Pressure relief device, battery monomer, battery, electric equipment and manufacturing method
Patent Information
- Application Number
- CN202280093853.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2022-11-09
- Publication Date
- 2024-11-08
AI Technical Summary
When a battery cell is impacted, the pressure relief structure often opens in advance, making it impossible to achieve normal pressure relief function.
A pressure relief device is designed, including a pressure relief part, a weak part and a welding part. The welding part anneals the weak part during molding, increases the thickness of the weak part to improve the resistance to external impact, and adjusts the The distance and position between the welding part and the weak part ensure that high temperature can effectively act on the weak part and ensure rapid pressure relief when the detonation pressure occurs.
It effectively reduces the risk of premature valve opening of the pressure relief structure, improves resistance to external impacts, reduces processing difficulty, and achieves rapid pressure relief.
Smart Images

Figure CN118922992A_ABST
Abstract
Description
Pressure relief device, battery cell, battery, electrical equipment and manufacturing method Technical Field
[0001] The present application relates to the field of batteries, and more specifically, to a pressure relief device, a battery cell, a battery, an electrical device, and a manufacturing method. Background Art
[0002] Batteries are widely used in new energy applications, such as electric vehicles and new energy vehicles, which have become a new trend in the automotive industry. The battery end caps are equipped with a pressure relief structure to release internal pressure when the battery reaches the detonation pressure. However, when a battery cell is impacted, the pressure relief structure often opens prematurely, preventing it from properly releasing pressure.
[0003] Summary of the Invention
[0004] The purpose of the embodiments of the present application is to provide a pressure relief device, a battery cell, a battery, an electrical device and a manufacturing method, which aims to improve the problem in the related art that the pressure relief structure often opens prematurely, resulting in the inability to achieve normal pressure relief function.
[0005] In a first aspect, an embodiment of the present application provides a pressure relief device for a battery cell, the pressure relief device comprising a pressure relief portion, a weakened portion, and a weld stamp portion, the weakened portion being arranged at the pressure relief portion, the weakened portion being configured to rupture when the battery cell is depressurized; the weld stamp portion being arranged at the pressure relief portion, the weld stamp portion being configured to anneal the weakened portion when it is formed.
[0006] In the above technical solution, the pressure relief device is provided with a welded portion on the pressure relief portion. The welded portion requires high-temperature ablation during the molding process. This high temperature will act on the weak portion, thereby annealing the weak portion (refining the material grains in the weak portion, releasing the internal stress of the material in the weak portion, and softening the weak portion). In this way, under the condition of consistent detonation pressure, the weak portion of the pressure relief device provided with the welded portion can be thicker than the weak portion of the pressure relief device without the welded portion. Increasing the thickness of the weak portion can improve resistance to external impacts and reduce the risk of premature valve opening. In addition, if the thickness of the weak portion is larger, the thickness required for processing and thinning is smaller, which can reduce the processing difficulty.
[0007] As an optional technical solution of the embodiment of the present application, in a direction perpendicular to the thickness direction of the pressure relief portion, a distance A between the welded portion and the weak portion satisfies: 0.5 mm ≤ A ≤ 10 mm.
[0008] In the above technical solution, the spacing between the weld stamp and the weak portion in a direction perpendicular to the thickness of the pressure relief portion is limited to between 0.5 and 10 mm. This ensures that the weak portion is effectively annealed during the weld stamp molding process while being less susceptible to damage. The spacing A cannot be too small, for example, if the spacing A is less than 0.5 mm, as this can easily damage the weak portion during the weld stamp molding process. The spacing A cannot be too large, for example, if the spacing A is greater than 10 mm, as this will cause the weld stamp to be too far from the weak portion, preventing the weak portion from being annealed during the weld stamp molding process.
[0009] As an optional technical solution of the embodiment of the present application, it also satisfies: 0.8mm≤A≤3mm.
[0010] In the above technical solution, in the direction perpendicular to the thickness direction of the pressure relief portion, the distance between the weld mark and the weak portion is limited to 0.8 to 3 mm, which can ensure a good annealing effect on the weak portion while not easily causing damage to the weak portion.
[0011] As an optional technical solution of the embodiment of the present application, the weld print portion is arranged around the weak portion.
[0012] In the above technical solution, the weld stamp is arranged around the weak part and located outside the weak part. In this way, during the forming process of the weld stamp, high temperature can act on the entire circumference of the weak part, achieving a good annealing effect. When the internal pressure of the battery cell reaches the detonation pressure, the weak part can quickly rupture and achieve rapid pressure relief.
[0013] As an optional technical solution of the embodiment of the present application, the weak portion is arranged around the weld print portion.
[0014] In the above technical solution, the weak portion is arranged around the weld mark, and the weld mark is located inside the weak portion. In this way, during the process of forming the weld mark, high temperature can also act on the entire circumference of the weak portion, achieving a good annealing effect. When the internal pressure of the battery cell reaches the detonation pressure, the weak portion can quickly rupture and achieve rapid pressure relief.
[0015] As an optional technical solution of an embodiment of the present application, the pressure relief device includes two weld prints, and the weak portion is located between the two weld prints along a first direction, and the first direction is perpendicular to the thickness direction of the pressure relief portion.
[0016] In the above technical solution, the weak portion is located between the two welded portions in the first direction. In this way, during the process of forming the two welded portions, the high temperature can fully act on the weak portion, achieving a good annealing effect. When the internal pressure of the battery cell reaches the detonation pressure, the weak portion can quickly rupture, thereby achieving rapid pressure relief.
[0017] As an optional technical solution of an embodiment of the present application, the weak portion is a closed structure extending along a closed trajectory.
[0018] In the above technical solution, by setting the weak part as a closed structure extending along a closed trajectory, when the internal pressure of the battery cell reaches the detonation pressure, the internal pressure can break open the weak part from all sides, making pressure release faster and easier.
[0019] As an optional technical solution of the embodiment of the present application, the welding portion is a closed structure extending along a closed track.
[0020] In the above technical solution, by setting the weld stamp as a closed structure extending along a closed track, the weld stamp can surround the weak part. In this way, during the forming process of the weld stamp, high temperature can fully act on the weak part, achieving a better annealing effect.
[0021] As an optional technical solution of the embodiment of the present application, the weld print portion includes a plurality of weld print segments, and the plurality of weld print segments are arranged at intervals along the circumference of the weak portion.
[0022] In the above technical solution, by arranging a plurality of weld printing sections at intervals along the circumference of the weak portion, compared with arranging weld printing sections along the entire circumference of the weak portion, energy consumption is lower, which can save production costs.
[0023] As an optional technical solution of the embodiment of the present application, the pressure relief portion is provided with a notched groove, and the pressure relief device forms the weak portion at the position of the notched groove.
[0024] In the above technical solution, a notched groove is provided on the pressure relief portion to form a weak portion, which is simple, convenient, easy to process and has a low production cost.
[0025] As an optional technical solution of the embodiment of the present application, along the thickness direction of the pressure relief portion, the notched groove and the weld mark are located on both sides of the pressure relief portion.
[0026] In the above technical solution, even if the notched groove and the weld stamp are located on both sides of the pressure relief portion along the thickness direction, during the process of forming the weld stamp, high temperature can be conducted to the location of the weak portion, thereby annealing the weak portion.
[0027] As an optional technical solution of the embodiment of the present application, along the thickness direction of the pressure relief portion, the notched groove and the weld mark portion are located on the same side of the pressure relief portion.
[0028] In the above technical solution, along the thickness direction, the notched groove and the weld stamp are located on the same side of the pressure relief portion. During the forming process of the weld stamp, high temperature is easily transferred to the location of the weak portion, thereby annealing the weak portion.
[0029] As an optional technical solution of the embodiment of the present application, the pressure relief device includes two weld prints, and along the thickness direction of the pressure relief portion, the two weld prints are located on both sides of the pressure relief portion.
[0030] In the above technical solution, during the process of forming the two welded portions, high temperature can be conducted to the location of the weak portion, thereby annealing the weak portion.
[0031] In a second aspect, an embodiment of the present application further provides a battery cell, wherein the battery cell includes the above-mentioned pressure relief device.
[0032] In a third aspect, an embodiment of the present application further provides a battery, which includes the above-mentioned battery cell.
[0033] In a fourth aspect, an embodiment of the present application further provides an electrical device, which includes the above-mentioned battery, and the battery is used to provide electrical energy.
[0034] In a fifth aspect, an embodiment of the present application further provides a method for manufacturing a pressure relief device, which is used for a battery cell. The method for manufacturing the pressure relief device includes: providing a pressure relief portion, which has a weak portion, and the weak portion is configured to crack when the battery cell is depressurized; and annealing the weak portion.
[0035] As an optional technical solution of an embodiment of the present application, in the step of annealing the weak portion: the pressure relief portion is laser welded to anneal the weak portion.
[0036] In the above technical solution, laser ablation of the pressure relief portion generates high temperatures that act on the weak portion, annealing it (refining the material grains in the weak portion, releasing internal stress in the material, and softening the weak portion). Thus, under the same detonation pressure, the weak portion of the pressure relief device with a welded portion can be thicker than the weak portion of the pressure relief device without a welded portion. Increasing the thickness of the weak portion improves resistance to external impacts and reduces the risk of premature valve opening. Furthermore, if the weak portion is thicker, a smaller thickness needs to be thinned, which reduces the processing difficulty.
[0037] As an optional technical solution of an embodiment of the present application, after the pressure relief part is laser welded, a weld mark part can be formed on the pressure relief part. In the direction perpendicular to the thickness direction of the pressure relief part, the distance between the weld mark part and the weak part is A, satisfying: 0.5mm≤A≤10mm.
[0038] In the above technical solution, the distance between the weld mark and the weak portion in a direction perpendicular to the thickness of the pressure relief portion is limited to between 0.5 and 10 mm. This ensures that the weak portion is effectively annealed during laser welding without damaging it. The distance A cannot be too small, for example, if the distance A is less than 0.5 mm, otherwise the weak portion may be easily damaged during laser welding. The distance A cannot be too large, for example, if the distance A is greater than 10 mm, otherwise the weld mark is too far from the weak portion, preventing annealing of the weak portion during laser welding. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the following is a brief introduction to the drawings required for use in the embodiments. It should be understood that the following drawings only show certain embodiments of the present application and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other relevant drawings can be obtained based on these drawings without creative work.
[0040] FIG1 is a schematic structural diagram of a vehicle provided in some embodiments of the present application;
[0041] FIG2 is an exploded view of a battery provided in some embodiments of the present application;
[0042] FIG3 is an exploded view of a battery cell provided in some embodiments of the present application;
[0043] FIG4 is a schematic structural diagram of a pressure relief device provided in some embodiments of the present application;
[0044] FIG5 is a schematic top view of a pressure relief device (with a welded portion disposed around a weak portion) provided in some embodiments of the present application;
[0045] FIG6 is a cross-sectional view taken along the line BB in FIG5 ;
[0046] FIG7 is a schematic top view of a pressure relief device (with a weak portion disposed around a welded portion) provided in some embodiments of the present application;
[0047] FIG8 is a cross-sectional view taken along the CC line in FIG7 ;
[0048] FIG9 is a schematic top view of a pressure relief device (a weak portion is located between two welded portions) provided in some embodiments of the present application;
[0049] FIG10 is a cross-sectional view of the DD position in FIG9;
[0050] FIG11 is a schematic top view of a pressure relief device (a weak portion is a non-enclosed structure extending along a non-enclosed track with a distance between the head and tail ends) provided in some embodiments of the present application;
[0051] FIG12 is a schematic top view of a pressure relief device (with multiple welded sections spaced apart along the circumference of a weak portion) provided in some embodiments of the present application;
[0052] FIG13 is a schematic top view of a pressure relief device provided in some other embodiments of the present application;
[0053] FIG14 is a cross-sectional view of the EE position in FIG13;
[0054] FIG15 is a schematic top view of a pressure relief device (with the notched groove and the welded portion located on both sides of the pressure relief portion) provided in some embodiments of the present application;
[0055] FIG16 is a cross-sectional view of the FF position in FIG15;
[0056] FIG17 is a schematic top view of a pressure relief device (two welded portions are located on both sides of the pressure relief portion) provided in some embodiments of the present application;
[0057] FIG18 is a cross-sectional view of the GG position in FIG17;
[0058] FIG19 is a schematic block diagram of a method for manufacturing a pressure relief device according to some embodiments of the present application.
[0059] Icons: 10-housing; 11-first part; 12-second part; 20-battery cell; 21-end cover; 22-electrode assembly; 23-housing; 24-pressure relief device; 241-weak part; 242-weld part; 2421-weld section; 243-notched groove; 244-pressure relief part; 30-manufacturing method of pressure relief device; 100-battery; 200-controller; 300-motor; 1000-vehicle. DETAILED DESCRIPTION
[0060] To make the purpose, technical solutions, and advantages of the embodiments of this application more clear, the technical solutions in the embodiments of this application will be clearly described below in conjunction with the drawings in the embodiments of this application. Obviously, the described embodiments are part of the embodiments of this application, not all of the embodiments. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of this application.
[0061] Unless otherwise defined, all technical and scientific terms used in this application have the same meanings as commonly understood by those skilled in the art to which this application belongs. The terms used in the specification of this application are for the purpose of describing specific embodiments only and are not intended to limit this application. The terms "including" and "having" and any variations thereof in the specification and claims of this application and the above-mentioned drawings are intended to cover non-exclusive inclusions. The terms "first" and "second" in the specification and claims of this application or the above-mentioned drawings are used to distinguish different objects, rather than to describe a specific order or a primary-secondary relationship.
[0062] References to "embodiments" in this application mean that a particular feature, structure, or characteristic described in connection with the embodiment may be included in at least one embodiment of the application. The appearance of this phrase in various places in the specification does not necessarily refer to the same embodiment, nor does it constitute an independent or alternative embodiment that is mutually exclusive of other embodiments.
[0063] In the description of this application, it should be noted that, unless otherwise expressly specified or limited, the terms "mounted," "connected," "connected," and "attached" should be understood in a broad sense. For example, they may refer to fixed connections, detachable connections, or integral connections; they may refer to direct connections, indirect connections through an intermediate medium, or internal connections between two components. Those skilled in the art will understand the specific meanings of the above terms in this application based on specific circumstances.
[0064] The term "and / or" in this application simply describes an association between related objects, indicating that three possible relationships exist. For example, A and / or B can represent: A exists alone, A and B exist simultaneously, and B exists alone. In addition, the character " / " in this application generally indicates that the related objects are in an "or" relationship.
[0065] In the embodiments of this application, the same reference numerals represent the same components, and for the sake of brevity, detailed descriptions of the same components in different embodiments are omitted. It should be understood that the thickness, length, width, and other dimensions of the various components in the embodiments of this application, as well as the overall thickness, length, width, and other dimensions of the integrated device shown in the drawings are merely illustrative and should not constitute any limitation on this application.
[0066] The term "plurality" used in this application refers to two or more (including two).
[0067] In this application, battery cells may include lithium-ion secondary batteries, lithium-ion primary batteries, lithium-sulfur batteries, sodium-lithium-ion batteries, sodium-ion batteries, or magnesium-ion batteries, etc., and the embodiments of this application do not limit this. Battery cells may be cylindrical, flat, rectangular, or other shapes, etc., and the embodiments of this application do not limit this. Battery cells are generally divided into three types based on the packaging method: cylindrical battery cells, prismatic battery cells, and soft-pack battery cells, and the embodiments of this application do not limit this.
[0068] The battery referred to in the embodiments of this application refers to a single physical module that includes one or more battery cells to provide higher voltage and capacity. For example, the battery referred to in this application may include a battery module or a battery pack. A battery generally includes a casing that encloses one or more battery cells. The casing prevents liquids or other foreign matter from affecting the charging or discharging of the battery cells.
[0069] A battery cell includes an electrode assembly and an electrolyte. The electrode assembly consists of a positive electrode sheet, a negative electrode sheet, and a separator. A battery cell primarily operates by the movement of metal ions between the positive and negative electrode sheets. The positive electrode sheet comprises a positive current collector and a positive active material layer. The positive active material layer is coated on the surface of the positive electrode collector. The portion of the positive electrode collector not coated with the positive active material layer protrudes from the portion coated with the positive active material layer. The portion of the positive electrode collector not coated with the positive active material layer serves as the positive electrode tab. For lithium-ion batteries, for example, the positive electrode current collector can be made of aluminum, and the positive active material can be lithium cobalt oxide, lithium iron phosphate, ternary lithium, or lithium manganese oxide. The negative electrode sheet comprises a negative current collector and a negative active material layer. The negative active material layer is coated on the surface of the negative electrode collector. The portion of the negative electrode collector not coated with the negative active material layer protrudes from the portion coated with the negative active material layer. The portion of the negative electrode collector not coated with the negative active material layer serves as the negative electrode tab. The negative electrode current collector can be made of copper, and the negative active material can be carbon or silicon, among others. To ensure high current flow without melting, multiple positive tabs are stacked together, and multiple negative tabs are stacked together. The separator can be made of materials such as PP (polypropylene) or PE (polyethylene). Furthermore, the electrode assembly can be a wound or laminated structure, but the present invention is not limited thereto.
[0070] Currently, market developments indicate that batteries are increasingly being used. They are not only used in energy storage systems such as hydropower, thermal, wind, and solar power plants, but are also widely used in electric vehicles like electric bicycles, electric motorcycles, and electric cars, as well as in military equipment and aerospace. As battery applications continue to expand, market demand is also growing.
[0071] The development of battery technology must take into account multiple design factors at the same time, such as energy density, cycle life, discharge capacity, charge and discharge rate and other performance parameters. In addition, battery safety must also be considered.
[0072] For battery cells, in order to ensure the safety of the battery cells, a pressure relief structure can be set on the end cover of the battery cells. For example, a weak part can be set on the end cover. When the internal pressure of the battery cell reaches the detonation pressure, the weak part opens to release the pressure inside the battery cell, thereby reducing the risk of explosion and fire of the battery cell.
[0073] The inventors have noticed that when a battery cell is impacted, the pressure relief structure often opens prematurely, resulting in failure to achieve a normal pressure relief function.
[0074] The inventors further discovered that when a battery cell is impacted, the external impact force is easily transmitted to the location of the pressure relief structure, causing the pressure relief structure to open prematurely, resulting in failure to achieve the normal pressure relief function.
[0075] In view of this, embodiments of the present application provide a pressure relief device comprising a pressure relief portion, a weakened portion, and a welded portion. The weakened portion is provided on the pressure relief portion and is configured to rupture when pressure is released from a battery cell. The welded portion is provided on the pressure relief portion and is configured to anneal the weakened portion during its formation.
[0076] The pressure relief device's pressure relief section is provided with a welded portion. This welded portion requires high-temperature ablation during the molding process. This high temperature acts on the weak portion, annealing it (refining the material grain size, releasing internal stress, and softening it). Thus, under the same detonation pressure, the weak portion of the pressure relief device with the welded portion can be thicker than the weak portion of the pressure relief device without the welded portion. Increasing the thickness of the weak portion improves resistance to external impacts and reduces the risk of premature valve opening.
[0077] In addition, if the thickness of the weak part is larger, the thickness that needs to be thinned is smaller, which can reduce the processing difficulty.
[0078] The technical solutions described in the embodiments of the present application are applicable to batteries and electrical devices using batteries.
[0079] Electrically powered devices may include vehicles, mobile phones, portable devices, laptop computers, ships, spacecraft, electric toys, and electric tools. Spacecraft include airplanes, rockets, space shuttles, and spacecraft. Electric toys include fixed or mobile electric toys, such as game consoles, electric car toys, electric ship toys, and electric airplane toys. Electric tools include metal cutting power tools, grinding power tools, assembly power tools, and railway power tools, such as electric drills, electric grinders, electric wrenches, electric screwdrivers, electric hammers, impact drills, concrete vibrators, and electric planers. The embodiments of the present application do not impose any special restrictions on the above-mentioned electrical devices.
[0080] For the convenience of description, the following embodiments are described by taking the electric device as a vehicle 1000 as an example.
[0081] Please refer to Figure 1, which is a schematic structural diagram of a vehicle 1000 provided in some embodiments of the present application. The vehicle 1000 can be a fuel vehicle, a gas vehicle or a new energy vehicle. The new energy vehicle can be a pure electric vehicle, a hybrid vehicle or an extended-range vehicle, etc. A battery 100 is provided inside the vehicle 1000, and the battery 100 can be provided at the bottom, head or tail of the vehicle 1000. The battery 100 can be used to power the vehicle 1000. For example, the battery 100 can serve as an operating power source for the vehicle 1000. The vehicle 1000 may also include a controller 200 and a motor 300. The controller 200 is used to control the battery 100 to power the motor 300, for example, for starting, navigating and driving the vehicle 1000.
[0082] In some embodiments of the present application, the battery 100 can serve not only as an operating power source for the vehicle 1000, but also as a driving power source for the vehicle 1000, replacing or partially replacing fuel or natural gas to provide driving power for the vehicle 1000.
[0083] Please refer to Figure 2, which is an exploded view of a battery 100 provided in some embodiments of the present application. The battery 100 includes a housing 10 and a battery cell 20, with the battery cell 20 housed within the housing 10. The housing 10 provides a storage space for the battery cell 20 and can have various structures. In some embodiments, the housing 10 can include a first portion 11 and a second portion 12, which overlap each other and together define a storage space for the battery cell 20. The second portion 12 can be a hollow structure with one end open. The first portion 11 can be a plate-like structure, with the first portion 11 overlapping the open side of the second portion 12, so that the first portion 11 and the second portion 12 together define a storage space. Alternatively, the first portion 11 and the second portion 12 can each be a hollow structure with one end open, with the open side of the first portion 11 overlapping the open side of the second portion 12. Of course, the housing 10 formed by the first portion 11 and the second portion 12 can have various shapes, such as a cylinder, a rectangular parallelepiped, etc.
[0084] In the battery 100, there may be multiple battery cells 20, and the multiple battery cells 20 may be connected in series, in parallel, or in a hybrid connection. A hybrid connection refers to a combination of series and parallel connections among the multiple battery cells 20. The multiple battery cells 20 may be directly connected in series, in parallel, or in a hybrid connection, and then the entire battery cell 20 may be housed within the housing 10. Alternatively, the battery 100 may be constructed by first connecting multiple battery cells 20 in series, in parallel, or in a hybrid connection to form a battery module, which is then connected in series, in parallel, or in a hybrid connection to form a complete battery module, and then housed within the housing 10. The battery 100 may also include other structures, such as a busbar assembly for electrically connecting the multiple battery cells 20.
[0085] Each battery cell 20 may be a secondary battery cell or a primary battery cell; it may also be a lithium-sulfur battery cell, a sodium-ion battery cell, or a magnesium-ion battery cell, but is not limited thereto. The battery cell 20 may be cylindrical, flat, rectangular, or in other shapes.
[0086] Please refer to Figure 3, which is an exploded view of a battery cell 20 provided in some embodiments of the present application. A battery cell 20 is the smallest unit that makes up a battery 100. As shown in Figure 3, a battery cell 20 includes an end cap 21, an electrode assembly 22, a housing 23, a pressure relief device 24 (not shown in Figure 3), and other functional components.
[0087] The end cap 21 refers to a component that covers the opening of the housing 23 to isolate the internal environment of the battery cell 20 from the external environment. Without limitation, the shape of the end cap 21 can be adapted to the shape of the housing 23 to match the housing 23. Optionally, the end cap 21 can be made of a material with a certain hardness and strength (such as an aluminum alloy). In this way, the end cap 21 is less likely to deform when squeezed or collided, so that the battery cell 20 can have a higher structural strength and improved safety performance. Functional components such as electrode terminals (not shown in the figure) can be provided on the end cap 21. The electrode terminals can be used to electrically connect to the electrode assembly 22 for outputting or inputting electrical energy from the battery cell 20. The material of the end cap 21 can also be various, such as copper, iron, aluminum, stainless steel, aluminum alloy, plastic, etc., and this embodiment of the present application does not impose any special restrictions on this. In some embodiments, an insulating member can also be provided on the inner side of the end cap 21. The insulating member can be used to isolate the electrical connection components in the housing 23 from the end cap 21 to reduce the risk of short circuits. For example, the insulating member may be made of plastic, rubber, or the like.
[0088] The housing 23 is a component that cooperates with the end cap 21 to form the internal environment of the battery cell 20. This internal environment can be used to accommodate the electrode assembly 22, electrolyte, and other components. The housing 23 and the end cap 21 can be separate components. An opening can be provided in the housing 23, and the end cap 21 is placed over the opening to form the internal environment of the battery cell 20. Alternatively, the end cap 21 and the housing 23 can be integrated. Specifically, the end cap 21 and the housing 23 can form a common connection surface before other components are inserted into the housing. When the interior of the housing 23 is to be enclosed, the end cap 21 is placed over the housing 23. The housing 23 can be of various shapes and sizes, such as a rectangular parallelepiped, a cylinder, or a hexagonal prism. Specifically, the shape of the housing 23 can be determined based on the specific shape and size of the electrode assembly 22. The housing 23 can be made of a variety of materials, such as copper, iron, aluminum, stainless steel, aluminum alloy, plastic, etc., and this embodiment of the present application does not impose any particular limitations on this.
[0089] The electrode assembly 22 is a component in the battery cell 20 where electrochemical reactions occur. One or more electrode assemblies 22 may be contained in the housing 23. The electrode assembly 22 is mainly formed by winding or stacking positive and negative electrode sheets, and a separator is usually provided between the positive and negative electrode sheets. The parts of the positive and negative electrode sheets with active materials constitute the main body of the electrode assembly 22, and the parts of the positive and negative electrode sheets without active materials each constitute a tab. The positive tab and the negative tab may be located together at one end of the main body or respectively at both ends of the main body. During the charge and discharge process of the battery 100, the positive electrode active material and the negative electrode active material react with the electrolyte, and the tabs connect the electrode terminals to form a current loop.
[0090] The pressure relief device 24 is a component that releases pressure within the battery cell 20. When the pressure within the battery cell 20 reaches the detonation pressure, the pressure within the battery cell 20 is released through the pressure relief device 24. The pressure relief device 24 can be a component installed on the end cap 21, or the housing 23 or the end cap 21 can function as the pressure relief device 24. The specific structure of the pressure relief device 24 is described in detail below with reference to the accompanying drawings.
[0091] Please refer to Figures 4, 5 and 6. Figure 4 is a schematic structural diagram of the pressure relief device 24 provided in some embodiments of the present application. Figure 5 is a schematic top view of the pressure relief device 24 (the weld stamp 242 is arranged around the weak portion 241) provided in some embodiments of the present application. Figure 6 is a cross-sectional view of the BB position in Figure 5. An embodiment of the present application provides a pressure relief device 24 for a battery cell 20. The pressure relief device 24 includes a pressure relief portion 244, a weak portion 241 and a weld stamp 242. The weak portion 241 is arranged in the pressure relief portion 244, and the weak portion 241 is configured to crack when the battery cell 20 is depressurized. The weld stamp 242 is arranged in the pressure relief portion 244, and the weld stamp 242 is configured to anneal the weak portion 241 when it is formed.
[0092] The pressure relief portion 244 can be a component mounted on the end cover 21, for example, the pressure relief portion 244 is a bursting disk mounted on the end cover 21. The pressure relief portion 244 can also serve as the entire end cover 21; the pressure relief portion 244 can be a part of the housing 23, for example, the pressure relief portion 244 can be a wall portion of the housing 23 or a part of a wall portion.
[0093] The weak portion 241 is the lower-strength portion of the pressure relief portion 244. When the internal pressure of the battery cell 20 reaches the detonation pressure, the weak portion 241 opens under the pressure, releasing the internal pressure of the battery cell 20 and reducing the risk of explosion or fire in the battery cell 20. It should be noted that the dotted line in Figure 6 is intended to indicate the extent of the weak portion 241 and does not represent the actual structure.
[0094] The weld mark portion 242 is a portion of the pressure relief portion 244 that is left with a weld mark after the pressure relief portion 244 is welded. The welding method is not limited, for example, gas welding, electric welding, laser welding, etc.
[0095] The pressure relief portion 244 of the pressure relief device 24 is provided with a welded portion 242. The welded portion 242 requires high-temperature ablation during the molding process. This high temperature acts on the weak portion 241, thereby annealing the weak portion 241 (refining the material grains of the weak portion 241, releasing the internal stress of the material of the weak portion 241, and softening the weak portion 241). Thus, under the same detonation pressure, the weak portion 241 of the pressure relief device 24 provided with the welded portion 242 can be thicker than the weak portion 241 of the pressure relief device 24 without the welded portion 242. Increasing the thickness of the weak portion 241 can improve resistance to external impacts and reduce the risk of premature valve opening. Furthermore, if the thickness of the weak portion 241 is greater, the thickness required for thinning is smaller, which can reduce the processing difficulty.
[0096] In some embodiments, in a direction perpendicular to the thickness direction of the pressure relief portion 244 , a distance A between the welded portion 242 and the weak portion 241 satisfies: 0.5 mm ≤ A ≤ 10 mm.
[0097] A represents the distance between the weld stamp 242 and the weak portion 241 in a direction perpendicular to the thickness of the pressure relief portion 244. "Spacing" refers to the distance between the edge of the weld stamp 242 on the side closest to the weak portion 241 and the edge of the weak portion 241 on the side closest to the weld stamp 242. The value of A can be the same or different at different locations, but the minimum value of A is no less than 0.5 mm and the maximum value is no more than 10 mm. In a direction perpendicular to the thickness of the pressure relief portion 244, the distance between the weld stamp 242 and the weak portion 241 can be: A = 0.5 mm, 1 mm, 2 mm, 3 mm, 4 mm, 5 mm, 6 mm, 7 mm, 8 mm, 9 mm, 10 mm, etc.
[0098] The distance between the weld stamp portion 242 and the weak portion 241 in a direction perpendicular to the thickness direction of the pressure relief portion 244 is limited to between 0.5 and 10 mm, so that the weak portion 241 can be annealed well during the forming process of the weld stamp portion 242 without being easily damaged.
[0099] Please refer to Table 1, which shows the test data of the detonation pressure of the battery cell 20 at different spacings. In the table, H1 is the thickness of the weak portion 241, in mm. P1 is the detonation pressure of the battery cell 20 before the weld stamp 242 is formed, in MPa. A is the distance between the weld stamp 242 and the weak portion 241 in a direction perpendicular to the thickness direction of the pressure relief portion 244, in mm. P2 is the detonation pressure of the battery cell 20 after the weld stamp 242 is formed, in MPa. H2 is the thickness of the weak portion 241 when the weld stamp 242 is not provided and the detonation pressure reaches P2, in mm. The notes are a brief description of the test data.
[0100] Table 1
[0101]
[0102] Refer to Table 1. It can be seen that the spacing A cannot be too small. For example, if the spacing A is less than 0.5 mm, the weak portion 241 may be easily damaged during the forming process of the weld stamp 242. The spacing A cannot be too large either. For example, if the spacing A is greater than 10 mm, the weld stamp 242 is too far away from the weak portion 241, and the weak portion 241 cannot be annealed during the forming process of the weld stamp 242.
[0103] In some embodiments, the following condition is also satisfied: 0.8 mm ≤ A ≤ 3 mm.
[0104] In a direction perpendicular to the thickness direction of the pressure relief portion 244 , a distance A between the welded portion 242 and the weak portion 241 satisfies: 0.8 mm ≤ A ≤ 3 mm.
[0105] In a direction perpendicular to the thickness direction of the pressure relief portion 244 , the distance between the welded portion 242 and the weak portion 241 may be: A=0.8mm, 0.9mm, 1mm, 1.2mm, 1.5mm, 1.7mm, 2mm, 2.2mm, 2.5mm, 2.8mm, 3mm, etc.
[0106] Refer to Table 1. It can be seen that when 3mm < A ≤ 10mm, the annealing effect is not significant, and the detonation pressure of the battery cell 20 behind the molded weld mark 242 decreases slightly. When 0.5mm ≤ A < 0.8mm, while the annealing effect is more significant, the spacing accuracy required is high. Even slight variations in spacing will result in significant changes in the detonation pressure of the battery cell 20 behind the molded weld mark 242, making it difficult to control the detonation pressure of the battery cell 20 behind the molded weld mark 242. Furthermore, since the distance to the weak portion 241 is closer when 0.5mm ≤ A < 0.8mm, the risk of damaging the weak portion 241 is greater.
[0107] In a direction perpendicular to the thickness direction of the pressure relief portion 244 , the distance between the weld stamp 242 and the weak portion 241 is limited to 0.8 to 3 mm, which can ensure a good annealing effect on the weak portion 241 while not easily causing damage to the weak portion 241 .
[0108] 5 and 6 , in some embodiments, the weld stamp 242 is disposed around the weak portion 241 .
[0109] The weld stamp 242 extends along the circumference of the weak portion 241 and is located outside the weak portion 241. For example, when the weak portion 241 is a strip-shaped structure, the weld stamp 242 may be a ring-shaped structure, surrounding the weak portion 241 so that the weak portion 241 is located inside the weld stamp 242. For another example, when the weak portion 241 is a ring-shaped structure, the weld stamp 242 may also be a ring-shaped structure, surrounding the weak portion 241 so that the weak portion 241 is located inside the weld stamp 242.
[0110] The welded portion 242 is disposed around the weak portion 241 and is located outside the weak portion 241. This allows high temperatures to be applied to the entire circumference of the weak portion 241 during the forming process, achieving a good annealing effect. This allows the weak portion 241 to rupture quickly when the internal pressure of the battery cell 20 reaches the detonation pressure, achieving rapid pressure relief.
[0111] Please refer to Figures 7 and 8. Figure 7 is a top view of a pressure relief device 24 (with a weakened portion 241 disposed around a welded portion 242) provided in some embodiments of the present application. Figure 8 is a cross-sectional view taken along the CC axis of Figure 7. In some embodiments, the weakened portion 241 is disposed around the welded portion 242.
[0112] The weld stamp 242 extends along the circumference of the weak portion 241 and is located inside the weak portion 241. For example, when the weak portion 241 is an annular structure, the weld stamp 242 may also be an annular structure, and the weak portion 241 surrounds the weld stamp 242, so that the weld stamp 242 is located inside the weak portion 241.
[0113] It should be noted that the dotted line in FIG8 is for marking the range of the weak portion 241 and does not represent the actual structure.
[0114] The weak portion 241 is arranged around the welded portion 242, and the welded portion 242 is located inside the weak portion 241. In this way, during the forming process of the welded portion 242, high temperature can also act on the entire circumference of the weak portion 241, achieving a good annealing effect. When the internal pressure of the battery cell 20 reaches the detonation pressure, the weak portion 241 can quickly rupture and achieve rapid pressure relief.
[0115] Please refer to Figures 9 and 10. Figure 9 is a schematic top view of a pressure relief device 24 (with a weak portion 241 located between two welded portions 242) provided in some embodiments of the present application. Figure 10 is a cross-sectional view taken along the DD axis of Figure 9. In some embodiments, the pressure relief device 24 includes two welded portions 242, with the weak portion 241 located between the two welded portions 242 along a first direction. The first direction is perpendicular to the thickness of the pressure relief portion 244.
[0116] The first direction is a direction perpendicular to the thickness direction of the pressure relief portion 244 .
[0117] The weak portion 241 is located between the two welded portions 242 in the first direction, or in other words, the weak portion 241 is located between the two welded portions 242 along the first direction. For example, the weak portion 241 and the two welded portions 242 are both ring-shaped structures, with one welded portion 242 located inside the weak portion 241 and the other welded portion 242 located outside the weak portion 241. For another example, the weak portion 241 and the two welded portions 242 are both strip-shaped structures, and the two welded portions 242 are located on either side of the weak portion 241 along the first direction.
[0118] It should be noted that the dotted line in FIG. 10 is for marking the range of the weak portion 241 and does not represent the actual structure.
[0119] By positioning the weak portion 241 between the two welded portions 242 in the first direction, high temperature can fully act on the weak portion 241 during the process of forming the two welded portions 242, achieving a good annealing effect. This allows the weak portion 241 to quickly rupture when the internal pressure of the battery cell 20 reaches the detonation pressure, thereby achieving rapid pressure relief.
[0120] In some embodiments, the weak portion 241 is a closed structure extending along a closed trajectory.
[0121] A "closed track" refers to a track that is connected at both ends. A closed track can be a circular track, an elliptical track, a polygonal track, etc. Since the weak portion 241 extends along the closed track, the weak portion 241 can also be circular, elliptical, polygonal, etc.
[0122] By configuring the weak portion 241 as a closed structure extending along a closed trajectory, when the internal pressure of the battery cell 20 reaches the detonation pressure, the internal pressure can open the weak portion 241 from all sides, making pressure release faster and easier.
[0123] Please refer to Figure 11, which is a top view of a pressure relief device 24 provided in some embodiments of the present application (where the weak portion 241 is a non-enclosed structure extending along a non-enclosed track with a distance between the end portions). In other embodiments, the weak portion 241 is a non-enclosed structure extending along a non-enclosed track with a distance between the end portions.
[0124] The non-closed track with a distance between the ends can be a U-shaped track, a C-shaped track, a circular arc track, a parabola track, etc. The weak portion 241 extends along the non-closed track with a distance between the ends, so the weak portion 241 can also be U-shaped, C-shaped, circular arc-shaped, parabola-shaped, etc.
[0125] In some embodiments, the weld print 242 is a closed structure extending along a closed track.
[0126] Since the weld mark portion 242 extends along a closed track, the weld mark portion 242 may also be circular, elliptical, polygonal, etc.
[0127] By setting the weld stamp 242 as a closed structure extending along a closed track, the weld stamp 242 can surround the weak portion 241. In this way, during the molding process of the weld stamp 242, high temperature can fully act on the weak portion 241, achieving a better annealing effect.
[0128] Please refer to Figure 12, which is a top view of a pressure relief device 24 provided in some embodiments of the present application (with multiple weld segments 2421 spaced apart along the circumference of a weakened portion 241). In some embodiments, the weld portion 242 includes multiple weld segments 2421 spaced apart along the circumference of the weakened portion 241.
[0129] The weld section 2421 is a part of the weld portion 242, and a plurality of weld sections 2421 form the weld portion 242. The weld section 2421 is also formed by welding the pressure relief portion 244. The welding method is not limited, for example, gas welding, electric welding, laser welding, etc.
[0130] By arranging a plurality of weld stamp segments 2421 at intervals along the circumference of the weak portion 241 , compared with arranging weld stamp portions 242 along the entire circumference of the weak portion 241 , energy consumption is lower, which can save production costs.
[0131] In some embodiments, the pressure relief portion 244 is provided with a notch groove 243 , and the pressure relief device 24 forms a weak portion 241 at the location of the notch groove 243 .
[0132] The notched groove 243 can be formed in a variety of ways, such as stamping, milling, etc. The notched groove 243 can be provided on the surface of the pressure relief portion 244 facing the interior of the housing 23, or on the surface of the pressure relief portion 244 facing away from the housing 23. Taking the pressure relief portion 244 as a rectangular flat plate structure as an example, the pressure relief portion 244 has an inner surface and an outer surface that are opposite to each other in the thickness direction, with the inner surface of the pressure relief portion 244 facing the interior of the housing 23 and the outer surface of the pressure relief portion 244 facing away from the housing 23. The notched groove 243 can be provided on the inner surface of the pressure relief portion 244, or on the outer surface of the pressure relief portion 244.
[0133] The scored groove 243 may be a groove recessed from the outer surface of the pressure relief portion 244 along the thickness direction of the pressure relief portion 244, and the weak portion 241 is the portion of the pressure relief portion 244 located between the inner surface and the bottom surface of the scored groove 243. The scored groove 243 may also be a groove recessed from the inner surface of the pressure relief portion 244 along the thickness direction of the pressure relief portion 244, and the weak portion 241 is the portion of the pressure relief portion 244 located between the outer surface and the bottom surface of the scored groove 243.
[0134] For example, the notched groove 243 may be a groove recessed from the outer surface of the pressure relief portion 244 along the thickness direction of the pressure relief portion 244 . The notched groove 243 may be a linear groove extending along a bending trajectory. For example, referring to FIG11 , the bending trajectory is a U-shaped trajectory, and the weak portion 241 is the U-shaped portion of the pressure relief portion 244 located between the inner surface and the bottom surface of the notched groove 243 .
[0135] For another example, please refer to Figures 13 and 14. Figure 13 is a schematic top view of the pressure relief device 24 provided in other embodiments of the present application. Figure 14 is a cross-sectional view of the EE position in Figure 13. The notched groove 243 is a strip groove extending along the width direction of the pressure relief portion 244. The weak portion 241 is the strip portion of the pressure relief portion 244 located between the inner surface and the bottom surface of the notched groove 243. It should be noted that the dotted line in Figure 14 is for marking the range of the weak portion 241 and does not represent the actual structure.
[0136] The notched groove 243 is provided on the pressure relief portion 244 to form the weak portion 241 , which is simple, convenient, easy to process and has a low production cost.
[0137] Please refer to Figures 15 and 16. Figure 15 is a top view of a pressure relief device 24 (with the notched groove 243 and the welded portion 242 located on either side of the pressure relief portion 244) provided in some embodiments of the present application. Figure 16 is a cross-sectional view taken at position FF in Figure 15. In some embodiments, the notched groove 243 and the welded portion 242 are located on either side of the pressure relief portion 244 along the thickness direction of the pressure relief portion 244.
[0138] The scored groove 243 can be a groove recessed from the outer surface of the pressure relief portion 244 along the thickness direction of the pressure relief portion 244. In this case, the welded portion 242 can be provided on the inner surface of the pressure relief portion 244. The scored groove 243 can be a groove recessed from the inner surface of the pressure relief portion 244 along the thickness direction of the pressure relief portion 244. In this case, the welded portion 242 can be provided on the outer surface of the pressure relief portion 244. In this way, the scored groove 243 and the welded portion 242 are located on both sides of the pressure relief portion 244 along the thickness direction.
[0139] It should be noted that the dotted line in Figure 15 indicates the position of the weld mark 242. The dotted line in Figure 16 is for marking the range of the weak portion 241 and does not represent the actual structure.
[0140] Even if the notched groove 243 and the weld stamp 242 are located on both sides of the pressure relief portion 244 along the thickness direction, during the process of forming the weld stamp 242 , high temperature can be conducted to the location of the weak portion 241 , thereby annealing the weak portion 241 .
[0141] In some embodiments, along the thickness direction of the pressure relief portion 244 , the score groove 243 and the weld stamp 242 are located on the same side of the pressure relief portion 244 .
[0142] The scored groove 243 can be a groove recessed from the outer surface of the pressure relief portion 244 along the thickness direction of the pressure relief portion 244. In this case, the weld stamp 242 can be provided on the outer surface of the pressure relief portion 244. The scored groove 243 can also be a groove recessed from the inner surface of the pressure relief portion 244 along the thickness direction of the pressure relief portion 244. In this case, the weld stamp 242 can be provided on the inner surface of the pressure relief portion 244. In this way, the scored groove 243 and the weld stamp 242 are located on the same side of the pressure relief portion 244 along the thickness direction.
[0143] Along the thickness direction, the notched groove 243 and the weld stamp 242 are located on the same side of the pressure relief portion 244 . During the forming process of the weld stamp 242 , high temperature is easily transferred to the location of the weak portion 241 , thereby annealing the weak portion 241 .
[0144] Please refer to Figures 17 and 18. Figure 17 is a top view of a pressure relief device 24 (with two welded portions 242 located on either side of the pressure relief portion 244) provided in some embodiments of the present application. Figure 18 is a cross-sectional view taken at position GG in Figure 17. In some embodiments, the pressure relief device 24 includes two welded portions 242 located on either side of the pressure relief portion 244 along its thickness.
[0145] The notch groove 243 may be provided on one of the inner surface of the pressure relief portion 244 and the outer surface of the pressure relief portion 244. The two weld marks 242 are provided on the outer surface of the pressure relief portion 244 and the inner surface of the pressure relief portion 244, respectively.
[0146] It should be noted that the dotted line in FIG18 is for marking the range of the weak portion 241 and does not represent the actual structure.
[0147] During the process of forming the two weld imprints 242 , the high temperature can be conducted to the location of the weak portion 241 , thereby annealing the weak portion 241 .
[0148] The embodiment of the present application further provides a battery cell 20 , which includes the above-mentioned pressure relief device 24 .
[0149] The embodiment of the present application further provides a battery 100 , which includes the above-mentioned battery cell 20 .
[0150] An embodiment of the present application further provides an electrical device, which includes the above-mentioned battery 100, and the battery 100 is used to provide electrical energy.
[0151] Please refer to FIG19, which is a schematic block diagram of a method 30 for manufacturing a pressure relief device according to some embodiments of the present application. The present application also provides a method 30 for manufacturing a pressure relief device, wherein the pressure relief device 24 is used for a battery cell 20. The method 30 for manufacturing a pressure relief device includes:
[0152] Step S1: providing a pressure relief portion 244. The pressure relief portion 244 has a weak portion 241, and the weak portion 241 is configured to break when the battery cell 20 is pressure-relieved.
[0153] Step S2: annealing the weak portion 241 .
[0154] In some embodiments, during the step of annealing the weak portion 241:
[0155] The pressure relief portion 244 is laser welded to anneal the weak portion 241. By laser ablation of the pressure relief portion 244, the high temperature generated by the laser ablation acts on the weak portion 241, thereby annealing the weak portion 241 (refining the material grains of the weak portion 241, releasing the internal stress of the material of the weak portion 241, and softening the weak portion 241). In this way, under the same detonation pressure, the weak portion 241 of the pressure relief device 24 with the welded portion 242 can be thicker than the weak portion 241 of the pressure relief device 24 without the welded portion 242. Increasing the thickness of the weak portion 241 can improve resistance to external impacts and reduce the risk of premature valve opening. In addition, if the thickness of the weak portion 241 is large, the thickness required for processing and thinning is smaller, which can reduce the processing difficulty.
[0156] In some embodiments, after laser welding the pressure relief portion 244, a weld mark 242 can be formed on the pressure relief portion 244. In a direction perpendicular to the thickness direction of the pressure relief portion 244, the distance between the weld mark 242 and the weak portion 241 is A, satisfying: 0.5mm≤A≤10mm.
[0157] The distance between the weld mark 242 and the weak portion 241, perpendicular to the thickness of the pressure relief portion 244, is limited to between 0.5 and 10 mm. This ensures that the weak portion 241 is effectively annealed during laser welding without being damaged. The distance A cannot be too small, for example, if the distance A is less than 0.5 mm, otherwise the weak portion 241 may be easily damaged during laser welding. The distance A cannot be too large, for example, if the distance A is greater than 10 mm, otherwise the weld mark 242 is too far from the weak portion 241, preventing the weak portion 241 from being annealed during laser welding.
[0158] In other embodiments, the weak portion 241 may be annealed by baking the weak portion 241 .
[0159] According to some embodiments of the present application, please refer to Figures 4 to 19.
[0160] The embodiment of the present application provides a pressure relief device 24 for a battery cell 20, and the pressure relief device 24 includes a pressure relief portion 244, a weak portion 241 and a weld stamp 242. The weak portion 241 is provided in the pressure relief portion 244, and the weak portion 241 is configured to crack when the battery cell 20 is depressurized. The weld stamp 242 is provided in the pressure relief portion 244, and the weld stamp 242 is configured to anneal the weak portion 241 during its molding. The pressure relief portion 244 of the pressure relief device 24 is provided with a weld stamp 242, and the weld stamp 242 requires high-temperature ablation during the molding process. This high temperature will act on the weak portion 241, and anneal the weak portion 241 (refine the material grains of the weak portion 241, release the internal stress of the material of the weak portion 241, and soften the weak portion 241 at the same time). Thus, under the same detonation pressure, the weak portion 241 of the pressure relief device 24 with the welded portion 242 can be thicker than the weak portion 241 of the pressure relief device 24 without the welded portion 242. Increasing the thickness of the weak portion 241 can improve resistance to external impacts and reduce the risk of premature valve opening. In addition, a thicker weak portion 241 requires less thickness to be machined, which reduces the difficulty of machining.
[0161] In a direction perpendicular to the thickness direction of the pressure relief portion 244, the spacing A between the weld stamp 242 and the weak portion 241 satisfies the following conditions: 0.5 mm ≤ A ≤ 10 mm. The spacing between the weld stamp 242 and the weak portion 241 in a direction perpendicular to the thickness direction of the pressure relief portion 244 is limited to between 0.5 and 10 mm, so that the weld stamp 242 can have a good annealing effect on the weak portion 241 during the molding process while not easily damaging the weak portion 241. It should be noted that the spacing A cannot be too small. For example, if the spacing A is less than 0.5 mm, the weak portion 241 can be easily damaged during the molding process of the weld stamp 242. The spacing A cannot be too large. For example, if the spacing A is greater than 10 mm, the weld stamp 242 is too far away from the weak portion 241, and the weak portion 241 cannot be annealed during the molding process of the weld stamp 242.
[0162] The welded portion 242 is disposed around the weak portion 241. The welded portion 242 surrounds the weak portion 241 and is located outside the weak portion 241. This allows high temperatures to be applied to the entire circumference of the weak portion 241 during the forming process, achieving a good annealing effect. This allows the weak portion 241 to quickly rupture when the internal pressure of the battery cell 20 reaches the detonation pressure, achieving rapid pressure relief.
[0163] An embodiment of the present application also provides a method 30 for manufacturing a pressure relief device. The pressure relief device 24 is used for a battery cell 20. The method 30 for manufacturing the pressure relief device includes: providing a pressure relief portion 244, the pressure relief portion 244 having a weak portion 241, and the weak portion 241 is configured to crack when the battery cell 20 releases pressure; and annealing the weak portion 241.
[0164] The above description is merely a preferred embodiment of the present application and is not intended to limit the present application. Various modifications and variations are possible for those skilled in the art. Any modifications, equivalent substitutions, or improvements made within the spirit and principles of the present application shall be included within the scope of protection of the present application.
Claims
1. A pressure relief device for a battery cell, wherein: include: Pressure relief unit; a weak portion, provided on the pressure relief portion, wherein the weak portion is configured to rupture when the battery cell releases pressure; The weld stamp portion is provided on the pressure relief portion, and the weld stamp portion is configured to anneal the weak portion during the forming process.
2. The pressure relief device according to claim 1, wherein: In a direction perpendicular to the thickness direction of the pressure relief portion, a distance A between the welded portion and the weak portion satisfies: 0.5 mm ≤ A ≤ 10 mm.
3. The pressure relief device according to claim 2, wherein: Also meets: 0.8mm≤A≤3mm.
4. The pressure relief device according to any one of claims 1 to 3, wherein: The weld print portion is arranged around the weak portion.
5. The pressure relief device according to any one of claims 1 to 3, wherein: The weak portion is arranged around the weld print portion.
6. The pressure relief device according to any one of claims 1 to 3, wherein: The pressure relief device includes two welded portions. Along a first direction, the weak portion is located between the two welded portions. The first direction is perpendicular to the thickness direction of the pressure relief portion.
7. The pressure relief device according to any one of claims 1 to 6, wherein: The weak portion is a closed structure extending along a closed track.
8. The pressure relief device according to any one of claims 1 to 7, wherein: The welding portion is a closed structure extending along a closed track.
9. The pressure relief device according to any one of claims 1 to 8, wherein: The weld printing portion includes a plurality of weld printing segments, and the plurality of weld printing segments are arranged at intervals along the circumference of the weak portion.
10. The pressure relief device according to any one of claims 1 to 9, wherein: The pressure relief portion is provided with a notch groove, and the pressure relief device forms the weak portion at the position of the notch groove.
11. The pressure relief device according to claim 10, wherein: Along the thickness direction of the pressure relief portion, the notched groove and the weld mark portion are located on both sides of the pressure relief portion.
12. The pressure relief device according to claim 10, wherein: Along the thickness direction of the pressure relief portion, the notched groove and the weld mark portion are located on the same side of the pressure relief portion.
13. The pressure relief device according to claim 10, wherein: The pressure relief device includes two welded portions, and along the thickness direction of the pressure relief portion, the two welded portions are located on both sides of the pressure relief portion.
14. A battery cell, wherein: Comprising a pressure relief device according to any one of claims 1-13.
15. A battery, wherein: The battery cell according to claim 14 is included.
16. An electrical device, wherein: The battery according to claim 15 is included for providing electrical energy.
17. A method for manufacturing a pressure relief device, wherein the pressure relief device is used for a battery cell, The manufacturing method of the pressure relief device comprises: providing a pressure relief portion having a weakened portion configured to rupture when the battery cell is depressurized; The weak portion is annealed.
18. The method for manufacturing a pressure relief device according to claim 17, wherein: In the step of annealing the weak portion: The pressure relief portion is welded by laser to anneal the weak portion.
19. The method for manufacturing a pressure relief device according to claim 18, wherein: After the pressure relief portion is laser welded, a weld mark portion can be formed on the pressure relief portion. In a direction perpendicular to the thickness direction of the pressure relief portion, a distance A between the weld mark portion and the weak portion satisfies: 0.5 mm ≤ A ≤ 10 mm.