Laser welding method, fuel cell and computer readable medium
By closing the laser emitter before the end point of the predetermined trajectory of the laser welding device, the perforation problem caused by heat concentration in bipolar plate welding is solved, and the welding strength and connection stability is achieved, fluid channel leakage is avoided, and welding efficiency is improved.
Patent Information
- Application Number
- CN202310531763.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-11
- Publication Date
- 2024-11-12
AI Technical Summary
During the bipolar plate welding of fuel cells, the concentration of heat caused by laser welding may lead to the burning and perforation of the bipolar plate, resulting in fluid channel leakage. In the prior art, incomplete fusion and insufficient welding strength are difficult to avoid in the short-range welds in the prior art. .
The welding strength is ensured by closing the laser emitter before the predetermined trajectory end of the laser welding device and keeping the alignment point moving along the trajectory, heat concentration is avoided and welding strength is ensured.
It effectively avoids the perforation defects of the bipolar plate welding, ensures the welding strength and connections, avoids leakage of fluid channels, and improves welding efficiency.
Smart Images

Figure CN118926688A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of fuel cells, and more particularly to a bipolar plate welding method in a fuel cell. Background Art
[0002] A fuel cell generally includes a plurality of battery cells, each of which includes a membrane electrode and a bipolar plate between the membrane electrodes. The bipolar plate divides the space between adjacent membrane electrode assemblies into an anode fluid channel, a cathode fluid channel and a cooling fluid channel.
[0003] Generally speaking, bipolar plates are formed by welding positive plates and negative plates, and the welds include peripheral welds along the periphery of the positive plates and negative plates and central welds in the central active areas of the positive plates and negative plates. The grooves are usually set between the flow channels of the bipolar plates. Since the groove width is narrow and the bipolar plates themselves are thin, laser welding is generally used. However, at the end of the weld, due to the concentrated energy, the bipolar plates may burn through and form perforations, which will cause leakage between the various fluid channels separated by the bipolar plates.
[0004] In order to avoid this defect, the prior art proposes a method of gradually increasing the laser power at the start of the weld and gradually reducing the laser power before the end point. However, this method is not feasible for short-range welds because it may result in incomplete fusion and insufficient weld strength. Summary of the invention
[0005] The purpose of this application is to solve or at least alleviate the problems existing in the prior art.
[0006] In one aspect, a laser welding method for a bipolar plate for a hydrogen fuel cell is provided, comprising: fixing the bipolar plate in place and affixing the to-be-welded regions of the bipolar plate; Determine a predetermined trajectory of an alignment point of a laser welding device on the area to be welded, wherein the predetermined trajectory includes a starting point and an end point; Moving the alignment point of the laser welding device from the starting point along the predetermined trajectory and activating the laser emitter of the laser welding device; and The laser emitter is turned off before the end point of the predetermined trajectory, and the alignment point is kept moving along the predetermined trajectory until the end point of the predetermined trajectory is reached.
[0007] A fuel cell is also provided, wherein the bipolar plates of the fuel cell are welded by the method according to an embodiment of the present invention.
[0008] A computer-readable medium is also provided, on which a computer program is recorded. When the computer program is read and executed by a processor of the laser welding device, the processor causes the laser welding device to execute the method according to an embodiment of the present invention.
[0009] The method and apparatus according to the embodiments of the present invention effectively avoid perforation defects in bipolar plate welding. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] The disclosure of the present application will become more easily understood with reference to the accompanying drawings. It is easy for those skilled in the art to understand that these drawings are only for illustrative purposes and are not intended to limit the scope of protection of the present application. In addition, similar numbers in the drawings are used to represent similar components, among which: Figure 1 shows a schematic diagram of a single plate with areas to be welded marked; Figure 2 A schematic cross-sectional view of the bipolar plate and membrane electrode assembly is shown; Figure 3 A schematic cross-sectional view of a bipolar plate during laser welding is shown; Figure 4 A schematic diagram showing a welding area and a predetermined trajectory according to one embodiment is shown; Figure 5 and Figure 6 shows laser transmitter power curves according to various embodiments; Figures 7 to 9 Schematic diagrams showing predetermined trajectories according to various embodiments; and Figures 10 to 13 A comparison of actual welds between a conventional welding method and a welding method according to an embodiment of the present invention is shown. DETAILED DESCRIPTION
[0011] First reference Figure 1 , showing a single plate with marked areas to be welded. The single plate 1 can be a cathode plate or an anode plate, which includes sealing areas at both ends and an activation area in the middle. The plate includes ports 11, 12, 13, 14, 15, 16 at the sealing areas at both ends, which are used for the entry and exit of hydrogen, oxygen and cooling water respectively.
[0012] like Figure 2 and Figure 3 As shown, in the active region, the plate includes a toothed shape to define a plurality of Figure 1 More specifically, as Figure 2As shown, the anode plate 1 includes protrusions 101, 102 and grooves 103 between adjacent protrusions 101, 102. The bipolar plates 1 and 2 need to be connected to each other before being assembled with the membrane electrode 3 and 4. In order to ensure a good connection between the bipolar plates 1 and 2, the bipolar plates 1 and 2 are connected by welds 17 along the periphery and welds 18 in the active zone. Figure 2 , an anode fluid channel 51 is defined between the anode plate 1 and the first membrane electrode 3, a cathode fluid channel 53 is defined between the cathode plate 2 and the second membrane electrode 4, and a cooling fluid channel 52 is defined between the first electrode plate 1 and the second electrode plate 2. Figure 3 As shown, the grooves of the anode plate 1 and the cathode plate 2 are closely attached, and the weld 18 in the active zone is mainly realized by laser welding the laser beam 3 along the grooves of the anode plate 1 and the cathode plate 2. The width a of the groove is, for example, less than 0.5 mm, for example, about 0.3 mm, and the thickness of the cathode plate and the anode plate is, for example, less than 0.1 mm, for example, 0.075 mm. If heat concentration occurs at the end point of welding, perforation occurs in the bipolar plate, which will cause leakage between the anode fluid channel 51 and the cathode fluid channel 53.
[0013] Continue to combine Figure 4 The following is an introduction to a laser welding method for bipolar plates for hydrogen fuel cells according to an embodiment of the present invention. The method comprises: fixing the bipolar plate in place and fitting the grooves between the flow channels in the area to be welded of the bipolar plate; determining a predetermined trajectory of the alignment point of the laser welding device on the area to be welded, the predetermined trajectory including a start point and an end point, Figure 4 As an example, the predetermined track 181 shown in FIG. 1 has a starting point 188 and an end point 189; the alignment point of the laser welding device is moved from the starting point 188 along the predetermined track 181, and the laser emitter of the laser welding device is started; and the laser emitter is turned off before the end point 189 of the predetermined track, and the alignment point is kept moving along the predetermined track until the end point 189 of the predetermined track is reached. According to the method of the present invention, the laser emitter is turned off before the end point 189 of the predetermined track of the alignment point, and the laser emitter is turned off before the end point 189 of the predetermined track of the alignment point. Figure 4 In the diagram, the laser transmitter's shut-off point is, for example, t 3 In other words, the method according to the present invention teaches that the alignment point is still moved a certain distance or time after the laser emitter is turned off. The inventors have found that this method can effectively avoid heat concentration and the resulting welding perforation problem, and can ensure the welding strength between the bipolar plates.
[0014] Continue to refer Figure 5 , which shows the laser transmitter power curve. Figure 5 In the embodiment shown, the laser transmitter is started with a first power P and maintains the first power P until t 3 The laser transmitter is turned off at time t 4It means that the alignment point stops moving, that is Figure 4 In addition, in this embodiment, the laser transmitter is activated when the alignment point is at the starting point of the predetermined trajectory, that is, the time point t at which the alignment point starts to move. 0 The start time of the laser transmitter is t 1 For the same time point. Continue to refer to Figure 6 An alternative embodiment of the laser transmitter power curve is introduced. In this alternative embodiment, the laser transmitter is at t 1 Start at the lowest power and gradually increase to the first power P(t 2 time point) and maintain the first power until the laser transmitter is turned off (t 3 In this embodiment, the laser transmitter is activated after the first delay time when the aiming point leaves the starting point of the predetermined trajectory, that is, the time point t at which the aiming point starts to move. 0 The start time of the laser transmitter is t 1 In some embodiments, the laser emitter is turned off at the time t 3 It can be associated with the end point of the predetermined trajectory, for example, the laser transmitter is turned off before the predetermined time or before the predetermined distance at the end point of the predetermined trajectory at the alignment point, for example, the total length of the weld is 4 mm, the welding speed is 1000 mm / s, and the total welding time is 4 ms (t 1 to 3 ), the predetermined time is greater than 0.5 ms, and the predetermined distance is greater than 0.5 mm. In some embodiments, the predetermined distance is greater than 1 / 10 of the total weld length, and the predetermined time is greater than 1 / 10 of the total welding time. In some embodiments, the predetermined time is greater than 0.5 ms, and the predetermined distance is greater than 0.5 mm. In actual operation, the weld length is pre-designed, and the predetermined trajectory is determined based on the required weld length. The time point t at which the laser emitter is turned off 3 and the time point t at which the trajectory ends 4 A variety of factors may be considered, and the value may also be determined experimentally or judged empirically.
[0015] In some embodiments, the laser welding device includes a laser emitter and a galvanometer, and the alignment point of the laser welding device is adjusted by the movement of the galvanometer. Therefore, the movement of the alignment point along the predetermined trajectory is achieved by moving the galvanometer of the laser welding device, and at t 3 After turning off the laser transmitter at time point, the galvanometer continues to move until time t 4 Stop the movement of the galvanometer. In some embodiments, the movement of the galvanometer is controlled so that the alignment point moves at a constant speed along a predetermined trajectory. In general, the laser emitter and the galvanometer of a laser welding device are turned off synchronously, while in the embodiments of the present application, the galvanometer is turned off later than the laser emitter, which can be achieved through software control.
[0016] Continue to refer Figures 7 to 9 In some embodiments, the predetermined trajectory is a straight line 181 ( Figure 7 ), alternatively, the predetermined trajectory may be a waveform along the flow channel direction (with the axis x parallel to the flow channel direction as the axis), wherein the waveform may be a sine wave 182 ( Figure 8 ), square wave or broken line wave 183 ( Fig. 9 ), the predetermined trajectory of the waveform can improve the welding strength.
[0017] Continue to refer Figures 10 to 13 ,in Fig.10 This is a photo of the weld when the laser emitter is turned off at the end of the predetermined trajectory (the laser emitter and the galvanometer are turned off synchronously). Fig.11 yes Fig.10 A magnified view of area C in the middle. Fig.10 and Fig.11 As can be seen in FIG. 1 , heat concentration and perforation occur at the end point of the predetermined trajectory. Fig.12 is a photo of a weld according to an embodiment of the present invention, Fig.13 for Fig.12 A magnified view of area D in the middle. Fig.12 and Fig.13 It can be seen that the weld depth is uniform and no heat concentration or perforation is found at the end of the weld.
[0018] According to other aspects of the present invention, a fuel cell is provided, wherein the bipolar plates of the fuel cell are welded by the method according to the embodiment of the present invention, and the weld seams on the obtained bipolar plates can be as follows: Fig.12 and Fig.13 As shown, it has a uniform depth. A further embodiment also includes a computer readable medium having a computer program recorded thereon, and when the computer program is read and executed by the processor of the laser welder device, the processor causes the laser welder device to perform the method according to the embodiment of the present invention. In some embodiments, the computer program causes the galvanometer to continue to move for a predetermined time after the laser emitter is turned off.
[0019] The device and method according to the present invention can achieve small deformation of the bipolar plate after welding, good forming and flatness, and the two bipolar plates are firmly connected without perforation after welding, thereby avoiding leakage of the bipolar plate and improving welding efficiency.
[0020] The specific embodiments described above in this application are only for more clearly describing the principle of this application, wherein each component is clearly shown or described to make the principle of the present invention easier to understand. Without departing from the scope of this application, those skilled in the art can easily make various modifications or changes to this application. Therefore, it should be understood that these modifications or changes should be included in the scope of patent protection of this application.
Claims
1. A laser welding method for bipolar plates for hydrogen fuel cells, include: Fixing the bipolar plates (1, 2) in place and making the areas to be welded of the bipolar plates (1, 2) fit together; Determining a predetermined trajectory of an alignment point of a laser welding device on the area to be welded, wherein the predetermined trajectory includes a starting point (188) and an end point (189); Moving the alignment point of the laser welding device from the starting point (188) along the predetermined trajectory and activating the laser emitter of the laser welding device; as well as The laser emitter is turned off before the end point (189) of the predetermined trajectory, and the alignment point is kept moving along the predetermined trajectory until the end point of the predetermined trajectory is reached.
2. The laser welding method according to claim 1, It is characterized in that The laser emitter is turned off before the alignment point is a predetermined time or a predetermined distance from the end point (189) of the predetermined trajectory; Optionally, the predetermined distance is greater than 1 / 10 of the total weld length, the predetermined time is greater than 1 / 10 of the total welding time, or The predetermined time is greater than 0.5 ms, and the predetermined distance is greater than 0.5 mm.
3. The laser welding method according to claim 1, It is characterized in that The method further includes: the laser emitter is started at a minimum power, gradually increased to a first power and maintained at the first power until the laser emitter is turned off, or the laser emitter is started at a first power and maintained at the first power until the laser emitter is turned off.
4. The laser welding method according to any one of claims 1 to 3, It is characterized in that The method further comprises: moving the alignment point by moving a galvanometer of the laser welding device, and continuing to move the galvanometer after turning off the laser emitter.
5. The laser welding method according to any one of claims 1 to 3, It is characterized in that The laser emitter is activated when the alignment point is at the starting point (188) of the predetermined trajectory, or the laser emitter is activated after a first delay time when the alignment point leaves the starting point (188) of the predetermined trajectory.
6. The laser welding method according to any one of claims 1 to 3, It is characterized in that The predetermined trajectory is a straight line parallel to the direction of the flow channel defined by the bipolar plate; or the predetermined trajectory is a waveform along the direction of the flow channel, wherein the waveform can be a sine wave, a square wave or a broken line wave.
7. The laser welding method according to any one of claims 1 to 3, It is characterized in that The alignment point moves along the predetermined trajectory at a constant speed.
8. The laser welding method according to any one of claims 1 to 3, It is characterized in that The bipolar plate includes sealing areas at both ends and an activation area in the middle, and each of the bipolar plates defines a plurality of parallel protrusions and grooves, and the area to be welded includes a groove located between adjacent protrusions in the activation area of the bipolar plate, wherein the bipolar plate has a thickness of less than 0.1 mm and a groove width of less than 0.5 mm.
9. A fuel cell, It is characterized in that The bipolar plates of the fuel cell are welded by the method according to any one of claims 1 to 8.
10. A computer readable medium having a computer program recorded thereon, It is characterized in that When the computer program is read and executed by the processor of the laser welding device, the processor enables the laser welding device to perform the method according to any one of claims 1 to 8.