Two-dimensional material-based track torque-driven magnetization turnover device and preparation method and application thereof
By using two-dimensional materials as the orbital Hall layer, combined with two-dimensional ferromagnetic materials and non-two-dimensional metal oxides, the electron transport characteristics are optimized, the problems of lattice matching and interface defects in the traditional heterojunction structure are solved, and the automatic Spin polarization efficiency and flipping efficiency achieve a more efficient orbital Hall effect.
Patent Information
- Application Number
- CN202410829878.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-25
- Publication Date
- 2024-10-25
AI Technical Summary
Traditional heterojunction structures have problems in MRAM due to lattice matching and interface defects, resulting in low efficiency of orbital Hall effect technology. Heavy metal materials are often used, making it difficult to avoid defects caused by magnetron sputtering preparation.
Using ultra-thin two-dimensional materials with clean surfaces and no dangling bonds as orbital Hall layer materials, combined with two-dimensional ferromagnetic materials and non-two-dimensional metal oxides, etc., by regulating the external field and temperature, the electron transport characteristics are optimized to achieve higher spin polarization efficiency.
It effectively avoids lattice matching and interface defect problems, improves the efficiency of the orbital Hall effect, achieves higher spin polarization efficiency and flipping efficiency, and reduces dependence on heavy metal materials.
Smart Images

Figure CN118843383A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of spin information storage, and in particular to an orbital torque driven magnetization reversal device based on two-dimensional materials, and a preparation method and application thereof. Background Art
[0002] In MRAM, the basic storage cell structure is a "sandwich structure" stacked up and down, usually composed of three layers. From top to bottom, they are the free layer, barrier layer and reference layer. Data is usually stored in the "free" layer whose magnetic properties can be changed. When the magnetic moment of the free layer is in the same direction as the magnetic moment of the reference layer, the stored data is "0". When the magnetic moment of the free layer is in the opposite direction to the magnetic moment of the reference layer, the stored data is "1". Reading data means reading the direction of the magnetic moment of the free layer.
[0003] In order to store data, we need to change the direction of the free layer magnetic moment. One of the most common methods is to use the spin current generated by the spin Hall effect to flip the free layer magnetic moment, which is SOT. SOT usually uses heavy metal materials with strong spin-orbit coupling. The OT flip is achieved by using the orbital Hall effect. The orbital Hall effect and the interfacial Rashba effect provide new methods for effectively generating orbital current and spin-orbit moment without the use of heavy metals. Even if spin-orbit coupling does not exist, the orbital structure generally produces the orbital Hall effect. When the spin-orbit coupling is strong, the orbital Hall effect is effectively converted into the spin Hall effect. Therefore, the orbital Hall effect is more fundamental than the spin Hall effect.
[0004] At present, the commonly used orbital Hall effect technology solutions usually use light metals and metal oxides as orbital Hall channels, use traditional ferromagnetic materials as magnetic free layers, and prepare ferromagnetic / non-magnetic heterojunctions. The orbital Hall effect of the non-magnetic layer and the spin-orbit coupling of the ferromagnetic layer are used to flip the magnetic moment of the ferromagnetic layer.
[0005] However, the traditional heterojunction structure may cause some problems due to lattice matching and interface defects. Therefore, it is urgent to expand new orbital Hall channel materials and develop new preparation methods to solve the above problems. Summary of the invention
[0006] The purpose of the present invention is to provide an orbital torque driven magnetization reversal structure based on two-dimensional materials and its preparation method and application, so as to avoid the use of heavy metals as orbital Hall channels and avoid the lattice matching and interface defect problems caused by heterojunctions prepared by magnetron sputtering.
[0007] The first aspect of the present invention is:
[0008] A device is provided.
[0009] A second aspect of the present invention is:
[0010] A method for preparing the device is provided.
[0011] The third aspect of the present invention is:
[0012] Applications of the device.
[0013] The invention also provides a spin information storage device.
[0014] The invention also provides a spin information storage device.
[0015] Specifically, the technical solution adopted according to the first aspect of the present invention is:
[0016] A device comprising the following structure:
[0017] Free layer;
[0018] An orbital Hall layer is provided on the lower surface of the free layer;
[0019] A substrate, disposed on the lower surface of the orbital Hall layer;
[0020] An electrode, disposed on the upper surface of the substrate and in contact with the orbital Hall layer;
[0021] The material of the free layer includes two-dimensional ferromagnetic material and non-two-dimensional ferromagnetic material;
[0022] The material of the orbital Hall layer includes at least one of a two-dimensional antiferromagnetic material, a two-dimensional transition metal sulfide, a non-two-dimensional metal oxide, a non-two-dimensional light metal and its oxide and nitride.
[0023] According to the embodiments of the present invention, one of the technical solutions has at least one of the following advantages or beneficial effects:
[0024] The present invention abandons the heterojunction prepared by magnetron sputtering, which usually uses light metal as the material of the orbital Hall layer; on the contrary, the present invention uses ultra-thin, surface-clean, dangling-bond-free, rotatably stacked two-dimensional materials as the material of the orbital Hall layer, avoiding problems that may be caused by lattice matching and interface defects.
[0025] In addition, the device of the present invention can be further expanded by further arranging a barrier layer and a reference layer on the free layer. The device of the present invention optimizes the electron transport characteristics and achieves higher spin polarization efficiency by adjusting the external field, temperature and material structure.
[0026] In the device of the present invention, the electrode is arranged on the upper surface of the substrate and is in contact with the orbital Hall layer. The electrode may or may not be in contact with the free layer and the electrode. The electrode is used to pass current in the device, thereby causing orbital flow in the orbital Hall layer, and finally realizing the reversal of the magnetic moment direction in the free layer.
[0027] According to one embodiment of the present invention, the two-dimensional antiferromagnetic material includes at least one of NiPS3, FePS3, and MnPS3.
[0028] According to one embodiment of the present invention, the two-dimensional transition metal sulfide includes at least one of MoS2, MoSe2, MoTe2, WS2, WTe2, and WSe2. Preferably, it is at least one of MoS2 and WTe2. Among the two-dimensional transition metal sulfides, WTe2 and MoS2 have larger orbital Hall angles, so using WTe2 and MoS2 as orbital Hall channels to achieve ferromagnetic layer reversal efficiency is higher.
[0029] According to one embodiment of the present invention, the non-two-dimensional metal oxide comprises CuO y At least one of the following, wherein y=1 or 0.5. CuO y The spin Hall conductivity of CuO is high. y When copper oxide (CuO) is used as the material of the orbital Hall channel, y )'s orbital Hall effect and the spin-orbit coupling of the ferromagnetic layer to achieve flipping.
[0030] According to one embodiment of the present invention, the material of the orbital Hall channel is CuO y Adding heavy metal Pt between the free layer can improve the switching efficiency.
[0031] According to one embodiment of the present invention, the two-dimensional ferromagnetic material comprises Fe 3-x GeTe、Fe 3-x GaTe, Cr2GeTe2, Cr2Ge2Te6, Mn2BiTe4, Mn4BiTe7, Mn6BiTe 10 At least one of , wherein x=0 or -2.
[0032] According to one embodiment of the present invention, the non-two-dimensional ferromagnetic material includes Co, CoFeB, Ni, Ni-Fe, CoFeB / Gd, [Co / Pt] n At least one of .
[0033] Specifically, the technical solution adopted according to the second aspect of the present invention is:
[0034] A method for preparing the device comprises the following steps:
[0035] S1 prepares the Hall Bar on the substrate, and transfers the material of the orbital Hall layer to the substrate by mechanical stripping to obtain the orbital Hall layer;
[0036] S2 transfers the material of the free layer to the surface of the orbital Hall layer to obtain the device.
[0037] According to an embodiment of the present invention, in step S1, a Hall Bar is prepared on a substrate, and the function of the Hall Bar is to pass current through the heterojunction and measure the Hall voltage.
[0038] According to an embodiment of the present invention, in step S1, when the material of the track Hall layer is transferred to the substrate, the size of the material of the track Hall layer can completely contact the electrode through which the current or voltage passes in the test.
[0039] A spin information storage device comprises the following structure:
[0040] Reference layer;
[0041] A barrier layer, disposed on the lower surface of the reference layer;
[0042] A base layer, disposed on the lower surface of the barrier layer, the base layer comprising a free layer and a track Hall layer;
[0043] The materials of the reference layer, the barrier layer and the free layer in the base layer are all two-dimensional materials or non-two-dimensional materials;
[0044] The material of the reference layer includes a ferromagnetic material, and the material of the barrier layer includes an insulating material.
[0045] According to one embodiment of the present invention, the insulating material includes at least one of two-dimensional boron nitride, fluorinated graphene and graphene oxide.
[0046] According to one embodiment of the present invention, when the material of the orbital Hall layer in the base layer is a two-dimensional antiferromagnetic material, a two-dimensional transition metal sulfide, a non-two-dimensional metal oxide, and a non-two-dimensional light metal and its oxide and nitride, the material of the reference layer of the spin information storage device includes Co, CoFeB, Ni, Ni-Fe, CoFeB / Gd, [Co / Pt] n Non-two-dimensional ferromagnetic materials, including Fe 3-x GeTe、Fe 3-x GaTe, Cr2GeTe2, Cr2Ge2Te6, Mn2BiTe4, Mn4BiTe7, Mn6BiTe 10 The free layer of the spin information storage device includes Co, CoFeB, Ni, Ni-Fe, CoFeB / Gd, [Co / Pt]n Non-two-dimensional ferromagnetic materials, including Fe 3-x GeTe、Fe 3-x GaTe, Cr2GeTe2, Cr2Ge2Te6, Mn2BiTe4, Mn4BiTe7, Mn6BiTe 10 The material of the barrier layer includes metal oxide insulating material and two-dimensional insulating material.
[0047] According to one embodiment of the present invention, the non-two-dimensional metal oxide insulating material includes at least one of magnesium oxide MgO, titanium oxide TiO2, hafnium oxide HfO2, and aluminum oxide Al2O3.
[0048] According to an embodiment of the present invention, a spin information storage device is a magnetic tunnel junction (MTJ) based on the orbital Hall effect, and the spin information storage device can achieve flipping based on the orbital Hall effect. The spin information storage device is constructed to present a vertically stacked sandwich structure, specifically, including the following structures stacked in sequence:
[0049] Reference layer, barrier layer, free layer, orbital Hall layer, substrate. The reference layer is made of two-dimensional ferromagnetic material, which includes Fe 3-x GeTe、Fe 3-x GaTe, Cr2GeTe2, Cr2Ge2Te6, Mn2BiTe4, Mn4BiTe7, Mn6BiTe 10 At least one of the following: a barrier layer, the barrier layer is made of insulating material, the insulating material includes at least one of two-dimensional boron nitride, fluorinated graphene and graphene oxide; the lower layer is a free layer, the free layer is made of two-dimensional ferromagnetic material, the two-dimensional ferromagnetic material includes Fe 3- x GeTe、Fe 3-x GaTe, Cr2GeTe2, Cr2Ge2Te6, Mn2BiTe4, Mn4BiTe7, Mn6BiTe 10 At least one of the following: the orbital Hall layer selects a two-dimensional antiferromagnetic material or a two-dimensional transition metal sulfide as the orbital Hall channel to flip the magnetic moment of the free layer, thereby changing the direction of the magnetic moment of the free layer, so that the magnetic moment of the free layer is parallel or antiparallel to the magnetic moment of the reference layer. When the magnetic moment of the free layer is parallel to the magnetic moment of the reference layer, the unit stores information "0", and when the magnetic moment of the free layer is antiparallel to the magnetic moment of the reference layer, the unit stores information "1".
[0050] According to an embodiment of the present invention, a spin information storage device is a magnetic tunnel junction (MTJ) based on the orbital Hall effect, and the spin information storage device can realize the orbital Hall effect by flipping. The spin information storage device is constructed to present a vertically stacked sandwich structure, specifically, including the following structures stacked in sequence:
[0051] Reference layer, barrier layer, free layer, orbital Hall layer, substrate. The reference layer is made of ferromagnetic material, including at least one of Co, CoFeB, Ni, Ni-Fe, and [Co / Pt]2; the barrier layer is made of metal oxide insulating material, including at least one of magnesium oxide MgO, titanium oxide TiO2, hafnium oxide HfO2, and aluminum oxide Al2O3; the free layer is made of ferromagnetic material, including at least one of Co, CoFeB, Ni, Ni-Fe, and [Co / Pt]2; the orbital Hall layer selects the above-mentioned non-two-dimensional metal oxides and non-two-dimensional light metals and their oxides and nitrides as the orbital Hall channel to flip the magnetic moment of the free layer, thereby changing the direction of the magnetic moment of the free layer, so that the magnetic moment of the free layer is parallel or antiparallel to the magnetic moment of the reference layer. When the magnetic moment of the free layer is parallel to the magnetic moment of the reference layer, the unit stores information "0", and when the magnetic moment of the free layer is antiparallel to the magnetic moment of the reference layer, the unit stores information "1".
[0052] According to an embodiment of the present invention, a spin information storage device is a magnetic tunnel junction (MTJ) based on the orbital Hall effect, and the spin information storage device can realize the orbital Hall effect by flipping. The spin information storage device is constructed to present a vertically stacked sandwich structure, specifically, including the following structures stacked in sequence:
[0053] Reference layer, barrier layer, free layer, orbital Hall layer, substrate. The reference layer is made of two-dimensional ferromagnetic materials, including Fe 3-x GeTe、Fe 3-x GaTe, Cr2GeTe2, Cr2Ge2Te6, Mn2BiTe4, Mn4BiTe7, Mn6BiTe 10 At least one of the following: the barrier layer is made of insulating material, the insulating material includes at least one of two-dimensional boron nitride, fluorinated graphene and graphene oxide; the lower layer is a free layer, the free layer is made of two-dimensional ferromagnetic material, the two-dimensional ferromagnetic material includes Fe 3-x GeTe、Fe 3-x GaTe, Cr2GeTe2, Cr2Ge2Te6, Mn2BiTe4, Mn4BiTe7, Mn6BiTe 10At least one of the following: the orbital Hall layer selects a metal oxide as the orbital Hall channel to flip the magnetic moment of the free layer, thereby changing the direction of the magnetic moment of the free layer, so that the magnetic moment of the free layer is parallel or antiparallel to the magnetic moment of the reference layer. When the magnetic moment of the free layer is parallel to the magnetic moment of the reference layer, the unit stores information "0", and when the magnetic moment of the free layer is antiparallel to the magnetic moment of the reference layer, the unit stores information "1".
[0054] Another aspect of the present invention further provides a spin information storage device, including the spin information storage device described in the above embodiment. Since the application adopts all the technical solutions of the above spin information storage device, it at least has all the beneficial effects brought by the technical solutions of the above embodiment.
[0055] Other features and advantages of the present invention will be set forth in the description which follows, and in part will be obvious from the description, or may be learned by practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0056] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the description of the embodiments in conjunction with the following drawings, in which:
[0057] Figure 1 Schematic diagram of the structure of the device in Example 1.
[0058] Figure 2 Schematic diagram of the structure of the spin information storage device in Example 1.
[0059] Figure 3 Schematic diagram of the electrode structure in the device in Example 1.
[0060] Reference numerals:
[0061] 100 - free layer, 200 - orbital Hall layer, 300 - substrate, 400 - barrier layer, 500 - reference layer. DETAILED DESCRIPTION
[0062] The embodiments of the present invention are described in detail below, and the same or similar reference numerals throughout the embodiments represent the same or similar elements or elements with the same or similar functions. The embodiments described below are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.
[0063] In the description of the present invention, if there is a description of first, second, etc., it is only for the purpose of distinguishing technical features, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features or implicitly indicating the order of the indicated technical features.
[0064] In the description of the present invention, it should be understood that descriptions involving orientation, such as orientation or positional relationship indicated as up, down, etc., are based on the orientation or positional relationship shown in the embodiments, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.
[0065] The words "preferably", "more preferably", etc. in the present invention refer to embodiments of the present invention that may provide certain beneficial effects in certain circumstances. However, other embodiments may also be preferred under the same circumstances or other circumstances. In addition, the description of one or more preferred embodiments does not imply that other embodiments are not applicable, nor is it intended to exclude other embodiments from the scope of the present invention.
[0066] When a numerical range is disclosed herein, the above range is considered to be continuous and includes the minimum and maximum values of the range, as well as every value between such minimum and maximum values. Further, when a range refers to an integer, every integer between the minimum and maximum values of the range is included. In addition, when multiple ranges are provided to describe features or characteristics, the ranges can be combined. In other words, unless otherwise indicated, all ranges disclosed herein should be understood to include any and all subranges included therein.
[0067] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of the present invention.
[0068] Unless otherwise specified, the reagents, methods and equipment used in the present invention are conventional reagents, methods and equipment in the art.
[0069] In the embodiment, the area of the substrate is larger than the reference layer, the area of the reference layer is larger than the barrier layer, the area of the barrier layer is larger than the free layer, and the area of the free layer is larger than the orbital Hall layer. Except for the substrate, the area of the lower layer in the remaining structural layers should be smaller than the upper layer to ensure the contact efficiency with the electrode, and ultimately ensure that the spin information storage device achieves higher spin polarization and faster spin flip speed.
[0070] Example 1
[0071] A device, the structural diagram of which is shown in Figure 1 As shown, specifically, it includes the following structures:
[0072] Free layer 100;
[0073] The orbital Hall layer 200 is disposed on the lower surface of the free layer 100;
[0074] The substrate 300 is disposed on the lower surface of the track Hall layer 200;
[0075] An electrode, disposed on the upper surface of the substrate 300 and in contact with the orbital Hall layer 200;
[0076] The material of the substrate 300 is Si / SiO2;
[0077] The material of the orbital Hall layer 200 is MoS2;
[0078] The material of the free layer 100 is Fe3GaTe2;
[0079] The method for preparing the above device comprises the following steps:
[0080] A1 fabricates Hall Bar on Si / SiO2 substrate 300 by micro-nano processing;
[0081] A2 places the bulk MoS2 material on a blue film tape, folds the tape several times to obtain a clean and thin MoS2 sample, and then sticks polydimethylsiloxane (PDMS) on the tape with the two-dimensional material, thereby obtaining a MoS2 material with a thickness of about 20nm on the PDMS;
[0082] A3 selects MoS2 material with a thickness of 20-30nm, a rectangular or square shape, and a size of about 12μm*8μm, which is adhered to PDMS, and performs directional transfer so that it covers all electrodes;
[0083] A4 places the bulk Fe3GaTe2 material on the blue film tape, folds the tape several times to obtain a clean and thin Fe3GaTe2 sample, and then sticks PDMS on the tape with the two-dimensional material, thereby obtaining a Fe3GaTe2 material with a thickness of about 20nm on the PDMS;
[0084] A5 selects Fe3GaTe2 material with a thickness of 15-20nm, a rectangular or square shape, and a size of about 12μm*8μm, which is adhered to PDMS, and performs directional transfer so that it covers the MoS2 material as much as possible to obtain the above-mentioned device.
[0085] A storage device, the structural diagram of which is as follows Figure 2 As shown, specifically, it includes the following structures:
[0086] Reference layer 500;
[0087] The barrier layer 400 is disposed on the lower surface of the reference layer 500;
[0088] The free layer 100 is disposed on the lower surface of the barrier layer 400;
[0089] The orbital Hall layer 200 is disposed on the lower surface of the free layer 100;
[0090] The substrate 300 is disposed on the lower surface of the track Hall layer 200;
[0091] The electrode is disposed on the upper surface of the substrate 300 and contacts the orbital Hall layer 200. The electrode comprises four sub-electrodes which are symmetrically placed and do not contact each other. The schematic diagram of the structure is shown in FIG. Figure 3 shown.
[0092] The preparation of the spin information storage device comprises the following steps:
[0093] S1: hBN is transferred onto the material Fe3GaTe2 of the free layer 100 of the above device as a barrier layer 400;
[0094] S2 transfers Fe3GaTe2 onto hBN as a reference layer 500 to obtain the above-mentioned spin information storage device.
[0095] Example 2
[0096] A device comprising the following structure:
[0097] Free layer 100;
[0098] The orbital Hall layer 200 is disposed on the lower surface of the free layer 100;
[0099] The substrate 300 is disposed on the lower surface of the track Hall layer 200;
[0100] An electrode, disposed on the upper surface of the substrate 300 and in contact with the orbital Hall layer 200;
[0101] The material of the substrate 300 is Si / SiO2;
[0102] The material of the orbital Hall layer 200 is WTe2;
[0103] The material of the free layer 100 is Fe3GaTe2;
[0104] The method for preparing the above device comprises the following steps:
[0105] A1 fabricates Hall Bar on Si / SiO2 substrate 300 by micro-nano processing;
[0106] A2: Place the bulk WTe2 material on a blue film tape, fold the tape several times to obtain a clean and thin WTe2 sample, and then attach PDMS to the tape with the two-dimensional material, thereby obtaining a WTe2 material with a thickness of about 20 nm on the PDMS;
[0107] A3 selects WTe2 material with a thickness of 20-30 nm, a rectangular or square shape, and a size of about 12 μm*8 μm, which is adhered to PDMS, and performs directional transfer so that it covers all electrodes;
[0108] A4 places the bulk Fe3GaTe2 material on the blue film tape, folds the tape several times to obtain a clean and thin Fe3GaTe2 sample, and then sticks PDMS on the tape with the two-dimensional material, thereby obtaining a Fe3GaTe2 material with a thickness of about 20nm on the PDMS;
[0109] A5 selects Fe3GaTe2 material with a thickness of 15-20nm, a rectangular or square shape, and a size of about 12μm*8μm, which is adhered to PDMS, and performs directional transfer so that it covers the WTe2 material as much as possible to obtain the above-mentioned device.
[0110] A spin information storage device comprises the following structure:
[0111] Reference layer 500;
[0112] The barrier layer 400 is disposed on the lower surface of the reference layer 500;
[0113] The free layer 100 is disposed on the lower surface of the barrier layer 400;
[0114] The orbital Hall layer 200 is disposed on the lower surface of the free layer 100;
[0115] The substrate 300 is disposed on the lower surface of the track Hall layer 200;
[0116] The electrode is disposed on the upper surface of the substrate 300 and is in contact with the track Hall layer 200 .
[0117] The preparation of the spin information storage device comprises the following steps:
[0118] S1: hBN is transferred onto the material Fe3GaTe2 of the free layer 100 of the above device as a barrier layer 400;
[0119] S2 transfers Fe3GaTe2 onto hBN as a reference layer 500 to obtain the above-mentioned spin information storage device.
[0120] Example 3
[0121] A device comprising the following structure:
[0122] Free layer 100;
[0123] The orbital Hall layer 200 is disposed on the lower surface of the free layer 100;
[0124] The substrate 300 is disposed on the lower surface of the track Hall layer 200;
[0125] An electrode, disposed on the upper surface of the substrate 300 and in contact with the orbital Hall layer 200;
[0126] The material of the substrate 300 is Si / SiO2;
[0127] The material of the track Hall layer 200 is NiPS3;
[0128] The material of the free layer 100 is Fe3GaTe2;
[0129] The method for preparing the above device comprises the following steps:
[0130] A1 fabricates Hall Bar on Si / SiO2 substrate 300 by micro-nano processing;
[0131] A2 places the bulk NiPS3 material on a blue film tape, folds the tape several times to obtain a clean and thin NiPS3 sample, and then sticks PDMS on the tape with the two-dimensional material, thereby obtaining a NiPS3 material with a thickness of about 20 nm on the PDMS;
[0132] A3 selects NiPS3 material with a thickness of 20-30 nm, a rectangular or square shape, and a size of about 12 μm*8 μm, which is adhered to PDMS, and performs directional transfer so that it covers all electrodes;
[0133] A4 places the bulk Fe3GaTe2 material on the blue film tape, folds the tape several times to obtain a clean and thin Fe3GaTe2 sample, and then sticks PDMS on the tape with the two-dimensional material, thereby obtaining a Fe3GaTe2 material with a thickness of about 20nm on the PDMS;
[0134] A5 selects Fe3GaTe2 material with a thickness of 15-20nm, a rectangular or square shape, and a size of about 12μm*8μm, which is adhered to PDMS, and performs directional transfer so that it covers the NiPS3 material as much as possible to obtain the above-mentioned device.
[0135] A spin information storage device comprises the following structure:
[0136] Reference layer 500;
[0137] The barrier layer 400 is disposed on the lower surface of the reference layer 500;
[0138] The free layer 100 is disposed on the lower surface of the barrier layer 400;
[0139] The orbital Hall layer 200 is disposed on the lower surface of the free layer 100;
[0140] The substrate 300 is disposed on the lower surface of the track Hall layer 200;
[0141] The electrode is disposed on the upper surface of the substrate 300 and is in contact with the track Hall layer 200 .
[0142] The preparation of the spin information storage device comprises the following steps:
[0143] S1: hBN is transferred onto the material Fe3GaTe2 of the free layer 100 of the above device as a barrier layer 400;
[0144] S2 transfers Fe3GaTe2 onto hBN as a reference layer 500 to obtain the above storage device.
[0145] Example 4
[0146] A device comprising the following structure:
[0147] Free layer 100;
[0148] The orbital Hall layer 200 is disposed on the lower surface of the free layer 100;
[0149] The substrate 300 is disposed on the lower surface of the track Hall layer 200;
[0150] An electrode, disposed on the upper surface of the substrate 300 and in contact with the orbital Hall layer 200;
[0151] The material of the substrate 300 is Si / SiO2;
[0152] The material of the orbital Hall layer 200 is CuO2;
[0153] The material of the free layer 100 is Fe3GaTe2;
[0154] The method for preparing the above device comprises the following steps:
[0155] A1 uses magnetron sputtering to grow a Cu film on a Si / SiO2 substrate 300 and oxidizes it in air;
[0156] A2 micro-nano processing to prepare Hall Bar on oxidized Cu film and grow Pt / Ti electrode;
[0157] A3 places the bulk Fe3GaTe2 material on the blue film tape, folds the tape several times to obtain a clean and thin Fe3GaTe2 sample, and then sticks PDMS on the tape with the two-dimensional material, thereby obtaining a Fe3GaTe2 material with a thickness of about 20nm on the PDMS;
[0158] A4 selects Fe3GaTe2 material with a thickness of 15-20nm, a rectangular or square shape, and a size of about 12μm*8μm, which is adhered to PDMS, and performs directional transfer to obtain the above-mentioned device.
[0159] A spin information storage device comprises the following structure:
[0160] Reference layer 500;
[0161] The barrier layer 400 is disposed on the lower surface of the reference layer 500;
[0162] The free layer 100 is disposed on the lower surface of the barrier layer 400;
[0163] The orbital Hall layer 200 is disposed on the lower surface of the free layer 100;
[0164] The substrate 300 is disposed on the lower surface of the track Hall layer 200;
[0165] The electrode is disposed on the upper surface of the substrate 300 and is in contact with the track Hall layer 200 .
[0166] The preparation of the spin information storage device comprises the following steps:
[0167] S1: hBN is transferred onto the material Fe3GaTe2 of the free layer 100 of the above device as a barrier layer 400;
[0168] S2 transfers Fe3GaTe2 onto hBN as a reference layer 500 to obtain the above-mentioned spin information storage device.
[0169] Example 5
[0170] The difference between Example 5 and Example 1 is that in Example 5, the material of the orbital Hall layer 200 is WSe2.
[0171] Example 6
[0172] The difference between Example 6 and Example 1 is that in Example 6, the material of the orbital Hall layer 200 is WS2.
[0173] Example 7
[0174] The difference between Example 7 and Example 1 is that in Example 7, the material of the orbital Hall layer 200 is MoSe2.
[0175] Example 8
[0176] The difference between Example 8 and Example 1 is that in Example 8, the material of the orbital Hall layer 200 is MoTe2.
[0177] Performance Test:
[0178] The devices prepared in Examples 1-7 were subjected to the following tests, and the test results are shown in Table 1.
[0179] The orbital Hall conductance is calculated from the momentum and orbital Berry curvature, and the test method is as follows:
[0180]
[0181] in,
[0182] is the orbital current density along the α direction, corresponding to the γ component of the orbital torque, generated by the electric field pointing in the β direction;
[0183] In a two-dimensional system, Vc corresponds to the surface unit area, so its conductivity is Dimension.
[0184] The Berry curvature in Eq. It can be calculated using the Kubo formula in the eigenvalue and eigenfunction, where n is the band index and the expression is:
[0185]
[0186] The orbital current operator is
[0187] where Lγ is the orbital angular momentum operator, is the speed operator.
[0188] Table 1
[0189]
[0190]
[0191] The above are only embodiments of the present invention, and are not intended to limit the patent scope of the present invention. Any equivalent transformations made using the contents of the present invention specification, or directly or indirectly applied in related technical fields, are also included in the patent protection scope of the present invention.
Claims
1. A device, characterized in that: Includes the following structures: Free layer (100); A track Hall layer (200) is provided on the lower surface of the free layer (100); A substrate (300) is provided on the lower surface of the track Hall layer (200); An electrode, provided on the upper surface of the substrate (300) and in contact with the orbital Hall layer (200); A protective layer, disposed on the upper surface of the free layer (100); The material of the free layer (100) includes a two-dimensional ferromagnetic material and a non-two-dimensional ferromagnetic material; The material of the orbital Hall layer (200) includes at least one of a two-dimensional antiferromagnetic material, a two-dimensional transition metal sulfide, a non-two-dimensional metal oxide, a non-two-dimensional light metal, and its oxide and nitride.
2. The device according to claim 1, wherein: The two-dimensional antiferromagnetic material includes at least one of NiPS3, FePS3, and MnPS3.
3. The device according to claim 1, wherein: The two-dimensional transition metal sulfide includes at least one of MoS2, MoSe2, MoTe2, WS2, WTe2, and WSe2.
4. The device according to claim 1, wherein: The non-two-dimensional metal oxide includes CuO y At least one of , wherein y=1 or 0.
5.
5. The device according to claim 1, wherein: The two-dimensional ferromagnetic material includes Fe 3-x GeTe、Fe 3- x GaTe, Cr2GeTe2, Cr2Ge2Te6, Mn2BiTe4, Mn4BiTe7, Mn6BiTe 10 At least one of , wherein x=0 or -2.
6. A device according to claim 1, characterized in that: The non-two-dimensional ferromagnetic materials include Co, CoFeB, Ni, Ni-Fe, CoFeB / Gd, [Co / Pt] n At least one of (n=1-30).
7. A method for preparing the device according to any one of claims 1 to 6, characterized in that: The following steps are involved: S1: preparing a Hall Bar electrode on a substrate (300), transferring the material of the orbital Hall layer (200) to the substrate (300), and obtaining the orbital Hall layer (200); S2 transfers the material of the free layer (100) to the surface of the orbital Hall layer (200), and covers it with a protective layer to obtain the device.
8. A memory device, characterized in that: Includes the following structures: Reference layer (500); a barrier layer (400) disposed on the lower surface of the reference layer (500); A free layer (100) is provided on the lower surface of the barrier layer (400); A track Hall layer (200) is provided on the lower surface of the free layer (100); A substrate (300) is provided on the lower surface of the track Hall layer (200); The materials of the reference layer (500), the barrier layer (400) and the free layer (100) are all two-dimensional materials or non-two-dimensional materials; The material of the reference layer (500) includes a ferromagnetic material, and the material of the barrier layer (400) includes an insulating material; The free layer (100), the orbital Hall layer (200) and the substrate (300) are structures included in the device according to any one of claims 1 to 6.
9. The memory device according to claim 8, wherein: The insulating material includes at least one of two-dimensional boron nitride, fluorinated graphene and graphene oxide.
10. A spin information storage device, characterized in that: Comprising the device according to any one of claims 1 to 6.