Activation method of fuel cell and activated fuel cell
Through the collaborative approach of electrode wetting, extreme current testing and rapid current surge, the problem of long time-consuming and harsh conditions for fuel cell activation is solved, fast, safe and efficient activation of fuel cells is achieved, and the electrocatalyst utilization rate and activity are significantly improved. , suitable for activation of single cells and battery stacks.
Patent Information
- Application Number
- CN202411150435.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-21
- Publication Date
- 2024-10-25
AI Technical Summary
Existing fuel cell activation methods are time-consuming or require harsh conditions, resulting in high costs, reduced production efficiency, and may have a negative impact on battery durability, and can easily cause safety issues such as local hot spots.
Using a method of coordinated electrode wetting, limit current testing and rapid current impact, the floating dust on the catalytic layer is blown away through electrode wetting. Under the limit current test, the voltage gradually decreases to broaden the reaction area. Under constant voltage current impact, heat is rapidly released to realize the electrode Structural change and catalyst activity improvement, suitable for activation of single cells and battery stacks.
It achieves fast, safe and efficient activation of fuel cells, significantly improves electrocatalyst utilization and activity, simplifies the activation process, is suitable for a wide range of membrane electrode activation and performance recovery, and can monitor the degree of activation in real time to avoid problems due to the passage of time. Insufficient activation or excessive fuel consumption caused by being too long or too short.
Smart Images

Figure CN118841597A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of fuel cells and relates to a fuel cell activation method and an activated fuel cell. Background Art
[0002] Proton exchange membrane fuel cells can convert chemical energy stored in hydrogen into electrical energy. They also have a series of advantages such as low noise, zero pollution, and high efficiency. They have attracted widespread attention and research in recent years. However, problems in cost and durability still prevent the further commercialization of fuel cells. Due to impurity contamination during the production process and other reasons, the performance of newly produced fuel cells is usually poor and cannot meet the requirements of use. Therefore, they must undergo an activation process before formal use. The fuel cell activation process includes: 1) PEM humidification process, which increases proton conductivity and reduces ohmic internal resistance; 2) The process of establishing electron, proton, gas and water transmission channels; 3) The process of optimizing the electrode structure, and some changes in the microstructure occur. Therefore, the activation process is not only a humidification process of the proton exchange membrane, but also a complex process with multiple effects and influences. During the activation process, microscopic changes and structures that are conducive to improving the utilization rate and activity of the electrocatalyst are established.
[0003] Currently commonly used activation methods are usually time-consuming or have harsh activation conditions, which not only increase costs and reduce production efficiency, but also easily have a negative impact on the durability of fuel cells.
[0004] CN117594834A discloses a fuel cell activation method and activation device, which provides an interactive hydrogen pump activation method. First, gas is introduced into the anode and cathode of the fuel cell to be activated, and the gas introduced into at least one side of the electrode contains hydrogen. Current excitation is applied to start forward or reverse hydrogen pump activation, and the current excitation is stopped after a duration of t1; when the normal working state is restored, the gas supply state of the anode and cathode of the fuel cell to be activated is restored, and the performance test is performed; when the activation time is reached or it is judged that the activation termination condition is reached, the activation is completed. Although the interactive hydrogen pump activation method shortens the activation time of the fuel cell to a certain extent (40 minutes), in the interactive hydrogen pump method, hydrogen passes through both the anode and cathode, and the hydrogen adheres to the surface of the catalyst layer and cannot be completely discharged. When the normal working state is restored, hydrogen and oxygen exist at the cathode at the same time and react directly, thereby generating local hot spots and damaging the battery. If hydrogen and oxygen reach a certain concentration, safety issues will arise.
[0005] CN114447376A relates to a rapid activation method for a fuel cell stack, which comprises the following steps: (1) pulling the current density of the electronic load to a first current density and running it at a constant current for a period of time; (2) selecting a number of current densities, and pulling the current density of the electronic load from low to high to the selected current density in sequence, and causing the cathode of the stack to discharge in anoxic state at each current density; (3) pulling the current density of the electronic load to a second current density and running it at a constant current for a period of time; (4) observing whether the voltage of the stack is stable, and if the voltage is unstable, repeating steps (2) and (3) until the voltage is stable, that is, the stack activation is completed. Although this method has the advantages of high activation efficiency, can shorten the activation time to less than 1 hour, and low hydrogen consumption, it is easy to have a situation where a high concentration of hydrogen and oxygen exist at the cathode at the same time, thereby generating local hot spots and damaging the battery.
[0006] Therefore, how to achieve rapid activation of fuel cells with excellent activation effect is a technical problem that needs to be solved urgently. Summary of the invention
[0007] In view of the shortcomings of the prior art, the purpose of the present invention is to provide a method for activating a fuel cell and an activated fuel cell. The activation method provided by the present invention is applicable to both single cell structures and fuel cell stacks, covering all membrane electrode activation and performance recovery in fuel cells, and has a wide range of applications; the activation process is simple and convenient, the activation process can be completed in a short time, and the activation effect is significant; at the same time, program control can be realized, one-button operation, convenient and efficient.
[0008] In order to achieve the purpose of the invention, the present invention adopts the following technical solutions:
[0009] In a first aspect, the present invention provides a method for activating a fuel cell, the activation method comprising the following steps:
[0010] (1) Electrode wetting: Wetting the electrodes of the fuel cell to be activated;
[0011] (2) Limiting current value test: After the electrodes are wetted, a first mixed gas containing oxygen is introduced into the cathode of the fuel cell to be activated, and hydrogen is introduced into the anode. Then, the voltage is gradually reduced from the open circuit voltage until the limiting current value appears.
[0012] (3) After step (2), a constant voltage current shock is performed;
[0013] Repeat steps (2)-(3) until the activation completion conditions are met and the activation is completed.
[0014] The activation method provided by the present invention cooperates with electrode wetting, limiting current test and rapid current impact. The electrode wetting process can blow away the dust on the surface of the catalyst layer and the gas diffusion layer, and at the same time, the battery reaches a preliminary wetting state; the limiting current test can not only make the cathode produce reducing conditions to reduce the oxidized substances that affect the cathode performance, but also widen the active area of the actual reaction as much as possible, increase the effective area of the reaction, and at the same time, the limiting current is obtained in the form of gradually reducing the voltage. Compared with the traditional current setting, the safety factor is high and the occurrence of reverse polarity hazards is effectively prevented; further, under the constant voltage current impact, heat is quickly released, so that the battery temperature quickly increases to The set value can be set and further activated; the degree of activation can be monitored in real time to make the process controllable, and the battery will not be fully activated due to a short activation time, nor will the fuel be consumed too much due to a long activation time; thereby changing the electrode structure, which is beneficial to the microscopic changes and structures that improve the utilization rate and activity of the electrocatalyst; at the same time, the activation method provided by the present invention is suitable for both single-cell structures and fuel cell stack activation, covering all membrane electrode activation and performance recovery in fuel cells, and has a wide range of applications; and the activation process is simple and convenient, the activation process can be completed in a short time, and the activation effect is significant; at the same time, program control and one-key operation can be realized, which is convenient and efficient.
[0015] In the present invention, electrode wetting, limiting current test and rapid current impact cooperate with each other and are indispensable. Without any one of the activation conditions, the activation effect in the present application cannot be achieved and the activation time cannot be reduced. At the same time, if the limiting current is not obtained by reducing the voltage, reverse polarity hazards are likely to occur.
[0016] The following are preferred technical solutions of the present invention, but are not intended to limit the technical solutions provided by the present invention. Through the following preferred technical solutions, the technical objectives and beneficial effects of the present invention can be better achieved and realized.
[0017] Preferably, the electrode wetting method comprises: independently purging the cathode and the anode of the fuel cell to be activated with wet nitrogen gas.
[0018] In the present invention, the humidity of the wet nitrogen is selected as a conventional technical solution. For example, saturated wet nitrogen can be selected for purging and wetting. By purging with wet nitrogen, a large amount of air can quickly open the gas and water transmission channels of the battery, blow away the floating dust on the surface of the catalyst layer and the gas diffusion layer, and at the same time make the battery reach an initial wetting state.
[0019] Preferably, the gas volume of the wet nitrogen is ≥2A / cm 2 , for example 2A / cm 2 , 2.5A / cm 2 、3A / cm 2 、3.5A / cm 2 , 4A / cm2 , 4.5A / cm 2 or 5A / cm 2 The above range is not limited to the listed values, and other values not listed within the above range are also applicable.
[0020] Preferably, the wet nitrogen purge time is 30 to 60 seconds, for example, 30 seconds, 35 seconds, 40 seconds, 45 seconds, 50 seconds, 55 seconds or 60 seconds, but is not limited to the listed values, and other values not listed within the numerical range are also applicable.
[0021] Preferably, the concentration of oxygen in the first mixed gas introduced is 0.5% to 3%, for example 0.5%, 0.8%, 1%, 1.3%, 1.5%, 1.8%, 2%, 2.3%, 2.5%, 2.8% or 3%, etc., but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0022] It should be noted that the source of oxygen in the first mixed gas of the present invention can be pure oxygen or air, and can be mixed with a conventional protective gas, such as a mixed gas of nitrogen and oxygen, a mixed gas of nitrogen and air, etc.; and when introduced, the addition ratio of each gas can be adjusted by adjusting the switch valve to achieve the adjustment of oxygen concentration.
[0023] Preferably, the process of gradually reducing the voltage from the open circuit voltage includes: each voltage reduction amplitude is performed at a first gradient value until the current value starts to decrease, and each voltage reduction amplitude is performed at a second gradient value.
[0024] It should be noted that the voltage reduction amplitude in the present invention is realized in an arithmetic decreasing pattern, that is, a regular decreasing pattern, which can better obtain the limiting current density value, while ensuring that the activation process is safe and controllable, and the activation effect is steadily improved.
[0025] Preferably, the first gradient value is 0.1-0.2 V / time, for example, 0.1 V / time, 0.11 V / time, 0.12 V / time, 0.13 V / time, 0.14 V / time, 0.15 V / time, 0.16 V / time, 0.17 V / time, 0.18 V / time, 0.19 V / time or 0.2 V / time, etc., but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0026] Preferably, the second gradient value is 0.02-0.05 V / time, such as 0.02 V / time, 0.03 V / time, 0.04 V / time or 0.05 V / time, but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0027] In the present invention, the first gradient value is greater than the second gradient value, that is, during the voltage reduction process, after the current is reduced, the voltage reduction amplitude is also reduced, so that the process is steadily advanced, and the occurrence of problems such as emergency stop of the test bench caused by excessive current reduction is prevented, which is more conducive to obtaining the limiting current density value.
[0028] Preferably, the judgment criterion of the limiting current value is: the current value does not change within 5 seconds under constant voltage, and the residence time when reaching the limiting current value is not less than 2 seconds, such as 2s, 3s, 4s, 5s or 6s, etc., but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0029] Preferably, in the process of repeating steps (2)-(3), step (2) is first subjected to at least one self-repeating process.
[0030] In the present invention, the self-repeating process obtains at least two limiting current values (the number of repetitions is the number of times the limiting current value is obtained), each time starting from the open circuit voltage and gradually decreasing, and the voltage reduction pattern is the same as the previous time, but the specific reduction range can be adjusted within a limited numerical range; and in the present invention, the test time of a limiting current value is 10 to 30 seconds (for example, 10 seconds, 15 seconds, 20 seconds, 25 seconds or 30 seconds, etc.), and the test process of a limiting current value can be completed in a short time.
[0031] Preferably, in the self-repeating process of step (2), the concentration of oxygen in the first mixed gas introduced into the cathode in the previous time is higher than the concentration of oxygen in the first mixed gas introduced into the cathode in the next time.
[0032] In the present invention, during the self-repeating process of step (2), the concentration of oxygen at the cathode end is reduced each time the cathode is repeated, which can better promote the cathode to continuously produce higher reducing conditions and reduce the oxidized substances that affect the cathode performance.
[0033] Preferably, the number of times the self-repeating process of step (2) is performed is 2 to 5 times, for example, 2 times, 3 times, 4 times or 5 times, but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0034] In the present invention, if the number of self-repeating processes in step (2) is too small, the oxidized substances on the cathode side cannot be fully reduced, while if the number of self-repeating processes is too large, the time will be prolonged and the cost will be increased.
[0035] Preferably, the step (3) comprises:
[0036] After step (2) is completed, air is introduced into the cathode, the hydrogen in the anode remains unchanged, and a constant voltage current shock is performed.
[0037] Preferably, during the constant voltage current impact process, the stoichiometric ratio of the gas introduced into the cathode is 2.0-3.0, for example, 2, 2.1, 2.2, 2.3, 2.4, 2.5, 2.6, 2.7, 2.8, 2.9 or 3, and the stoichiometric ratio of the gas introduced into the anode is 1.5-2.0, for example, 1.5, 1.6, 1.7, 1.8, 1.9 or 2, but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0038] Preferably, the constant voltage value is 0.3-0.5V, such as 0.3V, 0.4V or 0.5V, etc., but is not limited to the listed values, and other values not listed within the range are also applicable.
[0039] In the present invention, current shock is performed at a constant voltage value of 0.3 to 0.5 V, which can better improve the activation efficiency.
[0040] Preferably, the constant voltage current shock time is 1 to 4 minutes, such as 1 minute, 2 minutes, 3 minutes or 4 minutes, but is not limited to the listed values, and other values not listed within the numerical range are also applicable.
[0041] It should be noted that the duration of the constant voltage current impulse in the present invention can be adaptively adjusted according to the voltage value; for example, 0.3V is maintained for 1 to 2 minutes, 0.4V is maintained for 2 to 3 minutes, 0.5V is maintained for 3 to 4 minutes, etc.
[0042] Preferably, the number of repetitions of steps (2)-(3) is ≥ 2 times, such as 2 times, 3 times, 4 times or 5 times, but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0043] Preferably, the standard of the activation completion condition includes: the current deviation between the constant voltage current shock in the previous round of step (3) and the constant voltage current shock in the next round of step (3) is less than 1A, for example 0.1A, 0.2A, 0.3A, 0.4A, 0.5A, 0.6A, 0.7A, 0.8A, 0.9A or 1A, then the activation is completed, but it is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0044] In the present invention, if the current deviation of the constant voltage current shock is ≥1A, the process returns to step (2) and the limiting current value test is continued. If the current deviation is too large, exceeding 1A, activation is stopped, which may result in insufficient activation and unsatisfactory effects.
[0045] Preferably, the standard of the activation completion condition includes: the current value remains consistent for at least 20 seconds after the constant voltage current shock in step (3), and the activation is completed.
[0046] It should be noted that the standard of the activity completion condition in the present invention only requires satisfying one of the above-mentioned current deviation and current holding time, and does not require satisfying both conditions.
[0047] As a preferred technical solution, the activation method comprises the following steps:
[0048] (1) Electrode wetting: The cathode and anode of the fuel cell to be activated are independently subjected to gas flow ≥ 2A / cm 2 Purge with wet nitrogen for 30 to 60 seconds;
[0049] (2) Limiting current value test: After the electrodes are wetted, a first mixed gas with an oxygen concentration of 0.5% to 3% is introduced into the cathode of the fuel cell to be activated, and hydrogen is introduced into the anode. The voltage is reduced at a first gradient value of 0.1 to 0.2 V / time until the current value begins to decrease. The voltage is reduced at a second gradient value of 0.02 to 0.05 V / time until the current value does not change within 5 seconds under constant voltage, and the dwell time when the limiting current value is reached is not less than 2 seconds, thereby obtaining the limiting current value;
[0050] Step (2) is repeated 2 to 5 times, during which the concentration of oxygen in the first mixed gas introduced into the cathode in the previous process is higher than the concentration of oxygen in the first mixed gas introduced into the cathode in the next process; (3) after step (2) is completed, air is introduced into the cathode, the hydrogen in the anode remains unchanged, the stoichiometric ratio of the gas introduced into the cathode is 2.0 to 3.0, and the stoichiometric ratio of the gas introduced into the anode is 1.5 to 2.0, and a constant voltage current shock of 0.3 to 0.5 V is performed for 1 to 4 minutes;
[0051] Repeat steps (2)-(3) at least twice until the activation is complete;
[0052] The standard of the activation completion condition includes: the current deviation between the constant voltage current impact in the previous round of step (3) and the constant voltage current impact in the next round of step (3) is less than 1A, then the activation is completed;
[0053] or,
[0054] The standard of the activation completion condition includes: the current value remains the same for at least 20 seconds after the constant voltage current shock in step (3), and the activation is completed;
[0055] After activation is completed, activation ends.
[0056] It should be noted that the activation environment in the present invention can be adaptively selected and adjusted according to the properties of the fuel cell membrane electrode, that is, the temperature, pressure, humidity, etc., do not affect the normal activation process of the battery;
[0057] Furthermore, the present invention does not limit the specific type of fuel cell, and is applicable to both a single fuel cell structure and a fuel cell stack structure.
[0058] In a second aspect, the present invention further provides an activated fuel cell, wherein the activated fuel cell is obtained by activation by the activation method described in the first aspect.
[0059] Compared with the prior art, the present invention has the following beneficial effects:
[0060] The activation method provided by the present invention cooperates with electrode wetting, limiting current test and rapid current impact. The electrode wetting process can blow away the dust on the surface of the catalyst layer and the gas diffusion layer, and at the same time, the battery reaches a preliminary wetting state; the limiting current test can not only make the cathode produce reducing conditions to reduce the oxidized substances that affect the cathode performance, but also widen the active area of the actual reaction as much as possible, increase the effective area of the reaction, and at the same time, the limiting current is obtained in the form of gradually reducing the voltage. Compared with the traditional current setting, the safety factor is high and the occurrence of reverse polarity hazards is effectively prevented; further, under the constant voltage current impact, heat is quickly released, so that the battery temperature quickly increases to The set value can be set and further activated; the degree of activation can be monitored in real time to make the process controllable, and the battery will not be fully activated due to a short activation time, nor will the fuel be consumed too much due to a long activation time; thereby changing the electrode structure, which is beneficial to the microscopic changes and structures that improve the utilization rate and activity of the electrocatalyst; at the same time, the activation method provided by the present invention is suitable for both single-cell structures and fuel cell stack activation, covering all membrane electrode activation and performance recovery in fuel cells, and has a wide range of applications; and the activation process is simple and convenient, the activation process can be completed in a short time, and the activation effect is significant; at the same time, program control and one-key operation can be realized, which is convenient and efficient. BRIEF DESCRIPTION OF THE DRAWINGS
[0061] Figure 1 This is a curve diagram of the current value change during the constant voltage current impact process in the activation method provided in Example 1.
[0062] Figure 2 This is a comparison chart of the performance curves of the fuel cell activated by the activation methods provided in Example 1 and Comparative Example 1. DETAILED DESCRIPTION
[0063] The technical solution of the present invention is further described below by specific implementation methods. It should be understood by those skilled in the art that the embodiments are only to help understand the present invention and should not be regarded as specific limitations of the present invention.
[0064] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by technicians in the technical field to which this application belongs; the terms used herein are only for the purpose of describing specific embodiments and are not intended to limit this application; the terms "including" and "having" and any variations thereof in this application are intended to cover non-exclusive inclusions.
[0065] In the description of this application, the technical terms "first", "second", etc. are only used to distinguish different objects, and cannot be understood as indicating or implying relative importance or implicitly indicating the number, specific order or primary and secondary relationship of the indicated technical features. In the description of this application, the meaning of "plurality" is more than two, unless otherwise clearly and specifically defined.
[0066] In a specific embodiment, the present invention provides a single cell structure of a proton exchange membrane fuel cell to be activated, wherein the single cell structure as a single cell basic unit includes: a single-section membrane electrode and single-pole plates on both sides of the anode and cathode.
[0067] Furthermore, a proton exchange membrane fuel cell stack structure to be activated is also provided, wherein the fuel cell stack structure comprises membrane electrodes and bipolar plates alternately stacked, that is, a plurality of single cells are stacked in series.
[0068] The samples to be activated in the following examples and comparative examples all adopt the above-mentioned single cell structure or cell stack structure.
[0069] Example 1
[0070] This embodiment provides a method for activating a fuel cell, and the activation method is as follows:
[0071] (1) The activated single cell is installed on the performance test bench and the air tightness test is qualified;
[0072] (2) Electrode wetting: The positive and negative electrodes are respectively 2A / cm2 for the battery 2 Saturated wet nitrogen is introduced into the required amount of gas for 30 seconds to achieve the wetting process of the cathode and anode;
[0073] (3) Limiting current value test (the self-repeating process is repeated twice, that is, two limiting current values are obtained):
[0074] Set the required condition parameters; when the temperature reaches 40℃, switch the gas, hydrogen is introduced into the anode, and a mixture of nitrogen and air is introduced into the cathode (the concentration of oxygen in the mixture is 3%), and the voltage is reduced from the open circuit voltage according to the same gradient each time (the first gradient value is: 0.2V / each time). When the current decreases with the voltage change trend (that is, the current value begins to decrease), gradually reduce the voltage drop gradient (the second gradient value is 0.05V / each time), the current does not change within 5s under constant voltage, reaches the first limit current value, and the residence time is about 5s (that is, the limit current value standard is reached);
[0075] Then hydrogen is still introduced into the anode, and a mixture of nitrogen and air (the concentration of oxygen in the mixture is 0.5%) is introduced into the cathode. The voltage is reduced at the same gradient each time (the first gradient value is 0.1V / each time). When the current decreases with the voltage change trend, the voltage drop gradient is gradually reduced (the second gradient value is 0.02V / each time). Under constant voltage, the current does not change within 5s and reaches the second limiting current value. The residence time is about 5s.
[0076] (4) The anode gas remains unchanged, the cathode gas is switched to air, the stoichiometric ratio of the gas introduced is 1.5 for the anode and 2.5 for the cathode, and the current shock is performed at a constant voltage of 0.4 V for 2 to 3 minutes;
[0077] Figure 1 It shows that the current value change curve of the constant voltage current impact process in the activation method provided in Example 1 is from Figure 1 It can be seen that by repeating steps (3)-(4) and recording the current change during each rapid current shock, after three repetitions, the final current deviation between the current value after the second activation treatment of (3)-(4) and the current value after the third activation treatment of (3)-(4) is less than 1A, indicating that the activation is complete.
[0078] Example 2
[0079] This embodiment provides a method for activating a fuel cell, and the activation method is as follows:
[0080] (1) The activated single cell is installed on the performance test bench and the air tightness test is qualified;
[0081] (2) Electrode wetting: The positive and negative electrodes are respectively 2.5A / cm 2 Saturated wet nitrogen gas is introduced into the required amount of gas for 40 seconds to achieve the wetting process of the cathode and anode;
[0082] (3) Limiting current value test (the self-repeating process is repeated 3 times, that is, three limiting current values are obtained):
[0083] Set the required condition parameters; when the temperature reaches 40°C, switch the gas, hydrogen is introduced into the anode, and a mixture of nitrogen and air (the concentration of oxygen in the mixture is 5%) is introduced into the cathode, and the voltage is reduced from the open circuit voltage according to the same gradient each time (the first gradient value is: 0.2V / each time), when the current decreases with the voltage change trend (that is, the current value begins to decrease), gradually reduce the voltage drop gradient (the second gradient value is 0.05V / each time), the current does not change within 5s under constant voltage, reaches the first limit current value, and the residence time is about 5s (that is, the standard of the limit current value is reached);
[0084] Then hydrogen is still introduced into the anode, and a mixture of nitrogen and air (the concentration of oxygen in the mixture is 3%) is introduced into the cathode. The voltage is reduced at the same gradient each time (the first gradient value is 0.15V / each time). When the current decreases with the voltage change trend, the voltage drop gradient is gradually reduced (the second gradient value is 0.04V / each time). Under constant voltage, the current does not change within 5s and reaches the second limiting current value. The residence time is about 5s.
[0085] Then hydrogen is still introduced into the anode, and a mixture of nitrogen and air (the concentration of oxygen in the mixture is 1%) is introduced into the cathode. The voltage is reduced at the same gradient each time (the first gradient value is 0.1V / each time). When the current decreases with the voltage change trend, the voltage drop gradient is gradually reduced (the second gradient value is 0.02V / each time). Under constant voltage, the current does not change within 5s and reaches the third limiting current value. The residence time is about 5s.
[0086] (4) The anode gas remains unchanged, the cathode gas is switched to air, the stoichiometric ratio of the gas introduced is 2.0 for the anode and 3.0 for the cathode, and the current shock is performed at a constant voltage of 0.3 V for 1 to 2 minutes;
[0087] Repeat steps (3)-(4), record the current change during each rapid current shock, and after repeating twice, the final current deviation between the current value after the first activation treatment of (3)-(4) and the current value after the second activation treatment of (3)-(4) is less than 1A, and the activation is completed.
[0088] Example 3
[0089] This embodiment provides a method for activating a fuel cell, and the activation method is as follows:
[0090] (1) The activated single cell is installed on the performance test bench and the air tightness test is qualified;
[0091] (2) Electrode wetting: The positive and negative electrodes are respectively 3A / cm2 for the battery 2 Saturated wet nitrogen is introduced into the required amount of gas for 30 seconds to achieve the wetting process of the cathode and anode;
[0092] (3) Limiting current value test (the self-repeating process is repeated twice, that is, two limiting current values are obtained):
[0093] Set the required condition parameters; when the temperature reaches 40°C, switch the gas, hydrogen is introduced into the anode, and a mixture of nitrogen and air is introduced into the cathode (the concentration of oxygen in the mixture is 2%), and the voltage is reduced from the open circuit voltage according to the same gradient each time (the first gradient value is: 0.2V / each time). When the current decreases with the voltage change trend (that is, the current value begins to decrease), gradually reduce the voltage drop gradient (the second gradient value is 0.05V / each time), the current does not change within 5s under constant voltage, reaches the first limit current value, and the residence time is about 5s (that is, the limit current value standard is reached);
[0094] Then hydrogen is still introduced into the anode, and a mixture of nitrogen and air (the concentration of oxygen in the mixture is 1%) is introduced into the cathode. The voltage is reduced at the same gradient each time (the first gradient value is 0.1V / each time). When the current decreases with the voltage change trend, the voltage drop gradient is gradually reduced (the second gradient value is 0.02V / each time). Under constant voltage, the current does not change within 5s and reaches the second limiting current value. The residence time is about 5s.
[0095] (4) The anode gas remains unchanged, the cathode gas is switched to air, the stoichiometric ratio of the gas introduced is 2.0 for the anode and 3.0 for the cathode, and the current shock is performed at a constant voltage of 0.35 V for 2 to 3 minutes;
[0096] Repeat steps (3)-(4), record the current change during each rapid current shock, and after three repetitions, i.e. the third step (4), the current remains unchanged after 30 seconds under a constant voltage of 0.35 V, indicating that activation is complete.
[0097] Example 4
[0098] The difference between this embodiment and embodiment 1 is that in step (3) of this embodiment, only one limiting current value test process is performed, that is, the required condition parameters are set; when the temperature reaches 40°C, the gas is switched, hydrogen is introduced into the anode, and a mixture of nitrogen and air (the concentration of oxygen in the mixture is 3%) is introduced into the cathode, and the voltage is reduced from the open circuit voltage according to the same gradient each time (the first gradient value is: 0.2V / each time), when the current decreases with the voltage change trend (that is, the current value begins to decrease), the voltage drop gradient is gradually reduced (the second gradient value is 0.05V / each time), and the current does not change within 5s under constant voltage, reaching the first limiting current value, and the residence time is about 5s (that is, the standard of the limiting current value is reached);
[0099] Then proceed directly to step (3).
[0100] The remaining activation steps and parameters were the same as in Example 1.
[0101] Example 5
[0102] The difference between this embodiment and embodiment 1 is that in step (3) of this embodiment:
[0103] During the test of the first limiting current value, the voltage is reduced from the open circuit voltage each time according to the same first gradient value of 0.2V until the first limiting current value is obtained, that is, when the current decreases with the voltage change trend, the voltage reduction amplitude is still carried out at the first gradient value;
[0104] During the test of the second limiting current value, when the current decreases with the voltage variation trend, the voltage reduction amplitude is still performed at the first gradient value of 0.1 V / time.
[0105] The remaining activation steps and parameters were the same as in Example 1.
[0106] Example 6
[0107] The difference between this embodiment and embodiment 1 is that in this embodiment, during the test process of the second limiting current value in step (3), the concentration of oxygen in the mixed gas of nitrogen and air introduced into the cathode is still 3%.
[0108] The remaining activation steps and parameters were the same as in Example 1.
[0109] Example 7
[0110] The difference between this embodiment and embodiment 1 is that in step (4) of this embodiment, the pressure value of the constant pressure is 0.9V.
[0111] The remaining activation steps and parameters were the same as in Example 1.
[0112] Comparative Example 1
[0113] The difference between this comparative example and Example 1 is that this comparative example adopts a constant voltage activation method for activation treatment, and the specific process is as follows:
[0114] (1) The activated single cell is installed on the performance test bench and the air tightness test is qualified;
[0115] (2) Electrode wetting: Saturated wet nitrogen gas is passed into the cathode and anode respectively at the required gas volume of 2A / cm2 of the battery for 30 seconds to achieve the wetting process of the cathode and anode;
[0116] (3) Set the required condition parameters; the anode and cathode humidification temperature is 75°C, the gas pipeline is 75°C, and the battery temperature is 75°C. After the temperature reaches the set temperature, the N2 at the anode and cathode is switched to hydrogen and air, with the gas stoichiometric ratios of 1.5 and 2.5 respectively, and the anode and cathode back pressure is set to 100 kPa;
[0117] (4) The activation was completed after 8 h of constant voltage activation at 0.4 V.
[0118] Comparative Example 2
[0119] The difference between this comparative example and Example 1 is that in step (2) of this comparative example, the limiting current value is obtained by a method other than reducing the voltage, specifically:
[0120] Step (3) was changed to the following method to measure the limiting current: the anode and cathode humidification temperature was 75°C, the gas pipeline was 75°C, and the battery temperature was 75°C. After the temperature reached the set temperature, the N2 at the anode and cathode was switched to hydrogen and air, with the gas stoichiometric ratios of 1.5 and 2.5 respectively, and the anode and cathode back pressures were set to 100 kPa. The IV curve was tested to obtain the limiting current density.
[0121] The remaining activation steps and parameters were the same as in Example 1.
[0122] Comparative Example 3
[0123] The difference between this comparative example and Example 1 is that step (4) is not performed in this comparative example.
[0124] The remaining activation steps and parameters were the same as in Example 1.
[0125] The activation time and hydrogen fuel consumption of the activation methods provided in Examples 1-7 and Comparative Examples 1-3 were calculated, and the specific results are shown in Table 1.
[0126] Table 1
[0127] Activation time Hydrogen fuel consumption Example 1 8~10min ~12L Example 2 10~12min ~12.8L Example 3 8~10min ~12L Example 4 6~8min ~11.3L Example 5 8~10min ~12L Example 6 8~10min ~12L Example 7 8~10min ~12L Comparative Example 1 8~8.5h ~570L Comparative Example 2 2~3h ~142.5L Comparative Example 3 2~4min ~6L
[0128] Polarization curve tests were performed on the activated fuel cells provided in Examples 1-7 and Comparative Examples 1-3 to obtain the peak power density of the fuel cells. The specific test conditions were: the anode and cathode humidification temperatures were 75°C, the gas pipeline was 75°C, and the battery temperature was 75°C; the anode and cathode gases were hydrogen and air, respectively, the gas stoichiometric ratios were 1.5 and 2.5, respectively, and the anode and cathode back pressures were set to 100 kPa. The test results are shown in Table 2.
[0129] Figure 2 The performance curve comparison of the fuel cell activated by the activation method provided in Example 1 and Comparative Example 1 is shown. Figure 2 It can be seen that the activation method provided by the present invention can achieve the same activation effect as that of Comparative Example 1 in a short time.
[0130] Table 2
[0131] <![CDATA[Activation effect - Peak power density (W / cm 2 )]]> Example 1 2.03 Example 2 2.01 Example 3 2.02 Example 4 1.97 Example 5 1.96 Example 6 1.96 Example 7 1.97 Comparative Example 1 1.96 Comparative Example 2 1.89 Comparative Example 3 1.73
[0132] Depend on Figure 1-Figure 2 It can be seen from Table 1-Table 2 that the activation time and hydrogen consumption of Examples 1 to 7 are basically the same, and the activation effect (power density) of Examples 1 to 3 is better than that of Examples 4 to 7, and Example 1 is the best. The activation time and hydrogen consumption of Comparative Examples 1 and 2 are much greater than those of the Examples, with higher costs, lower efficiency, and poorer activation effects. Although the activation time of Comparative Example 3 is short, the activation effect is poor and the activation purpose cannot be achieved.
[0133] In summary, the activation method provided by the present invention is suitable for both single-cell structures and fuel cell stack activation, covering all membrane electrode activation and performance recovery in fuel cells, and has a wide range of applications; and the activation process is simple and convenient, the activation process can be completed in a short time, and the activation effect is significant; at the same time, program control and one-button operation can be realized, which is convenient and efficient.
[0134] The applicant declares that the above is only a specific implementation mode of the present invention, but the protection scope of the present invention is not limited thereto. Those skilled in the art should understand that any changes or substitutions that can be easily thought of by those skilled in the art within the technical scope disclosed by the present invention are within the protection scope and disclosure scope of the present invention.
Claims
1. A method for activating a fuel cell, characterized in that: The activation method comprises the following steps: (1) Electrode wetting: Wetting the electrodes of the fuel cell to be activated; (2) Limiting current value test: After the electrodes are wetted, a first mixed gas containing oxygen is introduced into the cathode of the fuel cell to be activated, and hydrogen is introduced into the anode. Then, the voltage is gradually reduced from the open circuit voltage until the limiting current value appears. (3) After step (2), a constant voltage current shock is performed; Repeat steps (2)-(3) until the activation completion conditions are met and the activation is completed.
2. The activation method according to claim 1, characterized in that The electrode wetting method comprises: independently purging the cathode and anode of the fuel cell to be activated with wet nitrogen; Preferably, the gas volume of the wet nitrogen is ≥2A / cm 2 ; Preferably, the wet nitrogen purge time is 30 to 60 seconds.
3. The activation method according to claim 1 or 2, characterized in that The concentration of oxygen in the first mixed gas introduced is 0.5% to 3%; Preferably, the process of gradually reducing the voltage from the open circuit voltage includes: the voltage is reduced at a first gradient value each time until the current value starts to decrease, and the voltage is reduced at a second gradient value each time; Preferably, the first gradient value is 0.1 to 0.2 V / time; Preferably, the second gradient value is 0.02 to 0.05 V / time; Preferably, the judgment criterion of the limiting current value is: the current value does not change within 5 seconds under constant voltage, and the residence time when reaching the limiting current value is not less than 2 seconds.
4. The activation method according to any one of claims 1 to 3, characterized in that: In the process of repeating steps (2)-(3), step (2) first performs a self-repeating process at least once; Preferably, during the self-repeating process of step (2), the concentration of oxygen in the first mixed gas introduced into the cathode in the previous time is higher than the concentration of oxygen in the first mixed gas introduced into the cathode in the next time; Preferably, the self-repeating process of step (2) is repeated 2 to 5 times.
5. The activation method according to any one of claims 1 to 4, characterized in that: The step (3) comprises: After step (2) is completed, air is introduced into the cathode, the hydrogen in the anode remains unchanged, and a constant voltage current shock is performed; Preferably, during the constant voltage current impact process, the stoichiometric ratio of the gas introduced into the cathode is 2.0-3.0, and the stoichiometric ratio of the gas introduced into the anode is 1.5-2.0; Preferably, the constant voltage value is 0.3-0.5V; Preferably, the constant voltage current shock time is 1 to 4 minutes.
6. The activation method according to any one of claims 1 to 5, characterized in that: The number of repetitions of steps (2)-(3) is ≥2 times.
7. The activation method according to any one of claims 1 to 6, characterized in that: The standard of the activation completion condition includes: if the current deviation between the constant voltage current impact in the previous round of step (3) and the constant voltage current impact in the next round of step (3) is less than 1A, the activation is completed.
8. The activation method according to any one of claims 1 to 6, characterized in that: The standard of the activation completion condition includes: the current value remains consistent for at least 20 seconds after the constant voltage current shock in step (3), and the activation is completed.
9. The activation method according to claim 1, characterized in that: The activation method comprises the following steps: (1) Electrode wetting: The cathode and anode of the fuel cell to be activated are independently subjected to gas flow ≥ 2A / cm 2 Purge with wet nitrogen for 30 to 60 seconds; (2) Limiting current value test: After the electrodes are wetted, a first mixed gas with an oxygen concentration of 0.5% to 3% is introduced into the cathode of the fuel cell to be activated, and hydrogen is introduced into the anode. The voltage is reduced at a first gradient value of 0.1 to 0.2 V / time until the current value begins to decrease. The voltage is reduced at a second gradient value of 0.02 to 0.05 V / time until the current value does not change within 5 seconds under constant voltage, and the dwell time when the limiting current value is reached is not less than 2 seconds, thereby obtaining the limiting current value; Step (2) is repeated 2 to 5 times, during which the concentration of oxygen in the first mixed gas introduced into the cathode in the previous process is higher than the concentration of oxygen in the first mixed gas introduced into the cathode in the next process; (3) after step (2) is completed, air is introduced into the cathode, the hydrogen in the anode remains unchanged, the stoichiometric ratio of the gas introduced into the cathode is 2.0 to 3.0, and the stoichiometric ratio of the gas introduced into the anode is 1.5 to 2.0, and a constant voltage current shock of 0.3 to 0.5 V is performed for 1 to 4 minutes; Repeat steps (2)-(3) at least twice until the activation is complete; The standard of the activation completion condition includes: the current deviation between the constant voltage current impact in the previous round of step (3) and the constant voltage current impact in the next round of step (3) is less than 1A, then the activation is completed; or, The standard of the activation completion condition includes: the current value remains the same for at least 20 seconds after the constant voltage current shock in step (3), and the activation is completed; After activation is completed, activation ends.
10. An activated fuel cell, characterized in that: The activated fuel cell is obtained by activation by the activation method according to any one of claims 1 to 9.
Citation Information
Cited By
Synchronous assembling and activating method of fuel cell stack, assembled and activated fuel cell stack and fuel cell
CN121885678A