Optical laminate, lens portion, and display method
By using optical laminates with specific thickness and refractive index characteristics in VR goggles, combined with a resin curing layer and anti-reflective function, the problems of lightweight VR goggles and insufficient visual recognition have been solved, achieving both lightweight design and improved visual effects.
Patent Information
- Application Number
- CN202380027343.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-12-28
- Filing Date
- 2023-03-08
- Publication Date
- 2024-11-01
AI Technical Summary
Existing VR goggles suffer from issues such as lightweight design and insufficient visual recognition.
An optical laminate comprising a substrate and a surface treatment layer and a phase retardation component, including a first and a second phase retardation layer, an adhesive layer with a thickness of 0.5 μm or more and 1.3 μm or less, a laminate surface smoothness of 0.7 arcmin or less, a resin curing layer and an anti-reflective surface treatment layer, refractive index characteristics satisfying a specific relationship, and a transmittance of 93% or more.
It achieves lightweight design and improved visual recognition of VR goggles, ensures the smoothness and durability of the lens, prevents light leakage and cracks, and improves image clarity and aesthetics.
Smart Images

Figure CN118891566A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to an optical layered body, a lens unit and a display method. Background Art
[0002] Image display devices represented by liquid crystal display devices and electroluminescent (EL) display devices (e.g., organic EL display devices) are rapidly becoming popular. In image display devices, optical components such as polarization components and phase difference components are generally used to realize image display and improve image display performance (e.g., refer to Patent Document 1).
[0003] In recent years, new uses for image display devices have been developed. For example, goggles with displays (VR goggles) for realizing Virtual Reality (VR) have begun to be commercialized. Since the use of VR goggles in various scenarios has been studied, it is expected that they will be lightweight and have improved visual recognition. Lightweighting can be achieved, for example, by thinning the lenses used for VR goggles. On the other hand, it is also expected to develop optical components suitable for display systems using thin lenses.
[0004] Prior art literature
[0005] Patent Literature
[0006] Patent Document 1: Japanese Patent Application Publication No. 2021-103286 Summary of the invention
[0007] Problems to be solved by the invention
[0008] In view of the above circumstances, a main object of the present invention is to provide an optical layered body capable of achieving weight reduction and improved visibility of VR goggles.
[0009] Solutions to the problem
[0010] 1. An optical laminate according to an embodiment of the present invention comprises a laminate film having a substrate and a surface-treated layer, and a phase difference component, wherein the substrate of the laminate film is arranged adjacent to the phase difference component, and the phase difference component sequentially comprises a first phase difference layer, an adhesive layer and a second phase difference layer, and the thickness of the adhesive layer is greater than or equal to 0.5 μm and less than or equal to 1.3 μm.
[0011] 2. The optical layered body described in 1 above may have a layered body smoothness of 0.7 arcmin or less.
[0012] 3. In the optical layered body described in 1 or 2 above, the adhesive layer may be a cured layer of a resin.
[0013] 4. In the optical layered body according to any one of 1 to 3 above, the surface smoothness of the layered film may be 0.5 arcmin or less.
[0014] 5. In the optical layered body according to any one of 1 to 4 above, the substrate of the layered film may contain a (meth)acrylic resin.
[0015] 6. In the optical layered body according to any one of 1 to 5 above, the surface treatment layer of the layered film may have an antireflection function.
[0016] 7. In the optical layered body described in any one of 1 to 6 above, the first retardation layer may exhibit a refractive index characteristic of nx>ny≥nz and may satisfy the relationship of Re(450)<Re(550)<Re(650).
[0017] 8. In the optical layered body according to any one of 1 to 7 above, the second retardation layer may exhibit a refractive index characteristic of nz>nx≥ny.
[0018] 9. The Y value of the visibility-corrected single body transmittance of the optical layered body according to any one of 1 to 8 above may be 93% or more.
[0019] 10. A lens unit according to an embodiment of the present invention is used in a display system for displaying an image to a user, wherein the lens unit comprises:
[0020] A reflective polarizing member that reflects light emitted forward from a display surface of a display element that displays an image and that passes through the polarizing member and the first λ / 4 member;
[0021] A first lens portion disposed on an optical path between the display element and the reflective polarization member;
[0022] a half mirror disposed between the display element and the first lens portion, transmitting light emitted from the display element and reflecting light reflected by the reflective polarizing member toward the reflective polarizing member;
[0023] A second lens portion disposed in front of the reflective polarization element; and
[0024] The optical layered body according to any one of 1 to 9 above, which is disposed on an optical path between the half mirror and the reflective polarization member.
[0025] 11. The display method according to the embodiment of the present invention has the following features:
[0026] a step of allowing the light of the display image emitted through the polarization element and the first λ / 4 element to pass through the half mirror and the first lens portion;
[0027] a step of allowing the light that has passed through the half mirror and the first lens portion to pass through the optical layered body described in any one of 1 to 9 above;
[0028] A step of reflecting the light after passing through the optical stack toward the half mirror at a reflective polarizing member;
[0029] A step of allowing the light reflected by the reflective polarization member and the half mirror to pass through the reflective polarization member via the optical stack; and
[0030] A step of allowing the light transmitted through the reflective polarization member to pass through a second lens unit.
[0031] Effects of the Invention
[0032] According to the optical layered body of the embodiment of the present invention, it is possible to achieve weight reduction and improvement of visibility of VR goggles. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] Figure 1 This is a schematic diagram showing a schematic configuration of a display system according to one embodiment of the present invention.
[0034] Figure 2 It is shown Figure 1 A schematic cross-sectional view showing an example of details of a lens unit of the display system shown.
[0035] Figure 3 This is a schematic perspective view showing an example of a multilayer structure included in a reflective polarizing film.
[0036] Explanation of symbols
[0037] 2 Display system
[0038] 4 Lens section
[0039] 12 Display components
[0040] 14 Reflective polarizing element
[0041] 16. First lens unit
[0042] 18 Half Mirror
[0043] 20 first phase difference member
[0044] 22. Second phase difference member
[0045] 24 Second lens unit
[0046] 28 Absorption type polarization element
[0047] 30 third phase difference member
[0048] 31 First protection member
[0049] 32. Second protective member
[0050] 41 Adhesive layer
[0051] 42 Adhesive layer
[0052] 43 Adhesive layer
[0053] 44 Adhesive layer
[0054] 45 Adhesive layer
[0055] 46 Adhesive layer
[0056] 50 Adhesive layer
[0057] 100 first laminated part (optical laminate)
[0058] 200 Second lamination unit DETAILED DESCRIPTION
[0059] Hereinafter, the embodiments of the present invention will be described with reference to the accompanying drawings, but the present invention is not limited to these embodiments. In order to explain more clearly, the drawings sometimes schematically show the width, thickness, shape, etc. of each part compared with the embodiments, but this is only an example and does not limit the interpretation of the present invention. In addition, with respect to the drawings, the same or equivalent elements are sometimes marked with the same symbols, and repeated descriptions are omitted.
[0060] (Definition of Terms and Symbols)
[0061] The definitions of terms and symbols in this specification are as follows.
[0062] (1) Refractive index (nx, ny, nz)
[0063] "nx" is the refractive index in the direction where the refractive index in the plane reaches the maximum (ie, the slow axis direction), "ny" is the refractive index in the direction orthogonal to the slow axis in the plane (ie, the fast axis direction), and "nz" is the refractive index in the thickness direction.
[0064] (2) In-plane phase difference (Re)
[0065] "Re(λ)" is the in-plane phase difference measured at 23°C with light of wavelength λnm. For example, "Re(550)" is the in-plane phase difference measured at 23°C with light of wavelength 550nm. When the thickness of the layer (film) is d(nm), Re(λ) can be calculated by the formula: Re(λ) = (nx-ny)×d.
[0066] (3) Retardation in the thickness direction (Rth)
[0067] "Rth(λ)" is the phase difference in the thickness direction measured at 23°C with light of wavelength λnm. For example, "Rth(550)" is the phase difference in the thickness direction measured at 23°C with light of wavelength 550nm. When the thickness of the layer (film) is d(nm), Rth(λ) can be calculated by the formula: Rth(λ) = (nx-nz)×d.
[0068] (4) Nz coefficient
[0069] The Nz coefficient can be calculated by Nz=Rth / Re.
[0070] (5) Angle
[0071] In this specification, when an angle is mentioned, the angle includes both clockwise and counterclockwise angles relative to a reference direction. Therefore, for example, "45°" means ±45°.
[0072] Figure 1 Schematic diagram showing a simplified structure of a display system according to an embodiment of the present invention. Figure 1 , the configuration and shape of each component of the display system 2 are schematically shown. The display system 2 includes a display element 12, a reflective polarization member 14, a first lens unit 16, a half mirror 18, a first phase difference member 20, a second phase difference member 22, and a second lens unit 24. The reflective polarization member 14 is arranged on the display surface 12a side of the display element 12, that is, in front, and can reflect the light emitted from the display element 12. The first lens unit 16 is arranged on the optical path between the display element 12 and the reflective polarization member 14, and the half mirror 18 is arranged between the display element 12 and the first lens unit 16. The first phase difference member 20 is arranged on the optical path between the display element 12 and the half mirror 18, and the second phase difference member 22 is arranged on the optical path between the half mirror 18 and the reflective polarization member 14.
[0073] Components arranged in front of the half mirror or the first lens unit (in the illustrated example, the half mirror 18 , the first lens unit 16 , the second phase difference element 22 , the reflective polarization element 14 , and the second lens unit 24 ) are sometimes collectively referred to as a lens unit (lens unit 4 ).
[0074] The display element 12 is, for example, a liquid crystal display or an organic EL display, and has a display surface 12a for displaying images. Light emitted from the display surface 12a passes through a polarizing member (typically a polarizing film) that may be included in the display element 12 and then emitted as first linearly polarized light.
[0075] The first phase difference member 20 includes a first λ / 4 member capable of converting the first linear polarization light incident on the first phase difference member 20 into a first circular polarization light. When the first phase difference member does not include a member other than the first λ / 4 member, the first phase difference member may be equivalent to the first λ / 4 member. The first phase difference member 20 may be integrally provided on the display element 12.
[0076] The half mirror 18 transmits the light emitted from the display element 12 and reflects the light reflected by the reflective polarization member 14 toward the reflective polarization member 14. The half mirror 18 is integrally provided with the first lens portion 16.
[0077] The second phase difference member 22 includes a second λ / 4 member that allows the light reflected by the reflective polarization member 14 and the half mirror 18 to pass through the reflective polarization member 14. When the second phase difference member does not include a member other than the second λ / 4 member, the second phase difference member may be equivalent to the second λ / 4 member. The second phase difference member 22 may be integrally provided on the first lens portion 16.
[0078] The first circularly polarized light emitted from the first λ / 4 member included in the first phase difference member 20 passes through the half mirror 18 and the first lens unit 16, and is converted into the second linearly polarized light by the second λ / 4 member included in the second phase difference member 22. The second linearly polarized light emitted from the second λ / 4 member does not pass through the reflective polarization member 14, but is reflected toward the half mirror 18. At this time, the polarization direction of the second linearly polarized light incident on the reflective polarization member 14 is the same direction as the reflection axis of the reflective polarization member 14. Therefore, the second linearly polarized light incident on the reflective polarization member 14 is reflected by the reflective polarization member 14.
[0079] The second linear polarized light reflected by the reflective polarization member 14 is converted into the second circular polarized light by the second λ / 4 member included in the second phase difference member 22, and the second circular polarized light emitted from the second λ / 4 member passes through the first lens unit 16 and is reflected by the half mirror 18. The second circular polarized light reflected by the half mirror 18 passes through the first lens unit 16 and is converted into the third linear polarized light by the second λ / 4 member included in the second phase difference member 22. The third linear polarized light is transmitted through the reflective polarization member 14. At this time, the polarization direction of the third linear polarized light incident on the reflective polarization member 14 is the same direction as the transmission axis of the reflective polarization member 14. Therefore, the third linear polarized light incident on the reflective polarization member 14 is transmitted through the reflective polarization member 14.
[0080] The light transmitted through the reflective polarization element 14 passes through the second lens portion 24 and enters the eye 26 of the user.
[0081] For example, the absorption axis of the polarization component included in the display element 12 and the reflection axis of the reflective polarization component 14 can be arranged approximately parallel to each other, or can be arranged approximately orthogonal to each other. The angle formed by the absorption axis of the polarization component included in the display element 12 and the slow axis of the 1st λ / 4 component included in the first phase difference component 20 is, for example, 40° to 50°, 42° to 48°, or approximately 45°. The angle formed by the absorption axis of the polarization component included in the display element 12 and the slow axis of the 2nd λ / 4 component included in the second phase difference component 22 is, for example, 40° to 50°, 42° to 48°, or approximately 45°.
[0082] The in-plane phase difference Re(550) of the first λ / 4 component is, for example, 100 nm to 190 nm, 110 nm to 180 nm, 130 nm to 160 nm, or 135 nm to 155 nm. The first λ / 4 component preferably exhibits an inverse dispersion wavelength characteristic in which the phase difference value increases with the wavelength of the measurement light. The first λ / 4 component preferably satisfies the relationship Re(450)<Re(550)<Re(650). Re(450) / Re(550) of the first λ / 4 component is, for example, greater than 0.75 and less than 1, or greater than 0.8 and less than 0.95.
[0083] The in-plane phase difference Re(550) of the second λ / 4 component is, for example, 100nm to 190nm, 110nm to 180nm, 130nm to 160nm, or 135nm to 155nm. The second λ / 4 component preferably exhibits an inverse dispersion wavelength characteristic in which the phase difference value increases with the wavelength of the measurement light. The second λ / 4 component preferably satisfies the relationship Re(450)<Re(550)<Re(650). Re(450) / Re(550) of the second λ / 4 component is, for example, greater than 0.75 and less than 1, or greater than 0.8 and less than 0.95.
[0084] In the lens portion 4, a space can be formed between the first lens portion 16 and the second lens portion 24. In this case, the component arranged between the first lens portion 16 and the second lens portion 24 is preferably provided integrally in any one of the first lens portion 16 and the second lens portion 24. For example, the component arranged between the first lens portion 16 and the second lens portion 24 is preferably integrated with any one of the first lens portion 16 and the second lens portion 24 via an adhesive layer. According to such a method, for example, the handling properties of each component can be excellent. The adhesive layer can be formed by an adhesive or an adhesive. Specifically, the adhesive layer can be an adhesive layer or an adhesive layer. The thickness of the adhesive layer is, for example, 0.05μm to 30μm.
[0085] Figure 2It is shown Figure 1 Schematic cross-sectional view of an example of the details of the lens unit of the display system shown. Specifically, Figure 2 The first lens portion, the second lens portion, and a member disposed therebetween are shown. The lens portion 4 includes: a first lens portion 16, a first laminated portion 100 disposed adjacent to the first lens portion 16, a second lens portion 24, and a second laminated portion 200 disposed adjacent to the second lens portion 24. Figure 2 In the example shown, the first stacked portion 100 and the second stacked portion 200 are arranged separately. Although not shown, the half mirror may be provided integrally with the first lens portion 16. Hereinafter, the first stacked portion may be referred to as an optical stacked body.
[0086] The first laminated portion 100 includes a second phase difference member 22, and an adhesive layer (e.g., an adhesive layer) 41 disposed between the first lens portion 16 and the second phase difference member 22, and is integrally provided on the first lens portion 16 through the adhesive layer 41. The first laminated portion 100 further includes a first protective member 31 disposed in front of the second phase difference member 22. The first protective member 31 is laminated on the second phase difference member 22 via an adhesive layer (e.g., an adhesive layer) 42, and is disposed adjacent to the second phase difference member 22. The first protective member 31 may be located on the outermost surface of the first laminated portion 100. It should be noted that in this specification, adjacent includes not only directly adjacent, but also adjacent via an adhesive layer.
[0087] exist Figure 2 In the example shown, the second phase difference component 22 includes a component (second phase difference layer) 22b whose refractive index characteristic shows the relationship of nz>nx≥ny in addition to the second λ / 4 component (first phase difference layer) 22a. The second phase difference component 22 has a stacked structure of the first phase difference layer 22a and the second phase difference layer 22b. By using the component 22b showing the relationship of nz>nx≥ny, light leakage (for example, light leakage in an oblique direction) can be prevented. Figure 2 As shown, in the second phase difference member 22, the second λ / 4 member 22a is preferably positioned further forward than the member 22b showing the relationship of nz>nx≥ny.
[0088] The second λ / 4 component (first phase difference layer) 22a and the component (second phase difference layer) 22b showing the relationship of nz>nx≥ny are stacked together via an adhesive layer 50. The second phase difference component 22 includes a first phase difference layer 22a, an adhesive layer 50 and a second phase difference layer 22b. By stacking the phase difference layers using an adhesive layer 50, the generation of rupture and cracks in the phase difference layer can be suppressed. In addition, peeling between the phase difference layers can be prevented. Moreover, an optical laminate with excellent durability can be obtained. For example, when the thickness of at least one of the first phase difference layer and the second phase difference layer (for example, the second phase difference layer) is less than 10μm, there is a tendency for rupture and cracks to occur easily.
[0089] The refractive index characteristics of the second λ / 4 component preferably show a relationship of nx>ny≥nz. Here, "ny=nz" includes not only the case where ny and nz are completely equal, but also the case where they are substantially equal. Therefore, within the range that does not impair the effect of the present invention, ny<nz may be sometimes used. The Nz coefficient of the second λ / 4 component is preferably 0.9 to 3, more preferably 0.9 to 2.5, further preferably 0.9 to 1.5, and particularly preferably 0.9 to 1.3.
[0090] The second λ / 4 member is formed of any appropriate material that can satisfy the above-mentioned characteristics. The second λ / 4 member may be, for example, a stretched film of a resin film or an alignment fixing layer of a liquid crystal compound.
[0091] As the resin contained in the above-mentioned resin film, there can be mentioned: polycarbonate resin, polyester carbonate resin, polyester resin, polyvinyl acetal resin, polyarylate resin, cyclic olefin resin, cellulose resin, polyvinyl alcohol resin, polyamide resin, polyimide resin, polyether resin, polystyrene resin, acrylic resin, etc. These resins can be used alone or in combination. As a method of combination, for example, blending and copolymerization can be mentioned. In the case where the second λ / 4 component shows a reverse dispersion wavelength characteristic, a resin film containing a polycarbonate resin or a polyester carbonate resin (hereinafter, sometimes referred to as a polycarbonate resin) can be suitably used.
[0092] As the above-mentioned polycarbonate resin, any appropriate polycarbonate resin can be used. For example, the polycarbonate resin contains structural units derived from fluorene dihydroxy compounds, structural units derived from isosorbide dihydroxy compounds, and structural units derived from at least one dihydroxy compound selected from alicyclic diols, alicyclic dimethanols, di, tri or polyethylene glycols and alkylene glycols or spirodiols. Preferably, the polycarbonate resin contains structural units derived from fluorene dihydroxy compounds, structural units derived from isosorbide dihydroxy compounds, structural units derived from alicyclic dimethanols and / or structural units derived from di, tri or polyethylene glycols; more preferably, it contains structural units derived from fluorene dihydroxy compounds, structural units derived from isosorbide dihydroxy compounds, and structural units derived from di, tri or polyethylene glycols. The polycarbonate resin may also contain structural units derived from other dihydroxy compounds as needed. It should be noted that details of the polycarbonate resin that can be suitably used for the second λ / 4 component and the method for forming the second λ / 4 component are recorded in, for example, Japanese Patent Gazette No. 2014-10291, Japanese Patent Gazette No. 2014-26266, Japanese Patent Gazette No. 2015-212816, Japanese Patent Gazette No. 2015-212817, and Japanese Patent Gazette No. 2015-212818, and the records in these gazettes are cited as references in this specification.
[0093] The thickness of the second λ / 4 member formed of a stretched film of a resin film is, for example, 10 μm to 100 μm, preferably 10 μm to 70 μm, and more preferably 20 μm to 60 μm.
[0094] The orientation fixing layer of the liquid crystal compound is a layer in which the liquid crystal compound is oriented in a given direction within the layer and its orientation state is fixed. It should be noted that the "orientation fixing layer" is a concept that includes an orientation fixing layer obtained by curing a liquid crystal monomer as described later. In the second λ / 4 component, representatively, the rod-shaped liquid crystal compound is oriented in a state arranged along the slow axis direction of the second λ / 4 component (parallel orientation (homogeneous alignment)). As rod-shaped liquid crystal compounds, for example, liquid crystal polymers and liquid crystal monomers can be cited. The liquid crystal compound is preferably capable of polymerization. If the liquid crystal compound is capable of polymerization, the orientation state of the liquid crystal compound can be fixed by polymerizing after orienting the liquid crystal compound.
[0095] The orientation fixing layer (liquid crystal orientation fixing layer) of the above-mentioned liquid crystal compound can be formed by the following method: an orientation treatment is applied to the surface of a given substrate, a coating liquid containing a liquid crystal compound is applied to the surface, and the liquid crystal compound is oriented along the direction corresponding to the above-mentioned orientation treatment to fix the orientation state. As an orientation treatment, any appropriate orientation treatment can be adopted. Specifically, mechanical orientation treatment, physical orientation treatment, and chemical orientation treatment can be cited. As specific examples of mechanical orientation treatment, friction treatment and stretching treatment can be cited. As specific examples of physical orientation treatment, magnetic field orientation treatment and electric field orientation treatment can be cited. As specific examples of chemical orientation treatment, inclined evaporation method and optical orientation treatment can be cited. The processing conditions of various orientation treatments can adopt any appropriate conditions according to the purpose.
[0096] The liquid crystal compound can be aligned by treating it at a temperature corresponding to the type of the liquid crystal compound at which it exhibits a liquid crystal phase. By such a temperature treatment, the liquid crystal compound is in a liquid crystal state and is aligned in the alignment treatment direction of the substrate surface.
[0097] In one embodiment, the alignment state is fixed by cooling the aligned liquid crystal compound as described above. When the liquid crystal compound is polymerizable or crosslinkable, the alignment state can be fixed by subjecting the aligned liquid crystal compound to polymerization or crosslinking treatment as described above.
[0098] As the above-mentioned liquid crystal compound, any appropriate liquid crystal polymer and / or liquid crystal monomer can be used. Liquid crystal polymer and liquid crystal monomer can be used alone or in combination. Specific examples of liquid crystal compounds and methods for making liquid crystal orientation fixing layers are described in, for example, Japanese Patent Publication No. 2006-163343, Japanese Patent Publication No. 2006-178389, and International Publication No. 2018 / 123551. The records of these publications are cited as references in this specification.
[0099] The thickness of the second λ / 4 member composed of the liquid crystal alignment fixing layer is, for example, 1 μm to 10 μm, preferably 1 μm to 8 μm, more preferably 1 μm to 6 μm, and further preferably 1 μm to 4 μm.
[0100] The phase difference Rth(550) in the thickness direction of the component (second phase difference layer) whose refractive index characteristics show the relationship of nz>nx≥ny is preferably -260nm~-10nm, more preferably -230nm~-15nm, and further preferably -215nm~-20nm. In one embodiment, the second phase difference layer is a so-called positive C plate whose refractive index shows the relationship of nx=ny. Here, "nx=ny" includes not only the case where nx and ny are strictly equal, but also the case where nx and ny are substantially equal. For example, the case where Re(550) is less than 10nm is also included. In another embodiment, the refractive index of the second phase difference layer shows the relationship of nx>ny. In this case, the in-plane phase difference Re(550) of the second phase difference layer is preferably 10nm~150nm, more preferably 10nm~80nm.
[0101] The component whose refractive index characteristics show the relationship of nz>nx≥ny can be formed by any appropriate material. It is preferably composed of a film containing a liquid crystal material fixed in a homeotropic orientation. The liquid crystal material (liquid crystal compound) capable of homeotropic orientation can be a liquid crystal monomer or a liquid crystal polymer. As specific examples of such a liquid crystal compound and a method for forming a film, there can be cited the liquid crystal compounds and formation methods described in
[0020] to
[0042] of Japanese Patent Gazette No. 2002-333642. In this case, the thickness is preferably 0.1μm to 5μm, more preferably 0.5μm to 4μm.
[0102] As another preferred specific example, the member having a refractive index characteristic showing the relationship of nz>nx≥ny may be a phase difference film made of a fumaric acid diester resin as described in Japanese Patent Application Laid-Open No. 2012-32784. In this case, the thickness is preferably 5 to 50 μm, more preferably 10 to 35 μm.
[0103] The adhesive layer 50 included in the second phase difference member 22 can be formed by any appropriate adhesive. For example, in the process of forming the adhesive layer, the state of the adhesive changes irreversibly from a liquid to a solid, and has the property of being fluid when applied and being cured by a curing treatment (for example, irradiation with active energy rays, heating). As an adhesive, a curing adhesive is preferably used. Specifically, the adhesive layer 50 is preferably a cured layer of a resin. As a curing adhesive, an ultraviolet curing adhesive can be preferably used.
[0104] The ultraviolet curing adhesive contains a curable monomer such as a compound having a (meth)acryloyl group and a compound having a vinyl group as a curable monomer. A compound having a (meth)acryloyl group can be preferably used. Here, the (meth)acryloyl group refers to an acryloyl group and / or a methacryloyl group.
[0105] The thickness of the adhesive layer contained in the phase difference component is less than 1.3 μm, preferably less than 1.1 μm, and more preferably less than 0.9 μm. According to such a thickness, an optical laminate with extremely excellent smoothness can be obtained. Specifically, when the adhesive layer is formed, the adhesive will shrink upon curing. The curing shrinkage will have a significant effect on the smoothness of the obtained optical laminate. In the above-mentioned display system, the image can be magnified in the lens portion (for example, by a convex lens), and the smoothness of the optical laminate will have a significant effect on visual recognition. According to the thin adhesive layer, the influence caused by curing shrinkage can be reduced, and an optical laminate with excellent smoothness can be obtained. In addition, according to such an optical laminate, significantly excellent visual recognition can be achieved in the above-mentioned display system. For example, a clear image without distortion can be achieved. On the other hand, for example, from the perspective of durability, the thickness of the adhesive layer contained in the phase difference component is preferably 0.5 μm or more.
[0106] Typically, the first protective member includes a substrate. The thickness of the substrate is preferably 5 μm to 80 μm, more preferably 10 μm to 50 μm, and further preferably 15 μm to 40 μm. The surface smoothness of the substrate is preferably 0.7 arcmin or less, more preferably 0.6 arcmin or less, and further preferably 0.5 arcmin or less. It should be noted that the surface smoothness can be measured by focusing the irradiated light on the surface of the object.
[0107] The substrate can be composed of any appropriate film. As the material of the main component of the film constituting the substrate, for example, cellulose resins such as triacetyl cellulose (TAC), polyesters, polyvinyl alcohols, polycarbonates, polyamides, polyimides, polyethersulfones, polysulfones, polystyrenes, cycloolefins such as polynorbornene, polyolefins, (meth) acrylic acid, acetate resins, etc. can be cited. Here, (meth) acrylic acid refers to acrylic acid and / or methacrylic acid. In one embodiment, the substrate is preferably formed by a (meth) acrylic resin. By adopting a (meth) acrylic resin, it is possible to achieve film formation of a substrate with excellent smoothness (for example, satisfying the above-mentioned surface smoothness) by extrusion molding. And a protective member with excellent smoothness can be obtained.
[0108] The first protective member is preferably composed of a laminated film having a substrate and a surface treatment layer formed on the substrate. The thickness of the laminated film is preferably 10 μm to 80 μm, more preferably 15 μm to 60 μm, and further preferably 20 μm to 45 μm. The thickness of the surface treatment layer is preferably 0.5 μm to 10 μm, more preferably 1 μm to 7 μm, and further preferably 2 μm to 5 μm.
[0109] Typically, the surface treatment layer includes a hard coat layer. Typically, the hard coat layer is formed by applying a hard coat forming material on a substrate and curing the coated layer. Typically, the hard coat forming material includes a curable compound as a layer forming component. As the curing mechanism of the curable compound, for example, a thermosetting type and a photocuring type can be cited. As the curable compound, for example, a monomer, an oligomer, and a prepolymer can be cited. It is preferred to use a multifunctional monomer or oligomer as the curable compound. As the multifunctional monomer or oligomer, for example, a monomer or oligomer having more than two (meth)acryloyl groups, a carbamate (meth)acrylate or an oligomer of a carbamate (meth)acrylate, an epoxy monomer or oligomer, and a silicone monomer or oligomer can be cited.
[0110] The thickness of the hard coat layer is preferably 0.5 μm to 10 μm, more preferably 1 μm to 7 μm, and even more preferably 2 μm to 5 μm.
[0111] The surface treatment layer preferably includes a functional layer. The functional layer preferably functions as an antireflection layer. In a preferred embodiment, the surface treatment layer includes the hard coating layer and the antireflection layer in order from the substrate side. The thickness of the functional layer is preferably 0.05 μm to 10 μm, more preferably 0.1 μm to 5 μm, and further preferably 0.1 μm to 2 μm.
[0112] The first protective member having a surface treatment layer can be configured so that the surface treatment layer is located on the front side. Specifically, the surface treatment layer can be located on the outermost surface of the first laminated portion. The surface treatment layer can have any appropriate function. For example, from the perspective of suppressing light loss at the interface with air and improving visual recognition, the surface treatment layer preferably has an anti-reflection function. In one embodiment, the maximum value of the 5° specular reflectance spectrum of the first protective member in the range of wavelengths of 420nm to 680nm is preferably 2.0% or less, more preferably 1.2% or less, further preferably 1.0% or less, and particularly preferably 0.8% or less. Here, the 5° specular reflectance can be measured, for example, as follows: a measurement sample is prepared by pasting the measurement object on a black acrylic plate using an adhesive, and a spectrophotometer (manufactured by Hitachi High-Tech Co., Ltd., trade name "U-4100") is used as a measuring device, and the incident angle of light on the measurement sample is set to 5° for measurement.
[0113] The surface smoothness of the first protective member is preferably less than 0.5 arcmin, more preferably less than 0.4 arcmin. The surface smoothness of the first protective member is, for example, substantially greater than 0.1 arcmin. The stack smoothness of the optical stack 100 is preferably less than 0.7 arcmin, more preferably less than 0.6 arcmin, and further preferably less than 0.5 arcmin. By making the optical stack satisfy such stack smoothness, the generation of diffuse light can be suppressed and the image can be suppressed from becoming unclear. The stack smoothness of the optical stack 100 is, for example, greater than 0.1 arcmin. It should be noted that the stack smoothness can be obtained by irradiating the object with irradiation light and detecting the reflection and transmittance of each component constituting the object (stack).
[0114] The optical laminate 100 may have excellent durability. For example, after the optical laminate 100 is placed in a temperature environment of 80°C for 500 hours, the laminate smoothness is preferably 0.7 arcmin or less, more preferably 0.6 arcmin or less, and further preferably 0.5 arcmin or less. In addition, after the optical laminate 100 is placed in a temperature environment of -40°C for 500 hours, the laminate smoothness is preferably 0.7 arcmin or less, more preferably 0.6 arcmin or less, and further preferably 0.5 arcmin or less.
[0115] The optical layered body 100 may have a high transmittance. For example, the Y value of the visibility-corrected single body transmittance of the optical layered body 100 is, for example, 90% or more, preferably 93% or more, more preferably 94% or more, and further preferably 95% or more.
[0116] The second stacking section 200 includes a reflective polarizing member 14 and an adhesive layer (e.g., an adhesive layer) disposed between the reflective polarizing member 14 and the second lens portion 24. From the perspective of improving visual recognition, the second stacking section 200, for example, further includes an absorptive polarizing member 28 disposed between the reflective polarizing member 14 and the second lens portion 24. The absorptive polarizing member 28 is stacked in front of the reflective polarizing member 14 via an adhesive layer (e.g., an adhesive layer) 44. The reflection axis of the reflective polarizing member 14 and the absorption axis of the absorptive polarizing member 28 can be arranged substantially parallel to each other, and the transmission axis of the reflective polarizing member 14 and the transmission axis of the absorptive polarizing member 28 can be arranged substantially parallel to each other. By stacking via an adhesive layer, the reflective polarizing member 14 and the absorptive polarizing member 28 can be fixed, thereby preventing the displacement of the axis configuration of the reflection axis and the absorption axis (transmission axis and transmission axis). In addition, it is possible to suppress the adverse effects caused by the air layer that may be formed between the reflective polarizing member 14 and the absorptive polarizing member 28.
[0117] The second laminated portion 200 further includes a second protective member 32 disposed behind the reflective polarizing member 14. The second protective member 32 is laminated on the reflective polarizing member 14 via an adhesive layer (e.g., an adhesive layer) 43. The second protective member 32 may be located on the outermost surface of the second laminated portion 200. The first protective member 31 and the second protective member 32 are disposed opposite to each other with a space therebetween. The second protective member, like the first protective member described above, may be a laminated film having a substrate and a surface treatment layer, representatively. In this case, the surface treatment layer may be located on the outermost surface of the second laminated portion. The same description as that of the first protective member described above may be applied to the details of the second protective member. Specifically, the same description as that of the first protective member described above may be applied to the reflective characteristics and effects, smoothness, thickness, and constituent materials of the second protective member.
[0118] exist Figure 2 In the example shown, the second stacked section 200 further includes a third phase difference member 30 disposed between the absorption type polarization member 28 and the second lens section 24. The third phase difference member 30 is stacked on the absorption type polarization member 28 via an adhesive layer (e.g., an adhesive layer) 45. In addition, the third phase difference member 30 is stacked on the second lens section 24 via an adhesive layer (e.g., an adhesive layer) 46, and the second stacked section 200 is integrally provided on the second lens section 24. The third phase difference member 30 includes, for example, a 3rd λ / 4 member. The angle formed by the absorption axis of the absorption type polarization member 28 and the slow axis of the 3rd λ / 4 member included in the third phase difference member 30 is, for example, 40° to 50°, may be 42° to 48°, or may be about 45°. By providing such a member, it is possible to prevent, for example, reflection of external light from the second lens section 16 side. In the case where the third phase difference member does not include a member other than the 3rd λ / 4 member, the third phase difference member may be equivalent to the 3rd λ / 4 member.
[0119] The above-mentioned reflective polarizing component can transmit polarized light (representatively linear polarized light) parallel to its transmission axis while maintaining its polarization state, and reflect light of other polarization states. As a reflective polarizing component, it is typically composed of a film with a multilayer structure (sometimes referred to as a reflective polarizing film). In this case, the thickness of the reflective polarizing component is, for example, 10 μm to 150 μm, preferably 20 μm to 100 μm, and more preferably 30 μm to 60 μm.
[0120] Figure 314 is a schematic stereoscopic diagram showing an example of a multilayer structure included in a reflective polarizing film. The multilayer structure 14a alternately comprises a layer A having birefringence and a layer B having substantially no birefringence. The total number of layers constituting the multilayer structure may be 50 to 1000. For example, the refractive index nx of the A layer in the x-axis direction is greater than the refractive index ny in the y-axis direction, the refractive index nx of the B layer in the x-axis direction is substantially the same as the refractive index ny in the y-axis direction, and the refractive index difference between the A layer and the B layer is large in the x-axis direction and substantially zero in the y-axis direction. As a result, the x-axis direction can be made a reflection axis and the y-axis direction can be made a transmission axis. The refractive index difference between the A layer and the B layer in the x-axis direction is preferably 0.2 to 0.3.
[0121] The above-mentioned A layer is typically formed of a material that exhibits birefringence by stretching. Examples of such materials include naphthalene dicarboxylic acid polyesters (e.g., polyethylene naphthalate), polycarbonates, and acrylic resins (e.g., polymethyl methacrylate). The above-mentioned B layer is typically formed of a material that does not substantially exhibit birefringence even when stretched. Examples of such materials include copolyesters of naphthalene dicarboxylic acid and terephthalic acid. The above-mentioned multilayer structure can be formed by combining coextrusion with stretching. For example, after the material constituting the A layer and the material constituting the B layer are extruded, they are multilayered (e.g., using a multiplier). Then, the obtained multilayer laminate is stretched. The x-axis direction of the illustrated example can correspond to the stretching direction.
[0122] Examples of commercially available reflective polarizing films include "DBEF" and "APF" manufactured by 3M Co., Ltd. and "APCF" manufactured by Nitto Denko Corporation.
[0123] The orthogonal transmittance (Tc) of the reflective polarizing component (reflective polarizing film) can be, for example, 0.01% to 3%. The single transmittance (Ts) of the reflective polarizing component (reflective polarizing film) can be, for example, 43% to 49%, preferably 45% to 47%. The polarization degree (P) of the reflective polarizing component (reflective polarizing film) can be, for example, 92% to 99.99%.
[0124] The above-mentioned orthogonal transmittance, single transmittance and polarization degree can be measured, for example, using an ultraviolet visible spectrophotometer. The polarization degree P can be measured using an ultraviolet visible spectrophotometer for single transmittance Ts, parallel transmittance Tp and orthogonal transmittance Tc, and can be obtained by the following formula based on the obtained Tp and Tc. It should be noted that Ts, Tp and Tc are Y values obtained by measuring with a 2-degree field of view (C light source) of JIS Z8701 and correcting for visibility.
[0125] Polarization degree P (%) = {(Tp-Tc) / (Tp+Tc)} 1 / 2 ×100
[0126] The absorption-type polarizing member may typically include a resin film containing a dichroic substance (sometimes referred to as an absorption-type polarizing film). The thickness of the absorption-type polarizing film is, for example, 1 μm to 20 μm, 2 μm to 15 μm, 12 μm to 10 μm, 8 μm to 8 μm, or 5 μm to 5 μm.
[0127] The absorption-type polarizing film may be produced by a single-layer resin film or by using a laminate of two or more layers.
[0128] In the case of a single-layer resin film, for example, a hydrophilic polymer film such as a polyvinyl alcohol (PVA) film, a partially formalized PVA film, or a partially saponified ethylene-vinyl acetate copolymer film can be subjected to dyeing treatment using a dichroic substance such as iodine or a dichroic dye, stretching treatment, etc., thereby obtaining an absorption-type polarizing film. Among them, an absorption-type polarizing film obtained by dyeing a PVA film with iodine and uniaxially stretching the film is preferred.
[0129] The dyeing using iodine can be performed by, for example, immersing the PVA film in an iodine aqueous solution. The stretching ratio of the uniaxial stretching is preferably 3 to 7 times. The stretching can be performed after the dyeing treatment or while dyeing. In addition, the dyeing can also be performed after the stretching. The PVA film can be subjected to swelling treatment, cross-linking treatment, cleaning treatment, drying treatment, etc. as needed.
[0130] As a laminate made using the above-mentioned two or more layers, there can be cited a laminate of a resin substrate and a PVA-type resin layer (PVA-type resin film) laminated on the resin substrate, or a laminate of a resin substrate and a PVA-type resin layer formed by coating on the resin substrate. The absorption-type polarizing film obtained by using a laminate of a resin substrate and a PVA-type resin layer formed by coating on the resin substrate can be made by the following method: for example, a PVA-type resin solution is applied to a resin substrate, dried to form a PVA-type resin layer on the resin substrate, and a laminate of a resin substrate and a PVA-type resin layer is obtained; the laminate is stretched and dyed to make the PVA-type resin layer into an absorption-type polarizing film. In this embodiment, it is preferred to form a polyvinyl alcohol-type resin layer containing a halide and a polyvinyl alcohol-type resin on one side of the resin substrate. Stretching typically includes immersing the laminate in a boric acid aqueous solution for stretching. In addition, stretching can further include stretching the laminate in a gas atmosphere at a high temperature (for example, above 95°C) before stretching in a boric acid aqueous solution as needed. In addition, in the present embodiment, it is preferred that the laminate is subjected to a drying shrinkage treatment in which the laminate shrinks by more than 2% in the width direction by heating while being conveyed in the length direction. Representatively, the manufacturing method of the present embodiment includes sequentially performing an auxiliary stretching treatment in a gas atmosphere, a dyeing treatment, a stretching treatment in an aqueous solution, and a drying shrinkage treatment on the laminate. By introducing auxiliary stretching, the crystallinity of the PVA can be improved even when the PVA is coated on the thermoplastic resin, and high optical properties can be achieved. In addition, by simultaneously improving the orientation of the PVA in advance, it is possible to prevent problems such as the reduction of the orientation and dissolution of the PVA when immersed in water in the subsequent dyeing process and the stretching process, and high optical properties can be achieved. In addition, when the PVA-type resin layer is immersed in a liquid, the orientation disorder of the polyvinyl alcohol molecules and the reduction of the orientation can be suppressed compared to the case where the PVA-type resin layer does not contain a halide. Thus, the optical properties of the absorption-type polarizing film obtained by the treatment process of immersing the laminate in a liquid such as a dyeing treatment and a stretching treatment in an aqueous solution can be improved. Further, the laminate is shrunk in the width direction by drying and shrinking treatment, thereby improving the optical properties. The obtained laminate of resin substrate / absorption type polarizing film can be used directly (that is, the resin substrate can be used as a protective layer of absorption type polarizing film), or the resin substrate can be peeled off from the laminate of resin substrate / absorption type polarizing film, and any appropriate protective layer corresponding to the purpose can be stacked on the peeling surface or on the side opposite to the peeling surface. The details of the manufacturing method of such an absorption type polarizing film are recorded in, for example, Japanese Patent Publication No. 2012-73580 and Japanese Patent No. 6470455. The records of these publications as a whole are cited in this specification as a reference.
[0131] The orthogonal transmittance (Tc) of the absorption type polarization component (absorption type polarizing film) is preferably 0.5% or less, more preferably 0.1% or less, and further preferably 0.05% or less. The single transmittance (Ts) of the absorption type polarization component (absorption type polarizing film) is, for example, 41.0% to 45.0%, and preferably 42.0% or more. The polarization degree (P) of the absorption type polarization component (absorption type polarizing film) is, for example, 99.0% to 99.997%, and preferably 99.9% or more.
[0132] The in-plane phase difference Re(550) of the above-mentioned third λ / 4 component is, for example, 100nm to 190nm, 110nm to 180nm, 130nm to 160nm, or 135nm to 155nm. The third λ / 4 component preferably shows an inverse dispersion wavelength characteristic in which the phase difference value increases corresponding to the wavelength of the measured light. The Re(450) / Re(550) of the third λ / 4 component is, for example, greater than 0.75 and less than 1, or greater than 0.8 and less than 0.95. The refractive index characteristics of the third λ / 4 component preferably show the relationship of nx>ny≥nz. The Nz coefficient of the third λ / 4 component is preferably 0.9 to 3, more preferably 0.9 to 2.5, further preferably 0.9 to 1.5, and particularly preferably 0.9 to 1.3.
[0133] The third λ / 4 member is formed of any appropriate material that can satisfy the above-mentioned characteristics. The third λ / 4 member may be, for example, a stretched film of a resin film or an alignment fixing layer of a liquid crystal compound. The same description as that of the second λ / 4 member may be applied to the third λ / 4 member formed of a stretched film of a resin film or an alignment fixing layer of a liquid crystal compound. The second λ / 4 member and the third λ / 4 member may be members having the same configuration (for example, forming material, thickness, optical characteristics, etc.) or members having different configurations.
[0134] The thickness of the laminated adhesive layer used for each of the above-mentioned components can be set to any appropriate thickness. The thickness of each laminated adhesive layer used for each of the above-mentioned components is preferably 3 μm or more and 20 μm or less, or 15 μm or less, or 12 μm or less, or 7 μm or less. According to such a thickness, the degree of concavity and convexity on the surface of the adhesive layer can be suppressed, and the smoothness of the laminated portion can be excellent.
[0135] Example
[0136] Hereinafter, the present invention will be specifically described in conjunction with the embodiments, but the present invention is not limited to these embodiments. It should be noted that the thickness, phase difference value and surface smoothness are values measured by the following measuring methods. In addition, as long as there is no special clear record, "part" and "%" are weight basis.
[0137] <Thickness>
[0138] The thickness of 10 μm or less was measured using a scanning electron microscope (manufactured by JEOL Ltd., product name “JSM-7100F”). The thickness exceeding 10 μm was measured using a digital micrometer (manufactured by Anritsu Co., Ltd., product name “KC-351C”).
[0139] <Phase difference value>
[0140] The phase difference value at each wavelength at 23° C. was measured using a Mueller matrix polarimeter (manufactured by Axometrics, product name “Axoscan”).
[0141] <Surface smoothness>
[0142] The surface smoothness was measured using a scanning white light interferometer (manufactured by Zygo Corporation, product name "NewView9000"). Specifically, the test sample was placed on a test table with an anti-vibration table, interference fringes were generated using a single white LED illumination, and an interference objective lens (1.4 times) with a reference surface was scanned along the Z direction (thickness direction), thereby selectively obtaining the smoothness of the outermost surface of the test object within the field of view of 12.4 mm□ (surface smoothness).
[0143] When the object to be measured is an adhesive layer, the adhesive layer was attached to a micro slide (manufactured by Matsunami Glass Industries, Ltd., product name "S200200"), and the smoothness of the exposed adhesive surface was measured. When the object to be measured is a film, a 5 μm thick acrylic adhesive layer with few uneven surfaces was formed on the above glass, and the film of the object to be measured was laminated to the adhesive surface in a manner that does not introduce foreign matter, bubbles, or deformed stripes, and the smoothness of the surface on the opposite side to the adhesive layer was measured. It should be noted that the surface smoothness of the above 5 μm thick acrylic adhesive layer with few uneven surfaces is 0.30 arcmin.
[0144] Regarding the analysis, a value obtained by multiplying the angle index "Slope magnitude RMS" by two (corresponding to 2σ) is defined as surface smoothness (unit: arcmin).
[0145] [Example 1]
[0146] (Fabrication of λ / 4 member)
[0147] The polymerization was carried out using a batch polymerization apparatus consisting of two vertical reactors equipped with stirring blades and a reflux condenser controlled at 100° C. 29.60 parts by mass (0.046 mol) of bis[9-(2-phenoxycarbonylethyl)fluoren-9-yl]methane, 29.21 parts by mass (0.200 mol) of isosorbide (ISB), 42.28 parts by mass (0.139 mol) of spiroglycol (SPG), 63.77 parts by mass (0.298 mol) of diphenyl carbonate (DPC), and 1.19×10-6 parts by mass of calcium acetate monohydrate as a catalyst were added. -2 Mass parts (6.78×10 -5 mol). After the reactor was replaced with nitrogen under reduced pressure, it was heated by a heat medium and stirring was started when the internal temperature reached 100°C. The internal temperature reached 220°C 40 minutes after the start of the temperature rise, and the pressure was reduced while controlling to maintain the temperature, so that it reached 13.3kPa after 90 minutes after reaching 220°C. The phenol vapor produced as a by-product during the polymerization reaction was introduced into a 100°C reflux condenser, so that a certain amount of monomer components contained in the phenol vapor was returned to the reactor, and the uncondensed phenol vapor was introduced into a 45°C condenser for recovery. After nitrogen was introduced into the first reactor to temporarily restore it to atmospheric pressure, the reaction liquid after oligomerization in the first reactor was transferred to the second reactor. Next, the temperature rise and pressure reduction in the second reactor were started, so that it reached an internal temperature of 240°C and a pressure of 0.2kPa after 50 minutes. Then, the polymerization was carried out until the given stirring power was reached. When the predetermined power was reached, nitrogen gas was introduced into the reactor to restore the pressure, and the produced polyester carbonate resin was extruded into water, and the strands were cut to obtain pellets.
[0148] The obtained polyester carbonate resin (pellets) was vacuum dried at 80°C for 5 hours, and then a film-making device equipped with a single screw extruder (manufactured by Toshiba Machine Co., Ltd., cylinder setting temperature: 250°C), a T-die (width 200 mm, setting temperature: 250°C), a chill roll (setting temperature: 120-130°C) and a winder was used to produce a long strip of resin film with a thickness of 135 μm. The obtained long strip of resin film was stretched in the width direction at a stretching temperature of 143°C and a stretching ratio of 2.8 times to obtain a stretched film with a thickness of 47 μm. The Re(550) of the obtained stretched film was 143 nm, the Re(450) / Re(550) was 0.86, and the Nz coefficient was 1.12.
[0149] (Formation of positive C plate)
[0150] A liquid crystal coating liquid was prepared by dissolving 20 parts by weight of a side chain liquid crystal polymer represented by the following chemical formula (1) (the numbers 65 and 35 in the formula represent the molar % of the monomer unit, and for convenience, the block polymer is represented: the weight average molecular weight is 5000), 80 parts by weight of a polymerizable liquid crystal showing a nematic liquid crystal phase (manufactured by BASF: trade name Paliocolor LC242), and 5 parts by weight of a photopolymerization initiator (manufactured by Chiba Specialty Chemicals: trade name IRGACURE 907) in 200 parts by weight of cyclopentanone. Then, the coating liquid was applied to a PET substrate subjected to a vertical alignment treatment using a wire bar coater, and then heated and dried at 80°C for 4 minutes to align the liquid crystal. The liquid crystal layer was irradiated with ultraviolet rays to cure the liquid crystal layer, thereby forming a positive C plate with a thickness of 4 μm and an Rth (550) of -100 nm on the substrate.
[0151] [Chemical formula 1]
[0152]
[0153] (Production of protective components)
[0154] The following hard coat forming material was applied to an acrylic film having a lactone ring structure (thickness 40 μm, surface smoothness 0.45 arcmin), heated at 90° C. for 1 minute, and irradiated with a high pressure mercury lamp to a cumulative light intensity of 300 mJ / cm 2 The coating layer was cured by ultraviolet rays to produce an acrylic film (thickness 44 μm, surface smoothness 0.4 arcmin on the hard coat side) having a hard coat layer having a thickness of 4 μm.
[0155] Next, the antireflection layer forming coating liquid A described below was applied onto the hard coating layer using a wire bar, and the applied coating liquid was heated at 80°C for 1 minute to dry to form a coating film. The dried coating film was irradiated with a high pressure mercury lamp at a cumulative light intensity of 300 mJ / cm 2 The coating was cured by ultraviolet light to form an anti-reflection layer A with a thickness of 140 nm.
[0156] Next, the following antireflection layer forming coating liquid B was applied onto the antireflection layer A using a wire bar, and the applied coating liquid was heated at 80° C. for 1 minute to dry to form a coating film. The dried coating film was irradiated with a high pressure mercury lamp at a cumulative light intensity of 300 mJ / cm 2 The coating was cured by ultraviolet light to form an anti-reflection layer B with a thickness of 105 nm.
[0157] In this manner, a protective member (thickness 44 μm, surface smoothness 0.4 arcmin on the antireflection layer side) was obtained.
[0158] (Hard coat forming material)
[0159] A urethane acrylate oligomer (“NK Oligo UA-53H” manufactured by Shin-Nakamura Chemical Co., Ltd.), 50 parts of a polyfunctional acrylate having pentaerythritol triacrylate as a main component (“Viscoat#300” manufactured by Osaka Organic Chemical Co., Ltd.), 30 parts of 4-hydroxybutyl acrylate (manufactured by Osaka Organic Chemical Co., Ltd.), 20 parts of leveling agent (“GRANDIC PC4100” manufactured by DIC Corporation), 1 part of a photopolymerization initiator (“IRGACURE907” manufactured by Ciba Japan Co., Ltd.) were mixed and diluted with methyl isobutyl ketone so as to have a solid content concentration of 50%, thereby preparing a hard coat layer forming material.
[0160] (Anti-reflection layer forming coating liquid A)
[0161] 100 parts by weight of a multifunctional acrylate (manufactured by Arakawa Chemical Industries, Ltd., trade name "OPSTAR KZ6728", solid content 20% by weight), 3 parts by weight of a leveling agent (manufactured by DIC Corporation, "GRANDIC PC4100"), and 3 parts by weight of a photopolymerization initiator (manufactured by BASF Corporation, trade name "OMNIRAD907", solid content 100% by weight) were mixed. The mixture was stirred using butyl acetate as a diluent so that the solid content became 12% by weight, thereby preparing a coating liquid A for forming an antireflection layer.
[0162] (Anti-reflection layer forming coating liquid B)
[0163] 100 parts by weight of a multifunctional acrylate containing pentaerythritol triacrylate as the main component (manufactured by Osaka Organic Chemical Industry Co., Ltd., trade name "Viscoat #300", solid content 100% by weight), 150 parts by weight of hollow nano-silica particles (manufactured by JGC Catalysts & Chemicals Co., Ltd., trade name "THRULYA 5320", solid content 20% by weight, weight average particle size 75 nm), 50 parts by weight of solid nano-silica particles (manufactured by Nissan Chemical Industries, Ltd., trade name "MEK-2140Z-AC", solid content 30% by weight, weight average particle size 10 nm), 12 parts by weight of an additive containing a fluorine element (manufactured by Shin-Etsu Chemical Co., Ltd., trade name "KY-1203", solid content 20% by weight), and 3 parts by weight of a photopolymerization initiator (manufactured by BASF, trade name "OMNIRAD 907", solid content 100% by weight) were mixed. A mixed solvent of TBA (tert-butyl alcohol), MIBK (methyl isobutyl ketone) and PMA (propylene glycol monomethyl ether acetate) in a weight ratio of 60:25:15 was added to the mixture as a diluent so that the overall solid content reached 4 weight %, and the mixture was stirred to prepare a coating liquid B for forming an anti-reflection layer.
[0164] (Preparation of Adhesive)
[0165] An adhesive was prepared by mixing 62 parts by weight of hydroxyethyl acrylamide (manufactured by Kojin Co., Ltd., trade name "HEAA"), 25 parts by weight of acryloyl morpholine (manufactured by Kojin Co., Ltd., trade name "ACMO"), 7 parts by weight of PEG400# diacrylate (manufactured by Kyoeisha Chemical Co., Ltd., trade name "LIGHT ACRYLATE 9EG-A"), 3 parts by weight of "IRGACURE 907" manufactured by BASF, and 3 parts by weight of "KAYACUREDETX-S" manufactured by Nippon Kayaku Co., Ltd. for 60 minutes.
[0166] (Production of optical laminate)
[0167] The adhesive was applied to the λ / 4 member (stretched film) so as to have a thickness of 0.6 μm after curing, and then the positive C plate was bonded thereto to obtain a phase difference member.
[0168] The protective member (acrylic film having a hard coat layer and an antireflection layer formed thereon) was bonded to the λ / 4 member side of the obtained phase difference member via an adhesive layer having a thickness of 12 μm and a surface smoothness of 0.25 arcmin. The acrylic film of the protective member was bonded to the λ / 4 member side.
[0169] Next, a pressure-sensitive adhesive layer having a thickness of 12 μm and a surface smoothness of 0.25 arcmin was formed on the positive C plate side of the phase difference member to obtain an optical laminate.
[0170] [Example 2]
[0171] An optical laminate was obtained in the same manner as in Example 1 except that the adhesive was applied to the λ / 4 member so as to have a thickness of 0.9 μm after curing and then a positive C plate was bonded thereto.
[0172] [Example 3]
[0173] An optical laminate was obtained in the same manner as in Example 1 except that the adhesive was applied to the λ / 4 member so as to have a thickness of 1.3 μm after curing and then a positive C plate was bonded thereto.
[0174] [Comparative Example 1]
[0175] An optical laminate was obtained in the same manner as in Example 1 except that the adhesive was applied to the λ / 4 member so as to have a thickness of 1.5 μm after curing and then a positive C plate was bonded thereto.
[0176] [Comparative Example 2]
[0177] An optical laminate was obtained in the same manner as in Example 1 except that the adhesive was applied to the λ / 4 member so as to have a thickness of 1.9 μm after curing and then a positive C plate was bonded thereto.
[0178] [Comparative Example 3]
[0179] An optical laminate was obtained in the same manner as in Example 1 except that a pressure-sensitive adhesive (thickness 5 μm) was used instead of the adhesive when bonding the positive C plate to the λ / 4 member.
[0180] The optical layered bodies obtained in Examples and Comparative Examples were evaluated as follows.
[0181] (1) Laminated body smoothness
[0182] The smoothness of the laminate was measured using a phase-shift laser interferometer (manufactured by Zygo Corporation, product name "DynaFiz"). Specifically, the optical laminate was laminated on a micro-slide (manufactured by Matsunami Glass Industries, Ltd., product name "S200200") in a manner that did not introduce foreign matter, bubbles, or deformed stripes. Next, in order to remove the influence of tiny bubbles, degassing was performed using a pressurized degassing device (autoclave). The degassing conditions were set to 50°C, 0.5MPa, and 30 minutes. After degassing, the sample was naturally cooled at room temperature for more than 30 minutes to obtain a measurement sample.
[0183] The sample is placed on a measuring table with an anti-vibration table, and a single wavelength (633 nm) laser is used to interfere with a reference device that ensures flatness. For analysis, the value obtained by doubling the angle index "Slope magnitude RMS" obtained by selecting the frequency value of 0.1 / mm to 1 / mm (equivalent to 2σ) was defined as the laminate smoothness (unit: arcmin).
[0184] (2) Aesthetics
[0185] The appearance (light transmitted through the lens) of the optical layered body was evaluated using an optical lens (manufactured by Thorabs, trade name “LA1145”) and a point light source (manufactured by Hamamatsu Photonics, model “L8425-01”).
[0186] Specifically, an optical laminate cut into a circular shape of 45 mm φ was laminated to the flat side of the optical lens in a manner that foreign matter, bubbles, and deformed stripes were not introduced to the surface. Next, in order to remove the influence of microbubbles, degassing using a pressurized degassing device (autoclave) was performed. The degassing conditions were set to 50° C., 0.5 MPa, and 30 minutes. After degassing, the sample was naturally cooled at room temperature for more than 30 minutes to obtain a measurement sample.
[0187] A point light source, an optical lens (measurement sample), and a screen were set up in sequence, and the light from the point light source after passing through the optical lens was projected onto the screen to evaluate its aesthetics. The lens was held by a holding fixture at a position where the light from the point light source was incident from the convex side of the optical lens. The distance from the point light source to the screen was set to 1050 mm, and the distance from the optical lens to the screen was set to 130 mm.
[0188] Note that 10 panelists visually observed the light projected on the screen through an optical lens to determine the presence or absence of wrinkles and waviness, thereby evaluating the aesthetics. Table 1 shows the number of panelists who determined that there were no wrinkles and waviness.
[0189] (3) Durability
[0190] The optical laminate was subjected to a thermal shock test using a thermal shock apparatus (manufactured by ESPEC Corporation, product name “TSA-303EL-W”).
[0191] After the optical laminate cut into a 45 mm φ circle by a laser processing machine was bonded to a glass plate, it was placed in a temperature environment of -40°C for 0.5 hours, and then placed in a temperature environment of 85°C for 0.5 hours. The time spent on heating and cooling was set to within 6 minutes. After repeating this operation 100 times, the appearance of the optical laminate was observed with the naked eye to confirm the presence or absence of cracks and peeling.
[0192] (Evaluation Criteria)
[0193] Good: No cracks or peeling were observed
[0194] ·Defective: Cracks and / or peeling were observed
[0195] (4) Transmittance
[0196] For the optical laminate, the single transmittance Ts was measured using an ultraviolet visible spectrophotometer (V-7100 manufactured by JASCO Corporation). Ts is a Y value obtained by measuring the 2-degree field of view (C light source) of JIS Z 8701 and correcting the visibility. It should be noted that the optical laminate is provided for measurement in a state where it is not attached to a substrate such as glass.
[0197] [Table 1]
[0198] Example 1 Example 2 Example 3 Comparative Example 1 Comparative Example 2 Comparative Example 3 Thickness of adhesive layer (μm) 0.6 0.9 1.3 1.5 1.9 - Thickness of adhesive layer (μm) - - - - - 5 Laminated body smoothness (arcmin) 0.5 0.6 0.7 0.9 1.0 0.4 Aesthetics 10 / 10 10 / 10 8 / 10 5 / 10 0 / 10 10 / 10 Durability good good good good good bad Single body transmittance Y(%) 95.0 95.3 95.2 95.2 95.0 95.0
[0199] In the durability evaluation, cracks were observed in the positive C plate thinner than the λ / 4 member in Comparative Example 3. The length of the cracks was 10 mm or more, and a plurality of cracks occurred from the end of the sample, and were visually recognizable.
[0200] On the other hand, the optical layered body of Example 1 was subjected to the above-mentioned various evaluations after being placed in a temperature environment of 80°C for 500 hours or in a temperature environment of -40°C for 500 hours. The same results as those obtained when such temperature treatment was not performed (results shown in Table 1) were obtained.
[0201] The present invention is not limited to the above-described embodiments, and various modifications are possible. For example, the above-described embodiments may be replaced with substantially the same configuration, a configuration that exhibits the same effects, or a configuration that achieves the same purpose.
[0202] Industrial Applicability
[0203] The optical layered body according to the embodiment of the present invention can be used for a display body such as VR goggles, for example.
Claims
1. An optical laminate comprising: A laminated film having a substrate and a surface treatment layer, and Phase difference component, The substrate of the laminated film is arranged adjacent to the phase difference member, The phase difference component includes a first phase difference layer, an adhesive layer and a second phase difference layer in sequence. The adhesive layer has a thickness of 0.5 μm or more and 1.3 μm or less. 2 . The optical layered body according to claim 1 , wherein the layered body has a smoothness of 0.7 arcmin or less.
3. The optical layered body according to claim 1, in, The adhesive layer is a cured layer of resin.
4. The optical layered body according to claim 1, in, The surface smoothness of the laminated film is 0.5 arcmin or less.
5. The optical layered body according to claim 1, in, The substrate of the laminate film includes a (meth)acrylic resin.
6. The optical layered body according to claim 1, in, The surface treatment layer of the laminated film has an anti-reflection function.
7. The optical laminate according to claim 1, in, The first phase difference layer exhibits a refractive index characteristic of nx>ny≥nz, and satisfies the relationship of Re(450)<Re(550)<Re(650), Here, Re(450) represents the in-plane phase difference measured at 23°C with light of wavelength 450nm, Re(550) represents the in-plane phase difference measured at 23°C with light of wavelength 550nm, and Re(650) represents the in-plane phase difference measured at 23°C with light of wavelength 650nm.
8. The optical layered body according to claim 1, in, The second phase difference layer exhibits a refractive index characteristic of nz>nx≥ny. 9 . The optical layered body according to claim 1 , wherein the Y value of the visibility-corrected single body transmittance is 93% or more.
10. A lens unit used in a display system for displaying an image to a user, The lens portion comprises: A reflective polarizing member that reflects light emitted forward from a display surface of a display element that displays an image and that passes through the polarizing member and the first λ / 4 member; a first lens portion disposed on an optical path between the display element and the reflective polarization member, a half mirror disposed between the display element and the first lens portion, transmitting light emitted from the display element and reflecting light reflected from the reflective polarizing member toward the reflective polarizing member; a second lens portion disposed in front of the reflective polarization component; as well as The optical layered body according to any one of claims 1 to 9, which is arranged on an optical path between the half mirror and the reflective polarizing member.
11. A display method, comprising: a step of allowing the light of the display image emitted through the polarization element and the first λ / 4 element to pass through the half mirror and the first lens portion; a step of allowing the light that has passed through the half mirror and the first lens portion to pass through the optical layered body according to any one of claims 1 to 9; A step of reflecting the light after passing through the optical stack toward the half mirror at a reflective polarizing member; A step of allowing the light reflected by the reflective polarization member and the half mirror to pass through the reflective polarization member via the optical stack; as well as A step of allowing the light transmitted through the reflective polarization member to pass through a second lens unit.