Treatment reagent for hardening of filter bag of dust remover and preparation method of treatment reagent

Through the treatment reagent composed of sodium hydroxide, softener and adsorbent, the gas phase dissolution removes the hardening of the filter bag of the dust collector, solving the problems of high cost and secondary pollution in the existing technology, and achieving efficient and convenient filter bag cleaning and performance recovery. .

CN118807342APending Publication Date: 2024-10-22XIAMEN SAVINGS ENVIRONMENTAL CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202411189132.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-28
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

The existing technology requires disassembly of the filter bag when dealing with the hardening of the dust collector filter bag, resulting in high labor costs and failure to maintain the original performance, and may cause secondary pollution after cleaning.

Method used

A treatment reagent composed of sodium hydroxide, softener and adsorbent is used to remove the hardened component ammonium sulfate through gas phase dissolution, and purify the exhaust gas through the adsorbent. The softener improves the flexibility and hydrophilicity of the filter bag and avoids disassembly operations.

Benefits of technology

It achieves efficient removal of hardening, reduces operating costs, ensures filter bag performance, avoids secondary pollution, and simplifies operation.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a treatment reagent for hardening of a filter bag of a dust remover and a preparation method of the treatment reagent. The treatment reagent comprises the following components in parts by weight: 8-10 parts of sodium hydroxide; 1-2 parts of a softening agent; 2-3 parts of an adsorbent; 40 to 45 parts of water; the softening agent is a mixture of stearamide methylene pyridine chloride, polyethylene silicon emulsion and water; the adsorbent is one or a mixture of more than two of activated carbon, a zeolite molecular sieve and a carbon molecular sieve. Therefore, according to the prepared treatment reagent for hardening of the filter bag of the dust remover, a main hardened adhesive component ammonium sulfate salt is removed by means of sodium hydroxide gas phase dissolution, ammonia waste gas possibly generated in reaction is adsorbed by an adsorbent technology, and a softening agent is used for helping the filter bag to recover the stiffness of the filter bag. Therefore, the effect of successfully removing the hardening of the filter bag is achieved, the waste gas is effectively collected without causing secondary pollution, the use function of the filter bag is ensured, and the operation is simple.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of bag dust collectors, in particular to a treatment agent for dust collector filter bag compaction and a preparation method thereof. Background Art

[0002] In the process of industrial production exhaust gas emission, the dust is often desulfurized and denitrated before the bag dust removal process. In this process, sulfur trioxide reacts with the escaped ammonia in the flue gas to produce substances such as ammonium bisulfate and ammonium sulfate. This ammonium sulfate salt substance is sticky and insoluble in water. Once it enters the dust collector with the dust, it will adhere to the surface of the dust collector or the filter bag. As the dust accumulates on the filter bag, it continues to gather more dust and form a compaction. The normal blowing pressure cannot shake it off, resulting in an increase in the pressure difference of the dust collector or a serious loss of filtration area.

[0003] Previously, the method to deal with this kind of compaction was very simple and complicated, which required the filter bag to be disassembled and cleaned to remove the compaction. However, this method consumes a huge amount of labor costs, wastes time costs during the disassembly process, and the performance of the cleaned filter bag cannot maintain the original standards.

[0004] In view of this, the present invention provides a treatment agent for the compaction of dust collector filter bags to solve the above-mentioned problems. Summary of the invention

[0005] The purpose of the present invention is to provide a treatment reagent for dust collector filter bag compaction and a preparation method thereof, which can effectively save manpower when cleaning dust compaction on the surface of the filter bag and achieve convenient and efficient effects, while at the same time ensuring the sustainable use of the filter bag to a certain extent without secondary pollution.

[0006] In order to achieve the above object, the solution of the present invention is: A treatment agent for dust collector filter bag compaction, comprising the following components in parts by weight: 8-10 parts of sodium hydroxide; 1-2 parts of softener; 2-3 parts of adsorbent; 40-45 parts of water; The softener is a mixture of stearamide methylene pyridinium chloride, polyvinyl silicon emulsion and water; The adsorbent is one or a mixture of two or more of activated carbon, zeolite molecular sieve and carbon molecular sieve.

[0007] Further, the softener includes the following components in parts by weight: 1-2 parts of stearylamide methylene pyridinium chloride; 1~2 parts of polyethylene silicone emulsion; 10~12 parts water

[0008] The present invention also provides a method for preparing the treatment agent for treating the compaction of filter bags of dust collectors, comprising the following steps: (1) Preparation of a softener: Stearamide methylene pyridinium chloride and water are mixed and stirred at room temperature to completely dissolve in the water to obtain a stearamide methylene pyridinium chloride solution; the stearamide methylene pyridinium chloride solution is then heated in a water bath at a temperature range of 50 to 60° C. and continuously stirred, and a polyethylene silicone emulsion is added to the stearamide methylene pyridinium chloride solution to dissolve and mix, thereby obtaining a softener; (2) Treatment of sodium hydroxide: mixing sodium hydroxide and water and stirring to completely dissolve the sodium hydroxide in the water to obtain a sodium hydroxide solution; (3) Mixing the softener and the sodium hydroxide solution: Add the softener into the sodium hydroxide solution and stir, and add the adsorbent at the same time until the adsorbent is completely soaked in the mixture of the softener and the sodium hydroxide solution; and perform ultrasonic dispersion on the mixture so that the adsorbent is completely dispersed in the mixture, and finally obtain the treatment reagent.

[0009] Furthermore, when preparing the softener, a mixed solution of stearylamide methylene pyridinium chloride and water is stirred at room temperature using a magnetic stirrer at a speed of 400 r / min for 20 to 30 minutes.

[0010] Furthermore, when preparing the softener, a magnetic stirrer is used to stir the mixed solution of the stearylamide methylene pyridinium chloride solution and the polyethylene silicone emulsion at a speed of 600 r / min for 30 to 40 minutes.

[0011] Furthermore, when the sodium hydroxide is treated, a magnetic stirrer is used to stir the mixed solution of sodium hydroxide and water at a speed of 400 r / min for 10 to 15 minutes.

[0012] Furthermore, when the softener and the sodium hydroxide solution are mixed, the softener is added to the sodium hydroxide solution and then stirred at a speed of 600 r / min using a magnetic stirrer for 20 to 30 minutes.

[0013] Furthermore, when the softener and the sodium hydroxide solution are mixed, ultrasonic dispersion is performed at least twice, the frequency of the ultrasonic dispersion is controlled at 450-500 KHz, and each ultrasonic dispersion lasts for 20-30 minutes; after each ultrasonic dispersion, the mixed solution of the softener and the sodium hydroxide solution is taken out, and after the bubbles on the surface are removed, ultrasonic dispersion is performed again.

[0014] Furthermore, the normal temperature is a temperature range of 15 to 30°C.

[0015] After adopting the above technical solution, the treatment reagent has the characteristic of efficiently removing the compacted components. The main component of the treatment reagent is sodium hydroxide, which can remove the main bonding component of the filter bag compaction, ammonium sulfate, by gas phase dissolution. Sodium hydroxide reacts with ammonium sulfate in the gas phase and converts it into a soluble salt, thereby achieving the purpose of removing the compaction. This process can be carried out inside the dust collector, does not involve the replacement of the filter bag, and does not require the removal of the filter bag, which reduces the operating cost.

[0016] Under the action of the treatment reagent, the problem of the dust collector filter bag being hardened has been effectively solved. However, at the same time, ammonia waste gas may be generated during the reaction process, causing environmental pollution. To solve this problem, adsorbent technology is used. The selective adsorption of the adsorbent separates ammonia from other gases to achieve the purpose of purifying the waste gas.

[0017] In addition, during the treatment process, the filter bag may be damaged due to long-term use and hardening, and lose its original stiffness. To restore the performance of the filter bag, softener is added. Softener can improve the flexibility and elasticity of the filter bag, making it have better pressure resistance during dust removal. At the same time, softener can also increase the hydrophilicity of the filter bag, improve its adsorption capacity for water molecules in the gas phase, and further reduce the occurrence of hardening. DETAILED DESCRIPTION

[0018] In order to make the purpose, technical solutions and advantages of the embodiments of the present application clearer, the technical solutions in the embodiments of the present application will be clearly and completely described below in combination with the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments.

[0019] The present invention provides a treatment agent for treating the compaction of a filter bag of a dust collector, comprising the following components in parts by weight: 8-10 parts of sodium hydroxide; 1-2 parts of softener; 2-3 parts of adsorbent; 40-45 parts of water; The softener is a mixture of stearamide methylene pyridinium chloride, polyvinyl silicon emulsion and water; The adsorbent is one or a mixture of two or more of activated carbon, zeolite molecular sieve and carbon molecular sieve.

[0020] The softener comprises the following components by weight: 1~2 parts of stearylamide methylene pyridinium chloride; 1~2 parts of polyethylene silicone emulsion; 10~12 parts of water.

[0021] Thus, the treatment agent has the characteristic of efficiently removing the compacted components. The main component of the treatment agent is sodium hydroxide, which can remove the main adhesive component of the filter bag compaction, ammonium sulfate, by gas phase dissolution. Sodium hydroxide reacts with ammonium sulfate in the gas phase and converts it into a soluble salt, thereby achieving the purpose of removing the compaction. This process can be carried out inside the dust collector without involving the replacement of the filter bag, reducing the operating cost.

[0022] Under the action of the treatment reagent, the problem of the dust collector filter bag being hardened has been effectively solved. However, at the same time, ammonia waste gas may be generated during the reaction process, causing environmental pollution. To solve this problem, adsorbent technology is used. The selective adsorption of the adsorbent separates ammonia from other gases to achieve the purpose of purifying the waste gas.

[0023] In addition, during the treatment process, the filter bag may be damaged due to long-term use and hardening, and lose its original stiffness. To restore the performance of the filter bag, softener is added. Softener can improve the flexibility and elasticity of the filter bag, making it have better pressure resistance during dust removal. At the same time, softener can also increase the hydrophilicity of the filter bag, improve its adsorption capacity for water molecules in the gas phase, and further reduce the occurrence of hardening.

[0024] This embodiment provides a method for preparing a treatment agent for treating the compaction of a dust collector filter bag, so as to prepare the above-mentioned treatment agent. The preparation method may specifically include the following steps: Preparation of softener: Add 2 parts of stearamide methylene pyridine chloride into a beaker containing 10 parts of water, stir it at a speed of 400 r / min for 20-30 minutes at room temperature of about 25°C with a magnetic stirrer to completely dissolve it, and obtain a stearamide methylene pyridine chloride solution; adjust the temperature of the water bath to 50-60°C, then put the stearamide methylene pyridine chloride solution into a water bath for water bath heating, and stir it at a speed of 600 r / min with a magnetic stirrer, and gradually add 1 part of polyethylene silicone emulsion to it to dissolve and mix it, and stir for 30-40 minutes to obtain a softener. (2) Treatment with sodium hydroxide: Place 8 parts of sodium hydroxide in a beaker containing 45 parts of water, and stir it at a speed of 400 r / min for 10-15 minutes at room temperature with a magnetic stirrer to obtain a sodium hydroxide solution; (3) Mixing of softener and sodium hydroxide solution: Add 1 part of softener into 48-55 parts of sodium hydroxide solution and stir, and use a magnetic stirrer to stir at a speed of 600 r / min for 20-30 minutes. At the same time, gradually add 2 parts of adsorbent until the adsorbent is completely soaked in the mixture of softener and sodium hydroxide solution; and perform ultrasonic dispersion on the mixture so that the adsorbent is completely dispersed in the mixture, and finally obtain the treatment reagent.

[0025] Specifically, the frequency of ultrasonic dispersion is controlled at 450-500 KHz. After 20-30 minutes of action, the mixed solution of softener and sodium hydroxide solution is taken out and the bubbles on the surface are removed before ultrasonic dispersion again. This is repeated two to three times to completely disperse the adsorbent in the reagent.

[0026] When using the above-mentioned treatment reagents to clean the dust collector filter bags, the following methods can be used: The configured treatment reagent is loaded into the vaporization device, which is used to vaporize the treatment reagent and send it into the dust collector, so that the treatment reagent can be evenly attached to the surface of the filter bag in a splashing manner to ensure that the treatment reagent can fully contact the filter bag.

[0027] After the treatment agent is sprayed, the filter bag needs to be left to stand for 30 minutes to allow the treatment agent to fully react with the surface of the filter bag. This period of time is enough for the agent to form a uniform film on the surface of the filter bag, preparing for the subsequent cleaning steps.

[0028] Next, use the original spray system of the dust collector to vibrate and clean the filter bags with compressed air, which can ensure the cleaning effect while avoiding damage to the filter bags.

[0029] After the first cleaning is completed, the treatment reagent is sprayed again.

[0030] This process needs to be repeated 3 to 5 times until all the hardening on the surface of the filter bag is dissolved and falls off.

[0031] In summary, the present invention can effectively treat the dust compaction on the surface of the filter bag without disassembling the filter bag by atomizing and spraying the treatment reagent. The prepared treatment reagent for the compaction of the filter bag of the dust collector relies on sodium hydroxide gas phase dissolution to remove the main bonding component ammonium sulfate salt of the compaction, uses adsorbent technology to adsorb the ammonia waste gas that may be generated in the reaction, and uses a softener to help the filter bag restore its own stiffness. Thereby achieving the effect of successfully removing the compaction of the filter bag, and effectively collecting the waste gas without causing secondary pollution, ensuring the use function of the filter bag, and simple operation.

[0032] The above is only a preferred embodiment of the present invention. The protection scope of the present invention is not limited to the above embodiments. All technical solutions under the concept of the present invention belong to the protection scope of the present invention. It should be pointed out that for ordinary technicians in this technical field, equivalent changes and modifications without departing from the principle of the present invention should still belong to the protection scope of the present invention. In addition, this application provides examples of various specific processes and materials, but ordinary technicians in this field can be aware of the application of other processes and / or the use of other materials.

Claims

1. A treatment agent for dust collector filter bag compaction, characterized in that: The composition comprises the following components by weight: 8-10 parts of sodium hydroxide; 1-2 parts of softener; 2-3 parts of adsorbent; 40-45 parts of water; The softener is a mixture of stearamide methylene pyridinium chloride, polyvinyl silicon emulsion and water; The adsorbent is one or a mixture of two or more of activated carbon, zeolite molecular sieve and carbon molecular sieve.

2. The reagent for treating the compaction of filter bags of dust collectors according to claim 1, characterized in that: The softener comprises the following components by weight: 1-2 parts of stearylamide methylene pyridinium chloride; 1~2 parts of polyethylene silicone emulsion; 10~12 parts water 3. A method for preparing a treatment agent for treating dust collector filter bag compaction as claimed in claim 1, characterized in that: The following steps are involved: (1) Preparation of a softener: Stearamide methylene pyridinium chloride and water are mixed and stirred at room temperature to completely dissolve in the water to obtain a stearamide methylene pyridinium chloride solution; the stearamide methylene pyridinium chloride solution is then heated in a water bath at a temperature range of 50 to 60° C. and continuously stirred, and a polyethylene silicone emulsion is added to the stearamide methylene pyridinium chloride solution to dissolve and mix, thereby obtaining a softener; (2) Treatment of sodium hydroxide: mixing sodium hydroxide and water and stirring to completely dissolve the sodium hydroxide in the water to obtain a sodium hydroxide solution; (3) Mixing the softener and the sodium hydroxide solution: Add the softener into the sodium hydroxide solution and stir, and add the adsorbent at the same time until the adsorbent is completely soaked in the mixture of the softener and the sodium hydroxide solution; and perform ultrasonic dispersion on the mixture so that the adsorbent is completely dispersed in the mixture, and finally obtain the treatment reagent.

4. The preparation method according to claim 3, characterized in that: When preparing the softener, a mixed solution of stearylamide methylene pyridinium chloride and water is stirred at a speed of 400 r / min using a magnetic stirrer at room temperature for 20 to 30 minutes.

5. The preparation method according to claim 3 or 4, characterized in that: When preparing the softener, a mixed solution of stearylamide methylene pyridinium chloride solution and polyethylene silicone emulsion is stirred at a speed of 600 r / min by a magnetic stirrer for 30 to 40 minutes.

6. The preparation method according to claim 3, characterized in that: When the sodium hydroxide is treated, a magnetic stirrer is used to stir the mixed solution of sodium hydroxide and water at a speed of 400 r / min for 10 to 15 minutes.

7. The preparation method according to claim 3, characterized in that: When the softener and the sodium hydroxide solution are mixed, the softener is added to the sodium hydroxide solution and then stirred at a speed of 600 r / min using a magnetic stirrer for 20 to 30 minutes.

8. The preparation method according to claim 3, characterized in that: When the softener and the sodium hydroxide solution are mixed, ultrasonic dispersion is performed at least twice, the frequency of the ultrasonic dispersion is controlled at 450-500 KHz, and each ultrasonic dispersion lasts for 20-30 minutes; after each ultrasonic dispersion, the mixed solution of the softener and the sodium hydroxide solution is taken out, and ultrasonic dispersion is performed again after the bubbles on the surface are removed.

9. The preparation method according to claim 3, characterized in that: The normal temperature is a temperature range of 15 to 30°C.

Citation Information

Patent Citations

  • Removal of ammonia in urea finishing

    CN102753518A

  • Leading protection device in dust remover bag district

    CN207025033U