (CH3)3SiN(CH3)2, C7H 17 NSi、C8H 20 N2Si、C8H 17 NO2Si、C7H 18N2O2Si, SiCl3H, SnCl4, GeCl3, CrO2Cl2, BBr3, TiF4, TiCl4, TiI4, Ti(OCH3)4, Ti(OC2H5)4, Ti(N(CH3)2)4, Ti(N(C2H5)2)4, Ti(N(CH3 )(C2H5))4, VOCl3, Zn, ZnCl2, Zn(CH3)2, Zn(C2H5)2, ZnI2, ZrCl4, ZrI4, Zr(N(CH3)2)4, Zr(N(C2H5)2)4, Zr(N(CH3)(C2H5))4, HfCl4, At least one of HfI4, Hf(NO3)4, Hf(N(CH3)(C2H5))4, Hf(N(CH3)2)4, Hf(N(C2H5)2)4, TaCl5, TaF5, TaI5, Ta(O(C2H5))5, Ta(N(CH3)2)5, Ta(N(C2H5)2)5 and TaBr5.
[0015] In any embodiment, the second reactant includes at least one of H2O, O2, O3, H2, S, (NH4)2S, H2Se, Se, H2Te, Te, HF, TiF4, TaF5, C2H4, CHCl3, H2O2, NO2, N2O, NH3, N2H4, HCOOH, CH3COOH and H2S and / or a plasma of at least one thereof.
[0016] By selecting the first reactant and the second reactant, the composition of the protective layer can be controlled, and the protective layer is uniform and dense, and has a strong bonding force with the substrate, thereby reducing the probability of internal corrosion and short circuit of the secondary battery.
[0017] In any embodiment, in steps (1) to (4), the temperature of the secondary battery is maintained at a temperature between 0° C. and 200° C. By maintaining the temperature of the secondary battery within a given range, the physical properties of specific reactants can be adapted.
[0018] In any embodiment, the steps (1) to (4) are repeated 1 to 100,000 times. The thickness of the protective layer can be controlled by controlling the number of repetitions of the steps (1) to (4).
[0019] In any embodiment, the steps (1) to (2) are first repeated 1 to 10 times, and then the steps (1) to (4) are repeated 1 to 100,000 times. In this way, the water in the secondary battery itself can be fully utilized as a reactant.
[0020] In any embodiment, the first reactant and the second reactant are introduced by a carrier gas, and the carrier gas includes at least one of nitrogen, argon, carbon dioxide, and helium. The introduction of the first reactant and the second reactant by the carrier gas can make the reactants enter the secondary battery more smoothly.
[0021] In any embodiment, the method further includes, before step (1), a step of pre-treating the inner surface of the secondary battery, comprising introducing at least one of Ar, N2, H2O, O2, O3, H2, S, (NH4)2S, H2Se, Se, H2Te, Te, HF, TiF4, TaF5, C2H4, CHCl3, H2O2, NO2, N2O, NH3, N2H4, HCOOH, CH3COOH, and H2S and / or a plasma of at least one of them into the secondary battery through the injection port. The pre-treatment step can enhance the bonding strength between the protective layer and the substrate.
[0022] In any embodiment, the secondary battery further includes an electrode assembly, a tab, a transition piece, a top cover assembly, and a housing. The protective layer is formed at the connection between the tab and the transition piece, the connection between the transition piece and the top cover assembly, the connection between the top cover assembly and the housing, the inner wall of the top cover assembly, the transition piece, the inner wall of the housing, and the outer peripheral surface of the electrode assembly. The protective layer can reduce heat generated during short-circuit bonding to mitigate safety hazards; it also acts as a physical barrier to prevent corrosion.
[0023] In any embodiment, the protective layer comprises at least one of carbides, nitrides, sulfides, oxides, fluorides, selenides, and tellurides of aluminum, silicon, tin, germanium, chromium, boron, titanium, vanadium, zinc, zirconium, hafnium, or tantalum, and optionally at least one of aluminum oxide, silicon oxide, silicon nitride, titanium oxide, and zinc oxide. By controlling the composition of the protective layer, the protective layer can be made more uniform and dense, and the bonding strength between the protective layer and the substrate can be enhanced.
[0024] In any embodiment, the method further includes, after step (2) and / or step (4), purging the secondary battery with a purge gas, wherein the purge gas includes at least one of N2, Ar, He, CO2, and the second reactant. The purge step can further improve the purity and bonding strength of the protective layer.
[0025] In any embodiment, the thickness of the protective layer is 1 nm to 1000 μm, optionally 50 nm to 500 nm. By controlling the protective layer within a suitable thickness range, while providing insulation protection, the overall mass energy density and volume energy density of the secondary battery are almost unaffected.
[0026] In any embodiment, the protective layer may be subjected to a post-treatment step, including temperature annealing, plasma annealing, or light radiation annealing in a specific atmosphere, wherein the specific atmosphere includes at least one of pyridine, N2, Ar, He, CO2, and the second reactant, and / or a plasma of at least one of these. This post-treatment step can further improve the quality of the protective layer.
[0027] A second aspect of the present application further provides a secondary battery protection device, comprising:
[0028] a cavity, for accommodating the secondary battery;
[0029] a first reactant tank, for storing a first reactant;
[0030] a second reactant tank, for storing a second reactant;
[0031] Vacuum pump;
[0032] A pressure gauge, used to detect the pressure inside the secondary battery in real time;
[0033] a flow regulating valve, for regulating the flow of the first reactant and the second reactant;
[0034] The second reactant is capable of reacting with the first reactant to form a protective layer;
[0035] The first reactant tank and the second reactant tank are respectively connected to the injection port of the secondary battery contained in the cavity to pass the first reactant and the second reactant into the interior of the secondary battery; and the vacuum pump is connected to the injection port of the secondary battery contained in the cavity to evacuate the secondary battery.
[0036] This allows reactants to mix and react inside the secondary battery.
[0037] A third aspect of the present application provides a secondary battery, wherein the secondary battery is protected by the secondary battery protection method described in the first aspect of the present application.
[0038] A fourth aspect of the present application provides a battery module including the secondary battery according to the third aspect of the present application.
[0039] The fifth aspect of the present application provides a battery pack comprising the battery module of the fourth aspect of the present application.
[0040] The sixth aspect of the present application provides an electrical device comprising at least one selected from the secondary battery of the third aspect of the present application, the battery module of the fourth aspect of the present application, or the battery pack of the fifth aspect of the present application.
[0041] The battery module, battery pack, and electric device of the present application include the secondary battery of the present application, and thus have at least the same advantages as the secondary battery. BRIEF DESCRIPTION OF THE DRAWINGS
[0042] FIG. 1 is an exploded view of a secondary battery according to an embodiment of the present application.
[0043] FIG. 2 is a schematic diagram of a secondary battery according to an embodiment of the present application.
[0044] FIG3 is a schematic diagram of a battery module according to an embodiment of the present application.
[0045] FIG4 is a schematic diagram of a battery pack according to an embodiment of the present application.
[0046] FIG. 5 is an exploded view of the battery pack shown in FIG. 4 according to an embodiment of the present application.
[0047] FIG6 is a schematic diagram of an electric device using a secondary battery as a power source according to an embodiment of the present application.
[0048] FIG. 7 is a schematic diagram of a secondary battery protection device according to an embodiment of the present application. DETAILED DESCRIPTION
[0049] Below, the embodiments of the secondary battery protection method and equipment, secondary battery, battery module, battery pack and electrical device of the present application are described in detail with appropriate reference to the accompanying drawings. However, there may be cases where unnecessary detailed descriptions are omitted. For example, there are cases where detailed descriptions of well-known matters and repeated descriptions of actually the same structures are omitted. This is to avoid the following description from becoming unnecessarily lengthy and to facilitate the understanding of those skilled in the art. In addition, the drawings and the following description are provided for those skilled in the art to fully understand the present application and are not intended to limit the subject matter described in the claims.
[0050] " range " disclosed in the application is limited in the form of lower limit and upper limit, and given range is limited by selecting a lower limit and an upper limit, and the selected lower limit and upper limit define the boundary of special range. The scope limited in this way can be to include end value or not include end value, and can be arbitrarily combined, that is, any lower limit can form a range with any upper limit combination. For example, if the scope of 60-120 and 80-110 is listed for specific parameters, it is understood that the scope of 60-110 and 80-120 is also expected. In addition, if minimum range values 1 and 2 are listed, and if maximum range values 3,4 and 5 are listed, then the following range can all be expected: 1-3, 1-4, 1-5, 2-3, 2-4 and 2-5. In this application, unless otherwise specified, numerical range " ab " represents the abbreviation of any real number combination between a and b, wherein a and b are all real numbers. For example, a numerical range of "0-5" indicates that all real numbers between "0-5" are listed herein, and "0-5" is simply an abbreviation for these numerical combinations. Furthermore, when a parameter is expressed as an integer ≥ 2, this is equivalent to disclosing that the parameter is, for example, an integer of 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, etc.
[0051] Unless otherwise specified, all embodiments and optional embodiments of the present application can be combined with each other to form a new technical solution.
[0052] Unless otherwise specified, all technical features and optional technical features of this application can be combined with each other to form a new technical solution.
[0053] Unless otherwise specified, all steps of the present application may be performed sequentially or randomly, preferably sequentially. For example, "the method includes steps (a) and (b)" indicates that the method may include steps (a) and (b) performed sequentially, or may include steps (b) and (a) performed sequentially. For example, "the method may further include step (c)" indicates that step (c) may be added to the method in any order, for example, the method may include steps (a), (b), and (c), or may include steps (a), (c), and (b), or may include steps (c), (a), and (b), etc.
[0054] Unless otherwise specified, the terms "include" and "comprising" used in this application may be open-ended or closed-ended. For example, "include" and "comprising" may mean that other components not listed may also be included or that only the listed components are included.
[0055] Unless otherwise specified, the term "or" is used in this application to be inclusive. For example, the phrase "A or B" means "A, B, or both A and B." More specifically, the condition "A or B" is satisfied if any of the following conditions are met: A is true (or exists) and B is false (or does not exist); A is false (or does not exist) and B is true (or exists); or both A and B are true (or exist).
[0056] With the development of electronic and intelligent devices, the demand for secondary batteries, especially high-energy-density batteries, is becoming increasingly urgent. Taking lithium-ion batteries as an example, the gradual increase in energy density is often accompanied by increased safety risks. These risks arise from several factors: First, aluminum foil, used as the positive electrode current collector, covers a large surface area with the positive electrode active material. However, its end faces are prone to burrs, increasing the probability of short circuits and, in turn, fires and other safety issues. Second, the battery has multiple exposed metal areas, which, in extreme situations, can also easily cause short circuits and corrosion.
[0057] Existing published patents, documents, etc. mainly provide single protection for the internal elements of the battery, that is, pre-processing the pole pieces or isolation membranes, and then assembling them into secondary batteries. However, firstly, this step-by-step processing method cannot provide protection for the welds generated later. These unprotected weld areas are still the weak link in short-circuit protection and are prone to safety hazards. Secondly, multi-step processing increases the number of manufacturing processes and the time consumed. At the same time, the pre-prepared protective layer is easily damaged in the subsequent production process, which will reduce the reliability of the protection and increase the probability of defects. Thirdly, before processing, in order not to affect welding, this method requires special protection of the pole ears, which affects production efficiency and reduces the yield rate.
[0058] Therefore, in existing industrial production, how to find an efficient, low-cost method that can simultaneously form multiple protective structures inside the battery has become a difficult problem.
[0059] The present application proposes a secondary battery protection method, which can simultaneously form a protective layer on the internal surface of the secondary battery, especially on the welding points, thereby reducing the probability of internal corrosion and short circuit of the secondary battery.
[0060] In one embodiment of the present application, a protection method for a secondary battery is provided. The secondary battery includes a liquid injection port. The method includes:
[0061] Step (1): evacuate the secondary battery through the liquid injection port to within 100 kPa, optionally within 100 Pa;
[0062] Step (2): introducing the first reactant into the secondary battery through the injection port until the pressure rises by more than 1 Pa, optionally by more than 1 kPa, and is maintained for more than 1 ms, optionally for 0.1 s to 600 s; and optionally,
[0063] Step (3): evacuating the secondary battery through the liquid injection port to within 100 kPa, optionally within 100 Pa; and
[0064] Step (4): introducing the second reactant into the secondary battery through the injection port until the pressure rises by more than 1 Pa, optionally by more than 1 kPa, and is maintained for more than 1 ms, optionally 0.1 s to 600 s;
[0065] thereby forming a protective layer on the inner surface of the secondary battery;
[0066] The second reactant can react with the first reactant to form a protective layer.
[0067] Although the mechanism is still unclear, the applicant unexpectedly discovered that the present application utilizes gas-solid interface reaction technology to protect the internal surface of the secondary battery. First, the exposed surface inside the battery, especially the surface of the welds produced during the subsequent assembly process, can be integrated to provide efficient insulation protection. Second, the protective layer formed on the internal surface can effectively reduce the risk of thermal runaway caused by internal short circuit of the battery, and can also reduce the corrosion of internal components of the battery, such as the electrolyte.
[0068] FIG1 is an exploded view of a secondary battery according to an embodiment of the present application. The secondary battery is a secondary battery that is not filled with liquid (electrolyte). Referring to FIG1 , the secondary battery includes an electrode assembly 30, positive and negative electrode tabs 41 and 42, positive and negative electrode adapters 21 and 22, a top cover assembly 10, and a housing 50. The top cover assembly 10 includes positive and negative electrode posts 11 and 12, a liquid injection port 13, and an explosion-proof valve 14. The housing 50 includes a bottom plate and side plates connected to the bottom plate, and the bottom plate and side plates together form a receiving cavity. The housing 50 has an opening connected to the receiving cavity, and the top cover assembly 10 can be covered on the opening to seal the receiving cavity. The electrode assembly 30 is formed by winding or laminating a positive electrode sheet, a negative electrode sheet, and a separator. The electrode assembly 30 is encapsulated in the receiving cavity. The number of electrode assemblies 30 contained in the secondary battery can be one or more, and those skilled in the art can select and optimize according to specific actual needs.
[0069] In an embodiment of the present application, a secondary battery is welded together by an electrode assembly 30, positive and negative electrode tabs 41 and 42, positive and negative electrode adapters 21 and 22, a top cover assembly 10, and a housing 50. For example, the electrode assembly 30 is first welded to the positive and negative electrode tabs 41 and 42, respectively; then, the positive and negative electrode tabs 41 and 42 are welded to the positive and negative electrode adapters 21 and 22, respectively; then, the positive and negative electrode adapters 21 and 22 are welded to the positive and negative electrode posts 11 and 12 of the top cover assembly 10, respectively; and finally, the top cover assembly 10 is welded to the housing 50 to obtain a secondary battery.
[0070] In some embodiments, the electrode assembly 30 itself has positive and negative electrode tabs 41 and 42 , that is, the electrode assembly 30 and the positive and negative electrode tabs 41 and 42 are an integrated structure.
[0071] In some embodiments, the positive and negative electrode tabs 41 and 42 are aluminum tabs and copper tabs, respectively. The positive and negative electrode adapters 21 and 22 are aluminum adapters and copper adapters, respectively.
[0072] In some embodiments, the internal surface of the secondary battery includes the inner wall of the top cover assembly 10, the inner wall of the shell 50, the end faces of the positive and negative electrode sheets, the edge of the isolation membrane, the surfaces of the positive and negative electrode tabs 41 and 42, the welding points between the positive and negative electrode tabs 41 and 42 and the positive and negative electrode adapter sheets 21 and 22 respectively, the surfaces of the positive and negative electrode adapter sheets 21 and 22, the welding points between the positive and negative electrode adapter sheets 21 and 22 and the positive and negative electrode posts 11 and 12 of the top cover assembly 10 respectively, and the welding point between the top cover assembly 10 and the shell 50.
[0073] In some embodiments, the first reactant includes at least one of a gaseous aluminum compound, a silicon compound, a tin compound, a germanium compound, a chromium compound, a boron compound, a titanium compound, a vanadium compound, a zinc element and a zinc compound, a zirconium compound, a hafnium compound, and a tantalum compound; optionally, the first reactant includes gaseous AlCl3, trimethylaluminum, Al(CH3)2Cl, Al(C2H5)3, Al(OC2H5)3, (CH3)2AlOCH(CH3)2, (CH3CH2)2AlOC2H5, Al(CH3)2OC2H5, Al(N(C2H5)2)3 , Al(N(CH3)2)3, SiCl4, SiCl2H2, Si2Cl6, Si(OC2H5)2H2, Si2H6, Si(OCH2CH3)4, Si(OCH3)4, SiH(OCH3)3, SiH(OC2H5)3, (C H3)2Si(OCH3)2, Si(NCO)4, Si(OC2H5)4, H2N(CH2)3Si(OC2H5)3, CH2=CHSi(OCH3)3, (CH2=CH)3SiOCH3, ((CH3)3CO)3SiOH, (CH3CH2C(CH3)2O)3SiOH, SiH[N(CH3)2]3, SiH2[N(CH3)2]2, SiH2[NH(C4H9)]2, SiH2[N(C2H5)2]2, SiH2[NC2H5CH3]2, S iH3N(C4H9)2, [Si(NHC2H5)3]2, Si(NHC2H5)4, SiH3N(C3H7)2, [SiH2N(C3H7)2]2, Si(N(CH3)2)4, (CH3)3SiN(CH3)2, C7H 17 NSi、C8H 20 N2Si、C8H 17 NO2Si、C7H 18N2O2Si, SiCl3H, SnCl4, GeCl3, CrO2Cl2, BBr3, TiF4, TiCl4, TiI4, Ti(OCH3)4, Ti(OC2H5)4, Ti(N(CH3)2) 4. Ti(N(C2H5)2)4, Ti(N(CH3)(C2H5))4, VOCl3, Zn, ZnCl2, Zn(CH3)2, Zn(C2H5)2, ZnI2, ZrCl4, ZrI4, Zr( At least one of N(CH3)2)4, Zr(N(C2H5)2)4, Zr(N(CH3)(C2H5))4, HfCl4, HfI4, Hf(NO3)4, Hf(N(CH3)(C2H5))4, Hf(N(CH3)2)4, Hf(N(C2H5)2)4, TaCl5, TaF5, TaI5, Ta(O(C2H5))5, Ta(N(CH3)2)5, Ta(N(C2H5)2)5 and TaBr5.
[0074] In the embodiment of the present application, the first reactant is introduced in gaseous form. If the first reactant is solid or liquid at room temperature, it can be converted into gas by the following methods: heating, magnetron sputtering, etc.
[0075] In some embodiments, the second reactant includes at least one of H2O, O2, O3, H2, S, (NH4)2S, H2Se, Se, H2Te, Te, HF, TiF4, TaF5, C2H4, CHCl3, H2O2, NO2, N2O, NH3, N2H4, HCOOH, CH3COOH and H2S and / or a plasma of at least one thereof.
[0076] By selecting the first reactant and the second reactant, the composition of the protective layer can be controlled, and the protective layer is uniform and dense, and has a strong bonding force with the substrate, thereby reducing the probability of internal corrosion and short circuit of the secondary battery.
[0077] In the embodiments of the present application, the substrate refers to the inner surface of the secondary battery.
[0078] In some embodiments, in steps (1) to (4), the temperature of the secondary battery is maintained at a temperature between 0° C. and 200° C. By maintaining the temperature of the secondary battery within a given range, the physical parameters of specific reactants can be adapted.
[0079] In some embodiments, steps (1) to (4) are repeated 1 to 100,000 times. By controlling the number of repetitions of steps (1) to (4), the thickness of the protective layer can be controlled.
[0080] In some embodiments, steps (1)-(2) are first repeated 1-10 times, and then steps (1)-(4) are repeated 1-100,000 times. Repeating steps (1)-(2) first can fully utilize the water in the secondary battery as a reactant.
[0081] In some embodiments, the first reactant and the second reactant are introduced by a carrier gas, and the carrier gas includes at least one of nitrogen, argon, carbon dioxide, and helium. By introducing the first reactant and the second reactant by a carrier gas, the reactants can enter the secondary battery more smoothly.
[0082] In some embodiments, the step of pre-treating the internal surface of the secondary battery is further included before step (1), which includes introducing at least one of Ar, N2, H2O, O2, O3, H2, S, (NH4)2S, H2Se, Se, H2Te, Te, HF, TiF4, TaF5, C2H4, CHCl3, H2O2, NO2, N2O, NH3, N2H4, HCOOH, CH3COOH and H2S and / or a plasma of at least one of them into the secondary battery through the injection port 13.
[0083] To further enhance the bonding strength between the protective layer and the substrate, a pre-treatment may be performed. As a pre-treatment, the present application performs plasma treatment of gases such as oxygen, water, or nitrogen on the internal surface of the secondary battery before forming the protective layer, plasma-forming the organic compound monomer for surface treatment, corona discharge treatment, UV irradiation treatment, ozone treatment, etc., which helps to form a compound layer with high bonding strength. The activity and number of the reactive groups can be adjusted according to the treatment intensity and time.
[0084] In some embodiments, the pretreatment step may include adjusting the gas type to clean the surface to be deposited, including cleaning with plasma such as Ar, N2, H2, O2, etc., for example, cleaning with Ar plasma, where the Ar plasma is generated by a radio frequency plasma gun with a power of 10-1000 W, a frequency of 13.56 MHz, and a holding time of 5s-60s.
[0085] In some embodiments, the protective layer is formed at the connection between the tabs 41, 42 and the adapter plates 21, 22, the connection between the adapter plates 21, 22 and the top cover assembly 10, the connection between the top cover assembly 10 and the shell 50, the inner wall of the top cover assembly 10, the adapter plates 21, 22, the inner wall of the shell 50, and the outer peripheral surface of the electrode assembly 30.
[0086] In some embodiments, the protective layer is formed on the inner wall of the top cover assembly 10, the inner wall of the shell 50, the end faces of the positive and negative electrode sheets, the edge of the isolation membrane, the surface of the positive and negative electrode tabs 41 and 42, the welding points between the positive and negative electrode tabs 41 and 42 and the positive and negative electrode adapter sheets 21 and 22 respectively, the surfaces of the positive and negative electrode adapter sheets 21 and 22, the welding points between the positive and negative electrode adapter sheets 21 and 22 and the positive and negative electrode posts 11 and 12 of the top cover assembly 10 respectively, and the welding point between the top cover assembly 10 and the shell 50.
[0087] This method can simultaneously coat the internal surfaces of secondary batteries, particularly those that only form during subsequent assembly, such as welds between components. The protective layer can reduce the heat generated during short-circuit connections, minimizing safety hazards. Furthermore, the protective layer acts as a physical barrier, preventing corrosion.
[0088] In some embodiments, the protective layer includes at least one of a carbide, nitride, sulfide, oxide, fluoride, selenide, and telluride of aluminum, silicon, tin, germanium, chromium, boron, titanium, vanadium, zinc, zirconium, hafnium, or tantalum, and optionally includes at least one of aluminum oxide, silicon oxide, silicon nitride, titanium oxide, and zinc oxide. By controlling the composition of the protective layer, the protective layer can be made more uniform and dense, and the bonding strength between the protective layer and the substrate can be enhanced.
[0089] In some embodiments, after step (2) and / or step (4), the secondary battery is purged with a purge gas, wherein the purge gas comprises at least one of N2, Ar, He, CO2, and the second reactant. This purge step can further enhance the purity and bonding strength of the protective layer.
[0090] In some embodiments, the purging step includes the steps of introducing and extracting a purge gas after the first reactant and / or the second reactant is introduced. The purge parameters include: the ventilation flow rate is related to the battery size and can be 0.01-1000sccm, and the introduction time can be optionally 0.1ms-120min.
[0091] In some embodiments, the thickness of the protective layer is 1 nm to 1000 μm, optionally 50 nm to 500 nm. By controlling the protective layer within a suitable thickness range, while providing insulation protection, the overall mass energy density and volume energy density of the secondary battery are almost unaffected.
[0092] In some embodiments, the protective layer may be subjected to a post-treatment step, including temperature annealing, plasma annealing, or light radiation annealing in a specific atmosphere comprising at least one of pyridine, N₂, Ar, He, CO₂, and the second reactant, and / or a plasma of at least one of these. This post-treatment step can further improve the quality of the protective layer.
[0093] In some embodiments, the temperature annealing treatment includes constant temperature (80-120°C) annealing (10 min-12 h), high temperature and low temperature alternating annealing (high temperature can be 80-120°C, low temperature can be 25-80°C, treatment time 10 min-12 h), etc.
[0094] In some embodiments, the plasma annealing treatment includes direct current pulse plasma, radio frequency plasma, or cyclotron resonance plasma treatment, with a power of generally 5-2000 W and a treatment time of generally 1-120 s.
[0095] In some embodiments, the optical radiation annealing process includes laser annealing, specifically characterized by continuous fiber laser with a power of P max =5W, focused spot r=200μm, scanning speed is 0.01-1mm / s, and the cumulative processing time per unit area is 1-300s.
[0096] In one embodiment of the present application, a secondary battery protection device is provided, comprising:
[0097] a cavity for accommodating a secondary battery;
[0098] a first reactant tank, for storing a first reactant;
[0099] a second reactant tank for storing a second reactant;
[0100] Vacuum pump;
[0101] A pressure gauge, used to detect the pressure inside the secondary battery in real time;
[0102] A flow regulating valve, used to regulate the flow of the first reactant and the second reactant;
[0103] The second reactant is capable of reacting with the first reactant to form a protective layer;
[0104] Among them, the first reactant tank and the second reactant tank are respectively connected to the injection port of the secondary battery contained in the cavity to pass the first reactant and the second reactant into the interior of the secondary battery; and the vacuum pump is connected to the injection port of the secondary battery contained in the cavity to evacuate the secondary battery.
[0105] Through the equipment of the present application, first, the protection reaction requirements can be achieved, including: clamping of unfilled secondary batteries, temperature regulation, real-time detection of air pressure, adjustment of the amount of each reactant, and high airtightness of the pipeline; second, the equipment is simple, which simplifies the protection process of unfilled secondary batteries, while improving efficiency, reducing costs, and facilitating industrial production.
[0106] Figure 7 is a schematic diagram of a protective device for a secondary battery according to one embodiment of the present application. As shown in Figure 7, the device includes a cavity 700 for accommodating a secondary battery 800; a first reactant tank 601 for storing a first reactant; and a second reactant tank 602 for storing a second reactant. The first and second reactant tanks can be connected to the injection ports of the secondary battery 800 contained within the cavity to allow the first and second reactants to enter the interior of the secondary battery; a vacuum pump (not shown) that can be connected to the injection ports of the secondary battery contained within the cavity to evacuate the secondary battery; a pressure gauge (not shown) for real-time monitoring of the pressure within the secondary battery; and flow control valves 611, 612, 613, and 614 for regulating the flow of the first and second reactants.
[0107] In some embodiments, the apparatus further comprises a pressure gauge for detecting the pressures of the first and second reactant tanks in real time.
[0108] In some embodiments, the number of reactant tanks may be increased or decreased according to the type of reactant. For example, a third reactant tank may be included to store a third reactant for deposition.
[0109] In addition, the secondary battery, battery module, battery pack, and electric device of the present application will be described below with reference to the drawings as appropriate.
[0110] In one embodiment of the present application, a secondary battery is provided, which is a secondary battery obtained by protecting by the method described in the first aspect of the present application.
[0111] Typically, a secondary battery consists of a positive electrode, a negative electrode, an electrolyte, and a separator. During the battery's charge and discharge processes, active ions are inserted and removed between the positive and negative electrodes. The electrolyte conducts ions between the positive and negative electrodes. The separator, located between the positive and negative electrodes, primarily prevents short circuits between the positive and negative electrodes while allowing ions to pass through.
[0112] [Positive electrode]
[0113] The positive electrode sheet may include a positive electrode current collector and a positive electrode film layer disposed on at least one surface of the positive electrode current collector, wherein the positive electrode film layer includes a positive electrode active material.
[0114] As an example, the positive electrode current collector has two surfaces opposite to each other in its thickness direction, and the positive electrode film layer is disposed on either or both of the two opposite surfaces of the positive electrode current collector.
[0115] In some embodiments, the positive electrode current collector may be a metal foil or a composite current collector. For example, aluminum foil may be used as the metal foil. The composite current collector may include a polymer material base layer and a metal layer formed on at least one surface of the polymer material base layer. The composite current collector may be formed by forming a metal material (aluminum, aluminum alloy, nickel, nickel alloy, titanium, titanium alloy, silver, and silver alloy, etc.) on a polymer material substrate (such as a substrate of polypropylene (PP), polyethylene terephthalate (PET), polybutylene terephthalate (PBT), polystyrene (PS), polyethylene (PE), etc.).
[0116] In some embodiments, the positive electrode active material may adopt the positive electrode active material for batteries that is well known in the art. As an example, the positive electrode active material may include at least one of the following materials: lithium-containing phosphates with an olivine structure, lithium transition metal oxides, and their respective modified compounds. However, the present application is not limited to these materials, and other materials that can be used as positive electrode active materials for batteries may also be used, such as positive electrode materials for sodium ion batteries. These positive electrode active materials may be used alone or in combination of two or more. Examples of lithium transition metal oxides may include, but are not limited to, lithium cobalt oxide (such as LiCoO2), lithium nickel oxide (such as LiNiO2), lithium manganese oxide (such as LiMnO2, LiMn2O4), lithium nickel cobalt oxide, lithium manganese cobalt oxide, lithium nickel manganese oxide, lithium nickel cobalt manganese oxide (such as LiNi 1 / 3 Co 1 / 3 Mn 1 / 3 O2 (also referred to as NCM333), LiNi 0.5 Co 0.2 Mn 0.3 O2 (also referred to as NCM523), LiNi 0.5 Co 0.25 Mn 0.25 O2 (also referred to as NCM211), LiNi 0.6 Co 0.2 Mn 0.2 O2 (also referred to as NCM622), LiNi 0.8 Co 0.1 Mn 0.1 O2 (also referred to as NCM811), lithium nickel cobalt aluminum oxide (such as LiNi 0.85 Co 0.15 Al 0.05O2) and its modified compounds. Examples of olivine-structured lithium-containing phosphates may include, but are not limited to, at least one of lithium iron phosphate (such as LiFePO4 (also referred to as LFP)), a composite material of lithium iron phosphate and carbon, lithium manganese phosphate (such as LiMnPO4), a composite material of lithium manganese phosphate and carbon, lithium iron manganese phosphate, and a composite material of lithium iron manganese phosphate and carbon.
[0117] In some embodiments, the positive electrode film layer may further optionally include a binder. As an example, the binder may include at least one of polyvinylidene fluoride (PVDF), polytetrafluoroethylene (PTFE), a vinylidene fluoride-tetrafluoroethylene-propylene terpolymer, a vinylidene fluoride-hexafluoropropylene-tetrafluoroethylene terpolymer, a tetrafluoroethylene-hexafluoropropylene copolymer, and a fluorine-containing acrylate resin.
[0118] In some embodiments, the positive electrode film layer may further include a conductive agent. For example, the conductive agent may include at least one of superconducting carbon, acetylene black, carbon black, Ketjen black, carbon dots, carbon nanotubes, graphene, and carbon nanofibers.
[0119] In some embodiments, the positive electrode sheet can be prepared by the following method: the components for preparing the positive electrode sheet, such as the positive electrode active material, the conductive agent, the binder and any other components, are dispersed in a solvent (such as N-methylpyrrolidone) to form a positive electrode slurry; the positive electrode slurry is coated on the positive electrode current collector, and after drying, cold pressing and other processes, the positive electrode sheet can be obtained.
[0120] [Negative electrode]
[0121] The negative electrode sheet may include a negative electrode current collector and a negative electrode film layer disposed on at least one surface of the negative electrode current collector, wherein the negative electrode film layer includes a negative electrode active material.
[0122] As an example, the negative electrode current collector has two surfaces opposite to each other in its thickness direction, and the negative electrode film layer is disposed on either or both of the two opposite surfaces of the negative electrode current collector.
[0123] In some embodiments, the negative electrode current collector may be a metal foil or a composite current collector. For example, copper foil may be used as the metal foil. The composite current collector may include a polymer substrate and a metal layer formed on at least one surface of the polymer substrate. The composite current collector may be formed by forming a metal material (copper, copper alloy, nickel, nickel alloy, titanium, titanium alloy, silver, and silver alloy, etc.) on a polymer substrate (such as a substrate of polypropylene (PP), polyethylene terephthalate (PET), polybutylene terephthalate (PBT), polystyrene (PS), polyethylene (PE), etc.).
[0124] In some embodiments, the negative electrode active material may adopt the negative electrode active material for batteries known in the art. As an example, the negative electrode active material may include at least one of the following materials: artificial graphite, natural graphite, soft carbon, hard carbon, silicon-based materials, tin-based materials, lithium titanate, metallic lithium negative electrode, etc. The silicon-based material may be selected from at least one of elemental silicon, silicon oxides, silicon-carbon composites, silicon-nitrogen composites, and silicon alloys. The tin-based material may be selected from at least one of elemental tin, tin oxides, and tin alloys. However, the present application is not limited to these materials, and other traditional materials that can be used as negative electrode active materials for batteries may also be used. These negative electrode active materials may be used alone or in combination of two or more.
[0125] In some embodiments, the negative electrode film layer may further include a binder. The binder may be selected from at least one of styrene-butadiene rubber (SBR), polyacrylic acid (PAA), sodium polyacrylate (PAAS), polyacrylamide (PAM), polyvinyl alcohol (PVA), sodium alginate (SA), polymethacrylic acid (PMAA), and carboxymethyl chitosan (CMCS).
[0126] In some embodiments, the negative electrode film layer may further include a conductive agent, which may be selected from at least one of superconducting carbon, acetylene black, carbon black, Ketjen black, carbon dots, carbon nanotubes, graphene, and carbon nanofibers.
[0127] In some embodiments, the negative electrode film layer may optionally include other additives, such as a thickener (eg, sodium carboxymethyl cellulose (CMC-Na)).
[0128] In some embodiments, the negative electrode sheet can be prepared by the following method: the components for preparing the negative electrode sheet, such as the negative electrode active material, the conductive agent, the binder and any other components, are dispersed in a solvent (such as deionized water) to form a negative electrode slurry; the negative electrode slurry is coated on the negative electrode current collector, and after drying, cold pressing and other processes, the negative electrode sheet can be obtained.
[0129] [Electrolytes]
[0130] The electrolyte conducts ions between the positive and negative electrodes. This application does not specify the type of electrolyte, and the electrolyte can be selected based on the needs. For example, the electrolyte can be liquid, gel, or solid.
[0131] In some embodiments, the electrolyte is an electrolyte solution comprising an electrolyte salt and a solvent.
[0132] In some embodiments, the electrolyte salt may be selected from at least one of lithium hexafluorophosphate, lithium tetrafluoroborate, lithium perchlorate, lithium hexafluoroarsenate, lithium bis(fluorosulfonyl)imide, lithium bis(trifluoromethanesulfonyl)imide, lithium trifluoromethanesulfonate, lithium difluorophosphate, lithium difluorooxalatoborate, lithium dioxalatoborate, lithium difluorodioxalatophosphate, and lithium tetrafluorooxalatophosphate.
[0133] In some embodiments, the solvent can be selected from at least one of ethylene carbonate, propylene carbonate, ethyl methyl carbonate, diethyl carbonate, dimethyl carbonate, dipropyl carbonate, methylpropyl carbonate, ethylpropyl carbonate, butylene carbonate, fluoroethylene carbonate, methyl formate, methyl acetate, ethyl acetate, propyl acetate, methyl propionate, ethyl propionate, propyl propionate, methyl butyrate, ethyl butyrate, 1,4-butyrolactone, cyclopentane, dimethyl sulfone, methyl ethyl sulfone and diethyl sulfone.
[0134] In some embodiments, the electrolyte may further include additives. For example, the additives may include negative electrode film-forming additives, positive electrode film-forming additives, and additives that can improve certain battery properties, such as additives that improve battery overcharge performance, and additives that improve battery high or low temperature performance.
[0135] [Isolation film]
[0136] In some embodiments, the secondary battery further includes a separator. The present application has no particular limitation on the type of separator, and any known porous separator with good chemical and mechanical stability can be selected.
[0137] In some embodiments, the material of the separator can be selected from at least one of glass fiber, non-woven fabric, polyethylene, polypropylene, and polyvinylidene fluoride. The separator can be a single-layer film or a multi-layer composite film, without particular limitation. When the separator is a multi-layer composite film, the materials of each layer can be the same or different, without particular limitation.
[0138] In some embodiments, the positive electrode sheet, the negative electrode sheet, and the separator can be formed into an electrode assembly through a winding process or a lamination process.
[0139] In some embodiments, the secondary battery may include an outer packaging that can be used to encapsulate the electrode assembly and the electrolyte.
[0140] In some embodiments, the outer packaging of the secondary battery can be a hard shell, such as a hard plastic shell, an aluminum shell, or a steel shell. Alternatively, the outer packaging of the secondary battery can be a soft shell, such as a pouch-type soft shell. The soft shell can be made of plastic, such as polypropylene, polybutylene terephthalate, and polybutylene succinate.
[0141] The present application does not specifically limit the shape of the secondary battery; it can be cylindrical, square, or any other shape. For example, Figure 2 shows a secondary battery 5 with a square structure as an example. Furthermore, the secondary battery of the present application is not limited to hard-shell batteries and may also include soft-pack batteries and other battery types.
[0142] In some embodiments, secondary batteries can be assembled into a battery module. The number of secondary batteries contained in the battery module can be one or more. The specific number can be selected by those skilled in the art according to the application and capacity of the battery module.
[0143] Figure 3 shows an example battery module 4. Referring to Figure 3 , within the battery module 4, multiple secondary batteries 5 may be arranged sequentially along the length of the battery module 4. Of course, any other arrangement is also possible. Furthermore, the multiple secondary batteries 5 may be secured together using fasteners.
[0144] Optionally, the battery module 4 may further include a housing having an accommodation space, and the plurality of secondary batteries 5 are accommodated in the accommodation space.
[0145] In some embodiments, the battery modules described above may also be assembled into a battery pack. The battery pack may contain one or more battery modules, and the specific number may be selected by those skilled in the art based on the application and capacity of the battery pack.
[0146] Figures 4 and 5 illustrate an example battery pack 1. Referring to Figures 4 and 5 , the battery pack 1 may include a battery box and multiple battery modules 4 disposed within the battery box. The battery box comprises an upper case 2 and a lower case 3. The upper case 2 can be placed over the lower case 3 to form an enclosed space for accommodating the battery modules 4. The multiple battery modules 4 can be arranged in any manner within the battery box.
[0147] In addition, the present application also provides an electric device, which includes at least one of the secondary battery, battery module, or battery pack provided in the present application. The secondary battery, battery module, or battery pack can be used as a power source for the electric device, and can also be used as an energy storage unit for the electric device. The electric device may include mobile devices (such as mobile phones, laptops, etc.), electric vehicles (such as pure electric vehicles, hybrid electric vehicles, plug-in hybrid electric vehicles, electric bicycles, electric scooters, electric golf carts, electric trucks, etc.), electric trains, ships and satellites, energy storage systems, etc., but is not limited thereto.
[0148] As the electrical device, a secondary battery, a battery module or a battery pack can be selected according to its usage requirements.
[0149] Figure 6 shows an example of an electric device. This device is a pure electric vehicle, a hybrid electric vehicle, or a plug-in hybrid electric vehicle. To meet the high power and high energy density requirements of the secondary battery, a battery pack or battery module can be used.
[0150] Another example device may be a mobile phone, a tablet computer, a notebook computer, etc. Such a device is generally required to be lightweight and thin, and may use a secondary battery as a power source.
[0151] Example
[0152] Below, the embodiment of the present application is described in conjunction with the accompanying drawings. The embodiment described below is exemplary and is only used to explain the present application, and is not to be construed as limiting the present application. Where specific techniques or conditions are not specified in the embodiments, the techniques or conditions described in the literature in this area or the product specifications are used. Where the manufacturer of the reagents or instruments is not specified, they are all conventional products that can be obtained commercially.
[0153] Example 1
[0154] [Preparation of positive electrode sheet]
[0155] The positive electrode active material LiNi 1 / 3 Co 1 / 3 Mn 1 / 3 O2 (NCM333), conductive carbon black, and binder polyvinylidene fluoride (PVDF) are thoroughly stirred and mixed in an appropriate amount of N-methylpyrrolidone (NMP) solvent in a weight ratio of 93:2:5 to form a uniform positive electrode slurry; the positive electrode slurry is coated on a 12μm thick aluminum foil, and after drying and other processes, a positive electrode sheet is obtained.
[0156] [Preparation of negative electrode sheet]
[0157] The negative electrode active material graphite, conductive carbon black, thickener sodium carboxymethyl cellulose (CMC), and binder styrene-butadiene rubber latex (SBR) are fully stirred and mixed in an appropriate amount of deionized water at a weight ratio of 96.5:1.0:1.0:1.5 to form a uniform negative electrode slurry; the negative electrode slurry is coated on an 8 μm thick copper foil, and after drying and other processes, a negative electrode sheet is obtained.
[0158] [Preparation of a non-filled secondary battery]
[0159] The positive electrode sheet, the separator (20 μm thick PP / PE / PP composite film), and the negative electrode sheet are stacked in sequence and then wound to obtain an electrode assembly. The electrode assembly itself has an aluminum positive electrode tab and a copper negative electrode tab. The positive and negative electrode tabs are welded to the aluminum positive electrode adapter and the copper negative electrode adapter, respectively. Then, the positive and negative electrode adapters are welded to the positive and negative electrode posts of the top cover assembly, respectively. Finally, the top cover assembly and the shell are laser welded to obtain a secondary battery without liquid injection, which is connected to the outside world through the liquid injection port on the top cover assembly.
[0160] [Protecting the inner surface of unfilled secondary batteries]
[0161] The internal surface of an unfilled secondary battery is protected by a secondary battery protection device, the device comprising a cavity for accommodating the secondary battery; a first reactant tank for storing a first reactant, and a second reactant tank for storing a second reactant, wherein the first and second reactant tanks can be respectively connected to the injection port of the secondary battery contained in the cavity to pass the first and second reactants into the interior of the secondary battery; a vacuum pump that can be connected to the injection port of the secondary battery contained in the cavity to evacuate the secondary battery; a pressure gauge for real-time detection of the pressure inside the unfilled secondary battery; and a flow regulating valve for regulating the flow of the first reactant and the second reactant. Protecting the internal surface of the unfilled secondary battery includes the following steps:
[0162] Step (1): controlling the temperature of the unfilled secondary battery at 70° C. and evacuating the unfilled secondary battery to 50 Pa through the liquid injection port;
[0163] Step (2): introducing the first reactant, gaseous trimethylaluminum, into the unfilled secondary battery through the liquid injection port until the pressure rises to 100 Pa and maintaining it for 1 second;
[0164] Step (3): evacuating the unfilled secondary battery to 50 Pa through the liquid filling port; and
[0165] Step (4): introducing the second reactant water vapor into the unfilled secondary battery through the liquid injection port until the pressure rises by 100 Pa and maintaining it for 5 seconds;
[0166] Repeat steps (1) to (4) for 1000 times to form an aluminum oxide protective layer with a nanometer thickness on the inner surface of the unfilled secondary battery.
[0167] [Preparation of finished secondary batteries]
[0168] The electrolyte (EC:EMC volume ratio is 3:7, LiPF6 is 1 mol / L) is injected into the non-liquid-injected secondary battery after the above protection, and then the lithium-ion secondary battery is obtained through sealing, standing, hot and cold pressing, and formation processes.
[0169] Example 2-11
[0170] The preparation methods of the secondary batteries of Examples 2-11 are similar to those of the secondary battery of Example 1, except that the conditions for protecting the inner surface of the secondary battery that is not filled with liquid are adjusted. See Table 1 for details.
[0171] Example 12
[0172] The preparation method of the secondary battery of Example 12 is similar to that of the secondary battery of Example 1, except that protecting the inner surface of the secondary battery that is not filled with liquid includes the following steps:
[0173] Step (1): controlling the temperature of the unfilled secondary battery at 75° C. and evacuating the unfilled secondary battery to 100 Pa through the injection port;
[0174] Step (2): introducing the first reactant, tris(dimethylamino)silane (TDMAS) in a gaseous state, into the unfilled secondary battery through the liquid injection port until the pressure rises by 100 Pa and maintaining the pressure for 5 seconds;
[0175] Step (3): evacuate the unfilled secondary battery to 50 Pa through the liquid filling port;
[0176] Step (4): Plasma is introduced through the liquid injection port. The plasma is achieved by discharging a mixture of Ar and O2 at 13.56 MHz radio frequency. The radio frequency power is 1000 W, the Ar carrier gas flow rate is 40 mL / min, and the O2 flow rate is 50 mL / min.
[0177] Repeat steps (1) to (4) for a total of 7,000 times to form a silicon oxide protective layer with a thickness of nanometer and micrometer levels on the inner surface of the secondary battery.
[0178] Example 13
[0179] The preparation method of the secondary battery of Example 13 is similar to that of the secondary battery of Example 12, except that the process conditions are adjusted in protecting the inner surface of the secondary battery that is not injected with liquid. See Table 1 for details.
[0180] Example 14
[0181] The preparation method of the secondary battery of Example 14 is similar to that of the secondary battery of Example 1, except that, in protecting the inner surface of the non-liquid-filled secondary battery, steps (1)-(2) are first repeated 10 times to use the secondary battery's own moisture as the second reactant, and then steps (1)-(4) are repeated 6990 times, wherein water vapor is used as the second reactant. Other process conditions are detailed in Table 1.
[0182] Example 15
[0183] The preparation method of the secondary battery of Example 15 is similar to that of the secondary battery of Example 1, except that before protecting the inner surface of the uninjected secondary battery, the inner surface of the uninjected secondary battery is pre-treated, including Ar plasma cleaning. The Ar plasma is generated by a radio frequency plasma gun with a power of 550 W, a frequency of 13.56 MHz, and a maintenance time of 30 s.
[0184] Example 16
[0185] The preparation method of the secondary battery of Example 16 is similar to that of the secondary battery of Example 1, except that, after step (2) and step (4), a purge step of introducing and extracting a purge gas is added: the purge parameters include: the purge gas is N2, the flow rate is 1 sccm, and the introduction time is 10 s. Other process conditions are detailed in Table 1.
[0186] Example 17
[0187] The preparation method of the secondary battery of Example 17 is similar to that of the secondary battery of Example 1, except that the protective layer is subjected to high-temperature treatment at a temperature of 105° C. for 8 hours.
[0188] Comparative Example 1
[0189] The secondary battery of Comparative Example 1 was prepared in a similar manner to the secondary battery of Example 1, except that the inner surface of the secondary battery not filled with liquid was not protected.
[0190] Parameter testing
[0191] 1. Protective layer thickness
[0192] Using a scanning electron microscope ZEISS sigma 300, 10 different locations were randomly selected in the test sample for testing, and the average value was taken to obtain the thickness of the protective layer.
[0193] 2. Composition of protective layer
[0194] The elemental analysis of the surface of the relevant area was carried out using energy-dispersive X-ray spectroscopy (EDS) equipped with a scanning electron microscope ZEISS sigma 300.
[0195] 3. Resistance
[0196] A conventional commercial G2A sheet resistance meter was used to randomly select 10 different locations in the test sample for testing, and the average value was taken.
[0197] The secondary batteries obtained in the above embodiment and comparative example were tested according to the above process. The specific values are shown in Table 2.
[0198] Table 1
[0199]
[0200]
[0201] As can be seen from Tables 1 and 2, by protecting unfilled secondary batteries using the protection method described in the present application, the exposed surfaces inside the battery, especially the surfaces of the welds produced during the subsequent assembly process, can be integrated, that is, a protective layer is formed on the surface. This protective layer increases the surface resistance, which can effectively reduce the risk of thermal runaway caused by internal short circuits in the battery. At the same time, the protective layer can also reduce the corrosion of internal battery components such as the electrolyte, thereby improving the safety performance of the secondary battery.
[0202] It should be noted that the present application is not limited to the above-mentioned embodiments. The above-mentioned embodiments are merely examples, and any embodiments having substantially the same structure and effect as the technical concept within the scope of the present application are all included in the technical scope of the present application. In addition, without departing from the scope of the present application, any other embodiments that can be conceived by those skilled in the art and that combine some of the constituent elements in the embodiments are also included in the scope of the present application.
Claims
1. A method for protecting a secondary battery, wherein the secondary battery includes a liquid injection port (13), the method comprising: Step (1): evacuating the secondary battery to a pressure within 100 kPa, optionally within 100 Pa, through the liquid injection port (13); Step (2): introducing a first reactant into the secondary battery through the injection port (13) until the pressure rises by more than 1 Pa, optionally by more than 1 kPa, and is maintained for more than 1 ms, optionally for 0.1 s to 600 s; and optionally, Step (3): evacuating the secondary battery through the liquid injection port (13) to within 100 kPa, optionally within 100 Pa; and Step (4): introducing a second reactant into the secondary battery through the injection port (13) until the pressure rises by more than 1 Pa, optionally by more than 1 kPa, and is maintained for more than 1 ms, optionally 0.1 s to 600 s; thereby forming a protective layer on the inner surface of the secondary battery; The second reactant can react with the first reactant to form the protective layer.
2. The secondary battery protection method according to claim 1, wherein: The first reactant includes at least one of a gaseous aluminum compound, a silicon compound, a tin compound, a germanium compound, a chromium compound, a boron compound, a titanium compound, a vanadium compound, a zinc element and a zinc compound, a zirconium compound, a hafnium compound and a tantalum compound; and optionally includes gaseous AlCl3, trimethylaluminum, Al(CH3)2Cl, Al(C2H5)3, Al(OC2H5)3, (CH3)2AlOCH(CH3)2, (CH3CH2)2AlOC2H5, Al(CH3)2OC2H5, Al(N(C2H5)2)3, Al(N(CH3)2)3, SiCl4, SiCl2H2, Si2Cl6, Si(OC2H5)2H2, Si2H6, Si(OC H2CH3)4, Si(OCH3)4, SiH(OCH3)3, SiH(OC2H5)3, (CH3)2Si(OCH3)2, Si(NCO)4, Si(OC2H5)4, H2N(CH2)3Si(OC2H5)3, CH2=CHSi(OCH3)3, (CH2=CH)3SiOCH3 , ((CH3)3CO)3SiOH, (CH3CH2C(CH3)2O)3SiOH, SiH[N(CH3)2]3, SiH2[N(CH3)2]2, SiH2[NH(C4H9)]2, SiH2[N(C2H5)2]2, SiH2[NC2H5CH3]2, SiH3N(C4H9)2, [Si(NHC2H5)3]2, Si(NHC2H5)4, SiH3N(C3H7)2, [SiH2N(C3H7)2]2, Si(N(CH3)2)4, (CH3)3SiN(CH3)2, C7H 17 NSi、C8H 20 N2Si、C8H 17 NO2Si、C7H 18 N2O2Si, SiCl3H, SnCl4, GeCl3, CrO2Cl2, BBr3, TiF4, TiCl4, TiI4, Ti(OCH3)4, Ti(OC2H5)4, Ti(N(CH3)2) 4. Ti(N(C2H5)2)4, Ti(N(CH3)(C2H5))4, VOCl3, Zn, ZnCl2, Zn(CH3)2, Zn(C2H5)2, ZnI2, ZrCl4, ZrI4, Zr( At least one of N(CH3)2)4, Zr(N(C2H5)2)4, Zr(N(CH3)(C2H5))4, HfCl4, HfI4, Hf(NO3)4, Hf(N(CH3)(C2H5))4, Hf(N(CH3)2)4, Hf(N(C2H5)2)4, TaCl5, TaF5, TaI5, Ta(O(C2H5))5, Ta(N(CH3)2)5, Ta(N(C2H5)2)5 and TaBr5.
3. The secondary battery protection method according to claim 1 or 2, wherein: The second reactant includes at least one of H2O, O2, O3, H2, S, (NH4)2S, H2Se, Se, H2Te, Te, HF, TiF4, TaF5, C2H4, CHCl3, H2O2, NO2, N2O, NH3, N2H4, HCOOH, CH3COOH and H2S and / or a plasma of at least one of them.
4. The secondary battery protection method according to any one of claims 1 to 3, wherein: In the steps (1) to (4), the temperature of the secondary battery is maintained at a temperature between 0°C and 200°C.
5. The secondary battery protection method according to any one of claims 1 to 4, wherein: The steps (1) to (4) are repeated 1 to 100,000 times.
6. The secondary battery protection method according to any one of claims 1 to 4, wherein: First, the steps (1) to (2) are repeated 1 to 10 times, and then the steps (1) to (4) are repeated 1 to 100,000 times.
7. The secondary battery protection method according to any one of claims 1 to 6, wherein: The first reactant and the second reactant are introduced by a carrier gas, and the carrier gas includes at least one of nitrogen, argon, carbon dioxide and helium.
8. The secondary battery protection method according to any one of claims 1 to 7, wherein: The method further includes a step of pre-treating the internal surface of the secondary battery before the step (1), which includes introducing at least one of Ar, N2, H2O, O2, O3, H2, S, (NH4)2S, H2Se, Se, H2Te, Te, HF, TiF4, TaF5, C2H4, CHCl3, H2O2, NO2, N2O, NH3, N2H4, HCOOH, CH3COOH and H2S and / or a plasma of at least one of them into the secondary battery through the injection port (13).
9. The secondary battery protection method according to any one of claims 1 to 8, wherein: The secondary battery further comprises an electrode assembly (30), tabs (41, 42), adapter sheets (21, 22), a top cover assembly (10) and a shell (50), wherein the protective layer is formed at the connection between the tabs (41, 42) and the adapter sheets (21, 22), the connection between the adapter sheets (21, 22) and the top cover assembly (10), the connection between the top cover assembly (10) and the shell (50), the inner wall of the top cover assembly (10), the adapter sheets (21, 22), the inner wall of the shell (50), and the outer peripheral surface of the electrode assembly (30).
10. The secondary battery protection method according to any one of claims 1 to 9, wherein: The protective layer includes at least one of carbides, nitrides, sulfides, oxides, fluorides, selenides and tellurides of aluminum, silicon, tin, germanium, chromium, boron, titanium, vanadium, zinc, zirconium, hafnium or tantalum, and optionally includes at least one of aluminum oxide, silicon oxide, silicon nitride, titanium oxide and zinc oxide.
11. The secondary battery protection method according to any one of claims 1 to 10, wherein: The method further includes, after step (2) and / or step (4), a step of purging the secondary battery with a purge gas, wherein the purge gas includes at least one of N2, Ar, He, CO2 and the second reactant.
12. The secondary battery protection method according to any one of claims 1 to 11, wherein: The thickness of the protective layer is 1 nm-1000 μm, optionally 50 nm-500 nm.
13. The secondary battery protection method according to any one of claims 1 to 12, wherein: It also includes a step of post-processing the protective layer, which includes temperature annealing, plasma annealing or light radiation annealing under a specific atmosphere; the specific atmosphere includes pyridine, N2, Ar, He, CO2 and at least one of the second reactants and / or a plasma of at least one of them.
14. A secondary battery protection device comprising: a cavity, for accommodating the secondary battery; a first reactant tank, for storing a first reactant; a second reactant tank, for storing a second reactant; Vacuum pump; A pressure gauge, used to detect the pressure inside the secondary battery in real time; a flow regulating valve, for regulating the flow of the first reactant and the second reactant; The second reactant is capable of reacting with the first reactant to form a protective layer; The first reactant tank and the second reactant tank are respectively connected to the injection port (13) of the secondary battery contained in the cavity to pass the first reactant and the second reactant into the interior of the secondary battery; and the vacuum pump is connected to the injection port (13) of the secondary battery contained in the cavity to evacuate the secondary battery.
15. A secondary battery, wherein: The secondary battery is a secondary battery protected by the secondary battery protection method according to any one of claims 1 to 13.
16. A battery module, wherein: The secondary battery according to claim 15 is included.
17. A battery pack, wherein: A battery module comprising the battery module according to claim 16.
18. An electrical device, wherein: The battery comprises at least one selected from the secondary battery of claim 15 , the battery module of claim 16 , or the battery pack of claim 17 .