Magnetization rotation element, magnetoresistive effect element, and magnetic memory
By using spin-orbit torque wiring in the magnetized rotating element to connect to the ferromagnetic layer, the spin Hall effect is used to generate spin current, which solves the power consumption problem caused by the increase in magnetic memory current and achieves low power consumption and Long life magnetoresistance effect element.
Patent Information
- Application Number
- CN202280091503.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-07
- Publication Date
- 2024-10-29
AI Technical Summary
In a magnetic memory, when the amount of current applied to each magnetoresistive effect element increases, the power consumption increases. Therefore, it is necessary to reduce the amount of current applied to each magnetoresistive effect element to suppress the power consumption of the magnetic memory.
A magnetized rotating element connected to the first ferromagnetic layer using spin-orbit torque wiring, the spin-orbit torque wiring containing amorphous structures such as oxides, nitrides or oxynitrides with different oxygen or nitrogen concentrations. Surface, equipped with an insulating layer to cover the spin-orbit torque wiring and a ferromagnetic layer, generates spin current through the spin Hall effect to reduce the current density required for magnetization reversal.
It achieves operation with less current, reduces the power consumption of the magnetic memory, and extends the life of the magnetoresistive effect element.
Smart Images

Figure CN118872058A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a magnetization rotation element, a magnetoresistance effect element and a magnetic memory. Background Art
[0002] Giant magnetoresistance (GMR) elements consisting of a multilayer film of a ferromagnetic layer and a non-magnetic layer, and tunnel magnetoresistance (TMR) elements using an insulating layer (tunnel barrier layer, barrier layer) in the non-magnetic layer are widely known as magnetoresistance elements. Magnetoresistance elements can be applied to magnetic sensors, high-frequency components, magnetic heads, and non-volatile random access memories (MRAM).
[0003] MRAM is a storage element integrated with a magnetoresistive element. MRAM uses the property that when the direction of the mutual magnetization of two ferromagnetic layers sandwiching a nonmagnetic layer in the magnetoresistive element changes, the resistance of the magnetoresistive element also changes to read and write data. The direction of the magnetization of the ferromagnetic layer is controlled by, for example, the magnetic field generated by the current. In addition, for example, the direction of the magnetization of the ferromagnetic layer is controlled by the spin transfer torque (STT) generated by flowing the current along the stacking direction of the magnetoresistive element.
[0004] When the direction of magnetization of the ferromagnetic layer is rewritten by STT, a current is passed in the stacking direction of the magnetoresistive element. The write current causes degradation of the characteristics of the magnetoresistive element.
[0005] In recent years, methods that do not require current to flow along the stacking direction of the magnetoresistive effect element during writing have attracted attention (for example, Patent Document 1). One of the methods is a writing method that utilizes spin-orbit torque (SOT). SOT is caused by a spin current generated by the spin-orbit interaction or the Raschba effect at the interface of different materials. The current used to cause SOT in the magnetoresistive effect element flows in a direction that intersects the stacking direction of the magnetoresistive effect element. In other words, there is no need to make the current flow along the stacking direction of the magnetoresistive effect element, and the life of the magnetoresistive effect element is expected to be extended.
[0006] Prior art literature
[0007] Patent Literature
[0008] Patent Document 1: Japanese Patent Application Publication No. 2017-216286 Summary of the invention
[0009] 1. Technical issues to be resolved
[0010] The magnetic memory has a plurality of integrated magnetoresistance effect elements. When the amount of current applied to each magnetoresistance effect element increases, the power consumption of the magnetic memory increases. It is required to reduce the amount of current applied to each magnetoresistance effect element and suppress the power consumption of the magnetic memory.
[0011] The present invention has been made in view of the above circumstances, and an object of the present invention is to provide a magnetization rotation element, a magnetoresistive element, and a magnetic memory that can operate with a small current.
[0012] (II) Technical solution
[0013] In order to solve the above-mentioned problems, the present invention provides the following means.
[0014] (1) A magnetization rotation element according to a first aspect includes a spin-orbit torque wiring and a first ferromagnetic layer connected to the spin-orbit torque wiring. The spin-orbit torque wiring includes an amorphous structure. The amorphous structure is any one of an oxide, a nitride, and an oxynitride.
[0015] (2) In the magnetization rotation element of the above aspect, the concentration of oxygen or nitrogen contained in the spin-orbit torque wiring may be lower than the concentration of oxygen or nitrogen in a stoichiometric composition determined from cations constituting the spin-orbit torque wiring.
[0016] (3) In the magnetization rotation element of the above aspect, the spin-orbit torque wiring may include an element having d electrons or f electrons.
[0017] (4) In the magnetization rotation element of the above aspect, the oxygen or nitrogen concentration on a first surface of the spin-orbit torque wiring that is close to the first ferromagnetic layer may be different from the oxygen or nitrogen concentration on a second surface that is opposite to the first surface.
[0018] (5) In the magnetization rotation element of the above aspect, the oxygen or nitrogen concentration of the second surface may be higher than the oxygen or nitrogen concentration of the first surface.
[0019] (6) In the magnetization rotation element of the above aspect, the concentration of oxygen or nitrogen may gradually decrease from the second surface toward the first surface.
[0020] (7) In the magnetization rotation element of the above aspect, the oxygen or nitrogen concentration may be maximum or minimum between the second surface and the first surface.
[0021] (8) In the magnetization rotation element of the above aspect, the spin-orbit torque wiring may have different oxygen or nitrogen concentrations at the center and at the side surfaces in any direction within the plane.
[0022] (9) The magnetization rotation element of the above aspect may further include a first insulating layer covering the first ferromagnetic layer and the side surfaces of the spin-orbit torque wiring. The first insulating layer is made of any one of oxide, nitride, and oxynitride.
[0023] (10) The magnetization rotation element of the above aspect may further include a second insulating layer covering a second surface of the spin-orbit torque wiring opposite to the first surface close to the first ferromagnetic layer. The second insulating layer is any one of oxide, nitride, and oxynitride.
[0024] (11) In the magnetization rotation element of the above aspect, the second insulating layer may include a metal element constituting the spin-orbit torque wiring.
[0025] (12) In the magnetization rotation element of the above aspect, the spin-orbit torque wiring may include a crystallized layer therein.
[0026] (13) In the magnetization rotation element of the above aspect, the crystallized layer may include any one selected from the group consisting of Ta, Al, Mg, Si, Ga, and Ge.
[0027] (14) A magnetoresistance effect element according to a second aspect includes the magnetization rotation element according to the above aspect, a second ferromagnetic layer, and a nonmagnetic layer. The nonmagnetic layer is interposed between the first ferromagnetic layer and the second ferromagnetic layer.
[0028] (15) A magnetic memory according to a third aspect includes a plurality of magnetoresistive effect elements according to the above aspect.
[0029] (III) Beneficial effects
[0030] The magnetization rotation element, magnetoresistance effect element, and magnetic memory of the present invention operate with a small current. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] Figure 1 is a circuit diagram of the magnetic memory according to the first embodiment.
[0032] Figure 2 It is a cross-sectional view of a characteristic portion of the magnetic memory according to the first embodiment.
[0033] Figure 3 It is a cross-sectional view of the magnetoresistive effect element according to the first embodiment.
[0034] Figure 4 It is a top view of the magnetoresistive effect element according to the first embodiment.
[0035] Figure 5 is a cross-sectional view of a magnetoresistive effect element according to a first modification.
[0036] Figure 6 is a cross-sectional view of a magnetoresistive effect element according to a second modification.
[0037] Figure 7 is a cross-sectional view of a magnetization rotation element according to a second embodiment. DETAILED DESCRIPTION
[0038] Hereinafter, the present embodiment will be described in detail with reference to the accompanying drawings as appropriate. For the accompanying drawings used in the following description, in order to facilitate understanding of the features, the features are sometimes enlarged for convenience, and the dimensional ratios of the various structural elements are sometimes different from the actual ones. The materials, dimensions, etc. illustrated in the following description are only examples, and the present invention is not limited to these contents, and can be implemented with appropriate changes within the scope of achieving the effects of the present invention.
[0039] First, define the direction. Figure 2 ) is set as the x direction, and the direction perpendicular to the x direction is set as the y direction. The x direction is, for example, the long side direction of the spin-orbit torque wiring 20. The z direction is a direction perpendicular to the x direction and the y direction. The z direction is an example of a stacking direction in which each layer is stacked. In the following, the +z direction is sometimes expressed as "up" and the -z direction is expressed as "down". Up and down are not necessarily consistent with the direction in which gravity is applied.
[0040] In this specification, "extending in the x direction" means, for example, that the dimension in the x direction is larger than the smallest dimension in the x direction, the y direction, and the z direction. The same applies to extending in other directions. In addition, in this specification, "connection" is not limited to physical connection. For example, it is not limited to the case where two layers are in physical contact, and the case where two layers are connected with other layers sandwiched between them is also included in "connection". In addition, "connection" in this specification also includes electrical connection.
[0041] "First embodiment"
[0042] Figure 1 1 is a structural diagram of a magnetic memory 200 according to the first embodiment. The magnetic memory 200 includes: a plurality of magnetoresistance effect elements 100, a plurality of write wirings WL, a plurality of common wirings CL, a plurality of read wirings RL, a plurality of first switch elements Sw1, a plurality of second switch elements Sw2, and a plurality of third switch elements Sw3. The magnetic memory 200 is, for example, a component in which the magnetoresistance effect elements 100 are arranged in a matrix.
[0043] Each write wiring WL electrically connects a power supply to one or more magnetoresistance effect elements 100. Each common wiring CL is a wiring used both when writing data and when reading data. Each common wiring CL electrically connects a reference potential to one or more magnetoresistance effect elements 100. The reference potential is, for example, grounded. The common wiring CL can be provided in each of the plurality of magnetoresistance effect elements 100, or can be provided across the plurality of magnetoresistance effect elements 100. Each read wiring RL electrically connects a power supply to one or more magnetoresistance effect elements 100. The power supply is connected to the magnetic memory 200 when in use.
[0044] Each magnetoresistance effect element 100 is connected to a first switch element Sw1, a second switch element Sw2, and a third switch element Sw3, respectively. The first switch element Sw1 is connected between the magnetoresistance effect element 100 and a write wiring WL. The second switch element Sw2 is connected between the magnetoresistance effect element 100 and a common wiring CL. The third switch element Sw3 is connected to a read wiring RL across a plurality of magnetoresistance effect elements 100.
[0045] When the predetermined first switch element Sw1 and the second switch element Sw2 are turned on, a write current flows between the write wiring WL and the common wiring CL connected to the predetermined magnetoresistance effect element 100. By flowing the write current, data is written to the predetermined magnetoresistance effect element 100. When the predetermined second switch element Sw2 and the third switch element Sw3 are turned on, a read current flows between the common wiring CL and the read wiring RL connected to the predetermined magnetoresistance effect element 100. By flowing the read current, data is read from the predetermined magnetoresistance effect element 100.
[0046] The first switch element Sw1, the second switch element Sw2, and the third switch element Sw3 are elements for controlling the flow of current. The first switch element Sw1, the second switch element Sw2, and the third switch element Sw3 are, for example, elements that utilize phase change of a crystal layer such as a transistor, an ovonic threshold switch (OTS), elements that utilize changes in energy band structure such as a metal insulator transition (MIT) switch, elements that utilize breakdown voltage such as a Zener diode and an avalanche diode, and elements whose conductivity changes with changes in atomic positions.
[0047] Figure 1 The magnetic memory 200 shown in the figure shares the third switch element Sw3 with the magnetoresistance effect element 100 connected to the same read wiring RL. The third switch element Sw3 may also be provided in each magnetoresistance effect element 100. In addition, the third switch element Sw3 may also be provided in each magnetoresistance effect element 100, and the first switch element Sw1 or the second switch element Sw2 may also be shared in the magnetoresistance effect element 100 connected to the same wiring.
[0048] Figure 2 It is a cross-sectional view of a characteristic portion of the magnetic memory 200 according to the first embodiment. Figure 2 This is a cross section of the magnetoresistive element 100 cut along an xz plane passing through the center of the width of a spin-orbit torque wiring 20 in the y direction, which will be described later.
[0049] Figure 2 The first switching element Sw1 and the second switching element Sw2 shown are transistors Tr. The third switching element Sw3 is electrically connected to the readout wiring RL, for example, Figure 2 The transistor Tr is, for example, a field effect transistor, which has a gate electrode G, a gate insulating film GI, and a source S and a drain D formed on a substrate Sub. The source S and the drain D are defined by the direction of current flow, and they are the same region. The positional relationship between the source S and the drain D can be reversed. The substrate Sub is, for example, a semiconductor substrate.
[0050] The transistor Tr is electrically connected to the magnetoresistive element 100 via the through-hole wiring V, the electrode E2, and the electrode E3. In addition, the transistor Tr is connected to the write wiring WL or the common wiring CL via the through-hole wiring V. The through-hole wiring V extends, for example, in the z direction. The read-out wiring RL is connected to the stacked body 10 via the electrode E1. The through-hole wiring V and the electrode E1 contain a conductive material. The through-hole wiring V and the electrode E2 can be integrated. In addition, the through-hole wiring V and the electrode E3 can also be integrated. That is, the electrode E2 can be a part of the through-hole wiring V, and the electrode E3 can also be a part of the through-hole wiring V.
[0051] The magnetoresistance effect element 100 and the transistor Tr are covered by an insulating layer 90. The insulating layer 90 is an insulating layer for insulating between wirings and between elements of the multilayer wiring. The insulating layer 90 is, for example, silicon oxide (SiO x )、Silicon Nitride(SiN x ), silicon carbide (SiC), chromium nitride, silicon carbonitride (SiCN), silicon oxynitride (SiON), aluminum oxide (Al 2 O 3 )、ZrO x ), magnesium oxide (MgO), aluminum nitride (AlN), etc.
[0052] Figure 3 is a cross-sectional view of the magnetoresistive effect element 100 . Figure 3 This is a cross section of the magnetoresistive effect element 100 cut along an xz plane passing through the center of the width of the spin-orbit torque wiring 20 in the y direction. Figure 4 This is a plan view of the magnetoresistive effect element 100 as viewed from the z direction.
[0053] The magnetoresistance effect element 100 includes, for example, a laminate 10, a spin-orbit torque wiring 20, and electrodes E1, E2, and E3. The magnetoresistance effect element 100 is covered with, for example, insulating layers 91, 92, 93, and 94. The insulating layers 91, 92, 93, and 94 are part of the insulating layer 90 described above.
[0054] The magnetoresistance effect element 100 is a magnetic element utilizing spin-orbit torque (SOT), and is sometimes referred to as a spin-orbit torque magnetoresistance effect element, a spin injection magnetoresistance effect element, or a spin-current magnetoresistance effect element.
[0055] The magnetoresistance effect element 100 is an element for recording and storing data. The magnetoresistance effect element 100 records data with the resistance value in the z direction of the stack 10. The resistance value in the z direction of the stack 10 is changed by applying a write current along the spin-orbit torque wiring 20 and injecting spins from the spin-orbit torque wiring 20 into the stack 10. The resistance value in the z direction of the stack 10 can be read by applying a read current along the z direction of the stack 10.
[0056] The spin-orbit torque line 20 is longer in the x direction than in the y direction when viewed from the z direction, and extends in the x direction. A write current flows in the x direction between the electrode E2 and the electrode E3 along the spin-orbit torque line 20. The spin-orbit torque line 20 is connected to the electrode E2 and the electrode E3, respectively.
[0057] The spin-orbit torque wiring 20 generates a spin current through the spin Hall effect when current flows, and injects spins into the first ferromagnetic layer 1. The spin-orbit torque wiring 20, for example, imparts a spin-orbit torque (SOT) to the magnetization of the first ferromagnetic layer 1 that can reverse the magnetization of the first ferromagnetic layer 1. The spin Hall effect is a phenomenon in which a spin current is caused in a direction orthogonal to the direction of current flow based on the spin-orbit interaction when current flows. The spin Hall effect is common to the conventional Hall effect in that the moving (moving) electric charge (electron) bends the direction of movement (movement). The conventional Hall effect is that the direction of movement of a charged particle moving in a magnetic field is bent by the Lorentz force. In contrast, in the spin Hall effect, even if there is no magnetic field, as long as the electron moves (as long as the current flows), the direction of movement of the spin will bend.
[0058] For example, when current flows in the x direction of the spin-orbit torque wiring 20, the first spin polarized in the -y direction and the second spin polarized in the +y direction are bent in the z direction due to the spin Hall effect. For example, the first spin polarized in the -y direction is bent from the x direction as the traveling direction to the +z direction, and the second spin polarized in the +y direction is bent from the x direction as the traveling direction to the -z direction.
[0059] The number of electrons in the first spin generated by the spin Hall effect of a non-magnetic body (non-ferromagnetic material) is equal to the number of electrons in the second spin. That is, the number of electrons in the first spin facing the +z direction is equal to the number of electrons in the second spin facing the -z direction. In the movement of the first spin and the second spin in the z direction, the flow of charge cancels each other, so the current is zero. The spin flow without current is particularly called pure spin flow.
[0060] If the flow of electrons of the first spin is represented by J ↑ , the flow of electrons with the second spin is represented by J ↓ , the spin current is represented by J S, then it is defined as J S =J ↑ -J ↓ . Spin Current J S The second spin is generated in the z direction. The second spin is injected from the spin-orbit torque wiring 20 into the first ferromagnetic layer 1 .
[0061] The spin-orbit torque wiring 20 includes an amorphous structure. The spin-orbit torque wiring 20 is composed of an amorphous structure, for example. An amorphous structure is a structure in which the atoms that constitute it do not have a clear crystalline structure. In the electron beam diffraction image of a transmission electron microscope, if no diffraction spots are confirmed, the material can be regarded as an amorphous structure. In addition, in many cases, a material having an amorphous structure cannot confirm a clear peak in X-ray diffraction.
[0062] The amorphous structure constituting the spin-orbit torque wiring 20 is any one of oxide, nitride, and oxynitride. The spin-orbit torque wiring 20 is, for example, any one of metal oxide, metal nitride, and metal oxynitride.
[0063] When the spin-orbit torque wiring 20 has an amorphous structure of any one of metal oxide, metal nitride, and metal oxynitride, ionic bonds between metal ions and oxygen or nitrogen ions and covalent bonds between metal elements exist in the spin-orbit torque wiring 20. When the bonding states between different atoms exist in a mixed state, the symmetry in the spin-orbit torque wiring 20 is destroyed. When the symmetry in the spin-orbit torque wiring 20 is destroyed when observed from the electron propagating the spin-orbit torque wiring 20, a large spin current is generated in the spin-orbit torque wiring 20. As a result, the spin current injected into the first ferromagnetic layer 1 increases, and the reversal current density required for the magnetization reversal of the first ferromagnetic layer 1 can be reduced.
[0064] The metal elements constituting the metal oxide, metal nitride, and metal oxynitride are, for example, non-magnetic heavy metals. The non-magnetic heavy metals have, for example, d electrons or f electrons in the outermost shell. When the spin-orbit torque wiring 20 includes the non-magnetic heavy metal, a strong spin-orbit interaction is generated in the spin-orbit torque wiring 20, and the spin current injected into the first ferromagnetic layer 1 increases.
[0065] The metal elements constituting the metal oxides, metal nitrides and metal oxynitrides are, for example, any one selected from the group consisting of Ti, Cr, Mn, Cu, Mo, Ru, Rh, Hf, Ta, W, Re, Os, Ir, Pt, Au, Pr, Nd, Sm, Eu, Gd, Tb, Dy and Ho.
[0066] The spin-orbit torque wiring 20 is composed of, for example, R 2 Ir 2 O 7An oxide represented by a composition formula of . R in the composition formula is one or more elements selected from the group consisting of Pr, Nd, Sm, Eu, Gd, Tb, Dy and Ho.
[0067] The concentration of oxygen or nitrogen contained in the spin-orbit torque wiring 20 is, for example, lower than the concentration of oxygen or nitrogen in the stoichiometric composition obtained from the cations constituting the spin-orbit torque wiring 20. For example, when the cations are R and Ir, the stoichiometric composition is R 2 Ir 2 O 7 In this case, the spin-orbit torque wiring 20 may also be an oxygen-deficient R 2 Ir 2 O 7-x Here, an example of oxide is shown, but in the case of nitride, nitrogen deficiency may be possible, and in the case of oxynitride, oxygen deficiency or nitrogen deficiency may be possible. When oxygen deficiency or nitrogen deficiency occurs, the conduction carriers in the spin-orbit torque wiring 20 increase, and the resistance of the spin-orbit torque wiring 20 can be reduced.
[0068] The oxygen or nitrogen concentration of the first surface S1 of the spin-orbit torque wiring 20 may be different from the oxygen or nitrogen concentration of the second surface S2, for example. When the oxygen or nitrogen concentration of the first surface S1 and the second surface S2 are different, the symmetry within the spin-orbit torque wiring 20 can be destroyed, and the reversal current density required for the magnetization reversal of the first ferromagnetic layer 1 can be reduced. The first surface S1 is the surface of the spin-orbit torque wiring 20 close to the first ferromagnetic layer 1 side. The second surface S2 is the surface opposite to the first surface S1.
[0069] The oxygen or nitrogen concentration of the second surface S2 may be higher than that of the first surface S1, for example. For example, the oxygen or nitrogen concentration may gradually decrease from the second surface S2 toward the first surface S1. The portion with low oxygen or nitrogen concentration has a large amount of oxygen deficiency or nitrogen deficiency, and the write current flows easily. When the amount of write current flowing near the first surface S1 close to the first ferromagnetic layer 1 increases, the spin injected into the first ferromagnetic layer 1 increases.
[0070] In addition, for example, the oxygen or nitrogen concentration may be maximum or minimum at any position between the second surface S2 and the first surface S1. Since the oxygen or nitrogen concentrations in the second surface S2 and the first surface S1 are different, the symmetry is destroyed, more spin currents are generated, and the reversal current can be reduced. In addition, the oxygen or nitrogen concentration of the first surface S1 may be higher than the oxygen or nitrogen concentration of the second surface S2, for example. This is because the resistance of the first surface S1 of the spin-orbit torque wiring 20 increases due to oxygen and nitrogen, resulting in a higher spin resistance. Since the spin resistance increases, the amount of the spin current injected into the first ferromagnetic layer 1 that returns to the spin-orbit torque wiring 20 can be suppressed, and the magnetization reversal of the first ferromagnetic layer 1 can be easily and efficiently generated by the injected spin current.
[0071] In addition, in any direction within the plane, the oxygen or nitrogen concentration of the spin-orbit torque wiring 20 may be different between the center C and the side S3. For example, the oxygen or nitrogen concentration may be different between the center C and the side S3 in the x direction. When the symmetry in the x direction is also broken, a larger spin current is generated in the spin-orbit torque wiring 20, which can further reduce the reversal current density required for the magnetization reversal of the first ferromagnetic layer 1. Here, an example in which the oxygen or nitrogen concentration is different in the x direction is shown, but the oxygen or nitrogen concentration may also be different in the y direction.
[0072] The resistivity of the spin-orbit torque wiring 20 is, for example, greater than 1 mΩ·cm. In addition, the resistivity of the spin-orbit torque wiring 20 is, for example, less than 10 mΩ·cm. When the resistivity of the spin-orbit torque wiring 20 is high, a high voltage can be applied to the spin-orbit torque wiring 20. When the potential of the spin-orbit torque wiring 20 becomes high, spins can be efficiently supplied from the spin-orbit torque wiring 20 to the first ferromagnetic layer 1. In addition, by having a certain conductivity or more of the spin-orbit torque wiring 20, a current path flowing along the spin-orbit torque wiring 20 can be ensured, and a spin current accompanied by a spin Hall effect can be efficiently generated.
[0073] The thickness of the spin-orbit torque wiring 20 is, for example, not less than 4 nm. The thickness of the spin-orbit torque wiring 20 may be, for example, not more than 20 nm.
[0074] The stacked body 10 is connected to the spin-orbit torque wiring 20. For example, the stacked body 10 is stacked on the spin-orbit torque wiring 20. Another layer may be provided between the stacked body 10 and the spin-orbit torque wiring 20.
[0075] The resistance value of the stacked body 10 in the z direction changes when spins are injected from the spin-orbit torque wiring 20 into the stacked body 10 (first ferromagnetic layer 1 ).
[0076] The stacked body 10 is sandwiched between the spin-orbit torque wiring 20 and the electrode E1 (see Figure 2 ). The stack 10 is a columnar body. The shape of the stack 10 when viewed from the z direction is, for example, circular, elliptical, or quadrilateral. The side surface of the stack 10 is, for example, inclined relative to the z direction.
[0077] The laminate 10 includes, for example, a first ferromagnetic layer 1, a second ferromagnetic layer 2, and a non-magnetic layer 3. The first ferromagnetic layer 1 is in contact with, for example, a spin-orbit torque wiring 20. The spin-orbit torque wiring 20 is, for example, laminated on the first ferromagnetic layer 1. Spins are injected from the spin-orbit torque wiring 20 into the first ferromagnetic layer 1. The magnetization of the first ferromagnetic layer 1 is subjected to a spin-orbit torque (SOT) due to the injected spins, and the orientation direction changes. The first ferromagnetic layer 1 and the second ferromagnetic layer 2 sandwich the non-magnetic layer 3 in the z direction.
[0078] The first ferromagnetic layer 1 and the second ferromagnetic layer 2 each have magnetization. When a predetermined external force is applied, the magnetization of the second ferromagnetic layer 2 is less likely to change its orientation direction than the magnetization of the first ferromagnetic layer 1. The first ferromagnetic layer 1 is sometimes referred to as a magnetization free layer, and the second ferromagnetic layer 2 is sometimes referred to as a magnetization fixed layer or a magnetization reference layer. Figure 3 The stack 10 shown has a fixed magnetization layer located closer to the substrate Sub than the free magnetization layer, which is called a bottom pin structure. The resistance value of the stack 10 changes depending on the relative angle of magnetization between the first ferromagnetic layer 1 and the second ferromagnetic layer 2 sandwiching the nonmagnetic layer 3.
[0079] The first ferromagnetic layer 1 and the second ferromagnetic layer 2 include a ferromagnetic material. The ferromagnetic material is, for example, a metal selected from the group consisting of Cr, Mn, Co, Fe, and Ni, an alloy containing one or more of these metals, an alloy containing these metals and at least one element of B, C, and N. The ferromagnetic material is, for example, Co-Fe, Co-Fe-B, Ni-Fe, Co-Ho alloy, Sm-Fe alloy, Fe-Pt alloy, Co-Pt alloy, and CoCrPt alloy.
[0080] The first ferromagnetic layer 1 and the second ferromagnetic layer 2 may also include a Heusler alloy. The Heusler alloy includes an XYZ or X 2 An intermetallic compound of the chemical composition of YZ. X is a transition metal element or a noble metal element of the Co, Fe, Ni, or Cu group in the periodic table, Y is a transition metal of the Mn, V, Cr, or Ti group or an element of X, and Z is a typical element of the IIIA group to the VA group. Heusler alloys, for example, are Co 2 FeSi、Co 2 FeGe、Co 2 FeGa、Co 2 MnSi、Co 2 Mn 1-a Fe a Al b Si 1-b 、Co 2 FeGe 1-c Ga cHeusler alloys have high spin polarizability.
[0081] The non-magnetic layer 3 includes a non-magnetic material. When the non-magnetic layer 3 is an insulator (a tunnel barrier layer), for example, Al 2 O 3 、SiO 2 , MgO and MgAl 2 O 4 In addition to these, materials in which a part of Al, Si, and Mg is replaced by Zn, Be, etc. can also be used. Among them, MgO, MgAl 2 O 4 It is a material that can realize coherent tunneling, so it can efficiently inject spins. When the non-magnetic layer 3 is a metal, as its material, Cu, Au, Ag, etc. can be used. Furthermore, when the non-magnetic layer 3 is a semiconductor, as its material, Si, Ge, CuInSe, etc. can be used. 2 、CuGaSe 2 、Cu(In,Ga)Se 2 wait.
[0082] The laminate 10 may include layers other than the first ferromagnetic layer 1, the second ferromagnetic layer 2, and the nonmagnetic layer 3. For example, an underlayer may be included between the spin-orbit torque wiring 20 and the second ferromagnetic layer 2. The underlayer improves the crystallinity of each layer constituting the laminate 10. In addition, for example, a cap layer may be included on the uppermost surface of the laminate 10.
[0083] In addition, the laminate 10 may be provided with a ferromagnetic layer via a spacer layer on the surface of the second ferromagnetic layer 2 opposite to the non-magnetic layer 3. The second ferromagnetic layer 2, the spacer layer, and the ferromagnetic layer form a synthetic antiferromagnetic structure (SAF structure). The synthetic antiferromagnetic structure is composed of two magnetic layers sandwiching a non-magnetic layer. The second ferromagnetic layer 2 is antiferromagnetically coupled with the ferromagnetic layer, so that the coercive force of the second ferromagnetic layer 2 becomes larger than that of the case without the ferromagnetic layer. The ferromagnetic layer is, for example, IrMn, PtMn, etc. The spacer layer, for example, contains at least one selected from the group consisting of Ru, Ir, and Rh.
[0084] When viewed from the z direction, the electrode E1 is located at a position overlapping the stack 10. The electrode E1 is connected to the readout wiring RL. When viewed from the z direction, the electrode E2 and the electrode E3 are connected to the spin-orbit torque wiring 20 at a position sandwiching the first ferromagnetic layer 1. The electrode E2 is connected to the write wiring WL, and the electrode E3 is connected to the common wiring CL. Other layers may also be provided between the electrode E2 and the spin-orbit torque wiring 20, and between the electrode E3 and the spin-orbit torque wiring 20. The electrodes E1, E2, and E3 are, for example, conductors that electrically connect the switch element to the magnetoresistive effect element 100. The electrodes E1, E2, and E3 are all conductive.
[0085] The insulating layer 91 is located at the same level as the electrode E1. The insulating layer 92 is located at the same level as the stack 10. The insulating layer 92 covers the side of the stack 10. The insulating layer 93 is located at the same level as the spin-orbit torque wiring 20. The insulating layer 93 covers the side of the spin-orbit torque wiring 20. The portion formed by combining the insulating layer 92 and the insulating layer 93 is called, for example, a first insulating layer. The insulating layer 94 is located at the same level as the electrodes E2 and E3. The insulating layer 94 is in contact with the second surface S2 of the spin-orbit torque wiring 20. The insulating layer 94 is called, for example, a second insulating layer.
[0086] The first insulating layer and the second insulating layer are any one of oxide, nitride, and oxynitride. The first insulating layer and the second insulating layer include the same material as the above-mentioned insulating layer 90. The first insulating layer and the second insulating layer are common to the spin-orbit torque wiring 20 in that they are any one of oxide, nitride, and oxynitride, but are different from the spin-orbit torque wiring 20 in that they have insulating properties.
[0087] The first insulating layer may also contain a metal element constituting the spin-orbit torque wiring. In addition, the second insulating layer may also contain a metal element constituting the spin-orbit torque wiring. For example, when the insulating layer 94 and the spin-orbit torque wiring 20 are made of the same material and the presence or absence of conductivity is different due to the difference in composition ratio, the insulating layer 94 and the spin-orbit torque wiring 20 can be formed simultaneously while changing the composition ratio.
[0088] Next, a method for manufacturing the magnetoresistive effect element 100 is described. The magnetoresistive effect element 100 is formed by a lamination process of each layer and a processing process of processing a part of each layer into a predetermined shape. The lamination of each layer can be performed using a sputtering method, a chemical vapor deposition (CVD) method, an electron beam evaporation method (EB evaporation method), an atomic laser deposition method, etc. The processing of each layer can be performed using photolithography, etc.
[0089] First, impurities are doped at predetermined positions of the substrate Sub to form a source S and a drain D. Next, a gate insulating film GI and a gate electrode G are formed between the source S and the drain D. The source S, the drain D, the gate insulating film GI, and the gate electrode G form a transistor Tr. A commercially available semiconductor circuit substrate on which a transistor Tr is formed may be used as the substrate Sub.
[0090] Next, a portion of the insulating layer 90 is formed so as to cover the transistor Tr. Furthermore, an electrode E1 is formed on the insulating layer 90, and its periphery is buried with the insulating layer 91. The write wiring WL and the common wiring CL are formed by stacking the insulating layer 90 to a predetermined thickness, forming a groove in the insulating layer 90, and filling the groove with a conductor.
[0091] Next, a ferromagnetic layer, a nonmagnetic layer, a ferromagnetic layer, and a hard mask layer are sequentially stacked on the insulating layer 91 and one surface of the electrode E1. Next, the hard mask layer is processed into a predetermined shape. The predetermined shape is, for example, the outer shape of the laminate 10. The ferromagnetic layer, the nonmagnetic layer, and the ferromagnetic layer are processed via the hard mask layer to obtain the second ferromagnetic layer 2, the nonmagnetic layer 3, and the first ferromagnetic layer 1. Then, the surrounding of the laminate 10 is buried with the insulating layer 92.
[0092] Next, a layer to be the spin-orbit torque wiring 20 and a hard mask layer are sequentially formed. The layer to be the spin-orbit torque wiring 20 is processed via the hard mask layer, and the spin-orbit torque wiring 20 is obtained.
[0093] The spin-orbit torque wiring 20 is surrounded by the insulating layer 93, and the electrodes E2 and E3 are formed. Through such steps, the magnetoresistance effect element 100 is obtained. Since the spin-orbit torque wiring 20 has an amorphous structure, heating for crystallizing the spin-orbit torque wiring 20 is not required.
[0094] The magnetoresistance effect element 100 of the first embodiment has an amorphous structure in which the spin-orbit torque wiring 20 is any one of metal oxide, metal nitride, and metal oxynitride. Therefore, in the spin-orbit torque wiring 20, the bonding states between different atoms are mixed, and the symmetry in the spin-orbit torque wiring 20 is destroyed. Therefore, the magnetoresistance effect element 100 injects a large amount of spin current into the first ferromagnetic layer 1, and the reversal current density required for the magnetization reversal of the first ferromagnetic layer 1 is small.
[0095] An example of the magnetoresistance effect element 100 according to the first embodiment has been described above, but addition, omission, replacement, and other changes in structure are possible without departing from the gist of the present invention.
[0096] (First Modification)
[0097] Figure 52 is a cross-sectional view of a magnetoresistive effect element 101 according to a first modification. Figure 5 is an xz cross section passing through the center of the spin-orbit torque wiring 20A in the y direction. Figure 5 In, with Figure 3 The same structures are denoted by the same reference numerals, and description thereof will be omitted.
[0098] The magnetoresistance effect element 101 according to the first modification example is different from the magnetoresistance effect element 100 in the structure of the spin-orbit torque wiring 20A.
[0099] The spin-orbit torque wiring 20A has a crystallized layer 21 inside. The crystallized layer 21 is sandwiched between, for example, amorphous layers 22.
[0100] The crystallized layer 21 includes, for example, any one selected from the group consisting of Ta, Al, Mg, Si, Ga, and Ge. The crystallized layer 21 is preferably Ta, Al, and Mg. Ta, Al, and Mg are easily crystallized. The amorphous layer 22 includes the same material as the amorphous structure mentioned in the above-mentioned spin-orbit torque wiring 20. The crystallized layer 21 can be formed by forming the above-mentioned metal film and performing rapid annealing after forming the amorphous layer 22 to be the lower layer.
[0101] When the number of interfaces between different compositions increases inside the spin-orbit torque wiring 20A, the amount of spin injection from the spin-orbit torque wiring 20A to the first ferromagnetic layer 1 increases due to the Raschbach effect.
[0102] The magnetoresistance effect element 101 according to the first modification can obtain the same effects as those of the magnetoresistance effect element 100 according to the first embodiment.
[0103] (Second Modification)
[0104] Figure 6 2 is a cross-sectional view of a magnetoresistive effect element 102 according to a second modification. Figure 6 is an xz cross section passing through the center of the spin-orbit torque wiring 20 in the y direction. Figure 6 In, with Figure 3 The same structures are denoted by the same reference numerals, and description thereof will be omitted.
[0105] Figure 6 The stacked body 10 shown has a top pin structure in which the magnetization fixed layer (second ferromagnetic layer 2) is located farther from the substrate Sub than the magnetization free layer (first ferromagnetic layer 1). The stacked body 10 is located on the spin-orbit torque wiring 20. The spin-orbit torque wiring 20 is located on the electrode E2 and the electrode E3.
[0106] The magnetoresistance effect element 102 of the second modification example is different only in the positional relationship of each structure, and can obtain the same effects as the magnetoresistance effect element 100 of the first embodiment.
[0107] "Second embodiment"
[0108] Figure 7 FIG. 1 is a cross-sectional view of a magnetization rotation element 110 according to the second embodiment. Figure 7 In the embodiment, the magnetization rotation element 110 is replaced by the magnetoresistance effect element 100 of the first embodiment.
[0109] The magnetization rotation element 110, for example, causes light to be incident on the first ferromagnetic layer 1 and evaluates the light reflected by the first ferromagnetic layer 1. When the orientation direction of magnetization changes due to the magnetic Kerr effect, the deflection state of the reflected light changes. The magnetization rotation element 110 can be used as an optical element such as an image display device that utilizes the difference in the deflection state of light.
[0110] Furthermore, the magnetization rotation element 110 can also be used independently as an anisotropic magnetic sensor, an optical element utilizing the magnetic Faraday effect, or the like.
[0111] The spin-orbit torque wiring 20 of the magnetization rotation element 110 includes an amorphous structure, and the amorphous structure is any one of oxide, nitride, and oxynitride.
[0112] The magnetization rotation element 110 of the second embodiment is obtained by removing only the nonmagnetic layer 3 and the second ferromagnetic layer 2 from the magnetoresistance effect element 102 , and can obtain the same effects as those of the magnetoresistance effect element 100 of the first embodiment.
[0113] Thus far, the preferred modes of the present invention have been described based on the first embodiment, the second embodiment, and the modified examples, but the present invention is not limited to these embodiments. For example, the characteristic structures in each embodiment and the modified examples may be applied to other embodiments and the modified examples.
[0114] Description of reference numerals:
[0115] 1: First ferromagnetic layer 2: Second ferromagnetic layer
[0116] 3: Non-magnetic layer 10: Laminated body
[0117] 20, 20A: spin-orbit torque wiring 21: crystallization layer
[0118] 22: amorphous layer 90, 91, 92, 93, 94: insulating layer
[0119] 100, 101, 102: magnetoresistance effect element 110: magnetization rotation element
[0120] 200: Magnetic memory E1, E2, E3: Electrode
[0121] C: Central CL: Common wiring
[0122] RL: Read wiring WL: Write wiring
[0123] S1: First side S2: Second side
[0124] S3: Side
Claims
1. A magnetization rotation element, comprising: Spin-orbit torque wiring, and a first ferromagnetic layer connected to the spin-orbit torque wiring, The spin-orbit torque wiring comprises an amorphous structure, The amorphous structure is any one of oxide, nitride, and oxynitride.
2. The magnetization rotation element according to claim 1, characterized in that: The concentration of oxygen or nitrogen contained in the spin-orbit torque wiring is lower than the concentration of oxygen or nitrogen in the stoichiometric composition obtained from the cations constituting the spin-orbit torque wiring.
3. The magnetization rotation element according to claim 1 or 2, characterized in that: The spin-orbit torque wiring includes an element having d electrons or f electrons.
4. The magnetization rotation element according to any one of claims 1 to 3, characterized in that The oxygen or nitrogen concentration in a first surface of the spin-orbit torque wiring on the side close to the first ferromagnetic layer is different from the oxygen or nitrogen concentration in a second surface on the opposite side to the first surface.
5. The magnetization rotation element according to claim 4, characterized in that: The oxygen or nitrogen concentration of the second surface is higher than the oxygen or nitrogen concentration of the first surface.
6. The magnetization rotation element according to claim 5, characterized in that: The oxygen or nitrogen concentration gradually decreases from the second surface toward the first surface.
7. The magnetization rotation element according to claim 4 or 5, characterized in that: The oxygen or nitrogen concentration is maximum or minimum between the second surface and the first surface.
8. The magnetization rotation element according to any one of claims 1 to 7, characterized in that: In the spin-orbit torque wiring, in any direction within a plane, the oxygen or nitrogen concentration is different between the center and the side surfaces.
9. The magnetization rotation element according to any one of claims 1 to 8, characterized in that: further comprising a first insulating layer covering the first ferromagnetic layer and the side surfaces of the spin-orbit torque wiring, The first insulating layer is any one of oxide, nitride, and oxynitride.
10. The magnetization rotation element according to any one of claims 1 to 9, characterized in that: further comprising a second insulating layer covering a second surface of the spin-orbit torque wiring opposite to the first surface on the side close to the first ferromagnetic layer, The second insulating layer is any one of oxide, nitride, and oxynitride.
11. The magnetization rotation element according to claim 10, characterized in that: The second insulating layer contains a metal element constituting the spin-orbit torque wiring.
12. The magnetization rotation element according to any one of claims 1 to 11, characterized in that: The spin-orbit torque wiring has a crystallized layer inside.
13. The magnetization rotation element according to claim 12, characterized in that: The crystallized layer includes any one selected from the group consisting of Ta, Al, Mg, Si, Ga, and Ge.
14. A magnetoresistance effect element comprising: The magnetization rotation element according to any one of claims 1 to 13, a second ferromagnetic layer, and Non-magnetic layer, The nonmagnetic layer is sandwiched between the first ferromagnetic layer and the second ferromagnetic layer. 15 . A magnetic memory comprising a plurality of the magnetoresistive effect elements according to claim 14 .