High-transmittance white toughened glass

By using sandwich structure and materials such as high-purity quartz sand and nano-oxides in tempered glass, the problems of insufficient impact resistance and light transmittance of traditional tempered glass are solved, and high light transmittance and environmentally friendly production processes are achieved, reducing the environment Pollution has good economic and social benefits.

CN118876523APending Publication Date: 2024-11-01HUIZHOU WANHE GLASS TECH CO LTD

Patent Information

Application Number
CN202410962663.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-18
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

Traditional tempered glass has shortcomings in impact resistance and light transmittance, and there are many chemical pollutants used in the production process, resulting in environmental pollution.

Method used

High-transparent white glass tempered glass with sandwich structure, using ultra-white tempered glass substrate, PVB film, explosion-proof film and nano-oxide materials, and by adding ceria and anti-ultraviolet additives to the glass substrate, the glass is improved. light transmittance and impact resistance and optimized in the process to reduce the use of contaminants.

Benefits of technology

It improves the light transmittance, impact resistance and durability of glass, reduces the use of sodium nitrate and arsenic, avoids environmental pollution, and has good economic and social benefits.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118876523A_ABST
    Figure CN118876523A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of glass, in particular to high-transmittance white glass tempered glass which comprises at least two glass substrates 3, an explosion-proof film 2 and a light-transmitting film 1, the glass substrates 3 are ultra-white tempered glass, an interlayer 4 is arranged between the glass substrates 3 and is a PVB film, and nano oxide, polyurethane and an anti-ultraviolet aid are added into the PVB film to improve the light transmittance of the PVB film. The glass substrate 3 is made of high-purity quartz sand, a proper amount of cerium dioxide is added into raw materials of the glass substrate 3, the quality of the glass is greatly improved, the glass is more environmentally friendly, the light-transmitting film 1 comprises a silica gel layer, a PET layer and an inorganic nano layer, the glass substrate 3 is ultra-white tempered glass, the interlayer 4 structure is adopted, and the glass substrate 3 is more transparent. Compared with the prior art, the impact resistance of the glass is improved, various components are added into the interlayer 4 to improve the light transmittance of the interlayer 4, cerium dioxide is added into the glass substrate 3 to improve the light transmittance of the glass substrate 3, chemical pollution is reduced, and the glass has high economic benefits and social benefits.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of glass, in particular to a high-transmittance white tempered glass. Background Art

[0002] Glass is an inorganic non-metallic material, mainly composed of some quartz sand and silicate raw materials with some reinforcing agents added. It is also an amorphous solid with irregular structure. It is widely used in buildings to block wind and let light in. The properties of the glass can be changed by controlling the content of various added metal elements or non-metallic elements in the glass. Glass of various colors can be produced, and fully transparent glass can also be produced. Now there are more and more types of glass, and the uses and requirements of glass are different in different industries and applications.

[0003] Traditional tempered glass technology generally uses a single-layer glass substrate to ensure sufficient light transmittance. Laminated tempered glass has a lower light transmittance due to the interlayer setting. The impact resistance of single-layer tempered glass is not high enough, and the service life is not enough. In addition, many substances that are prone to chemical pollution are used in the production process. Therefore, it is necessary to study a tempered glass with high transparency and higher performance. Summary of the invention

[0004] In order to solve the above problems, the present invention provides a high-transmittance white tempered glass, which adopts a sandwich structure and performs process optimization to maintain a high light transmittance of the interlayer and improve the comprehensive performance of the glass, and the process is more environmentally friendly.

[0005] In order to achieve the above object, the present invention adopts the following technical solutions: A high-transmittance white tempered glass comprises at least two glass substrates, an explosion-proof film and a light-transmitting film, wherein the glass substrates are ultra-white tempered glass, an interlayer is arranged between the glass substrates, the interlayer is a PVB film, nano-oxides, polyurethane and anti-ultraviolet additives are added to the PVB film to improve the light transmittance of the PVB film, the glass substrates are made of high-purity quartz sand, and an appropriate amount of cerium dioxide is added to the raw materials of the glass substrates.

[0006] Optionally, in one embodiment of the present invention, the added amount of cerium dioxide is 0.1%-0.5% to have a positive effect on the glass.

[0007] Optionally, in one embodiment of the present invention, the nano-oxide is any one of titanium dioxide or silicon dioxide, and the addition amount of the nano-oxide is 0.1%-1%.

[0008] Optionally, in one embodiment of the present invention, the thickness of the interlayer is ≤0.4 mm.

[0009] Optionally, in one embodiment of the present invention, the purity of the quartz sand is above 99.5%.

[0010] Optionally, in one embodiment of the present invention, the thickness of the glass substrate is 2 mm-6 mm.

[0011] Optionally, in one embodiment of the present invention, the added amount of the anti-ultraviolet additive is 0.4%-0.7%.

[0012] Optionally, in one embodiment of the present invention, the explosion-proof film is a PET explosion-proof film, to which anti-ultraviolet agents and antioxidants are added to improve weather resistance and anti-aging properties, and the surface of the explosion-proof film is corona treated to form an oxide layer, and the thickness of the explosion-proof film is ≤0.4mm.

[0013] Beneficial effects of the present invention The high-transmittance white tempered glass of the present invention adopts an interlayer structure to improve the impact resistance of the glass. Considering that the interlayer will reduce the light transmittance, multiple substances are added during the preparation of the interlayer to improve the light transmittance and bonding strength of the interlayer, and improve the smoothness and anti-aging performance of its surface. Cerium dioxide is added during the preparation of the glass substrate to play the role of a clarifier, improve the light transmittance of the glass, make the color more uniform, and also help to reduce bubbles and impurities in the glass. It can also play a role in ultraviolet absorption and improve the durability and stability of the glass. Compared with the traditional process, the amount of sodium nitrate used can be reduced in large quantities, and white arsenic can be replaced to avoid the pollution of white arsenic. It can also replace arsenic oxide to avoid the pollution of arsenic to the environment and glass, and has good economic and social benefits. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art are briefly introduced below.

[0015] Figure 1 This is a schematic diagram of the cross-sectional structure of a high-transmittance clear tempered glass according to Example 1 of the present invention.

[0016] Reference numerals: light-transmitting film 1, explosion-proof film 2, glass substrate 3, interlayer 4. DETAILED DESCRIPTION

[0017] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present invention. However, the present invention can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present invention, so the present invention is not limited by the specific embodiments disclosed below.

[0018] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.

[0019] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.

[0020] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0021] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" or "below" a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.

[0022] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "upper", "lower", "left", "right" and similar expressions used herein are for illustrative purposes only and are not intended to be the only implementation method.

[0023] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the specific implementation mode, structure, characteristics and effects of the present invention are described in detail below in combination with the accompanying drawings and preferred embodiments. Example 1

[0024] In order to produce tempered glass with better comprehensive performance, the traditional production process was improved and a high-transmittance white tempered glass was studied. The specific plan is as follows: like Figure 1 As shown, a high-transmittance white tempered glass includes at least two glass substrates 3, an explosion-proof film 2, and a light-transmitting film 1. The glass substrates 3 are ultra-white tempered glass. An interlayer 4 is provided between the glass substrates 3. The interlayer 4 is a PVB film. Nano-oxides, polyurethane and anti-ultraviolet additives are added to the PVB film to improve the light transmittance of the PVB film. The glass substrates 3 are made of high-purity quartz sand, and an appropriate amount of cerium dioxide is added to the raw materials of the glass substrates 3.

[0025] This solution uses ultra-clear glass for tempering to provide high strength and high light transmittance for the final tempered glass.

[0026] The glass structure of this solution is provided with two identical glass substrates 3, which are, from the outside to the inside, a light-transmitting film 1, an explosion-proof film 2, and a glass substrate 3, and the structures of the two glass substrates 3 are the same; The thickness of the glass substrate 3 is 2 mm-6 mm. The thickness of the glass substrate 3 in this solution is 4 mm. The tempered glass produced is used in buildings. In application scenarios with relatively low strength requirements, a 2 mm glass substrate 3 can be used.

[0027] The PVB film is located between two glass substrates 3, and the thickness of the interlayer 4 is controlled to be ≤0.4mm. In this solution, the thickness of the interlayer 4 is 0.4mm. The setting of the interlayer 4 can absorb the impact energy when the glass is impacted by external force, effectively preventing the glass from breaking, and even if it breaks, it will not fall off and hurt people.

[0028] The addition amount of cerium dioxide is 0.1%-0.5%, which has a positive effect on the glass. When the addition amount of cerium dioxide is 0.5%, the clarification effect is best. Cerium dioxide can replace part of the sodium sulfate as a clarifier, increase the transparency, improve the strength and water resistance of the glass, and reduce the pollution of sulfur dioxide to the environment and glass.

[0029] Cerium dioxide has excellent decolorization ability and can oxidize low-valent iron into ferric oxide. The coloring ability of trivalent iron is only one-tenth of that of divalent iron. During use, it can reduce selenium-cobalt by 70%-80%, reduce the coloring of glass, and thus improve the light transmittance of glass. Cerium dioxide decomposes and releases oxygen at high temperature, which promotes the growth and upward discharge of bubbles in the glass liquid. Therefore, it helps to reduce bubbles and impurities in the glass liquid and improve the transparency and quality of the glass. Cerium dioxide can absorb ultraviolet rays, thereby effectively protecting the glass, reducing ultraviolet erosion and damage, and improving the durability and stability of the glass. Cerium dioxide has a higher oxidation potential and can reduce the amount of sodium nitrate used by 20%-40%, making the production of tempered glass more environmentally friendly and with good economic and social benefits.

[0030] The nano oxide is any one of titanium dioxide or silicon dioxide, and the addition amount of the nano oxide is 0.1%-1%. The scheme of adding silicon dioxide is adopted in this scheme, and the addition amount is 0.5%. The addition of silicon dioxide can reduce the scattering and absorption of light during the propagation process and improve the transmittance of light.

[0031] The purity of quartz sand is above 99.5%. High-purity quartz sand can ensure that the glass has better transparency, optical stability and mechanical properties. In this solution, the raw materials for preparing the glass substrate 3 can refer to the raw materials for preparing tempered glass in the prior art.

[0032] In this embodiment, when the glass substrate 3 is prepared, any one of lithium peroxide, barium oxide, magnesium oxide or boron oxide with a small ion radius is also introduced to change the brittleness of the glass and further improve the strength of the glass. The addition of cerium dioxide can reduce the thermal expansion coefficient and elastic modulus of the glass and improve its temperature difference resistance.

[0033] The addition amount of anti-UV additive is 0.4%-0.7%. Adding an appropriate amount of anti-UV additive in the preparation of PVB film can extend the service life of PVB film and improve its anti-aging performance. In PVB film, polyurethane forms a dense film on the surface through spraying or sol-gel method to improve the surface smoothness.

[0034] The explosion-proof film 2 is a PET explosion-proof film 2, to which anti-ultraviolet agents and antioxidants are added to improve weather resistance and anti-aging. The surface of the explosion-proof film 2 is corona treated to form an oxidation layer, making the explosion-proof layer more wear-resistant and scratch-resistant, and helping to ensure high light transmittance. The thickness of the explosion-proof film is ≤0.4mm.

[0035] The tempered glass of this scheme adopts an interlayer 4 structure to improve the impact resistance of the glass. Considering that the interlayer 4 will reduce the light transmittance, a variety of substances are added during the preparation of the interlayer 4 to improve the light transmittance and bonding strength of the interlayer 4, and improve its surface smoothness and anti-aging performance. Cerium dioxide is added during the preparation of the glass substrate 3 to act as a clarifier, improve the light transmittance of the glass, make the color more uniform, and also help to reduce bubbles and impurities in the glass. It can also play a role in ultraviolet absorption and improve the durability and stability of the glass. Compared with traditional processes, it can reduce the amount of sodium nitrate used, and can replace white arsenic to avoid white arsenic pollution. It can also replace arsenic oxide to avoid arsenic pollution to the environment and glass, and has good economic and social benefits. Example 2

[0036] In this embodiment, the overall structure of the tempered glass is basically the same, and the glass substrate 3 is a hollow structure filled with inert gas to improve the sound insulation and heat insulation performance of the tempered glass.

[0037] The directions or positional relationships indicated by terms such as "center", "longitudinal", "lateral", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside" and "outside" are based on the directions or positional relationships shown in the accompanying drawings. They are merely simplified descriptions for the convenience of describing the present invention, and do not indicate or imply that the devices or elements referred to must have a specific direction, be constructed and operated in a specific direction. Therefore, they should not be understood as limitations on the protection content of the present invention.

[0038] The above are only preferred embodiments of the present invention, and are not intended to limit the present invention in any form. Although the present invention has been disclosed as above in the form of preferred embodiments, it is not intended to limit the present invention. Any technical personnel in the field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any brief modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of the technical solution of the present invention.

Claims

1. A high-transmittance clear tempered glass, characterized in that: It includes at least two glass substrates, an explosion-proof film, and a light-transmitting film. The glass substrates are ultra-white tempered glass. An interlayer is arranged between the glass substrates, and the interlayer is a PVB film. Nano oxides, polyurethane and anti-ultraviolet additives are added to the PVB film to improve the light transmittance of the PVB film. The glass substrates are made of high-purity quartz sand, and an appropriate amount of cerium dioxide is added to the raw materials of the glass substrates.

2. The high-transmittance clear tempered glass according to claim 1, characterized in that: The added amount of cerium dioxide is 0.1%-0.5% to have a positive effect on the glass.

3. The high-transmittance clear tempered glass according to claim 1, characterized in that: The nano-oxide is any one of titanium dioxide or silicon dioxide, and the addition amount of the nano-oxide is 0.1%-1%.

4. The high-transmittance clear tempered glass according to claim 1, characterized in that: The thickness of the interlayer is ≤0.4 mm.

5. The high-transmittance clear tempered glass according to claim 1, characterized in that: The purity of the quartz sand is above 99.5%.

6. The high-transmittance clear tempered glass according to claim 1, characterized in that: The thickness of the glass substrate is 2 mm to 6 mm.

7. The high-transmittance clear tempered glass according to claim 1, characterized in that: The added amount of the anti-ultraviolet additive is 0.4%-0.7%.

8. The high-transmittance clear tempered glass according to claim 1, characterized in that: The explosion-proof film is a PET explosion-proof film, to which anti-ultraviolet agents and antioxidants are added to improve weather resistance and anti-aging properties, and the surface of the explosion-proof film is subjected to corona treatment to form an oxide layer, and the thickness of the explosion-proof film is ≤0.4 mm.

Citation Information

Patent Citations

  • Ultraviolet-resistant ultra-white rolled glass with high transmittance and production process

    CN108516680A

  • Long-acting wear-resistant antifogging coating material liquid, and preparation method and application thereof

    CN113372773A

  • Bulletproof glass for cars

    CN203236794U

  • Glass laminate construction for optimized breakage performance

    WO2013181505A1

Cited By

  • High-refractive-index glass bead for road marking and preparation method of high-refractive-index glass bead

    CN121627313A

  • High refractive index glass microbeads for road marking and method for preparing the same

    CN121627313B