Anti-loose rivet integrated forming die and machining method

By designing an integrated mold for anti-loose rivets, the threads and neck breaking grooves are synchronized by using elliptical protrusions and slope structures, the problems of complex processing of traditional anti-loose rivets and waste of materials are solved, efficient production and cost savings are achieved, and the improvement of Product quality and market competitiveness.

CN118875183APending Publication Date: 2024-11-01ZHEJIANG WANYING HENGHUI THREAD TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411169545.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-24
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

The traditional anti-loose rivet processing process is complicated, which increases production costs and material waste, especially the generation of iron filings and low material utilization caused by the truck groove process.

Method used

An integrated molding mold is designed, including a moving plate and a static plate, equipped with a wire rubbing plate and a groove rubbing plate, and synchronous processing of threads and neck grooves is achieved through an elliptical projection and slope structure, reducing process and material waste.

Benefits of technology

It improves production efficiency, reduces production costs, eliminates the problem of "blade"-shaped thread protrusion, significantly improves product quality and qualification rate, meets market demand and creates economic benefits.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118875183A_ABST
    Figure CN118875183A_ABST
Patent Text Reader

Abstract

The anti-loose rivet integrated forming die comprises a movable plate and a static plate, the movable plate and the static plate are each composed of a thread rolling plate and a groove rolling plate, the groove rolling plates are provided with oval protrusions for machining neck breaking grooves, slopes with the angles ranging from 15 degrees to 30 degrees and 10 degrees to 20 degrees are designed at the starting positions of the protrusions, and reverse arc surface transition is arranged between the slopes. According to the die, the thread rolling procedure and the groove rolling procedure are integrated, the production efficiency is improved, and the daily output is increased to more than ten thousand pieces. Meanwhile, the broken neck groove is machined through material deformation, scrap iron generation and material waste are reduced, and the production cost is reduced. In addition, due to the design of the slope and the reverse arc surface, 'blade point '-shaped thread protrusions are effectively avoided, and the product quality and the qualified rate are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of anti-loosening rivet production, and in particular relates to an anti-loosening rivet integrated molding die and a processing method. Background Art

[0002] Anti-loosening rivets, also known as Hook bolts or torsion shear bolts, are a special fastener widely used in high-strength fastening scenarios. The product is mainly composed of four parts: rivet head, thread, neck groove and tail. Its working principle is to drive the rivet into the part that needs to be fixed, use a high-tensile bolt fixing machine to fix the nut or fixing on the thread, and then break the rivet tail at the neck groove to achieve permanent fixation of the fastener. Anti-loosening rivets play an important role in fixing scenarios such as steel construction due to their high strength and the characteristics of not loosening after fixing.

[0003] There are several significant problems in the traditional processing of anti-loosening rivets. First, the processing procedures are complicated, including two main processes: thread rolling and grooving. This multi-process production method not only increases production costs, but also reduces production efficiency. Secondly, the grooving process itself has limitations. In particular, during the grooving process, the workpiece needs to undergo additional cutting steps, which will generate a large amount of iron chips. These iron chips not only increase the difficulty of subsequent processing, but also lead to waste of raw materials and reduce the utilization rate of raw materials. Therefore, how to simplify the processing procedures, improve production efficiency and reduce material waste has become an urgent problem to be solved in the current field of anti-loosening rivet processing. Summary of the invention

[0004] In view of the fact that there are multiple processes in the traditional anti-loosening rivet processing, especially the groove turning process, which not only increases the production cost but also leads to significant waste of materials, the present invention aims to provide a processing die and a processing method for the integrated forming of the thread and groove of the anti-loosening rivet. Through this invention, it is intended to reduce the production process, improve the processing efficiency, reduce the waste of materials, and achieve the goal of reducing costs and increasing efficiency.

[0005] The technical solution of the present invention is achieved in this way:

[0006] The integrated forming die for anti-loosening rivets comprises a movable plate and a stationary plate, and is characterized in that the movable plate and the stationary plate are both provided with a thread rolling plate and a groove rolling plate, the thread rolling plate is provided with a thread rolling pattern, the groove rolling plate is provided with an elliptical protrusion for processing the anti-loosening rivet neck groove, and the elliptical protrusion has two slopes extending outward at the starting point of the workpiece processing.

[0007] In the anti-loosening rivet integrated forming die of the present invention, the angle of the first slope is 15° to 30°, and the angle of the second slope is 10° to 20°.

[0008] In the anti-loosening rivet integrated forming die of the present invention, a reverse arc surface transition is provided between the first slope and the second slope, and the radius R of the reverse arc surface is between 30 mm and 50 mm.

[0009] In the anti-loosening rivet integrated forming die of the present invention, the thread rolling plate and the groove rolling plate are detachably connected and are fixedly mounted on the thread rolling machine by clamping with a clamp.

[0010] In the anti-loosening rivet integrated forming die of the present invention, the length of the movable plate is greater than the length of the thread rolling plate to ensure that the anti-loosening rivet can be completely processed.

[0011] In the anti-loosening rivet integrated forming mold of the present invention, the rubbing plate is divided into a feeding area, a forming area and a discharging area, a groove is formed between the elliptical protrusion and the rubbing plate, and the groove is respectively provided with a feeding slope, a forming plane and a discharging slope corresponding to the feeding area, the forming area and the discharging area.

[0012] In the anti-loosening rivet integrated forming mold of the present invention, the height of the elliptical protrusion corresponding to the feeding area is lower than the height of the elliptical protrusion corresponding to the forming area, which further ensures the stability of the anti-loosening rivet and the integrity of the workpiece during the processing.

[0013] A method for processing an anti-loosening rivet integrated processing mold, the method comprising the following steps:

[0014] Step 1: placing the anti-loosening rivet blank between the moving plate and the stationary plate of the thread rolling machine, wherein the moving plate and the stationary plate are both composed of a thread rolling plate and a groove rolling plate, and the thread rolling plate and the groove rolling plate are detachably connected to form a whole;

[0015] Step 2: Start the thread rolling machine, so that the moving plate drives the anti-loosening rivet blank to roll on the static plate, and the thread is formed by the extrusion of the thread rolling plate, and the broken neck groove is formed by the elliptical protrusion structure of the groove rolling plate;

[0016] Step 3: Control the moving distance of the moving plate to ensure the synchronous processing of the thread and the broken neck groove until the processing is completed to obtain the finished anti-loosening rivet.

[0017] The anti-loosening rivet integrated forming die and processing method of the present invention have the following beneficial effects:

[0018] 1. Huge commercial success: The processing die and processing method of the integrated forming of the thread and groove of the anti-loosening rivet provided by the present invention greatly improve the production efficiency. Compared with the traditional two processes of thread rolling and groove cutting, the present invention combines the two into one process, so that the daily output of the product is increased from the original one or two hundred pieces to ten thousand pieces a day, which greatly meets the market demand and creates huge economic benefits for the company.

[0019] 2. Significant cost savings: The traditional slotting process will generate a lot of iron filings, resulting in material waste. The present invention realizes the processing of the broken neck groove by material deformation growth, and can adjust the length of the original blank in advance according to the deformation amount to ensure that the length of the finished product after processing meets the standard, reducing material waste, reducing production costs, and improving material utilization.

[0020] 3. Eliminate the blade phenomenon of threads and broken neck grooves: The present invention innovatively designs two slopes with bevel cutting and reverse arc surfaces on the convex structure of the groove plate, completely eliminating the "blade"-shaped thread protrusion problem generated during the processing process, greatly improving product quality and qualified rate. It not only improves product competitiveness, but also establishes a leading image for the company in the industry. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 This is a schematic structural diagram of the anti-loosening rivet integrated molding die of the present invention;

[0022] Figure 2 for Figure 1 Schematic diagram of another motion state;

[0023] Figure 3 for Figure 1 The structural diagram of the middle rubbing groove board;

[0024] Figure 4 for Figure 1 Another structural schematic diagram of the middle rubbing groove board;

[0025] Figure 5 for Figure 4 Left view of

[0026] Figure 6 for Figure 4 Right view of;

[0027] Figure 7 for Figure 4 Stereoscopic image of

[0028] Figure 8 for Figure 6 A magnified schematic diagram of part A;

[0029] Fig. 9 for Figure 1 Schematic diagram of the combination of the middle thread rolling plate and the groove rolling plate;

[0030] Fig.10 It is a schematic diagram of the structure of the anti-loosening rivet of the present invention before and after processing.

[0031] In the accompanying drawings, the components represented by the reference numerals are listed as follows:

[0032] Moving plate, 100; stationary plate, 200; thread rolling plate, 210; groove rolling plate, 220; elliptical protrusion, 221; first slope, 222; second slope, 223; reverse arc surface, 224; groove, 224; feed slope, 2241; forming plane, 2242; discharge slope, 2243; rivet, 300; neck breaking groove, 310. DETAILED DESCRIPTION

[0033] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0034] Example 1

[0035] like Figures 1 to 3 As shown, the integrated molding die of the anti-loosening rivet 300 in this embodiment includes a movable plate 100 and a static plate 200. Both the movable plate 100 and the static plate 200 are composed of a thread rolling plate 210 and a groove rolling plate 220. The thread rolling plate 210 is provided with thread rolling patterns, which include axial threads and lateral threads for forming the threaded portion of the rivet.

[0036] The thread rolling plate 210 and the groove rolling plate 220 are detachably connected and fixed on the thread rolling machine by a clamp. The length of the moving plate 100 is greater than the length of the static plate 200 to ensure that the anti-loosening rivet 300 can be completely processed.

[0037] The thread rolling plate 210 and the groove rolling plate 220 are detachably connected, which is convenient for replacement and maintenance. Specifically, the thread rolling plate 210 and the groove rolling plate 220 are connected by detachable locking such as existing clamps or high-precision bolts. This connection method allows that when a part of the mold (such as the groove rolling plate) is worn or damaged due to long-term processing pressure, only the part needs to be replaced separately, without replacing the entire mold assembly at the same time.

[0038] For example, considering that the thread rolling plate 210 can process about 1,000 screws under normal circumstances, while the groove rolling plate 220 has a lifespan limited to about 500 screws due to more stringent processing conditions. Therefore, after adopting a detachable design, when the groove rolling plate 220 reaches its lifespan limit, the operator can quickly remove it and replace it with a new groove rolling plate 220, while the thread rolling plate 210 can continue to be used until its lifespan is exhausted. This design simplifies the maintenance process of the mold and significantly reduces the additional cost and time expenditure caused by frequent replacement of the entire set of molds. At the same time, the matching accuracy between the thread rolling plate 210 and the groove rolling plate 220 can be flexibly adjusted to further ensure the stability of the processing process and the consistency of product quality.

[0039] The groove plate 220 is provided with an elliptical protrusion 221 for processing the broken neck groove 310 of the anti-loosening rivet 300. The elliptical protrusion 221 has two slopes extending outward at the starting point of workpiece processing: a first slope 222 and a second slope 223.

[0040] Regarding the first slope 222, the deformation direction of the processing area of ​​the broken neck groove 310 can be changed in the initial stage of processing, so that the deformation is biased to the outside, thereby effectively reducing the collision with the deformation force of the thread processing area, and effectively avoiding the generation of "blade"-shaped thread protrusions at the threads and the broken neck groove 310 of the anti-loosening rivet 300, which significantly improves the product qualification rate and reduces the generation of defective products.

[0041] Regarding the second slope 223, its function is to enable the broken neck groove 310 to smoothly transition to the subsequent elliptical protrusion 221 part during the subsequent rolling process, thereby ensuring the continuity and stability of the processing process and avoiding damage to the workpiece due to improper height connection.

[0042] The groove plate 220 is further divided into a feeding area, a forming area and a discharging area. A groove 224 is formed between the elliptical protrusion 221 and the groove plate. The groove 224 is provided with a feeding slope 2241, a forming plane 2242 and a discharging slope 2243 corresponding to the feeding area, the forming area and the discharging area. The height of the elliptical protrusion 221 corresponding to the feeding area is lower than that corresponding to the forming area, ensuring that the rivet blank can smoothly transition when it just enters the groove plate 220, avoiding impact and uneven deformation caused by sudden height changes.

[0043] The feed slope 2241, the molding plane 2242 and the discharge slope 2243 form a trapezoidal cross-section. When feeding, the trapezoidal cross-section gradually guides the blank into the processing state, reducing impact and stress concentration; when molding, the trapezoidal cross-section ensures the stability and uniformity of the processing area; when discharging, the trapezoidal cross-section smoothly sends the workpiece out of the processing area, avoiding deformation or damage caused by sudden unloading. Not only does it improve processing efficiency, but it also significantly improves product quality and stability.

[0044] The setting of the feeding slope 2241 enables the blank to gradually adapt to the processing environment, further reducing the stress concentration caused by sudden force, thereby protecting the workpiece from damage, improving the stability of the initial processing, and reducing the rate of defective products.

[0045] The forming area is the core area of ​​the groove plate 220, where the elliptical protrusion 221 reaches its highest point, and the groove 224 formed between the groove plate and the forming area is used to accurately process the neck-breaking groove 310. The design of the forming plane 2242 ensures that the blank can be evenly stressed during the rolling process, forming the neck-breaking groove 310 that meets the requirements.

[0046] The design of the discharge slope 2243 corresponding to the discharge area allows the processed workpiece to smoothly leave the rubbing plate 220, avoiding deformation or damage caused by uneven force during the discharge process. The existence of the discharge slope 2243 ensures the stability and integrity of the workpiece when leaving the processing area, further improving the qualified rate of the product.

[0047] The method for using the anti-loosening rivet 300 integrated molding die includes the following steps:

[0048] Step 1: Place the original blank of the anti-loosening rivet 300 between the moving plate 100 and the stationary plate 200 of the thread rolling machine, wherein the moving plate 100 and the stationary plate 200 are both composed of a thread rolling plate 210 and a groove rolling plate 220, and the thread rolling plate 210 and the groove rolling plate 220 are detachably connected to form a whole;

[0049] Step 2: Start the thread rolling machine, so that the moving plate 100 drives the anti-loosening rivet 300 blank to roll on the stationary plate 200, and the thread is formed by the extrusion of the thread rolling plate 210, and the broken neck groove 310 is formed by the elliptical protrusion 221 structure of the groove rolling plate 220;

[0050] Step 3: Control the moving distance of the movable plate 100 to ensure synchronous processing of the thread and the broken neck groove 310 until the processing is completed to obtain a finished anti-loosening rivet 300.

[0051] Through the above integrated molding die and method, the original groove turning process is reduced, the processing flow is more compact, the processing efficiency is significantly improved, and the daily output can be increased from the original hundreds of pieces to more than 10,000 pieces. The traditional groove turning process will produce a large amount of iron filings, resulting in material waste. The mold of the present invention realizes the processing of the broken neck groove 310 through material deformation, which reduces material loss and reduces processing costs.

[0052] Example 2

[0053] The difference from the first embodiment is the first slope 222 and the second slope 223, please refer to Figure 4 and Fig. 9 The angle between the first slope 222 and the horizontal plane is 25 degrees, and the angle between the second slope 223 and the horizontal plane is 18 degrees.

[0054] The angle between the first slope 222 and the horizontal plane is 25 degrees. In the initial stage when the anti-loosening rivet 300 blank enters the groove plate 220 for processing, the processing deformation direction of the broken neck groove 310 can be biased to the outside, effectively reducing the direct collision with the thread processing deformation area, and further reducing the risk of "blade"-shaped thread protrusions.

[0055] A reverse arc surface 224 is provided between the first slope 222 and the second slope 223, and the radius R of the reverse arc surface 224 is between 30 mm and 50 mm. This not only makes the processing smoother, but also further reduces the risk of damage to the workpiece due to sudden height changes, and completely eliminates the phenomenon of "blade"-shaped thread protrusions on the threads and the broken neck groove 310 of the anti-loosening rivet 300 during processing.

[0056] In the description of this specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.

[0057] The preferred embodiments of the present invention disclosed above are only used to help illustrate the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the present invention to the specific embodiments described. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.

Claims

1. Anti-loosening rivet integrated molding die, including moving plate and static plate, It is characterized in that The moving plate and the stationary plate are both provided with a thread rolling plate and a groove rolling plate, the thread rolling plate is provided with a thread rolling pattern, the groove rolling plate is provided with an elliptical protrusion for processing the anti-loosening rivet neck breaking groove, and the elliptical protrusion has two slopes extending outwards at the starting point of workpiece processing.

2. The anti-loosening rivet integrated molding die according to claim 1, It is characterized in that The slopes are respectively a first slope and a second slope, wherein the angle of the first slope is 15° to 30°, and the angle of the second slope is 10° to 20°.

3. The anti-loosening rivet integrated molding die according to claim 2, It is characterized in that A reverse arc surface transition is provided between the first slope and the second slope, and the radius R of the reverse arc surface is between 30 mm and 50 mm.

4. The anti-loosening rivet integrated molding die according to claim 1, It is characterized in that The thread rolling plate and the groove rolling plate are detachably connected and are fixedly mounted on the thread rolling machine by clamping with a clamp.

5. The anti-loosening rivet integrated molding die according to claim 1, It is characterized in that The rubbing groove plate is divided into a feeding area, a forming area and a discharging area. A groove is formed between the elliptical protrusion and the rubbing groove plate. The groove is respectively provided with a feeding slope, a forming plane and a discharging slope corresponding to the feeding area, the forming area and the discharging area.

6. The anti-loosening rivet integrated molding die according to claim 5, It is characterized in that The height of the elliptical protrusion corresponding to the feeding area is lower than the height of the elliptical protrusion corresponding to the forming area.

7. A processing method for an integrated processing mold for anti-loosening rivets, It is characterized in that The method comprises the following steps: Step 1: placing the anti-loosening rivet blank between the moving plate and the stationary plate of the thread rolling machine, wherein the moving plate and the stationary plate are both composed of a thread rolling plate and a groove rolling plate, and the thread rolling plate and the groove rolling plate are detachably connected to form a whole; Step 2: Start the thread rolling machine, so that the moving plate drives the anti-loosening rivet blank to roll on the static plate, and the thread is formed by the extrusion of the thread rolling plate, and the broken neck groove is formed by the elliptical protrusion structure of the groove rolling plate; Step 3: Control the moving distance of the moving plate to ensure the synchronous processing of the thread and the broken neck groove until the processing is completed to obtain the finished anti-loosening rivet.