Submarine pipeline residual strength prediction method and device and storage medium

By constructing a theoretical random field model and a nonlinear finite element analysis model, combined with a convolutional neural network, the problem of residual strength assessment of random corrosion defects in submarine pipelines is solved, and efficient and accurate prediction of the residual strength of submarine pipelines is achieved, reducing the cost Structural safety risks.

CN118798031AInactive Publication Date: 2024-10-18CHINA UNIV OF GEOSCIENCES (WUHAN)
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202410793508.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-19
Publication Date
2024-10-18
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

It is difficult to accurately assess the impact of random corrosion defects on the residual strength of submarine pipelines with existing technology, leading to increased structural safety risks.

Method used

A theoretical random field model based on the geometric parameters of corrosion defects is constructed, combined with nonlinear finite element analysis (RF-NFEA) and convolutional neural network (CNN) models, to predict the residual strength of submarine pipelines.

Benefits of technology

By constructing the RF-NFEA model and RF-NFEA-CNN model, we can accurately describe the geometric features of irregular defects and their impact on structural failure behavior, achieve efficient and accurate prediction of the remaining strength of submarine pipelines, and reduce the risk of structural failure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118798031A_ABST
    Figure CN118798031A_ABST
Patent Text Reader

Abstract

The invention provides a submarine pipeline residual strength prediction method and device and a storage medium, and relates to the field of oil and gas resource transportation. The method comprises the steps that a corrosion defect geometric model and a pipeline geometric model are constructed and assembled to obtain a geometric model of a pipeline with defects, the geometric model of the pipeline with the defects and an NFEA model are combined to obtain an RF-NFEA model, a data set is constructed based on the RF-NFEA model, the data set is used for training the constructed RF-NFEA-CNN model, and the trained RF-NFEA-CNN model is used for predicting the residual strength of the pipeline; the device and the storage medium are used for realizing the submarine pipeline residual strength prediction method. The method has the beneficial effects that the RF-NFEA model is constructed by considering the action mechanism of the residual wall thickness space variability of the corrosion defect material on the pipeline structure, the residual strength of the pipeline is accurately estimated, and the efficient and accurate prediction of the residual strength of the pipeline is realized by the constructed RF-NFEA-CNN model.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of oil and gas resource transportation, and in particular to a method, a device and a storage medium for predicting the residual strength of a submarine pipeline. Background Art

[0002] Due to its significant advantages such as economy and high efficiency, submarine pipelines have become the core basic unit in the current marine oil and gas development system, and undertake the important task of transporting oil and gas resources. Therefore, the structural safety of submarine pipelines is the primary prerequisite for ensuring the stability of oil and gas development and production. Compared with onshore pipelines, submarine pipelines have a more severe service environment, spanning the "five zones" of marine corrosion, and the corrosion problem is severe. Statistics show that corrosion is the main cause of submarine pipeline failure. Material loss caused by corrosion will cause stress concentration under the working internal pressure load of the pipeline, significantly reduce the ultimate bearing capacity of the structure, and lead to pipeline explosion and crude oil leakage. Therefore, accurately estimating the residual strength of pipelines with corrosion defects is the key to ensuring structural safety. However, due to the influence of many factors such as environment, materials, biochemical processes and their interactions, the marine corrosion mechanism is complex and contains significant uncertainty, which makes the generation and development of pipeline corrosion defects highly random, so the remaining material in the defect area has obvious spatial variability characteristics. Related research shows that the spatial distribution pattern of corrosion defects will change the stress-strain distribution characteristics of the structure under internal pressure load and the evolution mechanism of the failure path, thereby significantly affecting the residual strength of the pipeline structure. The traditional residual strength assessment method based on the regular defect assumption is no longer applicable.

[0003] In summary, there is no effective method for residual strength assessment of pipelines with random corrosion defects. Due to the lack of consideration of the mechanism of random corrosion defects on pipeline failure, the existing experimental, theoretical and numerical analysis models are not perfect, resulting in a large deviation between the residual strength assessment results and the actual results, which introduces potential risks to the safety of pipeline service. Summary of the invention

[0004] The purpose of the present invention is to solve the problem that it is difficult to evaluate the mechanism of action of random corrosion defects on residual strength in the prior art. The present invention provides a method, device and storage medium for predicting the residual strength of a submarine pipeline. A method for predicting the residual strength of a submarine pipeline mainly includes the following steps:

[0005] S1. Obtaining pipeline geometric parameters and corrosion defect geometric parameters;

[0006] S2. constructing a theoretical random field model of corrosion defects based on the geometric parameters of corrosion defects, and then obtaining a geometric model of corrosion defects;

[0007] S3. Establishing a pipeline geometric model through pipeline geometric parameters;

[0008] S4, assembling the pipeline assembly model and the corrosion defect geometric model into the same coordinate space, and obtaining the geometric model of the defective pipeline through Boolean operation;

[0009] S5. Combining the geometric model of the defective pipeline with the NFEA model to obtain the RF-NFEA model;

[0010] S6. Based on the constructed RF-NFEA model, the geometric model of the defective pipeline is sampled and calculated to obtain the spatial distribution field of the sample residual wall thickness and the residual strength of the pipeline, and the sample spatial data set is obtained by combining them.

[0011] S7, build the RF-NFEA-CNN model and use the sample space dataset for training;

[0012] S8. Input the spatial field of the remaining wall thickness of the corrosion defect to be predicted into the trained RF-NFEA-CNN model to obtain the remaining strength of the pipeline.

[0013] Further, the pipeline geometric parameters include the pipeline outer diameter, wall thickness and length;

[0014] The geometric parameters of corrosion defects include defect length and defect width.

[0015] Furthermore, step S2 is specifically as follows:

[0016] S21. Determine the axial and circumferential boundaries of the corrosion defect according to the defect length and defect width;

[0017] S22. Taking the area enclosed by the axial and circumferential boundaries of the corrosion defect as the topological space, a theoretical random field model of the corrosion defect is established in the cylindrical coordinate system according to the statistical characteristics of the defect depth;

[0018] S23, converting the coordinates of the theoretical random field model in the cylindrical coordinate system to the corrected coordinate system, and discretizing the theoretical random field in the corrected coordinate system to obtain a discretized theoretical random field model;

[0019] S24. Based on the nodes of the discrete random field, a sweeping mesh generation algorithm is used to generate corresponding meshes layer by layer along the radial direction of the pipeline until the outermost mesh surface coincides with the outer surface of the pipeline, and a corrosion defect mesh model is obtained. The corresponding corrosion defect geometric model is generated according to the outer surface node coordinates.

[0020] Furthermore, step S4 is specifically as follows:

[0021] S41, assembling the defect-free pipeline geometric model and the corrosion defect geometric model into the same Cartesian coordinate system;

[0022] S42, aligning the cross-section centers of the defect-free pipeline geometric model and the corrosion defect geometric model, determining an adjustment scheme according to the type of corrosion defect, and then adjusting the relative spatial positions of the models;

[0023] S43, performing Boolean operation on the adjusted model to obtain a geometric model of the defective pipeline.

[0024] Furthermore, step S6 is specifically as follows:

[0025] Based on the constructed RF-NFEA model, the Monte Carlo simulation method is used to sample and calculate the geometric model of the defective pipeline to obtain the spatial distribution field of the sample residual wall thickness and the residual strength of the pipeline, and the sample space data set is obtained by combining them.

[0026] Furthermore, the adjustment plan is determined according to the type of corrosion defect, specifically:

[0027] (1) For circumferentially distributed interaction defects, the random corrosion defect geometric model needs to be rotated circumferentially with the origin as the center; (2) For axially distributed interaction defects, the random corrosion defect geometric model Mc needs to be translated axially; (3) For single defects, no rotation or translation is required.

[0028] Furthermore, the RF-NFEA-CNN model is built based on the CNN network, which includes input layer, convolutional layer, fully connected layer, and output layer;

[0029] The input of the input layer is the spatial distribution field of the remaining wall thickness, and the output of the output layer is the predicted remaining strength of the pipeline. Furthermore, the training step of the RF-NFEA-CNN model adopts the gradient descent algorithm, and the specific steps are as follows:

[0030] S71, inputting the sample residual wall thickness spatial distribution field in the sample space data set into the input layer of the RF-NFEA-CNN model to obtain the predicted output pipeline residual strength of the sample residual wall thickness spatial distribution field;

[0031] S72, taking the sample residual wall thickness spatial distribution field in the sample space data set corresponding to the pipeline residual strength as the expected output, calculating the error between the expected output and the predicted output pipeline residual strength, transferring the error in reverse layer by layer, and correcting the weight and bias according to the chain rule;

[0032] S73, repeat steps S71-S72 until all iteration cycles are completed and the optimal weights and biases are obtained. The model at this time is used as the final RF-NFEA-CNN model

[0033] A storage medium stores instructions and data for implementing a method for predicting the residual strength of a submarine pipeline.

[0034] A computer device comprises: a processor and the storage medium; the processor loads and executes instructions and data in the storage medium to implement a method for predicting the remaining strength of a submarine pipeline.

[0035] The technical solution provided by the present invention has the following beneficial effects: by constructing an RF-NFEA model, the present invention realizes the theoretical description and numerical modeling of the geometric morphological characteristics of irregular defects in submarine pipelines under real conditions, takes into account the mechanism of the spatial variability of the remaining wall thickness of the corrosion defect material on the failure behavior of the pipeline structure under internal pressure load, and accurately estimates the residual strength of the pipeline; by constructing an RF-NFEA-CNN model, the spatial random field characterizing the geometric morphological characteristics of the corrosion defects is feature extracted, and a nonlinear mapping relationship between the spatial random field and the structural failure behavior is established, thereby realizing efficient and accurate prediction of the residual strength of the pipeline. BRIEF DESCRIPTION OF THE DRAWINGS

[0036] The present invention will be further described below with reference to the accompanying drawings and embodiments, in which:

[0037] Figure 1 is a flow chart of a method for predicting residual strength of a submarine pipeline in an embodiment of the present invention;

[0038] Figure 2 is a schematic diagram of the RF model and corrosion defects in different coordinate systems and coordinate transformation relationships in an embodiment of the present invention;

[0039] Figure 3 is a schematic diagram of the topological structure of the RF-NFEA-CNN model in an embodiment of the present invention;

[0040] Figure 4 is a linear regression diagram of the pipeline residual strength predicted by the RF-NFEA-CNN model in an embodiment of the present invention;

[0041] Figure 5 It is a schematic diagram of the operation of the hardware device in the embodiment of the present invention. DETAILED DESCRIPTION

[0042] In order to have a clearer understanding of the technical features, purposes and effects of the present invention, specific embodiments of the present invention are now described in detail with reference to the accompanying drawings.

[0043] Embodiments of the present invention provide a method, a device and a storage medium for predicting the residual strength of a submarine pipeline.

[0044] Please refer to Figure 1 , Figure 1 : is a flow chart of a method for predicting residual strength of a submarine pipeline in an embodiment of the present invention, which specifically includes the following steps:

[0045] The first step is to obtain the geometric parameters of the pipeline and the geometric parameters of the corrosion defects.

[0046] The pipeline geometric parameter information includes the pipeline outer diameter D, wall thickness t, and length L;

[0047] The geometric parameter information of the corrosion defect includes the defect length l d and defect width w d .

[0048] The second step is to build a theoretical random field model of corrosion defects based on the geometric parameters of corrosion defects, and then obtain the geometric model of corrosion defects. The specific steps include:

[0049] Step 1: According to the defect length l in the corrosion defect geometric parameters d and defect width w d , determine the axial and circumferential boundary conditions of the corrosion defect, mathematically expressed as:

[0050]

[0051] Where θ is the circumferential angle corresponding to any unit in the corrosion defect; z is the axial position corresponding to any unit in the corrosion defect; D is the outer diameter of the pipe; l d and d are the corrosion defect length and corrosion width respectively.

[0052] Step 2: Using the area enclosed by the axial and circumferential boundaries of the corrosion defect as the topological space, a theoretical random field model (theoretical RF model) of the corrosion defect is established in the cylindrical coordinate system according to the statistical characteristics of the defect depth.

[0053] The cylindrical coordinate system CSYScyl(R,θ,Z) is established with the center of the outer diameter of the pipe as its origin, and the axes corresponding to its radial, circumferential and axial directions are the R axis, θ axis and Z axis respectively.

[0054] Please refer to Figure 2 , Figure 2 Schematic diagrams of random fields and corrosion defects in different coordinate systems according to an embodiment of the present invention; (a) cylindrical coordinate system, (b) modified cylindrical coordinate system, and (c) Cartesian coordinate system.

[0055] like Figure 2 As shown in (a), according to the topological space D t And the defect depth w in the corrosion defect geometric parameters d The statistical properties of d , variance σ 2 d and autocorrelation distance l c , a theoretical RF model describing the spatial variability of corrosion defects was established RF (r,θ,z).

[0056]

[0057] In the formula, μ RF (·) represents the mean of the random field describing the spatial variation of the depth of the corrosion defect, which is the mean of the residual strength of the pipeline; (r, θ, z) is a point in the cylindrical coordinate system, r, θ, z correspond to the radial, circumferential, and axial coordinate positions of the corrosion defect in the cylindrical coordinate system, respectively; E(·) represents the mean function; Θ s is the sample space; θ s is the sample value corresponding to (r,θ,z) in the sample space; P(θ s ) is the probability of occurrence of (r,θ,z).

[0058] At this time, in the topological space D t Any node can be represented as A i (r p ·θ,y dum =y c =0,z), the corrosion depth is d RF,i (r·θ=r p ·θ,y dum =y c =0,z), the node on the erosion surface is B i (r·θ=r p ·θ,y dum +d RF,i =y c +d RF,i ,z)

[0059] Step 3: Convert the coordinates of the theoretical RF model in the cylindrical coordinate system to the corrected coordinate system, and discretize the theoretical RF model in the corrected coordinate system using the extended optimal linear estimation method to obtain a discretized theoretical RF model, which is specifically:

[0060] (1) Based on the arc length calculation principle, the cylindrical coordinate system is converted into a modified cylindrical coordinate system; Figure 2 As shown in (b), let X = R·θ, Z = Z, Y dum =DR,Y dum The axis direction is perpendicular to the X-axis direction, and the cylindrical coordinate system CSYS cyl The arc surface topological space in (R,θ,Z) is converted into a plane topological space.

[0061] (2) Take the center point of the topological space transformed into a plane as the origin, and the R·θ axis, Y dum Axis and Z axis are used as coordinate axes to establish the modified cylindrical coordinate system CSYS fla (R·θ,Y dum ,Z).

[0062] (3) Based on the above coordinate transformation principle, the theoretical RF model d RF (r·θ,ydum ,z) is expressed in the modified cylindrical coordinate system, and the mathematical expression is as follows:

[0063]

[0064] (4) The expansion optimal linear estimation (EOLE) method is used to discretize the theoretical RF model represented in the modified cylindrical coordinate system to obtain the discretized theoretical RF model The mathematical expression is as follows:

[0065]

[0066] In the formula, C HY is the covariance matrix between the random vectors corresponding to the discrete nodes and the random vectors corresponding to the mapping nodes in the theoretical random field RF model; is the discrete node autocovariance matrix C in the random field YY The eigenvalues ​​and eigenvectors of YY The order retained in the spectral expansion; {ξ i ; (i=1,2,3,…,M)} is a standard normal random vector.

[0067] Preferably, in order to facilitate the subsequent coupling of the RF model with the nonlinear finite element model, the discrete random field in the modified coordinate system is subsequently converted to the Cartesian coordinate system CSYS Car (X=R·cosθ, Y=R·sinθ, Z=Z): Let X=R·cosθ, Y=R·sinθ, Z=Z, such as Figure 2 As shown in (c), the topological space is transformed into a curved surface, and the discretized theoretical RF model can be expressed as Furthermore, the corresponding nodes, corrosion depths, and points on the corrosion surface can be expressed as B i ((rd rf,i )cosθ,(rd rf,i )sinθ,z).

[0068] Step 4: Discretize the theoretical RF model Based on the nodes, the swept mesh generation algorithm is used to generate corresponding meshes layer by layer along the pipeline radial direction until the outermost mesh surface coincides with the outer surface of the pipeline, and the corrosion defect mesh model M is obtained. c,ele (x,y,z); further, according to M c,ele (x, y, z) external surface node coordinates generate the corresponding corrosion defect geometry model M c .

[0069] The third step is to establish the pipeline geometric model through pipeline geometric parameters.

[0070] Based on the pipeline geometric parameter information, namely the pipeline outer diameter D, wall thickness t, and length L, the pipeline geometric model M is established. p df .

[0071] The fourth step is to assemble the pipeline geometry model and the corrosion defect geometry model into the same coordinate space, and obtain the geometry model of the defective pipeline through Boolean operation. The specific steps are as follows:

[0072] Step 1: transform the defect-free pipeline geometry model M p df and random corrosion defect geometry model M c The configuration is in the same Cartesian coordinate system, and the cross-section centers of the above models are aligned;

[0073] Step 2: Adjust the spatial position of the above model according to the corrosion defect type and its corresponding corrosion defect spacing, specifically for three cases:

[0074] First, for the circumferentially distributed interaction defects, the random corrosion defect geometric model M c Rotate around the origin, angle θ r The calculation formula is as follows:

[0075] θ r =(s c +w d ) / D

[0076] In the formula, θ r The circumferential rotation angle required to adjust the relative position of the corrosion defect geometric model and the defect-free pipeline model in space; s c is the annular spacing between adjacent defects in the annularly distributed interaction defects.

[0077] Second, for axially distributed interaction defects, the random corrosion defect geometry model M c Perform axial translation, axial translation distance dis t The calculation is shown below;

[0078] dis t =0.5×(l d +s l )

[0079] In the formula, s l is the axial distance between adjacent defects in the axially distributed interaction defects; t The axial translation distance required to adjust the relative spatial position of the corrosion defect geometric model and the defect-free pipeline model;

[0080] Third, for a single defect, no rotation or translation is required.

[0081] Step 3: After the model assembly and position adjustment are completed, Boolean operation is performed on the above geometric model to remove the geometric area surrounded by the random corrosion defect model from the defect-free pipeline model, and finally the geometric model M of the defective pipeline can be obtained. pc .

[0082] The fifth step is to combine the geometric model of the defective pipeline with the NFEA model to obtain the RF-NFEA model.

[0083] Based on the defective pipeline geometric model Mpc, an RF-NFEA model is constructed for the residual strength prediction of submarine pipelines. The construction method is as follows: (1) the isotropic hardening plastic flow criterion is used to describe the nonlinear characteristics of pipeline materials; (2) the defective pipeline geometric model is meshed, and free meshes are used for the corrosion defect area and structured meshes are used for the non-corroded area; (3) boundary condition definition: fixed end constraint is used for the far end of the pipeline; (4) external load definition: pressure load is applied to the inner surface of the pipeline.

[0084] The partial differential equation describing the RF-NFEA model is as follows:

[0085] Ku=F

[0086] K, u and F are the stiffness matrix, displacement matrix and load matrix of the described system respectively.

[0087] The arc length method is used to iteratively solve the above partial differential equation. The mathematical expression is as follows:

[0088]

[0089] In the formula, K i is the initial tangent stiffness matrix of the i-th load increment; u i is the initial displacement matrix of the i-th load increment; F i is the load of the ith load increment; is the displacement increment of the jth iteration step in the i-th load increment step; is the proportional load factor increment for the jth iteration step in the ith load increment step; is the residual of the jth iteration in the ith load increment; is the internal load of the node at the jth iteration step in the ith load increment; is the node external load at the jth iteration step in the ith load increment step.

[0090] During the RF-NFEA model solution process, in each incremental step, the proportional load factor λ is introduced to flexibly adjust the applied load increment to gradually approach the convergence state, so as to trace the complete loading failure process and post-buckling behavior of the structure and ensure the stability of the entire solution process; after the solution is completed, the residual strength pb of the structure is determined according to the stress-based failure criterion: when the Von-Mises stress in the corrosion defect area exceeds 0.9 times the ultimate tensile strength σuts of the material, the material fails, and the corresponding internal pressure load is the residual strength.

[0091] The residual strength prediction method proposed in the present invention is based on nonlinear finite element analysis. Firstly, the constructed random field-nonlinear finite element model (RF-NFEA model) needs to be verified.

[0092] In the relevant literature, a relatively extensive parametric study was conducted on the residual strength of pipelines containing random corrosion defects composed of pitting clusters under internal pressure loads through physical model experiments and finite element numerical simulations. A total of 11 working conditions were involved, and the pipes involved were X42 and X65 steels, with pipe diameters D = 273-762 mm, wall thicknesses t = 9.3-17.5 mm, lengths L = 1000-2300 mm, and the size of the corrosion defect was length l d =100-30mm, width w d =50-200mm, depth d d =0.25-0.75t. The RF-NFEA model constructed by the present invention is used to numerically reconstruct the above working conditions and solve the corresponding residual strength. The experimental settings and the residual strength comparison results are listed in Table 1.

[0093] Table 1 Comparison results of residual strength

[0094]

[0095]

[0096] Group (a) is the physical model experimental condition, the geometric and material properties of the selected pipe sample are: D = 273mm, t = 9.3mm, l = 1000mm, API-5LBX42; Group (b) is the finite element numerical simulation condition, the geometric and material properties of the selected pipe sample are: D = 762mm, t = 17.5mm, l = 2300mm, API-5LX65; b,lit represents the residual strength obtained from the analysis in the literature; p b,RF-NFEA is the residual intensity calculated by RF-NFEA model; ARE is the absolute relative error, ARE=|(p b,RF-NFEA -p b,lit ) / p b,lit |.

[0097] It can be seen that the residual strength obtained by the RF-NFEA model is in good agreement with the results in the relevant literature. The maximum, minimum and average values ​​of the absolute relative error are ARE max =4.4%,ARE max =0.46% and ARE mean =2.12%. The error is mainly caused by two aspects: (1) Due to the different random seeds used, the geometric morphology characteristics of random corrosion defects in the literature are different from the corresponding characteristics in RF-NFEA, which affects the stress-strain distribution characteristics of the pipeline under internal pressure load and the development of its failure path, resulting in deviations in the residual strength of the two; (2) The corrosion defects constructed by random pitting clusters in the literature simulated by random fields require careful calibration of the parameter-autocorrelation distance that characterizes the random field characteristics. Due to the lack of this information, inappropriate autocorrelation distance is also a potential cause of the final residual strength error. Nevertheless, on the whole, the RF-NFEA model constructed by the present invention can still better capture the mechanism of random corrosion defects on structural failure behavior, accurately estimate its residual strength, and provide a reliable data basis containing physical information for the construction of the prediction method.

[0098] In the sixth step, based on the constructed RF-NFEA model, a sampling calculation is performed on the geometric model of the defective pipeline to obtain the spatial distribution field of the sample residual wall thickness and the residual strength of the pipeline, and the sample spatial data set is constructed in combination.

[0099] The constructed RF-NFEA model uses Monte-Carlo simulation (MCS) to perform sampling calculations and obtain N s The spatial distribution field of the residual wall thickness corresponding to a group of random corrosion defects rt RF,i (r·θ,y dum ,z)=td RF,i (r·θ,y dum ,z) and its corresponding pipeline structure residual strength p b,i , to construct the sample space data set {(rt RF,i (r·θ,y dum ,z),p b,i}; (i=1,2,3,…,N s )}

[0100] Step 7: Build the RF-NFEA-CNN model and train it using the sample space dataset.

[0101] The RF-NFEA-CNN model is built based on the CNN network, which includes input layer, convolution layer, fully connected layer and output layer. Figure 2 As shown in the embodiment of the present invention, the model includes 1× input layer, 3× convolutional layers, 1× fully connected layer and 1× output layer. In the figure, n Convi Indicates the number of filters used in the i-th convolutional layer; n FC is the number of filters in the fully connected layer; L rt , W rt , and C rt are the length, width, and number of channels of the input data of the input layer respectively.

[0102] The input quantity of the input layer is the spatial distribution field of the remaining wall thickness, and the output quantity of the output layer is the predicted remaining strength of the pipeline.

[0103] The RF-NFEA-CNN model training step uses the gradient descent algorithm. The specific steps are as follows:

[0104] Step 1: Input the spatial distribution field of sample residual wall thickness in the sample space data set into the input layer of the RF-NFEA-CNN model to obtain the predicted output pipeline residual strength of the spatial distribution field of sample residual wall thickness.

[0105] The spatial distribution field of the sample residual wall thickness is forwarded to the output layer layer by layer, and its features are extracted and reorganized to construct a nonlinear mapping relationship between it and the structural response, and the predicted value of the pipeline residual strength is obtained. The formula is expressed as follows:

[0106]

[0107] In the formula, and are the output value and activation value of the unit at (x, y) of the jth feature map in the i-th convolutional layer; f(·) is the activation function; M is the number of feature maps, P and Q represent the length and width of the filter respectively; is the weight of the jth filter in the i-th convolutional layer corresponding to the mth feature map in the (i-1)th convolutional layer at (p,q); a (i-1) m,(x+p)(y+q) is the activation value of the unit at (x+p,y+q) in the m-th feature map in the (i-1)th convolutional layer; is the bias of the jth feature map in the i-th convolutional layer;

[0108]

[0109] In the formula, and is the output value and activation value of the jth unit in the i-th fully connected layer; a (i-1) m,p,q is the activation value of the unit at (p,q) in the mth feature map in the (i-1)th convolutional layer;

[0110]

[0111] In the formula, is the output value of the jth unit in the Lth layer (output layer), and L is the total number of layers of the RF-NFEA-CNN model; is the weight between the jth unit in the output layer and the i-th unit in the (L-1)th layer; is the bias of the jth unit in the output layer; is the output value of the i-th unit in the (L-1)-th layer.

[0112] Step 2: Take the residual strength of the pipeline corresponding to the spatial distribution field of the sample residual wall thickness in the sample space data set as the expected output, calculate the error between the expected output and the predicted output pipeline residual strength, transfer the error back layer by layer, and correct the weight and bias according to the chain rule;

[0113]

[0114]

[0115] Where e(W,b) is the error cost function; T is the expected output; η is the learning rate; W i i is the weight matrix between the i-th layer and the (i+1)-th layer; b i is the bias matrix of the i-th layer.

[0116] Step 3: Repeat steps 1 and 2 until all iterations are completed and the optimal weights and biases (W opt ,b opt ), the model at this time is the optimal RF-NFEA-CNN model (CNN opt (W opt ,b opt ,rt RF )).

[0117] In the eighth step, the spatial field of the remaining wall thickness of the corrosion defect to be predicted (obtained from measured data or numerical simulation) is input into the trained RF-NFEA-CNN model to obtain the remaining strength of the pipeline.

[0118] In a submarine pipeline project, the pipeline is made of X80 steel, and the elastic modulus, yield strength and ultimate tensile strength are E s =200GPa,σ y =534.1MPa and σ uts=718.2MPa, the pipe diameter and wall thickness are D=458.8mm and t=8.1mm respectively. The method proposed in the present invention is used to predict the residual strength of the target pipeline during its service life. Table 2 gives the detailed working condition settings in the application case, and the corrosion defect types are single defects, circumferential interaction defects and axial interaction defects.

[0119] Table 2 Working condition settings

[0120]

[0121] For each type of corrosion defect, considering the characteristics of corrosion defects deteriorating with service time, five groups of corrosion defect depths corresponding to the working conditions d are selected with gradually increasing depths. d / t=0.2:0.15:0.8 for analysis. The RF-NFEA model constructed in step 1 was used to perform sampling calculations 200 times for each corrosion depth condition, with a total of 5 groups of conditions. Therefore, each defect type was sampled and calculated 1000 times to form the corresponding sample data set. On this basis, the RF-NFEA-CNN model was constructed for training and prediction. For the test data set, the prediction results are as follows: Figure 4 As shown, Figure 4 The linear regression diagram of the RF-NFEA-CNN model predicting the residual strength of the pipeline in the embodiment of the present invention: (a) single defect I, (b) circumferential distribution interaction defect II-A, (c) axial distribution interaction defect II-B. In general, the results predicted by the RF-NFEA-CNN model are in good agreement with the results calculated by the RF-NFEA model, and its prediction performance is relatively stable. For the working conditions involving circumferential interaction defects and axial interaction defects with more complex nonlinear failure behaviors such as interaction between defects and stress redistribution, the prediction accuracy of the model does not decrease significantly. The error metrics (correlation coefficient R, mean absolute percentage error MAPE) are calculated using the following formula:

[0122]

[0123] In the formula, p b,FEA,i is the i-th sample value of the expected output calculated by the RF-NFEA model in the data set; p b,CNN,i is the i-th sample value of the predicted output obtained by RF-NFEA-CNN in the dataset; and is the mean of the expected output and predicted output in the data set; σ FEA and σ CNN is the standard deviation of the expected and predicted outputs in the data set.

[0124] Calculations show that the error metric, mean absolute percentage error, is maintained between R = 0.94-0.97 and MAPE = 1.8-3.06%. At the same time, for the same type of corrosion defect, the model prediction performance shows a non-monotonic change trend with the increase of corrosion depth, which is determined by the intrinsic relationship between the interaction between corrosion depth, geometric morphology characteristics, structural nonlinear response and the model learning prediction mechanism. Overall, the model prediction performance is still relatively stable. For example, when the defect type is an axial interaction defect (II-B), the corrosion depth d d When / t=0.2-0.8, the corresponding mean absolute percentage error is always maintained at MAPE≤10%, meeting the accuracy requirements of engineering design. In summary, the method proposed in the present invention can reasonably capture the influence of random corrosion defects on failure behavior under different corrosion defect types and different corrosion depth conditions, realize accurate and efficient evaluation of the residual strength of the structure, and provide an effective tool for pipeline safety design to reduce the failure risk of submarine pipeline systems during service.

[0125] Compared with the traditional method, the advantages of the present invention are:

[0126] 1. The present invention constructs a numerical model for evaluating the residual strength of pipelines containing random corrosion defects under internal pressure load.

[0127] Marine corrosion is a complex biochemical process that is affected by many factors and contains significant uncertainties. Therefore, the corrosion defects produced in submarine pipelines under real conditions are complex in shape and have obvious spatial variability, which will further affect the failure behavior and residual strength of the structure. Existing methods do not take this factor into consideration sufficiently, resulting in a large deviation between the residual strength assessment results and the true value. The present invention constructs a random field-nonlinear finite element analysis coupled numerical model RF-NFEA, which uses random fields to describe the geometric morphological characteristics of corrosion defects, and further uses finite element analysis to solve the nonlinear failure behavior of the corresponding pipeline structure under internal pressure loads, so as to achieve a reasonable assessment of the residual strength of the pipeline. Through random field theory and finite element coupling technology, a theoretical explicit description of the characteristics of corrosion defects and the establishment of numerical models can be achieved, which is helpful to carry out parametric analysis research to deeply explore the mechanism of the spatial distribution characteristics of corrosion defects on structural failure, as well as the construction of efficient alternative models.

[0128] 2. The present invention proposes a method for predicting the residual strength of a pipeline containing random corrosion defects.

[0129] The geometric morphological characteristics of random corrosion defects contain information on changes in multiple spatial dimensions and their correlations, and their mechanism of action on structural failure behavior is complex and generally needs to be described in the form of a field. It is difficult to effectively capture the dominant factors in the geometric characteristics that control the residual strength of the structure in the existing prediction methods, and the prediction accuracy is low. The present invention proposes a prediction method for the residual strength of pipelines containing random corrosion defects based on deep learning theory. Based on the filter-feature mapping-nonlinear weighted collaborative system of convolutional neural network theory, the random field spatial information describing the geometric morphological characteristics is extracted and abstracted, and a nonlinear mapping relationship between it and the structural response is constructed. This prediction method has a sufficient theoretical basis, and at the same time replaces the time-consuming iterative solution process in linear finite element analysis with feedforward matrix operations, ultimately achieving efficient and reliable prediction of residual strength, and providing a reliable tool for the safe design and protection of pipeline engineering.

[0130] See also Figure 5 , Figure 5 40 is a schematic diagram of the working of the hardware device of an embodiment of the present invention, wherein the hardware device specifically comprises: a computer device 401, a processor 402 and a storage medium 403.

[0131] A computer device 401: The computer device 401 implements the method for predicting the residual strength of a submarine pipeline.

[0132] Processor 402: The processor 402 loads and executes the instructions and data in the storage medium 403 to implement the method for predicting the residual strength of a submarine pipeline.

[0133] Storage medium 403: the storage medium 403 stores instructions and data; the storage medium 403 is used to implement the method for predicting the residual strength of a submarine pipeline.

[0134] The beneficial effects of the present invention are as follows: the present invention realizes the theoretical description and numerical modeling of the geometric morphological characteristics of irregular defects under real conditions by constructing an RF-NFEA model, considers the mechanism of the spatial variability of the residual wall thickness of the corrosion defect material on the failure behavior of the pipeline structure under internal pressure load, and accurately estimates the residual strength of the pipeline; by constructing an RF-NFEA-CNN model, the spatial random field characterizing the geometric morphological characteristics of the corrosion defect is extracted, and a nonlinear mapping relationship between the spatial random field and the structural failure behavior is established, so as to realize efficient and accurate prediction of the residual strength of the pipeline, reveal the intrinsic connection between the physical failure of the structure and the prediction mechanism of the data-driven model, and develop a structural response prediction method.

[0135] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A method for predicting residual strength of a submarine pipeline, characterized in that: The specific steps include: S1. Obtaining pipeline geometric parameters and corrosion defect geometric parameters; S2. constructing a theoretical random field model of corrosion defects based on the geometric parameters of corrosion defects, and then obtaining a geometric model of corrosion defects; S3. Establishing a pipeline geometric model through pipeline geometric parameters; S4, assembling the pipeline geometric model and the corrosion defect geometric model into the same coordinate space, and obtaining the geometric model of the defective pipeline through Boolean operation; S5. Combining the geometric model of the defective pipeline with the NFEA model to obtain the RF-NFEA model; S6. Based on the constructed RF-NFEA model, the geometric model of the defective pipeline is sampled and calculated to obtain the spatial distribution field of the sample residual wall thickness and the residual strength of the pipeline, and the sample spatial data set is constructed in combination; S7, build the RF-NFEA-CNN model and use the sample space dataset for training; S8. Input the spatial field of the remaining wall thickness of the corrosion defect to be predicted into the trained RF-NFEA-CNN model to obtain the remaining strength of the pipeline.

2. A method for predicting residual strength of a submarine pipeline according to claim 1, characterized in that: Pipeline geometry parameters include pipe outer diameter, wall thickness, and length; The geometric parameters of corrosion defects include defect length and defect width.

3. A method for predicting residual strength of a submarine pipeline according to claim 2, characterized in that: Step S2 includes: S21. Determine the axial and circumferential boundaries of the corrosion defect according to the defect length and defect width; S22. Taking the area enclosed by the axial and circumferential boundaries of the corrosion defect as the topological space, a theoretical random field model of the corrosion defect is established in the cylindrical coordinate system according to the statistical characteristics of the defect depth; S23, converting the coordinates of the theoretical random field model in the cylindrical coordinate system to the corrected coordinate system, and discretizing the theoretical random field model in the corrected coordinate system to obtain a discretized theoretical random field model; S24. Based on the nodes of the discrete random field, a sweeping mesh generation algorithm is used to generate corresponding meshes layer by layer along the radial direction of the pipeline until the outermost mesh surface coincides with the outer surface of the pipeline, and a corrosion defect mesh model is obtained. The corresponding corrosion defect geometric model is generated according to the outer surface node coordinates.

4. A method for predicting residual strength of a submarine pipeline according to claim 3, characterized in that: Step S4 is specifically as follows: S41, assembling the defect-free pipeline geometric model and the corrosion defect geometric model into the same Cartesian coordinate system; S42, aligning the cross-section centers of the defect-free pipeline geometric model and the corrosion defect geometric model, determining an adjustment scheme according to the type of corrosion defect, and then adjusting the relative spatial positions of the models; S43, performing Boolean operation on the adjusted model to obtain a geometric model of the defective pipeline.

5. A method for predicting residual strength of a submarine pipeline according to claim 4, characterized in that: The adjustment scheme is determined according to the type of corrosion defects, specifically: (1) For circumferentially distributed interaction defects, the random corrosion defect geometric model needs to be rotated circumferentially with the origin as the center; (2) For axially distributed interaction defects, the random corrosion defect geometric model Mc needs to be translated axially; (3) For single defects, no rotation or translation is required.

6. A method for predicting residual strength of a submarine pipeline according to claim 5, characterized in that: Step S6 is specifically as follows: Based on the constructed RF-NFEA model, the Monte Carlo simulation method is used to sample and calculate the geometric model of the defective pipeline to obtain the spatial distribution field of the sample residual wall thickness and the residual strength of the pipeline, and the sample space data set is obtained by combining them.

7. A method for predicting residual strength of a submarine pipeline according to claim 6, characterized in that: The RF-NFEA-CNN model is built based on the CNN network, including an input layer, a convolutional layer, a fully connected layer, and an output layer; The input quantity of the input layer is the spatial distribution field of the remaining wall thickness, and the output quantity of the output layer is the predicted remaining strength of the pipeline.

8. A method for predicting residual strength of a submarine pipeline according to claim 1, characterized in that: The RF-NFEA-CNN model training step adopts the gradient descent algorithm, and the specific steps are as follows: S71, inputting the sample residual wall thickness spatial distribution field in the sample space data set into the input layer of the RF-NFEA-CNN model to obtain the predicted output pipeline residual strength of the sample residual wall thickness spatial distribution field; S72, taking the sample residual wall thickness spatial distribution field in the sample space data set corresponding to the pipeline residual strength as the expected output, calculating the error between the expected output and the predicted output pipeline residual strength, transferring the error in reverse layer by layer, and correcting the weight and bias according to the chain rule; S73. Repeat steps S61-S62 until all iteration cycles are completed and the optimal weights and biases are obtained. The model at this time is used as the final RF-NFEA-CNN model.

9. A storage medium, characterized in that: The storage medium stores instructions and data for implementing a method for predicting residual strength of a submarine pipeline as described in any one of claims 1 to 8.

10. A computer device, characterized in that: include: A processor and a storage medium; the processor loads and executes instructions and data in the storage medium to implement a method for predicting residual strength of a submarine pipeline as described in any one of claims 1 to 8.

Citation Information

Patent Citations

  • Method, system and equipment for evaluating bearing performance of rusted steel structure and medium

    CN115034001A

  • Pipeline residual strength evaluation method, device and equipment and readable storage medium

    CN116227273A

  • Method and device for predicting corrosion fracture pressure of oil and gas pipeline

    CN117688725A

  • Method for establishing the geometrical imperfection database for the aerospace thin-walled structure