Grinding process for irregular forming block in hot forming die

By constructing adjustment surfaces and process supports on the parting surface and forming surface of the thermoforming mold forming block, the problem of the lack of a reference plane in the forming block is solved, stable positioning and high-precision grinding are achieved, and grinding accuracy and maintenance are improved. Convenience.

CN118789366AActive Publication Date: 2024-10-18QINGDAO YINGYUN AUTO PARTS CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411016345.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-27
Publication Date
2024-10-18
Estimated Expiration
2044-07-27

AI Technical Summary

Technical Problem

The thermoforming mold forming block lacks three mutually perpendicular reference planes during grinding, resulting in unstable positioning and low grinding accuracy. Especially when grinding the bottom surface, it is difficult to clamp and fix it, which affects the flatness accuracy.

Method used

A flat adjustment surface is constructed on the parting surface of the forming block, and multiple process supports are constructed on the forming surface to provide three mutually perpendicular reference planes for positioning and support of CNC fine milling and grinding operations.

Benefits of technology

By pre-constructing the adjustment surface and process supports, the stable positioning and high-precision flatness of the forming block during CNC fine milling and grinding are ensured, which improves grinding accuracy and maintenance convenience.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118789366A_ABST
    Figure CN118789366A_ABST
Patent Text Reader

Abstract

The invention discloses a grinding process for an irregular forming block in a hot forming die, and relates to the technical field of hot forming processes. S11, the formed block is transformed before being ground, and the formed block is transformed into a non-standard formed block; s12, grinding each surface of the non-standard forming block; in the step S11, the step of transforming the forming block before grinding comprises the following steps: constructing a flat adjusting surface on a parting surface of the forming block, and constructing a plurality of process supporting feet on a forming surface of the forming block; wherein the adjusting surface, the bottom surface on the forming block and the splicing surface form a three-surface reference of the forming block during CNC finish-milling operation. According to the method, the adjusting surface is constructed in advance before the parting surface of the forming block is formed, and three mutually-perpendicular reference planes are provided for the forming block in the CNC finish-milling machining procedure; according to the technical scheme, the process supporting feet are constructed on the forming face of the forming block in advance, in the grinding machining process, the process supporting feet guarantee the positioning stability of the forming block, and the planeness precision of bottom face grinding machining is also improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of thermoforming technology, and in particular to a grinding process for irregularly formed blocks in a thermoforming die. Background Art

[0002] Generally, thermoforming products are irregular in shape and vary in length from 500mm to 2200mm. To facilitate thermoforming mold processing and subsequent maintenance, the weight of a single thermoforming mold should not be too large. Therefore, the thermoforming mold must be split into several forming blocks of similar length as much as possible according to the characteristics of the thermoforming product.

[0003] The manufacturing of forming blocks requires the following steps: ① cutting the blank - ② CNC rough milling - ③ heat treatment - ④ grinding - ⑤ CNC fine milling; considering the later maintenance cost and the convenience of disassembly and assembly of the forming blocks, the length and width of a single forming block workpiece are usually controlled within 250mm*250mm, and the volume should not be too large.

[0004] Figure 1-Figure 2 A forming block 101 includes a forming surface 101b with an irregular top, a bottom surface 204 located at the bottom of the forming surface 101b, an assembling surface 205 located between the forming surface 101b and the bottom surface 204, and a parting surface 101a located on the adjacent side of the assembling surface 205; wherein the parting surface 101a has an uneven surface with a concave-convex structure.

[0005] At present, in the ④ grinding process, the forming block 101 encounters the following technical problems in the ④ grinding process:

[0006] 1. When the forming block 101 is processed by CNC milling, it is necessary to ensure that the forming block 101 has three mutually perpendicular reference planes, and the flatness and verticality of the three reference planes are required to be very small (within 0-0.03mm); however, the forming block 101 currently does not have three mutually perpendicular reference planes;

[0007] 2. The forming block 101 needs to be precisely positioned during grinding, especially during grinding of the bottom surface 204. The forming surface 101b of the forming block 101 needs to be clamped and fixed in advance. Since the forming surface 101b is irregular, the forming surface 101b of the forming block 101 cannot be precisely fixed, which not only affects the positioning stability of the forming block 101, but also affects the flatness accuracy of the bottom surface 204 after grinding.

[0008] Therefore, how to solve the above problems is a technical problem that technicians in this field urgently need to solve.

[0009] The information disclosed in this background technology section is only intended to enhance the understanding of the overall background of the invention and should not be regarded as an acknowledgment or any form of suggestion that the information constitutes the prior art already known to a person skilled in the art. Summary of the invention

[0010] In view of the above technical problems, an embodiment of the present invention provides a grinding process for irregularly formed blocks in a thermoforming mold to solve the problems raised in the above background technology.

[0011] The present invention provides the following technical solutions:

[0012] A grinding process for irregularly shaped blocks in a hot forming die, comprising:

[0013] S11, transforming the forming block before grinding, transforming the forming block into a non-standard forming block;

[0014] S12, grinding each surface of the non-standard forming block;

[0015] The step of modifying the forming block before grinding in step S11 includes: constructing a flat adjustment surface on the parting surface of the forming block, and constructing a plurality of process support feet on the forming surface of the forming block;

[0016] Among them, the adjustment surface, the bottom surface and the assembly surface on the forming block constitute the three-surface reference of the forming block during CNC fine milling operation; the process support foot is used as the supporting surface of the bottom surface of the forming block during grinding operation.

[0017] Preferably, the process support feet include four, and the four process support feet are respectively fixed at four corners of the forming surface.

[0018] Preferably, the step of grinding each surface of the non-standard formed block in S12 comprises:

[0019] S31, grinding process support foot;

[0020] The non-standard forming block is placed on the electromagnetic workbench of the grinder, and the bottom surface of the non-standard forming block is attached to the electromagnetic workbench of the grinder; the permanent magnetic fixture is placed close to the non-standard forming block on the electromagnetic workbench of the grinder, and the permanent magnetic chuck of the permanent magnetic fixture is attached to the assembly surface of the non-standard forming block;

[0021] The permanent magnetic fixture and the electromagnetic worktable of the grinder are turned on respectively, so that the non-standard forming block and the permanent magnetic fixture are adsorbed on the electromagnetic worktable of the grinder; the grinding wheel performs equal-height grinding on the end faces of multiple process support legs;

[0022] S32, grinding bottom surface;

[0023] The non-standard forming block in step S is turned over 180 degrees, and the process support feet are placed on the electromagnetic workbench of the grinder with the workpiece facing downward; the permanent magnetic fixture is placed on the electromagnetic workbench of the grinder, and the permanent magnetic chuck of the permanent magnetic fixture is attached to the assembly surface of the non-standard forming block;

[0024] The permanent magnetic fixture and the electromagnetic workbench of the grinder are turned on respectively, so that the non-standard forming block and the permanent magnetic fixture are adsorbed on the electromagnetic workbench of the grinder; the grinding wheel is used to grind the bottom surface;

[0025] S33, grinding assembly surface;

[0026] The non-standard formed block in step S32 is turned over 90 degrees, so that one assembly surface of the non-standard formed block is attached to the electromagnetic workbench of the grinder; the permanent magnetic fixture is placed on the electromagnetic workbench of the grinder, and the permanent magnetic chuck of the permanent magnetic fixture is attached to the bottom surface of the non-standard formed block;

[0027] The permanent magnetic fixture and the electromagnetic workbench of the grinder are turned on respectively, so that the non-standard forming block and the permanent magnetic fixture are adsorbed on the electromagnetic workbench of the grinder; the grinding wheel is used to grind the assembly surface;

[0028] After the grinding of the first assembly surface is completed, the non-standard formed block is turned 180 degrees, so that the other assembly surface of the non-standard formed block is attached to the electromagnetic workbench of the grinder, and then the operation in step S33 is repeated to grind the other assembly surface;

[0029] S34, grinding adjustment surface;

[0030] The non-standard forming block in step S33 is rotated 90° so that one adjustment surface of the non-standard forming block is attached to the electromagnetic workbench of the grinder, and the permanent magnetic fixture is placed on the electromagnetic workbench of the grinder, and the permanent magnetic chuck of the permanent magnetic fixture is attached to the bottom surface of the non-standard forming block;

[0031] The permanent magnetic fixture and the electromagnetic workbench of the grinder are turned on respectively, so that the non-standard forming block and the permanent magnetic fixture are adsorbed on the electromagnetic workbench of the grinder; the grinding wheel is used to grind the adjustment surface;

[0032] When the grinding of the first adjustment surface is completed, the non-standard forming block is flipped 180° so that the other adjustment surface of the non-standard forming block is attached to the electromagnetic workbench of the grinder, and then the operation in step S34 is repeated to grind the other adjustment surface to complete the grinding operation.

[0033] Preferably, in step S31, the non-standard forming block has a deformation error within 0.2 mm after heat treatment, and the bottom surface and assembly surface of the non-standard forming block cannot be well attracted to the permanent magnetic suction cup on the permanent magnetic tooling and the bottom surface of the tooling on the permanent magnetic tooling at the same time. It is necessary to pad a thin paper sheet in the gap between the bottom surface of the non-standard forming block and the surface of the electromagnetic workbench of the grinder so that the assembly surface can be well attracted to the surface of the permanent magnetic suction cup.

[0034] Preferably, in step S32, since the process support foot is relatively small, there may be a gap between the contact surface of the process support foot and the electromagnetic worktable surface of the grinder, and a hammer is used to tap the bottom surface to ensure that the gap between the contact surface of the process support foot and the electromagnetic worktable surface of the grinder is eliminated.

[0035] Preferably, in step S33, equal height blocks are placed between the assembly surface and the electromagnetic worktable of the grinder, so that the top surface of the assembly surface is higher than the top surface of the permanent magnetic tooling, which is convenient for the operation of the grinding wheel.

[0036] Preferably, in step S34, in order to ensure that the adjustment surface, the bottom surface, and the assembly surface are respectively vertical, it is necessary to check and adjust the verticality of the assembly surface and the electromagnetic worktable surface of the grinder by using a lever dial indicator.

[0037] Preferably, the permanent magnetic fixture is in a right-angle shape, including a fixture bottom surface and a permanent magnetic adsorption surface, and a permanent magnetic suction cup is fixedly arranged on the permanent magnetic adsorption surface.

[0038] A grinding process for an irregular forming block in a hot forming mold provided by an embodiment of the present invention has the following beneficial effects: the present invention pre-constructs an adjustment surface before the parting surface of the forming block is formed, providing three mutually perpendicular reference planes for the forming block in the CNC fine milling process; process support feet are pre-constructed on the forming surface of the forming block, and in the grinding process, the process support feet ensure the stability of the positioning of the forming block and also improve the accuracy of the flatness of the bottom surface grinding. BRIEF DESCRIPTION OF THE DRAWINGS

[0039] Figure 1 This is a structural schematic diagram of the forming block angle 1 in the present invention;

[0040] Figure 2 This is a schematic diagram of the structure of the forming block angle 2 in the present invention;

[0041] Figure 3 This is a schematic diagram of the structure of the non-standard forming block angle 1 in the present invention;

[0042] Figure 4 This is a schematic diagram of the structure of the non-standard forming block angle 2 in the present invention;

[0043] Figure 5 It is a structural schematic diagram of the permanent magnetic tooling in the present invention;

[0044] Figure 6 A demonstration diagram of the grinding process support foot in the present invention;

[0045] Figure 7 A demonstration diagram of grinding the bottom surface in the present invention;

[0046] Figure 8 A demonstration diagram of grinding the assembly surface in the present invention;

[0047] Fig. 9 A demonstration diagram of the grinding adjustment surface in the present invention;

[0048] Fig.10 It is a schematic diagram of the structure of the medium-high block of the present invention;

[0049] Fig.11 It is a schematic diagram of the three-dimensional structure of the grinding process support leg in the present invention. DETAILED DESCRIPTION

[0050] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present invention.

[0051] See also Figure 1-Figure 11 .

[0052] In view of the problems mentioned in the above background technology, an embodiment of the present invention provides a grinding process for irregularly formed blocks in a hot forming mold to solve the above technical problems. The technical solution is as follows:

[0053] A grinding process for an irregularly formed block 101 in a thermoforming die comprises:

[0054] S11, transforming the forming block 101 before grinding, transforming the forming block 101 into a non-standard forming block 201;

[0055] S12, grinding each surface of the non-standard forming block 201;

[0056] The step of modifying the forming block 101 before grinding in step S11 includes: constructing a flat adjustment surface 203 on the parting surface 101a of the forming block 101, and constructing a plurality of process legs 206 on the forming surface 101b of the forming block 101;

[0057] The adjustment surface 203, the bottom surface 204 and the assembly surface 205 on the forming block 101 constitute the three-surface reference of the forming block 101 during CNC fine milling operation; the three-surface reference can be understood as: the bottom surface 204, the assembly surface 205 and the adjustment surface 203 are perpendicular to each other;

[0058] The process support foot 206 is used as a support surface for the bottom surface 204 of the forming block 101 during the grinding operation; the process support foot 206 is parallel to the end surface of the bottom surface 204 and has the same height as that of the bottom surface 204 .

[0059] It should be noted that the adjustment surface 203 and the process support feet 206 are both completed in the ② CNC rough milling process. The addition of the adjustment surface 203 not only enables the forming block 101 to have three mutually perpendicular reference planes, but also makes the forming block 101 more stable after being placed on the grinder workbench; the adjustment surface 203 will be cut off by wire cutting after the ⑤ CNC fine milling process; the process support feet 206 are only used in the ④ grinding process to ensure the positioning stability of the forming block 101 and to improve the flatness accuracy of the bottom surface 204 after grinding. In the ⑤ CNC fine milling process, the process support feet 206 will be cut off.

[0060] In this embodiment, the step of grinding each surface of the non-standard formed block in S12 includes:

[0061] S31, grinding process support 206;

[0062] Figure 6 As shown, the non-standard forming block 201 is placed on the electromagnetic workbench 402 of the grinder, and the bottom surface 204 of the non-standard forming block 201 is attached to the electromagnetic workbench 402 of the grinder; the permanent magnetic fixture 301 is placed on the electromagnetic workbench 402 of the grinder close to the non-standard forming block 201, and the permanent magnetic chuck 302 of the permanent magnetic fixture 301 is attached to the assembly surface 205 of the non-standard forming block 201;

[0063] The permanent magnetic fixture 301 and the electromagnetic workbench 402 of the grinder are respectively turned on, so that the non-standard forming block 201 and the permanent magnetic fixture 301 are both adsorbed on the electromagnetic workbench 402 of the grinder; the grinding wheel 501 works to grind the end surface of the process support foot 206 at the same height;

[0064] S32, grinding the bottom surface 204;

[0065] like Figure 7 As shown, the non-standard forming block 201 in step S31 is turned 180 degrees, and the process support 206 is placed on the electromagnetic workbench 402 of the grinder with the process support 206 facing downward; the permanent magnetic fixture 301 is placed on the electromagnetic workbench 402 of the grinder, and the permanent magnetic chuck 302 of the permanent magnetic fixture 301 is attached to the assembly surface 205 of the non-standard forming block 201;

[0066] The permanent magnetic fixture 301 and the electromagnetic workbench 402 of the grinder are turned on respectively, so that the non-standard forming block 201 and the permanent magnetic fixture 301 are both adsorbed on the electromagnetic workbench 402 of the grinder; the grinding wheel 501 works to grind the bottom surface 204;

[0067] S33, grinding assembly surface 205;

[0068] like Figure 8As shown, the non-standard forming block 201 in step S32 is turned over 90 degrees, so that an assembly surface 205 of the non-standard forming block 201 is attached to the electromagnetic workbench 402 of the grinder; the permanent magnetic fixture 301 is placed on the electromagnetic workbench 402 of the grinder, and the permanent magnetic chuck 302 of the permanent magnetic fixture 301 is attached to the bottom surface 204 of the non-standard forming block 201;

[0069] The permanent magnetic fixture 301 and the electromagnetic workbench 402 of the grinder are turned on respectively, so that the non-standard forming block 201 and the permanent magnetic fixture 301 are both adsorbed on the electromagnetic workbench 402 of the grinder; the grinding wheel 501 works to grind the assembly surface 205;

[0070] After the grinding of the first assembly surface 205 is completed, the non-standard formed block 201 is turned 180° so that the other assembly surface 205 of the non-standard formed block 201 is attached to the electromagnetic workbench 402 of the grinder, and then the operation in step S33 is repeated to grind the other assembly surface 205;

[0071] S34, grinding adjustment surface 203;

[0072] like Fig. 9 As shown, the non-standard forming block 201 in step S33 is rotated 90° so that an adjustment surface 203 of the non-standard forming block 201 is attached to the electromagnetic workbench 402 of the grinder, and the permanent magnetic fixture 301 is placed on the electromagnetic workbench 402 of the grinder, and the permanent magnetic chuck 302 of the permanent magnetic fixture 301 is attached to the bottom surface 204 of the non-standard forming block 201;

[0073] The permanent magnetic fixture 301 and the electromagnetic workbench 402 of the grinder are turned on respectively, so that the non-standard forming block 201 and the permanent magnetic fixture 301 are both adsorbed on the electromagnetic workbench 402 of the grinder; the grinding wheel 501 works to grind the adjustment surface 203;

[0074] When the grinding of the first adjustment surface 203 is completed, the non-standard forming block 201 is flipped 180° so that the other adjustment surface 203 of the non-standard forming block 201 is attached to the electromagnetic worktable 402 of the grinder, and then the operation in step S34 is repeated to grind the other adjustment surface 203 to complete the grinding operation.

[0075] In this embodiment, in step S31, the non-standard forming block 201 has a deformation error within 0.2mm after heat treatment, and the bottom surface 204 and the assembly surface 205 of the non-standard forming block 201 cannot be well attracted with the permanent magnetic suction cup 302 on the permanent magnetic tooling 301 and the tooling bottom surface 307 on the permanent magnetic tooling 301 at the same time. It is necessary to pad a thin paper sheet (generally the thickness of the paper sheet is 0.06-0.08mm) in the gap between the bottom surface 204 of the non-standard forming block 201 and the surface of the electromagnetic workbench 402 of the grinder so that the assembly surface 205 can be well attracted with the surface of the permanent magnetic suction cup 302.

[0076] In this embodiment, in step S32, since the process support foot 206 is relatively small, there may be a gap between the contact surface of the process support foot 206 and the surface of the electromagnetic worktable 402 of the grinder, and a hammer is needed to tap the bottom surface 204 to ensure that the gap between the contact surface of the process support foot 206 and the surface of the electromagnetic worktable 402 of the grinder is eliminated.

[0077] In this embodiment, in step S33, an equal height block 601 is placed between the assembly surface 205 and the surface of the electromagnetic workbench 402 of the grinder, so that the top surface of the assembly surface 205 is higher than the top surface of the permanent magnetic tooling 301, which facilitates the operation of the grinding wheel 501.

[0078] In this embodiment, in step S34, to ensure that the adjustment surface 203, the bottom surface 204, and the assembly surface 205 are respectively vertical, it is necessary to check and adjust the verticality of the assembly surface 205 and the surface of the electromagnetic worktable 402 of the grinder by using a lever dial indicator (minimum scale 0.01 mm).

[0079] In this embodiment, the permanent magnetic fixture 301 is in a right angle shape, including a fixture bottom surface 307 and a permanent magnetic adsorption surface, on which a permanent magnetic suction cup 302 is fixedly arranged; the permanent magnetic suction cup 302 and the fixture bottom surface 307 must be installed vertically, and the verticality error is within 0.01 mm.

[0080] A rear longitudinal beam laser cutting fixture provided by an embodiment of the present invention has the following beneficial effects: the present invention pre-constructs an adjustment surface before the parting surface of the forming block is formed, providing three mutually perpendicular reference planes for the forming block in the CNC fine milling process; process support feet are pre-constructed on the forming surface of the forming block, and in the grinding process, the process support feet ensure the stability of the positioning of the forming block and also improve the accuracy of the flatness of the bottom surface grinding.

[0081] The device embodiments described above are merely illustrative, wherein the units described as separate components may or may not be physically separated, and the components shown as units may or may not be physical units, and may be located in one place or distributed over multiple network units. Some or all of the modules may be selected according to actual needs to achieve the purpose of the solution of this embodiment.

[0082] In the present invention, unless otherwise clearly stipulated and limited, the terms such as "installation", "setting", "connection", "fixation" and "screw-on" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium; it can be the internal connection of two elements or the interaction relationship between two elements. Unless otherwise clearly defined, ordinary technicians in this field can understand the specific meanings of the above terms in the present invention according to the specific circumstances.

[0083] It is understandable that those skilled in the art can make equivalent substitutions or changes based on the technical solution and concept of the present invention, and all these changes or substitutions should fall within the protection scope of the claims attached to the present invention.

Claims

1. A grinding process for irregularly shaped blocks in a thermoforming mold, characterized in that: include: S11, transforming the forming block before grinding, transforming the forming block into a non-standard forming block; S12, grinding each surface of the non-standard forming block; The step of modifying the forming block before grinding in step S11 includes: constructing a flat adjustment surface on the parting surface of the forming block, and constructing a plurality of process support feet on the forming surface of the forming block; Among them, the adjustment surface, the bottom surface and the assembly surface on the forming block constitute the three-surface reference of the forming block during CNC fine milling operation; the process support foot is used as the supporting surface of the bottom surface of the forming block during grinding operation.

2. The grinding process of irregularly shaped blocks in a thermoforming mold according to claim 1, characterized in that: The process support feet include four, and the four process support feet are respectively fixed at four corner positions of the forming surface.

3. The grinding process of irregularly shaped blocks in a thermoforming mold according to claim 1, characterized in that: The steps of grinding each surface of the non-standard forming block in S12 include: S31, grinding process support foot; The non-standard forming block is placed on the electromagnetic workbench of the grinder, and the bottom surface of the non-standard forming block is attached to the electromagnetic workbench of the grinder; the permanent magnetic fixture is placed close to the non-standard forming block on the electromagnetic workbench of the grinder, and the permanent magnetic chuck of the permanent magnetic fixture is attached to the assembly surface of the non-standard forming block; The permanent magnetic fixture and the electromagnetic worktable of the grinder are turned on respectively, so that the non-standard forming block and the permanent magnetic fixture are adsorbed on the electromagnetic worktable of the grinder; the grinding wheel performs equal-height grinding on the end faces of multiple process support legs; S32, grinding bottom surface; The non-standard formed block in step S31 is turned over 180 degrees, and the process support feet are placed on the electromagnetic workbench of the grinder with the workpiece facing downward; the permanent magnetic fixture is placed on the electromagnetic workbench of the grinder, and the permanent magnetic chuck of the permanent magnetic fixture is attached to the assembly surface of the non-standard formed block; The permanent magnetic fixture and the electromagnetic workbench of the grinder are turned on respectively, so that the non-standard forming block and the permanent magnetic fixture are adsorbed on the electromagnetic workbench of the grinder; the grinding wheel is used to grind the bottom surface; S33, grinding assembly surface; The non-standard formed block in step S32 is turned over 90 degrees, so that one assembly surface of the non-standard formed block is attached to the electromagnetic workbench of the grinder; the permanent magnetic fixture is placed on the electromagnetic workbench of the grinder, and the permanent magnetic chuck of the permanent magnetic fixture is attached to the bottom surface of the non-standard formed block; The permanent magnetic fixture and the electromagnetic workbench of the grinder are turned on respectively, so that the non-standard forming block and the permanent magnetic fixture are adsorbed on the electromagnetic workbench of the grinder; the grinding wheel is used to grind the assembly surface; After the grinding of the first assembly surface is completed, the non-standard formed block is turned 180 degrees, so that the other assembly surface of the non-standard formed block is attached to the electromagnetic workbench of the grinder, and then the operation in step S33 is repeated to grind the other assembly surface; S34, grinding adjustment surface; The non-standard forming block in step S33 is rotated 90° so that one adjustment surface of the non-standard forming block is attached to the electromagnetic workbench of the grinder, and the permanent magnetic fixture is placed on the electromagnetic workbench of the grinder, and the permanent magnetic chuck of the permanent magnetic fixture is attached to the bottom surface of the non-standard forming block; The permanent magnetic fixture and the electromagnetic workbench of the grinder are turned on respectively, so that the non-standard forming block and the permanent magnetic fixture are adsorbed on the electromagnetic workbench of the grinder; the grinding wheel is used to grind the adjustment surface; When the grinding of the first adjustment surface is completed, the non-standard forming block is flipped 180° so that the other adjustment surface of the non-standard forming block is attached to the electromagnetic workbench of the grinder, and then the operation in step S34 is repeated to grind the other adjustment surface to complete the grinding operation.

4. The grinding process of irregularly shaped blocks in a hot forming mold according to claim 3, characterized in that: In step S31, the non-standard forming block has a deformation error of less than 0.2mm after heat treatment, and the bottom surface and assembly surface of the non-standard forming block cannot be well attracted with the permanent magnetic suction cup on the permanent magnetic tooling and the bottom surface of the tooling on the permanent magnetic tooling at the same time. It is necessary to pad a thin paper sheet in the gap between the bottom surface of the non-standard forming block and the surface of the electromagnetic worktable of the grinder to make the assembly surface and the surface of the permanent magnetic suction cup attract well.

5. The grinding process of irregularly shaped blocks in a thermoforming mold according to claim 3, characterized in that: In step S32, since the process support foot is relatively small, there may be a gap between the contact surface of the process support foot and the electromagnetic worktable surface of the grinder, and a hammer is needed to tap the bottom surface to ensure that the gap between the contact surface of the process support foot and the electromagnetic worktable surface of the grinder is eliminated.

6. The grinding process of irregularly shaped blocks in a thermoforming mold according to claim 3, characterized in that: In step S33, equal height blocks are placed between the assembly surface and the electromagnetic worktable of the grinder, so that the top surface of the assembly surface is higher than the top surface of the permanent magnetic fixture, which is convenient for the grinding wheel to work.

7. The grinding process of irregularly shaped blocks in a thermoforming mold according to claim 3, characterized in that: In step S34, in order to ensure that the adjustment surface, the bottom surface and the assembly surface are respectively vertical, it is necessary to check and adjust the verticality of the assembly surface and the electromagnetic worktable surface of the grinder by using a lever dial indicator.

8. The grinding process of irregularly shaped blocks in a thermoforming mold according to claim 3, characterized in that: The permanent magnetic fixture is in a right-angle shape, and comprises a fixture bottom surface and a permanent magnetic adsorption surface, on which a permanent magnetic suction cup is fixedly arranged.

Citation Information

Patent Citations

  • Machining method for reference end face and non-reference end face of super-huge type thin-wall bearing ring

    CN102601697A

  • Stainless steel table board grinding and positioning tool and grinding and positioning method thereof

    CN117697624A

  • Device for planarizing semiconductor wafer

    JP2001053037A

  • Manufacturing method for glass substrate

    JP2010179395A

  • Diamond cutting tool and method for manufacturing the same

    JP2011088264A